{"id":109931,"date":"2017-11-08T06:30:22","date_gmt":"2017-11-07T22:30:22","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=109931"},"modified":"2017-11-06T20:09:22","modified_gmt":"2017-11-06T12:09:22","slug":"%e4%b8%ad%e7%a7%91%e9%99%a2%e7%89%a9%e7%90%86%e6%89%80%ef%bc%9a%e5%8f%91%e5%b1%95%e6%96%b0%e6%8a%80%e6%9c%af%e8%af%b1%e5%af%bc%e5%8d%95%e5%b1%82%e4%ba%8c%e7%a1%ab%e5%8c%96%e9%92%bc%e7%9b%b8%e5%8f%98","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=109931","title":{"rendered":"\u4e2d\u79d1\u9662\u7269\u7406\u6240\uff1a\u53d1\u5c55\u65b0\u6280\u672f\u8bf1\u5bfc\u5355\u5c42\u4e8c\u786b\u5316\u94bc\u76f8\u53d8"},"content":{"rendered":"<p><strong><b>\u3010<\/b><\/strong><strong><b>\u6210\u679c\u7b80\u4ecb<\/b><\/strong><strong><b>\u3011<\/b><\/strong><\/p>\n<p>\u8fd1\u671f\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u7269\u7406\u7814\u7a76\u6240\/\u5317\u4eac\u51dd\u805a\u6001\u7269\u7406\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\uff08\u7b79\uff09\u7eb3\u7c73\u7269\u7406\u4e0e\u5668\u4ef6\u5b9e\u9a8c\u5ba4N07\u7ec4\u535a\u58eb\u751f\u795d\u5efa\u7426\u5728\u7814\u7a76\u5458\u5f20\u5e7f\u5b87\u3001\u65f6\u4e1c\u971e\u7684\u6307\u5bfc\u4e0b\uff0c\u4e0e\u5317\u4eac\u5927\u5b66\u6559\u6388\u6c5f\u9896\u5408\u4f5c\uff0c\u5229\u7528\u4e00\u79cd\u7b80\u5355\u7684\u8868\u9762\u5904\u7406\u65b9\u6cd5\uff0c\u6210\u529f\u5b9e\u73b0\u4e862H\u52301T\u76f8\u7684\u53ef\u63a7\u8f6c\u53d8\u3002\u8fd9\u79cd\u65b9\u6cd5\u5229\u7528\u5177\u6709\u4e00\u5b9a\u52a8\u80fd\u7684\u6c29\u79bb\u5b50\u8f70\u51fb\u5355\u5c42\u4e8c\u786b\u5316\u94bc\u8868\u9762\uff0c\u6c29\u79bb\u5b50\u5c31\u50cf\u539f\u5b50\u4fdd\u9f84\u7403\u4e00\u6837\u53ef\u4ee5\u6709\u6548\u8bf1\u5bfc\u5355\u5c422H\u76f8\u4e8c\u786b\u5316\u94bc\u9876\u5c42\u786b-\u94bc\u952e\u7684\u626d\u8f6c\uff0c\u4ece\u800c\u5bfc\u81f4\u9876\u5c42\u786b\u539f\u5b50\u7684\u6574\u4f53\u6ed1\u79fb\uff0c\u4f7f\u4e8c\u786b\u5316\u94bc\u53d1\u751f2H-1T\u7684\u5c40\u57df\u76f8\u53d8\u3002\u501f\u52a9\u626b\u63cf\u96a7\u9053\u663e\u5fae\u955c\u6d4b\u91cf\uff0c\u4ed6\u4eec\u9a8c\u8bc1\u4e86\u540c\u65f6\u5b58\u5728\u7684\u5177\u6709\u76f4\u63a5\u5e26\u9699\u76842H\u76f8\u548c\u91d1\u5c5e\u6027\u76841T\u76f8\uff0c\u5e76\u786e\u8ba4\u6781\u5c11\u91cf\u7684\u786b\u539f\u5b50\u7a7a\u4f4d\u4f7f\u5f97\u8fd9\u79cd1T\/2H\u76f8\u5171\u5b58\u7684\u9a6c\u8d5b\u514b\u7ed3\u6784\u80fd\u591f\u8fbe\u5230\u7a33\u5b9a\u3002\u8fd9\u79cd\u65b9\u6cd5\u76f8\u8f83\u4e8e\u4f20\u7edf\u7684\u76f8\u53d8\u65b9\u6cd5\uff0c\u4e0d\u4f1a\u5f15\u5165\u591a\u4f59\u7684\u6742\u8d28\u4e14\u5feb\u901f\u3001\u53ef\u63a7\uff0c\u8fd8\u53ef\u4ee5\u5229\u7528\u56fe\u5f62\u5316\u6280\u672f\u4ec5\u4f7f\u6307\u5b9a\u533a\u57df\u53d1\u751f\u76f8\u53d8\u4ece\u800c\u6784\u5efa\u5f02\u8d28\u7ed3\u6784\u3002\u5c06\u8fd9\u79cd\u76f8\u53d8\u65b9\u6cd5\u7528\u5728\u573a\u6548\u5e94\u6676\u4f53\u7ba1\u4e2d\uff0c\u53ef\u4ee5\u4f7f\u4e0e\u91d1\u5c5e\u63a5\u89e6\u7684\u90e8\u5206\u8f6c\u53d8\u4e3a1T\u76f8\uff0c\u4ece\u800c\u51cf\u5c11\u63a5\u89e6\u7535\u963b\uff0c\u4f7f\u7535\u6d41\u5bc6\u5ea6\u63d0\u9ad8\u4e24\u500d\uff0c\u6676\u4f53\u7ba1\u7684\u5f00\u5173\u7279\u6027\u4e5f\u6709\u5f88\u5927\u63d0\u9ad8\u3002\u8fd9\u79cd\u57fa\u4e8e\u57fa\u4e8e\u539f\u5b50\u4fdd\u9f84\u7403\u6548\u5e94\u8bf1\u5bfc\u5355\u5c42\u4e8c\u786b\u5316\u94bc\u76f8\u53d8\u7684\u65b9\u6cd5\u6d01\u51c0\u3001\u9ad8\u6548\u3001\u53ef\u63a7\uff0c\u4e14\u548c\u73b0\u5b58\u7684\u5927\u89c4\u6a21\u96c6\u6210\u7535\u8def\u5236\u9020\u5de5\u827a\u517c\u5bb9\uff0c\u6709\u671b\u5e94\u7528\u4e8e\u4e8c\u786b\u5316\u94bc\u7535\u5b50\u5b66\u3001\u5149\u5b66\u3001\u80fd\u6e90\u7b49\u9886\u57df\u3002\u8be5\u5de5\u4f5c\u4ee5\u9898\u4e3a\u201cArgon Plasma Induced Phase Transition in Monolayer MoS<sub>2<\/sub>\u201d\u53d1\u8868\u4e8eJournal of the American Chemical Society\u4e0a\u3002 \u00a0\u3000<\/p>\n<p><strong><b>\u3010<\/b><\/strong><strong><b>\u56fe\u6587\u5bfc\u8bfb<\/b><\/strong><strong><b>\u3011<\/b><\/strong><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>1 <\/b><\/strong><strong><b>\u793a\u610f\u56fe\u53ca\u6027\u80fd\u8868\u5f81<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-109932\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/1-4.png\" alt=\"\" width=\"600\" height=\"429\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/1-4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/1-4-300x215.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\uff08a\uff09\u6c29\u7b49\u79bb\u5b50\u4f53\u76f8\u53d8\u5904\u7406\u793a\u610f\u56fe\u3002<\/p>\n<p>\uff08b\uff0cc\uff09\u4e0d\u540c\u76f8\u53d8\u5904\u7406\u65f6\u95f4\u7684\u62c9\u66fc\uff08b\uff09\u548c\u8367\u5149\u8868\u5f81\uff08c\uff09\u3002<\/p>\n<p>\uff08d\uff09\u76f8\u53d8\u524d\u540eXPS\u8868\u5f81\u3002<\/p>\n<p><strong><b>\u56fe2 <\/b><\/strong><strong><b>\u6027\u80fd\u8868\u5f81<\/b><\/strong><\/p>\n<p><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-109933\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/2-2.png\" alt=\"\" width=\"600\" height=\"410\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/2-2.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/2-2-300x205.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p>\uff08a\uff09\u539f\u59cb2H\u76f8\u4e8c\u786b\u5316\u94bc\u6837\u54c1STM\u8868\u5f81\u3002<\/p>\n<p>\uff08b\uff0cc\uff09\u76f8\u53d8\u5904\u7406\u540e\u6837\u54c1STM\u8868\u5f81\u3002<\/p>\n<p>\uff08d\uff0ce\uff09\u76f8\u53d8\u5904\u7406\u524d\u540eSTS\u8c31\u3002<\/p>\n<p><strong><b>\u3010\u7814\u7a76\u5185\u5bb9\u3011<\/b><\/strong><\/p>\n<p>\u5355\u5c42\u4e8c\u786b\u5316\u94bc\u662f\u4e00\u79cd\u5178\u578b\u7684\u4e8c\u7ef4\u8fc7\u6e21\u91d1\u5c5e\u786b\u5c5e\u5316\u7269\uff0c\u7531\u4e8e\u5176\u7279\u6b8a\u7684\u80fd\u5e26\u7ed3\u6784\u3001\u534a\u5bfc\u4f53\u6027\u8d28\u7b49\uff0c\u5728\u7eb3\u7c73\u7535\u5b50\u5668\u4ef6\u548c\u5149\u7535\u5b50\u5b66\u7b49\u8bf8\u591a\u9886\u57df\u5177\u6709\u5e7f\u9614\u7684\u5e94\u7528\u524d\u666f\u3002\u5355\u5c42\u4e8c\u786b\u5316\u94bc\u7531\u4e09\u4e2a\u539f\u5b50\u5c42\uff08\u786b-\u94bc-\u786