{"id":150423,"date":"2018-08-15T06:30:12","date_gmt":"2018-08-14T22:30:12","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=150423"},"modified":"2018-08-16T12:26:37","modified_gmt":"2018-08-16T04:26:37","slug":"energy-environmental-science-%e7%94%a8%e4%ba%8e%e8%b6%85%e9%ab%98%e7%a8%b3%e5%ae%9a%e6%80%a7%e9%92%be%e7%a6%bb%e5%ad%90%e5%ad%98%e5%82%a8%e7%9a%84%e9%9b%b6%e5%ba%94%e5%8f%98k0-6mn1f2-7%e4%b8%ad","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=150423","title":{"rendered":"Energy &amp; Environmental Science: \u7528\u4e8e\u8d85\u9ad8\u7a33\u5b9a\u6027\u94be\u79bb\u5b50\u5b58\u50a8\u7684\u96f6\u5e94\u53d8K0.6Mn1F2.7\u4e2d\u7a7a\u7eb3\u7c73\u7acb\u65b9\u4f53"},"content":{"rendered":"<p><span style=\"color: #0000ff;\"><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/span><\/p>\n<p>\u76ee\u524d\u9502\u79bb\u5b50\u7535\u6c60\u5df2\u5e7f\u6cdb\u7528\u4e8e\u624b\u673a\u3001\u7535\u8111\u7b49\u5c0f\u578b\u7535\u5b50\u8bbe\u5907\uff0c\u4f46\u662f\u7531\u4e8e\u9502\u8d44\u6e90\u5206\u5e03\u4e0d\u5747\uff0c\u4ef7\u683c\u6602\u8d35\u7b49\u539f\u56e0\u4f7f\u5176\u96be\u4ee5\u5e94\u7528\u4e8e\u5927\u578b\u7684\u50a8\u80fd\u8bbe\u5907\u3002\u56e0\u6b64\uff0c\u4ef7\u683c\u4f4e\u5ec9\u7684\u94a0\u79bb\u5b50\u548c\u94be\u79bb\u5b50\u7535\u6c60\u5e94\u8fd0\u800c\u751f\u3002\u7531\u4e8e\u5730\u58f3\u4e2d\u94be\u7684\u4e30\u5ea6\u8f83\u9ad8\u5e76\u4e14K\/K<sup>+<\/sup>\u8fd8\u539f\u5bf9\u7684\u7535\u52bf\u76f8\u6bd4\u4e8eNa\/Na<sup>+<\/sup>\u66f4\u4f4e\u7b49\u4f18\u52bf\uff0c\u94be\u79bb\u5b50\u7535\u6c60\uff08KIBs\uff09\u5728\u50a8\u80fd\u9886\u57df\u91cc\u53d7\u5230\u79d1\u7814\u4eba\u5458\u8d8a\u6765\u8d8a\u591a\u7684\u5173\u6ce8\u3002<br \/>\n \u94be\u79bb\u5b50\u7535\u6c60\u4e0e\u9502\u79bb\u5b50\u7535\u6c60\u6709\u7740\u76f8\u4f3c\u7684\u201c\u6447\u6905\u5f0f\u201d\u5145\u653e\u7535\u539f\u7406\u3002\u7136\u800c\uff0c\u94be\u79bb\u5b50\u7535\u6c60\u7684\u53d1\u5c55\u4ecd\u7136\u505c\u7559\u5728\u521d\u671f\u9636\u6bb5\uff0c\u56e0\u4e3a\u94be\u79bb\u5b50\u7684\u79bb\u5b50\u534a\u5f84\u6bd4\u9502\u79bb\u5b50\u7684\u5927\uff0c\u4f7f\u5f97\u94be\u79bb\u5b50\u5728\u7535\u6781\u6750\u6599\u4e2d\u7684\u5d4c\u5165\u53d8\u5f97\u56f0\u96be\uff0c\u4ece\u800c\u9020\u6210\u4e86\u8131\u94be\u548c\u5d4c\u94be\u8fc7\u7a0b\u4e2d\u7684\u4f4e\u5bb9\u91cf\u3001\u4f4e\u500d\u7387\u6027\u80fd\u548c\u77ed\u5faa\u73af\u5bff\u547d\u3002\u56e0\u6b64\uff0c\u7814\u53d1\u51fa\u4e00\u79cd\u53ef\u4ee5\u89e3\u51b3\u5d4c\u94be\u6240\u5f15\u53d1\u4f53\u79ef\u81a8\u80c0\u7684\u96f6\u5e94\u53d8\u6750\u6599\u5177\u6709\u91cd\u8981\u610f\u4e49\u3002<\/p>\n<p><strong><span style=\"color: #0000ff;\">\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/span><\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c<strong>\u5317\u4eac\u79d1\u6280\u5927\u5b66\u65b0\u6750\u6599\u6280\u672f\u7814\u7a76\u9662\u66f2\u9009\u8f89\u8bfe\u9898\u7ec4<\/strong>\u5728<strong>Energy &amp; Environmental Science\uff08IF=30.067\uff09<\/strong>\u4e0a\u53d1\u8868\u4e86\u9898\u4e3a\u201c<strong>Zero-strain K<sub>0.6<\/sub>Mn<sub>1<\/sub>F<sub>2.7<\/sub> hollow nanocubes for ultrastable potassium ion storage<\/strong>\u201d\u7684\u8bba\u6587\uff0c\u8be5\u5de5\u4f5c\u62a5\u9053\u4e86\u4e00\u79cd\u5408\u6210\u5747\u5300\u4e2d\u7a7aKMnF-NCs\u7684\u65b0\u65b9\u6cd5\uff0c\u5e76\u901a\u8fc7\u63a7\u5236\u523b\u8680\u53cd\u5e94\u65f6\u95f4\u5728\u6676\u4f53\u7ed3\u6784\u4e2d\u521b\u9020\u7f3a\u9677\u4e0e\u7a7a\u4f4d\u3002\u7531\u4e8eK\u548cF\u7a7a\u4f4d\u7684\u5b58\u5728\uff0c\u8fd9\u4e2a\u7279\u6b8a\u7ed3\u6784\u53ef\u4ee5\u5bb9\u7eb3\u7531\u4e8e\u94be\u79bb\u5b50\u63d2\u5165\u5f15\u8d77\u7684\u4f53\u79ef\u81a8\u80c0\uff0c\u8fdb\u800c\u63d0\u9ad8KIBs\u7684\u5bb9\u91cf\u3001\u500d\u7387\u6027\u80fd\u548c\u5faa\u73af\u7a33\u5b9a\u6027\u3002\u540c\u65f6\uff0c\u8be5\u7814\u7a76\u8868\u660eKMnF-NCs\u7684\u6676\u4f53\u7ed3\u6784\u7f3a\u9677\u5bf9\u523b\u8680\u53cd\u5e94\u5177\u6709\u91cd\u8981\u5f71\u54cd\u3002\u5728\u53ef\u9006\u5145\u653e\u7535\u8fc7\u7a0b\u4e2d\uff0c\u8be5\u7247\u5c42\u7ed3\u6784\u5305\u8986\u7684\u7a7a\u5fc3\u7eb3\u7c73\u5757\u53ef\u4ee5\u63d0\u4f9b\u8f83\u5927\u7684\u6bd4\u8868\u9762\u79ef\u5e76\u5177\u6709\u8d5d\u7535\u5bb9\u7279\u6027\uff0c\u8fdb\u800c\u4f7f\u6750\u6599\u5177\u6709\u5c55\u73b0\u51fa\u9ad8\u5bb9\u91cf\u3001\u9ad8\u7a33\u5b9a\u6027\u548c\u4f18\u79c0\u7684\u500d\u7387\u6027\u80fd\u3002\u5728400 mA\u00b7g<sup>-1<\/sup>\u7684\u5927\u7535\u6d41\u5bc6\u5ea6\u4e0b\u5faa\u73af10000\u5708\u4ecd\u53ef\u4fdd\u6301110 mAh\u00b7g<sup>-1<\/sup> \u7684\u5bb9\u91cf\uff0c\u5bb9\u91cf\u4fdd\u6301\u7387\u9ad8\u8fbe99%\u3002\u9664\u6b64\u4e4b\u5916\uff0c\u8be5\u5de5\u4f5c\u901a\u8fc7\u539f\u4f4dXRD\u548cDFT\u8ba1\u7b97\uff0c\u8bc1\u660e\u4e86\u8be5\u6750\u6599\u5728\u8131\u5d4cK\u79bb\u5b50\u8fc7\u7a0b\u4e2d\u7684\u4f53\u79ef\u53d8\u5316\u57fa\u672c\u53ef\u4ee5\u5ffd\u7565\uff0c\u8868\u660e\u523b\u8680\u540e\u7684KMnF-NCs\u53ef\u4ee5\u4f5c\u4e3a\u4e00\u7c7b\u65b0\u7684\u5177\u6709\u826f\u597d\u5faa\u73af\u7a33\u5b9a\u6027\u7684\u96f6\u5e94\u53d8KIBs\u8d1f\u6781\u6750\u6599\u3002\u5317\u4eac\u79d1\u6280\u5927\u5b66<strong>\u5218\u5fd7\u4f1f\u535a\u58eb<\/strong>\u548c<strong>\u674e\u5e73\u6559\u6388<\/strong>\u4e3a\u8be5\u8bba\u6587\u7684\u7b2c\u4e00\u4f5c\u8005\uff0c<strong>\u5317\u4eac\u5927\u5b66\u738b\u4f1f\u535a\u58eb<\/strong>\u4e3a\u5171\u540c\u901a\u8baf\u4f5c\u8005\u3002<\/p>\n<p><strong><span style=\"color: #0000ff;\">\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/span><\/strong><\/p>\n<p><strong>\u56fe1. KMnF-NC\u7ed3\u6784\u7684\u5408\u6210\u793a\u610f\u56fe\u53ca\u5fae\u89c2\u7ed3\u6784\u8868\u5f81<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-150426\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-1.jpg\" alt=\"\" width=\"600\" height=\"448\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-1-300x224.