{"id":130321,"date":"2018-03-27T06:30:47","date_gmt":"2018-03-26T22:30:47","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=130321"},"modified":"2018-05-15T20:59:51","modified_gmt":"2018-05-15T12:59:51","slug":"%e9%87%91%e5%b1%9e%e7%a6%bb%e5%ad%90%e7%94%b5%e6%b1%a0%e5%89%8d%e6%b2%bf%e7%a0%94%e7%a9%b6%e6%88%90%e6%9e%9c%e7%b2%be%e9%80%89%e3%80%90%e7%ac%ac5%e6%9c%9f%e3%80%91","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=130321","title":{"rendered":"\u91d1\u5c5e\u79bb\u5b50\u7535\u6c60\u524d\u6cbf\u7814\u7a76\u6210\u679c\u7cbe\u9009\u3010\u7b2c5\u671f\u3011"},"content":{"rendered":"<p>\u672c\u671f\u91d1\u5c5e\u79bb\u5b50\u7535\u6c60\u7d20\u6750\u7684\u53d1\u8868\u65f6\u95f4\u4ece2018\u5e741\u670831\u65e5\u52302018\u5e743\u67085\u65e5\u3002\u6d89\u53ca\u6539\u5584\u7535\u89e3\u8d28\u754c\u9762\u3001\u5168\u56fa\u6001\u94a0\u7535\u6c60\u3001\u9502\u679d\u6676\u7b49\u65b9\u5411\u3002<\/p>\n<p><strong>1\u3001Angew. Chem.Int.Ed.\uff1a\u78b3\u9178\u6c1f\u4e59\u70ef\u6539\u5584<\/strong><strong>\u5bcc\u542bLiF\u7684\u56fa\u4f53\u7535\u89e3\u8d28\u754c\u9762\u589e\u5f3aMoS<sub>2<\/sub>\u9633\u6781\u7684\u7a33\u5b9a\u6027<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-130322\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72474-17.png\" alt=\"\" width=\"600\" height=\"371\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72474-17.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72474-17-300x186.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u4f5c\u4e3a\u9502\u79bb\u5b50\u7535\u6c60\uff08LIB\uff09\u7684\u9ad8\u5bb9\u91cf\u8d1f\u6781\uff0cMoS<sub>2<\/sub>\u5bff\u547d\u77ed\uff0c\u90e8\u5206\u539f\u56e0\u662f\u5176\u56fa\u4f53\u7535\u89e3\u8d28\u754c\u9762\uff08SEI\uff09\u4e0d\u7a33\u5b9a\u3002\u8fd1\u65e5\uff0c<strong>\u65b0\u52a0\u5761\u5357\u6d0b\u7406\u5de5\u5927\u5b66Xiaodong Chen\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u7b49\u4eba\u901a\u8fc7\u7528\u6c1f\u4ee3\u78b3\u9178\u4e9a\u4e59\u916f\uff08FEC\uff09\u6dfb\u52a0\u5242\u64cd\u7eb5SEI\u53ef\u4ee5\u5927\u5927\u5ef6\u957fMoS<sub>2<\/sub>\u7684\u5faa\u73af\u5bff\u547d\u3002\u5177\u670910wt\uff05FEC\u7684\u7535\u89e3\u8d28\u4e2d\u7684MoS<sub>2<\/sub>\u57281 A g <sup>-1<\/sup>\u4e0b\u7a33\u5b9a\u5728\u7ea6770mAh g<sup>-1<\/sup> 200\u6b21\u5faa\u73af\uff0c\u5176\u8fdc\u8fdc\u8d85\u8fc7\u65e0FEC\u5bf9\u5e94\u7269\uff08150\u6b21\u5faa\u73af\u540e\u7ea640mAh g<sup>-1<\/sup>\uff09\u3002FEC\u7684\u5b58\u5728\u4f7f\u5f97LiF\u5bcc\u96c6\u7684SEI\u80fd\u591f\u6709\u6548\u5730\u6291\u5236\u6301\u7eed\u7684\u7535\u89e3\u8d28\u5206\u89e3\u3002\u5177\u6709LiNi<sub>0.5<\/sub>Co<sub>0.3<\/sub>Mn<sub>0.2<\/sub>O<sub>2<\/sub>\u6b63\u6781\u7684\u5168\u7535\u6c60\u5728\u542b\u6709FEC\u7684\u7535\u89e3\u8d28\u4e2d\u4e5f\u83b7\u5f97\u6539\u5584\u7684\u6027\u80fd\u3002\u8fd9\u4e9b\u7814\u7a76\u7ed3\u679c\u63ed\u793a\u4e86\u63a7\u5236SEI\u5728MoS<sub>2<\/sub>\u4e0a\u5f62\u6210\u4fc3\u8fdb\u9502\u50a8\u5b58\u7684\u91cd\u8981\u6027\uff0c\u4e3a\u5f00\u53d1\u7528\u4e8eLIB\u7684\u9ad8\u5bb9\u91cf\u7535\u6781\u7684\u91d1\u5c5e\u786b\u5316\u7269\u5f00\u8f9f\u4e86\u65b0\u7684\u9014\u5f84\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/ange.201712907\/full\" target=\"_blank\" rel=\"noopener\">Fluoroethylene Carbonate Enabling a Robust LiF-rich Solid Electrolyte Interphase to Enhance the Stability of the MoS2 Anode for Lithium-Ion Storage<\/a>\uff08Angew. Chem.Int.Ed.,2018,DOI:10.1002\/ange.201712907\uff09<\/p>\n<p><strong>2\u3001<\/strong><strong>Angew. Chem. Int. Ed.