{"id":116851,"date":"2017-12-13T06:30:53","date_gmt":"2017-12-12T22:30:53","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=116851"},"modified":"2017-12-12T19:19:21","modified_gmt":"2017-12-12T11:19:21","slug":"%e6%a0%b8%e9%a5%a5%e9%a5%bf%e4%ba%a7%e7%94%9f%e6%96%b0%e5%9e%8b%e9%87%91%e5%b1%9e%e7%8e%bb%e7%92%83","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=116851","title":{"rendered":"\u6838\u9965\u997f\u4ea7\u751f\u65b0\u578b\u91d1\u5c5e\u73bb\u7483"},"content":{"rendered":"<p><strong>\u6750\u6599\u725b\u6ce8<\/strong>\uff1a\u5927\u81ea\u7136\u8fd8\u6709\u5f88\u591a\u503c\u5f97\u6211\u4eec\u63a2\u7d22\u7684\u5730\u65b9\uff0c\u6709\u4e9b\u4e1c\u897f\u6211\u4eec\u53d1\u73b0\u4e86\u5b83\u7684\u5b58\u5728\uff0c\u5374\u4e0d\u4e00\u5b9a\u77e5\u9053\u5b83\u6709\u4ec0\u4e48\u4f5c\u7528\uff0c\u4f46\u662f\uff0c\u6b63\u662f\u8fd9\u6837\u4e00\u70b9\u4e00\u70b9\u5730\u4e0d\u65ad\u63a2\u7d22\uff0c\u4eba\u7c7b\u624d\u4f1a\u4e0d\u65ad\u8fdb\u6b65\u3002\u8036\u9c81\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u5c31\u8fd9\u6837\u53d1\u73b0\u4e86\u91d1\u5c5e\u73bb\u7483\u7684\u4e00\u4e2a\u65b0\u79d8\u5bc6\uff0c\u5f80\u540e\u5b83\u4e00\u5b9a\u4f1a\u53d1\u6325\u5176\u5e94\u6709\u7684\u4f5c\u7528\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-116852\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/20171210.jpg\" alt=\"\" width=\"616\" height=\"347\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/20171210.jpg 616w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/12\/20171210-300x169.jpg 300w\" sizes=\"(max-width: 616px) 100vw, 616px\" \/><\/p>\n<p>\u91d1\u5c5e\u73bb\u7483\u662f\u4e00\u79cd\u65b0\u5174\u6750\u6599\uff0c\u6240\u4ee5\u5173\u4e8e\u5b83\u7684\u79d8\u5bc6\u8fd8\u6709\u5f88\u591a\u672a\u88ab\u53d1\u73b0\u3002\u5728\u7814\u7a76\u8fd9\u79cd\u6750\u6599\u65f6\uff0c\u4e00\u7ec4\u8036\u9c81\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u901a\u8fc7\u5c06\u6837\u54c1\u7f29\u5c0f\u5230\u7eb3\u7c73\u7ea7\u76f4\u5230\u5f62\u6210\u72ec\u7279\u7684\u7ed3\u6676\u76f8\uff0c\u521b\u5efa\u4e86\u4e00\u79cd\u5168\u65b0\u7684\u91d1\u5c5e\u73bb\u7483\u3002<\/p>\n<p>\u901a\u5e38\uff0c\u56fa\u4f53\u91d1\u5c5e\u5177\u6709\u521a\u6027\u7684\u6676\u4f53\u539f\u5b50\u7ed3\u6784\uff0c\u4f46\u6b63\u5982\u5176\u540d\u79f0\u6240\u793a\uff0c\u91d1\u5c5e\u73bb\u7483\u66f4\u50cf\u662f\u73bb\u7483\uff0c\u5177\u6709\u968f\u673a\u6392\u5217\u7684\u539f\u5b50\u7ed3\u6784\uff0c\u5176\u7531\u590d\u6742\u7684\u5408\u91d1\u7ec4\u6210\uff0c\u5f53\u7194\u878d\u91d1\u5c5e\u51b7\u5374\u5f97\u975e\u5e38\u5feb\u65f6\uff0c\u5b83\u4eec\u4f1a\u5f62\u6210\u4e0d\u89c4\u5219\u7684\u7ed3\u6784\uff0c\u4ece\u800c\u9632\u6b62\u6676\u4f53\u7684\u5f62\u6210\u3002\u6700\u7ec8\u7684\u7ed3\u679c\u662f\uff0c\u8fd9\u79cd\u6750\u6599\u5728\u751f\u4ea7\u8fc7\u7a0b\u4e2d\u4e0e\u5851\u6599\u4e00\u6837\u67d4\u97e7\uff0c\u4f46\u968f\u540e\u53d8\u5f97\u575a\u786c\uff0c\u9002\u5408\u7528\u4f5c\u9ad