{"id":11852,"date":"2016-05-07T08:00:19","date_gmt":"2016-05-07T00:00:19","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=11852"},"modified":"2016-05-12T21:08:03","modified_gmt":"2016-05-12T13:08:03","slug":"%e9%a1%b6%e5%88%8a%e5%8a%a8%e6%80%81%ef%bd%9c4%e6%9c%88%e4%bb%bdscience%e6%9d%90%e6%96%99%e5%89%8d%e6%b2%bf%e7%a7%91%e7%a0%94%e6%88%90%e6%9e%9c%e7%b2%be%e9%80%89","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=11852","title":{"rendered":"\u9876\u520a\u52a8\u6001\uff5c4\u6708\u4efdScience\u6750\u6599\u524d\u6cbf\u79d1\u7814\u6210\u679c\u7cbe\u9009"},"content":{"rendered":"<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-11607\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/1-4.jpg\" alt=\"1\" width=\"700\" height=\"185\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/1-4.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/1-4-300x79.jpg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p><strong>Science\u56db\u6708\u70ed\u70b9\u9884\u89c8<\/strong>\uff1a<strong>\u5bbe\u5915\u6cd5\u5c3c\u4e9a\u5927\u5b66<\/strong>\u4ec5\u7528\u80f6\u4f53\u7eb3\u7c73\u6676\u5236\u6210\u67d4\u6027\u573a\u6548\u5e94\u7eb3\u7c73\u6676\u4f53\u7ba1\uff1b<strong>\u65b0\u7f55\u5e03\u4ec0\u5c14\u5dde\u5927\u5b66<\/strong>\u5236\u5907\u5177\u6709\u78c1\u6027\u7684\u6c22\u5316\u77f3\u58a8\u70ef\uff1b<strong>\u4e39\u9ea6\u79d1\u6280\u5927\u5b66<\/strong>\u901a\u8fc7\u9567\u7cfb\u91d1\u5c5e\u8c03\u8282\u94c2\u5408\u91d1\u7684\u7535\u50ac\u5316\u6027\u80fd\uff1b<strong>\u8377\u5170\u5948\u6885\u4ea8\u5927\u5b66<\/strong>\u7814\u5236\u51fa\u5355\u539f\u5b50\u5b58\u50a8\u5668\uff1b<strong>\u8377\u5170\u7eb3\u7c73\u5149\u5b50\u5b66\u7814\u7a76\u6240\u4e2d\u5fc3<\/strong>\u603b\u7ed3\u5149\u4f0f\u53d1\u7535\u7cfb\u7edf\u7814\u7a76\u8fdb\u5c55\u3002<\/p>\n<p><strong>1\u3001\u5bbe\u5915\u6cd5\u5c3c\u4e9a\u5927\u5b66\u4ec5\u7528\u80f6\u4f53\u7eb3\u7c73\u6676\u5236\u6210\u67d4\u6027\u573a\u6548\u5e94\u7eb3\u7c73\u6676\u4f53<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-11844\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/1-8.jpg\" alt=\"1\" width=\"500\" height=\"685\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/1-8.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/1-8-219x300.jpg 219w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p>\u80f6\u4f53\u7eb3\u7c73\u6676\u4f53\u6750\u6599\u53ef\u4ee5\u5236\u5907\u51fa\u6027\u80fd\u622a\u7136\u4e0d\u540c\u7684\u5668\u4ef6\uff0c\u6bd4\u5982\u5bfc\u4f53\u3001\u534a\u5bfc\u4f53\u548c\u7edd\u7f18\u4f53\u3002\u867d\u7136\u8fd9\u79cd\u6750\u6599\u5df2\u7ecf\u5e94\u7528\u4e8e\u7535\u5b50\u8bbe\u5907\uff0c\u4f46\u73b0\u6709\u8bbe\u5907\u91cc\u901a\u5e38\u53ea\u4f1a\u542b\u6709\u4e00\u79cd\u7528\u8be5\u6750\u6599\u5236\u5907\u7684\u7ec4\u4ef6\u3002<\/p>\n<p>\u5bbe\u5915\u6cd5\u5c3c\u4e9a\u5927\u5b66\u7684Ji-Hyuk