{"id":12053,"date":"2016-05-08T17:00:33","date_gmt":"2016-05-08T09:00:33","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=12053"},"modified":"2016-05-08T15:19:00","modified_gmt":"2016-05-08T07:19:00","slug":"%e9%a1%b6%e5%88%8a%e5%8a%a8%e6%80%81%e4%b8%a8nature%e5%ad%90%e5%88%8apnasjacsangewandte%e7%ad%89%e7%94%9f%e7%89%a9%e6%9d%90%e6%96%99%e5%ad%a6%e6%9c%af%e8%bf%9b%e5%b1%95%e6%b1%87%e6%80%bb%ef%bc%884","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=12053","title":{"rendered":"\u9876\u520a\u52a8\u6001\u4e28Nature\u5b50\u520a\/PNAS\/JACS\/Angewandte\u7b49\u751f\u7269\u6750\u6599\u5b66\u672f\u8fdb\u5c55\u6c47\u603b\uff084.27-5.5\uff09"},"content":{"rendered":"<p style=\"text-align: left;\"><strong>1\u3001Nature Nanotechnology\uff1a\u9ad8\u901f\u539f\u5b50\u529b\u663e\u5fae\u955c\u6709\u52a9\u4e8e\u7406\u89e3\u6838\u5b54\u590d\u5408\u4f53\u8fd0\u8f93\u673a\u7406<\/strong><\/p>\n<p style=\"text-align: center;\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12056\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72471-3.jpg\" alt=\"\u56fe\u72471\" width=\"500\" height=\"265\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72471-3.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72471-3-300x159.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><br \/>\n\u56fe1 \u6838\u5b54\u5bf9\u5927\u5206\u5b50\u7269\u8d28\u7684\u9009\u62e9\u6027\u8fd0\u8f93\u673a\u7406<\/p>\n<p>\u6838\u5b54\u590d\u5408\u4f53\uff08NPCs\uff09\u63a7\u5236\u7740\u5927\u5206\u5b50\u5728\u7ec6\u80de\u6838\u548c\u7ec6\u80de\u8d28\u4e4b\u95f4\u7684\u53cc\u5411\u8fd0\u8f93\uff0c\u8fd9\u4e2a\u8fc7\u7a0b\u9700\u8981\u65e0\u5b9a\u578b\u7684\u6838\u5b54\u86cb\u767d\u7684\u53c2\u4e0e\uff08Nups\uff09\uff0c\u4f46\u662fNPCs\u4e3a\u4ec0\u4e48\u5177\u6709\u9009\u62e9\u900f\u8fc7\u6027\u8fd8\u65e0\u6cd5\u5f97\u77e5\u3002<\/p>\n<p>\u6700\u8fd1\u745e\u58eb\u5df4\u585e\u5c14\u5927\u5b66\u7684Yusuke Sakiyama\u7b49\u4eba\u7528\u9ad8\u901f\u539f\u5b50\u529b\u663e\u5fae\u955c\uff08HS-AFM\uff09\u7814\u7a76\u4e86 Nups\u5728\u7eb3\u7c73\u5c3a\u5bf8\u4e0a\u7684\u65f6\u7a7a\u8fd0\u52a8\u3002\u4ed6\u4eec\u89c2\u5bdf\u5230\u4e86\u6838\u5b54\u5468\u56f4\u7684\u516b\u4e2aNups\uff0c\u8fd9\u4e9bNups\u4e00\u5934\u88ab\u56fa\u5b9a\u5728\u6838\u5b54\uff08\u4e0e\u7ec6\u80de\u8d28\u8fde\u63a5\u4e00\u9762\uff09\u7684\u56db\u5468\uff0c\u800c\u5269\u4e0b\u7684\u591a\u80bd\u94fe\u53ef\u4ee5\u5728\u5b54\u5185\u8fd0\u52a8\uff0c\u8fd9\u4e9b\u591a\u80bd\u94fe\u5f62\u6210\u4e00\u4e2a\u201c\u7b5b\u5b50\u201d\uff08\u7b5b\u5b50\u7684\u5f62\u72b6\u4e0d\u662f\u56fa\u5b9a\u7684\uff09\uff0c\u8fd0\u52a8\u5feb\u7684\u5c0f\u5206\u5b50\u53ef\u4ee5\u5f88\u5bb9\u6613\u901a\u8fc7\u8fd9\u4e2a\u7b5b\u5b50\uff0c\u8fd0\u52a8\u6162\u7684\u5927\u5206\u5b50\u5219\u5f88\u96be\u901a\u8fc7\uff0c\u800c\u8f7d\u6709\u201c\u8d27\u7269\u201d\u7684\u5927\u5206\u5b50\u56e0\u4e3a\u80fd\u4e0e\u591a\u80bd\u94fe\u7ed3\u5408\u4e5f\u80fd\u901a\u8fc7\u6838\u5b54\u3002\u8be5\u5b9e\u9a8c\u7b2c\u4e00\u6b21\u76f4\u63a5\u8bc1\u5b9eNups\u7684\u963b\u788d\u4f5c\u7528\uff0c\u4e5f\u8bc1\u660eHS-AFM\u5728\u7814\u7a76\u9ad8\u901f\u8fd0\u52a8\u5e76\u4e14\u65e0\u5b9a\u578b\u7cfb\u7edf\u65b9\u9762\u7684\u4f5c\u7528\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/www.nature.com\/nnano\/journal\/vaop\/ncurrent\/full\/nnano.2016.62.html\" target=\"_blank\">Spatiotemporal dynamics of the nuclear pore complex transport barrier resolved by high-speed atomic force microscopy<\/a><\/p>\n<p><strong>2\u3001Angewandte\uff1a\u4e00\u79cd\u975e\u8840\u7ea2\u7d20\u94c1\u6df7\u6742\u9176\u7684\u53d1\u73b0<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12057\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72472-3.jpg\" alt=\"\u56fe\u72472\" width=\"500\" height=\"300\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72472-3.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72472-3-300x180.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe2 AmbO5\u80fd\u50ac\u5316\u7684\u5364\u4ee3\u53cd\u5e94<\/p>\n<p>\u86cb\u767d\u8d28\u57fa\u50ac\u5316\u5242\u662f\u4e00\u79cd\u5f88\u6709\u524d\u666f\u7684\u80fd\u8ba9\u5364\u539f\u5b50\u53d6\u4ee3sp3\u6742\u5316\u7684\u78b3\u539f\u5b50\u4e0a\u6c22\u539f\u5b50\u7684\u50ac\u5316\u5242\uff0c\u800c\u5364\u5316\u9176WelO5\u5c31\u662f\u4e00\u79cd\u80fd\u8ba9\u5432\u54da\u7c7b\u751f\u7269\u78b1\u4e0a\u7684sp3\u6742\u5316\u78b3\u539f\u5b50\u53d1\u751f\u5364\u4ee3\u53cd\u5e94\u7684\u9176\uff0c\u4f46\u662f\u5b83\u53ea\u80fd\u50ac\u5316\u4e24\u4e2a\u53cd\u5e94\u3002<\/p>\n<p>\u6700\u8fd1\u7f8e\u56fd\u514b\u5179\u5821\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u53d1\u73b0AmbO5\uff08\u4e0eWelO5\u662f\u540c\u65cf\u5364\u4ee3\u9176\uff0c\u4e14\u5b83\u4eec\u670979%\u