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>(a) KMnF-NC\u7ed3\u6784\u5408\u6210\u793a\u610f\u56fe<\/p>\n<p>(b-e) \u523b\u8680\u65f6\u95f4\u5206\u522b\u4e3a0 h, 0.25 h, 1 h ,2 h\u7684TEM\u56fe\u50cf<\/p>\n<p>(f) \u523b\u86802 h\u540eKMnF-NC\u7684FESEM\u56fe\u50cf<\/p>\n<p>(g) \u523b\u86802 h\u540eKMnF-NC\u7684TEM\u56fe\u50cf<\/p>\n<p>(h) \u523b\u86802 h\u540eKMnF-NC\u7684HRTEM\u56fe\u50cf<\/p>\n<p>(i) \u523b\u86802 h\u540eKMnF-NC\u7684SAED\u56fe\u8c31<\/p>\n<p>(j) \u523b\u8680\u540eKMnF-NC\u7684STEM\u56fe\u50cf<\/p>\n<p>(k-m) \u523b\u8680\u540eKMnF-NC\u7684mapping\u56fe\u8c31<\/p>\n<p><strong>\u56fe2. KMnF-NC\u7ed3\u6784\u7684\u7269\u76f8\u8868\u5f81\u53caXPS\u8868\u5f81<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-150434\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-2-1.jpg\" alt=\"\" width=\"600\" height=\"294\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-2-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-2-1-300x147.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>(a) KMnF-LE\u7684XRD\u56fe\u8c31<\/p>\n<p>(b) KMnF-LE\u7684\u6c2e\u6c14\u5438\u8131\u9644\u66f2\u7ebf<\/p>\n<p>(c) KMnF-LE\u7684\u5b54\u5f84\u5206\u5e03\u66f2\u7ebf<\/p>\n<p>(e-f) KMnF-LE\u7684XPS\u66f2\u7ebf<\/p>\n<p><strong>\u56fe3. \u523b\u8680\u524d\u540eKMnF-NC\u7684\u7535\u5316\u5b66\u6027\u80fd<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-150435\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-3-1.jpg\" alt=\"\" width=\"600\" height=\"555\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-3-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-3-1-300x278.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>(a) KMnF-L\u7684\u5145\u653e\u7535\u66f2\u7ebf<\/p>\n<p>(b) KMnF-LE\u7684\u5145\u653e\u7535\u66f2\u7ebf<\/p>\n<p>(c) KMnF-L\u548cKMnF-LE\u7684\u5faa\u73af\u6027\u80fd<\/p>\n<p>(d) KMnF-L\u548cKMnF-LE\u7684\u500d\u7387\u6027\u80fd<\/p>\n<p>(e) 400 mA g-1 \u4e0bKMnF-LE\u7684\u957f\u5faa\u73af\u6027\u80fd<\/p>\n<p><strong>\u56fe4. \u4e0d\u540c\u7535\u6d41\u500d\u7387\u4e0bKMnF-L\u548cKMnF-LE\u7684\u5d4c\/\u8131\u94be\u884c\u4e3a\u793a\u610f\u56fe<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-150436\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-4-1.jpg\" alt=\"\" width=\"600\" height=\"508\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-4-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-4-1-300x254.