{"id":122282,"date":"2018-01-23T06:30:57","date_gmt":"2018-01-22T22:30:57","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=122282"},"modified":"2018-01-22T10:25:00","modified_gmt":"2018-01-22T02:25:00","slug":"%e5%8c%97%e4%ba%ac%e7%ba%b3%e7%b1%b3%e8%83%bd%e6%ba%90%e6%89%80nature%e5%ad%90%e5%88%8a%ef%bc%9a%e5%8f%af%e6%8b%89%e4%bc%b8%e6%89%a9%e5%b1%95%e7%9a%84%e5%a4%9a%e5%8a%9f%e8%83%bd%e9%9b%86%e6%88%90","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=122282","title":{"rendered":"\u5317\u4eac\u7eb3\u7c73\u80fd\u6e90\u6240Nature\u5b50\u520a\uff1a\u53ef\u62c9\u4f38\u6269\u5c55\u7684\u591a\u529f\u80fd\u96c6\u6210\u7535\u5b50\u76ae\u80a4"},"content":{"rendered":"<p><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/p>\n<p>\u4eba\u4f53\u76ae\u80a4\u662f\u4e00\u4e2a\u6d3b\u8dc3\u3001\u975e\u5e38\u654f\u611f\u548c\u9ad8\u5f39\u6027\u7684\u611f\u89c9\u5668\u5b98\uff0c\u4e3b\u8981\u627f\u62c5\u7740\u4fdd\u62a4\u8eab\u4f53\u3001\u6392\u6c57\u3001\u6e29\u5ea6\u8c03\u8282\u3001\u611f\u77e5\u51b7\u70ed\u548c\u538b\u529b\u7b49\u529f\u80fd\u3002\u4eba\u4f53\u8eaf\u4f53\u611f\u89c9\u7cfb\u7edf\u80fd\u591f\u901a\u8fc7\u76ae\u80a4\u4e2d\u7684\u89e6\u89c9\u3001\u6e29\u5ea6\u3001\u75db\u89c9\u7b49\u611f\u53d7\u5668\u5c06\u5916\u754c\u73af\u5883\u523a\u6fc0\u8f6c\u5316\u4e3a\u7535\u8109\u51b2\u4fe1\u53f7\uff0c\u7ecf\u8fc7\u795e\u7ecf\u901a\u8def\u4f20\u5bfc\u81f3\u795e\u7ecf\u4e2d\u67a2\uff0c\u4ece\u800c\u4f7f\u76ae\u80a4\u83b7\u5f97\u89e6\u89c9\u3001\u75db\u89c9\u7b49\u611f\u89c9\u529f\u80fd\u3002\u57fa\u4e8e\u76ae\u80a4\u8fd9\u79cd\u591a\u529f\u80fd\u751f\u7269\u6a21\u578b\uff0c\u79d1\u5b66\u5bb6\u4eec\u5f00\u5c55\u4e86\u4e00\u95e8\u65b0\u5174\u5b66\u79d1\u7814\u7a76\u2014\u2014\u89e6\u611f\u7535\u5b50\u5b66\uff08\u4fd7\u79f0\u201c\u7535\u5b50\u76ae\u80a4\u201d\uff0cElectronic skin, E-skin\uff09\uff0c\u7528\u6765\u6a21\u4eff\u76ae\u80a4\u7684\u611f\u89c9\u529f\u80fd\u5982\u89e6\u89c9\u3001\u6e29\u5ea6\u611f\u77e5\u7b49\u529f\u80fd\u3002\u76ee\u524d\uff0c\u7535\u5b50\u76ae\u80a4\u662f\u5728\u67d4\u6027\u6216\u5f39\u6027\u57fa\u5e95\u4e0a\u5236\u4f5c\u5177\u5907\u63a2\u6d4b\u538b\u529b\u3001\u6e29\u5ea6\u6216\u5176\u4ed6\u523a\u6fc0\u7684\u4f20\u611f\u5668\u53ca\u9635\u5217\uff0c\u80fd\u591f\u611f\u77e5\u5468\u56f4\u73af\u5883\u4e2d\u7684\u591a\u79cd\u7269\u7406\u3001\u5316\u5b66\u3001\u751f\u7269\u7b49\u4fe1\u53f7\uff0c\u5c06\u6709\u52a9\u4e8e\u5f00\u53d1\u65b0\u578b\u4eba\u673a\u63a5\u53e3\u3001\u667a\u80fd\u673a\u5668\u4eba\u3001\u4eff\u751f\u5047\u80a2\u7b49\u667a\u80fd\u5316\u7cfb\u7edf\u3002\u7535\u5b50\u76ae\u80a4\u7684