8\u5c14\u592b\u7403\u6746\u548c\u673a\u5668\u4eba\u9f7f\u8f6e\u7b49\u7269\u4ef6\u3002<\/p>\n<p>\u8036\u9c81\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u901a\u8fc7\u5bf9\u91d1\u5c5e\u73bb\u7483\u8fdb\u884c\u53d6\u6837\u5e76\u4ece\u5176\u4e2d\u63d0\u53d6\u51fa\u7eb3\u7c73\u68d2\uff0c\u5f00\u53d1\u51fa\u4e86\u4ed6\u4eec\u7684\u65b0\u6750\u6599\uff0c\u5176\u76f4\u5f84\u53ea\u670935\u7eb3\u7c73\uff0c\u8fd9\u4e9b\u7eb3\u7c73\u68d2\u662f\u975e\u5e38\u5c0f\uff0c\u4ee5\u81f3\u4e8e\u6ca1\u6709\u7ed9\u6838\u9884\u7559\u7a7a\u95f4\u3002\u7814\u7a76\u4eba\u5458\u5c06\u8fd9\u4e00\u8fc7\u7a0b\u79f0\u4e3a\u201c\u6838\u9965\u997f\u201d\uff0c\u7531\u6b64\u4ea7\u751f\u4e86\u8be5\u6750\u6599\u7684\u4e00\u4e2a\u65b0\u7684\u76f8\u3002<\/p>\n<p>\u8be5\u9879\u76ee\u7684\u9996\u5e2d\u7814\u7a76\u5458Judy Cha\u8bf4\uff1a\u201c\u8fd9\u7ed9\u4e86\u6211\u4eec\u4e00\u4e2a\u63a7\u5236\u6837\u672c\u4e2d\u6838\u6570\u91cf\u7684\u65b9\u6cd5\u3002\u5f53\u5b83\u6ca1\u6709\u4efb\u4f55\u6838\u5fc3\u65f6\u2014\u2014\u5c3d\u7ba1\u4e8b\u5b9e\u4e0a\u5927\u81ea\u7136\u544a\u8bc9\u6211\u4eec\u5e94\u8be5\u6709\u4e00\u4e2a\u2014\u2014\u5b83\u4ea7\u751f\u4e86\u6211\u4eec\u4ee5\u524d\u4ece\u672a\u89c1\u8fc7\u7684\u8fd9\u4e2a\u5168\u65b0\u7684\u6676\u76f8\uff0c\u8fd9\u662f\u4e00\u79cd\u4ece\u65e7\u6750\u6599\u4e2d\u521b\u9020\u65b0\u6750\u6599\u7684\u65b9\u6cd5\u3002\u201d<\/p>\n<p>\u867d\u7136\u5f88\u96be\u786e\u5207\u5730\u8bf4\u51fa\u91d1\u5c5e\u73bb\u7483\u7684\u8fd9\u79cd\u65b0\u5f62\u5f0f\u53ef\u80fd\u6709\u54ea\u4e9b\u5e94\u7528\uff0c\u4f46\u7814\u7a76\u4eba\u5458\u8bf4\uff0c\u5236\u9020\u8fd9\u79cd\u5f62\u5f0f\u7684\u65b9\u6cd5\u662f\u4e3b\u8981\u7684\u4f18\u52bf\u6240\u5728\u3002\u901a\u8fc7\u5236\u9020\u4e0d\u540c\u76f4\u5f84\u7684\u91d1\u5c5e\u73bb\u7483\u7eb3\u7c73\u68d2\uff0c\u7814\u7a76\u4eba\u5458\u53ef\u4ee5\u63a7\u5236\u5b83\u4eec\u6709\u591a\u5c11\u4e2a\u6838\uff0c\u4ece\u800c\u5f00\u8f9f\u51fa\u4e00\u7cfb\u5217\u65b0\u7684\u6676\u76f8\u3002\u5bf9\u8fd9\u4e9b\u65b0\u6750\u6599\u7684\u6027\u80fd\u8fdb\u884c\u6d4b\u8bd5\u540e\u53ef\u80fd\u4f1a\u4ea7\u751f\u4e00\u4e9b\u610f\u60f3\u4e0d\u5230\u7684\u5e94\u7528\u3002<\/p>\n<p>Cha\u8bf4\uff1a\u201c\u5f53\u6211\u4eec\u8fd9\u6837\u505a\u7684\u65f6\u5019\uff0c\u8d8a\u6765\u8d8a\u591a\u6709\u8da3\u7684\u73b0\u8c61\u51fa\u73b0\u4e86\u3002\u6211\u4eec\u6b63\u5728\u6162\u6162\u4e86\u89e3\u7eb3\u7c73\u5c3a\u5ea6\u4e0a\u53d1\u751f\u7684\u6240\u6709\u8fd9\u4e9b\u6709\u8da3\u7684\u73b0\u8c61\uff0c\u6211\u4eec\u5bf9\u8fd9\u4e9b\u4f53\u7cfb\u5e76\u4e0d\u662f\u5f88\u4e86\u89e3\uff0c\u5f53\u6211\u4eec\u5728\u66f4\u5c0f\u7684\u7eb3\u7c73\u5c3a\u5ea6\u4e0a\u5bf9\u5b83\u4eec\u8fdb\u884c\u7814\u7a76\u65f6\uff0c\u5c31\u51fa\u73b0\u4e86\u4e00\u95e8\u65b0\u7684\u79d1\u5b66\u548c\u4e00\u95e8\u65b0\u7684\u7269\u7406\u5b66\u3002\u56e0\u4e3a\u5b83\u544a\u8bc9\u6211\u4eec\uff0c\u8fd9\u4e9b\u6211\u4eec\u4ee5\u524d\u6839\u672c\u6ca1\u6709\u6ce8\u610f\u5230\u7684\u65b0\u7684\u6e38\u4e50\u573a\u6b63\u5728\u5f62\u6210\uff0c\u800c\u4e14\u8fd8\u6709\u66f4\u591a\u9700\u8981\u63a2\u7d22\u7684\u5730\u65b9\u3002\u201d<\/p>\n<p>\u8fd9\u9879\u7814\u7a76\u5df2\u7ecf\u53d1\u8868\u5728\u671f\u520aNature