{"id":14023,"date":"2016-05-17T17:00:38","date_gmt":"2016-05-17T09:00:38","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=14023"},"modified":"2016-05-17T14:47:19","modified_gmt":"2016-05-17T06:47:19","slug":"%e9%a1%b6%e5%88%8a%e5%8a%a8%e6%80%81%e4%b8%a8natureeesnano-letters%e7%ad%89%e6%9c%9f%e5%88%8a%e7%94%b5%e5%ad%90%e6%9d%90%e6%96%99%e5%ad%a6%e6%9c%af%e8%bf%9b%e5%b1%95%e6%b1%87%e6%80%bb%ef%bc%884-28-5","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=14023","title":{"rendered":"\u9876\u520a\u52a8\u6001\u4e28Nature\/EES\/Nano Letters\u7b49\u671f\u520a\u7535\u5b50\u6750\u6599\u5b66\u672f\u8fdb\u5c55\u6c47\u603b\uff084.28-5.10\uff09"},"content":{"rendered":"<p><strong>\u672c\u671f\u5bfc\u8bfb\uff1a<br \/>\n<\/strong><br \/>\n\u4eca\u5929\u7535\u5b50\u7535\u5de5\u6750\u6599\u5468\u62a5\u7ec4\u9080\u60a8\u4e00\u8d77\u6765\u770b\u770bNature communications\/ACS Nano\/EES\u7b49\u671f\u520a\u7535\u5b50\u6750\u6599\u9886\u57df\u6700\u65b0\u7684\u7814\u7a76\u8fdb\u5c55\u3002\u672c\u671f\u5185\u5bb9\u9884\u89c8\uff1a\u8ba1\u7b97\u673a\u4e0b\u7684\u6750\u6599\uff1a\u5355\u5c42Be5C2\u6709\u5e94\u7528\u4e8e\u7535\u5b50\u8bbe\u5907\u7684\u524d\u666f\uff1b\u5229\u7528\u6709\u673a\u94c1\u7535\u4f53\u4ea7\u751f\u96a7\u9053\u7535\u81f4\u7535\u963b\u6548\u5e94\uff1b\u586b\u5145\u7535\u8d1f\u6027\u79bb\u5b50\uff0c\u63d0\u9ad8\u65b9\u94b4\u77ff\u6750\u6599\u70ed\u7535\u6027\uff1b\u8367\u5149\u7eb3\u7c73\u94bb\u77f3\u7684\u53f0\u5f0f\u6c1f\u5316\u6cd5\uff1b\u667a\u80fd\u57ce\u5e02\u4e2d\u592a\u9633\u80fd\u548c\u98ce\u80fd\u7684\u6709\u6548\u6536\u96c6\uff1b3D\u6253\u5370\u9ad8\u6e29\u9ad8\u6548\u7387\u52a0\u70ed\u5668\uff1b\u4e00\u79cd\u5f3a\u5927\u78c1\u529f\u80fd\u7684\u5355\u5206\u5b50\u78c1\u4f53\uff1b\u63a5\u8fd1\u8026\u5408\u7684\u9ad8\u6e29\u94c1\u78c1\u62d3\u6251\u7edd\u7f18\u76f8\uff1bSnxSb1-xTe\u6750\u6599\u4f4e\u70ed\u5bfc\u7387\u7684\u6839\u6e90\uff1b\u81ea\u4f9b\u7535\u7684\u53ef\u7a7f\u6234\u7535\u5b50\u4ea7\u54c1\u7684\u70ed\u7535\u80fd\u6e90\u4ea7\u751f\u5668\u8bbe\u8ba1\uff1b\u591a\u5c42\u77f3\u58a8\u70ef\u7ed3\u6784\u6781\u5927\u5730\u63d0\u9ad8\u4e86\u77f3\u58a8\u70ef\/\u73af\u6c27\u6811\u8102\u590d\u5408\u6750\u6599\u7684\u70ed\u5bfc\u7387\u3002<\/p>\n<p><strong>1\u3001Nature communications: \u8ba1\u7b97\u673a\u4e0b\u7684\u6750\u6599\uff1a\u5355\u5c42Be5C2\u6709\u5e94\u7528\u4e8e\u7535\u5b50\u8bbe\u5907\u7684\u524d\u666f<\/strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14024\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72471-16.jpg\" alt=\"\u56fe\u72471\" width=\"431\" height=\"367\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72471-16.jpg 431w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72471-16-300x255.jpg 300w\" sizes=\"(max-width: 431px) 100vw, 431px\" \/>\u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 <strong>\u5355\u5c42Be5C2\u7684\u51e0\u4f55\u7ed3\u6784\u53ca\u7535\u5b50\u7ed3\u6784<\/strong><\/p>\n<p>\u4ece\u62d3\u6251\u6027\u8d28\u53ca\u51cf\u5c11\u7ef4\u5ea6\u65b9\u9762\u8bbe\u8ba1\uff0c\u5f80\u5f80\u53ef\u83b7\u5f97\u65b0\u578b\u6750\u6599\u3002C\u5c31\u662f\u4e00\u4e2a\u4f8b\u5b50\uff0c\u5b83\u53ef\u4e0e\u5176\u4ed6\u539f\u5b50\u5f62\u6210\u5e73\u9762\u56db\u914d\u4f4d\u7ed3\u6784(ptC)\u3001\u5e73\u9762\u4e94\u914d\u4f4d\u7ed3\u6784(ppC)\u548c\u5e73\u9762\u516d\u914d\u4f4d\u7ed3\u6784(phC)\uff0c\u8fd9\u4e9b\u6253\u7834\u5e38\u89c4\u5316\u5b66\u952e\u7684\u591a\u914d\u4f4dC\u5206\u5b50\uff0c\u5e38\u4ee5\u5176\u8f83\u4f4e\u7684\u80fd\u91cf\u7ed3\u6784\u53ef\u5e94\u7528\u4e8e\u7535\u5b50\u8bbe\u5907\u4e2d\u3002\u4f46\u5bf9\u6bd4ptC\u548cphC\uff0cppC\u6781\u5c11\u6269\u5c55\u5230\u56fa\u4f53\u7814\u7a76\u9886\u57df\u3002<\/p>\n<p>\u6765\u81ea\u5357\u4eac\u5e08\u8303\u5927\u5b66\u548c\u6ce2\u591a\u9ece\u5404\u5927\u5b66\u7684\u7814\u7a76\u8005\u4eec\u5bf9ppC\u80fd\u5426\u6269\u5c55\u5230\u56fa\u4f53\u9886\u57df\u8fdb\u884c\u4e86\u7814\u7a76\uff0c\u5e76\u57fa\u4e8e\u5bc6\u5ea6\u6cdb\u51fd\u7406\u8bba\u8ba1\u7b97\uff0c\u8bbe\u8ba1\u4e86\u4e8c\u7ef4\u6750\u6599\u2014\u2014\u5355\u5c42Be5C2\u3002\u56e0\u9002\u5ea6\u7684\u5185\u805a\u80fd\u3001\u6d3b\u8dc3\u7684\u58f0\u5b50\u6a21\u53ca\u9ad8\u7194\u70b9\uff0c\u5355\u5c42Be5C2\u8868\u73b0\u51fa\u5f88\u597d\u7684\u7a33\u5b9a\u6027\u3002\u540c\u65f6Be5C2\u5728\u4e8c\u7ef4\u7a7a\u95f4\u4e2d\u662f\u6700\u4f4e\u80fd\u7ed3\u6784\uff0c\u56e0\u6b64\u5f88\u6709\u53ef\u80fd\u5b9e\u73b0\u5b9e\u9a8c\u5408\u6210\u3002\u5355\u5c42Be5C2\u662f\u4e00\u79cd\u65e0\u80fd\u9699\u534a\u5bfc\u4f53\uff0c\u80fd\u5e26\u7ed3\u6784\u4e2d\u5177\u72c4\u62c9\u514b\u70b9\uff0c\u6cca\u677e\u6bd4\u4e3a\u8d1f\u503c\u3002\u56e0\u6b64\u82e5\u6210\u529f\u5408\u6210\uff0c\u5c06\u5728\u7535\u5b50\u53ca\u673a\u68b0\u8bbe\u5907\u4e2d\u6709\u5f88\u5927\u7684\u5e94\u7528\u524d\u666f\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/www.nature.com\/ncomms\/2016\/160503\/ncomms11488\/full\/ncomms11488.html\" target=\"_blank\"><strong>Semi-metallic