\u91cd\u8981\u53d1\u5c55\u8d8b\u52bf\u662f\uff1a\u591a\u529f\u80fd\u5316\u4ee5\u53ca\u591a\u91cd\u523a\u6fc0\u540c\u6b65\u76d1\u6d4b\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c\u6765\u81ea<strong>\u4e2d\u56fd\u79d1\u5b66\u9662\u5317\u4eac\u7eb3\u7c73\u80fd\u6e90\u4e0e\u7cfb\u7edf\u7814\u7a76\u6240\u6f58\u66f9\u5cf0\u7814\u7a76\u5458\u3001\u738b\u4e2d\u6797\u9662\u58eb\u7684\u7814\u7a76\u56e2\u961f<\/strong>\u5728Nature\u5b50\u520aNature Communications\u4e0a\u53d1\u8868\u9898\u4e3a\u201cSkin-inspired highly stretchable and conformable matrix networks for multifunctional sensing\u201d\u7684\u6587\u7ae0\u3002\u8be5\u6587\u7ae0\u62a5\u9053\u4e86\u4e00\u79cd\u67d4\u6027\u53ef\u62c9\u4f38\u6269\u5c55\u7684\u591a\u529f\u80fd\u96c6\u6210\u4f20\u611f\u5668\u9635\u5217\uff0c\u6210\u529f\u5730\u5c06\u7535\u5b50\u76ae\u80a4\u7684\u63a2\u6d4b\u80fd\u529b\u6269\u5c55\u52307\u79cd\uff0c\u5b9e\u73b0\u4e86\u6e29\u5ea6\u3001\u6e7f\u5ea6\u3001\u7d2b\u5916\u5149\u3001\u78c1\u3001\u5e94\u53d8\u3001\u538b\u529b\u548c\u63a5\u8fd1\u7b49\u591a\u79cd\u5916\u754c\u523a\u6fc0\u7684\u5b9e\u65f6\u540c\u6b65\u76d1\u6d4b\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u56fe\u4e00\uff1a\u76ae\u80a4\u542f\u53d1\u7684\u53ef\u62c9\u4f38\u6269\u5c55\u7684\u591a\u529f\u80fd\u96c6\u6210\u7535\u5b50\u76ae\u80a4\uff08<\/strong><strong>SCMN<\/strong><strong>\uff09<\/strong><\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-122283\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe1-13.jpg\" alt=\"\" width=\"600\" height=\"567\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe1-13.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe1-13-300x284.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p>a. \u7531\u76ae\u80a4\u7684\u7ed3\u6784\u548c\u529f\u80fd\u542f\u53d1\u7684\u6982\u5ff5\u793a\u610f\u56fe\uff1b<\/p>\n<p>b. \u5177\u5907\u53ef\u62c9\u4f38\u6269\u5c55\u529f\u80fd\u7684\u805a\u9170\u4e9a\u80fa\uff08PI\uff09\u62c9\u4f38\u7ed3\u6784\u7f51\u7edc\uff1b<\/p>\n<p>c. PI\u62c9\u4f38\u7ed3\u6784\u7f51\u7edc\u7684SEM\u56fe\uff1b<\/p>\n<p>d. SCMN\u7684\u7ed3\u6784\u793a\u610f\u56fe\uff1b<\/p>\n<p>e. SCMN\u7684\u67d4\u6027\u3001\u62c9\u4f38\u6027\u548c\u8d34\u5408\u6027\u7b49\u56fe\u3002<\/p>\n<p><strong>\u56fe\u4e8c\uff1a<\/strong><strong>PI<\/strong><strong>\u62c9\u4f38\u7ed3\u6784\u7684\u529b\u5b66\u548c\u7535\u5b66\u6027\u80fd<\/strong><\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-122284\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe2-8.jpg\" alt=\"\" width=\"600\" height=\"581\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe2-8.