\uff1a\u4e0e\u786b\u5316\u7269\u7535\u89e3\u8d28\u517c\u5bb9\u7684\u6709\u673a\u7535\u6781\u6750\u6599\u7528\u4e8e\u7a33\u5b9a\u7684\u5168\u56fa\u6001\u94a0\u7535\u6c60<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-130381\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72471-22.png\" alt=\"\" width=\"580\" height=\"488\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72471-22.png 580w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72471-22-300x252.png 300w\" sizes=\"(max-width: 580px) 100vw, 580px\" \/>\u5177\u6709\u4e0d\u53ef\u71c3\u7535\u89e3\u8d28\u7684\u5168\u56fa\u6001\u94a0\u7535\u6c60\uff08ASSSBs\uff09\u662f\u89e3\u51b3\u9502\u79bb\u5b50\u7535\u6c60\u5b89\u5168\u548c\u6210\u672c\u95ee\u9898\u7684\u6709\u524d\u666f\u7684\u89e3\u51b3\u65b9\u6848\u3002\u7136\u800c\uff0c\u8d85\u79bb\u5b50\u786b\u5316\u7269\u7535\u89e3\u8d28\u7684\u4f4e\u9633\u6781\u5206\u89e3\u7535\u4f4d\u4e0e\u94a0\u79bb\u5b50\u9634\u6781\u7684\u9ad8\u64cd\u4f5c\u7535\u4f4d\u4e4b\u95f4\u56fa\u6709\u7684\u4e0d\u5339\u914d\u5bfc\u81f4\u6b63\u6781-\u7535\u89e3\u8d28\u754c\u9762\u7684\u6325\u53d1\u548c\u4e0d\u7406\u60f3\u7684\u7535\u6c60\u6027\u80fd\u3002\u8fd1\u65e5\uff0c<strong>\u4f11\u65af\u6566\u5927\u5b66Yan Yao\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u7b49\u4eba\u62a5\u9053\u4e86\u4e00\u79cd\u9ad8\u5bb9\u91cf\u7684\u6709\u673a\u6b63\u6781Na<sub>4<\/sub>C<sub>6<\/sub>O<sub>6<\/sub>\uff0c\u5b83\u4e0e\u786b\u5316\u7269\u7535\u89e3\u8d28\u5177\u6709\u5316\u5b66\u548c\u7535\u5316\u5b66\u76f8\u5bb9\u6027\u3002\u5728\u63d2\u5c42\u5316\u5408\u7269\u57faASSSBs\u4e2d\u663e\u793a\u51fa\u9ad8\u6bd4\u5bb9\u91cf\uff08184 mAh g<sup>-1<\/sup>\uff09\u548c\u6700\u9ad8\u6bd4\u80fd\u91cf\u4e4b\u4e00\uff08395 Wh kg<sup>-1<\/sup>\uff09\u3002\u57280.2C\u4e0b400\u6b21\u5faa\u73af\u540e\u5bb9\u91cf\u4fdd\u6301\u7387\u4e3a70\uff05\uff0c0.1C 100\u6b21\u5faa\u73af\u540e\u5bb9\u91cf\u4fdd\u6301\u7387\u4e3a76\uff05\u3002 \u6b64\u5916\uff0cNa<sub>4<\/sub>C<sub>6<\/sub>O<sub>6<\/sub>\u53ef\u7528\u4f5c\u8d1f\u6781\u6750\u6599\uff0c\u4f7f\u5bf9\u79f0\u7684\u5168\u6709\u673aASSSBs\u4e2d\u7684\u9634\u6781\u548c\u9633\u6781\u6750\u6599\u90fd\u6709Na<sub>4<\/sub>C<sub>6<\/sub>O<sub>6<\/sub>\u5b58\u5728\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/anie.201712895\/full\" target=\"_blank\" rel=\"noopener\">Tailored Organic Electrode Material Compatible with Sulfide Electrolyte for Stable All-Solid-State Sodium Batteries<\/a>\uff08Angew. Chem. Int. Ed.,2018,DOI:<span class=\"article-header__meta-info-data\">10.1002\/anie.201712895<\/span>\uff09<\/p>\n<p><strong>3\u3001Advanced Functional Materials\uff1a\u6c27\u5316\u77f3\u58a8\u70ef\u5bf9Li\u679d\u6676\u7535\u9540\u7684\u534f\u540c\u589e\u6548\u4f5c\u7528<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-130383\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72472-21.png\" alt=\"\" width=\"600\" height=\"315\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72472-21.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72472-21-300x158.