{"id":115374,"date":"2017-12-09T06:30:32","date_gmt":"2017-12-08T22:30:32","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=115374"},"modified":"2017-12-07T16:50:13","modified_gmt":"2017-12-07T08:50:13","slug":"%e8%a7%82%e7%82%b9%e4%b8%a8%e4%b8%89%e7%bb%b4%e7%9f%b3%e5%a2%a8%e7%83%afvs%e4%ba%8c%e7%bb%b4%e7%9f%b3%e5%a2%a8%e7%83%af%ef%bc%8c%e8%b0%81%e6%9b%b4%e8%83%9c%e4%b8%80%e7%ad%b9%ef%bc%9f","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=115374","title":{"rendered":"\u89c2\u70b9\u4e28\u4e09\u7ef4\u77f3\u58a8\u70efVS\u4e8c\u7ef4\u77f3\u58a8\u70ef\uff0c\u8c01\u66f4\u80dc\u4e00\u7b79\uff1f"},"content":{"rendered":"<p>\u8981\u95ee\u4e16\u754c\u4e0a\u6700\u7ed3\u5b9e\u575a\u56fa\u662f\u795e\u9a6c\u4e1c\u897f\uff1f\u591a\u6570\u4eba\u7684\u7b54\u6848\u4f1a\u662f\u77f3\u58a8\u70ef\uff08\u5c11\u6570\u5403\u74dc\u7fa4\u4f17\u4e5f\u53ef\u80fd\u4f1a\u7b54\u94bb\u77f3\uff09\u3002<\/p>\n<p>\u662f\u554a\uff0c\u8fd9\u4e2a\u65e9\u572820\u4e16\u7eaa40\u5e74\u4ee3\u5c31\u5f00\u59cb\u7814\u7a76\u7684\u795e\u5947\u6750\u6599\uff0c\u88ab\u8ba4\u4e3a\u53f2\u4e0a\u6700\u7ed3\u5b9e\u3001\u6700\u8f7b\u8584\u3001\u4e5f\u662f\u6700\u6709\u524d\u9014\u7684\u8de8\u4e16\u7eaa\u6750\u6599\u3002\u82f1\u56fd\u66fc\u5f7b\u65af\u7279\u5927\u5b66\u4e24\u4f4d\u79d1\u5b66\u5bb6\u56e0\u4e3a\u77f3\u58a8\u70ef\u7684\u7a81\u7834\u6027\u5b9e\u9a8c\uff0c\u8fd8\u62ff\u5230\u4e862010\u5e74\u8bfa\u5956\u3002\u7531\u4e8e\u77f3\u58a8\u70ef\u5177\u6709\u4f18\u5f02\u7684\u529b\u5b66\u6027\u80fd\u3001\u70ed\u5b66\u6027\u80fd\uff0c\u7535\u5b66\u6027\u80fd\u4ee5\u53ca\u826f\u597d\u7684\u5ef6\u5c55\u6027\uff0c\u4f7f\u5176\u5728\u9ad8\u6027\u80fd\u7535\u5b50\u5668\u4ef6\u3001\u5bfc\u70ed\u3001\u50ac\u5316\u53ca\u80fd\u6e90\u9886\u57df\u6709\u7740\u5de8\u5927\u7684\u6f5c\u5728\u5e94\u7528\u4ef7\u503c\u3002\u751a\u81f3\u672a\u6765\u5b66\u6d3e\u3001\u6750\u6599\u5b66\u5bb6\u65ad\u5b9a\uff0c\u4e00\u767e\u5e74\u540e\u7684\u4e16\u754c\u90fd\u662f\u7531\u77f3\u58a8\u70ef\u5efa\u9020\u7684\u3002<\/p>\n<p>\u77f3\u58a8\u70efGraphene\u8ddf\u94bb\u77f3\u4e00\u6837\uff0c\u90fd\u662f\u7eaf\u78b3\uff0c\u7531\u516d\u8fb9\u5f62\u7f51\u72b6\u539f\u5b50\u6784\u6210\uff0c\u901a\u8fc7\u7535\u5b50\u663e\u5fae\u955c\u89c2\u5bdf\uff0c\u5b83\u5c31\u50cf\u8702\u5de2\u6216\u8005\u4e00\u5757\u7ec6\u94c1\u4e1d\u7f51\u3002\u539a\u5ea6\u53ea\u67090.335\u7eb3\u7c73\uff0c\u628a20\u4e07\u7247\u8584\u819c\u645e\u8d77\u6765\uff0c\u4e5f\u53ea\u6709\u4e00\u6839\u5934\u53d1\u4e1d\u90a3\u4e48\u539a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-115376\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/1-4.jpg\" alt=\"\" width=\"720\" height=\"405\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/1-4.jpg 