Be5C2 monolayer global minimum with quasi-planar pentacoordinate carbons and negative Poisson\u2019s ratio<\/strong><\/a><\/p>\n<p><strong>2\u3001Nature communications: \u5229\u7528\u6709\u673a\u94c1\u7535\u4f53\u4ea7\u751f\u96a7\u9053\u7535\u81f4\u7535\u963b\u6548\u5e94<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14025\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72472-13.jpg\" alt=\"\u56fe\u72472\" width=\"500\" height=\"388\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72472-13.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72472-13-300x233.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/>\u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0<strong> \u5728\u8d85\u8584PVDF\u819c\u4e0a\u7684\u94c1\u7535\u6027<\/strong><\/p>\n<p>\u5728\u94c1\u7535\u4f53\u96a7\u9053\u7ed3(FTJs)\u4e2d\uff0c\u8f6c\u6362\u4e24\u4e2a\u7535\u6781\u95f4\u7684\u8d85\u8584\u94c1\u7535\u58c1\u5792\u7684\u6781\u5316\u6765\u8c03\u8282\u96a7\u9053\u7535\u963b\uff0c\u4f1a\u5f15\u8d77\u5de8\u5927\u7684\u96a7\u9053\u7535\u81f4\u7535\u963b\u6548\u5e94(TER)\uff0c\u5229\u7528TER\u6548\u5e94\u53ef\u5236\u5907\u975e\u6613\u5931\u6027\u5b58\u50a8\u5668\u3002\u76ee\u524d\uff0c\u5927\u591a\u6570\u94c1\u7535\u58c1\u5792\u4e3a\u65e0\u673a\u7684\u9499\u949b\u77ff\u6c27\u5316\u7269\u8584\u819c\uff0c\u4f46\u8981\u5b9e\u73b0\u7eb3\u7c73\u5c3a\u5bf8\uff0c\u5236\u4f5c\u5de5\u827a\u4f1a\u975e\u5e38\u590d\u6742\uff0c\u96be\u4ee5\u5b9e\u73b0\u5927\u89c4\u6a21\u751f\u4ea7\u3002<\/p>\n<p>\u7531\u4e0a\u6d77\u548c\u6cd5\u56fd\u591a\u6240\u9662\u6821\u7ec4\u6210\u7684\u7814\u7a76\u56e2\u961f\u5c06\u6709\u673a\u7684PVDF\u8584\u819c\u4f5c\u4e3a\u94c1\u7535\u58c1\u5792\uff0c\u8c03\u8282\u5b83\u7684\u6781\u5316\u72b6\u6001\u53ef\u7f16\u7801\u5b58\u50a8\u4fe1\u606f\uff0c\u5e76\u8bfb\u51fa\u96a7\u9053\u7535\u6d41\u4ece\u800c\u5236\u5907\u51fa\u975e\u6613\u5931\u6027\u7684\u5b58\u50a8\u5668\u3002\u5bf9\u4e8e\u4e00\u5230\u4e8c\u5c42\u7684\u94c1\u7535\u805a\u5408\u7269\uff0c\u4ec5\u9700\u5f88\u4f4e\u7684\u7535\u538b\u5c31\u53ef\u5b9e\u73b0\u6781\u5316\u8f6c\u6362\u3002\u5e76\u4e14\u5728\u5ba4\u6e29\u4e0b\uff0c\u8fd9\u4e9b\u8584\u819c\u4e0a\u7684\u8d85\u5fae\u7c73\u7ea7\u96a7\u9053\u7ed3\u5c31\u80fd\u5c55\u73b0\u51fa1000%\u7684\u96a7\u9053\u7535\u81f4\u7535\u963b\u6548\u5e94\u3002\u540c\u65f6\uff0c\u7814\u7a76\u8005\u4eec\u4e5f\u63d0\u51fa\u5728\u7845\u6216\u5176\u4ed6\u67d4\u6027\u886c\u5e95\u4e0a\u5236\u5907\u6709\u673a\u94c1\u7535\u96a7\u9053\u7ed3\u7684\u4f4e\u6210\u672c\u3001\u5927\u89c4\u6a21\u5236\u5907\u7684\u65b9\u6cd5\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/www.nature.com\/ncomms\/2016\/160504\/ncomms11502\/full\/ncomms11502.html\" target=\"_blank\"><strong>Tunnel electroresistance through organic ferroelectric<\/strong>s<\/a><\/p>\n<p><strong>3\u3001Energy &amp; Environmental Science: \u586b\u5145\u7535\u8d1f\u6027\u79bb\u5b50\uff0c\u63d0\u9ad8\u65b9\u94b4\u77ff\u6750\u6599\u70ed\u7535\u6027<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14026\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72473-10.jpg\" alt=\"\u56fe\u72473\" width=\"500\" height=\"248\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72473-10.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72473-10-300x149.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/>\u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0<strong>\u586b\u5145\u7535\u8d1f\u6027\u79bb\u5b50\u540e\u65b9\u94b4\u77ff\u7684\u5f62\u6210\u80fd\u53ca\u6676\u683c\u70ed\u5bfc\u7387<\/strong><\/p>\n<p>\u901a\u8fc7\u5411\u4e3b\u6846\u67b6\u4e2d\u586b\u5145\u5176\u4ed6\u5143\u7d20\u5f62\u6210\u5305\u5408\u5316\u5408\u7269\u53ef\u8bbe\u8ba1\u51fa\u5177\u65b0\u529f\u80fd\u7684\u6750\u6599\uff0c\u800c\u5927\u591a\u662f\u5411\u5e26\u8d1f\u7535\u7684\u6846\u67b6\u4e2d\u586b\u5165\u7535\u6b63\u6027\u79bb\u5b50\u3002\u4e3a\u63d0\u9ad8\u65b9\u94b4\u77ff\u70ed\u7535\u6750\u6599\u7684\u6027\u80fd\uff0c\u4e5f\u53ef\u901a\u8fc7\u586b\u5145\u7535\u6b63\u6027\u79bb\u5b50\u3002\u4f46\u5411\u65b9\u94b4\u77ff\u4e2d\u586b\u5145