{"id":128677,"date":"2018-03-08T06:30:47","date_gmt":"2018-03-07T22:30:47","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=128677"},"modified":"2018-03-07T18:27:42","modified_gmt":"2018-03-07T10:27:42","slug":"%e5%8d%97%e4%ba%ac%e5%a4%a7%e5%ad%a6%e7%bc%aa%e5%b3%b0%e4%b8%8e%e8%a2%81%e6%b4%aa%e6%b6%9bnano-letters%ef%bc%9a%e4%b8%bb%e6%97%8f%e9%87%91%e5%b1%9e%e7%a1%ab%e5%8c%96%e7%89%a9%e7%95%8c%e9%9d%a2","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=128677","title":{"rendered":"\u5357\u4eac\u5927\u5b66\u7f2a\u5cf0\u4e0e\u8881\u6d2a\u6d9bNano Letters\uff1a\u4e3b\u65cf\u91d1\u5c5e\u786b\u5316\u7269\u754c\u9762\u8d85\u5bfc"},"content":{"rendered":"<p><strong><b>\u3010\u5f15\u8a00\u3011<\/b><\/strong><\/p>\n<p>\u8d85\u5bfc\u4f5c\u4e3a\u4e00\u79cd\u795e\u5947\u7684\u7269\u7406\u73b0\u8c61\uff0c\u88ab\u53d1\u73b0\u8ddd\u4eca\u5df2\u4e00\u767e\u591a\u5e74\u3002\u7531\u4e8e\u9ad8\u6e29\u8d85\u5bfc\u673a\u5236\u7b49\u8fd8\u6ca1\u6709\u5b8c\u5168\u88ab\u7406\u89e3\uff0c\u8d85\u5bfc\u4f9d\u65e7\u662f\u51dd\u805a\u6001\u7269\u7406\u9886\u57df\u6700\u70ed\u95e8\u7684\u8bdd\u9898\u4e4b\u4e00\uff0c\u4eba\u4eec\u4e5f\u4e00\u76f4\u6ca1\u6709\u505c\u6b62\u63a2\u7d22\u65b0\u5174\u8d85\u5bfc\u6750\u6599\u7684\u6b65\u4f10\u3002\u8fd1\u5e74\u6765\uff0c\u968f\u7740\u51dd\u805a\u6001\u7269\u7406\u5b9e\u9a8c\u6280\u672f\u7684\u53d1\u5c55\uff0c\u4e00\u4e9b\u539f\u672c\u88ab\u8ba4\u4e3a\u4e0d\u80fd\u8d85\u5bfc\u7684\u6750\u6599\uff0c\u88ab\u53d1\u73b0\u968f\u7740\u8f7d\u6d41\u5b50\u6d53\u5ea6\u7684\u589e\u52a0\u4e5f\u53ef\u4ee5\u51fa\u73b0\u8d85\u5bfc\u73b0\u8c61\u3002\u8fd9\u5176\u4e2d\u6709\u4e00\u79cd\u53eb\u505a\u79bb\u5b50\u6db2\u4f53\u95e8\uff08\u6216\u7535\u53cc\u5c42\u6676\u4f53\u7ba1\uff09\u7684\u6280\u672f\uff0c\u53ef\u5728\u6837\u54c1\u8868\u9762\u96c6\u805a\u6781\u9ad8\u7684\u8f7d\u6d41\u5b50\u6d53\u5ea6\uff0c\u8fdb\u800c\u8bf1\u5bfc\u65b0\u5947\u7684\u754c\u9762\u8d85\u5bfc\u73b0\u8c61\u3002<\/p>\n<p><strong><b>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/b><\/strong><\/p>\n<p>\u76ee\u524d\uff0c\u6765\u81ea<strong><b>\u5357\u4eac\u5927\u5b66\u7269\u7406\u5b66\u9662\u7684\u7f2a\u5cf0\u6559\u6388<\/b><\/strong>\u8bfe\u9898\u7ec4\u3001<strong>\u8881\u6d2a\u6d9b\u6559\u6388<\/strong>\u4e0e\u5408\u4f5c\u56e2\u961f\u5728<strong><b>\u300a\u7eb3\u7c73\u5feb\u62a5\u300b(<\/b><\/strong><strong><b>Nano Letters<\/b><\/strong><strong><b>)<\/b><\/strong>\u4e0a\u53d1\u8868\u9898\u4e3a&#8221;<strong><b>Gate-Induced Interfacial Superconductivity in 