{"id":13056,"date":"2016-05-13T17:00:34","date_gmt":"2016-05-13T09:00:34","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=13056"},"modified":"2016-05-13T17:48:55","modified_gmt":"2016-05-13T09:48:55","slug":"%e5%9b%bd%e5%86%85%e9%ab%98%e8%b4%a8%e9%87%8f%e5%ad%a6%e6%9c%af%e8%bf%9b%e5%b1%95%e6%b1%87%e6%80%bb%e5%8c%97%e4%ba%ac%e5%a4%a7%e5%ad%a6%e7%a0%94%e5%8f%91%e5%87%ba%e5%be%ae%e5%9e%8b%e7%9f%b3%e5%a2%a8","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=13056","title":{"rendered":"#\u56fd\u5185\u9ad8\u8d28\u91cf\u5b66\u672f\u8fdb\u5c55\u6c47\u603b#\u5317\u4eac\u5927\u5b66\u7814\u53d1\u51fa\u5fae\u578b\u77f3\u58a8\u70ef\u8584\u819c\u706f\u4e1d\u70ed\u7535\u5b50\u53d1\u5c04\u5668"},"content":{"rendered":"<p><strong>\u56fd\u5185\u5468\u62a5\u7b2c45\u671f\u6458\u8981\uff1a<\/strong>\u5317\u4eac\u5927\u5b66\u7814\u7a76\u56e2\u961f\u4f7f\u7528\u5fae\u52a0\u5de5\u5236\u9020\u65b9\u6cd5\u7814\u53d1\u51fa\u4ee5\u5fae\u5c3a\u5ea6\u77f3\u58a8\u70ef\u8584\u819c\u4f5c\u4e3a\u706f\u4e1d\u7684\u5fae\u578b\u70ed\u7535\u5b50\u53d1\u5c04\u5668\uff1b\u6e05\u534e\u5927\u5b66\u8fd0\u7528\u5bc6\u5ea6\u6cdb\u51fd\u6570\u7406\u8bba\u9a8c\u8bc1N\u6216O\u63ba\u6742\u53ef\u6709\u6548\u6291\u5236\u9502\u786b\u7535\u6c60\u7684\u98de\u68ad\u6548\u5e94\uff1b\u4e2d\u79d1\u5927\u7814\u5236\u51faTe\u7eb3\u7c73\u7ebf\/\u78b3\u7eb3\u7c73\u7ba1\u590d\u5408\u9634\u6781\u6750\u6599\u78b2\u7535\u6781\u9502\u7535\u6c60\uff1b\u4e2d\u56fd\u5de5\u7a0b\u7269\u7406\u7814\u7a76\u9662\u7b49\u673a\u6784\u5236\u5907\u51fa\u4e2d\u7a7a\u77f3\u58a8\u70ef\/\u5bfc\u7535\u805a\u5408\u7269\u590d\u5408\u7ea4\u7ef4\u5e76\u5c06\u5176\u7528\u4e8e\u5236\u9020\u65b0\u578b\u7ea4\u7ef4\u72b6\u7684\u8d85\u7ea7\u7535\u5bb9\u5668\uff1b\u5317\u4eac\u5de5\u4e1a\u5927\u5b66\u7b49\u9ad8\u6821\u7684\u7814\u7a76\u8005\u5236\u5907\u51fa\u9ad8\u5ea6\u7a33\u5b9a\u7684\u9506\u57faMOFs\u4ee5\u68c0\u6d4b\u548c\u53bb\u9664\u5e9f\u6c34\u4e2d\u7684\u6297\u751f\u7d20\u548c\u6709\u673a\u70b8\u836f\uff1b\u53a6\u95e8\u5927\u5b66\u5229\u7528\u9633\u79bb\u5b50\u4ea4\u6362\u53cd\u5e94\u6784\u5efa\u4e86\u5177\u6709\u4e0d\u540c\u5f62\u72b6\u7684Mn2+\u548cZn2+\u6c27\u5316\u94c1\u7eb3\u7c73\u9897\u7c92\uff1b\u4e2d\u79d1\u9662\u7406\u5316\u6280\u672f\u7814\u7a76\u6240\u5236\u5907\u51fa\u65b0\u578b\u7852\u6c5e\u5316\u7269BaHgSe2\uff1b\u4e2d\u79d1\u9662\u82cf\u5dde\u7eb3\u7c73\u6240\u91c7\u7528\u57fa\u4e8e\u79bb\u6563\u5076\u6781\u5b50\u8fd1\u4f3c\u65b9\u6cd5\u7814\u7a76\u4e86\u91d1\u5c5e\u56e2\u7c07\u5438\u9644\u5bf9\u7b49\u79bb\u5b50\u5171\u632f\u963b\u5c3c\u7684\u5f71\u54cd\uff0c\u7ed3\u679c\u8868\u660e\u963b\u5c3c\u4e3b\u8981\u662f\u7531\u7eb3\u7c73\u68d2\u4e24\u8fb9\u7684\u5438\u9644\u4ea7\u751f\u3002<\/p>\n<p><span style=\"color: #ff6600;\"><strong>\u3010\u6750\u6599\u725b\u91cd\u70b9\u5173\u6ce8\u3011<\/strong><\/span><\/p>\n<p><strong>\u5317\u4eac\u5927\u5b66\u7814\u53d1\u51fa\u5fae\u578b\u77f3\u58a8\u70ef\u8584\u819c\u706f\u4e1d\u70ed\u7535\u5b50\u53d1\u5c04\u5668<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-13068\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/10.jpg\" alt=\"10\" width=\"595\" height=\"257\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/10.jpg 