{"id":149640,"date":"2018-08-11T06:30:31","date_gmt":"2018-08-10T22:30:31","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=149640"},"modified":"2018-08-10T22:30:24","modified_gmt":"2018-08-10T14:30:24","slug":"%e6%96%b0%e5%9e%8b%e8%80%90%e9%ab%98%e6%b8%a9%e9%93%81%e7%b4%a0%e4%bd%93%e4%b8%8d%e9%94%88%e9%92%a2%e9%ab%98%e6%b8%a9%e6%8a%97%e6%b0%a7%e5%8c%96%e8%a1%8c%e4%b8%ba%e5%8f%8a%e6%9c%ba%e7%90%86%e7%a0%94","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=149640","title":{"rendered":"\u65b0\u578b\u8010\u9ad8\u6e29\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u9ad8\u6e29\u6297\u6c27\u5316\u884c\u4e3a\u53ca\u673a\u7406\u7814\u7a76\u53d6\u5f97\u65b0\u8fdb\u5c55"},"content":{"rendered":"<p>\u00a0 \u00a0 \u00a0 \u00a0 \u6700\u8fd1\uff0c\u4e1c\u5317\u5927\u5b66\u8f67\u5236\u6280\u672f\u53ca\u8fde\u8f67\u81ea\u52a8\u5316\u56fd\u5bb6\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u30012011\u94a2\u94c1\u5171\u6027\u6280\u672f\u534f\u540c\u521b\u65b0\u4e2d\u5fc3\u9648\u793c\u6e05\u6559\u6388\u7b49\u4eba\u5f00\u5c55\u4e86\u4e00\u9879\u5168\u65b0\u7814\u7a76\uff0c\u6df1\u5165\u63a2\u7d22\u4e86\u5143\u7d20W\u548c\u7a00\u571fCe\u5bf9\u65b0\u578b\u4e2d\u94ec\u8010\u9ad8\u6e29\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u9ad8\u6e29\u6297\u6c27\u5316\u884c\u4e3a\u7684\u5f71\u54cd\u53ca\u5176\u673a\u7406\u3002\u4ed6\u4eec\u8bbe\u8ba1\u4e86\u4e00\u7cfb\u5217\u4e0d\u540cW\u548cCe\u542b\u91cf\u7684444\u578b\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\uff0c\u5f00\u5c55\u4e86\u9ad8\u6e29\u4e0b\u6297\u6c27\u5316\u884c\u4e3a\u7684\u7814\u7a76\uff0c\u8fd0\u7528\u591a\u79cd\u5fae\u89c2\u5206\u6790\u624b\u6bb5\u5bf9\u5176\u754c\u9762\/\u57fa\u4f53\u5904\u6c27\u5316\u4ea7\u7269\u548c\u6790\u51fa\u7269\u7b49\u8fdb\u884c\u4e86\u8868\u5f81\u3002\u8be5\u7814\u7a76\u53d1\u73b0\uff1a\u6dfb\u52a0\u7a00\u571f\u5143\u7d20Ce\u6216\u540c\u65f6\u590d\u5408\u6dfb\u52a0\u4e00\u5b9a\u91cfW\u80fd\u663e\u8457\u964d\u4f4e\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u5728\u9ad8\u6e29\u4e0b\u7684\u6c27\u5316\u53cd\u5e94\u901f\u7387\uff0c\u6240\u5f62\u6210\u7684\u6c27\u5316\u819c\u66f4\u52a0\u5747\u5300\u81f4\u5bc6\uff0c\u5e76\u5177\u6709\u826f\u597d\u7684\u9644\u7740\u6027\uff0c\u5728\u6c27\u5316\u819c\/\u57fa\u4f53\u754c\u9762\u5904\u7f3a\u9677\u6570\u91cf\u660e\u663e\u51cf\u5c11\u3002\u4e0d\u540c\u7684W\u6dfb\u52a0\u91cf\u5bf9\u9ad8\u6e29\u6297\u6c27\u5316\u884c\u4e3a\u8d77\u4e0d\u540c\u7684\u4f5c\u7528\uff1b\u6dfb\u52a0Ce\u6216\u540c\u65f6\u6dfb\u52a0Ce\u548cW\u5143\u7d20\u53ef\u4ee5\u964d\u4f4e(Fe,Cr,Si)<sub>2<\/sub>(Nb,Mo)\u578bLaves\u76f8\u57281000-1050\u00baC\u4e0b\u7684\u56fa\u6eb6\u91cf\uff0cLaves\u76f8\u5728\u6676\u7c92\u5185\u6216\u6676\u754c\u5904\u6790\u51fa\u53ef\u6709\u6548\u6291\u5236\u53cd\u5e94\u5143\u7d20\u7684\u6269\u6563\u3002\u6b64\u5916\uff0c\u5728\u6c27\u5316\u819c\/\u57fa\u4f53\u754c\u9762\u5904\u6790\u51fa\u7684Laves\u76f8\u5bf9\u6c27\u5316\u819c\u7684\u751f\u957f\u884c\u4e3a\u548c\u5265\u843d\u673a\u5236\u4ea7\u751f\u91cd\u8981\u5f71\u54cd\uff0cLaves\u76f8\u7684\u5927\u91cf\u6790\u51fa\u4f1a\u5bfc\u81f4\u6c27\u5316\u819c\u7684\u5265\u843d\u3002<\/p>\n<p>\u00a0 \u00a0 \u00a0 \u00a0 \u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u56e0\u5177\u6709\u826f\u597d\u7684\u6210\u5f62\u6027\u3001\u4f18\u5f02\u7684\u8010\u5e94\u529b\u8150\u8680\u548c\u6297\u9ad8\u6e29\u6c27\u5316\u6027\u80fd\u53ca\u4f4e\u6210\u672c\u7b49\u4f18\u70b9\uff0c\u6df1\u53d7\u7814\u7a76\u8005\u548c\u4e1a\u754c\u7684\u9752\u7750\uff1b\u4e14\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u5177\u6709\u5408\u9002\u7684\u5bfc\u70ed\u7cfb\u6570\u53ca\u70ed\u81a8\u80c0\u7cfb\u6570\uff0c\u9002\u5408\u5e94\u7528\u4e8e\u70ed\u4ea4\u6362\u53ca\u70ed\u5faa\u73af\u7684\u573a\u5408\uff1b\u8fd9\u4e9b\u4f18\u70b9\u4f7f\u5f97\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u6210\u4e3a\u5236\u5907\u56fa\u4f53\u6c27\u5316\u7269\u71c3\u6599\u7535\u6c60(SOFC)\u8fde\u63a5\u4f53\u548c\u6c7d\u8f66\u6392\u6c14\u6b67\u7ba1\u7684\u6700\u4f73\u5019\u9009\u6750\u6599\u3002\u76ee\u524d\u7528\u4e8e\u5236\u9020\u6c7d\u8f66\u6392\u6c14\u6b67\u7ba1\u7684\u4f20\u7edf\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u7684\u5de5\u4f5c\u6e29\u5ea6\u7ea6\u4e3a900\u00baC\uff0c\u4f46\u4e3a\u4e86\u9002\u5e94\u73af\u4fdd\u8981\u6c42\u3001\u6ee1\u8db3\u65e5\u76ca\u4e25\u82db\u7684\u6c7d\u8f66\u5c3e\u6c14\u6392\u653e\u6807\u51c6\uff0c\u5e76\u8003\u8651\u6c7d\u6cb9\u5145\u5206\u71c3\u70e7\u540e\u7684\u6e29\u5347\uff0c\u6c7d\u8f66\u6392\u6c14\u6b67\u7ba1\u7684\u5c40\u90e8\u5de5\u4f5c\u6e29\u5ea6\u5c06\u8fbe\u5230950\u20131050\u00baC\uff0c\u751a\u81f3\u9ad8\u8fbe1100\u00baC\u3002\u4e3a\u9002\u5e94\u65b0\u4e00\u4ee3\u6c7d\u8f66\u6392\u6c14\u7cfb\u7edf\u70ed\u7aef\u5728\u5982\u6b64\u9ad8\u6e29\u73af\u5883\u4e0b\u4f7f\u7528\uff0c\u6709\u5fc5\u8981\u5728\u4e86\u89e3\u5408\u91d1\u5316\u673a\u7406\u8fdb\u884c\u5408\u91d1\u8bbe\u8ba1\u7684\u57fa\u7840\u4e0a\uff0c\u8fdb\u4e00\u6b65\u6df1\u5165\u8ba4\u8bc6\u65b0\u578b\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u7684\u9ad8\u6e29\u670d\u5f79\u53ca\u5176\u9000\u5316\u884c\u4e3a\u3002\u5df2\u6709\u7814\u7a76\u8868\u660e\uff0c\u901a\u8fc7\u6dfb\u52a0\u5408\u91d1\u5143\u7d20W\uff0c\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u7684\u6297\u70ed\u673a\u68b0\u75b2\u52b3\u6027\u80fd\u53ef\u5f97\u5230\u6539\u5584\uff0c\u4f46W\u5bf9\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u9ad8\u6e29\u6297\u6c27\u5316\u6027\u80fd\u7684\u5f71\u54cd\u7814\u7a76\u8f83\u5c11\u3002\u6b64\u5916\uff0c\u6dfb\u52a0\u7a00\u571f\u5143\u7d20\u4e5f\u6709\u5e0c\u671b\u63d0\u9ad8\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u6750\u6599\u7684\u9ad8\u6e29\u6297\u6c27\u5316\u6027\u80fd\u53ca\u8010\u70ed\u8150\u8680\u6027\u80fd\u3002\u4f46\u662f\uff0c\u8fc4\u4eca\u4e3a\u6b62\uff0c\u5408\u91d1\u5143\u7d20\u7684\u5408\u9002\u6dfb\u52a0\u91cf\u53ca\u5176\u4f5c\u7528\u673a\u7406\u4ecd\u4e0d\u660e\u786e\uff0c\u5c24\u5176\u662f\u9ad8\u7194\u70b9\u5408\u91d1\u5143\u7d20W\u548c\u7a00\