{"id":113584,"date":"2017-11-27T06:30:06","date_gmt":"2017-11-26T22:30:06","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=113584"},"modified":"2018-02-06T10:49:17","modified_gmt":"2018-02-06T02:49:17","slug":"%e7%ba%b3%e7%b1%b3%e6%9d%90%e6%96%99%e5%89%8d%e6%b2%bf%e7%a0%94%e7%a9%b6%e6%88%90%e6%9e%9c%e7%b2%be%e9%80%89%e3%80%90%e7%ac%ac4%e6%9c%9f%e3%80%91","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=113584","title":{"rendered":"\u7eb3\u7c73\u6750\u6599\u524d\u6cbf\u7814\u7a76\u6210\u679c\u7cbe\u9009\u3010\u7b2c4\u671f\u3011"},"content":{"rendered":"<p><strong>1\u3001ACS Nano: \u5316\u5b66\u6c14\u76f8\u6c89\u79ef\u6cd5\u5236\u5907\u5927\u9762\u79ef\u5355\u6676\u516d\u65b9\u6c2e\u5316\u787c<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-113560\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/1-48.png\" alt=\"\" width=\"600\" height=\"585\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/1-48.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/1-48-300x293.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><br \/>\n \u516d\u65b9\u6c2e\u5316\u787c(h-BN)\u662f\u4e00\u79cd\u4e0e\u77f3\u58a8\u70ef\u5177\u6709\u76f8\u4f3c\u6676\u683c\u7ed3\u6784\u7684\u5c42\u72b6\u6750\u6599\uff0c\u8fd9\u4e9b\u5c42\u7531\u8702\u7a9d\u72b6\u6392\u5217\u7684\u787c\u539f\u5b50\u548c\u6c2e\u539f\u5b50\u4ea4\u66ff\u7ec4\u6210\uff0c\u787c\u548c\u6c2e\u4e4b\u95f4\u7262\u56fa\u7684\u952e\u5408\u4f7f\u5176\u6210\u4e3a\u5bbd\u5e26\u9699\u7684\u6750\u6599\u3002\u7136\u800c\uff0c\u5728\u5b9e\u9645\u751f\u4ea7\u8fc7\u7a0b\u4e2d\uff0c\u5927\u591a\u6570\u65b9\u6cd5\u4e0d\u53ef\u907f\u514d\u5730\u4ea7\u751f\u5927\u91cf\u5c0fh-BN\u57df\uff0c\u5bfc\u81f4\u8fb9\u754c\u7f3a\u9677\u5bc6\u5ea6\u589e\u52a0\uff0c\u5668\u4ef6\u5747\u5300\u6027\u5dee\u3002\u8fd1\u65e5\uff0c\u7f8e\u56fd<strong>\u5eb7\u5948\u5c14\u5927\u5b66<\/strong>\u7684<strong>Michael G. Spencer<\/strong> (<strong>\u901a\u8baf\u4f5c\u8005<\/strong>)\u7b49\u4eba\u62a5\u9053\u4e86\u5236\u5907\u516d\u65b9\u6c2e\u5316\u787c\u7684\u65b0\u65b9\u6cd5\u3002\u4f5c\u8005\u901a\u8fc7\u4f4e\u538b\u5316\u5b66\u6c14\u76f8\u6c89\u79ef\u6280\u672f\uff0c\u5728\u591a\u6676\u94dc\u4e0a\u5236\u5907\u5355\u5c42\u7684\u3001\u53cc\u5c42\u7684\u548c\u4e09\u5c42\u7684\u5355\u6676\u516d\u65b9\u6c2e\u5316\u787c\u3002\u5355\u5c42h-BN\u7684\u6a2a\u5411\u5c3a\u5bf8\u4e3a300\u03bcm\uff0c\u53cc\u5c42\u548c\u4e09\u5c42h-BN\u7684\u6a2a\u5411\u5c3a\u5bf8\u5206\u522b\u4e3a60\u03bcm\u548c40\u03bcm\uff0c\u6bd4\u5178\u578b\u7684h-BN\u591a\u5c42\u7ed3\u6784\u5927\u51fa\u4e24\u4e2a\u6570\u91cf\u7ea7\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/10.1021\/acsnano.7b04841\" target=\"_blank\" rel=\"noopener\">Chemical Vapor Deposition Growth of Large Single-Crystal Mono-, Bi-, Tri-Layer Hexagonal Boron Nitride and Their Interlayer Stacking <\/a>(ACS Nano, 2017, DOI: 10.1021\/acsnano.7b04841\uff09<\/p>\n<p><strong>2\u3001Nature Communications: \u78b3\u7eb3\u7c73\u7ba1\u6fc0\u5b50\u7edd\u7f18\u4f53<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-113561\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/2-69.jpg\" alt=\"\" width=\"600\" height=\"1229\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/2-69.