595w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/10-300x130.jpg 300w\" sizes=\"(max-width: 595px) 100vw, 595px\" \/><\/p>\n<p>\u5fae\u52a0\u5de5\u7684\u7535\u5b50\u53d1\u5c04\u5668\u7531\u4e8e\u5176\u5728\u771f\u7a7a\u7535\u5b50\u4ea7\u54c1\u4e2d\u5177\u6709\u524d\u666f\u7684\u5e94\u7528\u800c\u53d7\u5230\u4eba\u4eec\u7684\u5e7f\u6cdb\u91cd\u89c6\u3002\u7136\u800c\uff0c\u5177\u6709\u5feb\u901f\u6e29\u5ea6\u54cd\u5e94\u548c\u53ef\u63a7\u7535\u5b50\u53d1\u5c04\u7684\u53ef\u8c03\u5fae\u52a0\u5de5\u7535\u5b50\u53d1\u5c04\u5668\u4ecd\u9762\u4e34\u91cd\u91cd\u6311\u6218\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u5317\u4eac\u5927\u5b66\u7684\u7814\u7a76\u56e2\u961f\u4f7f\u7528\u5fae\u52a0\u5de5\u5236\u9020\u7684\u65b9\u6cd5\u5236\u5907\u51fa\u4ee5\u5fae\u5c3a\u5ea6\u77f3\u58a8\u70ef\u8584\u819c\u4f5c\u4e3a\u706f\u4e1d\u7684\u5fae\u578b\u70ed\u7535\u5b50\u53d1\u5c04\u5668\u3002\u77f3\u58a8\u70ef\u5fae\u578b\u7535\u5b50\u53d1\u5c04\u5668\u7684\u53d1\u5c04\u7535\u6d41\u5728\u9002\u5ea6\u7684\u6805\u7535\u538b\u8303\u56f4\u5185\u53ef\u57286\u4e2a\u6570\u91cf\u7ea7\u5185\u8c03\u8282\uff0c\u5f00\u5173\u65f6\u95f4\u5c0f\u4e8e1\u5fae\u79d2\uff0c\u6bd4\u5927\u578b\u7535\u5b50\u53d1\u5c04\u5668\u7684\u5f00\u5173\u65f6\u95f4\u5feb\u4e865\u4e2a\u6570\u91cf\u7ea7\u3002\u66f4\u91cd\u8981\u7684\u662f\uff0c\u901a\u8fc7\u5fae\u52a0\u5de5\u5236\u9020\u6280\u672f\u8bbe\u8ba1\u77f3\u58a8\u70ef\u7684\u5c3a\u5bf8\u4f7f\u5f97\u77f3\u58a8\u70ef\u5fae\u578b\u7535\u5b50\u53d1\u5c04\u5668\u7684\u7535\u5b50\u53d1\u5c04\u6027\u80fd\u53ef\u63a7\u5e76\u4e14\u53ef\u518d\u751f\uff0c\u4ece\u800c\u5236\u9020\u51fa\u7684\u77f3\u58a8\u70ef\u9635\u5217\u7535\u5b50\u53d1\u5c04\u5668\u7684\u7535\u5b50\u53d1\u5c04\u6027\u80fd\u66f4\u52a0\u5747\u5300\u3002<\/p>\n<p>\u5fae\u578b\u77f3\u58a8\u70ef\u7535\u5b50\u53d1\u5c04\u5668\u4e3a\u5b9e\u73b0\u5927\u578b\u53ef\u5bfb\u5740\u7684\u7535\u5b50\u53d1\u5c04\u5668\u9635\u5217\u5728\u771f\u7a7a\u7535\u5b50\u5668\u4ef6\u7684\u5e94\u7528\u63d0\u4f9b\u4e86\u53ef\u80fd\u3002<\/p>\n<p>\u8be5\u9879\u6210\u679c\u53d1\u8868\u4e8e\uff1a<a href=\"http:\/\/www.nature.com\/ncomms\/2016\/160510\/ncomms11513\/abs\/ncomms11513.html\" target=\"_blank\">NATURE COMMUNICATIONS<\/a>\u3002<\/p>\n<p><span style=\"color: #ff6600;\"><strong>\u3010\u66f4\u591a\u5173\u6ce8\u3011<\/strong><\/span><\/p>\n<p><strong>\u6e05\u534e\u5927\u5b66\u9a8c\u8bc1N\u6216O\u63ba\u6742\u53ef\u6709\u6548\u6291\u5236\u9502\u786b\u7535\u6c60\u7684\u98de\u68ad\u6548\u5e94<\/strong><br \/>\n<img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-13059\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/2-7.png\" alt=\"2\" width=\"525\" height=\"385\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/2-7.png 503w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/2-7-300x220.png 300w\" sizes=\"(max-width: 525px) 