720w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/1-4-300x169.jpg 300w\" sizes=\"(max-width: 720px) 100vw, 720px\" \/><\/p>\n<p>\u8fd9\u79cd\u539f\u5b50\u539a\u7684\u78b3\u539f\u5b50\u94fe\u4e0d\u4ec5\u8d85\u7ea7\u7ed3\u5b9e\uff0c\u800c\u4e14\u8d85\u7ea7\u8f7b\u8584\uff0c\u67d4\u97e7\u6027\u4e5f\u8d85\u597d\uff0c\u751a\u81f3\u8ddf\u5851\u6599\u5305\u88c5\u4e00\u6837\uff0c\u53ef\u4ee5\u968f\u610f\u5f2f\u66f2\u3001\u6298\u53e0\uff0c\u50cf\u5377\u8f74\u4e00\u6837\u5377\u8d77\u6765\u3002\u77f3\u58a8\u70ef\u7684\u5e94\u7528\u975e\u5e38\u5e7f\u6cdb\uff0c\u89e6\u6478\u5c4f\u3001\u592a\u9633\u80fd\u7535\u6c60\u3001\u80fd\u91cf\u50a8\u5b58\u88c5\u7f6e\u3001\u9ad8\u901f\u7535\u8111\u82af\u7247\u3001\u5efa\u7b51\u6750\u6599\u3001\u9632\u6c34\u6d82\u5c42\u3001\u8fc7\u6ee4\u6e05\u6c61\u2026\u2026<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-115377\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/1-5.jpg\" alt=\"\" width=\"720\" height=\"540\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/1-5.jpg 720w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/1-5-300x225.jpg 300w\" sizes=\"(max-width: 720px) 100vw, 720px\" \/><\/p>\n<p>\u8bf4\u4e86\u8fd9\u4e48\u591a\u90fd\u662f\u4e3a\u4e86\u300c\u4f46\u662f\u300d\u505a\u94fa\u57ab\u7684\uff0c\u77f3\u58a8\u70ef\u6709\u4e2a\u663e\u8457\u7f3a\u70b9\uff0c\u6b63\u56e0\u4e3a\u5b83\u592a\u8584\u4e86\uff0c\u96be\u4ee5\u9020\u51fa\u4ee4\u4eba\u6ee1\u610f\u7684\u539a\u5ea6\uff0c\u8fd9\u5927\u5927\u9650\u5236\u4e86\u5927\u663e\u8eab\u624b\u7684\u673a\u4f1a\u3002\u6240\u4ee5\u5462\uff0c\u6280\u672f\u653b\u5173\u2014\u2014\u521b\u5efa3D\u7248\u7684\u77f3\u58a8\u70ef\u6210\u4e3a\u4e16\u754c\u9876\u5c16\u79d1\u6280\u9ad8\u624b\u7684\u9690\u5f62\u64c2\u53f0\u3002<\/p>\n<p>\u7ec8\u4e8e\u8fd9\u4e2a\u4e16\u754c\u7ea7\u6280\u672f\u96be\u5173\uff0c\u88ab\u7f8e\u56fd\u9ebb\u7701\u7406\u5de5\u5b66\u9662MIT\u4e00\u5e2e\u5b50\u79d1\u6280\u5927\u795e\u7ed9\u653b\u4e0b\u5566\u3002\u5c31\u57282017\u5e741\u67089\u65e5\uff0cScience Advances\u6742\u5fd7\u8be6\u7ec6\u62a5\u9053\u4e86\u8fd9\u4e00\u79d1\u7814\u6210\u679c\uff0cMIT\u7814\u7a76\u56e2\u961f\u5728\u5b9e\u9a8c\u5ba4\u91cc\u521b\u9020\u51fa\u3010\u5730\u7403\u4e0a\u6700\u7ed3\u5b9e\u7684\u65b0\u6750\u6599\u2014\u2014\u591a\u5b54\u7684\u4e09\u7ef4\u77f3\u58a8\u70ef\u6750\u6599\u3011\u3002\u5b83\u662f\u94a2\u6750\u5f3a\u5ea6\u768410\u500d\uff0c\u5bc6\u5ea6\u5374\u4e0d\u5230\u94a2\u6750\u76845%\uff0c\u751a\u81f3\u6bd4\u591a\u5b54\u77f3\u58a8\u70ef\u8fd8\u7ed3\u5b9e\u3002 \u5230\u5e95\u4eba\u5bb6\u662f\u600e\u4e48\u505a\u5230\u7684\uff1f\u8fd9\u4e2a\u9879\u76ee\u7814\u7a76\u5458Zhao