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/2-69-146x300.jpg 146w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/2-69-500x1024.jpg 500w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p> \u5728\u534a\u5bfc\u4f53\u4e2d\uff0c\u5982\u679c\u4e00\u4e2a\u7535\u5b50\u4ece\u6ee1\u7684\u4ef7\u5e26\u6fc0\u53d1\u5230\u7a7a\u7684\u5bfc\u5e26\u4e0a\u53bb\uff0c\u5219\u5728\u4ef7\u5e26\u5185\u4ea7\u751f\u4e00\u4e2a\u7a7a\u7a74\uff0c\u800c\u5728\u5bfc\u5e26\u5185\u4ea7\u751f\u4e00\u4e2a\u7535\u5b50\uff0c\u4ece\u800c\u5f62\u6210\u4e00\u4e2a\u7535\u5b50-\u7a7a\u7a74\u5bf9\u3002\u7a7a\u7a74\u5e26\u6b63\u7535\uff0c\u7535\u5b50\u5e26\u8d1f\u7535\uff0c\u5b83\u4eec\u4e4b\u95f4\u7684\u5e93\u4ed1\u4e92\u76f8\u5438\u5f15\u4f5c\u7528\u5728\u4e00\u5b9a\u7684\u6761\u4ef6\u4e0b\u4f1a\u4f7f\u5b83\u4eec\u5728\u7a7a\u95f4\u4e0a\u675f\u7f1a\u5728\u4e00\u8d77\uff0c\u8fd9\u6837\u5f62\u6210\u7684\u590d\u5408\u4f53\u79f0\u4e3a\u6fc0\u5b50\u3002\u78b3\u7eb3\u7c73\u7ba1\u4e3a\u4f4e\u80fd\u91cf\u7535\u5b50\u7684\u77f3\u58a8\u70ef\u5706\u67f1\u4f53\uff0c\u7531\u4e8e\u65e0\u6548\u7684\u4ecb\u7535\u5c4f\u853d\u548c\u4e00\u7ef4\u6027\u5bfc\u81f4\u7684\u589e\u5f3a\u76f8\u4e92\u4f5c\u7528\uff0c\u663e\u793a\u51fa\u5f3a\u70c8\u7684\u6fc0\u5b50\u6548\u5e94\u3002\u8fd1\u65e5\uff0c\u6765\u81ea\u610f\u5927\u5229<strong>CNR-NANO<\/strong>\u7684<strong>Massimo Rontani<\/strong>(<strong>\u901a\u8baf\u4f5c\u8005<\/strong>)\u7b49\u4eba\u901a\u8fc7\u5bf9\u96f6\u5e26\u9699\u78b3\u7eb3\u7c73\u7ba1\u7684\u591a\u4f53\u6270\u52a8\u7406\u8bba\u4ee5\u53ca\u91cf\u5b50\u8499\u7279\u5361\u7f57\u7684\u7b2c\u4e00\u539f\u7406\u8ba1\u7b97\uff0c\u53d1\u73b0\u4e86\u6fc0\u5b50\u7edd\u7f18\u4f53\u3002\u6fc0\u5b50\u53ef\u987a\u5e8f\u8c03\u8282\u4e24\u4e2a\u78b3\u539f\u5b50\u6676\u683c\u4e4b\u95f4\u7684\u7535\u8377\uff0c\u5176\u5c3a\u5ea6\u4e0e\u7ba1\u534a\u5f84\u7684\u5012\u6570\u6210\u6bd4\u4f8b\uff0c\u540c\u65f6\u4f9d\u8d56\u4e8e\u8f74\u5411\u78c1\u573a\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>\uff1a<a href=\"https:\/\/www.nature.com\/articles\/s41467-017-01660-8\" target=\"_blank\" rel=\"noopener\">Carbon nanotubes as excitonic insulator <\/a>(Nat. Commun., 2017, DOI: 10.1038\/s41467-017-01660-8\uff09<\/p>\n<p><strong>3\u3001Nature Communications: \u53cc\u5c42MoS<sub>2<\/sub>\u7684\u5e94\u53d8-\u526a\u5207\u8026\u5408<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-113562\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/3-62.jpg\" alt=\"\" width=\"600\" height=\"894\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/3-62.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/3-62-201x300.jpg 201w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><br \/>\n \u8fc7\u6e21\u91d1\u5c5e\u4e8c\u786b\u5316\u5408\u7269\u5c42\u72b6\u6750\u6599\u7531\u4e8e\u9762\u5185\u548c\u9762\u5916\u539f\u5b50\u95f4\u76f8\u4e92\u4f5c\u7528\u5f3a\u5ea6\u7684\u5dee\u5f02\u800c\u5177\u6709\u5404\u5411\u5f02\u6027\u7684\u529b\u5b66\u6027\u80fd\uff0c\u673a\u68b0\u6270\u52a8\u5bf9\u5176\u5c42\u5185\u6216\u5c42\u95f4\u76f8\u4e92\u4f5c\u7528\u7684\u5f71\u54cd\u5df2\u88ab\u4f17\u591a\u5b66\u8005\u6240\u7814\u7a76\uff0c\u7136\u800c\u5c42\u4e0e\u5c42\u4e4b\u95f4\u7684\u76f8\u4e92\u5173\u7cfb\u5374\u5f88\u5c11\u63d0\u53ca\u3002\u8fd1\u65e5\uff0c\u6765\u81ea\u97e9\u56fd<strong>\u897f\u6c5f\u5927\u5b66<\/strong>\u7684<strong>Hyeonsik Cheong<\/strong>\u548c<strong>\u97e9\u56fd\u9ad8\u7b49\u7814\u7a76\u9662<\/strong>\u7684<strong>Young-Woo