{"id":13182,"date":"2016-05-13T22:00:20","date_gmt":"2016-05-13T14:00:20","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=13182"},"modified":"2016-05-13T20:58:52","modified_gmt":"2016-05-13T12:58:52","slug":"%e9%87%8d%e7%a3%85%ef%bc%81%e5%8d%95%e8%b4%a8%e7%a3%b7%e7%94%a8%e4%ba%8e%e5%85%89%e5%82%ac%e5%8c%96%e5%88%b6%e6%b0%a2%e6%95%88%e7%8e%87%e5%88%9b%e5%8e%86%e5%8f%b2%e6%96%b0%e9%ab%98%e3%80%90%e6%96%b0","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=13182","title":{"rendered":"\u91cd\u78c5\uff01\u5355\u8d28\u78f7\u7528\u4e8e\u5149\u50ac\u5316\u5236\u6c22\u6548\u7387\u521b\u5386\u53f2\u65b0\u9ad8\u3010\u65b0\u80fd\u6e90160513\u671f\u3011"},"content":{"rendered":"<p>\u78f7\uff08P\uff09\u662f\u6700\u666e\u904d\u7684\u5143\u7d20\u4e4b\u4e00\uff0c\u5728\u5730\u7403\u4e0a\u7684\u50a8\u91cf\u6709\u5927\u7ea61000\u4ebf\u5428\uff0c\u4e14\u5728\u5316\u5b66\uff0c\u7269\u7406\u5b66\uff0c\u751f\u7269\u5b66\u548c\u751f\u6001\u5b66\u7b49\u9886\u57df\u5747\u5177\u6709\u91cd\u8981\u610f\u4e49\u3002\u81ea17\u4e16\u7eaa60\u5e74\u4ee3\u88ab\u53d1\u73b0\u4ee5\u6765\uff0c\u5bf9\u4e0d\u540c\u79cd\u7c7b\u7684P\u7684\u540c\u7d20\u5f02\u5f62\u4f53\u7684\u6539\u6027\uff0c\u5df2\u7ecf\u53d7\u5230\u79d1\u7814\u5de5\u4f5c\u8005\u5e7f\u6cdb\u7684\u5173\u6ce8\u3002<\/p>\n<p>\u5355\u8d28\u5177\u6709\u7684\u534a\u5bfc\u4f53\u6027\u8d28\u662f\u975e\u5e38\u6709\u8da3\u548c\u5f15\u4eba\u5173\u6ce8\u7684\u73b0\u8c61\uff0c\u6700\u8fd1\uff0c\u9999\u6e2f\u4e2d\u6587\u5927\u5b66\u7684Jimmy C. Yu\u6559\u6388\u8bfe\u9898\u7ec4\u53d6\u5f97\u4e00\u4e2a\u91cd\u5927\u7684\u7a81\u7834\uff0c\u7531Ruck\u7b49\u4eba\u5bf9\u7ea2\u78f7\u6539\u6027\u5f97\u5230\u7684\u7ea4\u7ef4\u76f8\u7ea2\u78f7\u80fd\u591f\u4f5c\u4e3a\u4e00\u79cd\u534a\u5bfc\u4f53\u5728\u53ef\u89c1\u5149\u533a\u8fdb\u884c\u5149\u50ac\u5316\u5236\u6c22\u3002\u5c0f\u5c3a\u5bf8\u7684\u7ea4\u7ef4\u78f7\u53ef\u4ee5\u901a\u8fc7\u8d1f\u8f7d\u5728\u5177\u6709\u5149\u6d3b\u6027\u7684\u4e8c\u6c27\u5316\u7845\u7684\u7ea4\u7ef4\u4e0a\u5f97\u5230\uff0c\u4e5f\u53ef\u4ee5\u901a\u8fc7\u8d85\u58f0\u5265\u79bb\u5f97\u5230\u3002\u8fd9\u4e24\u79cd\u65b9\u6cd5\u5f97\u5230\u7684\u7ea4\u7ef4\u78f7\u8868\u73b0\u51fa\u4e86\u7a33\u5b9a\u7684\u4ea7\u6c22\u901f\u7387\uff0c\u5206\u522b\u4e3a633 \u03bcmol h<sup>-1<\/sup>g<sup>-1<\/sup>\u548c684 \u03bcmol h<sup>-1<\/sup>g<sup>-1<\/sup>\u3002\u8fd9\u4e24\u4e2a\u6570\u503c\u662f\u8fdc\u9ad8\u4e8e\u5148\u524d\u65e0\u5b9a\u5f62\u78f7\uff080.6 \u03bcmol h<sup>-1<\/sup>g<sup>-1<\/sup>\uff09\u548c\u5e0c\u6258\u592b\u78f7\uff081.6 \u03bcmol