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>(a) \u4f4e\u500d\u7387\u4e0bKMnF-L\u548cKMnF-LE\u7684\u5d4c\/\u8131\u94be\u884c\u4e3a\u793a\u610f\u56fe<\/p>\n<p>(b) \u9ad8\u500d\u7387\u4e0bKMnF-L\u548cKMnF-LE\u7684\u5d4c\/\u8131\u94be\u884c\u4e3a\u793a\u610f\u56fe<\/p>\n<p><strong>\u56fe5. \u539f\u4f4dXRD\u8868\u5f81\u548c\u7b2c\u4e00\u6027\u539f\u7406\u8ba1\u7b97\u6a21\u62df<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-150437\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-5-1.jpg\" alt=\"\" width=\"600\" height=\"695\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-5-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/EES-5-1-259x300.jpg 259w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>(a) KMnF-LE\u9996\u6b21\u5145\u653e\u7535\u4e2d\u4e0d\u540c\u7535\u538b\u4e0b\u7684XRD\u8c31\u56fe<\/p>\n<p>(b) KMnF<sub>3<\/sub> (K<sub>8<\/sub>Mn<sub>8<\/sub>F<sub>24<\/sub>)\u7ed3\u6784\u793a\u610f\u56fe<\/p>\n<p>(c) \u4e00\u4e2a\u94be\u79bb\u5b50\u5d4c\u5165KMnF<sub>3<\/sub> (K<sub>9<\/sub>Mn<sub>8<\/sub>F<sub>24<\/sub>)\u793a\u610f\u56fe<\/p>\n<p>(d) \u542b\u6709\u7a7a\u4f4d\u7684KMnF<sub>3<\/sub>(K<sub>5<\/sub>Mn<sub>8<\/sub>F<sub>21<\/sub>)\u793a\u610f\u56fe<\/p>\n<p>(e) \u4e09\u4e2a\u94be\u79bb\u5b50\u5d4c\u5165\u542b\u6709\u7a7a\u4f4d\u7684KMnF<sub>3<\/sub> (K<sub>8<\/sub>Mn<sub>8<\/sub>F<sub>21<\/sub>)\u793a\u610f\u56fe<\/p>\n<p>(f) \u56db\u4e2a\u94be\u79bb\u5b50\u5d4c\u5165\u542b\u6709\u7a7a\u4f4d\u7684KMnF<sub>3<\/sub> (K<sub>9<\/sub>Mn<sub>8<\/sub>F<sub>21<\/sub>)\u793a\u610f\u56fe<\/p>\n<p>(g) \u516d\u4e2a\u94be\u79bb\u5b50\u5d4c\u5165\u542b\u6709\u7a7a\u4f4d\u7684KMnF<sub>3<\/sub> (K<sub>11<\/sub>Mn<sub>8<\/sub>F<sub>21<\/sub>)\u793a\u610f\u56fe<\/p>\n<p><strong><span style=\"color: #0000ff;\">\u3010\u5c0f\u7ed3\u3011<\/span><\/strong><\/p>\n<p>\u8be5\u7814\u7a76\u901a\u8fc7\u63a7\u5236\u523b\u8680\u53cd\u5e94\u6210\u529f\u7684\u5408\u6210\u4e86\u5177\u6709\u5747\u4e00\u5c3a\u5bf8\u5e76\u542b\u6709\u7f3a\u9677\u7684\u4e2d\u7a7aKMnF-NC\u7eb3\u7c73\u7ed3\u6784\u3002\u5728\u5145\u653e\u7535\u8fc7\u7a0b\u4e2d\uff0c\u8fd9\u79cd\u72ec\u7279\u7684\u7ed3\u6784\u53ef\u4ee5\u540c\u65f6\u5b9e\u73b0\u5feb\u901f\u4f20\u5bfc\u79bb\u5b50\u548c\u8f83\u9ad8\u7684\u5bfc\u7535\u6027\uff0c\u5177\u6709\u4f4e\u7684\u7535\u538b\u5e73\u53f0\u548c\u8d5d\u7535\u5bb9\u7279\u6027\uff0c\u6545\u800c\u5c55\u73b0\u51fa\u8f83\u9ad8\u5bb9\u91cf\u548c\u826f\u597d\u7684\u500d\u7387\u6027\u80fd\u3002\u5728400 mA\u00b7g<sup>-1<\/sup>\u7684\u5927\u7535\u6d41\u5bc6\u5ea6\u4e0b\u5faa\u73af10000\u5708\u4ecd\u53ef\u4fdd\u6301110 