\u7535\u8d1f\u6027\u79bb\u5b50\u5374\u5f88\u5c11\u6709\u7814\u7a76\u3002<\/p>\n<p>\u6765\u81ea\u6b66\u6c49\u7406\u5de5\u3001\u4e0a\u6d77\u5927\u5b66\u53ca\u534e\u76db\u987f\u5927\u5b66\u7684\u7814\u7a76\u56e2\u961f\u5219\u7814\u7a76\u4e86\u4e00\u7cfb\u5217\u7535\u8d1f\u6027\u79bb\u5b50\u586b\u5145\u81f3\u65b9\u94b4\u77ff\u540e\u8868\u73b0\u7684\u6027\u80fd\u3002\u7814\u7a76\u8868\u660e\u586b\u5165VIA\u65cf\u5143\u7d20\u5982S\u3001Se\u540e\uff0cS\u3001Se\u4f1a\u4e0e\u6846\u67b6\u4e3b\u5143\u7d20\u5f62\u6210\u5f3a\u6781\u6027\u7684\u5171\u4ef7\u952e\uff0c\u5bf9\u6676\u683c\u52a8\u529b\u5b66\u3001\u5143\u7d20\u586b\u5145\u540e\u5e26\u6765\u7684\u70b9\u7f3a\u9677\u5206\u5e03\u90fd\u4ea7\u751f\u5f88\u5927\u7684\u5f71\u54cd\uff0c\u5bfc\u81f4\u5f88\u4f4e\u7684\u6676\u683c\u70ed\u5bfc\u7387\u3002\u8fd9\u79cd\u5177\u5f00\u653e\u7ed3\u6784\u7684\u529f\u80fd\u5305\u5408\u5316\u5408\u7269\u5c06\u53ef\u7528\u4e8e\u5236\u5907\u9ad8\u6548\u7684\u70ed\u7535\u6750\u6599\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.rsc.org\/en\/content\/articlelanding\/2016\/ee\/c6ee00322b\" target=\"_blank\"><strong>Electronegative guests in CoSb3<\/strong><\/a><\/p>\n<p><strong>4\u3001AFM\uff1a \u8367\u5149\u7eb3\u7c73\u94bb\u77f3\u7684\u53f0\u5f0f\u6c1f\u5316\u6cd5<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14027\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72474-10.jpg\" alt=\"\u56fe\u72474\" width=\"360\" height=\"464\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72474-10.jpg 360w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72474-10-233x300.jpg 233w\" sizes=\"(max-width: 360px) 100vw, 360px\" \/>\u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 <strong>NDs\u6c1f\u5316\u7684\u50ac\u5316\u5faa\u73af\u7b80\u5316\u65b9\u6848<\/strong><\/p>\n<p>\u6c1f\u5316\u4f5c\u7528\u80fd\u8c03\u8282\u94bb\u77f3\u7684\u5149\u5b66\u6027\u80fd\u548c\u7535\u78c1\u5b66\u6027\u80fd\uff0c\u5e76\u80fd\u4ea7\u751f\u758f\u6c34\u8868\u9762\u3002\u8fd1\u671f\u7684\u4e00\u4e9b\u7814\u7a76\u8868\u660e\u6c1f\u5316\u4f5c\u7528\u8fd8\u80fd\u7a33\u5b9a\u94bb\u77f3\u3001\u7eb3\u7c73\u94bb\u77f3\u7684\u8367\u5149NV\u8272\u5fc3\u3002\u8367\u5149NV\u8272\u5fc3\u4f5c\u4e3a\u7075\u654f\u5ea6\u6781\u9ad8\u7684\u5355\u539f\u5b50\u7f3a\u9677\u5728\u91cf\u5b50\u7269\u7406\u548c\u9ad8\u5206\u8fa8\u751f\u7269\u6210\u50cf\u7b49\u4e00\u7cfb\u5217\u4f20\u611f\u5668\u65b9\u9762\u6709\u5e7f\u6cdb\u5e94\u7528\u3002\u7136\u800c\uff0c\u4f20\u7edf\u7684\u78b3\u7eb3\u7c73\u6750\u6599\u7684\u6c1f\u5316\u65b9\u6cd5\u5b9e\u9a8c\u6761\u4ef6\u82db\u523b\u590d\u6742\uff0c\u4ea7\u751f\u7684\u758f\u6c34\u8868\u9762\u5728\u65e0\u6c34\u73af\u5883\u4e2d\u5206\u6563\u6027\u5dee\u3002<\/p>\n<p>\u8fd1\u65e5\uff0cJan Havlik\u7b49\u4eba\u62a5\u9053\u4e86\u4e00\u79cdAg+\u50ac\u5316\u7684\u53f0\u5f0f\u6c1f\u5316\u65b9\u6cd5\u3002\u8be5\u65b9\u6cd5\u6761\u4ef6\u6e29\u548c\uff0c\u80fd\u5c06\u7fa7\u57fa\u5168\u90e8\u7528\u6c1f\u53d6\u4ee3\uff0c\u4ece\u800c\u5b9e\u73b0\u7eb3\u7c73\u94bb\u77f3\u7684\u6c1f\u5316\u3002\u548c\u5176\u4ed6\u65b9\u6cd5\u76f8\u6bd4\u8f83\uff0c\u8fd9\u79cd\u65b9\u6cd5\u4ea7\u7387\u9ad8\uff0c\u4e0d\u4f1a\u8150\u8680\u94bb\u77f3\u7684\u78b3\u539f\u5b50\uff0c\u8fd8\u80fd\u4ea7\u751f\u5e26\u6709C-F\u548cC-OH\u7aef\u57fa\u7684\u4eb2\u6c34\u8868\u9762\u3002C-F\u548cC-OH\u5b98\u80fd\u56e2\u6291\u5236\u4e86\u6709\u5bb3\u7684\u758f\u6c34\u8868\u9762\u53ca\u5176\u5bfc\u81f4\u7684\u7eb3\u7c73\u94bb\u77f3\u7684\u80f6\u4f53\u4e0d\u7a33\u5b9a\u6027\u3002\u7814\u7a76\u8fd8\u8868\u660e\u5373\u4f7f\u8868\u9762\u6c1f\u539f\u5b50\u5bc6\u5ea6\u76f8\u5bf9\u4f4e\u4e00\u4e9b\u4e5f\u6709\u52a9\u4e8e\u589e\u52a0\u7535\u8d1f\u6027NV\u8272\u5fc3\u7684\u7a33\u5b9a\u6027\uff0c\u63d0\u9ad8\u8367\u5149\u53d1\u5149\u3002Jan Havlik\u7b49\u4eba\u7684\u65b9\u6cd5\u80fd\u540c\u65f6\u63d0\u9ad8\u8868\u9762\u4eb2\u6c34\u6027\u548cNV\u8272\u5fc3\u8367\u5149\u53d1\u5149\uff0c\u8fd9\u6b63\u662f\u5c06\u8367\u5149\u7eb3\u7c73\u94bb\u77f3\u4f5c\u4e3a\u7eb3\u7c73\u4f20\u611f\u5668\u76f4\u63a5\u5e94\u7528\u4e8e\u751f\u7269\u73af\u5883\u4e2d\u7684\u91cf\u5b50\u5149\u5b66\u548c\u78c1\u5b66\u6d4b\u91cf\u7684\u5173\u952e\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adfm.201504857\/full\" target=\"_blank\"><strong>Benchtop Fluorination of Fluorescent Nanodiamonds on a Preparative Scale: Toward Unusually Hydrophilic Bright Particles<\/strong><\/a><\/p>\n<p><strong>5\u3001ACS Nano\uff1a\u667a\u80fd\u57ce\u5e02\u4e2d\u592a\u9633\u80fd\u548c\u98ce\u80fd\u7684\u6709\u6548\u6536\u96c6<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14028\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72475-8.jpg\" alt=\"\u56fe\u72475\" width=\"400\" height=\"242\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72475-8.jpg 400w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72475-8-300x182.jpg 300w\" sizes=\"(max-width: 400px) 100vw, 400px\" \/><strong>a.