1T-SnSe<\/b><\/strong><strong><sub><b>2<\/b><\/sub><\/strong>\u201d\u7684\u6587\u7ae0\u3002\u8be5\u6587\u7ae0\u62a5\u9053\u5229\u7528\u79bb\u5b50\u6db2\u4f53\u95e8\u6280\u672f\uff0c\u8c03\u8282\u4e8c\u7852\u5316\u9521\uff08\u4e00\u79cd\u5178\u578b\u7684\u4e3b\u65cf\u91d1\u5c5e\u786b\u65cf\u5316\u5408\u7269\uff09\u5230\u8d85\u9ad8\u7684\u8f7d\u6d41\u5b50\u6d53\u5ea6\u72b6\u6001\uff08\u224810<sup>14<\/sup>cm<sup>-2<\/sup>\uff09\uff0c\u9996\u6b21\u89c2\u6d4b\u5230\u4e8c\u7852\u5316\u9521\u7684\u672c\u5f81\u8d85\u5bfc\u73b0\u8c61\u3002\u56e2\u961f\u53d1\u73b0\u8d85\u5bfc\u4e34\u754c\u78c1\u573a\u4e0e\u89d2\u5ea6\u4e4b\u95f4\u6ee1\u8db3\u4e8c\u7ef4\u7684Tinkham\u6a21\u578b\u3002\u8be5\u8d85\u5bfc\u7684\u6f29\u6da1\u5b58\u5728\u4e24\u79cd\u72b6\u6001\uff1a\u5728\u6e29\u5ea6\u7565\u4f4e\u4e8e\u8d85\u5bfc\u6e29\u5ea6\u65f6\uff0c\u8d85\u5bfc\u6027\u8d28\u5904\u4e8e\u70ed\u6fc0\u53d1\u78c1\u901a\u6d41\u52a8\u72b6\uff1b\u968f\u7740\u6e29\u5ea6\u8fdb\u4e00\u6b65\u964d\u4f4e\uff0c\u8d85\u5bfc\u6f29\u6da1\u6001\u4ee5\u91cf\u5b50\u96a7\u7a7f\u7684\u65b9\u5f0f\u8fdb\u884c\u8815\u52a8\uff08\u91cf\u5b50\u8815\u52a8\u6001\uff09\u3002\u540c\u65f6\uff0c\u7814\u7a76\u56e2\u961f\u4e5f\u53d1\u73b0\u5e73\u884c\u78c1\u573a\u4e0b\u7684\u4e34\u754c\u78c1\u573a\u5728\u8d8b\u4e8e\u7edd\u5bf9\u96f6\u5ea6\u65f6\u8d85\u8fc7\u6ce1\u5229\u987a\u78c1\u6781\u96502\u52303\u500d\uff0c\u8be5\u73b0\u8c61\u548c\u7535\u573a\u8c03\u8282\u7684\u81ea\u65cb\u8f68\u9053\u8026\u5408\u6709\u5173\u3002\u8be5\u5de5\u4f5c\u4e3a\u63a8\u52a8\u63a2\u7d22\u65b0\u578b\u4e8c\u7ef4\u8d85\u5bfc\u6750\u6599\u53ca\u65b0\u5947\u7684\u8d85\u5bfc\u6027\u8d28\u8fc8\u51fa\u91cd\u8981\u4e00\u6b65\u3002\u5408\u4f5c\u7814\u7a76\u56e2\u961f\u8fd8\u5305\u62ec\u65af\u5766\u798f\u5927\u5b66\u7684\u5d14\u5c79\u6559\u6388\u8bfe\u9898\u7ec4\u3001Harold Hwang\u6559\u6388\u8bfe\u9898\u7ec4\u548c\u5357\u4eac\u5927\u5b66\u7684\u738b\u9e4f\u6559\u6388\u8bfe\u9898\u7ec4\u3002<\/p>\n<p><strong><b>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/b><\/strong><\/p>\n<p><strong><b>\u56fe1\u00a0<\/b><\/strong><strong><b>\u4e8c\u7852\u5316\u9521\u7684\u6676\u4f53\u7ed3\u6784\uff0c\u8f6c\u79fb\u66f2\u7ebf\u53ca\u8d85\u5bfc\u6027\u8d28<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-128678 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72471-10.png\" alt=\"\" width=\"600\" height=\"385\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72471-10.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72471-10-300x193.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>a. \u4e8c\u7852\u5316\u9521\u7684\u6676\u4f53\u7ed3\u6784\u56fe<\/p>\n<p>b. \u57fa\u4e8e\u79bb\u5b50\u6db2\u4f53\u95e8\u6280\u672f\u5236\u5907\u7684\u7535\u53cc\u5c42\u6676\u4f53\u7ba1\u793a\u610f\u56fe<\/p>\n<p>c. \u591a\u7aef\u970d\u5c14\u7ed3\u6784\u5668\u4ef6\u7684\u5149\u5b66\u663e\u5fae\u955c\u56fe<\/p>\n<p>d. \u573a\u6548\u5e94\u8f6c\u79fb\u66f2\u7ebf<\/p>\n<p>e. \u7535\u963b\u968f\u6e29\u5ea6\u7684\u53d8\u5316\u66f2\u7ebf\uff0c\u5728\u6e29\u5ea6\u4e3a3.9K\u53d1\u751f\u8d85\u5bfc<\/p>\n<p>f. \u4e0d\u540c\u78c1\u573a\u4e0b\u7684\u8d85\u5bfc\u8f6c\u53d8\u66f2\u7ebf<\/p>\n<p><strong><b>\u56fe2\u00a0<\/b><\/strong><strong><b>\u4e8c\u7ef4\u8d85\u5bfc\u6001\u7684\u786e\u5b9a<\/b><\/strong><\/p>\n<p><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-128679 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72472-10.png\" alt=\"\" width=\"600\" height=\"372\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72472-10.