100vw, 525px\" \/><br \/>\n\u5f53\u524d\u9502\u786b\u7535\u6c60\u7684\u7814\u7a76\u9ad8\u5ea6\u96c6\u4e2d\u5728\u9ad8\u5bb9\u91cf\u50a8\u80fd\u65b9\u9762\uff0c\u9762\u4e34\u7684\u4e25\u5cfb\u95ee\u9898\u4e4b\u4e00\u662f\u98de\u68ad\u6548\u5e94\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u6e05\u534e\u5927\u5b66\u7684\u7814\u7a76\u56e2\u961f\u8fd0\u7528\u5bc6\u5ea6\u6cdb\u51fd\u6570\u7406\u8bba\u5bf9\u63ba\u6742\u4e0d\u540c\u539f\u5b50\u7684\u7eb3\u7c73\u78b3\u6750\u6599\u8fdb\u884c\u5206\u6790\uff0c\u5e76\u5bf9\u9502\u786b\u7535\u6c60\u7684\u673a\u7406\u3001\u672a\u6765\u7684\u8bbe\u8ba1\u8fdb\u884c\u4e86\u8be6\u7ec6\u8bf4\u660e\u3002\u5b9e\u8df5\u8bc1\u660e\uff0c\u91c7\u7528N\u6216O\u63ba\u6742\u7684\u5316\u5b66\u6539\u6027\u65b9\u6cd5\u53ef\u4ee5\u901a\u8fc7\u5076\u6781-\u5076\u6781\u9759\u7535\u76f8\u4e92\u4f5c\u7528\u663e\u8457\u63d0\u9ad8\u78b3\u4e3b\u4f53\u548c\u591a\u786b\u5316\u7269\u95f4\u7684\u76f8\u4e92\u4f5c\u7528\uff0c\u4ece\u800c\u6709\u6548\u5730\u6291\u5236\u98de\u68ad\u6548\u5e94\uff0c\u63d0\u9ad8\u5bb9\u91cf\u548c\u5e93\u4f26\u6548\u7387\u3002\u76f8\u6bd4\u4e4b\u4e0b\uff0c\u5f15\u5165B\u3001F\u3001S\u3001P\u548cCl\u7684\u7ed3\u679c\u5374\u4e0d\u5c3d\u5982\u4eba\u610f\u3002\u56e0\u6b64\u4ed6\u4eec\u63d0\u51fa\u5728\u9502\u786b\u7535\u6c60\u4e2d\u63ba\u6742\u78b3\u652f\u67b6\u7684\u6784\u60f3\u4ee5\u5b9e\u73b0\u5f3a\u9759\u7535\u5076\u6781-\u5076\u6781\u76f8\u4e92\u4f5c\u7528\u3002<\/p>\n<p>\u6b64\u5916\uff0c\u7814\u7a76\u8005\u53ef\u4ee5\u901a\u8fc7\u5171\u63ba\u6742\u7684\u65b9\u6cd5\u5728\u9502\u786b\u7535\u6c60\u4e2d\u5b9e\u73b0\u66f4\u5f3a\u7684\u76f8\u4e92\u4f5c\u7528\u4ece\u800c\u201c\u56f0\u4f4f\u201d\u5145\u653e\u7535\u8fc7\u7a0b\u4e2d\u4ea7\u751f\u7684\u591a\u786b\u5316\u7269\u3002<\/p>\n<p>\u8be5\u7814\u7a76\u6210\u679c\u53d1\u8868\u4e8e\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/smll.201600809\/full\" target=\"_blank\">Small<\/a>\u3002<\/p>\n<p><strong>\u4e2d\u79d1\u5927\u7814\u5236\u51faTe\u7eb3\u7c73\u7ebf\/\u78b3\u7eb3\u7c73\u7ba1\u590d\u5408\u9634\u6781\u6750\u6599\u78b2\u7535\u6781\u9502\u7535\u6c60<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-13060\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/3-6.png\" alt=\"3\" width=\"525\" height=\"562\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/3-6.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/3-6-280x300.png 280w\" sizes=\"(max-width: 525px) 100vw, 525px\" \/><br \/>\n\u5728\u53ef\u5145\u7535\u9502\u79bb\u5b50\u7535\u6c60\u4e2d\uff0c\u57fa\u4e8e\u7b2c\u516d\u4e3b\u65cf\u5143\u7d20\u7684\u9634\u6781\u6750\u6599\u7531\u4e8e\u5177\u6709\u548cO\u3001S\u76f8\u5f53\u7684\u7406\u8bba\u4f53\u79ef\u5bb9\u91cf\u5bc6\u5ea6\u3001\u66f4\u9ad8\u7684\u4e0e\u9502\u53cd\u5e94\u6d3b\u6027\u800c\u5d2d\u9732\u5934\u89d2\u3002<\/p>\n<p>\u6765\u81ea\u4e2d\u56fd\u79d1\u5b66\u6280\u672f\u5927\u5b66\u7b49\u9ad8\u6821\u53ca\u7814\u7a76\u4e2d\u5fc3\u7684\u7814\u7a76\u8005\u5c06Te\u7eb3\u7c73\u7ebf\/\u53cc\u529f\u80fd\u5f39\u6027\u78b3\u7eb3\u7