\u5e38\u89c4\u98ce\u529b\u53d1\u7535\u673a\u7ec4\uff1bb.\u57ce\u5e02\u5efa\u7b51\u5c4b\u9876\u4e0a\u7684\u96c6\u6210\u5316SC\u5355\u5143\uff1bc.\u623f\u5b50\u5c4b\u9876\u4e0a\u96c6\u6210\u4e86\u7eb3\u7c73\u53d1\u7535\u673a\u7684\u6a21\u578b\u793a\u610f\u56fe<\/strong><\/p>\n<p>\u4e3a\u4e86\u5b9e\u73b0\u667a\u80fd\u57ce\u5e02\u7684\u53ef\u6301\u7eed\u80fd\u6e90\u4f9b\u7ed9\uff0c\u6700\u5927\u5316\u57ce\u5e02\u4e2d\u7684\u80fd\u91cf\u6536\u96c6\u5bf9\u5b9e\u73b0\u4e00\u4e9b\u667a\u80fd\u8bbe\u5907\u548c\u4f20\u611f\u5668\u7684\u81ea\u6211\u4f9b\u80fd\u529f\u80fd\u6765\u8bf4\u662f\u5fc5\u8981\u7684\u3002\u73b0\u6709\u7684\u6280\u672f\u5df2\u7ecf\u53ef\u4ee5\u5bf9\u592a\u9633\u80fd\u8fdb\u884c\u6709\u6548\u6536\u96c6\uff0c\u7136\u800c\uff0c\u7531\u4e8e\u4f20\u7edf\u7684\u98ce\u80fd\u53d1\u7535\u8bbe\u5907\u4f53\u79ef\u5927\uff0c\u4e0d\u5b89\u5168\uff0c\u53ea\u80fd\u5b89\u88c5\u5728\u504f\u8fdc\u5730\u533a\uff0c\u6240\u4ee5\u57ce\u5e02\u4e2d\u7684\u98ce\u80fd\u8fd8\u4e0d\u80fd\u88ab\u6709\u6548\u5229\u7528\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u6765\u81ea\u4e2d\u79d1\u9662\u7684\u7814\u7a76\u4eba\u5458\u8bbe\u8ba1\u4e86\u4e00\u6b3e\u6df7\u5408\u7eb3\u7c73\u53d1\u7535\u673a\uff0c\u5305\u62ec\u4e00\u4e2a\u592a\u9633\u80fd\u7535\u6c60\u548c\u4e00\u4e2a\u6469\u64e6\u8d77\u7535\u7684\u7eb3\u7c73\u53d1\u7535\u673a\u3002\u8fd9\u6b3e\u53d1\u7535\u673a\u53ef\u4ee5\u5355\u72ec\u6216\u540c\u65f6\u6536\u96c6\u592a\u9633\u80fd\u548c\u98ce\u80fd\uff0c\u80fd\u5728\u57ce\u5e02\u5efa\u7b51\u9876\u90e8\u5927\u91cf\u5b89\u88c5\u3002\u8bbe\u5907\u9762\u79ef\u7ea6\u4e3a120mm\u00d722mm\u65f6\uff0c\u8bbe\u5907\u4e2d\u7684\u592a\u9633\u80fd\u7535\u6c60\u6700\u5927\u8f93\u51fa\u529f\u7387\u4e3a8mV\uff0c\u800c\u6469\u64e6\u8d77\u7535\u7eb3\u7c73\u53d1\u7535\u673a\u6700\u5927\u8f93\u51fa\u529f\u7387\u53ef\u8fbe26mV\u3002\u901a\u8fc7\u4f7f\u7528\u4e00\u53f0\u8f6c\u6362\u5668\u964d\u4f4e\u6469\u64e6\u8d77\u7535\u53d1\u7535\u673a\u7684\u963b\u6297\u5b9e\u73b0\u4e86\u592a\u9633\u80fd\u7535\u6c60\u548c\u7eb3\u7c73\u53d1\u7535\u673a\u7684\u963b\u6297\u5339\u914d\u3002\u548c\u5355\u4e00\u7684\u592a\u9633\u80fd\u7535\u6c60\u6216\u6469\u64e6\u8d77\u7535\u7eb3\u7c73\u53d1\u7535\u673a\u76f8\u6bd4\uff0c\u8fd9\u79cd\u6df7\u5408\u7eb3\u7c73\u53d1\u7535\u673a\u7684\u8f93\u51fa\u7535\u6d41\u66f4\u5927\uff0c\u7535\u6027\u80fd\u66f4\u4f18\u5f02\u3002\u4e2d\u79d1\u9662\u7684\u8fd9\u9879\u7814\u7a76\u4e3a\u5728\u57ce\u5e02\u4e2d\u6700\u5927\u53ef\u80fd\u7684\u6536\u96c6\u592a\u9633\u80fd\u548c\u98ce\u80fd\u63d0\u4f9b\u4e86\u53ef\u884c\u65b9\u6848\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acsnano.6b02575\" target=\"_blank\"><strong>Efficient Scavenging of Solar and Wind Energies in a Smart City<\/strong><\/a><\/p>\n<p><strong>6\u3001ACS Nano\uff1a3D\u6253\u5370\u9ad8\u6e29\u9ad8\u6548\u7387\u52a0\u70ed\u5668<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14029\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72476-10.jpg\" alt=\"\u56fe\u72476\" width=\"500\" height=\"347\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72476-10.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72476-10-300x208.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/>\u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 <strong>\u00a0 \u00a03D\u6253\u5370\u52a0\u70ed\u5668\u539f\u7406\u6f14\u793a<\/strong><\/p>\n<p>\u9ad8\u6e29\u52a0\u70ed\u5668\u53ef\u4ee5\u5e7f\u6cdb\u5e94\u7528\u4e8e\u6750\u6599\u5408\u6210\u548c\u5668\u4ef6\u52a0\u5de5\u3002\u9a6c\u91cc\u5170\u5927\u5b66\u5e15\u514b\u5206\u6821\u7684\u7814\u7a76\u4eba\u5458\u5f00\u53d1\u51fa\u4e86\u4e09\u7ef4\uff083D\uff09\u5370\u5237\u6c27\u5316\u8fd8\u539f\u77f3\u58a8\u70ef\uff08RGO\uff09\u578b\u52a0\u70ed\u5668\uff0c\u8fd9\u662f\u4e00\u79cd\u5177\u6709\u9ad8\u6e29\u548c\u8d85\u5feb\u52a0\u70ed\u901f\u7387\u7684\u9ad8\u6027\u80fd\u70ed\u4f9b\u7ed9\u8bbe\u5907\u3002\u4e0e\u5176\u4ed6\u70ed\u6e90\u5982\u70ed\u5904\u7406\u7089\u3001\u6fc0\u5149\u548c\u7ea2\u5916\u8f90\u5c04\u52a0\u70ed\u5668\u76f8\u6bd4\uff0c3D\u6253\u5370\u52a0\u70ed\u5668\u5177\u6709\u4ee5\u4e0b\u