{"id":121764,"date":"2018-01-17T06:30:16","date_gmt":"2018-01-16T22:30:16","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=121764"},"modified":"2018-02-12T17:47:59","modified_gmt":"2018-02-12T09:47:59","slug":"%e4%b8%ad%e7%a7%91%e9%99%a2%e9%87%91%e5%b1%9e%e6%89%80%e9%99%88%e7%a7%8b%e6%98%9f%e4%b8%a8sci-china-mater-%e6%8b%93%e6%89%91%e9%87%8f%e5%ad%90%e5%82%ac%e5%8c%96%ef%bc%9a%e6%8b%93%e6%89%91%e7%8b%84","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=121764","title":{"rendered":"\u4e2d\u79d1\u9662\u91d1\u5c5e\u6240\u9648\u661f\u79cb\u4e28Sci. China Mater.\uff1a\u62d3\u6251\u91cf\u5b50\u50ac\u5316\uff1a\u62d3\u6251\u72c4\u62c9\u514b\u8282\u7ebf\u534a\u91d1\u5c5e\u7684\u6f5c\u5728\u6790\u6c22\u50ac\u5316\u529f\u80fd"},"content":{"rendered":"<p>\u4e2d\u56fd\u79d1\u5b66\u9662\u91d1\u5c5e\u7814\u7a76\u6240\u6c88\u9633\u6750\u6599\u79d1\u5b66\u56fd\u5bb6\u7814\u7a76\u4e2d\u5fc3<strong>\u9648\u661f\u79cb\u7814\u7a76\u56e2\u961f<\/strong>\u5229\u7528\u8282\u7ebf\u534a\u91d1\u5c5e\u4ea7\u751f\u7684\u9f13\u819c\u72b6\u8868\u9762\u6001\u4f5c\u4e3a\u6790\u6c22\u53cd\u5e94\u7684\u50ac\u5316\u5e73\u53f0\uff0c\u63d0\u51fa\u4e86\u62d3\u6251\u91cf\u5b50\u50ac\u5316\u7684\u65b0\u6982\u5ff5\uff0c\u5e76\u5efa\u8baeTiSi\u5bb6\u65cf\u6750\u6599\u4f5c\u4e3a\u8fd9\u79cd\u50ac\u5316\u5242\u7684\u6f5c\u5728\u5019\u9009\u8303\u672c\u3002\u8fd9\u4e00\u65b0\u6982\u5ff5\u5bf9\u4e8e\u65b0\u578b\u50ac\u5316\u6750\u6599\u7684\u8bbe\u8ba1\u5177\u6709\u6307\u5bfc\u610f\u4e49\u3002\u8be5\u6210\u679c\u5728<strong>Science China Materials <\/strong>2018\u5e74\u7b2c1\u671f\u4f5c\u4e3a\u5c01\u9762\u6587\u7ae0\u62a5\u9053\u3002<\/p>\n<p><span style=\"color: #ff0000\"><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/span><\/p>\n<p>\u5728\u51dd\u805a\u6001\u7269\u7406\u548c\u6750\u6599\u79d1\u5b66\u7684\u524d\u6cbf\u9886\u57df\u4e2d\uff0c\u62d3\u6251\u72c4\u62c9\u514b\u8282\u7ebf\u534a\u91d1\u5c5e\u56e0\u5176\u72ec\u7279\u7684\u62d3\u6251\u80fd\u5e26\u7ed3\u6784\u5438\u5f15\u4e86\u79d1\u7814\u4eba\u5458\u7684\u5e7f\u6cdb\u5173\u6ce8\u3002\u62d3\u6251\u8282\u7ebf\u534a\u91d1\u5c5e\u5177\u6709\u4f53\u6001\u80fd\u5e26\u53cd\u8f6c\u5bfc\u81f4\u7684\u7a33\u5b9a\u95ed\u5408\u73af\u72b6\u72c4\u62c9\u514b\u8282\u7ebf\uff0c\u5b83\u6295\u5f71\u5230\u67d0\u4e9b\u6750\u6599\u7684\u8868\u9762\u4f1a\u5f62\u6210\u95ed\u5408\u7684\u5708\uff0c\u5708\u5185\u5219\u8868\u73b0\u51fa\u53d7\u62d3\u6251\u4fdd\u62a4\u7684\u80fd\u91cf\u8272\u6563\u975e\u5e38\u5c0f\u7684\u9f13\u819c\u72b6\u62d3\u6251\u8868\u9762\u6001\uff0c\u4ece\u800c\u4f7f\u8868\u9762\u5904\u7684\u8d39\u7c73\u80fd\u7ea7\u5177\u6709\u6781\u9ad8\u7684\u7535\u5b50\u6001\u5bc6\u5ea