Qin\u89e3\u91ca\u8bf4\uff0c\u4ed6\u4eec\u5728\u77f3\u58a8\u70ef\u7684\u5408\u6210\u8fc7\u7a0b\u4e2d\uff0c\u52a0\u5927\u4e86\u70ed\u91cf\u548c\u538b\u529b\uff0c\u75283D\u6253\u5370\u673a\u8ba9\u5c0f\u7247\u77f3\u58a8\u70ef\u538b\u7f29\u5230\u4e00\u8d77\uff0c\u4ea7\u751f\u4e86\u7c7b\u4f3c\u4e8e\u73ca\u745a\u90a3\u79cd\u590d\u6742\u6d77\u7ef5\u72b6\u7ed3\u6784\uff0c\u4ed6\u4eec\u79f0\u4e3a\u300c\u87ba\u65cb\u72b6\u590d\u6742\u51e0\u4f55\u7ed3\u6784\u7684\u653e\u59273D\u6253\u5370\u6a21\u578b\u300d\u3002\u6700\u6700\u91cd\u8981\u7684\u662f\uff0c\u4ece\u7406\u8bba\u4e0a\u770b\uff0c\u8fd9\u662f\u80fd\u591f\u5f62\u6210\u65b0\u7684\u8d85\u5f3a\u548c\u8f7b\u8d28\u6750\u6599\u7684\u57fa\u7840\u6a21\u578b\uff0c\u8fd9\u4e9b\u6750\u6599\u7684\u57fa\u6750\u751a\u81f3\u4e0d\u5fc5\u5c40\u9650\u4e8e\u77f3\u58a8\u70ef\u3002\u660e\u767d\u4e86\u5427\uff0c\u91cd\u8981\u7684\u662f\u51e0\u4f55\u6a21\u578b\uff0c\u800c\u4e0d\u662f\u6750\u6599\u672c\u8eab\u3002\u5f53\u7136\u4e86\uff0c\u4eba\u5bb6\u7528\u8fd9\u79cd\u51e0\u4f55\u6a21\u578b\u8bbe\u8ba1\u4e0b\u7684\u77f3\u58a8\u70ef\uff0c\u81ea\u7136\u8981\u6bd4\u8be5\u56e2\u961f\u6b64\u524d\u521b\u9020\u7684\u6700\u5f3a\u591a\u5b54\u77f3\u58a8\u70ef\u66f4\u575a\u56fa\u66f4\u7ed3\u5b9e\uff0c\u582a\u79f0\u4e16\u754c\u6700\u5f3a\u6750\u6599\uff01<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-115378\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/1-6.jpg\" alt=\"\" width=\"720\" height=\"312\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/1-6.jpg 720w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/1-6-300x130.jpg 300w\" sizes=\"(max-width: 720px) 100vw, 720px\" \/><\/p>\n<p>\u8fd9\u5c31\u662f\u88abMIT\u79d1\u7814\u56e2\u961f\u79f0\u4e3a\u300c\u87ba\u65cb\u72b6\u590d\u6742\u51e0\u4f55\u7ed3\u6784\u7684\u653e\u59273D\u6253\u5370\u6a21\u578b\u300d\uff0c\u8ba1\u7b97\u673a\u6548\u679c\u5408\u6210\u7684\u4e09\u7ef4\u77f3\u58a8\u70ef\u6a21\u578b\u7ed3\u6784\u56fe\u3002\u770b\u61c2\u7684\uff0c\u5389\u5bb3\u4e86word\u54e5\u3002\u770b\u4e0d\u61c2\uff0c\u63a5\u7740\u770b\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-115379\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/1-7.jpg\" alt=\"\" width=\"720\" height=\"429\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/1-7.jpg 720w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/1-7-300x179.jpg 300w\" sizes=\"(max-width: 720px) 100vw, 