{"id":143949,"date":"2018-06-29T06:30:21","date_gmt":"2018-06-28T22:30:21","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=143949"},"modified":"2018-06-30T00:03:10","modified_gmt":"2018-06-29T16:03:10","slug":"%e6%9d%90%e6%96%99%e4%ba%ba%e6%8a%a5%e5%91%8a%e4%b8%a8%e6%98%af%e8%b0%81%e7%9a%84%e5%b0%8f%e7%9c%bc%e7%9d%9b%ef%bc%8c%e8%bf%98%e6%b2%a1%e7%9c%8b%e8%bf%87%e6%9d%a5%ef%bc%9a%e8%bf%91%e4%ba%94%e5%b9%b4","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=143949","title":{"rendered":"\u6750\u6599\u4eba\u62a5\u544a\u4e28\u662f\u8c01\u7684\u5c0f\u773c\u775b\uff0c\u8fd8\u6ca1\u770b\u8fc7\u6765\uff1a\u8fd1\u4e94\u5e74\u56fd\u5185Nature\u3001Science\u53d1\u6587\u6570\u636e\u7eb5\u89c8"},"content":{"rendered":"<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-144362 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/640.jpg\" alt=\"\" width=\"900\" height=\"383\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/640.jpg 900w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/640-300x128.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/640-768x327.jpg 768w\" sizes=\"(max-width: 900px) 100vw, 900px\" \/><\/p>\n<p>Nature\u548cScience\u4f5c\u4e3a\u5f53\u4eca\u5168\u7403\u6700\u5177\u6743\u5a01\u7684\u5b66\u672f\u671f\u520a\uff0c\u5728\u53d1\u8868\u539f\u59cb\u7814\u7a76\u8bba\u6587\u548c\u7efc\u8ff0\u7684\u540c\u65f6\uff0c\u4e5f\u5206\u6790\u5f53\u524d\u7814\u7a76\u548c\u79d1\u5b66\u653f\u7b56\uff0c\u8303\u56f4\u8986\u76d6\u4e86\u51e0\u4e4e\u6240\u6709\u5b66\u79d1\uff0c\u5728\u79d1\u5b66\u754c\u5177\u6709\u7edd\u5bf9\u7684\u5f71\u54cd\u529b\u3002\u6839\u636e\u671f\u520a\u5f15\u8bc1\u62a5\u544a\uff0cNature\u57282018\u5e74\u7684\u5f71\u54cd\u56e0\u5b50\u4e3a40.137\uff0c\u800cScience\u7684\u5f71\u54cd\u56e0\u5b50\u4e3a37.205\u3002<\/p>\n<p>Nature\u548cScience\u4f5c\u4e3a\u6700\u6743\u5a01\u7684\u5b66\u672f\u671f\u520a\uff0c\u662f\u4f17\u591a\u79d1\u7814\u5de5\u4f5c\u8005\u7684\u79d1\u7814\u6bbf\u5802\u3002\u5bf9\u6211\u56fd\u79d1\u7814\u56e2\u961f\u5728Nature\u3001Science\u53d1\u6587\u60c5\u51b5\u8fdb\u884c\u5206\u6790\u7814\u7a76\uff0c\u6709\u52a9\u4e8e\u4e86\u89e3\u6211\u56fd\u6750\u6599\u9886\u57df\u7684\u7814\u7a76\u73b0\u72b6\u3002\u8fd9\u91cc\uff0c\u5c0f\u7f16\u7814\u7a76\u4e86\u8fd1\u4e94\u5e74\uff082014-2018\uff09\u56fd\u5185\u56e2\u961fNature\u3001Science\u7684\u53d1\u6587\u6570\u636e\uff0c\u5e76\u5bf9\u5176\u8fdb\u884c\u5f52\u7eb3\u6574\u7406\u548c\u89e3\u6790\u3002<br \/>\n <strong><b>1. Nature\u3001Science\u53d1\u6587\u60c5\u51b5<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-143950\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/revised1.jpg\" alt=\"\" width=\"600\" height=\"429\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/revised1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/revised1-300x215.