7684\u4f18\u70b9\uff1a\uff081\uff09\u7531\u4e8e\u8be5\u79cd\u52a0\u70ed\u5668\u662f\u4ee5\u53ef\u6301\u7eed\u9ad8\u6e29\u78b3\u6750\u6599\u2014\u2014\u8fd8\u539f\u6c27\u5316\u77f3\u58a8\u70ef\u4e3a\u57fa\u7840\u7684\uff0c\u5176\u64cd\u4f5c\u6e29\u5ea6\u53ef\u9ad8\u8fbe3000K\uff1b\uff082\uff09\u52a0\u70ed\u5668\u7684\u6e29\u5ea6\u53ef\u4ee5\u4ee520000K\/S\u7684\u6781\u5feb\u901f\u5ea6\u4e0a\u5347\u6216\u8005\u4e0b\u964d\uff1b\uff083\uff09\u53ef\u4ee5\u76f4\u63a5\u6253\u5370\u4e0d\u540c\u5f62\u72b6\u7684\u5c0f\u5c3a\u5bf8\u52a0\u70ed\u5668\uff0c\u4ee5\u786e\u4fdd\u4e0d\u540c\u7684\u57fa\u4f53\u4e0a\u6240\u6709\u533a\u57df\u90fd\u53ef\u4ee5\u52a0\u70ed\u30023D\u6253\u5370\u7684\u8fd8\u539f\u6c27\u5316\u77f3\u58a8\u578b\u52a0\u70ed\u5668\u53ef\u5e7f\u6cdb\u5730\u5e94\u7528\u4e8e\u7eb3\u7c73\u5236\u9020\uff0c\u53ef\u7cbe\u786e\u5730\u63a7\u5236\u6e29\u5ea6\u3001\u65f6\u95f4\u3001\u4f4d\u7f6e\u548c\u5347\u6e29\u901f\u7387\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acsnano.6b01059\" target=\"_blank\"><strong>Three-Dimensional Printable High-Temperature and High-Rate Heaters<\/strong><\/a><\/p>\n<p><strong>7\u3001ACS Nano\uff1a\u4e00\u79cd\u5f3a\u5927\u78c1\u529f\u80fd\u7684\u5355\u5206\u5b50\u78c1\u4f53<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14030\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72477-10.jpg\" alt=\"\u56fe\u72477\" width=\"400\" height=\"269\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72477-10.jpg 400w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72477-10-300x202.jpg 300w\" sizes=\"(max-width: 400px) 100vw, 400px\" \/>\u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0<strong> \u00a0 \u00a0[DyPyNO]2\u7684\u5206\u5b50\u7ed3\u6784<br \/>\n<\/strong><br \/>\n\u5355\u5206\u5b50\u78c1\u4f53\u7684\u7ec4\u7ec7\u901a\u8fc7\u8868\u9762\u70ed\u5347\u534e\uff0c\u4e3a\u672a\u6765\u8bbe\u5907\u7684\u53d1\u5c55\u548c\u5229\u7528\u8fd9\u4e9b\u78c1\u5206\u5b50\u6765\u4e30\u5bcc\u81ea\u65cb\u7535\u5b50\u5b66\u4e2d\u7684\u78c1\u6027\u80fd\u63d0\u4f9b\u4e86\u524d\u63d0\u6761\u4ef6\u3002\u7136\u800c\uff0c\u901a\u8fc7\u89c2\u5bdf\u53d1\u73b0\uff0c\u4e00\u4e9b\u7279\u5b9a\u7684\u8868\u9762\u4f1a\u53d1\u751f\u76f8\u4e92\u4f5c\u7528\uff0c\u4ece\u800c\u4f7f\u5355\u5206\u5b50\u78c1\u4f53\u7684\u6027\u80fd\u4e5f\u53d1\u751f\u53d8\u5316\u3002<\/p>\n<p>Evan Kiefl\u7b49\u4eba\u63d0\u51fa\u4e86\u4e00\u4e2a\u5355\u5206\u5b50\u78c1\u4f53\u7cfb\u7edf\u7684\u7f55\u89c1\u4f8b\u5b50\uff0c\u5728\u91d1\u7684\u8868\u9762\u53ef\u4ee5\u53d1\u751f\u70ed\u5347\u534e\u800c\u4fdd\u6301\u5176\u5b8c\u6574\u7684\u5316\u5b66\u7ed3\u6784\u548c\u78c1\u6027\u80fd\u3002\u901a\u8fc7\u6d4b\u91cf\u4ea4\u6d41\u78c1\u5316\u7387\u8868\u660e\u4ecb\u5b50\u81ea\u65cb\u51cf\u5f31\uff0c\u4f46\u4e0d\u540c\u4e8e\u5176\u4ed6\u7684\u5355\u5206\u5b50\u78c1\u4f53\uff0c\u8584\u819c\u72b6\u7684\u78c1\u4f53\u7279\u6027\u4e0e\u90a3\u4e9b\u5757\u72b6\u78c1\u4f53\u975e\u5e38\u76f8\u4f3c\uff0c\u5305\u62ec\u6574\u4e2a\u8584\u819c\u78c1\u4f53\u5168\u90e8\u8868\u9762\u4ee5\u53ca\u9644\u8fd1\u7684\u91d1\u5c5e\u771f\u7a7a\u63a5\u53e3\u533a\u57df\u3002\u8fd9\u4e9b\u90fd\u5c55\u793a\u4e86\u5355\u5206\u5b50\u78c1\u4f53\u7a33\u5b9a\u7684\u5316\u5b66\u6027\u80fd\u548c\u590d\u6742\u7684\u78c1\u6027\u80fd\uff0c\u4e3a\u5355\u5206\u5b50\u78c1\u4f53\u7eb3\u7c73\u7ed3\u6784\u7684\u53d1\u5c55\u63d0\u4f9b\u4e86\u7ebf\u7d22\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acsnano.6b01817\" target=\"_blank\"><strong>Robust Magnetic Properties of a Sublimable Single-Molecule Magnet<\/strong><\/a><\/p>\n<p><strong>8\u3001Nature\uff1a\u63a5\u8fd1\u8026\u5408\u7684\u9ad8\u6e29\u94c1\u78c1\u62d3\u6251\u7edd\u7f18\u76f8<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14031\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72478-7.jpg\" alt=\"\u56fe\u72478\" width=\"500\" height=\"335\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72478-7.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72478-7-300x201.