{"id":14715,"date":"2016-05-25T17:00:54","date_gmt":"2016-05-25T09:00:54","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=14715"},"modified":"2016-05-25T11:16:01","modified_gmt":"2016-05-25T03:16:01","slug":"%e7%a2%b3%e7%ba%b3%e7%b1%b3%e7%ae%a1%e5%ae%9e%e7%8e%b0%e8%87%aa%e7%bb%84%e8%a3%85","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=14715","title":{"rendered":"\u79d1\u5b66\u5bb6\u5b9e\u73b0\u4e86\u8fdc\u8ddd\u79bb\u78b3\u7eb3\u7c73\u7ba1\u81ea\u7ec4\u88c5 \u8fd8\u80fd\u70b9\u4eaeLED"},"content":{"rendered":"<p><strong><b><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/teslaphoresis-1.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-15505 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/teslaphoresis-1.jpg\" width=\"700\" height=\"394\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/teslaphoresis-1.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/teslaphoresis-1-300x169.jpg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/a><br \/>\n\u6750\u6599\u725b\u6ce8\uff1a<\/b><\/strong>\u83b1\u65af\u5927\u5b66\u7684\u79d1\u5b66\u5bb6\u4eec\u4f7f\u7528\u7279\u65af\u62c9\u7ebf\u5708\u4f7f\u78b3\u7eb3\u7c73\u7ba1\u7684\u81ea\u7ec4\u88c5\u6210\u5f88\u957f\u7684\u7ebf\uff0c\u8fde\u63a5LED\u5e76\u4f7f\u4e4b\u53d1\u5149\u3002\u7814\u7a76\u8005\u4eec\u5c06\u4e4b\u79f0\u4e3a\u201cteslaphoresis\u73b0\u8c61\u3002\u201d<\/p>\n<p>\u7531\u83b1\u65af\u5927\u5b66\u7275\u5934\uff0c\u7530\u7eb3\u897f\u5927\u5b66\u3001\u5fb7\u514b\u8428\u65af\u00a0A&amp;M\u5927\u5b66\u5de5\u7a0b\u5b66\u9662\u3001\u7b2c\u4e8c\u6d78\u4f1a\u4e2d\u5b66\u53c2\u4e0e\uff0c\u5171\u540c\u7ec4\u6210\u7684\u7814\u7a76\u8005\u5c0f\u7ec4\u53d1\u73b0\u4e86\u7279\u65af\u62c9\u7ebf\u5708\u53ef\u4ee5\u5f15\u5bfc\u78b3\u7eb3\u7c73\u7ba1\u5b8c\u6210\u957f\u8ddd\u79bb\u7684\u81ea\u7ec4\u88c5\u3002\u4e3a\u4e86\u7eaa\u5ff5\u8457\u540d\u79d1\u5b66\u5bb6\u5c3c\u53e4\u62c9\u00b7\u7279\u65af\u62c9\u53d1\u660e\u4e86\u53d8\u538b\u5668\u7535\u8def\uff0c\u6240\u4ee5\u56e2\u961f\u628a\u8fd9\u4e2a\u73b0\u8c61\u79f0\u4e4b\u4e3a\u201cteslaphoresis\u73b0\u8c61\u3002<\/p>\n<p>\u8be5\u5c0f\u7ec4\u7684\u7ec4\u957fPaul Cherukuri\u4ecb\u7ecd\u9053\uff1a\u201c\u7535\u573a\u65e9\u5df2\u53ef\u4ee5\u7528\u6765\u79fb\u52a8\u5c0f\u7269\u4f53\uff0c\u4f46\u8fd9\u79cd\u73b0\u8c61\u53ea\u80fd\u5728\u8d85\u77ed\u8ddd\u79bb\u4e2d\u5b9e\u73b0\u3002\u968f\u7740Teslaphoresis\u7684\u53d1\u73b0\uff0c\u6211\u4eec\u6709\u80fd\u529b\u901a\u8fc7\u63d0\u9ad8\u7535\u573a\u6765\u589e\u52a0\u7269\u4f53\u7684\u79fb\u52a8\u8ddd\u79bb\u3002\u770b\u5230\u623f\u95f4\u53e6\u4e00\u5934\u7684\u78b3\u7eb3\u7c73\u7ba1\u6d3b\u4e86\u8d77\u6765\u5e76\u76f8\u4e92\u8fde\u63a5\u6210\u7ebf\uff0c\u8fd9\u4e2a\u666f\u8c61\u975e\u5e38\u8ba9\u4eba\u9707\u60ca\uff01\u201d<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/teslaphoresis-2.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-15524\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/teslaphoresis-2.jpg\" alt=\"teslaphoresis-2\" width=\"700\" height=\"466\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/teslaphoresis-2.jpg 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/05\/teslaphoresis-2-300x200.jpg 