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong><b>\u56fe1 \u56fd\u5185\u56e2\u961f\u5408\u4f5c\u53ca\u72ec\u7acb\u7814\u7a76\u5728Nature\u3001Science\u4e0a\u7684\u53d1\u6587\u60c5\u51b5<\/b><\/strong><\/p>\n<p>\u672c\u6b21\u8c03\u67e5\u62a5\u544a\u4ee5Web of Science\u4e3a\u68c0\u7d22\u5de5\u5177\uff0c\u57282014\u5e74\u52302018\u5e74\uff0c\u4e2d\u56fd\u9ad8\u6821\u53c2\u4e0e\u53ca\u5408\u4f5c\u7814\u7a76\u5171\u5728Nature\u548cScience\u4e0a\u53d1\u8868\u6587\u7ae0101\u7bc7\u3002\u5c3d\u7ba1\u603b\u6570\u91cf\u4ee4\u4eba\u53ef\u559c\uff0c\u4f46\u5176\u4e2d\u72ec\u7acb\u7814\u7a76\u7684\u5de5\u4f5c\u4ec5\u670915\u7bc7\uff0c\u8fd9\u8bf4\u660e\u56fd\u5185\u7684\u72ec\u7acb\u79d1\u7814\u6c34\u5e73\u80fd\u529b\u8fd8\u6709\u5f85\u63d0\u9ad8\u3002<\/p>\n<p><strong><b>2. \u56fd\u5185\u56e2\u961f\u5728Nature\u3001Science\u7684\u5386\u5e74\u53d1\u8868\u6587\u7ae0\u91cf<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-144088\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/revised2-1.jpg\" alt=\"\" width=\"600\" height=\"416\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/revised2-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/revised2-1-300x208.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong><b>\u56fe2 2014-2018\u5e74\u56fd\u5185\u56e2\u961f\u5728Nature\/Science\u5386\u5e74\u53d1\u8868\u6587\u7ae0\u91cf\uff082018\u5e74\u4ec5\u4e3a\u524d\u4e94\u4e2a\u6708\uff09<\/b><\/strong><\/p>\n<p>\u56fe2\u4e3a2014-2018\u5e74\u56fd\u5185\u56e2\u961f\u5386\u5e74\u5728Nature\u3001Science\u4e0a\u53d1\u8868\u6587\u7ae0\u7684\u6570\u91cf\u3002\u6570\u636e\u663e\u793a\uff0c\u4ece2014-2018\u5e74\u4e4b\u95f4\uff0c\u56fd\u5185\u56e2\u961f\u6bcf\u5e74\u5728Nature\u3001Science\u4e0a\u53d1\u8868\u7684\u6587\u7ae0\u91cf\u9010\u5e74\u589e\u52a0\u30022014\u5e74\u548c2015\u5e74\uff0c\u56fd\u5185\u56e2\u961f\u6bcf\u5e74\u5728Nature\u3001Science\u4e0a\u53d1\u8868\u6587\u7ae0\u4ec515\u7bc7\uff0c2016\u5e74\u589e\u52a0\u523025\u7bc7\uff0c\u800c\u57282017\u5e74\u8fbe\u5230\u4e8637\u7bc7\u3002\u8fd9\u4e2a\u6570\u636e\u8bf4\u660e\u56fd\u5185\u6574\u4f53\u7684\u79d1\u7814\u6c34\u5e73\u548c\u5b9e\u529b\u90fd\u6709\u5f88\u5927\u7684\u63d0\u5347\uff0c\u5b66\u672f\u5f71\u54cd\u529b\u4e5f\u5728\u9010\u6e10\u6269\u5927\uff0c\u5728Nature\u3001Science\u4e0a\u7684\u8d21\u732e\u503c\u4e5f\u5728\u9010\u5e74\u589e\u52a0\u3002<\/p>\n<p><strong><b>3. Nature\u3001Science\u53d1\u6587\u91cf\u524d10\u7684\u673a\u6784<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-144092\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/revised3-3.jpg\" alt=\"\" width=\"600\" height=\"434\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/revised3-3.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/revised3-3-300x217.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong><b>\u56fe3 