6\u3002\u76ee\u524d\uff0c\u50ac\u5316\u6d3b\u6027\u4f4d\u7f6e\u7684\u8bbe\u8ba1\u4e00\u822c\u9700\u8981\u6ee1\u8db3\u5728\u8d39\u7c73\u80fd\u7ea7\u5904\u5177\u6709\u8f83\u9ad8\u7684\u7535\u5b50\u6001\u5bc6\u5ea6\u3001\u9ad8\u8f7d\u6d41\u5b50\u8f93\u8fd0\u901f\u7387\u548c\u9002\u5f53\u7684\u70ed\u529b\u5b66\u7a33\u5b9a\u6027\u3002\u7406\u8bba\u4e0a\uff0c\u7531\u4e8e\u4e0d\u6613\u88ab\u7834\u574f\u7684\u9f13\u819c\u72b6\u62d3\u6251\u8868\u9762\u6001\u7684\u5b58\u5728\uff0c\u62d3\u6251\u8282\u7ebf\uff08\u534a\uff09\u91d1\u5c5e\u5929\u7136\u878d\u5408\u4e86\u8d39\u7c73\u80fd\u7ea7\u9ad8\u7684\u7535\u5b50\u6001\u5bc6\u5ea6\u548c\u9ad8\u8f7d\u6d41\u5b50\u8f93\u8fd0\u901f\u7387\u4f18\u52bf\uff0c\u53ef\u4e3a\u5176\u4f5c\u4e3a\u6f5c\u5728\u7684\u9ad8\u6548\u50ac\u5316\u5e73\u53f0\u63d0\u4f9b\u575a\u5b9e\u57fa\u7840\u3002<\/p>\n<p>\u57fa\u4e8e\u8fd9\u4e00\u8bbe\u60f3\uff0c\u6700\u8fd1\u4e2d\u79d1\u9662\u91d1\u5c5e\u6240\u9648\u661f\u79cb\u7814\u7a76\u56e2\u961f\u63d0\u51fa\u4e86\u62d3\u6251\u91cf\u5b50\u50ac\u5316\u7684\u65b0\u6982\u5ff5\uff0c\u5373\u4e3b\u8981\u5229\u7528\u56fa\u4f53\u62d3\u6251\u6750\u6599\u7684\u8868\u9762\u6001\u4f5c\u4e3a\u50ac\u5316\u6d3b\u6027\u5e73\u53f0\u3002\u57fa\u4e8e\u7b2c\u4e00\u6027\u539f\u7406\u8ba1\u7b97\u548c\u6a21\u578b\u5206\u6790\uff0c\u4ed6\u4eec\u5efa\u8bae\u62d3\u6251\u8282\u7ebf\u534a\u91d1\u5c5eTiSi\u65b0\u578b\u5bb6\u65cf\u6750\u6599\u53ef\u4f5c\u4e3a\u6f5c\u5728\u7535\u5316\u5b66\u6790\u6c22\u50ac\u5316\u5e73\u53f0\u3002\u8ba1\u7b97\u7ed3\u679c\u8868\u660e\u5728\u81ea\u65cb-\u8f68\u9053\u8026\u5408\u6548\u5e94\u8f83\u5f31\u7684TiSi\u91d1\u5c5e\u95f4\u5316\u5408\u7269\u4e2d\uff0c\u7531\u4e8eTi\u7684<em>d<\/em><sub>yz<\/sub>\u548c<em>d<\/em><sub>z<\/sub><sup>2<\/sup>\u8f68\u9053\u80fd\u5e26\u53cd\u8f6c\u800c\u5bfc\u81f4\u5728\u5e03\u91cc\u6e0a\u533a\u5185\u7684<em>k<\/em><sub>y<\/sub>=0\u5e73\u9762\u5185\u5f62\u6210\u4e86\u95ed\u5408\u7684\u72c4\u62c9\u514b\u8282\u7ebf\u73af\uff0c\u7528\u7d27\u675f\u7f1a\u6a21\u578b\u5206\u6790\u4e86<em>k<\/em><sub>y<\/sub>=0\u548c<em>k<\/em><sub>y<\/sub>=\u03c0\u4e24\u4e2a\u9762\u7684\u74e6\u5c3c\u5c14\u4e2d\u5fc3\u7684\u6f14\u5316\uff0c\u786e\u5b9a\u4e86\u8be5\u72c4\u62c9\u514b\u8282\u7ebf\u73af\u7684\u62d3\u6251\u975e\u5e73\u5eb8\u7684\u6027\u8d28\u3002\u5728\u4e0e<em>k<\/em><sub>y<\/sub>=0\u5e73\u9762\u5e73\u884c\u7684\uff08010\uff09\u8868\u9762\u51fa\u73b0\u4e86\u4e8c\u91cd\u7b80\u5e76\u7684\u975e\u5e73\u5eb8\u62d3\u6251\u8868\u9762\u6001\uff0c\u8be5\u8868\u9762\u6001\u7a7f\u8fc7\u8d39\u7c73\u80fd\u7ea7\uff0c\u5bfc\u81f4\uff08010\uff09\u8868\u9762\u51fa\u73b0\u4e86\u9ad8\u7684\u7535\u5b50\u6001\u5bc6\u5ea6\u3002\u6c22\u5438