Son<\/strong>(<strong>\u5171\u540c\u901a\u8baf\u4f5c\u8005<\/strong>)\u7b49\u4eba\u63d0\u51fa\u4e86\u5c42\u72b6\u6750\u6599\u5728\u9762\u5185\u5355\u5411\u5e94\u53d8\u548c\u5c42\u95f4\u526a\u5207\u4e4b\u95f4\u5177\u6709\u4e0d\u53ef\u907f\u514d\u7684\u8026\u5408\u6548\u5e94\u3002\u4f5c\u8005\u901a\u8fc7\u6d4b\u91cf\u5e94\u53d8\u4e0b\u53cc\u5c42MoS2\u526a\u5207\u6a21\u5f0f\u7684\u62c9\u66fc\u4f4d\u79fb\u786e\u8ba4\u8fd9\u4e2a\u6548\u5e94\u3002\u6b64\u5916\uff0c\u4f5c\u8005\u8fd8\u83b7\u5f97\u4e00\u4e2a\u672a\u63a2\u7d22\u7684\u975e\u5bf9\u89d2\u7ebf\u5f39\u6027\u5e38\u6570\uff0c\u8868\u660e\u62c9\u66fc\u5149\u8c31\u53ef\u4ee5\u786e\u5b9a\u51e0\u4e4e\u6240\u6709\u5c42\u72b6\u6750\u6599\u7684\u529b\u5b66\u5e38\u6570\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>: <a href=\"https:\/\/www.nature.com\/articles\/s41467-017-01487-3\" target=\"_blank\" rel=\"noopener\">Strain-shear coupling in bilayer MoS<sub>2 <\/sub><\/a>(Nat. Commun., 2017, DOI: 10.1038\/s41467-017-01487-3\uff09<\/p>\n<p><strong>4\u3001Nano Lett.\uff1a\u5364\u5316\u94c5\u7eb3\u7c73\u7ebf\u7684\u81ea\u50ac\u5316\u6c14\u6db2\u56fa\u751f\u957f\u53ca\u5176\u6742\u5316\u9499\u949b\u77ff\u7ed3\u6784\u8f6c\u53d8<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-113563\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/4-56.jpg\" alt=\"\" width=\"600\" height=\"350\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/4-56.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/4-56-300x175.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><br \/>\n \u94c5\u5364\u5316\u7269\u9499\u949b\u77ff(LHPs)\u5728\u5149\u7535\u5668\u4ef6\u3001\u5149\u7535\u63a2\u6d4b\u5668\u3001\u53d1\u5149\u4e8c\u6781\u7ba1\u548c\u6fc0\u5149\u5668\u4e2d\u5177\u6709\u826f\u597d\u7684\u5e94\u7528\u524d\u666f\u3002\u901a\u8fc7\u6c14\u76f8\u6cd5\u53ef\u4ee5\u7cbe\u786e\u5730\u63a7\u5236LHP\u7eb3\u7c73\u7ebf(NW)\u7684\u7ed3\u6676\u5ea6\u3001\u76f8\u7ec4\u6210\u548c\u5f62\u6001\u3002\u8fd1\u65e5\uff0c\u7f8e\u56fd<strong>\u5317\u5361\u7f57\u6765\u7eb3\u5927\u5b66\u6559\u5802\u5c71\u5206\u6821<\/strong>\u7684<strong>James F. Cahoon<\/strong>(<strong>\u901a\u8baf\u4f5c\u8005<\/strong>)\u7b49\u4eba\u62a5\u9053\u4e86\u5364\u5316\u94c5\u7eb3\u7c73\u7ebf\u7684\u81ea\u50ac\u5316\u6c14\u6db2\u56fa\u751f\u957f\u548cLHP\u8f6c\u53d8\u3002\u4f5c\u8005\u63d0\u51fa\u4e86PbX<sub>2<\/sub> \u7eb3\u7c73\u7ebf(NW)\u7684\u751f\u957f\u52a8\u529b\u5b66\u6a21\u578b\uff0c\u901a\u8fc7Pb\u548cX\u7684\u6c14\u76f8\u7ed3\u5408\uff0c\u6db2\u6001Pb\u50ac\u5316\u5242\u4e0e\u5364\u7d20X\u8fc7\u9971\u548c\uff0c\u4ece\u800c\u8bf1\u5bfcNW\u751f\u957f\u3002\u7814\u7a76\u7ed3\u679c\u8868\u660e\uff0cNWs\u8868\u73b0\u51fa\u9ad8\u6548\u7684\u5149\u5b66\u5929\u7ebf\u6548\u5e94\uff0c\u6563\u5c04\u6548\u7387\u548c\u5438\u6536\u6548\u7387\u663e\u8457\u63d0\u9ad8\uff0c\u8fbe\u5230\u4e86\u540c\u539a\u5ea6\u8584\u819c\u7684\u4e24\u500d\u4ee5\u4e0a\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/10.1021\/acs.nanolett.7b03514\" target=\"_blank\" rel=\"noopener\">Self-Catalyzed Vapor\u2013Liquid\u2013Solid Growth of Lead Halide Nanowires and Conversion to Hybrid Perovskites <\/a>(Nano Lett., 2017, DOI: 10.1021\/acs.nanolett.7b03514\uff09<\/p>\n<p><strong>5\u3001J. Am. Chem. Soc.