Communications\u4e0a\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"https:\/\/newatlas.com\/yale-metallic-glass-material\/52529\/\" target=\"_blank\" rel=\"noopener\">New metallic glass material created by starving it of nuclei<\/a><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/www.nature.com\/articles\/s41467-017-02153-4\" target=\"_blank\" rel=\"noopener\">Tailoring crystallization phases in metallic glass nanorods via nucleus starvation<\/a><\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u9ec4\u4e9a\u7f16\u8bd1\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener noreferrer\">\u70b9\u6211\u52a0\u5165\u6750\u6599\u4eba\u7f16\u8f91\u90e8<\/a>\u3002<\/p>\n<p><strong>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1aRDD-2011-CHERISH\uff0c\u4efb\u4e39\u4e39\uff0c\u6211\u4eec\u4f1a\u9080\u8bf7\u5404\u4f4d\u8001\u5e08\u52a0\u5165\u4e13\u5bb6\u7fa4\u3002<\/strong><\/p>\n<p>\u4eea\u5668\u8bbe\u5907\u3001\u8bd5\u5242\u8017\u6750\u3001\u6750\u6599\u6d4b\u8bd5\u3001\u6570\u636e\u5206\u6790\uff0c\u627e<a href=\"http:\/\/lab.cailiaoren.com\/\" target=\"_blank\" rel=\"noopener noreferrer\">\u6750\u6599\u4eba<\/a>\u3001\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener noreferrer\">\u6d4b\u8bd5\u8c37<\/a>\uff01<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u5927\u81ea\u7136\u8fd8\u6709\u5f88\u591a\u503c\u5f97\u6211\u4eec\u63a2\u7d22\u7684\u5730\u65b9\uff0c\u6709\u4e9b\u4e1c\u897f\u6211\u4eec\u53d1\u73b0\u4e86\u5b83\u7684\u5b58\u5728\uff0c\u5374\u4e0d\u4e00\u5b9a\u77e5\u9053\u5b83\u6709\u4ec0\u4e48\u4f5c\u7528\uff0c\u4f46\u662f\uff0c\u6b63\u662f\u8fd9\u6837\u4e00\u70b9\u4e00\u70b9\u5730\u4e0d\u65ad\u63a2\u7d22\uff0c\u4eba\u7c7b\u624d\u4f1a\u4e0d\u65ad\u8fdb\u6b65\u3002\u8036\u9c81\u5927\u5b66\u7684&#8230;<\/p>\n","protected":false},"author":954,"featured_media":116852,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[293,54,33],"class_list":["post-116851","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-keji","tag-nature","tag-making","tag-nano"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/116851"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/954"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=116851"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/116851\/revisions"}],"predecessor-version":[{"id":116859,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/116851\/revisions\/116859"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/116852"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=116851"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=116851"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=116851"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}