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u9502\uff08Li\uff09\u7684\u6811\u679d\u72b6\u751f\u957f\u4e25\u91cd\u963b\u788d\u4e86\u9502\u91d1\u5c5e\u7535\u6c60\u7684\u5b9e\u9645\u5e94\u7528\u3002\u8fd1\u65e5\uff0c<strong>\u4f0a\u5229\u8bfa\u4f0a\u5927\u5b66\u829d\u52a0\u54e5\u5206\u6821Reza Shahbazian-Yassar\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u7b49\u4eba\u62a5\u9053\u4e86\u4e00\u79cd\u4e09\u7ef4\u4fdd\u5f62\u7684\u6c27\u5316\u77f3\u58a8\u70ef\u7eb3\u7c73\u7247\uff08GOn\uff09\u6d82\u5c42\uff0c\u5b83\u88ab\u9650\u5236\u5728\u4e00\u4e2a\u73bb\u7483\u7ea4\u7ef4\u9694\u79bb\u5c42\u7684\u7ec7\u9020\u7ed3\u6784\u4e2d\uff0c\u4ece\u800c\u5141\u8bb8\u9502\u79bb\u5b50\u4ee5\u5176\u7ed3\u6784\u7684\u65b9\u5f0f\u4f20\u8f93\uff0c\u540c\u65f6\u8c03\u8282Li\u7684\u6c89\u79ef\u3002\u7535\u5316\u5b66\u6d4b\u91cf\u663e\u793a\u9502\u91d1\u5c5e\u9633\u6781\u7684\u5faa\u73af\u5bff\u547d\u548c\u7a33\u5b9a\u6027\u663e\u8457\u63d0\u9ad8\uff0c\u8fd9\u53ef\u4ee5\u901a\u8fc7\u5404\u79cd\u663e\u5fae\u955c\u548c\u6a21\u62df\u7ed3\u679c\u6765\u89e3\u91ca\u3002\u5229\u7528\u626b\u63cf\u7535\u5b50\u663e\u5fae\u955c\uff0c\u805a\u7126\u79bb\u5b50\u675f\u548c\u5149\u5b66\u6210\u50cf\uff0c\u63ed\u793a\u4e86\u5728GO\u6539\u6027\u6837\u54c1\u7684\u60c5\u51b5\u4e0b\u5728\u7535\u6781\u8868\u9762\u4e0a\u5f62\u6210\u5747\u5300\u7684Li\u819c\u3002\u4ece\u5934\u7b97\u5206\u5b50\u52a8\u529b\u5b66\uff08AIMD\uff09\u6a21\u62df\u8868\u660e\uff0c\u9502\u79bb\u5b50\u6700\u521d\u5438\u9644\u5230\u4eb2\u9502\u79bb\u5b50GOn\uff0c\u7136\u540e\u901a\u8fc7\u7f3a\u9677\u4f4d\u70b9\u6269\u6563\u3002\u8fd9\u79cd\u5ef6\u8fdf\u7684Li\u8f6c\u79fb\u6d88\u9664\u4e86\u5bfc\u81f4\u66f4\u5747\u5300\u7684Li\u6210\u6838\u7684\u201c\u5c16\u7aef\u6548\u5e94\u201d\u3002\u8fd9\u79cd\u65b0\u7684\u8ba4\u8bc6\u662f2D\u6750\u6599\u8c03\u8282Li\u6c89\u79ef\u8fc8\u51fa\u7684\u91cd\u8981\u4e00\u6b65\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adfm.201705917\/full\" target=\"_blank\" rel=\"noopener\">Synergistic Effect of Graphene Oxide for Impeding the Dendritic Plating of Li<\/a>\uff08Adv.Funct.Mater., 2018, DOI:<span class=\"article-header__meta-info-data\">10.1002\/adfm.201705917<\/span>\uff09<\/p>\n<p><strong>4\u3001Angew. Chem.Int.Ed.\uff1a\u9502\u7a7a\u6c14\u7535\u6c60\u7684\u81f4\u547d\u5f31\u70b9\uff1a\u78b3\u9178\u9502<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-130386\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72474-18.png\" alt=\"\" width=\"600\" height=\"395\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72474-18.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72474-18-300x198.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u9502-\u7a7a\u6c14\u7535\u6c60\uff08LAB\uff09\u88ab\u8ba4\u4e3a\u662f\u7406\u60f3\u7684\u80fd\u91cf\u5b58\u50a8\u88c5\u7f6e\uff0c\u56e0\u4e3a\u5176\u5728\u6240\u6709\u5df2\u77e5\u7535\u6c60\u4e2d\u5177\u6709\u6700\u9ad8\u7684\u7406\u8bba\u6bd4\u80fd\u91cf\u3002\u7136\u800c\uff0c\u5bc4\u751f\u53cd\u5e94\u4f1a\u5bf9LAB\u7684\u6548\u7387\u548c\u5bff\u547d\u4ea7\u751f\u4ee4\u4eba\u5934\u75db\u7684\u95ee\u9898\uff0c\u5176\u4e2d\u78b3\u9178\u9502Li<sub>2<\/sub>CO<sub>3<\/sub>\u7684\u5f62\u6210\u548c\u5206\u89e3\u662f\u6700\u91cd\u8981\u7684\u3002Li<sub>2<\/sub>CO<sub>3<\/sub>\u4f5c\u4e3a\u78b3\u9178\u76d0\u57fa\u7535\u89e3\u8d28\u4e2d\u7684\u4e3b\u8981\u653e\u7535\u4ea7\u7269\u7684\u53d1\u73b0\u66fe\u7ecf\u4f7f\u7814\u7a76\u4eba\u5458\u57282010\u5e74\u521d\u5f00\u59cb\u51fa\u73b0\u201c\u7530\u56ed\u8bd7\u822c\u7684\u7ed3\u5c40\u201d\u3002\u5728\u8fc7\u53bb\u7684\u51e0\u5e74\u4e2d\uff0c\u4e3a\u4e86\u7406\u89e3