\uff1aCdSe\/CdS\u6838\u58f3\u7ed3\u6784\u7eb3\u7c73\u6676\u4f53\u7684\u5236\u5907\u53ca\u5176\u5149\u81f4\u53d1\u5149\u7279\u6027<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-113564\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/5-38.jpg\" alt=\"\" width=\"600\" height=\"230\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/5-38.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/5-38-300x115.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><br \/>\n \u91cf\u5b50\u70b9(QDs)\u5c3a\u5bf8\u7684\u80f6\u4f53\u534a\u5bfc\u4f53\u7eb3\u7c73\u6676\u4f5c\u4e3a\u91cd\u8981\u7684\u53d1\u5149\u6750\u6599\u5f97\u5230\u4e86\u8fc5\u901f\u53d1\u5c55\u3002\u7279\u522b\u662f\u5728\u663e\u793a\u9886\u57df\uff0c\u8272\u7eaf\u5ea6\u9ad8\u3001\u53d1\u5149\u6548\u7387\u9ad8\u3001\u7a33\u5b9a\u6027\u597d\u548c\u826f\u597d\u7684\u6eb6\u6db2\u53ef\u52a0\u5de5\u6027\u4f7f\u5f97\u91cf\u5b50\u70b9\u6210\u4e3a\u6700\u7406\u60f3\u7684\u53d1\u5c04\u5668\u3002\u7136\u800c\uff0c\u76ee\u524d\u79d1\u5b66\u5bb6\u4eec\u5bf9\u91cf\u5b50\u70b9\u6fc0\u53d1\u6001\u7684\u7efc\u5408\u63a7\u5236\u8fd8\u5904\u4e8e\u521d\u6b65\u7684\u7406\u89e3\u548c\u7814\u7a76\u9636\u6bb5\u3002\u8fd1\u65e5\uff0c<strong>\u6d59\u6c5f\u5927\u5b66\u5f6d\u7b11\u521a\u6559\u6388<\/strong>(<strong>\u901a\u8baf\u4f5c\u8005<\/strong>)\u7b49\u4eba\u62a5\u9053\u4e86CdSe\/CdS\u6838\u58f3\u7ed3\u6784\u91cf\u5b50\u70b9\u7684\u5236\u5907\u53ca\u5176\u5149\u81f4\u53d1\u5149\u7279\u6027\u7684\u6700\u65b0\u7814\u7a76\u7ed3\u679c\u3002\u7814\u7a76\u4eba\u5458\u4ee5CdSe\/CdS\u6838\u58f3\u7ed3\u6784QDs\u4e3a\u6a21\u578b\uff0c\u7cfb\u7edf\u7814\u7a76\u4e86\u58f3\u5916\u5ef6\u3001\u914d\u4f53\u4ea4\u6362\u3001\u5f62\u6001\u8f6c\u53d8\u7b49\u5bf9CdSe\/CdS\u6838\u58f3\u7ed3\u6784\u7eb3\u7c73\u6676\u7684\u5149\u7269\u7406\u548c\u5149\u5316\u5b66\u6027\u8d28\u7684\u5f71\u54cd\uff0c\u5efa\u7acb\u4e86\u5408\u6210\u5177\u6709\u76ee\u6807\u6027\u8d28\u7684QDs\u7684\u6280\u672f\u8def\u7ebf\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/10.1021\/jacs.7b07434\" target=\"_blank\" rel=\"noopener\">Ideal CdSe\/CdS Core\/Shell Nanocrystals Enabled by Entropic Ligands and Their Core Size-, Shell Thickness-, and Ligand-Dependent Photoluminescence Properties <\/a>(J. Am. Chem. Soc., 2017, DOI: 10.1021\/jacs.7b07434\uff09<\/p>\n<p><strong>6\u3001Angew. Chem. Int. Ed.\uff1a\u5c42\u5c42\u81ea\u7ec4\u88c5\u5236\u5907\u5bfc\u7535MOF\u7eb3\u7c73\u819c\u5728\u5ba4\u6e29\u5316\u5b66\u7535\u963b\u4f20\u611f\u5668\u4e0a\u7684\u5e94\u7528<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-113565\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/6-18.png\" alt=\"\" width=\"600\" height=\"640\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/6-18.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/6-18-281x300.png 281w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><br \/>\n \u7535\u5b50\u5bfc\u7535\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6(EC-MOFs)\u662f\u4e00\u79cd\u65b0\u5174\u7684\u591a\u5b54\u5bfc\u7535\u6750\u6599\uff0c\u5728\u573a\u6548\u5e94\u6676\u4f53\u7ba1(FET)\u3001\u8d85\u7ea7\u7535\u5bb9\u5668\u3001\u70ed\u7535\u5668\u4ef6\u3001\u6c27\u8fd8\u539f\u53cd\u5e94\u7535\u50ac\u5316\u5242\u548c\u5316\u5b66\u6c14\u4f53\u4f20\u611f\u5668\u7b49\u65b9\u9762\u6709\u7740\u5e7f\u6cdb\u7684\u5e94\u7528\u3002\u7136\u800c\uff0c\u9ad8\u8d28\u91cfEC-MOFs\u7eb3\u7c73\u819c\u7684\u7f3a\u4e4f\u4e25\u91cd\u9650\u5236\u4e86\u5176\u5728\u9ad8\u6027\u80fd\u5668\u4ef6\u4e2d\u7684\u5e94\u7528\u3002\u8fd1\u65e5\uff0c<strong>\u798f\u5efa\u7269\u8d28\u7ed3\u6784\u7814\u7a76\u6240\u5f90\u521a\u7814\u7a76\u5458<\/strong>(<strong>\u901a\u8baf\u4f5c\u8005<\/strong>)\u7b49\u4eba\u62a5\u9053\u4e86\u5236\u5907EC-MOFs\u7eb3\u7c73\u819c\u7684\u65b0\u65b9\u6cd5\u3002\u4f5c\u8005\u901a\u8fc7\u55b7\u6d82\u9010\u5c42\u6db2\u76f8\u5916\u5ef6\u6cd5\u5236\u5907EC-MOF\u7684\u53ef\u63a7\u8584\u819c\uff0c\u8584\u819c\u4e0d\u4ec5\u80fd\u7cbe\u786e\u5236\u5907\uff0c\u800c\u4e14\u8868\u9762\u5149\u6ed1\u3001\u7ed3\u6676\u6027\u597d\u3001\u53d6\u5411\u5ea6\u9ad8\uff0c\u5728\u6c14\u4f53\u4f20\u611f\u5668\u7b49\u65b9\u9762\u5177\u6709\u5f88\u5927\u7684\u5e94\u7528\u6f5c\u529b\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/anie.201709558\/full\" target=\"_blank\" rel=\"noopener\">Layer-by-Layer Assembled Conductive Metal\u2013Organic Framework Nanofilms for Room-Temperature Chemiresistive Sensing <\/a>(Angew. Chem. Int. Ed., 2017, DOI: 10.1002\/anie.201709558\uff09<\/p>\n<p><strong>7\u3001Adv. Funct. Mater.\uff1a\u5177\u6709\u5149\u81f4\u7535\u5316\u5b66\u6d3b\u6027\u548c\u73af\u5883\u7a33\u5b9a\u7684CsPbBr3\/TiO2\u6838\u58f3\u7ed3\u6784\u7eb3\u7c73\u6676<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-113566\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/7-14.png\" alt=\"\" width=\"600\" height=\"516\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/7-14.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/7-14-300x258.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><br \/>\n \u9499\u949b\u77ff\u7eb3\u7c73\u6676(NCs)\u5dee\u7684\u7a33\u5b9a\u6027\u662f\u963b\u788d\u5176\u5e7f\u6cdb\u5e94\u7528\u7684\u91cd\u8981\u56e0\u7d20\u3002\u8fd1\u65e5\uff0c\u6765\u81ea\u7f8e\u56fd<strong>\u96ea\u57ce\u5927\u5b66<\/strong>\u7684<strong>Weiwei Zheng<\/strong> (\u901a\u8baf\u4f5c\u8005)\u7b49\u4eba\u62a5\u9053\u4e86\u5177\u6709\u4f18\u5f02\u73af\u5883\u7a33\u5b9a\u6027\u7684CsPbBr<sub>3<\/sub>\/TiO<sub>2<\/sub>\u6838\u58f3\u7ed3\u6784\u9499\u949b\u77ff\u7eb3\u7c73\u6676\u4f53\u53ca\u5176\u5149\u81f4\u7535\u5316\u5b66\u6d3b\u6027\u3002\u7814\u7a76\u4eba\u5458\u9996\u5148\u91c7\u7528TiO2\u524d\u9a71\u4f53\u5bf9\u80f6\u4f53CsPbBr<sub>3<\/sub> NC\u8fdb\u884c\u5305\u8986\uff0c\u7136\u540e\u5728300\u2103\u4e0b\u7145\u70e7\u5f97\u5230TiO<sub>2<\/sub>\u58f3\u5305\u8986\u7684CsPbBr<sub>3<\/sub>\u6838\u58f3\u7ed3\u6784\u3002\u8fd9\u4e9b\u8fd1\u5355\u5206\u6563\u7684CsPbBr<sub>3<\/sub>\/TiO<sub>2<\/sub>\u6838\u58f3\u7ed3\u6784\u7eb3\u7c73\u6676\u5177\u6709\u5341\u5206\u4f18\u5f02\u7684\u6c34\u7a33\u5b9a\u6027\uff0c\u5176\u5c3a\u5bf8\u3001\u7ed3\u6784\u3001\u5f62\u6001\u548c\u5149\u5b66\u6027\u8d28\u53ef\u4fdd\u63013\u4e2a\u6708\u4ee5\u4e0a\u4e0d\u53d8\u5316\uff0c\u662f\u8fc4\u4eca\u4e3a\u6b62\u6c34\u7a33\u5b9a\u6027\u6700\u597d\u7684\u65e0\u673a\u58f3\u949d\u5316\u7684\u9499\u949b\u77ff\u7eb3\u7c73\u6676\u3002\u53e6\u5916\uff0cTiO2\u58f3\u80fd\u591f\u6291\u5236\u9634\u79bb\u5b50\u4ea4\u6362\u548c\u5149\u964d\u89e3\uff0c\u5927\u5927\u63d0\u9ad8\u4e86CsPbBr<sub>3<\/sub>\u6838\u7684\u5316\u5b66\u7a33\u5b9a\u6027\u548c\u5149\u7a33\u5b9a\u6027\uff1b\u800c\u4e14\uff0c\u5149\u81f4\u53d1\u5149(PL)\u548c(\u5149\u81f4)\u7