Choi\u3001Cherie R. Kagan\u7b49\u4eba\uff0c\u91c7\u7528\u57fa\u4e8e\u6eb6\u6db2\u52a0\u5de5\u7684\u65b9\u6cd5\uff0c\u901a\u8fc7\u9009\u62e9\u5408\u9002\u7684\u6750\u6599\u3001\u754c\u9762\u76f8\u5bb9\u6761\u4ef6\u4ee5\u53ca\u52a0\u5de5\u5de5\u827a\uff0c\u4ece\u800c\u8c03\u8282\u7eb3\u7c73\u6676\u4f53\u7ba1\u7684\u5c3a\u5bf8\u3001\u5f62\u72b6\u548c\u7ec4\u6210\uff0c\u4ee5\u5236\u6210\u4e0d\u7528\u6027\u80fd\u7684\u7ec4\u4ef6\u3002\u4ed6\u4eec\u4ee5\u6b64\u5236\u5907\u4e86\u5851\u6599\u67d4\u6027\u573a\u6548\u5e94\u7eb3\u7c73\u6676\u4f53\u7ba1\u6240\u9700\u7684\u6240\u6709\u7ec4\u4ef6\uff0c\u8be5\u6676\u4f53\u7ba1\u7684\u7535\u5b50\u8fc1\u79fb\u7387\u4e3a21.7cm2\/vs\u3002<\/p>\n<p>\u8fd9\u79cd\u67d4\u6027\u6676\u4f53\u7ba1\u6210\u672c\u4f4e\u3001\u6027\u80fd\u597d\u3001\u5e94\u7528\u5e7f\u6cdb\uff0c\u63d0\u9ad8\u4e86\u80f6\u4f53\u7eb3\u7c73\u6676\u4f53\u7684\u7ade\u4e89\u4f18\u52bf\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/science.sciencemag.org\/content\/352\/6282\/205\" target=\"_blank\">Exploiting the colloidal nanocrystal library to conelectronic struct devices<\/a><\/p>\n<p><strong>2\u3001\u65b0\u7f55\u5e03\u4ec0\u5c14\u5dde\u5927\u5b66\u5236\u5907\u5177\u6709\u78c1\u6027\u7684\u6c22\u5316\u77f3\u58a8\u70ef<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-11853\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/2-1-1.jpg\" alt=\"Science Magazine\" width=\"500\" height=\"300\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/2-1-1.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/2-1-1-300x180.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p>\u7814\u7a76\u6700\u5e7f\u6cdb\u7684\u4e8c\u7ef4\u6676\u4f53\u5c31\u662f\u77f3\u58a8\u70ef\uff0c\u6027\u80fd\u4f18\u5f02\uff0c\u672c\u8eab\u5374\u6ca1\u6709\u78c1\u6027\u3002\u5f15\u5165\u78c1\u6027\u6700\u597d\u7684\u65b9\u6cd5\u662f\u53bb\u6389\u4e2a\u522b\u78b3\u539f\u5b50\uff0c\u6216\u8005\u6c22\u5316\u3002\u4f46\u7531\u4e8e\u5176\u5316\u5b66\u6027\u8d28\u7a33\u5b9a\uff0c\u73b0\u5728\u4ecd\u662f\u4e00\u4e2a\u96be\u9898\u3002<\/p>\n<p>\u65b0\u7f55\u5e03\u4ec0\u5c14\u5dde\u5927\u5b66Gonzales-Herrero\u7b49\u4eba\uff0c\u9996\u5148\u5229\u7528STM\u9488\u5c16\u53bb\u9664\u4e86\u77f3\u58a8\u70ef\u4e0a\u4e00\u4e2a\u533a\u57df\u5185\u6240\u6709\u7684\u6c22\u539f\u5b50\uff0c\u968f\u540e\u6709\u5e8f\u5730\u589e\u52a0\u4e8614\u4e2a\u6c22\u539f\u5b50\u3002\u5b9e\u9a8c\u7ed3\u679c\u548c\u6a21\u62df\u7ed3\u679c\u90fd\u663e\u793a\uff0c\u8fd9\u79cd\u6750\u6599\u5177\u6709\u4f4e\u78c1\u6027\u3002<\/p>\n<p>\u8fd9\u79cd\u65b9\u6cd5\u4e00\u65e6\u5b9e\u73b0\u5de5\u4e1a\u5316\uff0c\u501f\u52a9\u77f3\u58a8\u70ef\u7279\u5f02\u7684\u7ed3\u6784\uff0c\u53ef\u4ee5\u7528\u4e8e\u50a8\u5b58\u9ad8\u5bc6\u5ea6\u7684\u4fe1\u606f\u3002S. M. Hollen\u8bc4\u4ef7\u8fd9\u79cd\u65b9\u6cd5\u7c7b\u4f3c\u4e8e\u5728\u753b\u677f\u4e0a\u753b\u753b\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/science.sciencemag.org\/content\/352\/6284\/437\" target=\"_blank\">Atomic-scale