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/>\u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 <strong>\u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0Bi2Se3\u2013EuS\u53cc\u5c42\u7ed3\u6784\u7684XRD\u4ee5\u53ca\u9ad8\u5206\u8fa8\u7387\u7684TEM\u56fe\u50cf<br \/>\n<\/strong><br \/>\n\u62d3\u6251\u7edd\u7f18\u4f53\u662f\u7edd\u7f18\u6750\u6599\uff0c\u53ef\u901a\u8fc7\u65f6\u95f4\u53cd\u6f14\u5bf9\u79f0\u6027\u5bf9\u5bfc\u7535\u8868\u9762\u72b6\u6001\u8fdb\u884c\u4fdd\u62a4\uff0c\u4e5f\u5c31\u662f\u7535\u5b50\u81ea\u65cb\u52a8\u91cf\u88ab\u9501\u5b9a\u3002\u8fd9\u79cd\u72ec\u7279\u7684\u6027\u80fd\u4e3a\u521b\u9020\u65b0\u4e00\u4ee3\u7684\u7535\u5b50\u3001\u81ea\u65cb\u7535\u5b50\u5b66\u548c\u91cf\u5b50\u8ba1\u7b97\u8bbe\u5907\u5f00\u8f9f\u4e86\u65b0\u7684\u673a\u9047\u3002<\/p>\n<p>Ferhat Katmis\u7b49\u4eba\u7528\u81ea\u65cb\u6781\u5316\u4e2d\u5b50\u53cd\u5c04\u7387\u5b9e\u9a8c\u8bc1\u660e\uff1a\u5728\u62d3\u6251\u7edd\u7f18\u4f53\uff08Bi2Se3\uff09\u53cc\u5c42\u7cfb\u7edf\u4e2d\u901a\u8fc7\u8026\u5408\u94c1\u78c1\u7edd\u7f18\u4f53\u4f7f\u5f97\u62d3\u6251\u754c\u9762\u78c1\u6027\uff08EUS\uff09\u589e\u5f3a\u3002\u754c\u9762\u4e2d\u7684\u78c1\u6027\u4e3b\u8981\u7531\u81ea\u65cb\u8f68\u9053\u76f8\u4e92\u4f5c\u7528\u4ea7\u751f\uff0c\u5e76\u4e14\u62d3\u6251\u7edd\u7f18\u4f53\u8868\u9762\u7684\u81ea\u65cb\u52a8\u91cf\u9501\u5b9a\u4f7f\u5f97\u8fd9\u79cd\u53cc\u5c42\u7cfb\u7edf\u7684\u78c1\u6709\u5e8f\uff08\u5c45\u91cc\uff09\u6e29\u5ea6\u5927\u5927\u7684\u63d0\u9ad8\u3002\u7531\u4e8e\u94c1\u78c1\u77ed\u8ddd\u79bb\u7684\u4ea4\u4e92\u4f5c\u7528\u6027\u8d28\uff0c\u5728\u62d3\u6251\u7edd\u7f18\u4f53\u7684\u8868\u9762\u9644\u8fd1\u65f6\u95f4\u53cd\u6f14\u5bf9\u79f0\u6027\u4f1a\u88ab\u6253\u7834\u800c\u8fdc\u79bb\u8868\u9762\u7684\u4e0d\u53d7\u5f71\u54cd\u3002\u62d3\u6251\u78c1\u7535\u673a\u7684\u8bbe\u8ba1\u5c31\u662f\u6e90\u4e8e\u8fd9\u79cd\u62d3\u6251\u7edd\u7f18\u4f53\uff0c\u53ef\u4ee5\u901a\u8fc7\u4e00\u4e2a\u7535\u573a\u6709\u6548\u5730\u64cd\u7eb5\u78c1\u5316\u52a8\u529b\u5b66\uff0c\u4e3a\u672a\u6765\u4ee5\u81ea\u65cb\u4e3a\u57fa\u7840\u7684\u6280\u672f\u63d0\u4f9b\u4e86\u4e00\u4e2a\u9ad8\u6548\u8282\u80fd\u7684\u62d3\u6251\u63a7\u5236\u673a\u5236\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/www.nature.com\/nature\/journal\/vaop\/ncurrent\/full\/nature17635.html\" target=\"_blank\"><strong>A high-temperature ferromagnetic topological insulating phase by proximity coupling<\/strong><\/a><\/p>\n<p><strong>9\u3001EES\uff1aSnxSb1-xTe\u6750\u6599\u4f4e\u70ed\u5bfc\u7387\u7684\u6839\u6e90<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14032\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72479-4.jpg\" alt=\"\u56fe\u72479\" width=\"500\" height=\"237\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72479-4.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u72479-4-300x142.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><strong>\uff08a\uff09\u4e3aSnxSb1-xTe\u572810%\u8bef\u5dee\u8303\u56f4\u5185\u6e29\u5dee\u7535\u4f18\u503c\u968f\u6e29\u5ea6\u7684\u53d8\u5316\uff08b\uff09\u4e0e\u5176\u4ed6\u6750\u6599\u76f8\u6bd4SnxSb1-xTe\u7684\u97e6\u6c0f\u786c\u5ea6\u503c<\/strong><\/p>\n<p>\u5728\u70ed\u7535\u5e94\u7528\u9886\u57df\uff0c\u4f4e\u70ed\u5bfc\u7387\u7684\u65e0\u673a\u6750\u6599\u5f15\u8d77\u4e86\u4f17\u591a\u4eba\u7684\u5174\u8da3\u3002\u901a\u8fc7\u58f0\u5b50\u6563\u5c04\u5f62\u6210\u7684\u7eb3\u7c73\u7ed3\u6784\u662f\u964d\u4f4e\u6750\u6599\u5bfc\u70ed\u7387\u7684\u91cd\u8981\u9014\u5f84\u3002<\/p>\n<p>\u6765\u81ea\u8d3e\u74e6\u54c8\u62c9\u5c14\u00b7\u5c3c\u8d6b\u9c81\u5148\u8fdb\u79d1\u5b66\u7814\u7a76\u4e2d\u5fc3\u7684\u79d1\u7814\u56e2\u961f\uff0c\u6700\u8fd1\u53d1\u73b0\u4e86\u5728SnTe\u4e2d\u7531\u4e8e\u7eb3\u7c73\u7ed3\u6784Sb\u548cSnmSb2nTe3n+m\u4ea4\u4e92\u751f\u957f\u4f7f\u5f97SnxSb1-xTe\u5177\u6709\u63a5\u8fd1\u6700\u4f4e\u7406\u8bba\u6676\u683c\u70ed\u5bfc\u7387\u3002\u5728&lt;111&gt;\u65b9\u5411\uff0cSb\u4e0eSnTe\u76f8\u4e92\u5206\u79bb\uff0c\u5bfc\u81f4\u4e86\u8d85\u70b9\u9635\u7ed3\u6784\u7684\u751f\u6210\u3002\u540c\u65f6\uff0c\u8be5\u8d85\u70b9\u9635\u7ed3\u6784\u5f15\u8d77\u4e86\u663e\u8457\u7684\u58f0\u5b50\u6563\u5c04\u3002\u53e6\u5916\uff0cSb\u63ba\u6742\u5728SnTe\u4e2d\u4f1a\u964d\u4f4ep\u578b\u8f7d\u6d41\u5b50\u5bc6\u5ea6\u3002\u7531\u4e8e\u8f7d\u6d41\u5b50\u5bc6\u5ea6\u81ea\u53d1\u51cf\u5c11\u4ee5\u53ca\u7531\u7eb3\u7c73\u5c3a\u5ea6\u4e3b\u5bfc\u7684\u8d85\u7ed3\u6784\u7684\u8fc7\u6ee4\u95ee\u9898\u4f7f\u585e\u8d1d\u514b\u7cfb\u6570\u6709\u4e86\u5f88\u5927\u7684\u63d0\u9ad8\u3002\u6240\u4ee5\uff0c\u5728800K\uff0cSn0.85Sb0.15Te\u53ef\u4ee5\u83b7\u5f97\u6700\u4f18\u7684\u70ed\u7535\u4f18\u503c\uff0c\u5176\u7ef4\u6c0f\u786c\u5ea6\u5927\u6982\u6709136Hv\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.rsc.org\/en\/content\/articlelanding\/2016\/ee\/c6ee00728g\" target=\"_blank\"><strong>The origin of low thermal conductivity in Sn1-xSbxTe: phonon scatteringvialayered\u00a0intergrowth