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/a><\/p>\n<p>\u4e3a\u6b64\uff0c\u7814\u7a76\u56e2\u961f\u5728\u7279\u65af\u62c9\u73af\u8fde\u63a5\u4e86\u4e00\u4e2a\u5929\u7ebf\u4ee5\u4fbf\u5c06\u9ad8\u538b\u7535\u573a\u5411\u5916\u53d1\u5c04\uff0c\u4f7f\u5343\u4e07\u5355\u58c1\u78b3\u7eb3\u7c73\u7ba1\u8fde\u63a5\u5728\u4e00\u8d77\uff0c\u957f\u5230\u53ef\u4ee5\u5728\u5b8f\u89c2\u5c3a\u5ea6\u4e0b\u4f7f\u7528\uff0c\u6700\u957f\u8fbe\u5230\u4e8615\u5398\u7c73\u3002\u7279\u65af\u62c9\u7ebf\u5708\u6fc0\u53d1\u7684\u7535\u573a\u53ef\u4ee5\u4f7f\u7eb3\u7c73\u7ba1\u4e2d\u7684\u6b63\u8d1f\u7535\u8377\u53d1\u751f\u632f\u8361\uff0c\u4fc3\u4f7f\u5b83\u4eec\u7ec4\u88c5\u6210\u957f\u8ddd\u79bb\u6392\u5217\uff0c\u65b9\u5411\u671d\u5411\u7ebf\u5708\u3002\u66f4\u4ee4\u4eba\u60ca\u8bb6\u7684\u662f\uff0c\u78b3\u7eb3\u7c73\u7ba1\u4e5f\u53ef\u4ece\u7279\u65af\u62c9\u7ebf\u5708\u4e2d\u5438\u6536\u80fd\u91cf\uff0c\u5e76\u4f7fLED\u706f\u53d1\u5149\u3002<\/p>\n<p>\u636e\u6b64\uff0c\u7814\u7a76\u56e2\u961f\u8ba4\u4e3a\u8fd9\u79cd\u4f7f\u78b3\u7eb3\u7c73\u7ba1\u81ea\u7ec4\u88c5\u6210\u957f\u7ebf\u7684\u73b0\u8c61\u663e\u793a\u4e86Teslaphoresis\u5177\u5907\u4e86\u4ece\u5fae\u89c2\u76f4\u63a5\u5b9a\u5411\u7ec4\u88c5\u6210\u5b8f\u89c2\u7269\u4f53\u7684\u5e94\u7528\u6f5c\u80fd\u3002\u56e2\u961f\u6210\u5458Lindsey Bornhoeft\u4ecb\u7ecd\uff1a\u201c\u7eb3\u7c73\u7ba1\u7ebf\u7684\u751f\u957f\u548c\u4eba\u4f53\u795e\u7ecf\u4e00\u6837\uff0c\u81ea\u4e0a\u800c\u4e0b\u5730\u63a7\u5236\u7740\u7ec4\u88c5\u7eb3\u7c73\u6750\u6599\uff0c\u5b83\u4e3a\u53ef\u518d\u751f\u533b\u5b66\u7a0b\u5e8f\u6a21\u677f\u800c\u8fd0\u7528\u3002\u201d<\/p>\n<p>Cherukuri\u8865\u5145\u9053\uff1a\u201c\u5b83\u53ef\u4ee5\u627e\u5230\u5f88\u591a\u5e94\u7528\uff0c\u4f8b\u5982\u4eba\u4eec\u53ef\u4ee5\u5229\u7528\u5f3a\u5927\u7684\u7535\u573a\u529b\u6709\u6548\u5730\u63a7\u5236\u751f\u7269\u7cfb\u7edf\u548c\u4eba\u5de5\u7cfb\u7edf\u4e2d\u7269\u8d28\u7684\u884c\u4e3a\u3002\u751a\u81f3\uff0c\u968f\u7740\u4eba\u4eec\u7684\u4e0d\u65ad\u7814\u7a76\u8fd8\u4f1a\u53d1\u73b0\u66f4\u591a\u57fa\u7840\u7269\u7406\u3001\u5316\u5b66\u7684\u5185\u5bb9\uff0c\u73b0\u5728\u4ec5\u4ec5\u662f\u8be5\u8fc7\u7a0b\u7684\u7b2c\u4e00\u6b65\u3002\u201d<\/p>\n<p>\u539f\u6587\u53c2\u8003\u94fe\u63a5\uff1a<a href=\"http:\/\/ceramics.org\/ceramic-tech-today\/video-teslaphoresis-self-assembles-carbon-nanotubes-to-wire-and-light-led\" target=\"_blank\">Teslaphoresis self assembles carbon nanotubes to wire and light LED<\/a><\/p>\n<p>\u8bba\u6587\u5730\u5740\uff1a<a href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acsnano.6b02313\" target=\"_blank\">Teslaphoresis of Carbon Nanotubes<\/a><\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u5c01\u857e\u63d0\u4f9b\u7d20\u6750\uff0c\u59dc\u7f8e\u8363\u7f16\u8bd1\uff0c\u674e\u9510\u5ba1\u6838\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u83b1\u65af\u5927\u5b66\u7684\u79d1\u5b66\u5bb6\u4eec\u4f7f\u7528\u7279\u65af\u62c9\u7ebf\u5708\u4f7f\u78b3\u7eb3\u7c73\u7ba1\u7684\u81ea\u7ec4\u88c5\u6210\u5f88\u957f\u7684\u7ebf\uff0c\u8fde\u63a5LED\u5e76\u4f7f\u4e4b\u53d1\u5149\u3002\u7814\u7a76\u8005\u4eec\u5c06\u4e4b\u79f0\u4e3a\u201cteslaphoresis\u73b0\u8c61\u3002\u201d \u7531\u83b1\u65af\u5927\u5b66\u7275&#8230;<\/p>\n","protected":false},"author":230,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[76],"class_list":["post-14715","post","type-post","status-publish","format-standard","hentry","category-keji","tag-carbon"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/14715"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=14715"}],"version-history":[{"count":10,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/14715\/revisions"}],"predecessor-version":[{"id":15540,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/14715\/revisions\/15540"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=14715"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=14715"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=14715"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}