76f8\u540c\u7684\u6c28\u57fa\u9178\u5e8f\u5217\uff09\u80fd\u4f7f7\u79cd\uff08\u5305\u542bWelO5\u80fd\u50ac\u5316\u7684\u4e24\u79cd\uff09\u5b98\u80fd\u56e2\u3001\u78b3\u9aa8\u67b6\u548c\u6784\u8c61\u90fd\u4e0d\u540c\u7269\u8d28\u53d1\u751f\u5364\u4ee3\u53cd\u5e94\u3002\u4ed6\u4eec\u8ba4\u4e3aAmbO5\u548cWelO5\u662f\u7531\u540c\u4e00\u79cd\u86cb\u767d\u8d28\u6f14\u5316\u6765\u7684\uff0c\u5e76\u4e14\u901a\u8fc7\u5c06AmbO5\u548cWelO5\u7ec4\u5408\u548c\u5bf9\u4fee\u6539WelO5\u4e0a\u768418\u4e2a\u6c28\u57fa\u9178\u5e8f\u5217\u518d\u8fdb\u884c\u50ac\u5316\u5b9e\u9a8c\u521d\u6b65\u8bc1\u5b9e\u4ed6\u4eec\u7684\u731c\u6d4b\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/anie.201601447\/full\" target=\"_blank\">Discovery of a Promiscuous Non-Heme Iron Halogenase in Ambiguine Alkaloid Biogenesis: Implication for an Evolvable Enzyme Family for Late-Stage Halogenation of Aliphatic Carbons in Small Molecules<\/a><\/p>\n<p><strong>3\u3001Angewandte\uff1aDNA\u635f\u4f24\u4fee\u590d\u673a\u7406<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12058\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72473-3.jpg\" alt=\"\u56fe\u72473\" width=\"410\" height=\"161\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72473-3.jpg 410w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72473-3-300x118.jpg 300w\" sizes=\"(max-width: 410px) 100vw, 410px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe3 AZT\u548cT-AU\u5728\u4e0d\u540c\u5149\u7167\u4e0b\u7684\u76f8\u4e92\u8f6c\u6362<\/p>\n<p>\u7d2b\u5916\u7ebf\u53ef\u4ee5\u4f7fDNA\u94fe\u4e0a\u76f8\u90bb\u7684\u5627\u5576\u4ee5\u5171\u4ef7\u952e\u8fde\u6210\u4e8c\u805a\u4f53\uff08\u4e3b\u8981\u5305\u62ec\u73af\u4e01\u70f7\u5627\u5576\u4e8c\u805a\u4f53\uff08CPD\uff09\u548c\uff086-4\uff09\u5149\u4ea7\u7269\uff086-4PP\uff09\uff09\uff0c\u4ece\u800c\u4f7fDNA\u53d7\u5230\u635f\u4f24\u3002\u5149\u4fee\u590d\u9176\u80fd\u5229\u7528\u9633\u5149\u6765\u4fee\u590d\u8fd9\u4e9b\u53d7\u635f\u7684DNA\uff0c\u5149\u4fee\u590d\u9176\u7531\u4e24\u90e8\u5206\u7ec4\u6210\uff0c\u7b2c\u4e00\u90e8\u5206\u5438\u6536\u5149\u80fd\u5e76\u5c06\u80fd\u91cf\u8f6c\u79fb\u5230\u7b2c\u4e8c\u90e8\u5206\uff0c\u7b2c\u4e8c\u90e8\u5206\u5219\u5c06\u7535\u5b50\u8f6c\u79fb\u5230CPD\u4e0a\u4f7f\u73af\u4e01\u70f7\u5206\u88c2\u4ece\u800c\u4fee\u590dDNA\u3002\u4f46\u662f\u5149\u4fee\u590d\u9176\u4fee\u590d6-4PP\u7684\u673a\u7406\u8fd8\u4e0d\u662f\u5f88\u6e05\u695a\u3002<\/p>\n<p>\u6700\u8fd1\uff0c\u897f\u73ed\u7259\u7684\u79d1\u5b66\u5bb6\u5229\u7528CPD\u7684\u7c7b\u4f3c\u7269AZT\u6765\u6a21\u62df\u5149\u4fee\u590d\u9176\u4fee\u590d6-4PP\u7684\u8fc7\u7a0b\u3002AZT\u7531T-AU\u5728\u5149\u7167\u6761\u4ef6\u4e0b\u53d1\u751f\u73af\u52a0\u6210\u53cd\u5e94\u5f97\u5230\uff0c\u800cAZT\u5728\u5149\u4fee\u590d\u9176\u548c\u5149\u7684\u4f5c\u7528\u4e0b\u53c8\u751f\u6210T-AU\u3002\u8be5\u5b9e\u9a8c\u9996\u6b21\u8bc1\u660e\u5149\u4fee\u590d\u9176\u5728\u5149\u7684\u8bf1\u5bfc\u4e0b\u53ef\u4ee5\u5c06\u4e00\u4e2a\u7535\u5b50\u6ce8\u5165\u5230CPD\u7c7b\u4f3c\u7269\u4e2d\u5f15\u8d77\u73af\u4e01\u70f7\u7684\u5206\u88c2\u4ece\u800c\u4fee\u590d\u6838\u7877\u57fa\uff0c\u8be5\u53d1\u73b0\u6709\u52a9\u4e8e\u7406\u89e36-4PP\u5149\u4fee\u590d\u9176\u7684\u4fee\u590d\u673a\u7406\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/anie.201601475\/full\" target=\"_blank\">Repair of a Dimeric Azetidine Related to the Thymine\u2013Cytosine (6-4) Photoproduct by Electron Transfer Photoreduction<\/a><\/p>\n<p><strong>4\u3001JACS\uff1aSiO2\u7eb3\u7c73\u82b1\u7c89\u589e\u5f3a\u7c98\u9644\u52a9\u529b\u957f\u671f\u6291\u83cc<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12059\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72474-3.jpg\" alt=\"\u56fe\u72474\" width=\"476\" height=\"468\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72474-3.jpg 476w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72474-3-300x295.jpg 300w\" sizes=\"(max-width: 476px) 100vw, 476px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe4 \uff08a\uff09\u5236\u5907\u7eb3\u7c73\u82b1\u7c89\u7684\u793a\u610f\u56fe\uff1b\uff08b\uff09\u88c5\u6709\u6eb6\u83cc\u9176\u7684\u82b1\u7c89\u7c98\u9644\u5728\u7ec6\u83cc\u8868\u9762<\/p>\n<p>\u82b1\u7c89\u9897\u7c92\u8868\u9762\u5f88\u7c97\u7cd9\uff0c\u6700\u5916\u5c42\u957f\u6709\u5f88\u591a\u201c\u9489\u5b50\u201d\uff0c\u8fd9\u4e9b\u9489\u5b50\u6709\u52a9\u4e8e\u82b1\u7c89\u7c98\u9644\u5728\u6606\u866b\u7684\u76ae\u6bdb\u4e0a\uff0c\u4ece\u800c\u5728\u6606\u866b\u7684\u5e2e\u52a9\u4e0b\u5b8c\u6210\u6388\u7c89\u3002<\/p>\n<p>\u53d7\u5230\u82b1\u7c89\u7684\u542f\u53d1\uff0c\u6fb3\u6d32\u6606\u58eb\u5170\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u7528\u7b80\u5355\u7684\u65b9\u6cd5\u5236\u5907\u4e86