720px\" \/><\/p>\n<p>\u8fd9\u662f\u4e0d\u540c\u539f\u5b50\u6750\u65993D\u6253\u5370\u51fa\u6765\u7684\u6a21\u578b\uff0c\u770b\u5f97\u76f4\u89c2\u4e9b\u3002\u8fd8\u662f\u90a3\u53e5\u8bdd\uff1a\u91cd\u8981\u7684\u662f\u51e0\u4f55\u6a21\u578b\uff0c\u800c\u4e0d\u662f\u6750\u6599\u672c\u8eab\u3002\u5c3d\u7ba1\u5bf9\u4e8e\u8fd9\u79cd\u8d85\u7ea7\u65b0\u6750\u6599\uff0c\u9ebb\u7701\u7406\u5de5\u6750\u6599\u7814\u7a76\u56e2\u961f\u8fd8\u6ca1\u6765\u5f97\u53ca\u7ed9TA\u53d6\u4e2a\u6b63\u5f0f\u540d\u79f0\uff0c\u4f46\u4ed6\u4eec\u8fd8\u662f\u8feb\u4e0d\u53ca\u5f85\u5730\u5e0c\u671b\uff0c\u8fd9\u79cd\u8d85\u7ea7\u6750\u6599\u548c\u80cc\u540e\u7684\u51e0\u4f55\u6a21\u578b\u80fd\u591f\u5c3d\u65e9\u6295\u5165\u5e94\u7528\uff0c\u4ece\u4e2a\u4eba\u8bbe\u5907\u5230\u5efa\u7b51\u7269\u2026\u2026<\/p>\n<p><strong>\u5927PK\uff1a<\/strong><\/p>\n<p><strong>\u4e8c\u7ef4\u77f3\u58a8\u70ef<\/strong>\u662f\u7531\u78b3\u516d\u5143\u73af\u7ec4\u6210\u7684\u4e24\u7ef4(2D)\u5468\u671f\u8702\u7a9d\u72b6\u70b9\u9635\u7ed3\u6784, \u5b83\u53ef\u4ee5\u7fd8\u66f2\u6210\u96f6\u7ef4(0D)\u7684\u5bcc\u52d2\u70ef(fullerene),\u5377\u6210\u4e00\u7ef4(1D)\u7684\u78b3\u7eb3\u7c73\u7ba1(carbon nano-tube, CNT)\u6216\u8005\u5806\u579b\u6210\u4e09\u7ef4(3D)\u7684\u77f3\u58a8(graphite), \u56e0\u6b64\u77f3\u58a8\u70ef\u662f\u6784\u6210\u5176\u4ed6\u77f3\u58a8\u6750\u6599\u7684\u57fa\u672c\u5355\u5143\u3002<\/p>\n<p>\u5176\u6027\u80fd\u7684\u5177\u4f53\u53c2\u6570\u5305\u62ec\uff1a<\/p>\n<p>1\u3001\u5438\u5149\u7387\u7ea6\u4e3a2.3%<\/p>\n<p>2\u3001\u5bfc\u70ed\u7cfb\u6570\u9ad8\u8fbe5300 W\/m\u00b7K\uff08\u9ad8\u4e8e\u78b3\u7eb3\u7c73\u7ba1\u548c\u91d1\u521a\u77f3\uff09<\/p>\n<p>3\u3001\u5e38\u6e29\u4e0b\u5176\u7535\u5b50\u8fc1\u79fb\u7387\u8d85\u8fc715000 cm<sup>2<\/sup>\/V\u00b7s\uff08\u6bd4\u7eb3\u7c73\u78b3\u7ba1\u6216\u7845\u6676\u4f53\u9ad8\uff09<\/p>\n<p>4\u3001\u7535\u963b\u7387\u7ea610E<sup>-8<\/sup> \u03a9\u00b7m\uff08\u6bd4\u94dc\u6216\u94f6\u66f4\u4f4e\uff0c\u4e3a\u4e16\u4e0a\u7535\u963b\u7387\u6700\u5c0f\u7684\u6750\u6599\uff09<\/p>\n<p><strong>\u4e09\u7ef4\u77f3\u58a8\u70ef\uff08\u591a\u5b54\u77f3\u58a8\u70ef\uff09<\/strong>\u6750\u6599\u662f\u5728\u77f3\u58a8\u70ef\u7684\u7247\u5c42\u4e2d\u901a\u8fc7\u7269\u7406\u6216\u5316\u5b66\u7684\u65b9\u6cd5\u5236\u9020\u4e00\u4e9b\u5177\u6709\u7eb3\u7c73\u5c3a\u5bf8\u7684\u5b54\u6d1e\uff0c\u8fd9\u4e9b\u65b9\u6cd5\u5305\u62ec\uff1a\u5316\u5b66\u6c14\u76f8\u6c89\u79ef\u6cd5\uff0c\u6eb6\u6db2\u6cd5\uff0c\u6c34\u70ed\u6cd5\u7b49\u3002\u7531\u4e8e\u4e09\u7ef4\u77f3\u58a8\u70ef\u7684\u5236\u5907\u65b9\u6cd5\u6bd4\u8f83\u591a\uff0c\u6240\u4ee5\u5177\u4f53\u7684\u6027\u80fd\u53c2\u6570\u5c1a\u6ca1\u6709\u7edf\u4e00\u7684\u6570\u636e\u3002\u6839\u636e\u76ee\u524d\u7684\u8fdb\u5c55\uff0c\u53ef\u4ee5\u5927\u81f4\u5f97\u51fa\u8fd9\u6837\u7684\u7ed3\u8bba\uff1a<\/p>\n<p>1\u3001\u5b54\u7ed3\u6784\u8f83\u597d<\/p>\n<p>2\u3001\u8868\u9762\u6d3b\u6027\u8f83\u9ad8<\/p>\n<p>3\u3001\u5bfc