h<sup>-1<\/sup>g<sup>-1<\/sup>\uff09\u3002\u5230\u76ee\u524d\u4e3a\u6b62\uff0c\u8fd9\u662f\u5355\u5143\u7d20\u7269\u8d28\u4f5c\u4e3a\u5149\u50ac\u5316\u5242\u4e2d\u7684\u6700\u9ad8\u7eaa\u5f55\u3002\u8fd9\u4e2a\u53d1\u73b0\u6709\u52a9\u4e8e\u8fdb\u4e00\u6b65\u7406\u89e3\u5355\u8d28\u7684\u534a\u5bfc\u4f53\u6027\u8d28\u3002\u540c\u65f6\uff0c\u8fd9\u5bf9\u5143\u7d20\u5149\u50ac\u5316\u5242\u7684\u53d1\u5c55\u5341\u5206\u6709\u5229\u3002<\/p>\n<p>\u4ee5\u4e0b\u662f\u8be5\u5de5\u4f5c\u6587\u732e\u5bfc\u8bfb\uff1a<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-13183 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe1-5.jpg\" alt=\"\u56fe1\" width=\"648\" height=\"454\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe1-5.jpg 648w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe1-5-300x210.jpg 300w\" sizes=\"(max-width: 648px) 100vw, 648px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe1.<\/strong> \u5de6\u56fe\uff1a\u5149\u654f\u7684\u5fae\u7ea4\u7ef4P\/SiO<sub>2<\/sub>\uff1b\u53f3\u56fe\uff1a\u57fa\u4e8e\u5728\u7ea4\u7ef4\u76f8\u7ea2\u78f7\u4e0a\u7c89\u788e\u7684\u7ea4\u7ef4\u78f7\u3002<\/p>\n<p>\u4ee5\u4e0a\u5de6\u53f3\u4e24\u56fe\uff1a\u7ea4\u7ef4P\u5728\u5149\u7167\u7684\u6761\u4ef6\u4ea7\u751f\u7535\u5b50\u548c\u7a7a\u7a74\uff0c\u8f7d\u6d41\u5b50\u8fc1\u79fb\u5230\u6750\u6599\u7684\u8868\u9762\u4e0a\u7684P\u539f\u5b50\uff0c\u5176\u518d\u4f9d\u6b21\u87af\u5408\u8d28\u5b50\uff0c\u8d28\u5b50\u4e0e\u8d28\u5b50\u6210\u952e\uff0c\u8131\u79bbP\u539f\u5b50\uff0c\u5728\u8fd9\u4e2a\u8fc7\u7a0b\u4e2d\uff0c\u6750\u6599\u8868\u9762\u7684\u7535\u5b50\u53c2\u4e0e\u4e86\u6c22\u79bb\u5b50\u7684\u8fd8\u539f\uff0c\u4ece\u800c\u5f97\u5230\u6c22\u6c14\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-13184 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe2-5.jpg\" alt=\"\u56fe2\" width=\"648\" height=\"506\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe2-5.jpg 648w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe2-5-300x234.jpg 300w\" sizes=\"(max-width: 648px) 100vw, 648px\" \/><\/p>\n<p><strong>\u56fe2.<\/strong> \u626b\u63cf\u7535\u955c\uff08SEM\uff09\u56fe\uff1aa\uff0c\u5fae\u7ea4\u7ef4P\/SiO<sub>2<\/sub>, b\uff0c\u7c89\u788e\u7ea4\u7ef4P\u3002XRD\u56fe\uff1ac,\u5fae\u7ea4\u7ef4P\/SiO<sub>2<\/sub>,d\uff0c\u7c89\u788e\u7ea4\u7ef4P\uff0c\u672c\u4f53\u7ea4\u7ef4P\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-13185 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe3-3.jpg\" alt=\"\u56fe3\" width=\"551\" height=\"428\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe3-3.jpg 551w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe3-3-300x233.jpg 300w\" sizes=\"(max-width: 551px) 100vw, 