SiO2\u7eb3\u7c73\u201c\u82b1\u7c89\u201d\uff0c\u8fd9\u4e9b\u82b1\u7c89\u7684\u76f4\u5f84\u5927\u7ea6\u4e3a257nm\uff0c\u8868\u9762\u5f62\u8c8c\u4e0e\u771f\u5b9e\u7684\u82b1\u7c89\u76f8\u4f3c\uff0c\u56e0\u6b64\u5f88\u5bb9\u6613\u7c98\u9644\u5728\u7ec6\u83cc\u8868\u9762\u7684\u7ea4\u6bdb\u4e0a\u3002\u4ed6\u4eec\u5728\u82b1\u7c89\u8868\u9762\u7684\u5c0f\u5b54\u91cc\u88c5\u4e0a\u6eb6\u83cc\u9176\uff0c\u5f53\u8f7d\u6709\u6eb6\u83cc\u9176\u7684\u82b1\u7c89\u7c98\u9644\u5728\u7ec6\u83cc\u8868\u9762\u540e\uff0c\u6eb6\u83cc\u9176\u88ab\u7f13\u6162\u7684\u91ca\u653e\u51fa\u6765\u3002\u4e8e\u662f\u82b1\u7c89\u4e0d\u4ec5\u63d0\u9ad8\u4e86\u6eb6\u83cc\u9176\u7684\u5229\u7528\u6548\u7387\uff0c\u800c\u4e14\u8fd8\u5ef6\u957f\u4e86\u5b83\u7684\u6291\u83cc\u5468\u671f\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/jacs.6b00243\" target=\"_blank\">Silica Nano-Pollens Enhance Adhesion for Long-Term Bacterial Inhibition<\/a><\/p>\n<p><strong>5\u3001Angewandte\uff1a\u94c1\u57fa\u50ac\u5316\u5242\u9009\u62e9\u6027\u6c27\u5316\u753e\u4f53\u5e95\u7269\u4e0a\u7684\u78b3\u539f\u5b50<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12060\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72475-3.jpg\" alt=\"\u56fe\u72475\" width=\"500\" height=\"327\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72475-3.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72475-3-300x196.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe5 \u5408\u6210\u7684\u56db\u79cd\u50ac\u5316\u5242<\/p>\n<p>\u9009\u62e9\u6027\u6c27\u5316\u70f7\u57fa\u4e0a\u7684C-H\u952e\u5728\u6709\u673a\u5408\u6210\u4e2d\u662f\u5f88\u91cd\u8981\u7684\u4e00\u7c7b\u53cd\u5e94\uff0c\u4f46\u662f\u80fd\u88ab\u6c27\u5316\u7684\u5f80\u5f80\u662f\u6bd4\u8f83\u6d3b\u8dc3\u7684C-H\u952e\uff0c\u800c\u5927\u90e8\u5206\u7684C-H\u952e\u662f\u4e0d\u80fd\u88ab\u6c27\u5316\u7684\u3002<\/p>\n<p>\u6700\u8fd1\u897f\u73ed\u7259\u7684\u7814\u7a76\u4eba\u5458\u5408\u6210\u4e86\u56db\u79cd\u94c1\u57fa\u590d\u5408\u7269\uff08\u5176\u4e2d\u4e24\u79cd\u8ddf\u53e6\u5916\u4e24\u79cd\u5206\u522b\u662f\u624b\u6027\u5bf9\u79f0\u7684\uff09\uff0c\u5b83\u4eec\u4e0d\u4ec5\u80fd\u9009\u62e9\u6027\u6c27\u5316\u753e\u4f53\u5e95\u7269\u4e0a\u7684\u70f7\u57faC-H\u952e\uff0c\u800c\u4e14\u624b\u6027\u4e0d\u540c\u65f6\u5b83\u4eec\u5bf9\u4e0d\u540cC-H\u952e\u7684\u6c27\u5316\u80fd\u529b\u6539\u53d8\uff0c\u8fd9\u662f\u9996\u6b21\u5728\u5408\u6210\u7684\u50ac\u5316\u5242\u4e0a\u89c2\u5bdf\u5230\u8fd9\u79cd\u73b0\u8c61\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/anie.201600785\/full\" target=\"_blank\">Readily Accessible Bulky Iron Catalysts exhibiting Site Selectivity in the Oxidation of Steroidal Substrates<\/a><\/p>\n<p><strong>6\u3001Angewandte\uff1a\u5fae\u80f6\u56ca\u63d0\u9ad8\u5927\u80a0\u6746\u83cc\u4ee3\u8c22\u4ea7\u7269\u4e2d\u82ef\u4e59\u70ef\u7684\u542b\u91cf<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12061\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72476-3.jpg\" alt=\"\u56fe\u72476\" width=\"274\" height=\"143\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe6 \u82ef\u4e59\u70ef\u5728\u5fae\u80f6\u56ca\u91cc\u5bcc\u96c6<\/p>\n<p>\u5229\u7528\u5fae\u751f\u7269\u6765\u5408\u6210\u4e00\u4e9b\u91cd\u8981\u7684\u5c0f\u5206\u5b50\u6709\u673a\u7269\u662f\u7eff\u8272\u5408\u6210\u7684\u91cd\u8981\u7ec4\u6210\u90e8\u5206\uff0c\u8fd9\u4e9b\u5c0f\u5206\u5b50\u4e00\u822c\u662f\u5fae\u751f\u7269\u7684\u4ee3\u8c22\u4ea7\u7269\uff0c\u5b83\u4eec\u5bf9\u5fae\u751f\u7269\u6709\u4e00\u5b9a\u7684\u6bd2\u6027\uff0c\u8d85\u8fc7\u4e00\u5b9a\u7684\u6d53\u5ea6\u4f1a\u4f7f\u5fae\u751f\u7269\u6b7b\u4ea1\uff0c\u56e0\u6b64\u8fd9\u79cd\u65b9\u6cd5\u83b7\u5f97\u7684\u5c0f\u5206\u5b50\u4ea7\u91cf\u662f\u6709\u9650\u7684\u3002<\/p>\n<p>\u6700\u8fd1\uff0c\u54c8\u4f5b\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u53d1\u73b0\u4e00\u4e9b\u4e24\u4eb2\u6027\u7ef4\u751f\u7d20E\u884d\u751f\u7269\u5728\u57f9\u517b\u6db2\u4e2d\u80fd\u5f62\u6210\u5fae\u80f6\u56ca\uff0c\uff08\u80fd\u751f\u6210\u82ef\u4e59\u70ef\u7684\uff09\u50ac\u5316\u5242\u548c\u53cd\u5e94\u7269\u5728\u5fae\u80f6\u56ca\u91cc\u5bcc\u96c6\uff0c\u5e76\u4e14\u751f\u6210\u7684\u82ef\u4e59\u70ef\u4e5f\u7559\u5728\u5fae\u80f6\u56ca\u4e2d\uff0c\u56e0\u6b64\u964d\u4f4e\u4e86\u82ef\u4e59\u70ef\u5bf9\u5fae\u751f\u7269\u7684\u6bd2\u6027\uff0c\u4f7f\u5f97\u82ef\u4e59\u70ef\u7684\u4ea7\u91cf\u63d0\u9ad8\u4e86\u51e0\u500d\u3002\u8fd9\u79cd\u6280\u672f\u5728\u751f\u7269\u5408\u6210\u5c0f\u5206\u5b50\u65b9\u9762\u5f88\u6709\u524d\u666f\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/anie.201600966\/full\" target=\"_blank\">Designer Micelles Accelerate Flux Through Engineered Metabolism in\u00a0E. coli\u00a0and Support Biocompatible Chemistry<\/a><\/p>\n<p><strong>7\u3001ACS Nano\uff1a\u7528\u6c27\u5316\u77f3\u58a8\u70ef\u63a2\u6d4b\u9176\u7684\u6d3b\u6027\u4ee5\u53ca\u7b5b\u9009\u6291\u5236\u5242<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12062\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72477-3.jpg\" alt=\"\u56fe\u72477\" width=\"500\" height=\"218\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72477-3.