\u9644\u8fc7\u7a0b\u8ba1\u7b97\u8868\u660e\uff08010\uff09\u8868\u9762\u6c22\u5438\u9644\u81ea\u7531\u80fd\u25b3<em>G<\/em>\u51e0\u4e4e\u6070\u597d\u4e3a0\uff0c\u8868\u660e\u6c22\u65e2\u4e0d\u90a3\u4e48\u5f3a\u4e5f\u4e0d\u90a3\u4e48\u5f31\u5730\u88ab\uff08010\uff09\u8868\u9762\u5438\u9644\u3002\u56e0\u6b64\uff0c\u8be5\uff08010\uff09\u8868\u9762\u65e2\u6709\u5229\u4e8e\u6c22\u79bb\u5b50\u5f97\u5230\u7535\u5b50\u88ab\u8fd8\u539f\uff0c\u53c8\u6709\u5229\u4e8e\u6c22\u6c14\u7684\u6790\u51fa\u3002\u540c\u65f6\uff0c\u62d3\u6251\u7535\u8377\u4e5f\u88ab\u63ed\u793a\u53c2\u4e0e\u4e86\u6790\u6c22\u53cd\u5e94\u8fc7\u7a0b\u3002<\/p>\n<p>\u6839\u636e\u8fd9\u4e2a\u601d\u8def\uff0c\u4ed6\u4eec\u63d0\u51fa\u4e86TiSi\u5bb6\u65cf\u6750\u6599\u4e0d\u4ec5\u6709\u5e0c\u671b\u6210\u4e3a\u6790\u6c22\u53cd\u5e94\u7684\u50ac\u5316\u5242\uff0c\u66f4\u91cd\u8981\u7684\u662f\u5b83\u6307\u660e\u5229\u7528\u56fa\u4f53\u6750\u6599\u7684\u62d3\u6251\u8868\u9762\u6001\u8bbe\u8ba1\u65b0\u578b\u50ac\u5316\u5242\u7684\u65b0\u8def\u7ebf\u2014\u2014\u62d3\u6251\u91cf\u5b50\u50ac\u5316\u3002\u8fd9\u4e00\u5229\u7528\u62d3\u6251\u8282\u7ebf\u6750\u6599\u975e\u5e73\u5eb8\u8868\u9762\u6001\u4f5c\u4e3a\u50ac\u5316\u6d3b\u6027\u4f4d\u7f6e\u7684\u601d\u8def\u4e0e\u4ee5\u5f80\u5229\u7528\u7eb3\u7c73\u3001\u6784\u7b51\u3001\u7f3a\u9677\u3001\u6676\u754c\u7b49\u8c03\u63a7\u8bbe\u8ba1\u50ac\u5316\u5242\u5177\u6709\u672c\u8d28\u4e0d\u540c\u3002<\/p>\n<p>\u8be5\u7814\u7a76\u5f97\u5230\u4e86\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u548c\u56fd\u5bb6\u6770\u51fa\u9752\u5e74\u57fa\u91d1\u7684\u8d44\u52a9\u3002<\/p>\n<p><span style=\"color: #ff0000\"><strong>\u3010\u56fe\u6587\u8be6\u89e3\u3011<\/strong><\/span><\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-121812\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/1-17.png\" alt=\"\" width=\"600\" height=\"317\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/1-17.png 716w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/1-17-300x158.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p><strong>\u56fe1.\u00a0<\/strong>\u62d3\u6251\u5916\u5c14\u534a\u91d1\u5c5e(TWs)\u548c\u72c4\u62c9\u514b\u8282\u7ebf\u534a\u91d1\u5c5e\uff08DNLs\uff09\u5728\u52a8\u91cf\u7a7a\u95f4\u4e2d\u7684\u793a\u610f\u56fe\u53ca\u5176\u6001\u5bc6\u5ea6\uff08DOSs\uff09\u56fe\u3002\uff08a\uff09\u6750\u6599\u4f53\u5185\u7684\u4e00\u5bf9Weyl\u8282\u70b9\uff08\u5de6\u4e0b\u56fe\uff09\u548c\u5176\u8868\u9762\u5f62\u6210\u7684\u8d39\u7c73\u5f27\u8868\u9762\u6001\uff08\u5de6\u4e0a\u56fe\uff09\u53ca\u5b83\u4eec\u76f8\u5e94\u7684\u6001\u5bc6\u5ea6\u56fe\uff08\u53f3\u56fe\uff09\uff1b\uff08b\uff09\u6750\u6599\u4f53\u5185\u7684DNL\uff08\u5de6\u4e0b\u56fe\uff09\u4ee5\u53ca\u8868\u9762\u4e0a\u51e0\u4e4e\u5e73\u5766\u7684\u9f13\u819c\u72b6\u7684\u975e\u5e73\u5eb8\u8868\u9762\u6001\uff08\u5de6\u4e0a\u56fe\uff09\u548c\u5b83\u4eec\u5bf9\u5e94\u7684\u6001\u5bc6\u5ea6\u56fe\uff08\u53f3\u56fe\uff09\u3002<\/p>\n<p>&nbsp;<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-121813 