control of graphene magnetism by using hydrogen atoms<br \/>\n<\/a><br \/>\n<strong>3\u3001\u4e39\u9ea6\u79d1\u6280\u5927\u5b66\u901a\u8fc7\u9567\u7cfb\u91d1\u5c5e\u8c03\u8282\u94c2\u5408\u91d1\u7684\u7535\u50ac\u5316\u6027\u80fd<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-11854\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/3-1-1.jpg\" alt=\"3-1\" width=\"500\" height=\"169\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/3-1-1.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/3-1-1-300x101.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p>\u71c3\u6599\u7535\u6c60\u6c7d\u8f66\u5f25\u8865\u4e86\u9502\u7535\u6c7d\u8f66\u5145\u7535\u65f6\u95f4\u957f\uff0c\u7eed\u822a\u80fd\u529b\u77ed\uff0c\u65e0\u6cd5\u5728\u4f4e\u6e29\u4e0b\u4f7f\u7528\u7684\u7f3a\u70b9\u3002\u94c2\u4f5c\u4e3a\u805a\u5408\u7269\u819c\u71c3\u6599\u7535\u6c60\u7684\u9634\u6781\u50ac\u5316\u5242\uff0c\u5177\u6709\u5f88\u9ad8\u7684ORR\u50ac\u5316\u6027\u80fd\u3002\u4f46\u7531\u4e8e\u94c2\u4e3a\u8d35\u91d1\u5c5e\uff0c\u56e0\u6b64\u51cf\u5c11\u94c2\u7684\u4f7f\u7528\uff0c\u540c\u65f6\u83b7\u5f97\u9ad8ORR\u50ac\u5316\u6027\u80fd\u5c31\u663e\u5f97\u5c24\u4e3a\u5fc5\u8981\u3002<\/p>\n<p>\u4e39\u9ea6\u79d1\u6280\u5927\u5b66Escudero-Escribano\u7b49\u4eba\u7814\u7a76\u4e86\u4e00\u7cfb\u5217\u94c2\u4e0e\u9567\u7cfb\u5143\u7d20\u548c\u78b1\u91d1\u5c5e\u7ec4\u6210\u7684\u5408\u91d1\u7684ORR\u50ac\u5316\u6027\u80fd\u3002\u76f8\u8f83\u4e8e\u7eaf\u94c2\uff0c\u6027\u80fd\u6700\u9ad8\u63d0\u5347\u4e866\u500d\u3002\u9567\u7cfb\u91d1\u5c5e\u4e0e\u94c2\u6709\u7740\u5f88\u597d\u7684\u534f\u540c\u4f5c\u7528\uff0c\u8fd9\u4f7f\u5f97\u94c2\u5408\u91d1\u7684ORR\u50ac\u5316\u6027\u80fd\u4f18\u4e8e\u7eaf\u94c2\u3002\u7cbe\u5fc3\u7684\u8c03\u63a7\u5408\u91d1\u7ec4\u6210\u52a0\u4e4b\u5408\u7406\u7684\u9000\u706b\u5904\u7406\u5de5\u827a\uff0c\u5c06\u4f1a\u83b7\u5f97\u5341\u5206\u4f18\u5f02\u7684\u50ac\u5316\u6d3b\u6027\u548c\u957f\u4e45\u7684\u7a33\u5b9a\u6027\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/science.sciencemag.org\/content\/352\/6281\/73\" target=\"_blank\">Tuning the activity of Pt alloy electrocatalysts by means of the lanthanide contraction<\/a><\/p>\n<p><strong>4\u3001\u8377\u5170\u5948\u6885\u4ea8\u5927\u5b66\u7814\u5236\u51fa\u5355\u539f\u5b50\u5b58\u50a8\u5668<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-11855\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/4-1-1.jpg\" alt=\"4-1\" width=\"500\" height=\"441\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/4-1-1.