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72477-3-300x131.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe7 \u6c27\u5316\u77f3\u58a8\u70ef\u8367\u5149\u5f3a\u5ea6\u6539\u53d8\u7684\u673a\u7406<\/p>\n<p>\u8001\u5e74\u75f4\u5446\u75c7\uff08AD\uff09\u4e00\u822c\u88ab\u8ba4\u4e3a\u4e0e\u4e59\u9170\u80c6\u78b1\u916f\u9176\uff08AChE\uff09\u50ac\u5316\u4e59\u9170\u80c6\u78b1\uff08ATCh\uff09\u751f\u6210\u786b\u4ee3\u80c6\u78b1\u548c\u4e59\u9178\u7684\u53cd\u5e94\u6709\u5173\u3002\u6291\u5236AChE\u7684\u6d3b\u6027\u662f\u4e00\u79cd\u5ef6\u7f13AD\u53d1\u75c5\u7684\u6709\u6548\u65b9\u6cd5\uff0c\u4f46\u662f\u76ee\u524d\u8fd8\u6ca1\u6709\u63a2\u6d4bAChE\u6d3b\u6027\u7684\u7b80\u4fbf\u65b9\u6cd5\uff0c\u56e0\u6b64\u4e5f\u5f88\u96be\u53d1\u73b0\u80fd\u6291\u5236AChE\u6d3b\u6027\u7684\u7269\u8d28\u3002<\/p>\n<p>\u6700\u8fd1\uff0c\u97e9\u56fd\u6c49\u9633\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u7528\u591a\u7cd6\u6765\u975e\u5171\u4ef7\u952e\u5730\u4fee\u9970\u6c27\u5316\u77f3\u58a8\u70ef\uff08PhO-dex-GO\uff09\uff0cPhO-dex-GO\u80fd\u5728\u591a\u79cd\u6eb6\u6db2\u4e2d\u4fdd\u6301\u5206\u6563\u72b6\u6001\uff0c\u5b83\u7684\u8367\u5149\u5f3a\u5ea6\u968f\u4e59\u9178\uff08\u53cd\u5e94\u4ea7\u7269\uff09\u7684\u6d53\u5ea6\u589e\u52a0\u800c\u589e\u52a0\uff0c\u800c\u4e0eAChE\u548cATCh\u7684\u6d53\u5ea6\u65e0\u5173\u3002\u56e0\u6b64\u901a\u8fc7PhO-dex-GO\u7684\u8367\u5149\u5f3a\u5ea6\u80fd\u5f88\u5bb9\u6613\u786e\u5b9aAChE\u7684\u6d3b\u6027\uff0c\u4ece\u800c\u80fd\u66f4\u52a0\u65b9\u4fbf\u7684\u53d1\u73b0\u5bf9\u6291\u5236AChE\u6d3b\u6027\u8d77\u6291\u5236\u4f5c\u7528\u7684\u7269\u8d28\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acsnano.6b01495\" target=\"_blank\">Optical Detection of Enzymatic Activity and Inhibitors on Non-Covalently Functionalized Fluorescent Graphene Oxide<\/a><\/p>\n<p><strong>8\u3001Angewandte\uff1a\u6ce8\u6cb9\u591a\u5b54\u8868\u9762\u80fd\u9632\u6c61\u57a2\u548c\u6740\u6b7b\u6eb6\u6db2\u4e2d\u7684\u75c5\u539f\u4f53<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12063\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72478-1.jpg\" alt=\"\u56fe\u72478\" width=\"500\" height=\"212\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72478-1.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72478-1-300x127.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe8 SLIPS\u8868\u9762\u7684\u9632\u6c61\u57a2\u6548\u679c<\/p>\n<p>\u6da6\u6ed1\u6db2\u4f53\u6ce8\u5165\u591a\u5b54\u8868\u9762\uff08SLIPS\uff09\u662f\u5c06\u6cb9\u6ce8\u5165\u591a\u5b54\u8868\u9762\u5f62\u6210\u7684\u4e00\u79cd\u81ea\u6e05\u6d01\u8868\u9762\uff0c\u5229\u7528SLIPS\u6765\u9632\u6c61\u57a2\u662f\u6700\u8fd1\u53d1\u5c55\u8d77\u6765\u7684\u4e00\u79cd\u9632\u6c61\u57a2\u65b9\u6cd5\uff0c\u4f46\u662f\u8fd9\u79cd\u65b9\u6cd5\u4e0d\u80fd\u6740\u6b7b\u8868\u9762\u9644\u8fd1\u6eb6\u6db2\u91cc\u7684\u5fae\u751f\u7269\u3002<\/p>\n<p>\u6700\u8fd1\uff0c\u7f8e\u56fd\u5a01\u65af\u5eb7\u661f\u5927\u5b66\u7684Uttam Manna\u7b49\u4eba\u8fdb\u4e00\u6b65\u53d1\u5c55\u4e86SLIPS\uff0c\u4ed6\u4eec\u5148\u5f80\u591a\u5b54\u7684\u805a\u5408\u7269\u591a\u5c42\u819c\u6ce8\u5165\u4e00\u79cd\u6297\u5fae\u751f\u7269\u7684\u836f\u7269\uff08triclosan\uff09\uff0c\u7136\u540e\u518d\u6ce8\u5165\u7845\u916e\u3002\u56e0\u4e3atriclosan\u4e0d\u5f71\u54cd\u7845\u916e\u7684\u6027\u8d28\uff0c\u6240\u4ee5\u8fd9\u79cd\u8868\u9762\u4e0d\u4ec5\u80fd\u591f\u9632\u6c61\u57a2\uff0c\u800c\u4e14\u7531\u4e8etriclosan\u80fd\u7f13\u6162\u91ca\u653e\u5230\u6eb6\u6db2\u4e2d\uff0c\u5b83\u8fd8\u80fd\u6740\u6b7b\u8868\u9762\u9644\u8fd1\u6eb6\u6db2\u7684\u5fae\u751f\u7269\u3002\u7531\u4e8e\u53ef\u4ee5\u7528\u4e0d\u540c\u7684\u6cb9\u548c\u6297\u5fae\u751f\u7269\u836f\u7269\u505a\u6210\u8fd9\u79cd\u8868\u9762\uff0c\u56e0\u6b64\u8fd9\u79cd\u8868\u9762\u6709\u5f88\u5e7f\u6cdb\u7684\u5e94\u7528\u524d\u666f\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adfm.201505522\/full\" target=\"_blank\">Slippery Liquid-Infused Porous Surfaces that Prevent Microbial Surface Fouling and Kill Non-Adherent Pathogens in Surrounding Media: A Controlled Release