c73\u7ba1\u6c14\u51dd\u80f6\u590d\u5408\u6750\u6599\u7528\u4e8e\u9634\u6781\u6750\u6599\uff0c\u5e76\u7ec4\u88c5\u51fa\u4e24\u79cd\u7c7b\u578b\u7684\u7c98\u5408\u5242\/\u96c6\u7535\u6781-\u78b2\u7535\u6781\u9502\u7535\u6c60\u3002\u78b3\u7eb3\u7c73\u7ba1\u9ad8\u7684\u5bfc\u7535\u6027\u548c\u591a\u5b54\u7ed3\u6784\u4fdd\u8bc1\u7a33\u5b9a\u7684\u7535\u63a5\u89e6\u4ee5\u53ca\u9502\u79bb\u5b50\u7684\u4f20\u8f93\uff0c\u4e0e\u6b64\u540c\u65f6\u5c06Te\u548cLi2Te\u201c\u56f0\u5728\u201d\u7f51\u7edc\u4e2d\uff0c\u4ece\u800c\u5feb\u901f\u89e6\u53d1\u4ee5\u53ca\u7a33\u5b9a\u5176\u7535\u5316\u5b66\u7279\u6027\u3002\u9634\u6781\u4e5f\u5177\u6709\u826f\u597d\u7684\u53ef\u538b\u7f29\u6027\uff0c\u4ee5\u7f13\u51b2\u9502\u5316\/\u8131\u9502\u5316\u8fc7\u7a0b\u4e2d\u7684\u4f53\u79ef\u81a8\u80c0\uff0c\u63d0\u9ad8\u7535\u6781\u5b8c\u6574\u6027\u3002<\/p>\n<p>\u8be5\u9634\u6781\u6750\u6599\u5177\u6709\u6bd4\u5bb9\u91cf\u9ad8\u3001\u5faa\u73af\u7a33\u5b9a\u6027\u597d\u548c\u500d\u7387\u6027\u80fd\u597d\u7b49\u4f18\u70b9\uff0c\u6709\u671b\u5f00\u542f\u4e0b\u4e00\u4ee3\u9ad8\u80fd\u91cf\u7535\u6c60\u7684\u201c\u8d85\u9502\u201d\u65f6\u4ee3\u3002<\/p>\n<p>\u8be5\u9879\u6210\u679c\u53d1\u8868\u4e8e\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adfm.201600640\/full\" target=\"_blank\">Advanced Functional Materials\u3002<\/a><\/p>\n<p><strong>\u4e2d\u56fd\u5de5\u7a0b\u7269\u7406\u7814\u7a76\u9662\u7b49\u673a\u6784\u7814\u5236\u51fa\u65b0\u578b\u7ea4\u7ef4\u72b6\u8d85\u7ea7\u7535\u5bb9\u5668<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-13061\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/4-7.png\" alt=\"4\" width=\"561\" height=\"218\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/4-7.png 561w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/4-7-300x117.png 300w\" sizes=\"(max-width: 561px) 100vw, 561px\" \/><\/p>\n<p>\u8fd1\u65e5\uff0c\u6765\u81ea\u4e2d\u56fd\u5de5\u7a0b\u7269\u7406\u7814\u7a76\u9662\u5316\u5b66\u6750\u6599\u7814\u7a76\u6240\u548c\u590d\u65e6\u5927\u5b66\u9ad8\u5206\u5b50\u6750\u6599\u79d1\u5b66\u4e0e\u5de5\u7a0b\u5b66\u9662\u7814\u7a76\u8005\u5236\u5907\u51fa\u9ad8\u529b\u5b66\u6027\u80fd\u7684\u4e2d\u7a7a\u77f3\u58a8\u70ef\/\u5bfc\u7535\u805a\u5408\u7269\u590d\u5408\u7ea4\u7ef4\u5e76\u5c06\u5176\u7528\u4e8e\u5236\u9020\u65b0\u578b\u7ea4\u7ef4\u72b6\u7684\u8d85\u7ea7\u7535\u5bb9\u5668\uff0c\u5177\u6709\u9ad8\u7684\u80fd\u91cf\u5bc6\u5ea6\u548c\u4f18\u5f02\u7684\u5bff\u547d\u7a33\u5b9a\u6027\u3002\u8fd9\u79cd\u7ea4\u7ef4\u8d85\u7ea7\u7535\u5bb9\u5668\u7ec7\u6210\u7684\u67d4\u6027\u4f9b\u7535\u7eba\u7ec7\u54c1\uff0c\u5728\u4fbf\u643a\u5f0f\u548c\u53ef\u7a7f\u6234\u7535\u5b50\u4ea7\u54c1\u9886\u57df\u5177\u6709\u5de8\u5927\u524d\u666f\u3002<\/p>\n<p>\u8be5\u9879\u6210\u679c\u53d1\u8868\u4e8e\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adma.201670128\/full\" target=\"_blank\">Advanced