u571fCe\u7684\u534f\u540c\u4f5c\u7528\u5bf9\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u9ad8\u6e29\u6297\u6c27\u5316\u6027\u80fd\u7684\u5f71\u54cd\u673a\u7406\u9700\u8981\u8fdb\u4e00\u6b65\u63a2\u7d22\u3002\u5bf9\u591a\u5143\u5408\u91d1\u5316\u8010\u9ad8\u6e29\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u7684\u9ad8\u6e29\u6297\u6c27\u5316\u884c\u4e3a\u53ca\u673a\u7406\u53d6\u5f97\u6df1\u5165\u7684\u8ba4\u8bc6\uff0c\u5c06\u5bf9\u65b0\u578b\u8010\u9ad8\u6e29\u94c1\u7d20\u4f53\u4e0d\u9508\u94a2\u7684\u8bbe\u8ba1\u548c\u5e94\u7528\u8d77\u91cd\u8981\u5173\u952e\u4f5c\u7528\u3002<\/p>\n<p>\u00a0 \u00a0 \u00a0 \u00a0 \u8be5\u7814\u7a76\u7ed3\u679c\u4e8e<strong>2018\u5e747\u670817\u65e5<\/strong>\u4ee5\u201c<strong>High temperature oxidation behavior of ferritic stainless steel containing W and Ce<\/strong>\u201d\u4e3a\u9898\uff0c\u5728\u7ebf\u53d1\u8868\u5728\u56fd\u9645\u8457\u540d\u671f\u520a\u201c<strong>Corrosion Science<\/strong>\u201d\u4e0a(5\u5e74\u5f71\u54cd\u56e0\u5b50\u4e3a5.238)\u3002\u8be5\u6587\u7684\u7b2c\u4e00\u4f5c\u8005\u4e3a\u535a\u58eb\u7814\u7a76\u751f\u9b4f\u4eae\u4eae\uff0c<strong>\u9648\u793c\u6e05\u6559\u6388\u4e3a\u8be5\u6587\u901a\u8baf\u4f5c\u8005<\/strong>\u3002\u7814\u7a76\u5de5\u4f5c\u5f97\u5230\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u59d4\u5458\u4f1a\u2014\u4e2d\u56fd\u5b9d\u6b66\u94a2\u94c1\u96c6\u56e2\u6709\u9650\u516c\u53f8\u94a2\u94c1\u8054\u5408\u7814\u7a76\u57fa\u91d1\u91cd\u70b9\u9879\u76ee\u7684\u8d44\u52a9(\u9879\u76ee\u7f16\u53f7\uff1aU1660205)\u3002<\/p>\n<p><b><\/b><br \/>\n <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-149642\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/12-1.jpg\" alt=\"\" width=\"368\" height=\"433\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/12-1.jpg 368w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/12-1-255x300.jpg 255w\" sizes=\"(max-width: 368px) 100vw, 368px\" \/><\/p>\n<p style=\"text-align: center;\"><span lang=\"EN-US\" style=\"margin: 0px; line-height: 150%; font-family: 'Times New Roman',serif; font-size: 12pt;\"><span style=\"color: #000000;\"><b>\u56fe1.\u5728<span lang=\"EN-US\">1000<\/span>\u2103\u4e0b\uff0c\u6c27\u5316\u5b9e\u9a8c\u94a2\u6c27\u5316\u5c42\u7684<span lang=\"EN-US\">BSE<\/span>\u663e\u5fae\u7167\u7247\u53ca<span lang=\"EN-US\">EPMA<\/span>\u5143\u7d20\u56fe<\/b><\/span><\/span><\/p>\n<p> <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-149643\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/13-1.jpg\" alt=\"\" width=\"452\" height=\"432\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/13-1.jpg 452w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/13-1-300x287.jpg 300w\" sizes=\"(max-width: 452px) 100vw, 452px\" \/><\/p>\n<p style=\"text-align: center;\"><b>\u56fe2.