{"id":105300,"date":"2017-10-05T14:00:31","date_gmt":"2017-10-05T06:00:31","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=105300"},"modified":"2017-10-05T08:51:13","modified_gmt":"2017-10-05T00:51:13","slug":"%e5%90%88%e8%82%a5%e7%a0%94%e7%a9%b6%e9%99%a2%e7%94%b0%e5%85%b4%e5%8f%8b%e5%9b%a2%e9%98%9f%ef%bc%9a%e5%9c%a8%e5%85%88%e8%bf%9b%e7%94%b5%e5%ad%90%e5%b0%81%e8%a3%85%e6%9d%90%e6%96%99%e7%a0%94%e7%a9%b6","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=105300","title":{"rendered":"\u5408\u80a5\u7814\u7a76\u9662\u7530\u5174\u53cb\u56e2\u961f\uff1a\u5728\u5148\u8fdb\u7535\u5b50\u5c01\u88c5\u6750\u6599\u7814\u7a76\u4e2d\u53d6\u5f97\u7cfb\u5217\u8fdb\u5c55"},"content":{"rendered":"<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u5408\u80a5\u7269\u8d28\u79d1\u5b66\u7814\u7a76\u9662\u5e94\u7528\u6280\u672f\u7814\u7a76\u6240\u5148\u8fdb\u6750\u6599\u4e2d\u5fc3\u7814\u53d1\u56e2\u961f\uff0c\u5728\u5148\u8fdb\u7535\u5b50\u5c01\u88c5\u6750\u6599\u7814\u7a76\u65b9\u9762\u53d6\u5f97\u7cfb\u5217\u8fdb\u5c55\uff0c\u76f8\u5173\u6210\u679c\u53d1\u8868\u5728<em><i>Composites Part A: Applied Science and Manufacturing<\/i><\/em>\u3001<em><i>Material Research Express<\/i><\/em>\u3001<em><i>Composites Part A: Applied Science and Manufacturing<\/i><\/em>\u3001<em><i>Composites Part A: Applied Science and Manufacturing<\/i><\/em>\u4e0a\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u56fe1 \u81ea\u7ec4\u88c5\u6d41\u7a0b\u56fe<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-105301\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/10\/1-9.jpg\" alt=\"\" width=\"500\" height=\"342\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/10\/1-9.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/10\/1-9-300x205.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p>\u4e8c\u4e59\u57fa\u4e09\u80fa\uff08DETA\uff09\u540c\u6b65\u6c28\u57fa\u5316\u8fd8\u539f\u6c27\u5316\u77f3\u58a8\u70ef\u4ee5\u53ca\u5176\u4e0e\u5e26\u76f8\u53cd\u7535\u6027\u7684\u4e73\u6db2\u9897\u7c92\u4e4b\u95f4\u7684\u9759\u7535\u81ea\u7ec4\u88c5\u6d41\u7a0b\u56fe<\/p>\n<p><strong>\u56fe2 \u7ed3\u6784\u53ca\u6027\u80fd\u793a\u610f\u56fe<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-105302\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/10\/2-9.jpg\" alt=\"\" width=\"500\" height=\"410\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/10\/2-9.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/10\/2-9-300x246.