Materials\u3002<\/a><\/p>\n<p><strong>\u5317\u4eac\u5de5\u4e1a\u5927\u5b66\u5236\u5907\u51fa\u9ad8\u5ea6\u7a33\u5b9a\u7684\u9506\u57faMOFs<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-13062\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/5-7.png\" alt=\"5\" width=\"523\" height=\"357\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/5-7.png 395w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/5-7-300x205.png 300w\" sizes=\"(max-width: 523px) 100vw, 523px\" \/><\/p>\n<p>\u5e9f\u6c34\u4e2d\u4e3b\u8981\u6c61\u67d3\u7269\u2014\u2014\u6297\u751f\u7d20\u548c\u6709\u673a\u70b8\u836f\u7684\u68c0\u6d4b\u548c\u6e05\u9664\u5341\u5206\u91cd\u8981\u4f46\u5177\u6709\u6311\u6218\u6027\u3002\u4f5c\u4e3a\u4e00\u7c7b\u65b0\u578b\u7684\u591a\u5b54\u6750\u6599\uff0c\u91d1\u5c5e\u6709\u673a\u9aa8\u67b6\u5316\u5408\u7269\uff08MOFs\uff09\u5728\u4f20\u611f\u548c\u5438\u9644\u9886\u57df\u5177\u6709\u826f\u597d\u7684\u5e94\u7528\u524d\u666f\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u5317\u4eac\u5de5\u4e1a\u5927\u5b66\u7b49\u9ad8\u6821\u7684\u7814\u7a76\u8005\u5236\u5907\u51fa\u9ad8\u5ea6\u7a33\u5b9a\u7684\u9506\u57faMOFs\u4ee5\u68c0\u6d4b\u548c\u53bb\u9664\u5e9f\u6c34\u4e2d\u7684\u6297\u751f\u7d20\u548c\u6709\u673a\u70b8\u836f\u3002\u56e2\u961f\u4f7f\u7528\u62d3\u6251\u7ed3\u6784\u5206\u6790\u65b9\u6cd5\u8bbe\u8ba1\u5e76\u5408\u6210\u51fa\u4e24\u7c7b\u7a33\u5b9a\u7684\u9506\u57faMOFs\uff1aZr6O4(OH)8(H2O)4(CTTA)8\/3(BUT-12)\u548cZr6O4(OH)8(H2O)4 (TTNA)8\/3(BUT-13)\uff0c\u4e24\u8005\u5206\u522b\u5177\u6709\u9ad8\u8fbe3387m2\/g\u30013498m2\/g\u7684\u5e03\u9c81\u8bfa\u5c14-\u57c3\u7c73\u7279-\u6cf0\u52d2\uff08BET\uff09\u8868\u9762\u79ef\uff0cBUT-13\u5728\u76ee\u524d\u6c34\u7a33\u5b9a\u6027MOF\u4e2d\u6027\u80fd\u6700\u4e3a\u7a81\u51fa\u3002\u53ef\u4ee5\u901a\u8fc7\u8ffd\u8e2a\u6c34\u4e2d\u544b\u5583\u897f\u6797\uff08NZF\uff09\u548c\u544b\u5583\u59a5\u56e0\uff08NFT\uff09\u6297\u751f\u7d20\u4ee5\u53ca2,4,6-\u4e09\u785d\u57fa\u82ef\u915a\uff08TNP\uff09\u548c\u5bf9\u785d\u57fa\u82ef\u915a\uff084-NP\uff09\u7684\u6570\u91cf\u5f97\u77e5\u8fd9\u4e9bMOFs\u5177\u6709\u4f18\u5f02\u7684\u8367\u5149\u6027\u80fd\u3002\u5b83\u4eec\u62e5\u6709MOFs\u57fa\u4f20\u611f\u6750\u6599\u7684\u6700\u9ad8\u6c34\u5e73\uff1a\u5bf9\u4e8e\u5341\u4ebf\u5206\u7387\u542b\u91cf\u7684\u6c34\u5e73\u611f\u5e94\u4ecd\u7136\u5341\u5206\u7075\u654f\u3002\u540c\u65f6\uff0c\u5b83\u4eec\u5bf9\u4e8e\u8fd9\u4e9b\u6709\u673a\u5206\u5b50\u8fd8\u5177\u6709\u9ad8\u7684\u5438\u9644\u4f5c\u7528\uff0c\u7814\u7a76\u53d1\u73b0\uff0c\u5438\u9644\u53ef\u8fdb\u4e00\u6b65\u63d0\u9ad8\u8367\u5149\u6dec\u706d\u6548\u7387\uff0c\u5bf9\u4e8e\u5438\u9644\u7269\u7684\u5206\u6790\u5177\u6709\u91cd\u8981\u4f5c\u7528\u3002\u8fd9\u4e9b\u7ed3\u679c\u8868\u660e\uff0cBUT-12\u548c13\u53ef\u4ee5\u540c\u65f6\u9009\u62e9\u6027\u68c0\u6d4b\u548c\u53bb\u9664\u7279\u5b9a\u6297\u751f\u7d20\u548c\u7206\u70b8\u6027\u6709\u673a\u7269\uff0c\u5728\u6c34\u8d28\u76d1\u6d4b\u548c\u6c61\u6c34\u5904\u7406\u65b9\u9762\u5177\u6709\u6f5c\u5728\u4f5c\u7528\u3002<\/p>\n<p>\u8be5\u7814\u7a76\u6210\u679c\u53d1\u8868\u4e8e\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