Approach<\/a><\/p>\n<p><strong>9\u3001Angewandte\uff1a\u786e\u5b9a\u5bf9\u751f\u7269\u5408\u6210\u73ab\u7470\u9ec4\u8272\u7d20\u8d77\u5173\u952e\u4f5c\u7528\u7684\u9176<\/strong><\/p>\n<p>\u7ef4\u751f\u7d20\u7c7b\u4f3c\u7269\u662f\u65b0\u578b\u6297\u751f\u7d20\u7684\u6765\u6e90\uff0c\u73ab\u7470\u9ec4\u8272\u7d20\uff08RoF\uff09\u662f\u7ef4\u751f\u7d20B2\u7684\u7c7b\u4f3c\u7269\uff0c\u4eceB2\u5408\u6210RoF\u7684\u8fc7\u7a0b\u4e2d\u4f1a\u751f\u6210\u51e0\u79cd\u4e2d\u95f4\u4ea7\u7269\uff0cAF\u5c31\u662f\u5176\u4e2d\u7684\u4e00\u79cd\uff0c\u4f46\u662f\u7a76\u7adf\u662f\u4ec0\u4e48\u9176\u53c2\u4e0eAF\u7684\u5408\u6210\u8fd8\u4e0d\u6e05\u695a\u3002<\/p>\n<p>\u6700\u8fd1\u5fb7\u56fd\u7684\u7814\u7a76\u4eba\u5458\u4ece\u53c2\u4e0e\u5b8c\u6574RoF\u5408\u6210\u7684\u57fa\u56e0\u7247\u6bb5\u5165\u624b\uff0c\u786e\u5b9a\u4e86\u67d0\u79cd\u7ec6\u83cc\u4e0a\u7684BN159_7989\u57fa\u56e0\uff08RosB\uff09\u5bf9B2\u8f6c\u6362\u4e3aAF\u8d77\u4e3b\u8981\u4f5c\u7528\u3002RosB\u5728\u5316\u5b66\u5408\u6210\u65b9\u9762\u6709\u5f88\u5927\u7684\u4f5c\u7528\uff0c\u901a\u8fc7\u5bf9RosB\u7684\u6539\u6027\uff0c\u80fd\u4f7f\u591a\u73af\u82b3\u70c3\u4e0a\u7279\u5b9a\u4f4d\u7f6e\u7684\u7532\u57fa\u88ab\u6c28\u57fa\u53d6\u4ee3\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/anie.201600581\/full\" target=\"_blank\">Identification of the Key Enzyme of Roseoflavin Biosynthesis<\/a><\/p>\n<p><strong>10\u3001Nano Letters\uff1a\u538c\u6c27\u7ec6\u83cc\u5728\u80bf\u7624\u6210\u50cf\u548c\u6cbb\u7597\u65b9\u9762\u7684\u5e94\u7528<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12064\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724710.jpg\" alt=\"\u56fe\u724710\" width=\"268\" height=\"415\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724710.jpg 268w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724710-194x300.jpg 194w\" sizes=\"(max-width: 268px) 100vw, 268px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe10 \u5de6\u56fe\u4e3a\u7528\u7b2c\u4e8c\u79cd\u65b9\u6cd5\u6cbb\u7597\u80bf\u7624\u7684\u6548\u679c\uff0c\u53f3\u56fe\u4e3a\u4e00\u822c\u6cbb\u7597\u7684\u6548\u679c<\/p>\n<p>\u80bf\u7624\u662f\u5f53\u4ee3\u5bfc\u81f4\u6b7b\u4ea1\u7684\u4e3b\u8981\u56e0\u7d20\uff0c\u80bf\u7624\u5468\u56f4\u4e00\u822c\u4f1a\u5f62\u6210\u4e00\u4e2a\u7f3a\u6c27\u548c\u4f4ePH\u503c\u7684\u533a\u57df\uff0c\u8fd9\u4e2a\u533a\u57df\u7684\u5b58\u5728\u963b\u788d\u4e86\u80bf\u7624\u7684\u6cbb\u7597\u3002\u4f46\u662f\u8fd9\u79cd\u73af\u5883\u5374\u9002\u5408\u538c\u6c27\u7ec6\u83cc\u7684\u751f\u957f\uff0c\u8fd9\u4e3a\u6cbb\u7597\u764c\u75c7\u63d0\u4f9b\u4e86\u4e00\u4e2a\u65b0\u7684\u601d\u8def\u3002<\/p>\n<p>\u6700\u8fd1\u53f0\u6e7e\u56fd\u7acb\u6210\u529f\u5927\u5b66\u7684Cheng-Hung Luo\u7b49\u4eba\u7814\u7a76\u4e86\u4e24\u79cd\u5229\u7528\u538c\u6c27\u7ec6\u83cc\u6297\u764c\u7684\u65b9\u6cd5\u3002\u7b2c\u4e00\u79cd\u662f\u5c06\u529f\u80fd\u7eb3\u7c73\u7c92\u5b50\uff08\u4e0a\u8f6c\u6362\u6750\u6599\u548c\u91d1\u7eb3\u7c73\u68d2\uff09\u4e0e\u538c\u6c27\u7ec6\u83cc\u7ed3\u5408\u7136\u540e\u6ce8\u5165\u4f53\u5185\uff1b\u7b2c\u4e8c\u79cd\u662f\u5148\u5c06\u538c\u6c27\u7ec6\u83cc\u7684\u5b62\u5b50\u6ce8\u5165\u4f53\u5185\uff0c\u7136\u540e\u518d\u5c06\u4e0e\u6297\u4f53\u7ed3\u5408\u7684\u7eb3\u7c73\u7c92\u5b50\u6ce8\u5165\u4f53\u5185\u3002\u56e0\u4e3a\u538c\u6c27\u7ec6\u83cc\u53ea\u80fd\u5728\u7f3a\u6c27\u7684\u6761\u4ef6\u4e0b\u5b58\u6d3b\uff0c\u6240\u4ee5\u5b83\u4eec\u4f1a\u5728\u80bf\u7624\u5185\u5bcc\u96c6\u3002\u4ed6\u4eec\u5148\u7528\u4e0a\u8f6c\u6362\u6750\u6599\u8bc1\u5b9e\u4e86\u7ec6\u83cc\u4f1a\u5728\u80bf\u7624\u5185\u5bcc\u96c6\uff0c\u7136\u540e\u5229\u7528\u8fd1\u7ea2\u5916\u5149\u7167\u5c04\u91d1\u7eb3\u7c73\u68d2\u4f7f\u5176\u53d1\u70ed\u6740\u6b7b\u764c\u7ec6\u80de\u3002\u603b\u4f53\u4e0a\u6765\u8bf4\uff0c\u7b2c\u4e8c\u79cd\u65b9\u6cd5\u7684\u6548\u679c\u66f4\u597d\u3002\u8fd9\u79cd\u65b9\u6cd5\u6709\u671b\u7528\u6765\u6cbb\u7597\u591a\u79cd\u764c\u7ec6\u80de\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acs.nanolett.6b00262\" target=\"_blank\">Bacteria-mediated hypoxia-specific delivery of nanoparticles for tumors imaging and therapy<\/a><\/p>\n<p><strong>11\u3001Nature Communications\uff1a\u7528\u67d4\u6027\u51dd\u80f6\u7535\u6781\u5236\u5907\u7684\u751f\u7269\u4fe1\u53f7\u653e\u5927\u5668<\/strong><\/p>\n<p style=\"text-align: center;\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12065\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724711.jpg\" alt=\"\u56fe\u724711\" width=\"412\" height=\"283\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724711.jpg 412w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724711-300x206.jpg 300w\" sizes=\"(max-width: 412px) 100vw, 412px\" \/><br \/>\n\u56fe11 \u7531\u78b3\u7eb3\u7c73\u7ba1\u51dd\u80f6\u590d\u5408\u6750\u6599\u548c\u6709\u673a\u6676\u4f53\u7ba1\u7ec4\u6210\u7684\u653e\u5927\u7cfb\u7edf<\/p>\n<p>\u4f53\u5185\u7535\u5b50\u76d1\u63a7\u7cfb\u7edf\u6709\u52a9\u4e8e\u6211\u4eec\u7406\u89e3\u751f\u547d\u4f53\u5185\u7684\u751f\u7269\u6d3b\u52a8\uff0c\u662f\u5f88\u6709\u524d\u9014\u7684\u4e0b\u4e00\u4ee3\u533b\u5b66\u7535\u5b50\u8bbe\u5907\u3002\u4f46\u662f\u76ee\u524d\u4f7f\u7528\u7684\u8bbe\u5907\u5728\u4f53\u5185\u7684\u7a33\u5b9a\u6027\u4e0d\u597d\uff0c\u4e14\u5bf9\u751f\u7269\u4fe1\u53f7\u7684\u7075\u654f\u5ea6\u4e0d\u9ad8\u3002<\/p>\n<p>\u6700\u8fd1\u65e5\u672c\u4e1c\u4eac\u5927\u5b66\u7684Tsuyoshi Sekitani\u7b49\u4eba\u5c06\u591a\u58c1\u78b3\u7eb3\u7c73\u7ba1\u5206\u6563\u5728\u805a\u8f6e\u70f7\u51dd\u80f6\u4e0a\u5236\u5907\u4e86\u4e00\u79cd\u751f\u7269\u76f8\u5bb9\u6027\u826f\u597d\u548c\u5bfc\u7535\u7387\u9ad8\u7684\u51dd\u80f6\u590d\u5408\u6750\u6599\u3002\u8fd9\u79cd\u51dd\u80f6\u590d\u5408\u6750\u6599\u5177\u6709100\u2009mS\u2009cm\u22122\u7684\u5bfc\u7eb3\uff0c\u751a\u81f3\u5728\u4f4e\u9891\u8303\u56f4\u4e5f\u4fdd\u6301\u9ad8\u5bfc\u7eb3\u3002\u5c06\u8fd9\u79cd\u590d\u5408\u6750\u6599\u505a\u6210\u7535\u6781\u6ce8\u5165\u76ae\u4e0b\u7ec4\u7ec74\u5468\u65f6\uff0c\u4ea7\u751f\u7684\u5f02\u7269\u53cd\u5e94\u6bd4\u5e38\u7528\u7684\u7684\u91d1\u5c5e\u7535\u6781\u5c0f\u7684\u591a\u3002\u8fd9\u79cd\u7535\u6781\u80fd\u591f\u5728\u4e0d\u5747\u5300\u7684\u5fc3\u810f\u8868\u9762\u5168\u90e8\u94fa\u5c55\u5f00\u6765\uff0c\u5c06\u5b83\u4e0e\u6709\u673a\u6676\u4f53\u7ba1\u4fe1\u53f7\u653e\u5927\u88c5\u7f6e\u8fde\u63a5\u65f6\uff0c\u53ef\u4ee5\u5c06\u5c0f\u9f20\u5fc3\u810f\u4ea7\u751f\u76841mV\u7535\u4fe1\u53f7\u653e\u5927200\u500d\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/www.nature.com\/ncomms\/2016\/160429\/ncomms11425\/full\/ncomms11425.html\" target=\"_blank\">Ultraflexible organic amplifier with biocompatible gel electrodes<\/a><\/p>\n<p><strong>12\u3001Angewandte:B\u7c7bG-\u86cb\u767d\u5076\u8054\u53d7\u4f53\uff08GPCR\uff09\u7684\u5149\u63a7\u53d8\u6784<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12066\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724712.jpg\" alt=\"\u56fe\u724712\" width=\"500\" height=\"122\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724712.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724712-300x73.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe12 PhotoETP\u7684\u4f5c\u7528\u793a\u610f\u56fe<\/p>\n<p>\u53d8\u6784\u8c03\u8282\u662f\u6307\u5c0f\u5206\u5b50\u5316\u5408\u7269\u4e0e\u9176\u86cb\u767d\u5206\u5b50\u6d3b\u6027\u4e2d\u5fc3\u4ee5\u5916\u7684\u67d0\u4e00\u90e8\u4f4d\u7ed3\u5408\uff0c\u5f15\u8d77\u9176\u86cb\u767d\u5206\u5b50\u6784\u50cf\u53d8\u5316\u4ece\u800c\u6539\u53d8\u9176\u7684\u6d3b\u6027\u3002<\/p>\n<p>\u8fd1\u65e5\u5fb7\u56fd\u79d1\u5b66\u5bb6\u5408\u6210\u4e86\u4e00\u79cd\u6b63\u522b\u6784\u8c03\u8282\u7269\uff08PhotoETP\uff09\uff0c\u8fd9\u79cd\u5316\u5408\u7269\u53ef\u4ee5\u5206\u522b\u7528440\u548c330nm\u7684\u5149\u7167\u5c04\u6765\u5f97\u5230\u987a\u5f0f\uff08cis)\u548c\u53cd\u5f0f(trans)\u6784\u8c61\u3002trans-PhotoETP\u53ef\u4ee5\u901a\u8fc7\u4e0eG-\u86cb\u767d\u5076\u8054\u53d7\u4f53\u7ed3\u5408\u4fc3\u8fdb\u7ec6\u80de\u95f4Ca2+\u7684\u8fd0\u52a8\u548c\u80f0\u5c9b\u7d20\u7684\u5206\u6ccc\uff0c\u800ccis-PhotoETP\u5374\u6ca1\u6709\u8fd9\u4e2a\u4f5c\u7528\uff0c\u5e76\u4e14PhotoETP\u5bf9\u7ec6\u80de\u7684\u5f71\u54cd\u5f88\u5c0f\uff0cPhotoETP\u6709\u52a9\u4e8e\u7406\u89e3\u522b\u6784\u73b0\u8c61\u548cB\u7c7bGPCR\u7684\u4fe1\u53f7\u4f20\u8f93\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/anie.201600957\/full\" target=\"_blank\">Allosteric Optical Control of a Class B G-Protein-Coupled Receptor<\/a><\/p>\n<p><strong>13\u3001Advanced Functional Materials\uff1a\u4eff\u751f\u8d3b\u8d1d\u7684\u6cbb\u7597\u5fc3\u808c\u6897\u585e\u7684\u5fc3\u810f\u8865\u4e01<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12067\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724713.jpg\" alt=\"\u56fe\u724713\" width=\"500\" height=\"187\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724713.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724713-300x112.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe13 \u8865\u4e01\u7684\u663e\u5fae\u7ed3\u6784\uff0c\u53f3\u56fe\u4e2d\u7684\u5c0f\u70b9\u4e3aPpy<\/p>\n<p>\u76ee\u524d\u6cbb\u7597\u5fc3\u808c\u6897\u585e\u7684\u4e3b\u8981\u65b9\u6cd5\u662f\u4fee\u590d\u574f\u6b7b\u7684\u5fc3\u808c\u5c42\uff0c\u4fee\u590d\u7684\u65b9\u6cd5\u662f\u76f4\u63a5\u5c06\u76f8\u5173\u7684\u7ec6\u80de\u6ce8\u5165\u53d7\u635f\u90e8\u4f4d\uff0c\u4f46\u662f\u8fd9\u4e9b\u7ec6\u80de\u4e0d\u80fd\u56fa\u5b9a\u5728\u53d7\u635f\u90e8\u4f4d\uff0c\u5f88\u5bb9\u6613\u8f6c\u79fb\u5230\u5fc3\u5ba4\u8154\u6216\u8005\u8840\u7ba1\u91cc\uff0c\u56e0\u6b64\u6cbb\u7597\u6548\u679c\u4e0d\u660e\u663e\u3002\u4e00\u79cd\u6cbb\u7597\u7684\u65b0\u601d\u8def\u662f\uff1a\u5c06\u5fc3\u808c\u7ec6\u80de\u5438\u9644\u5728\u9ad8\u5206\u5b50\u9aa8\u67b6\uff08\u6709\u7c7b\u4f3c\u5fc3\u808c\u5c42\u7684\u7ed3\u6784\u548c\u529f\u80fd\uff09\u4e0a\u505a\u6210\u8865\u4e01\u201c\u8d34\u5728\u201d\u53d7\u635f\u90e8\u4f4d\uff0c\u4ece\u800c\u4f7f\u5fc3\u810f\u529f\u80fd\u6062\u590d\u3002<\/p>\n<p>\u6700\u8fd1\u5357\u65b9\u533b\u79d1\u5927\u5b66\u7684Leyu