Li<sub>2<\/sub>CO<sub>3<\/sub>\u7684\u5f62\u6210\u548c\u5206\u89e3\u673a\u5236\u4ee5\u53ca\u6784\u60f3\u65b0\u7684\u5316\u5b66\/\u6750\u6599\u7b56\u7565\u6765\u6291\u5236Li<sub>2<\/sub>CO<sub>3<\/sub>\u7684\u5f62\u6210\u5e76\u4fc3\u8fdbLi<sub>2<\/sub>CO<sub>3<\/sub>\u5206\u89e3\uff0c\u5df2\u505a\u51fa\u4e86\u5de8\u5927\u52aa\u529b\u3002\u800c\u4e14\uff0cLABs\u4e2dLi<sub>2<\/sub>CO<sub>3<\/sub>\u7684\u7814\u7a76\u6b63\u5728\u5f00\u62d3\u80fd\u6e90\u6280\u672f\u9886\u57df\u7684\u65b0\u7814\u7a76\u9886\u57df\u3002\u8003\u8651\u5230\u5feb\u901f\u53d1\u5c55\u548c\u65e0\u6570\u65b0\u5174\u95ee\u9898\uff0c<strong>\u4e2d\u79d1\u9662\u957f\u6625\u5e94\u5316\u6240\u5f6d\u7ae0\u6cc9\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u7b49\u4eba\u91cd\u65b0\u6982\u62ec\u5f53\u524d\u7684\u8ba4\u8bc6\uff0c\u786e\u5b9a\u6a21\u7cca\u6027\u548c\u79d1\u5b66\u5dee\u8ddd\uff0c\u5e76\u8ba8\u8bba\u4e86\u4eca\u540e\u7814\u7a76\u7684\u65b9\u5411\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/anie.201710156\/full\" target=\"_blank\" rel=\"noopener\">Achilles\u2019 Heel of Lithium\u2013Air Batteries: Lithium Carbonate<\/a>\uff08Angew. Chem. Int. Ed.,2018,DOI:<span class=\"article-header__meta-info-data\">10.1002\/anie.201710156<\/span>\uff09<\/p>\n<p><strong>5\u3001ACS Nano\uff1a\u7528\u4e8e\u589e\u5f3a\u578b\u7535\u5316\u5b66\u94a0\u79bb\u5b50\u8d2e\u5b58\u7684Ni<sub>3<\/sub>S<sub>4<\/sub>\u7eb3\u7c73\u68d2\u7684\u5408\u7406\u5408\u6210\u548c\u7ec4\u88c5<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-130390\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/5-1.gif\" alt=\"\" width=\"500\" height=\"376\" \/><\/p>\n<p>\u867d\u7136\u4e3b\u5f20\u4f5c\u4e3a\u5f53\u524d\u9502\u79bb\u5b50\u6280\u672f\u7684\u6f5c\u5728\u4f4e\u6210\u672c\u66ff\u4ee3\u54c1\uff0c\u4f46\u94a0\u79bb\u5b50\u7535\u6c60\u7684\u5b9e\u9645\u53ef\u884c\u6027\u4ecd\u7136\u662f\u865a\u5e7b\u7684\uff0c\u5e76\u53d6\u51b3\u4e8e\u9ad8\u6027\u80fd\u7535\u6781\u6750\u6599\u7684\u53d1\u5c55\u3002\u76ee\u524d\u53ef\u7528\u7684\u5019\u9009\u6750\u6599\u5f88\u5c11\u80fd\u591f\u540c\u65f6\u6ee1\u8db3\u5bb9\u91cf\uff0c\u901f\u7387\u80fd\u529b\u548c\u5faa\u73af\u5bff\u547d\u7684\u8981\u6c42\u3002\u8fd1\u65e5\uff0c<strong>\u82cf\u5dde\u5927\u5b66\u674e\u5f66\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u56e2\u961f\u62a5\u9053\u4e86\u4e00\u79cd\u9ad8\u6e29\u6eb6\u6db2\u6cd5\u5236\u5907\u5c3a\u5bf8\u5747\u5300\u7684Ni<sub>3<\/sub>S<sub>4<\/sub>\u7eb3\u7c73\u68d2\u3002\u8fd9\u4e9b\u80f6\u4f53\u7eb3\u7c73\u68d2\u5bb9\u6613\u81ea\u7ec4\u88c5\uff0c\u5e76\u5f62\u6210\u5fae\u89c2\u7684\u8d85\u7ed3\u6784\uff0c\u8fd9\u4e0d\u5e78\u5730\u5426\u5b9a\u4e86\u5355\u4e2a\u7eb3\u7c73\u68d2\u7684\u7eb3\u7c73\u7ea7\u7279\u5f81\u3002\u4e3a\u6b64\uff0c\u8fdb\u4e00\u6b65\u5f15\u5165\u4e8c\u7ef4\u77f3\u58a8\u70ef\u7eb3\u7c73\u7247\u4f5c\u4e3a\u95f4\u9694\u7269\u6765\u4e2d\u65ad\u7eb3\u7c73\u68d2\u81ea\u7ec4\u88c5\u3002\u5408\u6210\u7684\u590d\u5408\u6750\u6599\u5728Na<sup>+<\/sup>\u7684\u7535\u5316\u5b66\u50a8\u5b58\u65b9\u9762\u5177\u6709\u660e\u663e\u7684\u4f18\u52bf\u3002\u8bc1\u660e\u5728\u534a\u7535\u6c60\u4e2d\u5b83\u8868\u73b0\u51fa\u8d85\u8fc7600mAh\/g\u7684\u5927\u7684\u53ef\u9006\u6bd4\u5bb9\u91cf\uff0c\u9ad8\u901f\u7387\u80fd\u529b\uff0c\u4fdd\u6301\u57284 A\/g\u65f6&gt; 300 