551px\" \/><\/p>\n<p><strong>\u56fe3. <\/strong>a,\u7406\u8bba\u8ba1\u7b97\u7ea4\u7ef4P\u7684\u80fd\u5e26\u7ed3\u6784\u56fe\uff0cb\uff0c\u7ea4\u7ef4P\u7684\u539f\u5b50\u7ed3\u6784\u56fe\uff0cc,\u7d2b\u5916\u5438\u6536\u5149\u8c31\uff0cd\uff0c\u7531\u7d2b\u5916\u5438\u6536\u5149\u8c31\u8f6c\u5316\u7684Kubelka\u2013Munk\u56fe\u3002<\/p>\n<p>a\u56fe\u662f\u7528\u68af\u5ea6\u6821\u6b63\u4ea4\u6362\u76f8\u5173\u80fd(GGA)\u5bf9\u7ea4\u7ef4P\u7684\uff080 1 0\uff09\u8fdb\u884c\u8ba1\u7b97\u5f97\u5230\u7684\u80fd\u5e26\u56fe\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-13186 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe4-3.jpg\" alt=\"\u56fe4\" width=\"663\" height=\"447\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe4-3.jpg 663w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe4-3-300x202.jpg 300w\" sizes=\"(max-width: 663px) 100vw, 663px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe4. <\/strong>\u5fae\u7ea4\u7ef4P\/SiO2\u548c\u7c89\u788e\u7ea4\u7ef4P\u7684\u5149\u50ac\u5316\u5236\u6c22\u7684\u4ea7\u7387<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-13192 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe5-4.jpg\" alt=\"\u56fe5\" width=\"583\" height=\"435\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe5-4.jpg 583w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe5-4-300x224.jpg 300w\" sizes=\"(max-width: 583px) 100vw, 583px\" \/><\/p>\n<p style=\"text-align: center;\"><strong>\u56fe5. <\/strong>P\u7684\u540c\u7d20\u5f02\u5f62\u4f53\u7684\u4ea7\u6c22\u901f\u7387\u4e0e\u5176\u4ed6\u5355\u8d28\u5143\u7d20\u5149\u50ac\u5316\u5242\u7684\u4ea7\u6c22\u5bf9\u6bd4\u56fe<\/p>\n<p style=\"text-align: center;\"><img loading=\"lazy\" decoding=\"async\" class=\"alignnone wp-image-13188 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe6.jpg\" alt=\"\u56fe6\" width=\"540\" height=\"402\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe6.jpg 540w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe6-300x223.jpg 300w\" sizes=\"(max-width: 540px) 100vw, 540px\" \/><\/p>\n<p><strong>\u56fe6. <\/strong>a,b,c\u56fe\u662f\u4e0d\u540c\u6761\u4ef6\u4e0b\u5149\u7535\u6d41\u5bc6\u5ea6\u3002a\uff0c\u57280.1 M NaSO<sub>4<\/sub>\u7535\u89e3\u6db2\u4e2d\uff0cb,\u5728\u6ca1\u67090.001 M MVCl<sub>2<\/sub>\u4f5c\u4e3a\u7535\u5b50\u6355\u83b7\u5242\u7684\u6761\u4ef6\u4e0b\uff0cc,\u5728\u67090.1 M NaSO<sub>4<\/sub>\u7535\u89e3\u6db2\u548c0.001 M