Wang\u7b49\u5229\u7528\u4ece\u8d3b\u8d1d\u817f\u4e2d\u63d0\u53d6\u51fa\u6765\u7684\u7c98\u6027\u5f88\u5f3a\u7684\u86cb\u767d\u8d28\u5236\u5907\u4e86\u4e00\u79cd\u591a\u5df4\u80fa\uff0c\u5c06\u8fd9\u79cd\u591a\u5df4\u80fa\u548c\u4e00\u4e9b\u52a9\u5242\u5236\u6210\u9ad8\u5206\u5b50\u9aa8\u67b6\uff0c\u518d\u52a0\u5165\u5fc3\u808c\u7ec6\u80de\u5f97\u5230\u5fc3\u810f\u8865\u4e01\u3002\u8fd9\u79cd\u8865\u4e01\u6709\u5bfc\u7535\u6027\u3001\u826f\u597d\u7684\u751f\u7269\u76f8\u5bb9\u6027\u3001\u4e0e\u5fc3\u808c\u5c42\u76f8\u4f3c\u7684\u6768\u6c0f\u6a21\u91cf\uff0c\u8865\u4e01\u91cc\u9762\u7684Ppy\u52a9\u5242\u8fd8\u80fd\u878d\u5165\u5fc3\u808c\u7ec6\u80de\u4e2d\u4fc3\u8fdb\u67d0\u4e9b\u86cb\u767d\u7684\u4ea7\u751f\u3002\u5c06\u8fd9\u79cd\u8865\u4e01\u8d34\u5230\u5c0f\u9f20\u5fc3\u808c\u6897\u585e\u7684\u90e8\u4f4d\uff0c\u53d7\u635f\u7684\u90e8\u4f4d\u53d8\u5c0f\u4e86\uff0c\u4e14\u5fc3\u810f\u7684\u529f\u80fd\u5f97\u5230\u6539\u5584\u3002\u8fd9\u79cd\u591a\u5df4\u80fa\u5f88\u6709\u5e0c\u671b\u4f5c\u4e3a\u4fee\u590d\u6897\u585e\u7ec4\u7ec7\u7684\u9aa8\u67b6\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adfm.201505372\/full\" target=\"_blank\">Mussel-Inspired Conductive Cryogel as Cardiac Tissue Patch to Repair Myocardial Infarction by Migration of Conductive Nanoparticles<\/a><\/p>\n<p><strong>14\u3001Advanced Functional Materials\uff1a\u6cbb\u7597\u5916\u4f24\u6027\u8111\u635f\u4f24\u7684\u6c27\u53cd\u5e94\u6027\u805a\u5408\u7269<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12068\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724714.jpg\" alt=\"\u56fe\u724714\" width=\"500\" height=\"104\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724714.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724714-300x62.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe14 ORP\u7684\u5408\u6210\u65b9\u6cd5\u548c\u7ed3\u6784<\/p>\n<p>\u5916\u4f24\u6027\u8111\u635f\u4f24\u662f\u7531\u8111\u90e8\u53d7\u5230\u5916\u529b\u9020\u6210\u7684\uff0c\u5916\u529b\u76f4\u63a5\u5bfc\u81f4\u795e\u7ecf\u5143\u53d7\u635f\uff0c\u8fc7\u4e00\u6bb5\u65f6\u95f4\u540e\uff0c\u6d3b\u6027\u6c27\u7c07\uff08ROS\uff09\u5728\u53d7\u635f\u90e8\u4f4d\u805a\u96c6\uff0c\u9020\u6210\u7ee7\u53d1\u6027\u8111\u635f\u4f24\u3002\u6cbb\u7597\u7ee7\u53d1\u6027\u8111\u635f\u4f24\u7684\u4e3b\u8981\u65b9\u6cd5\u662f\u6e05\u9664ROS\u3002<\/p>\n<p>\u6700\u8fd1\u7f8e\u56fd\u534e\u76db\u987f\u5927\u5b66\u7684Julia Xu\u7b49\u4eba\u5236\u5907\u4e86\u4e00\u79cd\u5305\u62ec\u6cbb\u7597\u548c\u6210\u50cf\u529f\u80fd\u7684\u7eb3\u7c73\u6c27\u53cd\u5e94\u6027\u805a\u5408\u7269\uff08ORP\uff09\u3002\u8fd9\u79cd\u805a\u5408\u7269\u91cc\u9762\u5305\u542b\u7518\u9187\uff08\u63d0\u9ad8\u751f\u7269\u76f8\u5bb9\u6027\u548c\u5faa\u73af\u5bff\u547d\uff09\u3001Gd\uff08\u63d0\u4f9b\u6210\u50cf\u886c\u5ea6\uff09\u548c\u786b\u919a\uff08\u6e05\u9664ROS\uff09\uff0c\u5c06ORP\u6ce8\u5165\u4f53\u5185\u540e\uff0c\u5b83\u4eec\u5728\u8111\u635f\u4f24\u90e8\u4f4d\u5bcc\u96c6\u3002ORP\u80fd\u6709\u6548\u7684\u51cf\u5c11\u53d7\u635f\u90e8\u4f4d\u53ca\u9644\u8fd1\u7684ROS\uff0c\u4ece\u800c\u51cf\u7f13\u7ee7\u53d1\u6027\u8111\u635f\u4f24\u5f15\u8d77\u7684\u795e\u7ecf\u5143\u53d8\u6027\u3002ORP\u6709\u671b\u7528\u6765\u63d0\u9ad8\u8111\u635f\u4f24\u7684\u6cbb\u7597\u6548\u679c\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adfm.201504416\/full\" target=\"_blank\">Theranostic Oxygen Reactive Polymers for Treatment of Traumatic Brain Injury<\/a><\/p>\n<p><strong>15\u3001PNAS\uff1a\u79bb\u5b50\u5728\u80f6\u4f53\u6676\u4f53\u81ea\u6108\u884c\u4e3a\u4e2d\u7684\u4f5c\u7528<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-12069\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724715.jpg\" alt=\"\u56fe\u724715\" width=\"500\" height=\"237\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724715.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724715-300x142.