{"id":141618,"date":"2018-06-07T06:30:33","date_gmt":"2018-06-06T22:30:33","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=141618"},"modified":"2018-06-06T21:25:59","modified_gmt":"2018-06-06T13:25:59","slug":"advance-materials%e7%90%83%e5%bd%a2%e7%a2%b3%e7%a1%bc%e7%83%b7%e9%85%8d%e4%bd%93%e6%9e%84%e5%bb%ba%e7%9a%84mof%e6%9d%90%e6%96%99%e4%b8%89%e7%bb%b4%e5%88%b0%e4%ba%8c%e7%bb%b4%e7%9a%84%e7%bb%93","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=141618","title":{"rendered":"Advance materials:\u7403\u5f62\u78b3\u787c\u70f7\u914d\u4f53\u6784\u5efa\u7684MOF\u6750\u6599\u4e09\u7ef4\u5230\u4e8c\u7ef4\u7684\u7ed3\u6784\u53ef\u9006\u8f6c\u53d8"},"content":{"rendered":"<p><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/p>\n<p>\u6b63\u5982\u7535\u5f71\u4e2d\u7684\u53d8\u5f62\u91d1\u521a\uff0c\u4eff\u771f\u673a\u5668\u4eba\u5177\u6709\u4efb\u610f\u53d8\u5f62\u7684\u80fd\u529b\uff0c\u53ef\u5c06\u81ea\u8eab\u91cd\u65b0\u7ec4\u88c5\u83b7\u5f97\u6240\u9700\u5f62\u6001\uff0c\u5982\uff0c\u6c7d\u8f66\uff0c\u5766\u514b\u6216\u6b66\u5668\u3002\u76ee\u524d\uff0c\u7814\u7a76\u4eba\u5458\u901a\u8fc7\u5b9e\u9a8c\u5f97\u5230\u4e86\u4e00\u79cd\u80fd\u591f\u5728\u5916\u754c\u6fc0\u53d1\u4e0b\u901a\u8fc7\u7ed3\u6784\u91cd\u7ec4\u4ece\u4e09\u7ef4\u7eb3\u7c73\u591a\u5b54\u7ed3\u6784\u8f6c\u53d8\u6210\u4e3a\u4e8c\u7ef4\u65e0\u5b54\u7ed3\u6784\u7684\u6750\u6599\uff0c\u540c\u65f6\uff0c\u5728\u5916\u754c\u8fdb\u4e00\u6b65\u6fc0\u53d1\u4e0b\uff0c\u53ef\u4ee5\u5b9e\u73b0\u7ed3\u6784\u7684\u9006\u8f6c\u53d8\uff0c\u5373\u4ece\u4e8c\u7ef4\u6062\u590d\u5230\u6700\u521d\u7684\u4e09\u7ef4\u591a\u5b54\u7ed3\u6784\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u8be5\u7814\u7a76\u5df2\u4e8e\u8fd1\u65e5\u53d1\u8868\u5728<em>Advanced Materials<\/em>\u671f\u520a\u4e0a\uff0c\u201cAn Unprecedented Stimuli\u2010Controlled Single\u2010Crystal Reversible Phase Transition of a Metal\u2013Organic Framework and Its Application to a Novel Method of Guest Encapsulation\u201d \u4f5c\u8005\u4e3aDr. Jose Giner\u548c\u5176\u535a\u58eb\u7814\u7a76\u751f\u8c2d\u6609\u7545\uff0c\u8be5\u8bfe\u9898\u7ec4\u96b6\u5c5e\u4e8e\u5df4\u585e\u7f57\u90a3\u6750\u6599\u79d1\u5b66\u7814\u7a76\u6240\u7684\u65e0\u673a\u6750\u6599\u50ac\u5316\u5b9e\u9a8c\u5ba4\u3002\u4ed6\u4eec\u5c06\u5177\u6709\u67d4\u6027\u4e14\u5bcc\u542b\u787c\u5143\u7d20\u7684\u4e8c\u5341\u9762\u4f53\u7403\u5f62\u6709\u673a\u7269\u4f5c\u4e3a\u914d\u4f53\uff0c\u5408\u6210\u51fa\u8be5\u53ef\u8f6c\u53d8\u6750\u6599\u3002\u201c\u76f8\u5bf9\u4e8e\u4f20\u7edf\u7684\u4e8c\u7ef4\u7fa7\u9178\u914d\u4f53\uff0c\u8fd9\u79cd\u65b0\u578b\u4e09\u7ef4\u7403\u5f62\u914d\u4f53\u662f\u5b9e\u73b0\u7ed3\u6784\u8f6c\u53d8\u56de\u521d\u59cb\u7684\u72b6\u6001\u5173\u952e\uff0c\u5b83\u4f7f\u9aa8\u67b6\u5404\u90e8\u5206\u91cd\u7ec4\u7684\u540c\u65f6\u8fd8\u80fd\u4fdd\u6301\u7ed3\u6784\u7684\u7a33\u5b9a\u3002\u201d<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<br \/>\n <\/strong><br \/>\n \u56fe\u4e00\u6839\u636e\u5355\u6676\u884d\u5c04\u7ed8\u5236\u7684MOF\u6676\u4f53\u7ed3\u6784<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/mof1.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-141620\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/mof1.png\" alt=\"\" width=\"456\" height=\"193\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/mof1.png 456w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/mof1-300x127.png 300w\" sizes=\"(max-width: 456px) 100vw, 456px\" \/><\/a><\/p>\n<p>a \u6676\u4f53\u5177\u6709\u6cbf\u7740b\u8f74\u7684\u5b54\u9053\uff0c \u8be5\u5b54\u9053\u80fd\u5bb9\u7eb3\u4e0d\u540c\u7684\u6eb6\u5242\u5206\u5b50<\/p>\n<p>b \u914d\u4f53H<sub>3<\/sub>BTB\u7684\u5206\u5b50\u5f0f1,3,5-tris(4-carboxyphenyl)benzene<\/p>\n<p>c \u78b3\u787c\u70f7\u914d\u4f53\uff0c\u5176\u4e2d<em>m<\/em>eta-carborane fragment, C<sub>2<\/sub>B<sub>10<\/sub>H<sub>10<\/sub> \u95f4\u4f4d\u78b3\u787c\u70f7\u7528\u6a59\u8272\u7684\u4e8c\u5341\u9762\u4f53\u8868\u793a\uff0c\u9ed1\u70b9\u4ee3\u8868\u78b3\u539f\u5b50\u3002<\/p>\n<p>\u56fe\u4e8c MOF 1 \u4e0eMOF 2\u53ef\u9006\u8f6c\u53d8\u7684\u53cd\u5e94\u6761\u4ef6\u53ca\u5176\u5bf9\u5bcc\u52d2\u70ef\u7684\u5305\u8986\uff0c\u5176\u4e2dMOF 1 \u548cMOF 2 \u7684\u7ed3\u6784\u6839\u636e\u5355\u6676\u884d\u5c04\u6570\u636e\u7ed8\u5236\uff0cMOF 1\u5305\u8986\u5bcc\u52d2\u70ef\u7ed3\u6784\u6839\u636eDFT\u7ed3\u679c\u4f18\u5316\u5f97\u5230\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/mof2.png\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-141621\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/mof2.png\" alt=\"\" width=\"436\" height=\"295\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/mof2.png 436w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/mof2-300x203.png 300w\" sizes=\"(max-width: 436px) 100vw, 436px\" \/><\/a><\/p>\n<p><strong>\u3010\u5c0f\u7ed3\u3011<\/strong><\/p>\n<p>\u7814\u7a76\u4eba\u5458\u9996\u6b21\u62a5\u9053\u4e86\u65b0\u578b\u7eb3\u7c73\u591a\u5b54\u4e09\u7ef4\u7ed3\u6784\u6750\u6599\u7684\u67d4\u6027\u548c\u52a8\u6001\u8f6c\u53d8\u3002\u901a\u8fc7\u63a7\u5236\u5b54\u9053\u4e2d\u7684\u6eb6\u5242\u5206\u5b50\uff0c\u8be5\u6750\u6599\u53ef\u4ee5\u5b9e\u73b0\u4e09\u7ef4\u4e0e\u4e8c\u7ef4\u7ed3\u6784\u7684\u53ef\u9006\u8f6c\u53d8\u3002\u57fa\u4e8e\u7403\u5f62\u78b3\u787c\u70f7\u4e3a\u4e3b\u8981\u6210\u5206\u7684\u914d\u4f53\u63d0\u9ad8\u4e86\u9aa8\u67b6\u7684\u7a33\u5b9a\u6027\u907f\u514d\u8f6c\u53d8\u8fc7\u7a0b\u7ed3\u6784\u584c\u9677\u3002\u8be5MOF\u591a\u5b54\u6750\u6599\u53ef\u4ee5\u5e94\u7528\u4e8e\u5206\u5b50\u5438\u9644\u53ca\u5206\u79bb\uff0c\u6d3b\u6027\u7ec4\u5206\u8f7d\u4f53\u7684\u5305\u8986\u548c\u7f13\u91ca\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong>\u201cAn Unprecedented Stimuli\u2010Controlled Single\u2010Crystal Reversible Phase Transition of a Metal\u2013Organic Framework and Its Application to a Novel Method of Guest Encapsulation\u201d https:\/\/onlinelibrary.wiley.com\/doi\/abs\/10.1002\/adma.201800726<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com.<\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaokefu\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u6b63\u5982\u7535\u5f71\u4e2d\u7684\u53d8\u5f62\u91d1\u521a\uff0c\u4eff\u771f\u673a\u5668\u4eba\u5177\u6709\u4efb\u610f\u53d8\u5f62\u7684\u80fd\u529b\uff0c\u53ef\u5c06\u81ea\u8eab\u91cd\u65b0\u7ec4\u88c5\u83b7\u5f97\u6240\u9700\u5f62\u6001\uff0c\u5982\uff0c\u6c7d\u8f66\uff0c\u5766\u514b\u6216\u6b66\u5668\u3002\u76ee\u524d\uff0c\u7814\u7a76\u4eba\u5458\u901a\u8fc7\u5b9e\u9a8c\u5f97\u5230\u4e86\u4e00\u79cd\u80fd\u591f\u5728\u5916\u754c\u6fc0\u53d1&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[2789],"class_list":["post-141618","post","type-post","status-publish","format-standard","hentry","category-jiedu","tag-mofs"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/141618"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=141618"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/141618\/revisions"}],"predecessor-version":[{"id":141624,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/141618\/revisions\/141624"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=141618"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=141618"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=141618"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}