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72472-10-300x186.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong>a. \u4e0d\u540c\u78c1\u573a\u65b9\u5411\u4e0b\u78c1\u963b\u968f\u78c1\u573a\u53d8\u5316\u66f2\u7ebf\uff0c\u63d2\u56fe\u5b9a\u4e49\u78c1\u573a\u65b9\u5411<\/p>\n<p>b. \u8d85\u5bfc\u4e34\u754c\u78c1\u573a\u4e0e\u78c1\u573a\u89d2\u5ea6\u7684\u5173\u7cfb\uff0c\u63d2\u56fe\u4e3a\u5728\u5e73\u884c\u78c1\u573a\u9644\u8fd1\u7684\u653e\u5927\u56fe<\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>3\u00a0<\/b><\/strong><strong><b>\u8d85\u5bfc\u6f29\u6da1\u6001\u5206\u6790<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-128680 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72473-10.png\" alt=\"\" width=\"600\" height=\"599\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72473-10.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72473-10-150x150.png 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72473-10-300x300.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>a. \u4e0d\u540c\u78c1\u573a\u4e0b\u7684\u8d85\u5bfc\u8f6c\u53d8\u66f2\u7ebf\uff08Arrhenius plot\uff09<\/p>\n<p>b. \u78c1\u573a\u4f9d\u8d56\u7684\u70ed\u6fc0\u6d3b\u80fd<\/p>\n<p>c. \u57281.6 K\u4e0b\u7535\u963b\u968f\u6e29\u5ea6\u7684\u53d8\u5316\u66f2\u7ebf\uff0c\u9ed1\u7ebf\u4e3a\u91cf\u5b50\u8815\u52a8\u6001\u66f2\u7ebf<\/p>\n<p>d. \u6f29\u6da1\u6001\u7684\u76f8\u56fe\u3002\u6a58\u9ec4\u8272\u4ee3\u8868\u70ed\u6fc0\u53d1\u78c1\u901a\u6d41\u52a8\u6001\uff08TAFF\uff09\uff0c\u7eff\u8272\u4e3a\u91cf\u5b50\u8815\u52a8\u6001\uff0c\u9ec4\u8272\u662f\u9000\u9489\u624e\u6001<\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>4\u00a0<\/b><\/strong><strong><b>\u5e73\u884c\u78c1\u573a\u4e0b\u4e0d\u540c\u6e29\u5ea6\u7684\u8d85\u5bfc\u4e34\u754c\u78c1\u573a<\/b><\/strong><\/p>\n<p><strong><b>\u00a0<img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-128681 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72474-10.png\" alt=\"\" width=\"600\" height=\"593\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72474-10.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72474-10-300x297.