/pdf\/10.1021\/jacs.6b01663\" target=\"_blank\">JACS<\/a>\u3002<\/p>\n<p><strong>\u53a6\u95e8\u5927\u5b66\u5229\u7528\u9633\u79bb\u5b50\u4ea4\u6362\u53cd\u5e94\u6784\u5efa\u4e86Mn2+\u548cZn2+\u6c27\u5316\u94c1\u7eb3\u7c73\u9897\u7c92<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-13063\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/6-3.png\" alt=\"6\" width=\"526\" height=\"329\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/6-3.png 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/6-3-300x188.png 300w\" sizes=\"(max-width: 526px) 100vw, 526px\" \/><\/p>\n<p>\u9633\u79bb\u5b50\u4ea4\u6362\u662f\u4e00\u79cd\u5728\u4fdd\u6301\u5f62\u6001\u60c5\u51b5\u4e0b\uff0c\u901a\u8fc7\u590d\u5408\u53d8\u5316\u6765\u8c03\u8282\u7eb3\u7c73\u6676\u4f53\u6027\u8d28\u7684\u6709\u529b\u624b\u6bb5\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u53a6\u95e8\u5927\u5b66\u7b49\u9ad8\u6821\u7684\u7814\u7a76\u56e2\u961f\u63ed\u793a\u4e86\uff0c\u9633\u79bb\u5b50\u4ea4\u6362\u53ef\u4ee5\u6539\u53d8\u94c1\u6c27\u5316\u7269\u7eb3\u7c73\u6676\u4f53\u7684\u7ec4\u6210\uff0c\u4ee5\u5728\u6838\u78c1\u5171\u632f\u6210\u50cf\u4e2d\u663e\u8457\u63d0\u9ad8\u5176\u5bf9\u6bd4\u5ea6\u3002\u4ed6\u4eec\u5229\u7528\u9633\u79bb\u5b50\u4ea4\u6362\u53cd\u5e94\u6210\u529f\u5730\u6784\u5efa\u4e86\u5177\u6709\u4e0d\u540c\u5f62\u72b6\uff08\u7403\u4f53\uff0c\u7acb\u65b9\u4f53\uff0c\u548c\u516b\u500d\u4f53\uff09\u7684Mn2+\u548cZn2+\u6c27\u5316\u94c1\u7eb3\u7c73\u9897\u7c92\u3002Mn2+\u548cZn2+\u8fdb\u5165\u94c1\u6c27\u4f53\u7684\u6676\u683c\uff0c\u4e14\u5927\u591a\u6570\u90fd\u5206\u5e03\u5728\u94c1\u7d20\u4f53\u7684TD\u4f4d\u70b9\u3002\u8fd9\u4e9b\u5de5\u7a0b\u7684\u5f62\u72b6\u5404\u5411\u5f02\u6027\u7684\u6c27\u5316\u94c1\u7eb3\u7c73\u9897\u7c92\u5177\u6709\u9ad8\u9971\u548c\u78c1\u5316\u5f3a\u5ea6\u548c\u8f83\u5927\u7684\u6709\u6548\u8fb9\u754c\u534a\u5f84\uff0c\u56e0\u6b64\u6a2a\u5411\u5f1b\u8c6b\u7387\u5341\u5206\u663e\u8457\u3002<\/p>\n<p>\u8fd9\u4e9b\u6c27\u5316\u94c1\u7eb3\u7c73\u7c92\u5b50\u53ef\u4ee5\u4f5c\u4e3a\u4f53\u5185\u6838\u78c1\u5171\u632f\u6210\u50cf\u9ad8\u6027\u80fd\u7684\u9020\u5f71\u5242\u5728\u4f53\u5185\u6210\u50cf\uff0c\u4f7f\u65e9\u671f\u809d\u80bf\u7624\u548c\u809d\u8f6c\u79fb\u7624\u5f97\u4ee5\u7075\u654f\u6210\u50cf\uff08\u5c0f\u81f30.4\u6beb\u7c73\uff09\uff0c\u5728\u764c\u75c7\u7684\u53ca\u65f6\u53d1\u73b0\u4ee5\u53ca\u8f6c\u79fb\u65b9\u9762\u5177\u6709\u5de8\u5927\u6f5c\u529b\u3002<\/p>\n<p>\u8be5\u7814\u7a76\u6210\u679c\u53d1\u8868\u4e8e\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/ipdf\/10.1021\/acs.chemmater.6b01256\" target=\"_blank\">Chemistry of Materials<\/a>\u3002<\/p>\n<p><strong>\u4e2d\u79d1\u9662\u7406\u5316\u6280\u672f\u7814\u7a76\u6240\u5236\u5907\u51fa\u65b0\u578b\u7852\u6c5e\u5316\u7269BaHgSe2<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-13064 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/7-3.png\" alt=\"7\" width=\"575\" height=\"405\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/7-3.png 