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p style=\"text-align: left;\">\u56fe15 \u80f6\u4f53\u7c92\u5b50\u7684\u7ed3\u6784\u793a\u610f\u56fe\u3002\u84dd\u8272\u7684\u4e3a\u80f6\u4f53\u7c92\u5b50\uff0c\u5916\u9762\u7ea2\u8272\u7684\u4e3a\u88ab\u675f\u7f1a\u7684\u53cd\u79bb\u5b50\u5c42\uff0c\u5c0f\u7ea2\u70b9\u4e3a\u6e38\u79bb\u7684\u53cd\u79bb\u5b50<\/p>\n<p>\u6742\u8d28\u7ecf\u5e38\u5728\u6676\u4f53\u4e2d\u5f62\u6210\u70b9\u7f3a\u9677\u751a\u81f3\u963b\u788d\u7ed3\u6676\uff0c\u4f46\u662f\u5bf9\u80f6\u4f53\u6676\u4f53\u6765\u8bf4\u5374\u4e0d\u662f\u8fd9\u6837\u3002\u80f6\u4f53\u6676\u4f53\u662f\u6307\u76f4\u5f84\u548c\u5916\u5f62\u76f8\u540c\u7684\u6216\u79f0\u5177\u6709\u5355\u5206\u6563\u5ea6\u7684\u7403\u5f62\u80f6\u4f53\u9897\u7c92\uff08\u76f4\u5f84\u4e00\u822c\u5728100nm\u52301000nm\uff09\u5728\u6c34\u8fd9\u7c7b\u6db2\u4f53\u4e2d\u6309\u7c7b\u4f3c\u4e8e\u539f\u5b50\u6676\u4f53\u7ed3\u6784\u6392\u5217\u65b9\u5f0f\u6392\u5217\u800c\u6210\u7684\u4e00\u79cd\u6676\u4f53\u3002\u5728\u4e00\u5b9a\u6761\u4ef6\u4e0b\uff0c\u5982\u679c\u76f4\u5f84\u4e0d\u540c\u7684\u80f6\u4f53\u7c92\u5b50\u6df7\u5408\uff0c\u76f4\u5f84\u5927\u7684\u7c92\u5b50\u4f1a\u6536\u7f29\u4ece\u800c\u4e0e\u5c0f\u7684\u7c92\u5b50\u4e00\u8d77\u7ed3\u6676\uff08\u8fd9\u5c31\u662f\u6240\u8c13\u7684\u201c\u81ea\u6108\u201d\u5427\uff09\u3002<\/p>\n<p>\u6700\u8fd1\u745e\u58eb\u79d1\u5b66\u5bb6Andrea Scotti\u7b49\u4eba\u901a\u8fc7\u5b9e\u9a8c\u63d0\u51fa\u4e86\u5927\u9897\u7c92\u6536\u7f29\u7684\u673a\u7406\u3002\u4ed6\u4eec\u7528\u805aN-\u5f02\u4e19\u57fa\u4e19\u70ef\u9170\u80fa\uff08pNIPAM\uff09\u5236\u5907\u4e86\u4e24\u79cd\u534a\u5f84\u4e0d\u540c\u7684\u7c92\u5b50\uff08\u5206\u522b\u4e3a180\u548c135nm\uff09\uff0c\u5c06\u8fd9\u4e9b\u7c92\u5b50\u7ecf\u8fc7\u5145\u5206\u6eb6\u80c0\uff0c\u5355\u72ec\u6216\u6309\u4e0d\u540c\u6bd4\u4f8b\u6df7\u5408\u60ac\u6d6e\u5728\u6eb6\u6db2\u4e2d\u3002\u7ecf\u8fc7\u4e00\u7cfb\u5217\u5b9e\u9a8c\uff0c\u4ed6\u4eec\u63d0\u51fa\u4e86\u4e0b\u9762\u7684\u673a\u7406\u6765\u89e3\u91ca\u5927\u9897\u7c92\u6536\u7f29\u7684\u73b0\u8c61\uff1apNIPAM\u8868\u9762\u6709\u53ef\u4ee5\u7535\u79bb\u7684\u5b98\u80fd\u56e2\uff0c\u7535\u79bb\u51fa\u6765\u7684\u53cd\u79bb\u5b50\u88ab\u675f\u7f1a\u5728\u9897\u7c92\u7684\u5916\u8868\u9762\uff0c\u56e0\u4e3a\u8868\u9762\u5185\u5916\u7684\u7c92\u5b50\u6d53\u5ea6\u4e0d\u540c\uff0c\u5bf9\u9897\u7c92\u4ea7\u751f\u6e17\u900f\u538b\uff0c\u5f53\u6e17\u900f\u538b\u5927\u4e8e\u9897\u7c92\u7684\u6768\u6c0f\u6a21\u91cf\u65f6\u9897\u7c92\u5c31\u4f1a\u6536\u7f29\u3002\u5f53\u9897\u7c92\u7684\u6d53\u5ea6\u5927\u4e8e\u4e00\u5b9a\u503c\u65f6\uff0c\u9897\u7c92\u4f1a\u76f8\u4e92\u9760\u8fd1\uff0c\u4f7f\u5f97\u53cd\u79bb\u5b50\u7684\u6d53\u5ea6\u589e\u52a0\uff0c\u4f1a\u8fdb\u4e00\u6b65\u538b\u7f29\u9897\u7c92\uff0c\u4f46\u662f\u7531\u4e8e\u5927\u9897\u7c92\u7684\u6768\u6c0f\u6a21\u91cf\u66f4\u5c0f\uff0c\u56e0\u6b64\u538b\u7f29\u7684\u66f4\u4e3a\u660e\u663e\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/www.pnas.org\/content\/early\/2016\/04\/27\/1516011113.abstract\" target=\"_blank\">The role of ions in the self-healing behavior of soft particle suspensions<\/a><\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u751f\u7269\u6750\u6599\u5b66\u4e60\u5c0f\u7ec4CZM\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n<p>\u6b22\u8fce\u52a0\u5165\u6750\u6599\u4eba\u751f\u7269\u6750\u6599\u5b66\u4e60\u5c0f\u7ec4\uff0c\u4e00\u8d77\u63a2\u8ba8\u751f\u7269\u6750\u6599\u7684\u4e13\u4e1a\u95ee\u9898\uff0c\u5173\u6ce8\u751f\u7269\u6750\u6599\u7684\u6700\u65b0\u52a8\u6001\u3002\u52a0\u5165\u65b9\u5f0f\uff1a\u6dfb\u52a0\u6750\u6599\u4eba\u751f\u7269\u6750\u6599\u4ea4\u6d41\u7fa4\uff08124806506\uff09\uff0c\u79c1\u4fe1\u7ba1\u7406\u5458\u201c\u9648\u662d\u94ed\uff08QQ\uff1a1982342885\uff09\u201d\u62a5\u540d\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>1\u3001Nature Nanotechnology\uff1a\u9ad8\u901f\u539f\u5b50\u529b\u663e\u5fae\u955c\u6709\u52a9\u4e8e\u7406\u89e3\u6838\u5b54\u590d\u5408\u4f53\u8fd0\u8f93\u673a\u7406 \u56fe1 \u6838\u5b54\u5bf9\u5927\u5206\u5b50\u7269\u8d28\u7684\u9009\u62e9\u6027\u8fd0\u8f93\u673a\u7406 \u6838\u5b54\u590d\u5408\u4f53\uff08NPCs\uff09\u63a7\u5236&#8230;<\/p>\n","protected":false},"author":382,"featured_media":12059,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[67],"tags":[75,33],"class_list":["post-12053","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-zhoubao","tag-biomaterial","tag-nano"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/12053"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/382"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=12053"}],"version-history":[{"count":10,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/12053\/revisions"}],"predecessor-version":[{"id":12133,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/12053\/revisions\/12133"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/12059"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=12053"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=12053"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=12053"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}