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/4-1-1-300x265.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p>\u5355\u539f\u5b50\u78c1\u94c1\u96c6\u5408\u5b58\u50a8\u4fe1\u606f\u662f\u6570\u636e\u5b58\u50a8\u6280\u672f\u5c0f\u578b\u5316\u7684\u6838\u5fc3\uff0c\u6bcf\u4e00\u4e2a\u539f\u5b50\u6709\u4e24\u4e2a\u65b9\u5411\u53ef\u5b58\u50a8\u5c11\u91cf\u4fe1\u606f\u3002\u7136\u800c\uff0c\u5f88\u96be\u5728\u5355\u539f\u5b50\u4e2d\u4fdd\u7559\u5269\u78c1\uff0c\u56e0\u4e3a\u8981\u524a\u5f31\u5916\u754c\u73af\u5883\u6ce2\u52a8\u7684\u5f71\u54cd\uff0c\u5c06\u4e0d\u53ef\u907f\u514d\u5730\u7834\u574f\u78c1\u533a\uff0c\u4f7f\u78c1\u6027\u5b58\u50a8\u5668\u4fe1\u606f\u88ab\u64e6\u9664\u3002Alexander Ako Khajetoorians\u7b49\u53d1\u73b0\u5355\u4e00\u94ac\uff08Ho\uff09\u539f\u5b50\u5177\u6709\u5269\u78c1\u6027\uff0c\u6e29\u5ea6\u4e0a\u9650\u53ef\u8fbe40 K\uff0c\u4e14\u5927\u5c0f\u548c\u7a33\u5b9a\u6027\u8fdc\u9ad8\u4e8e\u539f\u5b50\u5c3a\u5ea6\u4e3a3-12\u4e2a\u78c1\u94c1\u539f\u5b50\u7684\u73b0\u6709\u8bb0\u5f55\u3002<\/p>\n<p>\u5355\u539f\u5b50\u78c1\u94c1\u96c6\u5408\u80fd\u591f\u7528\u4f5c\u672a\u6765\u7684\u5b58\u50a8\u8bbe\u5907\uff0c\u5728\u5de5\u7a0b\u4e0a\u4e5f\u53ef\u4ee5\u4e3a\u65cb\u8f6c\u78c1\u573a\u4e2d\u5fc3\u7684\u78c1\u529b\u8026\u5408\u5668\u63d0\u4f9b\u4e00\u4e2a\u9002\u5b9c\u7684\u8def\u5f84\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/science.sciencemag.org\/content\/352\/6283\/296.full\" target=\"_blank\">Toward single-atom memory<\/a><\/p>\n<p><strong>5\u3001\u8377\u5170\u7eb3\u7c73\u5149\u5b50\u5b66\u7814\u7a76\u6240\u4e2d\u5fc3\u603b\u7ed3\u5149\u4f0f\u53d1\u7535\u7cfb\u7edf\u7814\u7a76\u8fdb\u5c55<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-11856\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/5-1-1.jpg\" alt=\"5-1\" width=\"500\" height=\"282\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/5-1-1.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/5-1-1-300x169.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p>\u8fd1\u51e0\u5e74\u7684\u5927\u578b\u5149\u4f0f\u53d1\u7535\u7cfb\u7edf\u9ad8\u901f\u53d1\u5c55\u3002\u7531\u4e8e\u5149\u4f0f\u53d1\u7535\u7cfb\u7edf\u7684\u6210\u672c\u5728\u4e00\u5b9a\u7a0b\u5ea6\u4e0a\u4ec5\u53d6\u51b3\u4e8e\u592a\u9633\u80fd\u7535\u6c60\u7684\u6210\u672c\uff0c\u56e0\u6b64\u9700\u8981\u63d0\u9ad8\u7535\u6c60\u6548\u7387\u4ee5\u964d\u4f4e\u592a\u9633\u80fd\u53d1\u7535\u6210\u672c\u3002\u76ee\u524d\u6709\u51e0\u4e2a\u673a\u6784\u6b63\u5728\u7814\u7a76\uff0c\u4ee5\u7814\u5236\u51fa\u9ad8\u6548\u7387\u3001\u4f4e\u6210\u672c\u7684\u5149\u4f0f\u53d1\u7535\u7cfb\u7edf\u3002Albert