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe2-8-300x291.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p>a. \u873f\u8712\u62c9\u4f38\u7ed3\u6784\u7684\u529b\u5b66\u548c\u7535\u5b66\u6d4b\u8bd5\uff1b<\/p>\n<p>b. \u873f\u8712\u62c9\u4f38\u7ed3\u6784\u5728\u4e0d\u540c\u62c9\u4f38\u500d\u7387\u7684\u56fe\u7247\uff1b<\/p>\n<p>e. \u873f\u8712\u62c9\u4f38\u7ed3\u6784\u7684\u8010\u4e45\u6027\u6d4b\u8bd5\uff1b<\/p>\n<p>f. \u873f\u8712\u62c9\u4f38\u7ed3\u6784\u7684\u5f2f\u6298\u6027\u6d4b\u8bd5\uff1b<\/p>\n<p>g. PI\u62c9\u4f38\u7ed3\u6784\u7f51\u7edc\u7684\u9762\u79ef\u6269\u5f20\uff1b<\/p>\n<p>h. PI\u62c9\u4f38\u7ed3\u6784\u7f51\u7edc\u7684\u626d\u66f2\u56fe\u7247\u3002<\/p>\n<p><strong>\u56fe\u4e09\uff1a<\/strong><strong>SCMN<\/strong><strong>\u7684\u591a\u529f\u80fd\u4f20\u611f\u7279\u6027<\/strong><\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-122285\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe3-8.jpg\" alt=\"\" width=\"600\" height=\"955\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe3-8.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe3-8-188x300.jpg 188w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p>a. \u6e29\u5ea6\u4f20\u611f\u5668\u7684\u54cd\u5e94\u66f2\u7ebf\uff1b<\/p>\n<p>b. \u6e29\u5ea6\u4f20\u611f\u5668\u9635\u5217\u7684\u7a7a\u95f4\u6e29\u5ea6\u63a2\u6d4b\u6210\u50cf\u56fe\uff1b<\/p>\n<p>c. \u5e94\u53d8\u4f20\u611f\u5668\u7684\u54cd\u5e94\u66f2\u7ebf\uff1b<\/p>\n<p>d. \u5e94\u53d8\u4f20\u611f\u5668\u5bf9\u4e0d\u540c\u5e94\u53d8\u7684\u54cd\u5e94\u8fc7\u7a0b\uff1b<\/p>\n<p>e. \u6e7f\u5ea6\u4f20\u611f\u5668\u7684\u54cd\u5e94\u66f2\u7ebf\uff1b<\/p>\n<p>f. \u6e7f\u5ea6\u4f20\u611f\u5668\u7684\u9635\u5217\u7684\u7a7a\u95f4\u6e7f\u5ea6\u63a2\u6d4b\u6210\u50cf\u56fe\uff1b<\/p>\n<p>g. \u7d2b\u5916\u5149\u4f20\u611f\u5668\u7684\u54cd\u5e94\u66f2\u7ebf\uff1b<\/p>\n<p>h. \u7d2b\u5916\u5149\u4f20\u611f\u5668\u5bf9\u4e0d\u540c\u5149\u5f3a\u7684\u54cd\u5e94\u8fc7\u7a0b\uff1b<\/p>\n<p>i. \u78c1\u4f20\u611f\u5668\u7684\u54cd\u5e94\u66f2\u7ebf\uff1b<\/p>\n<p>j. \u78c1\u4f20\u611f\u5668\u63a2\u6d4b\u7531\u6c38\u78c1\u4f53\u9760\u8fd1\/\u79bb\u5f00\u5f15\u8d77\u7684\u78c1\u573a\u53d8\u5316\u3002<\/p>\n<p><strong>\u56fe\u56db\uff1a\u538b\u529b\u548c\u63a5\u8fd1\u4f20\u611f\u7279\u6027\u4ee5\u53ca<\/strong><strong>SCMN<\/strong><strong>\u63a2\u6d4b\u9762\u79ef\u6269\u5f20<\/strong><\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-122286\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe4-8.jpg\" alt=\"\" width=\"600\" height=\"613\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe4-8.