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p>\uff08a\uff09\u516d\u65b9\u6c2e\u5316\u787c@\u529f\u80fd\u5316\u77f3\u58a8\u70ef\u7ed3\u6784\u793a\u610f\u56fe<br \/>\n \uff08b\uff09\u590d\u5408\u6750\u6599\u5bfc\u70ed\u6027\u80fd\u793a\u610f\u56fe<br \/>\n \uff08c\uff09\u6a21\u62df\u590d\u5408\u6750\u6599\u5728\u5b9e\u9645\u7535\u5b50\u5668\u4ef6\u4e2d\u7684\u6563\u70ed\u6548\u679c<\/p>\n<p><strong>\u3010\u7814\u7a76\u5185\u5bb9\u3011<\/strong><\/p>\n<p>\u65b0\u578b\u5904\u7406\u5668\u7684\u8fd0\u884c\u901f\u5ea6\u8d8a\u6765\u8d8a\u5feb\uff0c\u9ad8\u6027\u80fd\u4eea\u5668\u7684\u80fd\u8017\u5728\u4e0d\u65ad\u589e\u52a0\uff0c\u8fd9\u8feb\u4f7f\u5ec9\u4ef7\u7684\u201c\u8f85\u52a9\u57fa\u677f\u201d\u6216\u201c\u4f9d\u8d56\u8bbe\u5907\u201d\u8981\u8ddf\u4e0a\u53d1\u5c55\u7684\u6b65\u4f10\uff0c\u70ed\u7ba1\u7406\u6280\u672f\u9010\u6e10\u6210\u4e3a\u5de5\u7a0b\u5e08\u4eec\u5fc5\u987b\u8003\u8651\u7684\u95ee\u9898\uff0c\u5bf9\u7edd\u7f18\u573a\u5408\u7528\u4f5c\u5c01\u88c5\u548c\u70ed\u754c\u9762\u6750\u6599\u4f7f\u7528\u7684\u9ad8\u70ed\u7edd\u7f18\u6750\u6599\u7684\u9700\u6c42\u8d8a\u6765\u8d8a\u9ad8\u3002\u5728\u534a\u5bfc\u4f53\u7ba1\u4e0e\u6563\u70ed\u5668\u7684\u5c01\u88c5\u3001\u7ba1\u82af\u7684\u4fdd\u62a4\u3001\u7ba1\u58f3\u7684\u5bc6\u5c01\uff0c\u6574\u6d41\u5668\u3001\u70ed\u654f\u7535\u963b\u5668\u7684\u5bfc\u70ed\u7edd\u7f18\uff0c\u5fae\u5305\u88c5\u4e2d\u591a\u5c42\u677f\u7684\u5bfc\u70ed\u7edd\u7f18\u7ec4\u88c5\u53ca\u65b0\u578b\u9ad8\u6563\u70ed\u7535\u8def\u57fa\u677f\u7b49\u65b9\u9762\u90fd\u9700\u8981\u4e0d\u540c\u5de5\u827a\u6027\u80fd\u7684\u5bfc\u70ed\u7edd\u7f18\u6750\u6599\u3002\u7814\u7a76\u548c\u5f00\u53d1\u9ad8\u5bfc\u70ed\u7edd\u7f18\u3001\u529b\u5b66\u6027\u80fd\u4f18\u5f02\u7684\u5bfc\u70ed\u6750\u6599\u663e\u5f97\u975e\u5e38\u91cd\u8981\u3002<\/p>\n<p>\u77f3\u58a8\u70ef\u3001\u78b3\u7eb3\u7c73\u7ba1\u7b49\u78b3\u6750\u6599\u5177\u5907\u4f18\u5f02\u7684\u4f20\u70ed\u6027\u80fd\uff0c\u4f46\u5176\u5bfc\u7535\u6027\u80fd\u9650\u5236\u4e86\u5b83\u4eec\u5728\u7535\u5b50\u6750\u6599\u4e2d\u7684\u5e94\u7528\u3002\u516d\u65b9\u6c2e\u5316\u787c\uff08hBN\uff09\u4f5c\u4e3a\u77f3\u58a8\u70ef\u7684\u7b49\u7535\u5b50\u4f53\uff0c\u5177\u6709\u4e00\u5b9a\u7684\u80fd\u9699\u3001\u539f\u5b50\u7ea7\u5e73\u6574\u7684\u8868\u9762\uff0c\u4e14\u8868\u9762\u6ca1\u6709\u60ac\u6302\u952e\uff0c\u9002\u5408\u4e0e\u77f3\u58a8\u70ef\u901a\u8fc7\u975e\u5171\u4ef7\u952e\u8fdb\u884c\u6742\u5316\u3002\u8bfe\u9898\u7ec4\u5728\u4e0d\u7834\u574f\u6750\u6599\u7ed3\u6784\u7684\u60c5\u51b5\u4e0b\uff0c\u8bbe\u8ba1\u81ea\u7ec4\u88c5\u5408\u6210\u51fa\u7cfb\u5217\u77f3\u58a8\u70ef\/\u516d\u65b9\u6c2e\u5316\u787c\uff08Graphene\/hBN\uff09\u6742\u5316\u7ed3\u6784\uff08\u56fe1-3\uff09\u3002\u5229\u7528\u5bfc\u70ed\u7ec4\u5206\u5728\u805a\u5408\u7269\u4e2d\u9009\u62e9\u6027\u5206\u5e03\uff0c\u83b7\u5f97\u7edd\u7f18\u5bfc\u70ed\u6742\u5316\u7ed3\u6784\uff08\u56fe4\uff09\u3002\u901a\u8fc7\u6a21\u62df\uff0c\u9a8c\u8bc1\u4e86\u8be5\u6742\u5316\u6750\u6599\u5728\u6563\u70ed\u9886\u57df\u7684\u5e94\u7528