mAh\/g\uff0c\u5e76\u4e14\u5728\u4e0d\u540c\u7535\u6d41\u901f\u7387\u4e0b\u5faa\u73af\u5bff\u547d\u957f\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/pubs.acs.org\/doi\/10.1021\/acsnano.7b08625\" target=\"_blank\" rel=\"noopener\">Rational Synthesis and Assembly of Ni3S4 Nanorods for Enhanced Electrochemical Sodium Ion Storage<\/a>\uff08ACS Nano,2018,DOI:10.1021\/acsnano.7b08625\uff09<\/p>\n<p><strong>6\u3001Advanced Energy Materials\uff1a\u7528\u4e8e\u9ad8\u7a33\u5b9a\u94a0\u91d1\u5c5e\u9633\u6781\u76843D\u67d4\u6027\u78b3\u6be1\u4e3b\u4f53<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-130403\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/201802012F10.1002_aenm.201702764.jpg\" alt=\"\" width=\"433\" height=\"389\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/201802012F10.1002_aenm.201702764.jpg 433w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/201802012F10.1002_aenm.201702764-300x270.jpg 300w\" sizes=\"(max-width: 433px) 100vw, 433px\" \/><\/p>\n<p>\u5177\u6709\u9ad8\u7406\u8bba\u5bb9\u91cf\u548c\u6700\u4f4e\u7535\u5316\u5b66\u7535\u4f4d\u7684\u94a0\uff08Na\uff09\u91d1\u5c5e\u88ab\u8ba4\u4e3a\u662f\u7528\u4e8e\u94a0\u91d1\u5c5e\u7535\u6c60\u7684\u6709\u524d\u666f\u7684\u8d1f\u6781\u6750\u6599\u3002\u7136\u800c\uff0cNa\u7684\u679d\u6676\u751f\u957f\u548c\u5faa\u73af\u4e2d\u7684\u5927\u4f53\u79ef\u53d8\u5316\u4e25\u91cd\u963b\u788d\u4e86\u5176\u5b9e\u9645\u5e94\u7528\u3002\u8fd1\u65e5\uff0c<strong>\u5317\u4eac\u79d1\u6280\u5927\u5b66\u8303\u4e3d\u73cd\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u7b49\u4eba\u8868\u660e\u5df2\u7ecf\u5927\u89c4\u6a21\u5546\u4e1a\u5316\u76843D\u67d4\u6027\u78b3\uff08C\uff09\u6be1\u53ef\u4ee5\u7528\u4e8e\u901a\u8fc7\u7194\u878d\u6ce8\u5165\u7b56\u7565\u9884\u5b58Na\u7684\u4e3b\u4f53\uff0c\u901a\u8fc7\u8be5\u6ce8\u5165\u7b56\u7565\u83b7\u5f97Na\/C\u590d\u5408\u8d1f\u6781\u3002\u7531\u4e8e\u91d1\u5c5eNa\u88ab\u9650\u5236\u5728\u5bfc\u7535\u78b3\u6be1\u4e3b\u4f53\u4e2d\uff0c\u6240\u4ee5\u5f97\u5230\u7684\u8d1f\u6781\u5728\u5bf9\u79f0\u7535\u6c60\u4e2d\u7684\u78b3\u9178\u76d0\u57fa\u7535\u89e3\u8d28\u4e2d\u8868\u73b0\u51fa\u7a33\u5b9a\u7684\u7535\u538b\u5206\u5e03\u548c120\u6b21\u5faa\u73af\u7684\u5c0f\u6ede\u540e\uff0c\u8fd9\u589e\u52a0\u4e86Na<sup>+<\/sup>\u6c89\u79ef\u4f4d\u70b9\u4ee5\u964d\u4f4e\u6709\u6548\u7535\u6d41\u5bc6\u5ea6\u5e76\u4f7fNa\u5f62\u6838\u5747\u5300\uff0c\u4ece\u800c\u9650\u5236\u7535\u5316\u5b66\u5faa\u73af\u4e2d\u7684\u5c3a\u5bf8\u53d8\u5316\u3002\u66f4\u91cd\u8981\u7684\u662f\uff0c\u53ef\u4ee5\u6709\u6548\u6291\u5236\u94a0\u679d\u6676\u751f\u957f\u548c\u5927\u4f53\u79ef\u53d8\u5316\u3002\u5f53\u4e0eNa<sub>0.67<\/sub>Ni<sub>0.33<\/sub>Mn<sub>0.67<\/sub>O<sub>2<\/sub>\u6b63\u6781\u7ed3\u5408\u65f6\uff0cNa\/C\u590d\u5408\u6750\u6599\u5728\u5168\u7535\u6c60\u4e2d\u8868\u73b0\u51fa\u826f\u597d\u7684\u9002\u7528\u6027\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/wol1\/doi\/10.1002\/aenm.201702764\/abstract\" target=\"_blank\" rel=\"noopener\">3D Flexible Carbon Felt Host for Highly Stable Sodium Metal Anodes<\/a>\uff08Adv.Energy.Mater. ,2018, DOI:10.1002\/aenm.201702764\uff09<\/p>\n<p><strong>7\u3001Advanced Energy Materials\uff1a\u4f7f\u7528\u6a21\u677f\u6cd5\u548c\u653e\u7535\u7b49\u79bb\u5b50\u70e7\u7ed3\u6280\u672f\u5236\u9020\u7684\u9502\u79bb\u5b50\u7535\u6c60\u7528\u65e0\u7c98\u5408\u5242\u539a\u7535\u6781\u663e\u793a\u51fa\u9ad8\u9762\u79ef\u5bb9\u91cf<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-130400\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72475-13.png\" alt=\"\" width=\"600\" height=\"316\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72475-13.