<\/b><b><strong>\u5728<\/strong><span lang=\"EN-US\">1050<\/span>\u2103\u4e0b\u6c27\u5316<span lang=\"EN-US\">100h<\/span>\uff0c\u5b9e\u9a8c\u94a2\u6c27\u5316\u5c42\u7684<span lang=\"EN-US\">BSE<\/span>\u663e\u5fae\u7167\u7247\u548c<span lang=\"EN-US\">EPMA<\/span>\u5143\u7d20\u56fe<\/b><\/p>\n<p>&nbsp;<\/p>\n<p><strong>\u539f\u6587\u94fe\u63a5<\/strong>\uff1a<a href=\"https:\/\/doi.org\/10.1016\/j.corsci.2018.07.017\" target=\"_blank\" rel=\"noopener\"><span style=\"float: none; background-color: transparent; color: #333333; cursor: text; font-family: Georgia,'Times New Roman','Bitstream Charter',Times,serif; font-size: 16px; font-style: normal; font-variant: normal; font-weight: 400; letter-spacing: normal; text-align: left; text-decoration: none; text-indent: 0px;\">High temperature oxidation behavior of ferritic stainless steel containing W and Ce\u00a0<\/span><\/a>(Corrosion Science, 2018,\u00a0<a class=\"doi\" title=\"Persistent link using digital object identifier\" href=\"https:\/\/doi.org\/10.1016\/j.corsci.2018.07.017\" target=\"_blank\" rel=\"noopener\" aria-label=\"Persistent link using digital object identifier\">doi.org\/10.1016\/j.corsci.2018.07.017<\/a>)<\/p>\n<p><span style=\"color: #000000;\">\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1<span lang=\"EN-US\" style=\"margin: 0px; font-family: 'Times New Roman',serif; font-size: 12pt;\"><b>tougao@cailiaoren.com<\/b><span style=\"font-family: Georgia,'Times New Roman','Bitstream Charter',Times,serif;\">\u3002<\/span><\/span><\/span><\/p>\n<p><strong>\u6750\u6599\u6d4b\u8bd5\uff0c\u6570\u636e\u5206\u6790\uff0c\u4e0a<span lang=\"EN-US\" style=\"margin: 0px; line-height: 150%; font-family: 'Times New Roman',serif; font-size: 12pt;\"><a href=\"http:\/\/www.ceshigu.com\/\" target=\"_blank\" rel=\"noopener\"><span lang=\"EN-US\">\u6d4b\u8bd5\u8c37<\/span><\/a><\/span>\uff01<\/strong><\/p>\n<p>&nbsp;<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u00a0 \u00a0 \u00a0 \u00a0 \u6700\u8fd1\uff0c\u4e1c\u5317\u5927\u5b66\u8f67\u5236\u6280\u672f\u53ca\u8fde\u8f67\u81ea\u52a8\u5316\u56fd\u5bb6\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u30012011\u94a2\u94c1\u5171\u6027\u6280\u672f\u534f\u540c\u521b\u65b0\u4e2d\u5fc3\u9648\u793c\u6e05\u6559\u6388\u7b49\u4eba\u5f00\u5c55\u4e86\u4e00\u9879\u5168\u65b0\u7814\u7a76\uff0c\u6df1\u5165\u63a2\u7d22\u4e86\u5143\u7d20W\u548c\u7a00\u571fCe\u5bf9&#8230;<\/p>\n","protected":false},"author":230,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215,2],"tags":[],"class_list":["post-149640","post","type-post","status-publish","format-standard","hentry","category-jiedu","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/149640"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=149640"}],"version-history":[{"count":6,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/149640\/revisions"}],"predecessor-version":[{"id":150270,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/149640\/revisions\/150270"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=149640"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=149640"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=149640"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}