Nature\/Science\u6536\u5f55\u6587\u7ae0\u6570\u56fd\u5185\u6392\u540dTOP10\u673a\u6784<\/b><\/strong><\/p>\n<p>\u4e2d\u79d1\u9662\u51ed\u501f\u5176\u5e9e\u5927\u7684\u89c4\u6a21\u4ee518\u7bc7\u6587\u7ae0\u4f4d\u5c45\u699c\u9996\uff0c\u5c55\u73b0\u4e86\u76f8\u5f53\u5f3a\u7684\u79d1\u7814\u5b9e\u529b\uff1b\u540c\u65f6\uff0c\u6e05\u534e\u5927\u5b66\u3001\u5317\u4eac\u5927\u5b66\u548c\u4e0a\u6d77\u79d1\u6280\u5927\u5b66\u4ee56\u7bc7\u7d27\u968f\u5176\u540e\u3002\u503c\u5f97\u6ce8\u610f\u7684\u662f\uff0c\u6e05\u534e\u5927\u5b66\u548c\u5317\u4eac\u5927\u5b66\u5747\u6709\u5de5\u4f5c\u4e3a\u56fd\u5185\u56e2\u961f\u72ec\u7acb\u5b8c\u6210\uff0c\u4e0a\u6d77\u79d1\u6280\u5927\u5b66\u7684\u5de5\u4f5c\u4e3b\u8981\u901a\u8fc7\u4e0e\u56fd\u5916\u8bfe\u9898\u7ec4\u5408\u4f5c\u7684\u5f62\u5f0f\u5b8c\u6210\u3002\u4ece\u6574\u4f53\u4e0a\u770b\uff0c\u76ee\u524d\u56fd\u5185\u56e2\u961f\u5728Nature\u3001Science\u53d1\u8868\u6587\u7ae0\uff0c\u4e3b\u8981\u4ee5\u4e0e\u56fd\u5916\u5408\u4f5c\u7684\u5f62\u5f0f\u3002\u8fd9\u4e2a\u6570\u636e\u53ef\u4ee5\u8bf4\u660e\u4e24\u70b9\u95ee\u9898\uff0c\u9996\u5148\u662f\u56e2\u961f\u4e4b\u95f4\u7684\u5408\u4f5c\u548c\u8d44\u6e90\u4e92\u7528\u5df2\u7ecf\u6210\u4e3a\u4e00\u79cd\u4e3b\u5bfc\uff0c\u5176\u6b21\u662f\u56fd\u5185\u7684\u72ec\u7acb\u79d1\u7814\u6c34\u5e73\u8fd8\u6709\u66f4\u591a\u8fdb\u6b65\u7684\u7a7a\u95f4\u3002<\/p>\n<p><strong><b>4. Nature\u3001Science\u53d1\u6587\u5173\u952e\u8bcd<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-144093\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/revised4-1.jpg\" alt=\"\" width=\"600\" height=\"424\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/revised4-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/06\/revised4-1-300x212.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\"><strong><b>\u56fe4 Nature\/Science\u6536\u5f55\u6587\u7ae0\u6570\u7814\u7a76\u9886\u57df\u5206\u5e03<\/b><\/strong><\/p>\n<p>\u901a\u8fc7\u5bf9\u8fd1\u4e94\u5e74\u4e2d\u56fd\u56e2\u961f\u5728Nature\/Science\u4e0a\u6240\u53d1\u8868\u7684\u6587\u7ae0\u8fdb\u884c\u603b\u7ed3\u5f52\u7eb3\uff0c\u53d1\u73b0\u5728\u7eb3\u7c73\u6750\u6599\u3001\u80fd\u6e90\u6750\u6599\u3001\u91d1\u5c5e\u6750\u6599\u3001\u50ac\u5316\u3001\u7535\u5b50\u6750\u6599\u3001\u4e8c\u7ef4\u6750\u6599\u548cMOF\u8fd9\u4e03\u4e2a\u7814\u7a76\u9886\u57df\u7684\u5de5\u4f5c\u6700\u4e3a\u96c6\u4e2d\u3002\u5176\u4e2d\u7eb3\u7c73\u6750\u6599\u7684\u6587\u7ae0\u8fbe\u5230\u4e8630\u7bc7\uff0c\u5927\u5927\u8d85\u8fc7\u4e86\u5176\u4ed6\u9886\u57df\uff0c\u8bf4\u660e\u76ee\u524d\u5bf9\u7eb3\u7c73\u6750\u6599\u7814\u7a76\u7684\u706b\u70ed\u7a0b\u5ea6\u3002\u7d27\u968f\u5176\u540e\u7684\u662f\u80fd\u6e90\u6750\u6599\uff0c\u4e00\u5171\u670913\u7bc7\u6587\u7ae0\u3002\u80fd\u6e90\u95ee\u9898\u4e00\u76f4\u662f\u4eba\u7c7b\u793e\u4f1a\u53d1\u5c55\u7684\u4e00\u4e2a\u5de8\u5927\u95ee\u9898\uff0c\u968f\u7740\u65b0\u80fd\u6e90\u7684\u53d1\u5c55\uff0c\u5bf9\u5149\u4f0f\u6750\u6599\u3001\u7535\u6781\u6750\u6599\u7b49\u80fd\u6e90\u6750\u6599\u7684\u7814\u7a76\u4e5f\u5438\u5f15\u4e86\u5f88\u591a\u6765\u81ea\u79d1\u5b66\u754c\u7684\u76ee\u5149\u3002\u5176\u540e\u7684\u91d1\u5c5e\u3001\u50ac\u5316\u548c\u7535\u5b50\u6750\u6599\u7b49\u4f20\u7edf\u6750\u6599\u9886\u57df\uff0c\u6587\u7ae0\u6570\u91cf\u4e5f\u670912\u7bc7\u3002\u524d\u5341\u5e74\u5927\u70ed\u7684\u4e8c\u7ef4\u6750\u6599\u6587\u7ae0\u6570\u670911\uff0c\u503c\u5f97\u6ce8\u610f\u7684\u662f\uff0c\u5176\u4e2d\u67095\u7bc7\u90fd\u662f\u4ee5\u77f3\u58a8\u70ef\u4e3a\u57fa\u7840\u7684\uff0c\u8bf4\u660e\u79d1\u5b66\u754c\u5bf9\u77f3\u58a8\u70ef\u7684\u70ed\u60c5\u8fd8\u672a\u6d88\u51cf\u3002\u7b2c\u4e03\u4e2a\u662f\u91d1\u5c5e\u6709\u673a\u6846\u67b6\uff0c\u6587\u7ae0\u6570\u4e3a5\u7bc7\u3002\u8fd9\u4e03\u4e2a\u7814\u7a76\u9886\u57df\u7684\u53d1\u6587\u603b\u91cf\u5df2\u7ecf\u5360\u636e\u4e86\u56fd\u5185\u56e2\u961f\u5728Nature\/Science\u4e0a\u53d1\u8868\u6587\u7ae0\u603b\u91cf\u7684\u5927\u534a\u6c5f\u5c71\uff0c\u6709\u5174\u8da3\u5728Nature\u3001Science\u4e0a\u53d1\u8868\u6587\u7ae0\u7684\u79d1\u7814\u5de5\u4f5c\u8005\u4e0d\u59a8\u5bf9\u76f8\u5173\u7814\u7a76\u9886\u57df\u591a\u52a0\u5173\u6ce8\u3002<\/p>\n<p><strong><b>5. Nature\u3001Science\u6587\u7ae0\u88ab\u5f15\u7528\u60c5\u51b5<\/b><\/strong><\/p>\n<p>\u901a\u8fc7\u5bf9\u8fd1\u4e94\u5e74\u4e2d\u56fd\u56e2\u961f\u5728Nature\/Science\u4e0a\u6240\u53d1\u8868\u7684\u6587\u7ae0\u7684\u88ab\u5f15\u6b21\u6570\u8fdb\u884c\u5f52\u7eb3\u548c\u603b\u7ed3\uff0c\u6211\u4eec\u53d1\u73b0\u5728\u6240\u53d1\u8868\u7684101\u7bc7\u6587\u7ae0\u4e2d\uff0c\u670953\u7bc7\u5165\u9009ESI\u9ad8\u88ab\u5f15\u8bba\u6587\uff0c\u6bd4\u4f8b\u8fbe\u5230\u4e8650%\u4ee5\u4e0a\uff0c\u8bf4\u660e\u8fd9\u4e9b\u5de5\u4f5c\u5728\u76f8\u5173\u7814\u7a76\u9886\u57df\u4e2d\u7684\u5f71\u54cd\u529b\u5f88\u5927\u3002<\/p>\n<p>\u6587\u7ae0\u7ed3\u5c3e\u9001\u798f\u5229\uff0c\u4e0b\u6587\u5217\u51fa10\u7bc7Nature\u3001Science\u4e2d\u5f15\u7528\u91cf\u6700\u9ad8\u7684\u8bba\u6587<\/p>\n<p><a href=\"http:\/\/science.sciencemag.org\/content\/sci\/345\/6194\/295.full.pdf\"><u>1.A hole-conductor-free, fully printable mesoscopic perovskite solar cells with high stability<\/u><\/a><\/p>\n<p>\u88ab\u5f15\u6b21\u6570\uff1a1203<\/p>\n<p><a href=\"http:\/\/science.sciencemag.org\/content\/sci\/347\/6225\/970.full.pdf\"><u>2.Metal-free efficient photocatalyst for stable visible water splitting via a two-electron pathway<\/u><\/a><\/p>\n<p>\u88ab\u5f15\u6b21\u6570\uff1a1110<\/p>\n<p><a href=\"http:\/\/science.sciencemag.org\/content\/sci\/343\/6177\/1339.full.pdf\"><u>3.Highly crystalline multimetallic nanoframes with three-dimensional electrocatalytic surfaces<\/u><\/a><\/p>\n<p>\u88ab\u5f15\u6b21\u6570\uff1a863<\/p>\n<p><a href=\"http:\/\/science.sciencemag.org\/content\/sci\/350\/6263\/944.full.pdf\"><u>4.Efficient and stable large-area perovskite solar cells with inorganic charge extraction layers<\/u><\/a><\/p>\n<p>\u88ab\u5f15\u6b21\u6570\uff1a687<\/p>\n<p><a href=\"http:\/\/science.sciencemag.org\/content\/sci\/343\/6172\/752.full.pdf\"><u>5.Precise and ultrafast molecular sieving through graphene oxide membranes<\/u><\/a><\/p>\n<p>\u88ab\u5f15\u6b21\u6570\uff1a662<\/p>\n<p><a href=\"https:\/\/www.nature.com\/articles\/nature13792.pdf\"><u>6.Piezoelectricity of single-atomic-layer MoS<\/u><u><sub>2\u00a0<\/sub><\/u><u>for energy conversion and piezotronics<\/u><\/a><\/p>\n<p>\u88ab\u5f15\u6b21\u6570\uff1a484<\/p>\n<p><a href=\"http:\/\/science.sciencemag.org\/content\/350\/6267\/1508.full.pdf\"><u>7.Nitrogen-doped