mAh\u00b7g<sup>-1<\/sup> \u7684\u5bb9\u91cf\uff0c\u5bb9\u91cf\u4fdd\u6301\u7387\u9ad8\u8fbe99%\u3002\u9664\u6b64\u4e4b\u5916\uff0c\u8be5\u5de5\u4f5c\u901a\u8fc7\u539f\u4f4dXRD\u548cDFT\u8ba1\u7b97\uff0c\u8bc1\u660e\u4e86\u8be5\u6750\u6599\u5728\u8131\u5d4cK\u79bb\u5b50\u8fc7\u7a0b\u4e2d\u7684\u4f53\u79ef\u53d8\u5316\u57fa\u672c\u53ef\u4ee5\u5ffd\u7565\uff0c\u8868\u660e\u523b\u8680\u540e\u7684KMnF-LE\u53ef\u4ee5\u4f5c\u4e3a\u4e00\u7c7b\u65b0\u7684\u5177\u6709\u826f\u597d\u5faa\u73af\u7a33\u5b9a\u6027\u7684\u96f6\u5e94\u53d8KIBs\u8d1f\u6781\u6750\u6599\u3002<\/p>\n<p><strong><span style=\"color: #0000ff;\">\u3010\u56e2\u961f\u4ecb\u7ecd\u4ee5\u53ca\u76f8\u5173\u6210\u679c\u3011<\/span><\/strong><\/p>\n<p>\u5317\u4eac\u79d1\u6280\u5927\u5b66\u65b0\u6750\u6599\u6280\u672f\u7814\u7a76\u9662\u66f2\u9009\u8f89\u6559\u6388\u56e2\u961f\u957f\u671f\u4ece\u4e8b\u7279\u79cd\u7c89\u4f53\u6750\u6599\u5236\u5907\u3001\u7c89\u672b\u51b6\u91d1\u8fd1\u7ec8\u5f62\u6210\u5f62\u6280\u672f\u7684\u7814\u7a76\u3002\u8fd1\u5e74\u6765\uff0c\u8be5\u56e2\u961f\u5728\u66f2\u9009\u8f89\u3001\u79e6\u660e\u793c\u548c\u674e\u5e73\u6559\u6388\u7684\u5e26\u9886\u4e0b\uff0c\u81f4\u529b\u4e8e\u5c06\u65b0\u578b\u7c89\u4f53\u6750\u6599\u6280\u672f\u5e94\u7528\u4e8e\u96be\u7194\u91d1\u5c5e\u3001\u8f6f\u78c1\u5408\u91d1\u3001\u9ad8\u5bfc\u70ed\u6c2e\u5316\u94dd\u3001\u9502\u79bb\u5b50\u548c\u94be\u79bb\u5b50\u7535\u6781\u6750\u6599\u53ca\u71c3\u6599\u7535\u6c60\u50ac\u5316\u5242\u4e2d\u3002\u7814\u5236\u7684\u8fd1\u7403\u5f62\u5fae\u7ec6\uff08\u7eb3\u7c73\uff09\u94a8\u7c89\u3001\u94c1\u7c89\u548c\u6c2e\u5316\u94dd\u9676\u74f7\u7c89\u6ee1\u8db3\u4e86\u7c89\u672b\u6ce8\u5c04\u6210\u5f62\u6280\u672f\u7684\u9700\u8981\uff0c\u5b9e\u73b0\u4e86\u8fd9\u7c7b\u96be\u52a0\u5de5\u6750\u6599\u5236\u54c1\u7684\u8fd1\u7ec8\u5f62\u7cbe\u5bc6\u5236\u9020\u3002\u76f8\u5173\u4ea7\u54c1\u5df2\u5728\u56fd\u9632\u548c\u6c11\u7528\u9886\u57df\u83b7\u5f97\u5e94\u7528\uff0c\u66fe\u83b7\u56fd\u5bb6\u53d1\u660e\u4e13\u522940\u4f59\u9879\uff0c\u6559\u80b2\u90e8\u6280\u672f\u53d1\u660e\u4e00\u7b49\u59561\u9879\uff082011\u5e74\u5ea6\uff09\u3001\u4e2d\u56fd\u6709\u8272\u91d1\u5c5e\u5de5\u4e1a\u79d1\u5b66\u6280\u672f\u5956\uff08\u6280\u672f\u53d1\u660e\uff09\u4e00\u7b49\u59562\u9879\uff082016\u30012017\u5e74\u5ea6\uff09\u30022016\u5e74\u4ee5\u6765\u8be5\u56e2\u961f\u8bbe\u8ba1\u5408\u6210\u4e86\u4e00\u7cfb\u5217\u65b0\u578b\u7684\u7535\u6781\u6750\u6599\uff0c\u663e\u8457\u63d0\u9ad8\u9502\u79bb\u5b50\u548c\u94be\u79bb\u5b50\u7535\u6c60\u5faa\u73af\u5bb9\u91cf\u4e0e\u7a33\u5b9a\u6027\u3002\u540c\u65f6\uff0c\u4e3a\u4e86\u964d\u4f4e\u8d35\u91d1\u5c5e\u50ac\u5316\u5242\u5728\u50ac\u5316\u9886\u57df\u7684\u7528\u91cf\uff0c\u63d0\u51fa\u4e86\u8d35\u91d1\u5c5e\u50ac\u5316\u5242\u7eb3\u7c73\u6676\u5728\u78b3\u4e0e\u975e\u8d35\u91d1\u5c5e\u50ac\u5316\u5242\u8868\u9762\u56fa\u5b9a\u7684\u6982\u5ff5\u3002\u57fa\u4e8e\u8fd9\u4e9b\u65b0\u6750\u6599\uff0c\u8be5\u56e2\u961f\u63a2\u7d22\u4e86\u5176\u5728\u7535\u5bb9\u5668\uff0c\u7535\u89e3\u6c34\u6790\u6c22\u3001\u6790\u6c27\u4ee5\u53ca\u5438\u6ce2\u6750\u6599\u7b49\u9886\u57df\u7684\u5e94\u7528\u3002\u8be5\u7cfb\u5217\u521b\u65b0\u6027\u6210\u679c\u53d1\u8868\u5728Adv. Funct