575w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/7-3-300x211.png 300w\" sizes=\"(max-width: 575px) 100vw, 575px\" \/><\/p>\n<p>\u8fd1\u65e5\uff0c\u4e2d\u79d1\u9662\u7406\u5316\u6280\u672f\u7814\u7a76\u6240\u7684\u7814\u7a76\u56e2\u961f\u5236\u5907\u51fa\u65b0\u578b\u7852\u5316\u6c5eBaHgSe2\u5177\u8f83\u9ad8\u7684\u975e\u7ebf\u6027\u5149\u5b66\u54cd\u5e94\u4ee5\u53ca\u5171\u540c\u7194\u70b9\u3002\u8be5\u7ed3\u6784\u5728\u5e73\u9762\u4e09\u89d2\u5f62\u5355\u5143\u4e2d\u5305\u542b[HgSe3]4\u2212\u9634\u79bb\u5b50\u7684\u89d2\u5171\u4eab\u94fe\uff0c\u5728\u7ea2\u5916\u975e\u7ebf\u6027\u5149\u5b66\u6750\u6599\u4e2d\u5145\u5f53\u65b0\u7684\u57fa\u672c\u5b98\u80fd\u56e2\u4ee5\u8d4b\u4e88\u6750\u6599\u5927\u7684\u975e\u7ebf\u6027\u6781\u5316\u7387\u548c\u7406\u5316\u7a33\u5b9a\u6027\u3002<\/p>\n<p>\u8fd9\u6837\u7684\u5e73\u9762\u4e09\u89d2\u5f62\u5355\u5143\u6709\u52a9\u4e8e\u7814\u7a76\u8005\u5728\u5bfb\u627e\u4e0e\u4f20\u7edf\u9ec4\u94dc\u6750\u6599\u5b8c\u5168\u4e0d\u540c\u7684\u5b9e\u7528\u7ea2\u5916\u975e\u7ebf\u6027\u5149\u5b66\u6750\u6599\u7684\u8fc7\u7a0b\u4e2d\u53e6\u8f9f\u8e4a\u5f84\u3002<\/p>\n<p>\u8be5\u7814\u7a76\u6210\u679c\u53d1\u8868\u4e8e\uff1a<a href=\"http:\/\/xueshu.baidu.com\/s?wd=paperuri%3A%28be0c1d1e1a0795f1cb11b5f133b669df%29&amp;filter=sc_long_sign&amp;tn=SE_xueshusource_2kduw22v&amp;sc_vurl=http%3A%2F%2Fpubs.acs.org%2Fdoi%2Fsuppl%2F10.1021%2Fjacs.6b03107&amp;ie=utf-8&amp;sc_us=2558540658935266551\" target=\"_blank\">JACS<\/a>\u3002<\/p>\n<p><strong>\u4e2d\u79d1\u9662\u82cf\u5dde\u7eb3\u7c73\u6240\u7814\u7a76\u4e86\u91d1\u5c5e\u56e2\u7c07\u5438\u9644\u5bf9\u7b49\u79bb\u5b50\u5171\u632f\u963b\u5c3c\u7684\u5f71\u54cd<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-13065\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/8-5.png\" alt=\"8\" width=\"526\" height=\"361\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/8-5.png 526w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/8-5-300x206.png 300w\" sizes=\"(max-width: 526px) 100vw, 526px\" \/><\/p>\n<p>\u901a\u8fc7\u91d1\u5c5e\u5438\u9644\u5bf9\u7b49\u79bb\u5b50\u4f53\u7eb3\u7c73\u7c92\u5b50\u8fdb\u884c\u8868\u9762\u4fee\u9970\u5728\u7b49\u79bb\u5b50\u4f53\u611f\u5e94\u3001\u7b49\u79bb\u5b50\u4f53\u589e\u5f3a\u5149\u50ac\u5316\u5242\u4e2d\u5177\u6709\u91cd\u8981\u7684\u5e94\u7528\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u82cf\u5dde\u7eb3\u7c73\u6280\u672f\u4e0e\u7eb3\u7c73\u4eff\u751f\u7814\u7a76\u6240\u7684\u76f8\u5173\u56e2\u961f\u7814\u7a76\u4e86\u91d1\u5c5e\u56e2\u7c07\u5438\u9644\u5bf9\u7b49\u79bb\u5b50\u5171\u632f\u963b\u5c3c\u7684\u5f71\u54cd\uff0c\u5e94\u7528\u5355\u7c92\u5b50\u6697\u573a\u5149\u8c31\u6d4b\u8bd5\u94c2\u63ba\u6742\u524d\u540e\u7684\u540c\u6837\u7684\u91d1\u7eb3\u7c73\u68d2\u3002\u7814\u7a76\u53d1\u73b0\u7531\u4e8e\u7ebf\u5bbd\u589e\u52a0\u800c\u5bfc\u81f4\u7684\u94c2\u8bf1\u5bfc\u963b\u5c3c\u7b49\u79bb\u5b50\u4f53\u4f9d\u8d56\u4e8e\u6d4b\u91cf\u7eb3\u7c73\u68d2\u7684\u5171\u632f\u6ce2\u957f\uff0c\u5176\u672c\u8d28\u4e0a\u662