{"id":111255,"date":"2017-11-15T06:30:38","date_gmt":"2017-11-14T22:30:38","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=111255"},"modified":"2017-11-15T13:12:57","modified_gmt":"2017-11-15T05:12:57","slug":"%e4%b8%ad%e7%a7%91%e9%99%a2%e5%90%88%e8%82%a5%e7%a0%94%e7%a9%b6%e9%99%a2%ef%bc%9a%e5%85%89%e5%82%ac%e5%8c%96%e5%88%b6%e6%b0%a2%e6%9d%90%e6%96%99%e7%a0%94%e7%a9%b6%e5%8f%96%e5%be%97%e8%bf%9b%e5%b1%95","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=111255","title":{"rendered":"\u4e2d\u79d1\u9662\u5408\u80a5\u7814\u7a76\u9662\uff1a\u5149\u50ac\u5316\u5236\u6c22\u6750\u6599\u7814\u7a76\u53d6\u5f97\u8fdb\u5c55"},"content":{"rendered":"<p><strong><b>\u3010<\/b><\/strong><strong><b>\u6210\u679c\u7b80\u4ecb<\/b><\/strong><strong><b>\u3011<\/b><\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u5408\u80a5\u7269\u8d28\u79d1\u5b66\u7814\u7a76\u9662\u5e94\u7528\u6280\u672f\u7814\u7a76\u6240\u5148\u8fdb\u6750\u6599\u4e2d\u5fc3\u7814\u7a76\u56e2\u961f\uff0c\u5728\u91d1\u5c5e\/\u534a\u5bfc\u4f53\u590d\u5408\u5149\u50ac\u5316\u5236\u6c22\u6750\u6599\u7814\u7a76\u65b9\u9762\u53d6\u5f97\u4e86\u65b0\u8fdb\u5c55\uff0c\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5Photocatalytic hydrogen production over plasmonic AuCu\/CaIn<sub>2<\/sub>S<sub>4<\/sub>\u00a0composites with different AuCu atomic arrangements\u4e3a\u9898\uff0c\u53d1\u8868\u5728Applied Catalysis B-Environmental\u4e0a\u3002 \u00a0\u3000\u3000 \u00a0\u3000<\/p>\n<p><strong><b>\u3010<\/b><\/strong><strong><b>\u56fe\u6587\u5bfc\u8bfb<\/b><\/strong><strong><b>\u3011<\/b><\/strong><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>1 \u5177\u6709\u4e0d\u540cAuCu\u539f\u5b50\u6392\u5217\u65b9\u5f0f\u7684AuCu\/CaIn2S4\u590d\u5408\u5149\u50ac\u5316\u5242\u5728\u53ef\u89c1\u5149\u548c\u4e0d\u540c\u6ce2\u957f\u5165\u5c04\u5149\u4e0b\u7684\u5149\u50ac\u5316\u5236\u6c22\u6027\u80fd\u00a0<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-111256\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/1-43.jpg\" alt=\"\" width=\"600\" height=\"338\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/1-43.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/1-43-300x169.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u56fe2 <\/b><\/strong><strong><b>\u6027\u80fd\u8868\u5f81<\/b><\/strong><\/p>\n<p><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-111257\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/2-22.png\" alt=\"\" width=\"600\" height=\"486\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/2-22.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/2-22-300x243.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p>CIS, A5\/CIS, C5\/CIS, C1\/A4\/CIS\u548cA4C1\/CIS\u5149\u50ac\u5316\u5242\u7684XRD\u56fe\u8c31<\/p>\n<p><strong><b>\u3010\u7814\u7a76\u5185\u5bb9\u3011<\/b><\/strong><\/p>\n<p>\u5149\u50ac\u5316\u53ef\u5b9e\u73b0\u592a\u9633\u80fd\u5230\u5316\u5b66\u80fd\u7684\u8f6c\u5316\uff08\u5982\u5149\u50ac\u5316\u5206\u89e3\u6c34\u5236\u6c22\uff09\uff0c\u662f\u83b7\u53d6\u65b0\u80fd\u6e90\u7684\u7406\u60f3\u9014\u5f84\u4e4b\u4e00\uff0c\u5f00\u53d1\u5bbd\u5149\u8c31\u54cd\u5e94\u3001\u9ad8\u8f7d\u6d41\u5b50\u5206\u79bb\u6548\u7387\u7684\u5149\u50ac\u5316\u6750\u6599\uff0c\u662f\u5b9e\u73b0\u592a\u9633\u80fd\u9ad8\u6548\u5149\u5316\u5b66\u8f6c\u5316\u7684\u524d\u63d0\u548c\u57fa\u7840\u3002\u7814\u7a76\u4eba\u5458\u5236\u5907\u4e86\u5177\u6709\u4e0d\u540cAuCu\u539f\u5b50\u6392\u5217\u65b9\u5f0f\uff08\u5408\u91d1\u7ed3\u6784\u548c\u6838\u58f3\u7ed3\u6784\uff09\u7684AuCu\/CaIn<sub>2<\/sub>S<sub>4<\/sub>\u590d\u5408\u5149\u50ac\u5316\u6750\u6599\uff0c\u53d1\u73b0AuCu\u53cc\u91d1\u5c5e\u7eb3\u7c73\u9897\u7c92\u7684\u8d1f\u8f7d\u53ef\u4ee5\u6709\u6548\u6291\u5236\u5149\u751f\u8f7d\u6d41\u5b50\u7684\u590d\u5408\uff0cAuCu\u7684\u8868\u9762\u7b49\u79bb\u5171\u632f\u6548\u5e94\u8fd8\u53ef\u4ee5\u62d3\u5bbd\u5149\u50ac\u5316\u6750\u6599\u5bf9\u592a\u9633\u5149\u7684\u5229\u7528\u8303\u56f4\uff08\u6700\u957f\u5149\u50ac\u5316\u5236\u6c22\u54cd\u5e94\u6ce2\u957f\u53ef\u8fbe\u5230600\u00a0nm\uff09\u3002\u5176\u4e2d\uff0cAuCu\u5408\u91d1\u7ed3\u6784\u5728\u8f7d\u6d41\u5b50\u5206\u79bb\u6548\u7387\u3001\u5149\u8c31\u54cd\u5e94\u8303\u56f4\u7b49\u65b9\u9762\u8981\u4f18\u4e8eAuCu\u6838\u58f3\u7ed3\u6784\uff0c\u8868\u73b0\u51fa\u66f4\u597d\u7684\u5149\u50ac\u5316\u5236\u6c22\u6027\u80fd\uff0c\u6700\u9ad8\u4ea7\u6c22\u901f\u7387\u8fbe\u5230452.8\u00a0\u03bcmol\/h\uff08\u621645.28\u00a0mmol\/hg\uff09\u3002\u8be5\u7814\u7a76\u5bf9\u57fa\u4e8e\u91d1\u5c5e\/\u534a\u5bfc\u4f53\u7ed3\u6784\u7684\u8868\u9762\u7b49\u79bb\u5149\u50ac\u5316\u6750\u6599\u7684\u5408\u7406\u8bbe\u8ba1\u5177\u6709\u53c2\u8003\u610f\u4e49\u3002 \u00a0\u3000\u3000\u7814\u7a76\u5de5\u4f5c\u5f97\u5230\u4e86\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u3001\u5b89\u5fbd\u7701\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u3001\u5408\u80a5\u7814\u7a76\u9662\u9662\u957f\u57fa\u91d1\u7b49\u7684\u8d44\u52a9\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/www.cas.cn\/syky\/201711\/t20171108_4621186.shtml\" target=\"_blank\" rel=\"noopener\">http:\/\/www.cas.cn\/syky\/201711\/t20171108_4621186.shtml<\/a><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/www.sciencedirect.com\/science\/article\/pii\/S0926337317310196\" target=\"_blank\" rel=\"noopener\">Photocatalytic hydrogen production over plasmonic AuCu\/CaIn2S4 composites with different AuCu atomic arrangements <\/a>(Applied Catalysis B-Environmental, 2017, DOI:https:\/\/doi.org\/10.1016\/j.apcatb.2017.10.045)<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u77f3\u5c0f\u6885\u7f16\u8f91\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener\">\u6d4b\u8bd5\u8c37<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u6210\u679c\u7b80\u4ecb\u3011 \u8fd1\u65e5\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u5408\u80a5\u7269\u8d28\u79d1\u5b66\u7814\u7a76\u9662\u5e94\u7528\u6280\u672f\u7814\u7a76\u6240\u5148\u8fdb\u6750\u6599\u4e2d\u5fc3\u7814\u7a76\u56e2\u961f\uff0c\u5728\u91d1\u5c5e\/\u534a\u5bfc\u4f53\u590d\u5408\u5149\u50ac\u5316\u5236\u6c22\u6750\u6599\u7814\u7a76\u65b9\u9762\u53d6\u5f97\u4e86\u65b0\u8fdb\u5c55\uff0c\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5Phot&#8230;<\/p>\n","protected":false},"author":2832,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[2529],"class_list":["post-111255","post","type-post","status-publish","format-standard","hentry","category-jiedu","tag-2529"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/111255"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2832"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=111255"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/111255\/revisions"}],"predecessor-version":[{"id":112035,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/111255\/revisions\/112035"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=111255"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=111255"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=111255"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}