nanostructures<\/strong><\/a><\/p>\n<p><strong>10\u3001EES\uff1a\u81ea\u4f9b\u7535\u7684\u53ef\u7a7f\u6234\u7535\u5b50\u4ea7\u54c1\u7684\u70ed\u7535\u80fd\u6e90\u4ea7\u751f\u5668\u8bbe\u8ba1<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14033\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724710-3.jpg\" alt=\"\u56fe\u724710\" width=\"400\" height=\"179\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724710-3.jpg 400w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724710-3-300x134.jpg 300w\" sizes=\"(max-width: 400px) 100vw, 400px\" \/>\u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 <strong>\u00a0 \u5de6\u56fe\u4e3a\u4ece\u8eab\u4f53\u4e2d\u5fc3\u81f3\u73af\u5883\u7684\u6e29\u5ea6\u53d8\u5316\uff1b\u53f3\u56fe\u4e3a\u5355\u817f\u5468\u56f4\u70ed\u963b\u76843-D\u793a\u610f\u56fe<\/strong><\/p>\n<p>\u968f\u7740\u53ef\u7a7f\u6234\u4f20\u611f\u5668\u4ee5\u53ca\u7535\u5b50\u5668\u4ef6\u6027\u80fd\u7684\u63d0\u9ad8\uff0c\u5176\u5728\u533b\u7597\u548c\u73af\u5883\u76d1\u6d4b\u4e2d\u4e5f\u8d8a\u6765\u8d8a\u53d7\u6b22\u8fce\u3002\u70ed\u7535\u80fd\u6e90\u4ea7\u751f\u5668\u5229\u7528\u4eba\u4f53\u70ed\u91cf\u6765\u5b9e\u73b0\u81ea\u6211\u4f9b\u80fd\uff0c\u53ef\u662f\u7a7a\u6c14\u754c\u9762\u7684\u7535\u963b\u503c\u592a\u5927\uff0c\u8fd9\u4e00\u95ee\u9898\u51b3\u5b9a\u7740\u70ed\u7535\u80fd\u6e90\u4ea7\u751f\u5668\u7684\u6027\u80fd\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u6765\u81ea\u5317\u5361\u5dde\u7acb\u5927\u5b66\u7684\u79d1\u7814\u4eba\u5458\u8bbe\u8ba1\u4e86\u4e00\u79cd\u7406\u8bba\u8ba1\u7b97\u6709\u6548\u5e76\u4e14\u51c6\u786e\u7684\u4e09\u7ef4\u70ed\u7535\u53d1\u7535\u673a\u6a21\u5f0f\u3002\u8be5\u6a21\u5f0f\u53ef\u4ee5\u63a2\u7d22\u6ee1\u8db3\u521a\u6027\u70ed\u7535\u53d1\u7535\u673a\u53d1\u5c55\u73b0\u72b6\u7684\u8bbe\u8ba1\u6807\u51c6\u4ee5\u53ca\u67d4\u6027\u7ec4\u4ef6\u7684\u5e94\u7528\u524d\u666f\u3002Francisco\u00a0suarez\u7b49\u4eba\u7814\u7a76\u4e86\u70ed\u7535\u6750\u6599\uff0c\u7ec4\u4ef6\u8bbe\u8ba1\u548c\u7ef4\u6570\uff0c\u6563\u70ed\u5668\uff0c\u586b\u5145\u6750\u6599\uff0c\u70ed\u7f38\uff0c\u76ae\u80a4\u63a5\u89e6\u7535\u963b\u5bf9\u5668\u4ef6\u6027\u80fd\u7684\u5f71\u54cd\uff1b\u660e\u786e\u4e86\u6750\u6599\u70ed\u4f20\u5bfc\u901a\u8fc7\u585e\u8d1d\u514b\u7cfb\u6570\u548c\u70ed\u7535\u963b\u5bf9\u63d0\u9ad8\u53ef\u7a7f\u6234\u4f20\u611f\u5668\u548c\u7535\u5b50\u5668\u4ef6\u8f93\u51fa\u529f\u7387\u7684\u91cd\u8981\u6027\u3002\u5bf9\u4e8e\u67d4\u6027\u70ed\u7535\u53d1\u7535\u673a\uff0c\u4ed6\u4eec\u7814\u7a76\u4e86\u586b\u5145\u6750\u6599\u7684\u70ed\u4f20\u5bfc\u3002\u6700\u540eFrancisco\u00a0suarez\u7b49\u7528\u8be5\u6a21\u5f0f\u8bbe\u8ba1\u4e86\u4e00\u6b3e\u6750\u6599\u6027\u80fd\u6709\u6240\u63d0\u9ad8\u7684\u5b9a\u5236\u70ed\u7535\u53d1\u7535\u673a\u5e76\u8fdb\u884c\u4e86\u5668\u4ef6\u8bbe\u8ba1\u3002\u6d4b\u8bd5\u7ed3\u679c\u8868\u660e\u548c\u5546\u4e1a\u70ed\u7535\u53d1\u7535\u673a\u76f8\u6bd4\uff0c\u5728\u9762\u79ef\u76f8\u540c\u7684\u6761\u4ef6\u4e0b\uff0c\u7528\u8be5\u6a21\u5f0f\u8bbe\u8ba1\u7684\u70ed\u7535\u53d1\u7535\u673a\u8f93\u51fa\u529f\u7387\u63d0\u9ad8\u4e86\u8fd13\u500d\uff0c\u548c\u7406\u8bba\u8ba1\u7b97\u7684\u9884\u6d4b\u9ad8\u5ea6\u4e00\u81f4\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.rsc.org\/en\/content\/articlelanding\/2016\/ee\/c6ee00456c#!divAbstract\" target=\"_blank\"><strong>Designing thermoelectric generators for self-powered wearable electronics<\/strong><\/a><\/p>\n<p><strong>11\u3001NANO LETTERS\uff1a\u591a\u5c42\u77f3\u58a8\u70ef\u7ed3\u6784\u6781\u5927\u5730\u63d0\u9ad8\u4e86\u77f3\u58a8\u70ef\/\u73af\u6c27\u6811\u8102\u590d\u5408\u6750\u6599\u7684\u70ed\u5bfc\u7387<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14034\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724711-2.jpg\" alt=\"\u56fe\u724711\" width=\"500\" height=\"385\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724711-2.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u56fe\u724711-2-300x231.