{"id":136829,"date":"2018-05-02T06:30:20","date_gmt":"2018-05-01T22:30:20","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=136829"},"modified":"2018-05-01T20:22:13","modified_gmt":"2018-05-01T12:22:13","slug":"%e6%be%b3%e5%a4%a7%e5%88%a9%e4%ba%9a%e6%82%89%e5%b0%bc%e7%a7%91%e6%8a%80%e5%a4%a7%e5%ad%a6%e6%b1%aa%e5%9b%bd%e7%a7%80%e7%a0%94%e7%a9%b6%e5%9b%a2%e9%98%9f%e5%9c%a8%e6%b5%b7%e6%b0%b4%e6%b7%a1%e5%8c%96","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=136829","title":{"rendered":"\u6fb3\u5927\u5229\u4e9a\u6089\u5c3c\u79d1\u6280\u5927\u5b66\u6c6a\u56fd\u79c0\u7814\u7a76\u56e2\u961f\u5728\u6d77\u6c34\u6de1\u5316\u65b9\u9762\u7684\u7814\u7a76\u53d6\u5f97\u91cd\u8981\u8fdb\u5c55"},"content":{"rendered":"<p><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/p>\n<p>\u8fdb\u5165\u4e8c\u5341\u4e00\u4e16\u7eaa,\u4f34\u968f\u7740\u4e16\u754c\u4eba\u53e3\u548c\u5168\u7403\u5de5\u4e1a\u5316\u8fdb\u7a0b\u7684\u5feb\u901f\u589e\u957f,\u80fd\u6e90\u4e0e\u73af\u5883\u95ee\u9898\u65e5\u76ca\u7a81\u51fa,\u7279\u522b\u662f\u5168\u7403\u7684\u6de1\u6c34\u8d44\u6e90\u5371\u673a,\u5df2\u7ecf\u523b\u4e0d\u5bb9\u7f13\u3002\u6c34\u8d44\u6e90\u7684\u7f3a\u4e4f\u4f7f\u6d77\u6c34\u6de1\u5316\u6280\u672f\u7684\u7814\u53d1\u66f4\u52a0\u7d27\u8feb\u3002\u4f20\u7edf\u7684\u8131\u76d0\u6280\u672f,\u5982\u53cd\u6e17\u900f\u3001\u7535\u6e17\u6790\u548c\u79bb\u5b50\u4ea4\u6362,\u7531\u4e8e\u5176\u672c\u8eab\u4e0d\u53ef\u5ffd\u89c6\u7684\u9ad8\u80fd\u8017\u53ca\u4f4e\u6548\u7387\u7b49\u95ee\u9898,\u5df2\u7ecf\u4e0d\u80fd\u6ee1\u8db3\u4eba\u7c7b\u96c6\u7ea6\u578b\u793e\u4f1a\u53d1\u5c55\u7684\u8981\u6c42\u3002<\/p>\n<p>\u7535\u5bb9\u53bb\u79bb\u5b50\u6280\u672f(Capacitive deionization, CDI) \u53c8\u79f0\u7535\u5438\u9644\u53bb\u79bb\u5b50\u6280\u672f,\u5b83\u5177\u6709\u8131\u76d0\u6548\u7387\u9ad8\u3001\u4f4e\u80fd\u8017\u3001\u73af\u5883\u53cb\u597d\u7b49\u4f18\u70b9, \u7535\u5438\u9644\u53bb\u79bb\u5b50(CDI)\u662f\u4e00\u79cd\u4ee4\u4eba\u5174\u594b\u7684\u7535\u5316\u5b66\u65b9\u6cd5\uff0c\u53ea\u9700\u8981\u4fdd\u6301\u4e24\u4e2a\u7531\u591a\u5b54\u6750\u6599\u5236\u4f5c\u7684\u7535\u6781\u4e4b\u95f4\u5b58\u5728\u7a33\u5b9a\u7684\u7535\u538b\uff0c\u9700\u51c0\u5316\u7684\u6c34\u4ece\u4e24\u5757\u7535\u6781\u4e4b\u95f4\u6d41\u8fc7\u4e4b\u540e\u5c31\u4f1a\u53d8\u6210\u6e05\u6d01\u6c34\uff0c\u4e0e\u84b8\u998f\u548c\u53cd\u6e17\u900f\u7b49\u66ff\u4ee3\u65b9\u6cd5\u4e0d