Polman\u7b49\u4eba\uff0c\u5168\u9762\u7cfb\u7edf\u5730\u56de\u987e\u4e86\u9886\u5148\u7684\u5019\u9009\u6750\u6599\uff0c\u63d0\u51fa\u4e86\u6bcf\u4e2a\u7cfb\u7edf\u7684\u5c40\u9650\u6027\uff0c\u5e76\u5206\u6790\u4e86\u5982\u4f55\u514b\u670d\u8fd9\u4e9b\u56f0\u96be\uff0c\u4ee5\u4f7f\u6574\u4f53\u6027\u80fd\u63d0\u9ad8\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/science.sciencemag.org\/content\/352\/6283\/aad4424\" target=\"_blank\">Photovoltaic materials: Present efficiencies and future challenges<\/a><\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u79d1\u666e\u56e2\u961f\u63d0\u4f9b\uff0c\u6211\u4eec\u6301\u7eed\u8ddf\u8e2a\u56fd\u9645\u5b66\u672f\u52a8\u6001\uff0c\u5c06\u6750\u6599\u76f8\u5173\u9ad8\u8d28\u91cf\u520a\u7269\u4e2d\u5907\u53d7\u5173\u6ce8\u7684\u5b66\u672f\u6210\u679c\u8fdb\u884c\u6574\u7406\u548c\u6c47\u603b\uff0c\u4ee5\u5468\u62a5\u6216\u8005\u6708\u62a5\u7684\u5f62\u5f0f\u53d1\u5e03\uff0c\u6b22\u8fce\u5173\u6ce8\u3002<\/p>\n<p>\u6b22\u8fce\u52a0\u5165\u6750\u6599\u4eba\u79d1\u666e\u56e2\u961f\uff0c<a href=\"http:\/\/cailiaoren.mikecrm.com\/f.php?t=6qSdMU\" target=\"_blank\">\u70b9\u51fb\u83b7\u5f97\u62a5\u540d\u8868<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>Science\u56db\u6708\u70ed\u70b9\u9884\u89c8\uff1a\u5bbe\u5915\u6cd5\u5c3c\u4e9a\u5927\u5b66\u4ec5\u7528\u80f6\u4f53\u7eb3\u7c73\u6676\u5236\u6210\u67d4\u6027\u573a\u6548\u5e94\u7eb3\u7c73\u6676\u4f53\u7ba1\uff1b\u65b0\u7f55\u5e03\u4ec0\u5c14\u5dde\u5927\u5b66\u5236\u5907\u5177\u6709\u78c1\u6027\u7684\u6c22\u5316\u77f3\u58a8\u70ef\uff1b\u4e39\u9ea6\u79d1\u6280\u5927\u5b66\u901a\u8fc7\u9567\u7cfb\u91d1\u5c5e\u8c03\u8282\u94c2\u5408\u91d1\u7684&#8230;<\/p>\n","protected":false},"author":418,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2,67],"tags":[116,27,46,33],"class_list":["post-11852","post","type-post","status-publish","format-standard","hentry","category-keji","category-zhoubao","tag-catalyst","tag-cell","tag-graphene","tag-nano"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/11852"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/418"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=11852"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/11852\/revisions"}],"predecessor-version":[{"id":11861,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/11852\/revisions\/11861"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=11852"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=11852"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=11852"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}