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/2-14.png\" alt=\"\" width=\"596\" height=\"499\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/2-14.png 596w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/2-14-300x251.png 300w\" sizes=\"(max-width: 596px) 100vw, 596px\" \/><\/p>\n<p><strong>\u56fe2. <\/strong>TiSi\u7684\u6676\u4f53\u7ed3\u6784\uff0c\u5e03\u91cc\u6e0a\u533a\uff08BZ\uff09\u548c\u58f0\u5b50\u8c31\u3002\uff08a\uff09\u5177\u6709<em>Pnma<\/em>\u7a7a\u95f4\u7fa4\u7684\u659c\u65b9\u6676\u683c\uff0c\uff08b\uff09\u6676\u683c\u7684\u5e03\u91cc\u6e0a\u533a\uff08BZ\uff09\u548c\u9ad8\u5bf9\u79f0k\u70b9\uff0c\u9634\u5f71\u533a\u57df\u8868\u793a\u72c4\u62c9\u514b\u8282\u7ebf\u5728k<sub>y<\/sub> = 0\u5e73\u9762\u7684\u76f8\u5e94\u4f4d\u7f6e\uff0c\uff08c\uff09DFT\u8ba1\u7b97\u5f97\u5230\u7684\u58f0\u5b50\u8c31\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-121814\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/3-11.png\" alt=\"\" width=\"450\" height=\"622\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/3-11.png 534w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/3-11-217x300.png 217w\" sizes=\"(max-width: 450px) 100vw, 450px\" \/><\/p>\n<p><strong>\u56fe3.<\/strong> TiSi\u7684\u7535\u5b50\u80fd\u5e26\u7ed3\u6784\u548cWannier\u4e2d\u5fc3\u7684\u6f14\u5316\u3002\uff08a\uff09\u6ca1\u6709\u5305\u542b\u81ea\u65cb\u8f68\u9053\u8026\u5408\uff08SOC\uff09\u7684\u7535\u5b50\u80fd\u5e26\u7ed3\u6784\u3002\u5728\uff08a\uff09\u4e2d\uff0c\u7a7a\u5fc3\u5706\u8868\u793aTi\u539f\u5b50\u00a0d<sub>yz<\/sub>\u6001\u7684\u6743\u91cd\uff0c\u5b9e\u5fc3\u65b9\u5757\u8868\u793aTi \u539f\u5b50d<sub>z<\/sub><sup>2<\/sup>\u6001\u7684\u6743\u91cd\uff0c\uff08b\uff0cc\uff09\u8868\u793aWannier\u4e2d\u5fc3\u6cbf\u7740k<sub>x<\/sub>\u65b9\u5411\u7684\u6f14\u5316\u3002\u6f14\u5316\u7ebf\u5206\u522b\u5728k<sub>y<\/sub> = 0\u548ck<sub>y<\/sub> = \u03c0\u5e73\u9762\u4e0a\u4e0e\u53c2\u8003\u7ebf\uff08\u7ea2\u8272\u865a\u7ebf\uff09\u76f8\u4ea4\u5947\u6570\u548c\u5076\u6570\u6b21\u3002k<sub>y<\/sub>\u548ck<sub>x<\/sub>\u4e3a\u56fe2b\u6240\u793a\u7684\u65b9\u5411\u3002\uff08d-f\uff09TiSi\uff0cTiGe\u548cTiSn\u7684k<sub>y<\/sub> = 