b\uff09\u5806\u53e0\u800c\u6210\uff0c\u4e0d\u540c\u7684\u5806\u53e0\u6b21\u5e8f\u4f7f\u5176\u6784\u6210\u4e24\u79cd\u4e0d\u540c\u7684\u76f8\uff0c\u53732H\u548c1T\u76f8\u30022H\u76f8\u5c42\u4e0e\u5c42\u4e4b\u95f4\u6309\u7167ABA\u5806\u579b\uff0c\u91d1\u5c5e\u539f\u5b50\u4e3a\u4e09\u68f1\u67f1\u914d\u4f4d\uff0c\u5177\u67092.2\u00a0eV\u7684\u534a\u5bfc\u4f53\u6027\u3002\u800c1T\u76f8\u5bf9\u5e94ABC\u7684\u5806\u579b\u65b9\u5f0f\uff0c\u91d1\u5c5e\u539f\u5b50\u4e3a\u516b\u9762\u4f53\u914d\u4f4d\uff0c\u5448\u73b0\u91d1\u5c5e\u6027\u3002\u53ef\u63a7\u5730\u5b9e\u73b02H\u548c1T\u4e4b\u95f4\u7684\u76f8\u53d8\u4e0d\u4ec5\u5bf9\u7814\u7a76\u5355\u5c42\u4e8c\u786b\u5316\u94bc\u7684\u672c\u5f81\u7269\u7406\u6027\u8d28\u4e5f\u5bf9\u76f8\u5173\u5e94\u7528\u5177\u6709\u91cd\u8981\u610f\u4e49\u3002<\/p>\n<p>\u8be5\u9879\u7814\u7a76\u5de5\u4f5c\u5f97\u5230\u56fd\u5bb6\u91cd\u70b9\u7814\u53d1\u8ba1\u5212\u3001\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u3001\u4e2d\u79d1\u9662\u524d\u6cbf\u79d1\u5b66\u91cd\u70b9\u7814\u7a76\u9879\u76ee\u4ee5\u53ca\u4e2d\u79d1\u9662\u6218\u7565\u6027\u5148\u5bfc\u79d1\u6280\u4e13\u9879\u7684\u8d44\u52a9\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/www.cas.cn\/syky\/201711\/t20171102_4620343.shtml\" target=\"_blank\" rel=\"noopener\">http:\/\/www.cas.cn\/syky\/201711\/t20171102_4620343.shtml<\/a><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/10.1021\/jacs.7b05765\" target=\"_blank\" rel=\"noopener\">Argon Plasma Induced Phase Transition in Monolayer MoS2 <\/a>(J. Am. Chem. Soc, 2017, DOI:10.1021\/jacs.7b05765)<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u77f3\u5c0f\u6885\u7f16\u8f91\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u6210\u679c\u7b80\u4ecb\u3011 \u8fd1\u671f\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u7269\u7406\u7814\u7a76\u6240\/\u5317\u4eac\u51dd\u805a\u6001\u7269\u7406\u56fd\u5bb6\u5b9e\u9a8c\u5ba4\uff08\u7b79\uff09\u7eb3\u7c73\u7269\u7406\u4e0e\u5668\u4ef6\u5b9e\u9a8c\u5ba4N07\u7ec4\u535a\u58eb\u751f\u795d\u5efa\u7426\u5728\u7814\u7a76\u5458\u5f20\u5e7f\u5b87\u3001\u65f6\u4e1c\u971e\u7684\u6307\u5bfc\u4e0b\uff0c\u4e0e\u5317\u4eac\u5927\u5b66\u6559\u6388\u6c5f&#8230;<\/p>\n","protected":false},"author":2832,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[2502],"class_list":["post-109931","post","type-post","status-publish","format-standard","hentry","category-keji","tag-2502"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/109931"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2832"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=109931"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/109931\/revisions"}],"predecessor-version":[{"id":110479,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/109931\/revisions\/110479"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=109931"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=109931"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=109931"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}