mesoporous carbon of extraordinary capacitance for electrochemical energy storage<\/u><\/a><\/p>\n<p>\u88ab\u5f15\u6b21\u6570\uff1a476<\/p>\n<p><a href=\"http:\/\/science.sciencemag.org\/content\/sci\/350\/6267\/1513.full.pdf\"><u>8.Synthesis of borophenes: anisotropic, two-dimensional boron polyporphs<\/u><\/a><\/p>\n<p>\u88ab\u5f15\u6b21\u6570\uff1a413<\/p>\n<p><a href=\"http:\/\/science.sciencemag.org\/content\/sci\/351\/6269\/141.full.pdf\"><u>9.Ultrahigh power factor and thermoelectric performance in hole-doped single-crystal SnSe<\/u><\/a><\/p>\n<p>\u88ab\u5f15\u6b21\u6570\uff1a389<\/p>\n<p><a href=\"http:\/\/science.sciencemag.org\/content\/349\/6253\/1208.full.pdf\"><u>10.Covalent organic frameworks comprising cobalt porphyrins for catalytic CO<\/u><u><sub>2\u00a0<\/sub><\/u><u>reduction in water<\/u><\/a><\/p>\n<p>\u88ab\u5f15\u6b21\u6570\uff1a364<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u65b0\u80fd\u6e90\u5b66\u672f\u7ec4gaxy\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n<p>\u6750\u6599\u4eba\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u8fd9\u91cc\u6c47\u96c6\u4e86\u5404\u5927\u9ad8\u6821\u7855\u535a\u751f\u3001\u4e00\u7ebf\u79d1\u7814\u4eba\u5458\u4ee5\u53ca\u884c\u4e1a\u4ece\u4e1a\u8005\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c<a href=\"http:\/\/www.cailiaoniu.com\/25127.html\"><u>\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8<\/u><\/a>\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n<p><strong><b>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1a<\/b><\/strong><strong><b>cailiaokefu<\/b><\/strong><strong><b>\u3002<\/b><\/strong><\/p>\n","protected":false},"excerpt":{"rendered":"<p>Nature\u548cScience\u4f5c\u4e3a\u5f53\u4eca\u5168\u7403\u6700\u5177\u6743\u5a01\u7684\u5b66\u672f\u671f\u520a\uff0c\u5728\u53d1\u8868\u539f\u59cb\u7814\u7a76\u8bba\u6587\u548c\u7efc\u8ff0\u7684\u540c\u65f6\uff0c\u4e5f\u5206\u6790\u5f53\u524d\u7814\u7a76\u548c\u79d1\u5b66\u653f\u7b56\uff0c\u8303\u56f4\u8986\u76d6\u4e86\u51e0\u4e4e\u6240\u6709\u5b66\u79d1\uff0c\u5728\u79d1\u5b66\u754c\u5177\u6709\u7edd\u5bf9\u7684&#8230;<\/p>\n","protected":false},"author":7336,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1187],"tags":[942],"class_list":["post-143949","post","type-post","status-publish","format-standard","hentry","category-zhuanlan","tag-report"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/143949"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/7336"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=143949"}],"version-history":[{"count":13,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/143949\/revisions"}],"predecessor-version":[{"id":144365,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/143949\/revisions\/144365"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=143949"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=143949"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=143949"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}