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72475-13-300x158.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u6a21\u677f\u6cd5\u662f\u4e00\u79cd\u7528\u4e8e\u5236\u5907\u5177\u6709\u4e92\u76f8\u63a7\u5236\u826f\u597d\u7684\u5b54\u5f84\u548c\u5f62\u6001\u7684\u591a\u5b54\u7535\u6781\u7684\u6709\u6548\u65b9\u6cd5\u3002\u5b54\u7ed3\u6784\u8bbe\u8ba1\u7684\u4f18\u5316\u4fc3\u8fdb\u4e86\u7535\u89e3\u8d28\u6e17\u900f\u5e76\u4e3a\u9502\u79bb\u5b50\u63d0\u4f9b\u4e86\u5feb\u901f\u6269\u6563\u8def\u5f84\uff0c\u8fd9\u5bf9\u4e8e\u591a\u5b54\u7535\u6781\u66f4\u4e3a\u91cd\u8981\u3002\u8fd1\u65e5\uff0c<strong>\u76ae\u5361\u7b2c\u5112\u52d2-\u51e1\u5c14\u7eb3\u5927\u5b66Arnaud Demorti\u00e8re\u3001Vincent Seznec\uff08\u5171\u540c\u901a\u8baf\uff09<\/strong>\u7b49\u4eba\u4f7f\u7528\u653e\u7535\u7b49\u79bb\u5b50\u70e7\u7ed3\u6280\u672f\uff0c\u5c06NaCl\u5fae\u7c73\u9897\u7c92\u7528\u4f5c\u5236\u59071mm\u539a\u7684\u591a\u5b54LiFePO<sub>4<\/sub>\u548cLi<sub>4<\/sub> Ti<sub>5<\/sub>O<sub>12<\/sub>\u590d\u5408\u7535\u6781\u7684\u6a21\u677f\u5242\u3002\u8fd9\u4e9b\u65e0\u70e7\u7ed3\u7c98\u5408\u5242\u7684\u7535\u6781\u662f\u81ea\u652f\u6491\u7684\u5e76\u4e14\u5177\u6709\u76f8\u5bf9\u5747\u5300\u5b54\u9699\u7684\u5927\u5b54\u9699\u7387\uff0840\uff05\uff09\u3002\u534a\u7535\u6c60\u548c\u5168\u7535\u6c60\u7684\u7535\u5316\u5b66\u6027\u80fd\u8868\u73b0\u51fa\u660e\u663e\u7684\u6bd4\u5bb9\u91cf\uff0820 mA h cm<sup>-2<\/sup>\uff09\uff0c\u6bd4\u4f20\u7edf\u9502\u79bb\u5b50\u7535\u6c60\uff085 mA h cm<sup>-2<\/sup>\uff09\u4e2d\u7684100\u03bcm\u539a\u7535\u6781\u9ad84\u500d\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/wol1\/doi\/10.1002\/aenm.201703031\/abstract\" target=\"_blank\" rel=\"noopener\">Thick Binder-Free Electrodes for Li\u2013Ion Battery Fabricated Using Templating Approach and Spark Plasma Sintering Reveals High Areal Capacity<\/a>\uff08Adv.Energy.Mater.,2018,DOI:10.1002\/aenm.201703031\uff09<\/p>\n<p><strong>8\u3001Advanced Energy Materials\uff1a\u9530\u5bf9\u94dd\u5728\u9502\u79bb\u5b50\u7535\u6c60\u5c42\u72b6\u6c27\u5316\u7269\u6b63\u6781\u957f\u671f\u53ef\u5faa\u73af\u6027\u7684\u7efc\u5408\u8bc4\u4f30<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-130401\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72476-10.png\" alt=\"\" width=\"600\" height=\"254\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72476-10.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72476-10-300x127.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u7531LiNi<sub>1-x-y<\/sub>Co<sub>x<\/sub>Mn<sub>y<\/sub>O<sub>2<\/sub>\uff08NCM\uff0c\uff081-x-y\uff09\u22650.6\uff09\u7ec4\u6210\u7684\u5bcc\u954d\u5c42\u72b6\u6c27\u5316\u7269\u6b63\u6781\u6536\u5230\u5e7f\u6cdb\u5173\u6ce8\uff0c\u5176\u53ef\u7528\u4e8e\u7535\u52a8\u6c7d\u8f66\u7684\u9ad8\u80fd\u91cf\u5bc6\u5ea6\u7535\u6c60\u3002\u4f46\u662f\uff0c\u76ee\u524d\u7f3a\u4e4f\u5bf9\u5176\u7535\u5316\u5b66\u8010\u4e45\u6027\u7684\u7efc\u5408\u8bc4\u4f30\u3002\u8fd1\u65e5\uff0c<strong>\u5fb7\u514b\u8428\u65af\u5927\u5b66\u5965\u65af\u6c40\u5206\u6821Arumugam