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/>\u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 \u00a0 <strong>\u4e0d\u540c\u77f3\u58a8\u70ef\u5c42\u6570\u4e0b\u7684\u70ed\u5bfc\u7387\u968f\u77f3\u58a8\u70ef\u4f53\u79ef\u5206\u6570\u7684\u53d8\u5316<\/strong><\/p>\n<p>\u5728\u73b0\u4ee3\u7535\u5b50\u8bbe\u5907\u4e2d\uff0c\u5feb\u901f\u6563\u70ed\u5df2\u6210\u4e3a\u4e00\u4e2a\u6025\u9700\u89e3\u51b3\u7684\u95ee\u9898\u3002\u77f3\u58a8\u70ef\u81ea\u88ab\u53d1\u73b0\u4ee5\u6765\u5176\u4f18\u5f02\u7684\u6027\u80fd\u4e00\u76f4\u5907\u53d7\u77a9\u76ee\uff0c\u5728\u6563\u70ed\u9886\u57df\uff0c\u4eba\u4eec\u671f\u671b\u5f97\u5230\u4e00\u79cd\u4f4e\u77f3\u58a8\u70ef\u542b\u91cf\u9ad8\u5bfc\u70ed\u7387\u7684\u73af\u6c27\u6811\u8102\u57fa\u590d\u5408\u6750\u6599\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c\u9999\u6e2f\u79d1\u6280\u5927\u5b66\u548c\u6e05\u534e\u5927\u5b66\u7684\u7814\u7a76\u4eba\u5458\u63a2\u7d22\u4e86\u591a\u5c42\u77f3\u58a8\u70ef\u7247\u7684\u5c42\u6570\u548c\u5c3a\u5bf8\u5bf9\u73af\u6c27\u6811\u8102\u57fa\u590d\u5408\u6750\u6599\u5bfc\u70ed\u7387\u7684\u5f71\u54cd\u3002\u5206\u5b50\u52a8\u529b\u5b66\u6a21\u62df\u663e\u793a\u5f53\u77f3\u58a8\u70ef\u7247\u5c42\u6570\u589e\u52a0\u65f6\u591a\u5c42\u77f3\u58a8\u70ef\u548c\u77f3\u58a8\u70ef\/\u73af\u6c27\u6811\u8102\u754c\u9762\u7684\u5bfc\u70ed\u7387\u589e\u52a0\u3002\u4f46\u662f\uff0c\u5177\u6709\u9ad8\u5bfc\u70ed\u7387\u7684\u591a\u5c42\u77f3\u58a8\u70ef\u5e76\u4e0d\u80fd\u4f7f\u591a\u5c42\u77f3\u58a8\u70ef\/\u73af\u6c27\u6811\u8102\u5177\u6709\u9ad8\u7684\u5bfc\u70ed\u7387\uff0c\u9664\u975e\u591a\u5c42\u77f3\u58a8\u70ef\u6709\u8f83\u5927\u7684\u4fa7\u9762\u5c3a\u5bf8\u4f7f\u5f97\u5176\u5177\u6709\u4e0e\u5355\u5c42\u77f3\u58a8\u70ef\u76f8\u6bd4\u7684\u9ad8\u5bbd\u6bd4\u3002\u5b9e\u9a8c\u63ed\u793a\u4e86\u4f7f\u7528\u591a\u5c42\u77f3\u58a8\u70ef\u7684\u597d\u5904\u5728\u4e8e\uff1a\u4e0e\u76f8\u540c\u542b\u91cf\u7684\u5355\u5c42\u6216\u5c11\u5c42\u77f3\u58a8\u70ef\u4f53\u79ef\u5206\u65702.8%\u65f6\u7684\u76f4\u5f84\u4e3a30 \u03bcm\u591a\u5c42\u77f3\u58a8\u70ef\uff08\u5c42\u6570\u5927\u4e8e10\uff09\u5bfc\u70ed\u7387\u5927\u6982\u4e3a1.5W m\u22121K\u22121\u3002\u672c\u53d1\u73b0\u4e3a\u9ad8\u6027\u4ef7\u6bd4\u7684\u591a\u5c42\u77f3\u58a8\u70ef\u505a\u4e3a\u5bfc\u70ed\u586b\u6599\u5728\u5404\u79cd\u70ed\u7ba1\u7406\u5e94\u7528\u63d0\u4f9b\u4e86\u6307\u5bfc\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acs.nanolett.6b00722\" target=\"_blank\"><strong>Multi-Layer Graphene Enables Higher Efficiency in Improving Thermal Conductivities of Graphene\/Epoxy Composites<\/strong><\/a><\/p>\n<p>\u672c\u671f\u5185\u5bb9\u7531\u6750\u6599\u4eba\u7535\u5b50\u7535\u5de5\u6750\u6599\u5b66\u4e60\u5c0f\u7ec4\u6811\u82d7\uff0cZZZZ\uff0c\u5927\u9ed1\u5929\uff0c\u4ee5\u4ea6\u7b49\u4eba\u7f16\u5199\u3002\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n<p>\u5982\u679c\u4f60\u5bf9\u7535\u5b50\u6750\u6599\u611f\u5174\u8da3\uff0c\u613f\u610f\u4e0e\u7535\u5b50\u7535\u5de5\u9886\u57df\u4eba\u624d\u4ea4\u6d41\uff0c\u5e76\u4e14\u60f3\u53ca\u65f6\u638c\u63e1\u7535\u5b50\u6750\u6599\u7814\u7a76\u5b66\u672f\u52a8\u6001\u5e76\u6df1\u5165\u5256\u6790\u884c\u4e1a\u73b0\u72b6\uff0c\u8bf7\u52a0\u5165\u6750\u6599\u4eba\u7535\u5b50\u7535\u5de5\u6750\u6599\u5b66\u4e60\u5c0f\u7ec4\uff08\u52a0\u5165\u65b9\u5f0f\uff1a\u53d1\u9001<a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/\u6750\u6599\u4eba\u7f51-\uff08\u65b0\uff09\u6750\u6599\u4eba\u7f51\u79d1\u7814\u5b66\u4e60\u5c0f\u7ec4\u7533\u8bf7\u8868-V1.2\u7248-1.doc\" target=\"_blank\">\u7533\u8bf7\u8868<\/a>\u548c\u4e2a\u4eba\u7b80\u5386\u81f3msdd0816@163.com\u6216\u8005\u7533\u8bf7\u52a0\u5165\u6211\u4eec\u5b66\u4e60\u5c0f\u7ec4QQ\u7fa4\uff1a482842474)<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u672c\u671f\u5bfc\u8bfb\uff1a \u4eca\u5929\u7535\u5b50\u7535\u5de5\u6750\u6599\u5468\u62a5\u7ec4\u9080\u60a8\u4e00\u8d77\u6765\u770b\u770bNature communications\/ACS Nano\/EES\u7b49\u671f\u520a\u7535\u5b50\u6750\u6599\u9886\u57df\u6700\u65b0\u7684\u7814\u7a76\u8fdb\u5c55\u3002\u672c\u671f\u5185\u5bb9\u9884&#8230;<\/p>\n","protected":false},"author":99,"featured_media":14024,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[67],"tags":[31],"class_list":["post-14023","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-zhoubao","tag-dianzi"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/14023"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/99"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=14023"}],"version-history":[{"count":15,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/14023\/revisions"}],"predecessor-version":[{"id":14058,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/14023\/revisions\/14058"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/14024"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=14023"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=14023"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=14023"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}