{"id":14620,"date":"2016-05-20T08:00:04","date_gmt":"2016-05-20T00:00:04","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=14620"},"modified":"2016-05-21T12:15:02","modified_gmt":"2016-05-21T04:15:02","slug":"%e7%a6%8f%e7%89%b9%e6%ac%b2%e6%8d%95%e8%8e%b7%e4%ba%8c%e6%b0%a7%e5%8c%96%e7%a2%b3%e5%88%b6%e9%80%a0%e5%a1%91%e6%96%99%e5%92%8c%e6%b3%a1%e6%b2%ab-%e6%af%8f%e5%b9%b4%e6%88%96%e5%8f%af%e8%8a%82%e7%9c%812","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=14620","title":{"rendered":"\u798f\u7279\u6b32\u6355\u83b7\u4e8c\u6c27\u5316\u78b3\u5236\u9020\u5851\u6599\u548c\u6ce1\u6cab \u6bcf\u5e74\u6216\u53ef\u8282\u770127.2\u4e07\u5428\u77f3\u6cb9"},"content":{"rendered":"<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14622\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/ford-co2-developed-plastics-8.jpg\" alt=\"ford-co2-developed-plastics-8\" width=\"700\" height=\"394\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/ford-co2-developed-plastics-8.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/ford-co2-developed-plastics-8-300x169.jpg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u6750\u6599\u725b\u6ce8\uff1a\u636e\u798f\u7279\u516c\u53f8\u900f\u9732\uff0c\u5176\u5c06\u91c7\u7528\u6355\u83b7\u78b3\u5236\u9020\u5851\u6599\u548c\u6ce1\u6cab\uff0c\u5728\u672a\u67655\u5e74\u5185\u5e94\u7528\u4e8e\u8f66\u578b\u3002<\/p>\n<p>\u968f\u7740\u78b3\u6392\u653e\u89c4\u5b9a\u8d8a\u6765\u8d8a\u4e25\u82db\uff0c\u592a\u591a\u7684\u76ee\u5149\u6295\u5411\u4e86\u5982\u4f55\u8ba9\u5f15\u64ce\u7684\u6548\u7387\u66f4\u9ad8\u3002\u4f46\u5f15\u64ce\u5e76\u975e\u6c7d\u8f66\u4e2d\u552f\u4e00\u4e00\u4e2a\u5bf9\u73af\u5883\u4e0d\u53cb\u597d\u7684\u90e8\u4ef6\u3002\u73af\u7ed5\u8f66\u53a2\u5185\u7684\u5851\u6599\u548c\u6ce1\u6cab\u5728\u5236\u9020\u8fc7\u7a0b\u4e2d\u5bf9\u73af\u5883\u7684\u7834\u574f\u4e5f\u4e0d\u9051\u591a\u8ba9\u3002\u56e0\u6b64\uff0c\u798f\u7279\u6b63\u5728\u5bfb\u6c42\u7528\u6355\u83b7\u4e8c\u6c27\u5316\u78b3\u6765\u5236\u9020\u5851\u6599\u548c\u6ce1\u6cab\u6765\u89e3\u51b3\u8fd9\u4e2a\u95ee\u9898\u3002<\/p>\n<p>\u8fd9\u4e2a\u5728\u52a0\u5de5\u5382\u4e2d\u6355\u6349\u78b3\u4ee5\u5408\u6210\u9ad8\u5206\u5b50\u7528\u4e8e\u6ce1\u6cab\u548c\u5851\u6599\u7684\u8ba1\u5212\u59cb\u4e8e2013\u5e74\u3002\u798f\u7279\u65b0\u578b\u6ce1\u6cab\u4e2d50%\u7684\u591a\u5143\u9187\u662f\u4e8c\u6c27\u5316\u78b3\u57fa\u7684\uff0c\u610f\u5473\u7740\u6ce1\u6cab\u5236\u4f5c\u8fc7\u7a0b\u4e2d\u8f83\u5c11\u5730\u7528\u5230\u4e86\u77f3\u6cb9\u3002\u798f\u7279\u6709\u8ba1\u5212\u5c06\u8fd9\u6837\u7684\u6ce1\u6cab\u5e94\u7528\u4e8e\u6c7d\u8f66\u7684\u5ea7\u4f4d\u548c\u5e95\u5c42\u4e0a\uff0c\u5e76\u79f0\u6b64\u4e3e\u6bcf\u5e74\u5c06\u8282\u7ea627.2\u4e07\u5428\u77f3\u6cb9\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14623\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/ford-co2-developed-plastics-2.jpg\" alt=\"ford-co2-developed-plastics-2\" width=\"740\" height=\"389\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/ford-co2-developed-plastics-2.jpg 740w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/ford-co2-developed-plastics-2-300x158.jpg 