MVCl<sub>2<\/sub>\u4f5c\u4e3a\u7535\u5b50\u6355\u83b7\u5242\u7684\u6761\u4ef6\u4e0b\u3002d\u56fe:\u4e0d\u540c\u6ce2\u957f\u4e0b\u7684\u5149\u7535\u8f6c\u6362\u6548\u7387\u3002<\/p>\n<p><strong>\u5c55\u671b<\/strong><\/p>\n<p>\u5fae\u7ea4\u7ef4P\u548c\u7c89\u788e\u7ea4\u7ef4P\u5728\u53ef\u89c1\u5149\u533a\u5c55\u73b0\u4e86\u5f88\u9ad8\u7684\u5149\u50ac\u5316\u5236\u6c22\u901f\u7387\uff08\u662f\u76ee\u524d\u62a5\u9053\u6700\u9ad8\u7684\uff09\u3002\u8fd9\u4e2a\u53d1\u73b0\u6709\u52a9\u4e8e\u8fdb\u4e00\u6b65\u7684\u7406\u89e3\u7ea2\u78f7\u7684\u534a\u5bfc\u4f53\u6027\u8d28\uff0c\u540c\u65f6\uff0c\u4e5f\u6709\u5229\u4e8e\u5355\u8d28\u5149\u50ac\u5316\u5242\u7684\u53d1\u5c55\u3002<\/p>\n<p>\u8be5\u5de5\u4f5c\u53d1\u8868\u4e8eAngewandte Chemie\uff0c\u539f\u6587\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/wol1\/doi\/10.1002\/anie.201603331\/abstract\" target=\"_blank\">An Elemental Phosphorus Photocatalyst with a Record High Hydrogen Evolution Efficiency<\/a><\/p>\n<p>\u8be5\u6587\u732e\u5bfc\u8bfb\u7531\u6750\u6599\u4eba\u65b0\u80fd\u6e90\u5b66\u672f\u5c0f\u7ec4\u00a0 theory\u00a0\u00a0 \u4f9b\u7a3f\uff0c\u53c2\u4e0e\u65b0\u80fd\u6e90\u8bdd\u9898\u8ba8\u8bba\u8bf7\u52a0\u5165\u201c\u6750\u6599\u4eba\u65b0\u80fd\u6e90\u6750\u6599\u4ea4\u6d41\u7fa4 422065952\u201d\uff0c\u82e5\u60f3\u53c2\u4e0e\u65b0\u80fd\u6e90\u6587\u732e\u89e3\u8bfb\u548c\u6587\u732e\u6c47\u603b\u3001\u65b0\u80fd\u6e90\u77e5\u8bc6\u79d1\u666e\u548c\u6df1\u5ea6\u6316\u6398\u65b0\u80fd\u6e90\u5b66\u672f\u4ea7\u4e1a\u4fe1\u606f\uff0c\u8bf7\u52a0qq 2728811768\u3002<\/p>\n<p>\u6b22\u8fce\u5404\u5927\u8bfe\u9898\u7ec4\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u78f7\uff08P\uff09\u662f\u6700\u666e\u904d\u7684\u5143\u7d20\u4e4b\u4e00\uff0c\u5728\u5730\u7403\u4e0a\u7684\u50a8\u91cf\u6709\u5927\u7ea61000\u4ebf\u5428\uff0c\u4e14\u5728\u5316\u5b66\uff0c\u7269\u7406\u5b66\uff0c\u751f\u7269\u5b66\u548c\u751f\u6001\u5b66\u7b49\u9886\u57df\u5747\u5177\u6709\u91cd\u8981\u610f\u4e49\u3002\u81ea17\u4e16\u7eaa60\u5e74\u4ee3\u88ab\u53d1\u73b0\u4ee5\u6765\uff0c\u5bf9\u4e0d\u540c\u79cd\u7c7b\u7684P&#8230;<\/p>\n","protected":false},"author":90,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-13182","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/13182"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/90"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=13182"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/13182\/revisions"}],"predecessor-version":[{"id":13197,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/13182\/revisions\/13197"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=13182"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=13182"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=13182"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}