\u53ef\u884c\u6027\u3002\u8be5\u7c7b\u805a\u5408\u7269\u57fa\u590d\u5408\u6750\u6599\u62e5\u6709\u4f18\u5f02\u7684\u4f20\u70ed\u6027\u80fd\u548c\u7535\u7edd\u7f18\u6027\u80fd\uff0c\u8be5\u6750\u6599\u5728\u5148\u8fdb\u7535\u5b50\u5c01\u88c5\u9886\u57df\u4ee5\u53ca\u70ed\u7ba1\u7406\u9886\u57df\u5177\u6709\u5e7f\u9614\u7684\u5e94\u7528\u524d\u666f\u3002<\/p>\n<p>\u5728\u4e0a\u8ff0\u5de5\u4f5c\u7684\u57fa\u7840\u4e0a\uff0c\u5408\u80a5\u7814\u7a76\u9662\u5e94\u7528\u6240\u7814\u7a76\u5458\u7530\u5174\u53cb\u4e3b\u6301\u4e00\u9879\u56fd\u5bb6\u91cd\u70b9\u7814\u53d1\u8ba1\u5212\u9879\u76ee\uff0c\u5c06\u5e26\u9886\u8bfe\u9898\u7ec4\u8fdb\u4e00\u6b65\u5f00\u5c55\u5bfc\u70ed\u57fa\u677f\u6750\u6599\u7684\u7814\u7a76\u4e0e\u5e94\u7528\u5f00\u53d1\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/www.cas.cn\/syky\/201709\/t20170929_4616503.shtml\" target=\"_blank\" rel=\"noopener\">http:\/\/www.cas.cn\/syky\/201709\/t20170929_4616503.shtml<\/a><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/www.sciencedirect.com\/science\/article\/pii\/S1359835X17301379\" target=\"_blank\" rel=\"noopener\">Enhanced thermal conductivity of functionalized-graphene\/boron nitride flexible laminated composite adhesive via a facile latex approach<\/a>\uff08Compos Part A-Appl S,2017,DOI:10.1016\/j.compositesa.2017.03.033\uff09<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8Allen\u7f16\u8f91\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener noreferrer\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener noreferrer\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u6210\u679c\u7b80\u4ecb\u3011 \u8fd1\u65e5\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u5408\u80a5\u7269\u8d28\u79d1\u5b66\u7814\u7a76\u9662\u5e94\u7528\u6280\u672f\u7814\u7a76\u6240\u5148\u8fdb\u6750\u6599\u4e2d\u5fc3\u7814\u53d1\u56e2\u961f\uff0c\u5728\u5148\u8fdb\u7535\u5b50\u5c01\u88c5\u6750\u6599\u7814\u7a76\u65b9\u9762\u53d6\u5f97\u7cfb\u5217\u8fdb\u5c55\uff0c\u76f8\u5173\u6210\u679c\u53d1\u8868\u5728Composites &#8230;<\/p>\n","protected":false},"author":349,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-105300","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/105300"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/349"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=105300"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/105300\/revisions"}],"predecessor-version":[{"id":105413,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/105300\/revisions\/105413"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=105300"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=105300"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=105300"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}