535\u5316\u5b66\u8868\u5f81\u663e\u793a\u5bfc\u7535\u7684TiO2\u58f3\u80fd\u591f\u63d0\u9ad8\u7535\u8377\u5206\u79bb\u6548\u7387\uff0c\u4ece\u800c\u63d0\u5347\u5176\u6c34\u4e2d\u7684\u5149\u7535\u6d3b\u6027\u3002\u8be5\u7814\u7a76\u4e3a\u6c34\u76f8\u9499\u949b\u77ff\u578b\u7eb3\u7c73\u6676\u5728\u5149\u7535\u548c\u5149\u50ac\u5316\u7b49\u9886\u57df\u7684\u5e94\u7528\u63d0\u4f9b\u4e86\u65b0\u601d\u8def\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adfm.201704288\/full\" target=\"_blank\" rel=\"noopener\">Photoelectrochemically Active and Environmentally Stable CsPbBr3\/TiO2 Core\/Shell Nanocrystals <\/a>(Adv. Funct. Mater., 2017, DOI: 10.1002\/adfm.201704288\uff09<\/p>\n<p><strong>8\u3001ACS Nano\uff1a\u77f3\u58a8\u578b\u6c2e\u89e6\u53d1\u78b3\u91cf\u5b50\u70b9\u7684\u7ea2\u8272\u8367\u5149<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-113567\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/8-14.jpg\" alt=\"\" width=\"600\" height=\"338\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/8-14.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/8-14-300x169.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><br \/>\n \u78b3\u91cf\u5b50\u70b9(CDs)\u662f\u4e00\u79cd\u7a33\u5b9a\u7684\u548c\u9ad8\u5ea6\u751f\u7269\u76f8\u5bb9\u7684\u8367\u5149\u6750\u6599\uff0c\u5728\u7ec6\u80de\u6807\u8bb0\u3001\u5149\u5b66\u6210\u50cf\u3001LED\u548c\u5149\u7535\u5b50\u6280\u672f\u65b9\u9762\u6709\u7740\u5e7f\u6cdb\u7684\u5e94\u7528\u3002\u8fd1\u65e5\uff0c\u6765\u81ea<strong>\u6377\u514b\u5e15\u62c9\u8328\u57fa\u5927\u5b66<\/strong>\u7684<strong>Radek Zbo\u0159il<\/strong> (<strong>\u901a\u8baf\u4f5c\u8005<\/strong>)\u7b49\u4eba\u62a5\u9053\u4e86\u4e00\u79cd\u5177\u6709\u4f18\u79c0\u53ef\u63a7\u8367\u5149\u7684\u5168\u8272\u5f69CD\u3002\u7ecfXPS\u5206\u6790\u8868\u660e\uff0c\u77f3\u58a8\u578b\u6c2e\u6d53\u5ea6\u7684\u589e\u52a0\u662f\u5bfc\u81f4N-CD\u4ece\u84dd\u8272\u5230\u7ea2\u8272\u8367\u5149\u8f6c\u53d8\u7684\u5173\u952e\u56e0\u7d20\u3002\u6b64\u5916\uff0c\u4f5c\u8005\u8fd8\u901a\u8fc7\u7406\u8bba\u8ba1\u7b97\u8be6\u7ec6\u89e3\u91ca\u4e86\u77f3\u58a8\u578b\u6c2e\u5728CD\u8367\u5149\u7ea2\u79fb\u4e2d\u7684\u4f5c\u7528\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/10.1021\/acsnano.7b06399\" target=\"_blank\" rel=\"noopener\">Graphitic Nitrogen Triggers Red Fluorescence in Carbon Dots <\/a>(ACS Nano, DOI: 2017, 10.1021\/acsnano.7b06399\uff09<\/p>\n<p><strong>9\u3001Science Advances \uff1a\u4e00\u79cd\u4eba\u4f53\u8f90\u5c04\u52a0\u70ed\u548c\u51b7\u5374\u7684\u53cc\u6a21\u5f0f\u7eba\u7ec7\u6750\u6599<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-113568\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/9-11.jpg\" alt=\"\" width=\"600\" height=\"219\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/9-11.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/9-11-300x110.