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe4-8-294x300.jpg 294w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p>a. \u538b\u529b\u4f20\u611f\u5668\u7684\u54cd\u5e94\u66f2\u7ebf\uff1b<\/p>\n<p>b. \u538b\u529b\u4f20\u611f\u5668\u5bf9\u5fae\u5c0f\u538b\u529b\u7684\u5b9e\u65f6\u63a2\u6d4b\uff1b<\/p>\n<p>c. \u538b\u529b\u4f20\u611f\u5668\u9635\u5217\u7684\u7a7a\u95f4\u538b\u529b\u63a2\u6d4b\u6210\u50cf\u56fe\uff1b<\/p>\n<p>d. \u538b\u529b\u548c\u63a5\u8fd1\u63a2\u6d4b\u7684\u8026\u5408\u8fc7\u7a0b\uff1b<\/p>\n<p>e. \u63a5\u8fd1\u4f20\u611f\u5668\u7684\u54cd\u5e94\u66f2\u7ebf\uff1b<\/p>\n<p>f. \u63a5\u8fd1\u4f20\u611f\u5668\u9635\u5217\u7684\u7a7a\u95f4\u63a5\u8fd1\u63a2\u6d4b\u6210\u50cf\u56fe\uff1b<\/p>\n<p>g. SCMN\u63a2\u6d4b\u9762\u79ef\u6269\u5f20\u5bf9\u6bd4\u56fe\uff1b<\/p>\n<p>h. SCMN\u63a2\u6d4b\u9762\u79ef\u6269\u5f20\u524d\u540e\u7684\u538b\u529b\u6210\u50cf\u56fe\u3002<\/p>\n<p><strong>\u56fe\u4e94\uff1a<\/strong><strong>SCMN<\/strong><strong>\u5bf9\u591a\u79cd\u523a\u6fc0\u7684\u5b9e\u65f6\u540c\u6b65\u76d1\u6d4b<\/strong><\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-122287\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe5-9.jpg\" alt=\"\" width=\"600\" height=\"263\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe5-9.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe5-9-300x132.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p>a. SCMN\u5bf9\u6e29\u5ea6\u3001\u538b\u529b\u548c\u63a5\u8fd1\u7b49\u523a\u6fc0\u7684\u5b9e\u65f6\u76d1\u6d4b\uff1b<\/p>\n<p>b. SCMN\u5bf9\u78c1\u573a\u3001\u538b\u529b\u548c\u63a5\u8fd1\u7b49\u523a\u6fc0\u7684\u5b9e\u65f6\u76d1\u6d4b\u3002<\/p>\n<p><strong>\u56fe\u516d\uff1a\u5b9a\u5236\u5316\u529f\u80fd\u96c6\u6210\u7684\u667a\u80fd\u5047\u80a2<\/strong><\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-122288\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe6-3.jpg\" alt=\"\" width=\"600\" height=\"444\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe6-3.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/\u56fe6-3-300x222.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/strong><\/p>\n<p>a. \u4eba\u6293\u53d6\u676f\u5b50\u8fc7\u7a0b\u4e2d\u6e29\u5ea6\u611f\u77e5\u7684\u6982\u5ff5\u56fe\uff1b<\/p>\n<p>b. \u667a\u80fd\u5047\u80a2\u5bf9\u676f\u5b50\u7684\u6293\u53d6\u548c\u91ca\u653e\uff1b<\/p>\n<p>c. \u538b\u529b\u3001\u6e29\u5ea6\u4f20\u611f\u5668\u5728\u5047\u80a2\u624b\u6307\u4e0a\u7684\u5206\u5e03\u793a\u610f\u4ee5\u53ca\u6293\u53d61\u2103\u6c34\u6e29\u676f\u5b50\u65f6\u5404\u624b\u6307\u