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p>\u51e0\u79cd\u6709\u4ee3\u8868\u6027\u6750\u6599\u4e0d\u540c\u6e29\u5ea6\u7684\u8d85\u5bfc\u4e34\u754c\u78c1\u573a\u548c\u6ce1\u5229\u987a\u78c1\u6781\u9650\u7684\u6bd4\u503c\uff08<em>B<\/em><sub>c2<\/sub><sup>\u2161<\/sup>\/<em>B<\/em><sub>c\u00a0<\/sub><sup>p<\/sup>\uff09\u4e0e\u4e8c\u7852\u5316\u9521\u4e2d\u7684\u5bf9\u6bd4\u3002<\/p>\n<p><strong><b>\u3010\u5c0f\u7ed3\u3011<\/b><\/strong><\/p>\n<p>\u8fd9\u9879\u7814\u7a76\u5de5\u4f5c\u4e0d\u4ec5\u62a5\u9053\u4e86\u9996\u6b21\u5728\u4e3b\u65cf\u91d1\u5c5e\u786b\u65cf\u5316\u5408\u7269\u6750\u6599\u4f53\u7cfb\uff08\u4e8c\u7852\u5316\u9521\uff09\u4e2d\u901a\u8fc7\u8c03\u8282\u8d85\u9ad8\u8f7d\u6d41\u5b50\u6d53\u5ea6\u6765\u8bf1\u5bfc\u6750\u6599\u7684\u672c\u5f81\u4e8c\u7ef4\u8d85\u5bfc\u6001\uff0c\u63ed\u793a\u8be5\u4e8c\u7ef4\u8d85\u5bfc\u6001\u7684\u65b0\u5947\u7269\u7406\u6027\u8d28\uff1b\u540c\u65f6\u4e5f\u4e3a\u63a2\u7d22\u4e0d\u540c\u6750\u6599\u4f53\u7cfb\u4e2d\u53ef\u80fd\u51fa\u73b0\u7684\u8d85\u5bfc\u6001\u548c\u5947\u5f02\u7684\u8d85\u5bfc\u6027\u8d28\u63d0\u4f9b\u4e86\u65b0\u7684\u65b9\u5411\u3002<\/p>\n<p><strong><b>\u6587\u732e\u94fe\u63a5\uff1a<\/b><\/strong>\u00a0<a href=\"https:\/\/pubs.acs.org\/doi\/10.1021\/acs.nanolett.7b05157\" target=\"_blank\" rel=\"noopener\">Gate-Induced Interfacial Superconductivity in 1T-SnSe<sub>2<\/sub><\/a>\u00a0(Nano Lett. 18, 1410 (2018), DOI: 10.1021\/acs.nanolett.7b05157)<\/p>\n<p>\u672c\u6587\u7531\u5357\u4eac\u5927\u5b66\u7269\u7406\u5b66\u9662\u7684\u7f2a\u5cf0\u6559\u6388\u8bfe\u9898\u7ec4\u63d0\u4f9b\uff0c\u7279\u6b64\u611f\u8c22\uff01<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8\u5927\u5bb6\u5ead<\/a>\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n<p><strong>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener\">\u6d4b\u8bd5\u8c37<\/a>\uff01<\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u8d85\u5bfc\u4f5c\u4e3a\u4e00\u79cd\u795e\u5947\u7684\u7269\u7406\u73b0\u8c61\uff0c\u88ab\u53d1\u73b0\u8ddd\u4eca\u5df2\u4e00\u767e\u591a\u5e74\u3002\u7531\u4e8e\u9ad8\u6e29\u8d85\u5bfc\u673a\u5236\u7b49\u8fd8\u6ca1\u6709\u5b8c\u5168\u88ab\u7406\u89e3\uff0c\u8d85\u5bfc\u4f9d\u65e7\u662f\u51dd\u805a\u6001\u7269\u7406\u9886\u57df\u6700\u70ed\u95e8\u7684\u8bdd\u9898\u4e4b\u4e00\uff0c\u4eba\u4eec\u4e5f\u4e00\u76f4\u6ca1\u6709\u505c\u6b62\u63a2\u7d22&#8230;<\/p>\n","protected":false},"author":7350,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[113,2509],"class_list":["post-128677","post","type-post","status-publish","format-standard","hentry","category-jiedu","tag-semiconductor","tag-2509"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/128677"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/7350"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=128677"}],"version-history":[{"count":8,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/128677\/revisions"}],"predecessor-version":[{"id":128819,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/128677\/revisions\/128819"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=128677"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=128677"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=128677"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}