\u540c\uff0c\u5b83\u65e2\u4e0d\u9700\u8981\u9ad8\u6e29\u4e5f\u4e0d\u9700\u8981\u538b\u529b\u6765\u64cd\u4f5c\u3002\u867d\u7136CDI\u6280\u672f\u7684\u4e3b\u8981\u6982\u5ff5\u65e9\u57281960\u5e74\u5c31\u5df2\u7ecf\u786e\u7acb\uff0c\u4f46\u4f20\u7edf\u7684\u78b3\u57faCDI\u7535\u6781\u53ea\u5728\u6eb6\u6db2\u76d0\u5ea6\u8f83\u4f4e\u65f6\uff0c\u8868\u73b0\u5f97\u8f83\u4e3a\u51fa\u8272\uff0c\u4ec5\u9002\u5408\u5904\u7406\u5fae\u54b8\u6c34\u800c\u4e0d\u662f\u6d77\u6c34\uff0c\u56e0\u6b64\uff0cCDI\u6280\u672f\u8fdb\u5165\u5de5\u4e1a\u89c4\u6a21\u7684\u6d77\u6c34\u6de1\u5316\u5e94\u7528\uff0c\u8feb\u5207\u9700\u8981\u5f00\u53d1\u9ad8\u6548\u7684\u65b0\u578b\u7535\u6781\u6750\u6599\u548c\u8bbe\u8ba1\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-136840\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/04\/QQ\u56fe\u724720180429123011-1.jpg\" alt=\"\" width=\"600\" height=\"607\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/04\/QQ\u56fe\u724720180429123011-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/04\/QQ\u56fe\u724720180429123011-1-297x300.jpg 297w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/p>\n<p>\u6fb3\u5927\u5229\u4e9a\u6089\u5c3c\u79d1\u6280\u5927\u5b66\u6c6a\u56fd\u79c0\u6559\u6388\u7814\u7a76\u56e2\u961f\u548c\u7f8e\u56fd\u5fb7\u96f7\u585e\u5c14\u5927\u5b66\u7684Yury Gogotsi\u6559\u6388\uff08\u5171\u540c\u901a\u8baf\uff09\u7814\u7a76\u56e2\u961f\u5728\u80fd\u6e90\u9886\u57df\u77e5\u540d\u671f\u520a\u300a\u7126\u8033\u300b<strong>Joule<\/strong> 2 (2018) 778 &#8211; 787\u4e0a\u53d1\u8868\u4e86\u8bba\u6587\uff0c\u9898\u4e3a\uff1a\u201cPorous Cryo-Dried MXene for Efficient Capacitive Deionization\u3002\u7814\u7a76\u4eba\u5458\u4ece\u50a8\u80fd\u7535\u6781\u6750\u6599\u7684\u7814\u7a76\u4e2d\u5f97\u5230\u542f\u53d1\uff0c\u4ed6\u4eec\u8bbe\u8ba1\u548c\u5236\u5907\u4e86\u4ee5\u6c14\u51dd\u80f6\u72b6\u591a\u5b54MXene\u4e3a\u8f7d\u4f53\u7684CDI\u5668\u4ef6\uff0c\u8be5\u5668\u4ef6\u5728\u9ad8\u6eb6\u6db2\u76d0\u5ea6\u4e2d\uff0c\u8868\u73b0\u51fa\u8272\uff0c\u80fd\u591f\u63d0\u4f9b\u6781\u9ad8\u7684\u7535\u5438\u9644\u80fd\u529b\uff0c\u5728\u6781\u9ad8\u6d53\u5ea6\u7684\u76d0\u6c34\uff0810000 \u6beb\u514b\/\u5347\uff09\u4e2d\u53ef\u83b7\u5f97\u4e86118 \u6beb\u514b\/\u5e73\u65b9\u5398\u7c73\u7684\u9ad8\u5438\u9644\u5bb9\u91cf\uff0c\u6bd4\u4f20\u7edf\u7684\u78b3\u57fa\u7535\u6781\u6750\u6599\u7684\u5438\u9644\u5bb9\u91cf\u9ad8\u51fa\u4e86\u4e00\u4e2a\u6570\u91cf\u7ea7\u3002\u591a\u5b54MXene-CDI\u5668\u4ef6\u663e\u8457\u7684\u63d0\u9ad8\u4e86CDI\u6280\u672f\u7684\u5438\u9644\u6548\u7387\uff0c\u4f7f\u5f97CDI\u6280\u672f\u7684\u53d1\u5c55\u8fdb\u5165\u5230\u4e86\u5de5\u4e1a\u89c4\u6a21\u7684\u6d77\u6c34\u6de1\u5316\u7684\u65b0\u9636\u6bb5\u3002<\/p>\n<p>\u4e8c\u7ef4\u7684\u91d1\u5c5e\u78b3\u5316\u7269\u6216\u6c2e\u5316\u7269\uff08MXenes\uff09\u4f5c\u4e3a\u65b0\u578b\u7684\u4e8c\u7ef4\u4e07\u80fd\u6750\u6599\uff0c\u5177\u6709\u9ad8\u6bd4\u8868\u9762\u79ef\u3001\u9ad8\u7535\u5bfc\u7387\u7684\u7279\u70b9\uff0c\u53c8\u5177\u5907\u7ec4\u5206\u7075\u6d3b\u53ef\u8c03\uff0c\u6700\u5c0f\u7eb3\u7c73\u5c42\u539a\u53ef\u63a7\u7b49\u4f18\u52bf\uff0c\u5728\u50a8\u80fd\u548c\u6c34\u5904\u7406\u4ee5\u53ca\u5149\u7535\u5316\u5b66\u50ac\u5316\u7b49\u9886\u57df\u62e5\u6709\u5de8\u5927\u6f5c\u529b\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-136841\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/04\/QQ\u56fe\u724720180429123027-1.jpg\" alt=\"\" width=\"775\" height=\"629\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/04\/QQ\u56fe\u724720180429123027-1.jpg 775w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/04\/QQ\u56fe\u724720180429123027-1-300x243.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/04\/QQ\u56fe\u724720180429123027-1-768x623.jpg 768w\" sizes=\"(max-width: 775px) 100vw, 775px\" \/><\/p>\n<p>\u591a\u5b54Ti3C2Tx-CDI\u5668\u4ef6\u7684\u7535\u5438\u9644\u7279\u6027: (A) \u4e0d\u540cNaCl\u6d53\u5ea6\u4e2d\uff0c\u591a\u5b54Ti3C2Tx-CDI\u5668\u4ef6\u4ee5\u53ca Ti3C2Tx-CDI\u5668\u4ef6\u548c\u6d3b\u6027\u70ad-CDI\u5668\u4ef6\u7684\u7535\u5438\u9644\u5bb9\u91cf\u66f2\u7ebf\uff08NaCl\u6d53\u5ea6\u7684\u4ece100 mg\/L\u81f31\u4e07mg\/L\uff09\u3002(B) 500 mg \/ L \u7684NaCl\u6d53\u5ea6\u4e2d\uff0c\u591a\u5b54Ti3C2Tx-CDI\u5668\u4ef6\u4ee5\u53ca Ti3C2Tx-CDI\u5668\u4ef6\u548c\u6d3b\u6027\u70ad-CDI\u5668\u4ef6\u7684\u7535\u5438\u9644\u5bb9\u91cf\u66f2\u7ebf\u3002(C) 500 mg \/ L \u7684NaCl\u6d53\u5ea6\u4e2d\uff0c\u591a\u5b54\u7535\u6781\u591a\u5b54Ti3C2Tx-CDI\u5668\u4ef6\u7684\u7535\u5438\u9644\u548c\u8131\u9644\u5faa\u73af\u66f2\u7ebf\u3002(D) 500mg \/L