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><br \/>\n \u4fdd\u6301\u4f53\u6e29\u662f\u4eba\u4f53\u6700\u57fa\u672c\u7684\u9700\u6c42\u4e4b\u4e00\u3002\u4e3a\u4e86\u6269\u5927\u73af\u5883\u6e29\u5ea6\u8303\u56f4\uff0c\u540c\u65f6\u4fdd\u6301\u4eba\u4f53\u7684\u70ed\u8212\u9002\u6027\uff0c\u901a\u8fc7\u4eba\u4f53\u7ea2\u5916\u8f90\u5c04\u6765\u63a7\u5236\u8863\u7269\u7684\u52a0\u70ed\u548c\u51b7\u5374\u4ece\u800c\u5b9e\u73b0\u4eba\u4f53\u7684\u70ed\u91cf\u7ba1\u7406\u5f97\u5230\u4e86\u79d1\u5b66\u5bb6\u4eec\u7684\u5e7f\u6cdb\u5173\u6ce8\u3002\u8fd1\u65e5\uff0c\u6765\u81ea<strong>\u65af\u5766\u798f\u5927\u5b66<\/strong>\u7684<strong>\u5d14\u5c79\u6559\u6388<\/strong>(<strong>\u901a\u8baf\u4f5c\u8005<\/strong>)\u7b49\u4eba\u62a5\u9053\u4e86\u4e00\u79cd\u7279\u6b8a\u7684\u7eba\u7ec7\u6750\u6599\uff0c\u5728\u65e0\u4efb\u4f55\u80fd\u91cf\u7684\u8f93\u5165\u7684\u60c5\u51b5\u4e0b\uff0c\u80fd\u591f\u5b9e\u73b0\u88ab\u52a8\u7684\u8f90\u5c04\u52a0\u70ed\u548c\u51b7\u5374\u53cc\u5de5\u4f5c\u6a21\u5f0f\u3002\u8be5\u53cc\u6a21\u5f0f\u7eba\u7ec7\u6750\u6599\u7531\u53cc\u5c42\u53d1\u5c04\u4f53\u5305\u57cb\u5728\u53ef\u7ea2\u5916\u900f\u8fc7\u7684\u7eb3\u7c73\u591a\u5b54\u805a\u4e59\u70ef(nanoPE)\u5c42\u5185\u6784\u6210\u3002\u7814\u7a76\u8868\u660e\uff0c\u53d1\u5c04\u7387\u548cnanoPE\u539a\u5ea6\u7684\u4e0d\u5bf9\u79f0\u7279\u6027\u53ef\u4ee5\u5f62\u6210\u4e24\u79cd\u4e0d\u540c\u7684\u4f20\u70ed\u7cfb\u6570\u548c\u52a0\u70ed\/\u51b7\u5374\u4e24\u79cd\u5de5\u4f5c\u6a21\u5f0f\u3002\u5f53\u4f4e\u53d1\u5c04\u7387\u5c42\u671d\u5916\u65f6\u4e3a\u52a0\u70ed\u72b6\u6001\uff1b\u5f53\u9ad8\u53d1\u5c04\u7387\u5c42\u671d\u5916\u65f6\uff0c\u5c06\u901a\u8fc7\u7ec7\u7269\u5185\u90e8\u78e8\u635f\u5b9e\u73b0\u51b7\u5374\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>\uff1a<a href=\"http:\/\/advances.sciencemag.org\/content\/3\/11\/e1700895.full\" target=\"_blank\" rel=\"noopener\">A dual-mode textile for human body radiative heating and cooling <\/a>(Science Advances, 2017, DOI:10.1126\/sciadv.1700895\uff09<\/p>\n<p><strong>10\u3001Science Advances \uff1a\u8d85\u8584Si\u819c\u7684\u590d\u6742\u53bb\u6da6\u6e7f\u82b1\u6837\u7528\u4e8e\u6784\u7b51\u5927\u89c4\u6a21\u7eb3\u7c73\u7ed3\u6784<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-113559\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/10-9.jpg\" alt=\"\" width=\"600\" height=\"451\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/10-9.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/11\/10-9-300x226.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><br \/>\n \u53bb\u6da6\u6e7f\u662f\u81ea\u7136\u754c\u4e2d\u975e\u5e38\u666e\u904d\u7684\u79cd\u73b0\u8c61\uff0c\u5f88\u591a\u6709\u673a\u548c\u65e0\u673a(\u5982\u6db2\u4f53\uff0c\u805a\u5408\u7269\uff0c\u91d1\u5c5e\u548c\u534a\u5bfc\u4f53)\u7684\u8584\u819c\u90fd\u5177\u6709\u8fd9\u79cd\u7531\u8868\u9762\u5f20\u529b\u548c\u4f20\u8d28\u6240\u9a71\u52a8\u7684\u5f62\u72b6\u4e0d\u7a33\u5b9a\u6027\u3002\u8fd1\u65e5\uff0c\u6765\u81ea\u5fb7\u56fd<strong>\u5fb7\u7d2f\u65af\u987f\u5de5\u4e1a\u5927\u5b66<\/strong>\u7684<strong>Marco Salvalaglio<\/strong>\u3001\u6cd5\u56fd<strong>\u571f\u4f26\u5927\u5b66<\/strong>\u7684 <strong>Marco Abbarchi<\/strong>\u548c\u610f\u5927\u5229<strong>IFN-CNR<\/strong>\u7684<strong>Monica