Mater, 2018, Accepted; Energy Storage Mater, 2018, 10, 268. J. Mater. Chem. A, 2018, 6, 11147; J. Mater. Chem. A, 2018, 6, 7053; ACS Appl. Mater. Inter, 2016, 8, 15582; ACS Appl. Mater. Inter, 2016, 8, 25954, Chem. Commun, 2017, 53, 2922\u7b49\u56fd\u9645\u77e5\u540d\u671f\u520a\u4e0a\u3002<\/p>\n<p><strong>\u611f\u8c22\u66f2\u9009\u8f89\u6559\u6388\u5bf9\u672c\u6587\u7684\u65a7\u6b63\u548c\u5bf9\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u7684\u6307\u5bfc\uff01<\/strong><\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong> <a href=\"http:\/\/pubs.rsc.org\/is\/content\/articlelanding\/2018\/ee\/c8ee01611a#!divAbstract\" target=\"_blank\" rel=\"noopener\">Zero-strain K<sub>0.6<\/sub>Mn<sub>1<\/sub>F<sub>2.7<\/sub> hollow nanocubes for ultrastable potassium ion storage<\/a> (Energy Environ. Sci., 2018, DOI: 10.1039\/C8EE01611A)<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u7eb3\u7c73\u7ec4\u6a59\u590f\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1\uff1atougao@cailiaoren.com\u3002<\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaokefu\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u76ee\u524d\u9502\u79bb\u5b50\u7535\u6c60\u5df2\u5e7f\u6cdb\u7528\u4e8e\u624b\u673a\u3001\u7535\u8111\u7b49\u5c0f\u578b\u7535\u5b50\u8bbe\u5907\uff0c\u4f46\u662f\u7531\u4e8e\u9502\u8d44\u6e90\u5206\u5e03\u4e0d\u5747\uff0c\u4ef7\u683c\u6602\u8d35\u7b49\u539f\u56e0\u4f7f\u5176\u96be\u4ee5\u5e94\u7528\u4e8e\u5927\u578b\u7684\u50a8\u80fd\u8bbe\u5907\u3002\u56e0\u6b64\uff0c\u4ef7\u683c\u4f4e\u5ec9\u7684\u94a0\u79bb\u5b50\u548c\u94be\u79bb\u5b50\u7535&#8230;<\/p>\n","protected":false},"author":9685,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[33,1689],"class_list":["post-150423","post","type-post","status-publish","format-standard","hentry","category-jiedu","tag-nano","tag-1689"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/150423"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/9685"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=150423"}],"version-history":[{"count":7,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/150423\/revisions"}],"predecessor-version":[{"id":150704,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/150423\/revisions\/150704"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=150423"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=150423"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=150423"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}