300w\" sizes=\"(max-width: 740px) 100vw, 740px\" \/><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-14625\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/ford-co2-developed-plastics-6.jpg\" alt=\"ford-co2-developed-plastics-6\" width=\"740\" height=\"389\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/ford-co2-developed-plastics-6.jpg 740w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/ford-co2-developed-plastics-6-300x158.jpg 300w\" sizes=\"(max-width: 740px) 100vw, 740px\" \/><\/p>\n<p>\u798f\u7279\u7684\u9ad8\u7ea7\u6280\u672f\u4e3b\u7ba1Debbie Mielewski\u4ecb\u7ecd\uff0c\u201c\u798f\u7279\u5728\u79ef\u6781\u5730\u901a\u8fc7\u964d\u4f4e\u4f7f\u7528\u5316\u77f3\u5236\u9020\u7684\u5851\u6599\u548c\u6ce1\u6cab\u6765\u6539\u5584\u73af\u5883\u3002\u800c\u8fd9\u9879\u6280\u672f\u7684\u6fc0\u52a8\u4eba\u5fc3\u4e4b\u5904\u662f\u5e2e\u52a9\u89e3\u51b3\u51e0\u4e4e\u4e0d\u53ef\u80fd\u89e3\u51b3\u7684\u95ee\u9898\u2014\u2014\u6c14\u5019\u53d8\u5316\u201d<\/p>\n<p>\u636e\u798f\u7279\u65b9\u9762\u4ecb\u7ecd\uff0c\u4ed6\u4eec\u6709\u8ba1\u5212\u52a0\u5927\u4f7f\u7528\u6355\u6349\u78b3\u5236\u9020\u7684\u5851\u6599\u548c\u6ce1\u6cab\uff0c\u4ee5\u964d\u4f4e\u5bf9\u77f3\u6cb9\u7684\u4ee5\u6765\uff0c\u800c\u8fd9\u79cd\u751f\u7269\u6750\u6599\u5c06\u5728\u672a\u6765\u4e94\u5e74\u5185\u5e94\u7528\u4e8e\u4ed6\u4eec\u7684\u8f66\u578b\u4e2d\u3002<\/p>\n<p>\u798f\u7279\u65b9\u9762\u7684\u62a5\u9053\uff1a<a href=\"https:\/\/media.ford.com\/content\/fordmedia\/fna\/us\/en\/news\/2016\/05\/17\/preserving-mother-earth-ford-first-automaker-captured-co2.html\" target=\"_blank\">PRESERVING MOTHER EARTH: FORD FIRST AUTOMAKER TO USE CAPTURED CO2 TO DEVELOP FOAM AND PLASTIC FOR VEHICLES<\/a><\/p>\n<p>\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u636e\u798f\u7279\u516c\u53f8\u900f\u9732\uff0c\u5176\u5c06\u91c7\u7528\u6355\u83b7\u78b3\u5236\u9020\u5851\u6599\u548c\u6ce1\u6cab\uff0c\u5728\u672a\u67655\u5e74\u5185\u5e94\u7528\u4e8e\u8f66\u578b\u3002 \u968f\u7740\u78b3\u6392\u653e\u89c4\u5b9a\u8d8a\u6765\u8d8a\u4e25\u82db\uff0c\u592a\u591a\u7684\u76ee\u5149\u6295\u5411\u4e86\u5982\u4f55\u8ba9\u5f15\u64ce\u7684\u6548\u7387\u66f4\u9ad8\u3002\u4f46\u5f15\u64ce\u5e76\u975e\u6c7d\u8f66&#8230;<\/p>\n","protected":false},"author":2,"featured_media":14623,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[3],"tags":[38,76,15],"class_list":["post-14620","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-yejie","tag-plastic","tag-carbon","tag-cheyong"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/14620"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=14620"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/14620\/revisions"}],"predecessor-version":[{"id":14898,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/14620\/revisions\/14898"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/14623"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=14620"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=14620"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=14620"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}