Bollani<\/strong>(<strong>\u5171\u540c\u901a\u8baf\u4f5c\u8005<\/strong>)\u7b49\u4eba\u62a5\u9053\u4e86\u4e00\u79cd\u5229\u7528\u56fa\u6001\u53bb\u6da6\u6e7f\u73b0\u8c61\u5728\u7edd\u7f18\u4f53\u4e0a(\u65e0\u5b9a\u578bSiO<sub>2<\/sub>\u57fa\u4f53)\u5236\u5907\u5927\u89c4\u6a21\u548c\u8d85\u7cbe\u7ec6\u7eb3\u7c73\u7ed3\u6784\u5355\u6676Si\u8584\u819c\u7684\u65b9\u6cd5\uff0c\u5e76\u5bf9\u5236\u5907\u8fc7\u7a0b\u8fdb\u884c\u4e86\u76f8\u573a(PF)\u6a21\u62df\uff0c\u63ed\u793a\u4e86\u8868\u9762\u6269\u6563\u7684\u91cd\u8981\u4f5c\u7528\uff0c\u6a21\u62df\u7ed3\u679c\u4e0e\u5b9e\u9a8c\u7ed3\u679c\u9ad8\u5ea6\u543b\u5408\u3002\u7814\u7a76\u4eba\u5458\u8fdb\u4e00\u6b65\u5c06\u5236\u5907\u7684Si\u8584\u819c\u82b1\u6837\u7528\u4f5c\u7eb3\u7c73\u538b\u5370\u4e3b\u4f53\uff0c\u53ef\u5c06\u590d\u6742\u7684\u7eb3\u7c73\u7ed3\u6784\u8f6c\u79fb\u5230\u91d1\u5c5e\u6c27\u5316\u7269\u5e72\u51dd\u80f6\u4e0a\uff0c\u4e3a\u4e0d\u540c\u6750\u6599\u7684\u7eb3\u7c73\u56fe\u6848\u5316\u63d0\u4f9b\u53e6\u4e00\u79cd\u9009\u62e9\u3002\u8fd9\u79cd\u53bb\u6da6\u6e7f\u7684\u64cd\u63a7\u5728\u7eb3\u7c73\u7535\u8def\u3001\u6ce2\u5bfc\u3001\u8d85\u8868\u9762\u3001\u5fae\u6d41\u4f53\u5668\u4ef6\u548c\u751f\u7269\u533b\u836f\u4f20\u611f\u7b49\u9886\u57df\u5177\u6709\u5e7f\u9614\u7684\u5e94\u7528\u6f5c\u529b\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>\uff1a<a href=\"http:\/\/advances.sciencemag.org\/content\/3\/11\/eaao1472.full\" target=\"_blank\" rel=\"noopener\">Complex dewetting scenarios of ultrathin silicon films for large-scale nanoarchitectures<\/a> (Science Advances, 2017, DOI: 10.1126\/sciadv.aao1472\uff09<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u7eb3\u7c73\u5b66\u672f\u7ec4jcfxs01\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u8fd9\u91cc\u6c47\u96c6\u4e86\u5404\u5927\u9ad8\u6821\u7855\u535a\u751f\u3001\u4e00\u7ebf\u79d1\u7814\u4eba\u5458\u4ee5\u53ca\u884c\u4e1a\u4ece\u4e1a\u8005\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8\u5927\u5bb6\u5ead<\/a>\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n<p><strong>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1aRDD-2011-CHERISH\uff0c\u4efb\u4e39\u4e39\uff0c\u6211\u4eec\u4f1a\u9080\u8bf7\u5404\u4f4d\u8001\u5e08\u52a0\u5165\u4e13\u5bb6\u7fa4\u3002<\/strong><\/p>\n<p><strong>\u6750\u6599\u6d4b\u8bd5\u3001\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener\">\u6d4b\u8bd5\u8c37<\/a>\uff01<\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>1\u3001ACS Nano: \u5316\u5b66\u6c14\u76f8\u6c89\u79ef\u6cd5\u5236\u5907\u5927\u9762\u79ef\u5355\u6676\u516d\u65b9\u6c2e\u5316\u787c \u516d\u65b9\u6c2e\u5316\u787c(h-BN)\u662f\u4e00\u79cd\u4e0e\u77f3\u58a8\u70ef\u5177\u6709\u76f8\u4f3c\u6676\u683c\u7ed3\u6784\u7684\u5c42\u72b6\u6750\u6599\uff0c\u8fd9\u4e9b\u5c42\u7531\u8702\u7a9d\u72b6\u6392\u5217\u7684\u787c\u539f\u5b50\u548c\u6c2e\u539f&#8230;<\/p>\n","protected":false},"author":4915,"featured_media":113565,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[293,155,2548,33],"class_list":["post-113584","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-nature","tag-science","tag-2548","tag-nano"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/113584"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/4915"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=113584"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/113584\/revisions"}],"predecessor-version":[{"id":113587,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/113584\/revisions\/113587"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/113565"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=113584"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=113584"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=113584"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}