\u7535\u6027\u53ca\u8d1f\u8f7d\u91cf\u8f83\u597d\uff08\u53ef\u4ee5\u8d1f\u8f7d\u9176\u7528\u4f5c\u751f\u7269\u71c3\u6599\u7535\u6c60\uff09<\/p>\n<p>4\u3001\u4f20\u8d28\u901f\u7387\u8f83\u9ad8\uff08\u53ef\u7528\u4f5c\u4f20\u611f\u5668\uff09<\/p>\n<p>\u5176\u5b9e\uff0c\u4ed6\u4fe9\u5b70\u4f18\u5b70\u52a3\u53ea\u6709\u7528\u4ed6\u4eec\u7684\u6750\u6599\u4eba\u624d\u597d\u8bf4\uff0c\u4e0d\u540c\u7684\u7814\u7a76\u65b9\u5411\uff0c\u4e0d\u540c\u7684\u5e94\u7528\u573a\u5408\u90fd\u4f1a\u51fa\u73b0\u4e0d\u540c\u7684\u89c2\u70b9\uff0c\u6216\u8bb8\u4e8c\u7ef4\u77f3\u58a8\u70ef\u5728\u9ad8\u6027\u80fd\u7535\u5b50\u5668\u4ef6\u4e0a\u66f4\u80dc\u4e00\u7b79\uff0c\u53c8\u6216\u8bb8\u4e09\u7ef4\u77f3\u58a8\u70ef\u5728\u8d85\u7ea7\u7535\u5bb9\u5668\u4e2d\u540e\u6765\u5c45\u4e0a\u3002\u5c0f\u7f16\u60f3\u77e5\u9053\uff0c\u4f60\u7684\u89c2\u70b9\u662f\u4ec0\u4e48\u5462\uff1f<\/p>\n<p>\u672c\u6587\u8f6c\u8f7d\u81ea\u77e5\u4e4e\uff0c\u94fe\u63a5\uff1a<a href=\"https:\/\/zhuanlan.zhihu.com\/p\/24869410\" target=\"_blank\" rel=\"noopener\">https:\/\/zhuanlan.zhihu.com\/p\/24869410<\/a>\u4ee5\u53ca<a href=\"https:\/\/www.zhihu.com\/question\/22461087\" target=\"_blank\" rel=\"noopener\">https:\/\/www.zhihu.com\/question\/22461087<\/a>\u3002<\/p>\n<p>\u6750\u6599\u725b\u77f3\u5c0f\u6885\u7f16\u8f91\u6574\u7406\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u8981\u95ee\u4e16\u754c\u4e0a\u6700\u7ed3\u5b9e\u575a\u56fa\u662f\u795e\u9a6c\u4e1c\u897f\uff1f\u591a\u6570\u4eba\u7684\u7b54\u6848\u4f1a\u662f\u77f3\u58a8\u70ef\uff08\u5c11\u6570\u5403\u74dc\u7fa4\u4f17\u4e5f\u53ef\u80fd\u4f1a\u7b54\u94bb\u77f3\uff09\u3002 \u662f\u554a\uff0c\u8fd9\u4e2a\u65e9\u572820\u4e16\u7eaa40\u5e74\u4ee3\u5c31\u5f00\u59cb\u7814\u7a76\u7684\u795e\u5947\u6750\u6599\uff0c\u88ab\u8ba4\u4e3a\u53f2\u4e0a\u6700\u7ed3\u5b9e\u3001\u6700&#8230;<\/p>\n","protected":false},"author":2832,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[234],"tags":[],"class_list":["post-115374","post","type-post","status-publish","format-standard","hentry","category-guandian"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/115374"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2832"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=115374"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/115374\/revisions"}],"predecessor-version":[{"id":115380,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/115374\/revisions\/115380"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=115374"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=115374"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=115374"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}