f\u5206\u6563\u7684\u3002\u57fa\u4e8e\u79bb\u6563\u5076\u6781\u5b50\u8fd1\u4f3c\u65b9\u6cd5\u7684\u4eff\u771f\u7ed3\u679c\u8868\u660e\u963b\u5c3c\u4e3b\u8981\u662f\u7531\u68d2\u4e24\u8fb9\u7684\u5438\u9644\u4ea7\u751f\u3002\u91d1\u3001\u94f6\u3001\u94c2\u5177\u6709\u4e0d\u540c\u7684\u4f53\u79ef\u4ecb\u7535\u51fd\u6570\uff0c\u56e0\u6b64\u4ece\u5b64\u7acb\u7684\u96c6\u7fa4\u5230\u4e00\u4e2a\u5b8c\u6574\u7684\u58f3\u7684\u8fc7\u6e21\u8fc7\u7a0b\u8868\u73b0\u51fa\u5de8\u5927\u7684\u5dee\u5f02\u3002<\/p>\n<p>\u8fd9\u4e00\u53d1\u73b0\u5c06\u4e3a\u7814\u7a76\u8005\u8bbe\u8ba1\u548c\u5236\u9020\u91d1\u5c5e\u5f02\u8d28\u7ed3\u6784\u7eb3\u7c73\u529f\u80fd\u6750\u6599\u63d0\u4f9b\u65b0\u7684\u601d\u8def\u3002<\/p>\n<p>\u8be5\u7814\u7a76\u6210\u679c\u53d1\u8868\u4e8e\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/smll.201600533\/full\" target=\"_blank\">Small<\/a>\u3002<\/p>\n<p>\u4ee5\u4e0a\u6211\u4eec\u5217\u4e3e\u7684\u4ec5\u4e3a\u8fc7\u53bb\u4e00\u5468\u5185\uff085.5-5.11\uff09\u6211\u56fd\u5148\u8fdb\u6750\u6599\u7814\u7a76\u7684\u6700\u65b0\u8fdb\u5c55\u7684\u4ee3\u8868\u3002\u6574\u7406\u8fc7\u7a0b\u4e2d\u96be\u514d\u5b58\u5728\u758f\u5ffd\uff0c\u8fd8\u671b\u5404\u4f4d\u8bfb\u8005\u8c05\u89e3\u5e76\u8bda\u631a\u6b22\u8fce\u5927\u5bb6\u63d0\u51fa\u610f\u89c1\/\u5efa\u8bae\uff0c\u6216\u63a8\u8350\u6700\u65b0\u7684\u56fd\u5185\u6750\u6599\u7814\u7a76\u65b0\u95fb\u7ebf\u7d22\u7ed9\u6211\u4eec\uff1atougao@cailiaoren.com\u3002<\/p>\n<p>\u672c\u671f\u5468\u62a5\u7531\u56fd\u5185\u6750\u6599\u5468\u62a5\u5c0f\u7ec4\u5434\u957f\u9752\u64b0\u5199\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u56fd\u5185\u5468\u62a5\u7b2c45\u671f\u6458\u8981\uff1a\u5317\u4eac\u5927\u5b66\u7814\u7a76\u56e2\u961f\u4f7f\u7528\u5fae\u52a0\u5de5\u5236\u9020\u65b9\u6cd5\u7814\u53d1\u51fa\u4ee5\u5fae\u5c3a\u5ea6\u77f3\u58a8\u70ef\u8584\u819c\u4f5c\u4e3a\u706f\u4e1d\u7684\u5fae\u578b\u70ed\u7535\u5b50\u53d1\u5c04\u5668\uff1b\u6e05\u534e\u5927\u5b66\u8fd0\u7528\u5bc6\u5ea6\u6cdb\u51fd\u6570\u7406\u8bba\u9a8c\u8bc1N\u6216O\u63ba\u6742\u53ef\u6709\u6548\u6291\u5236\u9502&#8230;<\/p>\n","protected":false},"author":176,"featured_media":13068,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[67],"tags":[43,33],"class_list":["post-13056","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-zhoubao","tag-composite","tag-nano"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/13056"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/176"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=13056"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/13056\/revisions"}],"predecessor-version":[{"id":13081,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/13056\/revisions\/13081"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/13068"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=13056"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=13056"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=13056"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}