NaCl\u6eb6\u6db2\u4e2d\uff0c\u591a\u5b54Ti3C2Tx-CDI\u5668\u4ef6\u5728\u4e0d\u540c\u5de5\u4f5c\u7535\u538b\u4e0b\u7684\u7535\u5438\u9644\u5bb9\u91cf\u53d8\u5316\u3002<\/p>\n<p>\u4e3a\u4e86\u5229\u7528MXenes\u7684\u826f\u597d\u6027\u80fd\u4f5c\u4e3a\u7535\u6781\u6750\u6599\uff0c\u9700\u8981\u786e\u4fdd\u7535\u6781\u6750\u6599\u6709\u4e00\u4e2a\u8f83\u5927\u7684\u7684\u6bd4\u8868\u9762\u79ef\u4ee5\u8fbe\u5230\u6700\u5927\u7684\u7535\u5bb9\u5438\u9644\u548c\u79bb\u5b50\u4f20\u8f93\u3002\u7136\u800c\u7531\u4e8e\u8303\u5fb7\u74e6\u5c14\u65af\u5728\u5c42\u95f4\u7684\u4f5c\u7528\u529b\uff0c\u4f7f\u5f97\u88ab\u5265\u79bb\u7684MXne\u8584\u7247\u5bb9\u6613\u91cd\u65b0\u5806\u53e0\uff0c\u6bd4\u8868\u9762\u79ef\u51cf\u5c0f\uff0c\u7814\u7a76\u4eba\u5458\u5de7\u5999\u7684\u91c7\u7528\u6c2f\u4eff\u4f5c\u4e3a\u7f6e\u6362\u5206\u5b50\uff0c\u4f7f\u6c2f\u4eff\u6eb6\u5242\u5206\u5b50\u8fdb\u5165\u5230MXene\u8584\u7247\u4e2d\u7f6e\u6362\u5c42\u7ea7\u7684\u76f4\u5f84\u8f83\u5c0f\u7684\u79bb\u5b50\uff0c\u5e76\u8fdb\u4e00\u6b65\u7684\u6269\u5927\u5c42\u95f4\u8ddd\uff0c\u800c\u540e\u901a\u8fc7\u4f4e\u6e29\u771f\u7a7a\u51b7\u51bb\u5e72\u71e5\u6280\u672f\uff0c\u9664\u53bb\u6eb6\u5242\u5206\u5b50\uff0c\u5236\u5907\u8936\u76b1\u72b6\u7684\u4e09\u7ef4\u7684\u6c14\u51dd\u80f6\u72b6\u591a\u5b54MXene\u6750\u6599\u3002<\/p>\n<p>\u4ee5\u6c14\u51dd\u80f6\u72b6\u591a\u5b54MXene\u4e3a\u8f7d\u4f53\u7684\u8d85\u7ea7\u7535\u5bb9\u5668\u5668\u4ef6\u663e\u793a\u51fa\u4e86\u6781\u9ad8\u7684\u7535\u5bb9\u6bd4\u5bb9\u91cf\uff08410 F\/cm3 )\uff0c\u4e0e\u6b64\u540c\u65f6\uff0c\u5728\u76f8\u540c\u6d53\u5ea6\u7684\u76d0\u6c34\u4e2d\uff0c\u591a\u5b54MXene-CDI\u5668\u4ef6\u7684\u7535\u5bb9\u5438\u9644\u5bb9\u91cf\u53d1\u6325\u662f\u4f20\u7edf\u6d3b\u6027\u70ad-CDI\u5668\u4ef6\u768412.8\u500d\u4e4b\u591a\u3002\u6b64\u5916\uff0c\u591a\u5b54\u7535\u6781\u7ed3\u6784\u7684\u8bbe\u8ba1\u6709\u6548\u7684\u63d0\u9ad8\u4e86\u79bb\u5b50\u4f20\u8f93\u6027\u80fd\uff0c\u53ef\u5728\u8f83\u77ed\u7684\u65f6\u95f4\u5185\u8fbe\u5230\u4e86\u6700\u5927\u7684\u7535\u5438\u9644\u5bb9\u91cf\u3002<\/p>\n<p><strong>\u3010\u5c0f\u7ed3\u3011<\/strong><\/p>\n<p>\u591a\u5b54MXene-CDI\u5668\u4ef6\u7684\u6210\u529f\u5f00\u53d1\uff0c\u6709\u6548\u7684\u89e3\u51b3\u4e86\u4f20\u7edfCDI\u5668\u4ef6\u5728\u9ad8\u76d0\u6d53\u5ea6\u4e0b\uff0c\u5438\u9644\u6548\u7387\u4f4e\u7684\u79d1\u5b66\u96be\u9898\uff0c\u4f7f\u5f97\u7535\u5bb9\u5438\u9644\u6d77\u6c34\u6de1\u5316\u6280\u672f\u7684\u7814\u7a76\u5411\u524d\u8fc8\u51fa\u4e86\u91cd\u8981\u7684\u4e00\u6b65\uff0c\u4e3a\u6d77\u6c34\u6de1\u5316\u7684\u7814\u7a76\u63d0\u4f9b\u4e86\u65b0\u7684\u8bbe\u8ba1\u7814\u7a76