90e8\u4f4d\u7684\u53d7\u529b\u60c5\u51b5\uff1b<\/p>\n<p>d. \u667a\u80fd\u5047\u80a2\u5728\u6293\u53d64\u79cd\u4e0d\u540c\u6c34\u6e29\u676f\u5b50\u65f6\u538b\u529b\u548c\u6e29\u5ea6\u54cd\u5e94\u66f2\u7ebf\uff1b<\/p>\n<p>e. \u667a\u80fd\u5047\u80a2\u53ef\u4ee5\u4f9d\u636e\u6e29\u5ea6\u54cd\u5e94\u60c5\u51b5\u6765\u5224\u65ad\u676f\u4e2d\u6c34\u6e29\u3002<\/p>\n<p><strong>\u3010\u5c0f\u7ed3\u3011<\/strong><\/p>\n<p>\u901a\u8fc7\u5fae\u7eb3\u52a0\u5de5\u6280\u672f\uff0c\u5236\u5907\u51fa\u4e86\u5927\u500d\u7387\uff088\u500d\u53ca\u4ee5\u4e0a\uff0c\u53ef\u6839\u636e\u9700\u8981\u8bbe\u8ba1\uff09\u7684\u805a\u9170\u4e9a\u80fa\uff08PI\uff09\u62c9\u4f38\u7ed3\u6784\u7f51\u7edc\uff0c\u5176\u4e2d\u5305\u62ec\u8bb8\u591a\u4f20\u611f\u5668\u8282\u70b9\u548c\u873f\u8712\u62c9\u4f38\u7ed3\u6784\u3002\u57fa\u4e8e\u8fd9\u79cd\u62c9\u4f38\u7ed3\u6784\u7f51\u7edc\uff0c\u591a\u79cd\u4f20\u611f\u5668\u80fd\u591f\u4ee5\u4e8c\u7ef4\u5206\u5e03\u5f0f\u6216\u4e09\u7ef4\u53e0\u5c42\u5f0f\u7ed3\u6784\u8fdb\u884c\u591a\u529f\u80fd\u5316\u96c6\u6210\uff0c\u5e76\u4e14\u591a\u79cd\u4f20\u611f\u5355\u5143\u53ef\u72ec\u7acb\u5de5\u4f5c\u800c\u4e0d\u4e92\u76f8\u5f71\u54cd\uff0c\u5229\u7528\u57fa\u5e95\u7684\u53ef\u62c9\u4f38\u6027\u80fd\u5b9e\u73b0\u4e86\u7535\u5b50\u76ae\u80a4\u7684\u63a2\u6d4b\u9762\u79ef\u6269\u5f20\uff0c\u5e76\u4e3a\u5176\u8fdb\u4e00\u6b65\u7684\u529f\u80fd\u6269\u5c55\u63d0\u4f9b\u4e86\u6781\u5927\u4fbf\u5229\u3002\u53e6\u5916\uff0c\u8fd8\u5c06\u8fd9\u79cd\u7535\u5b50\u76ae\u80a4\u7528\u4e8e\u5236\u9020\u4e86\u4e00\u79cd\u5177\u6709\u5b9a\u5236\u5316\u529f\u80fd\u96c6\u6210\u7684\u667a\u80fd\u5047\u80a2\uff0c\u65e2\u8d4b\u4e88\u4e86\u5047\u80a2\u89e6\u89c9\u529f\u80fd\uff0c\u540c\u65f6\u4f7f\u5047\u80a2\u5177\u5907\u4e86\u6e29\u5ea6\u611f\u77e5\u7684\u80fd\u529b\uff0c\u8fd9\u5c06\u6709\u5229\u4e8e\u6539\u5584\u6b8b\u75be\u60a3\u8005\u7684\u5eb7\u590d\u53ca\u751f\u6d3b\u6761\u4ef6\u3002\u591a\u529f\u80fd\u96c6\u6210\u7535\u5b50\u76ae\u80a4\u4e0d\u4ec5\u53ef\u4ee5\u5b9e\u65f6\u540c\u6b65\u76d1\u6d4b\u5468\u8fb9\u73af\u5883\u591a\u79cd\u53d8\u91cf\uff0c\u540c\u65f6\u8fd8\u80fd\u7528\u4e8e\u4eba\u4f53\u5065\u5eb7\u76d1\u6d4b\u7b49\u9886\u57df\u3002\u5b83\u5c06\u4f5c\u4e3a\u4e00\u79cd\u667a\u80fd\u7ec8\u7aef\uff0c\u6784\u5efa\u65b0\u578b\u7684\u201c\u4e92\u52a8\u7f51\u201d\uff08Internet of \u2018action\u2019, IoA\uff09\uff0c\u6539\u53d8\u6211\u4eec\u4e0e\u79d1\u6280\u7684\u4ea4\u4e92\u65b9\u5f0f\uff0c\u8ba9\u6211\u4eec\u7684\u751f\u6d3b\u56e0\u79d1\u6280\u53d8\u5f97\u66f4\u7f8e\u597d\uff01<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>\uff1a<a