0\u5e73\u9762\u7684\u72c4\u62c9\u514b\u8282\u7ebf\u793a\u610f\u56fe\u3002\u4e0a\u56fe\u548c\u4e0b\u56fe\u5206\u522b\u8868\u793a\u5b83\u4eec\u7684\u4e09\u7ef4\u53ef\u89c6\u5316\u56fe\u548c\u5b83\u4eec\u5728\uff08010\uff09\u5e73\u9762\u4e0a\u5bf9\u5e94\u7684\u4e8c\u7ef4\u6295\u5f71\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-121815 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/4-13.png\" alt=\"\" width=\"526\" height=\"394\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/4-13.png 526w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/4-13-300x225.png 300w\" sizes=\"(max-width: 526px) 100vw, 526px\" \/><\/p>\n<p><strong>\u56fe4.\u00a0<\/strong>\uff08a\uff0cb\uff0950\u4e2a\u539f\u5b50\u5c42\u7684\uff08010\uff09-I\u8868\u9762\u53ca\u5176\u5438\u9644\u6c22\u540e\u7684\u8868\u9762\u7535\u5b50\u7ed3\u6784\u3002\u62d3\u6251\u4fdd\u62a4\u7684\u8868\u9762\u6001\u6807\u8bb0\u4e3a\u56f4\u7ed5\u0393\u7684SF-band1\uff0c\u5e73\u5eb8\u7684\u8868\u9762\u5e26\u6807\u8bb0\u4e3a\u6cbf\u7740\u0393-X\u7684SF-band2\u3002\uff08c\uff09TiSi\u4f53\u76f8\u548c\uff08010\uff09\u8868\u9762\u9876\u5c42\u539f\u5b50\u4e4b\u95f4\u6001\u5bc6\u5ea6\uff08DOSs\uff09\u7684\u6bd4\u8f83\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-121816\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/5-11.png\" alt=\"\" width=\"600\" height=\"400\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/5-11.png 978w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/5-11-300x200.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/5-11-768x512.png 768w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u56fe5.\u00a0<\/strong>\u62d3\u6251DNLs\u5bf9TiSi\u7684HER\u50ac\u5316\u6d3b\u6027\u7684\u5f71\u54cd\u3002\uff08a\uff09DNL\u8bf1\u5bfc\u7684\u8868\u9762\u6001\u63d0\u4f9bHER\u53cd\u5e94\u6d3b\u6027\u5e73\u9762\u7684\u793a\u610f\u56fe\u3002\uff08b\uff09\uff08010\uff09-I\u8868\u9762\u62d3\u6251\u6001\u7684\u53ef\u89c6\u5316\u5c40\u90e8\u7535\u8377\u3002\u7535\u8377\u5177\u6709\u6700\u4e0a\u9762Ti\u539f\u5b50\u7684\u7c7b\u4f3cd<sub>yz<\/sub>\u8f68\u9053\u7684\u7279\u5f81\u3002\uff08c\uff0cd\uff09\u5728\uff08010\uff09-I\u8868\u9762\u53ef\u89c6\u5316\u7684H\u539f\u5b50\u5c40\u90e8\u7535\u8377\u805a\u96c6\u548cTi\u539f\u5b50\u5468\u56f4\u7535\u8377\u7684\u6d88\u8017\u3002\uff08e\uff09\u5728\u6807\u51c6\u6761\u4ef6\u4e0b\uff08pH = 0\uff09\uff0c\u7535\u6781\u53cd\u5e94\u5e73\u8861\uff08U = 0\uff09\u65f6\u8ba1\u7b97\u5f97\u5230\u7684\u6790\u6c22\u81ea\u7531\u80fd\u56fe\u3002\u5728\u6807\u51c6\u6761\u4ef6\u4e0b\u5e73\u8861\u65f6\uff0cH <sup>+<\/sup> + e <sup>&#8211;<\/sup> \u7684\u81ea\u7531\u80fd\u4e0e1\/2 H <sub>2<\/sub>\u76f8\u540c\uff08\u65b9\u6cd5\u00a0[62]\uff09\u3002\u5176\u4e2dMoS<sub>2<\/sub>\uff08\u8fb9\u7f18\u72b6\u6001-0.08 