\u601d\u8def\u3002<\/p>\n<p>\u4f5c\u4e3a\u300a\u7ec6\u80de\u300b\uff08Cell\uff09\u7684\u59ca\u59b9\u520a\uff0c\u300a\u7126\u8033\u300b\u662f\u4e00\u672c\u81f4\u529b\u4e8e\u5e94\u5bf9\u5168\u7403\u6311\u6218\u3001\u53d1\u5c55\u53ef\u6301\u7eed\u80fd\u6e90\u4e3a\u76ee\u6807\uff0c\u62a5\u9053\u80fd\u6e90\u9886\u57df\u6700\u65b0\u8fdb\u5c55\u7684\u77e5\u540d\u5b66\u672f\u671f\u520a\u3002<\/p>\n<p>\u8bba\u6587\u5f97\u5230\u4e86Joule \u6742\u5fd7\u7f16\u8f91\u90e8\u7684\u9ad8\u5ea6\u91cd\u89c6\uff0c\u64b0\u5199\u4e86\u9898\u4e3a\u201cMaxing Out Water Desalination with MXenes\u201d\u7684\u540c\u671f\u8bc4\u8ff0\uff0c\u5bf9\u8be5\u5de5\u4f5c\u8fdb\u884c\u4e86\u8be6\u7ec6\u4ecb\u7ecd\u548c\u89e3\u8bfb<\/p>\n<p>\u539f\u6587\u514d\u8d39\u4e0b\u8f7d\u94fe\u63a5:<a href=\"https:\/\/authors.elsevier.com\/a\/1WvS4925JE5pxA\">https:\/\/authors.elsevier.com\/a\/1WvS4925JE5pxA<\/a><\/p>\n<p>\u7f16\u8f91\u8bc4\u8ff0 \u539f\u6587\u4e0b\u8f7d\u94fe\u63a5\uff1ahttp:\/\/www.cell.com\/joule\/fulltext\/S2542-4351(18)30138-7<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u8fdb\u5165\u4e8c\u5341\u4e00\u4e16\u7eaa,\u4f34\u968f\u7740\u4e16\u754c\u4eba\u53e3\u548c\u5168\u7403\u5de5\u4e1a\u5316\u8fdb\u7a0b\u7684\u5feb\u901f\u589e\u957f,\u80fd\u6e90\u4e0e\u73af\u5883\u95ee\u9898\u65e5\u76ca\u7a81\u51fa,\u7279\u522b\u662f\u5168\u7403\u7684\u6de1\u6c34\u8d44\u6e90\u5371\u673a,\u5df2\u7ecf\u523b\u4e0d\u5bb9\u7f13\u3002\u6c34\u8d44\u6e90\u7684\u7f3a\u4e4f\u4f7f\u6d77\u6c34\u6de1\u5316\u6280\u672f\u7684&#8230;<\/p>\n","protected":false},"author":272,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215,2],"tags":[3134],"class_list":["post-136829","post","type-post","status-publish","format-standard","hentry","category-jiedu","category-keji","tag-3134"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/136829"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/272"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=136829"}],"version-history":[{"count":7,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/136829\/revisions"}],"predecessor-version":[{"id":137057,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/136829\/revisions\/137057"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=136829"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=136829"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=136829"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}