href=\"https:\/\/www.nature.com\/articles\/s41467-017-02685-9\" target=\"_blank\" rel=\"noopener\">Skin-inspired highly stretchable and conformable matrix networks for multifunctional sensing<\/a> (Nat. Commun., 2018, DOI:10.1038\/s41467-017-02685-9)<\/p>\n<p>\u672c\u6587\u7531\u4e2d\u56fd\u79d1\u5b66\u9662\u5317\u4eac\u7eb3\u7c73\u80fd\u6e90\u4e0e\u7cfb\u7edf\u7814\u7a76\u6240\u6f58\u66f9\u5cf0\u8001\u5e08\u63d0\u4f9b\u3002<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8\u5927\u5bb6\u5ead<\/a>\u3002\u5982\u679c\u4f60\u5bf9\u7535\u5b50\u6750\u6599\u611f\u5174\u8da3\uff0c\u613f\u610f\u4e0e\u7535\u5b50\u7535\u5de5\u9886\u57df\u4eba\u624d\u4ea4\u6d41\uff0c\u8bf7\u52a0\u5165\u6750\u6599\u4eba\u7535\u5b50\u7535\u5de5\u6750\u6599\u5b66\u4e60\u5c0f\u7ec4\uff08QQ\u7fa4\uff1a482842474\uff09\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1aRDD-2011-CHERISH , \u4efb\u4e39\u4e39\uff0c\u6211\u4eec\u4f1a\u9080\u8bf7\u5404\u4f4d\u8001\u5e08\u52a0\u5165\u4e13\u5bb6\u7fa4\u3002<\/p>\n<p>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener\">\u6d4b\u8bd5\u8c37<\/a>\uff01<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u4eba\u4f53\u76ae\u80a4\u662f\u4e00\u4e2a\u6d3b\u8dc3\u3001\u975e\u5e38\u654f\u611f\u548c\u9ad8\u5f39\u6027\u7684\u611f\u89c9\u5668\u5b98\uff0c\u4e3b\u8981\u627f\u62c5\u7740\u4fdd\u62a4\u8eab\u4f53\u3001\u6392\u6c57\u3001\u6e29\u5ea6\u8c03\u8282\u3001\u611f\u77e5\u51b7\u70ed\u548c\u538b\u529b\u7b49\u529f\u80fd\u3002\u4eba\u4f53\u8eaf\u4f53\u611f\u89c9\u7cfb\u7edf\u80fd\u591f\u901a\u8fc7\u76ae\u80a4\u4e2d\u7684\u89e6\u89c9\u3001\u6e29\u5ea6\u3001&#8230;<\/p>\n","protected":false},"author":99,"featured_media":122290,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215,2],"tags":[1302,31,2754],"class_list":["post-122282","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","category-keji","tag-wangzhonglin","tag-dianzi","tag-2754"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/122282"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/99"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=122282"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/122282\/revisions"}],"predecessor-version":[{"id":122641,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/122282\/revisions\/122641"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/122290"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=122282"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=122282"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=122282"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}