eV\uff09\u548cPt\uff08-0.09 eV\uff09\u7684\u6570\u636e\u6765\u81ea\u53c2\u8003\u6587\u732e [52]\u3002\uff08f\uff09\u5728\u706b\u5c71\u56fe\u4e2d\uff0cTiSi\u7684HER\u884c\u4e3a\u4e0e\u5404\u79cd\u7eaf\u91d1\u5c5e\uff08Pt\uff0cPd\uff0cNi\uff0cIr\uff0cCo\uff0cRh\uff0cAg\uff0cCu\uff0cMo\u548cW\u7684\u5b9e\u9a8c\u6570\u636e\u00a0[61]\uff09\uff0cTWs\uff08NbP\uff0cTaP\uff0cNbAs\u548cTaAs\u7684\u8ba1\u7b97\u6570\u636e\uff09\u4ee5\u53ca\u5176\u4ed6\u5019\u9009\u7269\uff08TaS<sub>2<\/sub>\uff082H\uff09\uff0cMoTe<sub>2<\/sub>\uff081T&#8217;\uff09\uff0cMoTe<sub>2<\/sub>\uff08Td\uff09\u548cTaS<sub>2<\/sub>\uff081T\uff09\u7684\u7406\u8bba\u6570\u636e\u00a0[50]\uff09\u7684\u6bd4\u8f83\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1a<a href=\"https:\/\/link.springer.com\/article\/10.1007\/s40843-017-9178-4\"><strong>Topological quantum catalyst: Dirac nodal line states and a potential electrocatalyst of hydrogen evolution in the TiSi family<\/strong><strong>.\u00a0<\/strong><strong><em>Science China Materials<\/em>, 2018, 61(1): 23-29.<\/strong><\/a><\/p>\n<p>\u672c\u6587\u8f6c\u8f7d\u81ea\u4e2d\u56fd\u79d1\u5b66\u6750\u6599\uff0c\u7531\u6750\u6599\u4eba\u7279\u7ea6\u4f5c\u8005\u3001Science China Materials\u5b9e\u4e60\u7f16\u8f91\u5434\u79b9\u7ff0\u7f16\u8f91\u3001\u53d1\u5e03\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4e2d\u56fd\u79d1\u5b66\u9662\u91d1\u5c5e\u7814\u7a76\u6240\u6c88\u9633\u6750\u6599\u79d1\u5b66\u56fd\u5bb6\u7814\u7a76\u4e2d\u5fc3\u9648\u661f\u79cb\u7814\u7a76\u56e2\u961f\u5229\u7528\u8282\u7ebf\u534a\u91d1\u5c5e\u4ea7\u751f\u7684\u9f13\u819c\u72b6\u8868\u9762\u6001\u4f5c\u4e3a\u6790\u6c22\u53cd\u5e94\u7684\u50ac\u5316\u5e73\u53f0\uff0c\u63d0\u51fa\u4e86\u62d3\u6251\u91cf\u5b50\u50ac\u5316\u7684\u65b0\u6982\u5ff5\uff0c\u5e76\u5efa\u8baeTiSi\u5bb6\u65cf&#8230;<\/p>\n","protected":false},"author":4695,"featured_media":121781,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-121764","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/121764"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/4695"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=121764"}],"version-history":[{"count":10,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/121764\/revisions"}],"predecessor-version":[{"id":125844,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/121764\/revisions\/125844"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/121781"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=121764"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=121764"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=121764"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}