Manthiram\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u7b49\u4eba\u5728\u4e24\u4e2a\u5185\u90e8\u6b63\u6781LiNi<sub>0.8<\/sub>Co<sub>0.15<\/sub>Al<sub>0.05<\/sub>O<sub>2<\/sub>\u548cLiNi<sub>0.7<\/sub>Co<sub>0.15<\/sub>Mn<sub>0.15<\/sub>O<sub>2<\/sub>\u5728\u9ad8\u538b\u77f3\u58a8\u5168\u7535\u6c60\u4e2d\u8fdb\u884c\u4e861500\u6b21\u5145\u653e\u7535\u5faa\u73af\uff08\u8f66\u8f86\u4f7f\u7528\u5bff\u547d\u7ea6\u4e3a5 &#8211; 10\u5e74\uff09\u7684\u7814\u7a76\u3002\u5c3d\u7ba1\u954d\u542b\u91cf\u8f83\u4f4e\uff0cNCM\u8868\u73b0\u51fa\u6bd4NCA\u66f4\u9ad8\u7684\u6027\u80fd\u52a3\u5316\u3002\u5173\u952e\u7684\u964d\u89e3\u8fc7\u7a0b\uff0c\u5305\u62ec\u5316\u5b66\uff0c\u7ed3\u6784\u548c\u673a\u68b0\u65b9\u9762\uff0c\u90fd\u662f\u901a\u8fc7\u4e00\u7cfb\u5217\u8868\u5f81\u6280\u672f\u8fdb\u884c\u5206\u6790\u7684\u3002\u603b\u4f53\u800c\u8a00\uff0cMn\u53d6\u4ee3\u5728\u6291\u5236\u5c42\u72b6\u6c27\u5316\u7269\u9634\u6781\u7684\u6d3b\u6027\u8d28\u91cf\u6eb6\u89e3\u548c\u4e0d\u53ef\u9006\u76f8\u53d8\u65b9\u9762\u4f3c\u4e4e\u8fdc\u4e0d\u5982Al\u6709\u6548\u3002\u6d3b\u6027\u8d28\u91cf\u6eb6\u89e3\u52a0\u901f\u4e86\u77f3\u58a8\u8d1f\u6781\u4e0a\u7684\u5bc4\u751f\u53cd\u5e94\uff0c\u4ece\u800c\u52a0\u901f\u4e86\u5bb9\u91cf\u4e0b\u964d\uff0c\u800c\u76f8\u53d8\u4e3b\u8981\u5bfc\u81f4\u7535\u6c60\u7535\u963b\u589e\u52a0\u548c\u7535\u538b\u8870\u51cf\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/wol1\/doi\/10.1002\/aenm.201703154\/abstract\" target=\"_blank\" rel=\"noopener\">Mn versus Al in Layered Oxide Cathodes in Lithium-Ion Batteries: A Comprehensive Evaluation on Long-Term Cyclability\uff08<\/a>Adv.Energy.Mater.,2018,DOI:10.1002\/aenm.201703154\uff09<\/p>\n<p><strong>9\u3001Advanced Functional Materials\uff1a\u94a0\u79bb\u5b50\u7535\u6c60\uff1a\u901a\u8fc7\u7528\u78f7\u9178\u94a0\u6539\u6027\u8868\u9762\u6765\u957f\u671f\u5faa\u73af\u5236\u9020\u6709\u6548\u7684\u5c42\u72b6\u6b63\u6781\u6750\u6599<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-130402\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72477-7.png\" alt=\"\" width=\"600\" height=\"363\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72477-7.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/\u56fe\u72477-7-300x182.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u6b63\u6781\u6750\u6599\u7684\u8868\u9762\u7a33\u5b9a\u5316\u662f\u786e\u4fdd\u957f\u671f\u53ef\u5faa\u73af\u6027\u7684\u5173\u952e\uff0c\u5e76\u4e14\u5728\u4f7f\u7528\u8150\u8680\u6027Na\u57fa\u7535\u89e3\u8d28\u7684Na\u7535\u6c60\u4e2d\u662f\u5f88\u91cd\u8981\u7684\u3002\u8fd1\u65e5\uff0c<strong>\u97e9\u56fd\u4e16\u5b97\u5927\u5b66Seung-Taek Myung\u3001\u6c49\u9633\u5927\u5b66Yang-Kook Sun\uff08\u5171\u540c\u901a\u8baf\uff09<\/strong>\u7b49\u4eba\u5c06P2\u578b\u5c42\u72b6Na<sub>2\/3<\/sub> [Ni<sub>1\/3<\/sub>Mn<sub>2\/3<\/sub>] O<sub>2<\/sub>\u7684\u8868\u9762\u7ecf\u79bb\u5b50\u5bfc\u7535\u78f7\u9178\u94a0\uff08NaPO<sub>3<\/sub>\uff09\u7eb3\u7c73\u5c42\u6539\u6027\uff0c\u224810nm\u539a\uff0c\u7ecf300\u2103\u7194\u878d\u6d78\u6e0d;\u7eb3\u7c73\u5c42\u7531NH<sub>4<\/sub>H<sub>2<\/sub>PO<sub>4<\/sub>\u4e0e\u8868\u9762\u94a0\u6b8b\u57fa\u7684\u53cd\u5e94\u81ea\u53d1\u5f62\u6210\u3002\u5c3d\u7ba1\u6750\u6599\u7531\u4e8e\u4ece4V\u76f8\u5bf9\u4e8eNa<sup>+<\/sup>\/Na\u8f6c\u53d8\u6210P2\u5230O2\u76f8\u800c\u5728c\u8f74\u4e0a\u5177\u6709\u5927\u7684\u5404\u5411\u5f02\u6027\u53d8\u5316\uff0c\u4f46NaPO<sub>3<\/sub>\u6d82\u8986\u7684Na<sub>2\/3<\/sub> [Ni<sub>1\/3<\/sub>Mn<sub>2\/3<\/sub>] O<sub>2<\/sub>\u5168\u7535\u6c60\u5728300\u6b21\u5faa\u73af\u4e2d\u8868\u73b0\u51fa73\uff05\u4f18\u5f02\u7684\u5bb9\u91cf\u4fdd\u6301\u7387\u3002\u8868\u9762NaPO<sub>3<\/sub>\u7eb3\u7c73\u5c42\u901a\u8fc7\u6e05\u9664\u7535\u89e3\u8d28\u4e2d\u7684HF\u548cH<sub>2<\/sub>O\u800c\u5bf9\u7535\u6c60\u6027\u80fd\u4ea7\u751f\u79ef\u6781\u5f71\u54cd\uff0c\u5bfc\u81f4\u6b63\u6781\u8868\u9762\u4e0a\u526f\u4ea7\u7269\u5f62\u6210\u8f83\u5c11\uff0c\u8fd9\u964d\u4f4e\u4e86\u7535\u6c60\u7535\u963b\u3002\u65f6\u95f4\u5206\u8fa8\u539f\u4f4d\u9ad8\u6e29X\u5c04\u7ebf\u884d\u5c04\u7814\u7a76\u8868\u660e\uff0cNaPO<sub>3<\/sub>\u6d82\u5c42\u5ef6\u8fdf\u5206\u89e3\u6210Mn<sub>3<\/sub>O<sub>4<\/sub>\uff0c\u7531\u6b64\u6291\u5236\u9ad8\u5ea6\u8131\u6eb6\u89e3\u72b6\u6001\u4e0b\u7684\u6c27\u91ca\u653e\uff0c\u4ece\u800c\u5ef6\u8fdf\u653e\u70ed\u5206\u89e3\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adfm.201705968\/full\" target=\"_blank\" rel=\"noopener\">Sodium-Ion Batteries: Building Effective Layered Cathode Materials with Long-Term Cycling by Modifying the Surface via Sodium Phosphate<\/a>\uff08Adv.Funct.Mater.,2018,DOI:<span class=\"article-header__meta-info-data\">10.1002\/adfm.201705968\uff09<\/span><\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u65b0\u80fd\u6e90\u7ec4Allen\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u6574\u7406\u7f16\u8f91\u3002<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u8fd9\u91cc\u6c47\u96c6\u4e86\u5404\u5927\u9ad8\u6821\u7855\u535a\u751f\u3001\u4e00\u7ebf\u79d1\u7814\u4eba\u5458\u4ee5\u53ca\u884c\u4e1a\u4ece\u4e1a\u8005\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\" target=\"_blank\" rel=\"noopener\">\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8\u5927\u5bb6\u5ead<\/a>\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n<p><strong><b>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaokefu\u3002<br \/>\n <\/b><\/strong><\/p>\n<p><strong>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<\/strong><a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener\"><strong>\u6d4b\u8bd5\u8c37<\/strong><\/a><strong>\uff01<\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u672c\u671f\u91d1\u5c5e\u79bb\u5b50\u7535\u6c60\u7d20\u6750\u7684\u53d1\u8868\u65f6\u95f4\u4ece2018\u5e741\u670831\u65e5\u52302018\u5e743\u67085\u65e5\u3002\u6d89\u53ca\u6539\u5584\u7535\u89e3\u8d28\u754c\u9762\u3001\u5168\u56fa\u6001\u94a0\u7535\u6c60\u3001\u9502\u679d\u6676\u7b49\u65b9\u5411\u3002 1\u3001Angew. Chem.Int&#8230;.<\/p>\n","protected":false},"author":349,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2810],"tags":[2548,2980],"class_list":["post-130321","post","type-post","status-publish","format-standard","hentry","category-huizong","tag-2548","tag-2980"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/130321"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/349"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=130321"}],"version-history":[{"count":10,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/130321\/revisions"}],"predecessor-version":[{"id":139162,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/130321\/revisions\/139162"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=130321"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=130321"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=130321"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}