{"id":151080,"date":"2018-08-17T06:36:46","date_gmt":"2018-08-16T22:36:46","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=151080"},"modified":"2018-08-16T21:32:41","modified_gmt":"2018-08-16T13:32:41","slug":"%e9%93%9d%e5%90%88%e9%87%91%ef%bc%9a%e6%b1%bd%e8%bd%a6%e8%bd%bb%e9%87%8f%e5%8c%96%e7%9a%84%e4%b8%bb%e5%8a%9b","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=151080","title":{"rendered":"\u94dd\u5408\u91d1\uff1a\u6c7d\u8f66\u8f7b\u91cf\u5316\u7684\u4e3b\u529b"},"content":{"rendered":"<p>1.\u7531\u94dd\u5408\u91d1\u76f8\u4f34\u7684\u6c7d\u8f66\u8f7b\u91cf\u5316\u6f6e\u6d41<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-151081 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/1-33.png\" alt=\"\" width=\"600\" height=\"336\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/1-33.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/1-33-300x168.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe1. \u6b27\u6d32\u6c7d\u8f66\u5e73\u5747\u7528\u94dd\u91cf\u53d8\u5316<\/p>\n<p>\u5982\u4eca\uff0c\u201c\u8f7b\u91cf\u5316\u201d\u8fd9\u4e2a\u8bcd\u5df2\u7ecf\u7531\u6c7d\u8f66\u884c\u4e1a\u7684\u672f\u8bed\u53d1\u5c55\u4e3a\u5a92\u4f53\u65b0\u95fb\u91cc\u7684\u9ad8\u9891\u8bcd\u6c47\u3002\u300a\u4e2d\u56fd\u5236\u90202025\u300b\u4e2d\uff0c\u4e5f\u5df2\u628a\u8f7b\u91cf\u5316\u5f53\u6210\u6c7d\u8f66\u4ea7\u4e1a\u53d1\u5c55\u7684\u91cd\u8981\u65b9\u5411\u3002\u7b80\u5355\u6765\u8bf4\uff0c\u8f7b\u91cf\u5316\u5c31\u662f\u5728\u4fdd\u8bc1\u6c7d\u8f66\u5f3a\u5ea6\u548c\u5b89\u5168\u6027\u80fd\u7684\u524d\u63d0\u4e0b\uff0c\u5c3d\u53ef\u80fd\u964d\u4f4e\u6c7d\u8f66\u6574\u8f66\u91cd\u91cf\uff0c\u4ece\u800c\u63d0\u9ad8\u6c7d\u8f66\u52a8\u529b\u6027\uff0c\u51cf\u5c11\u71c3\u6599\u6d88\u8017\uff0c\u964d\u4f4e\u6392\u6c14\u6c61\u67d3\u3002\u8fd1\u5e74\u6765\uff0c\u7531\u4e8e\u73af\u4fdd\u548c\u8282\u80fd\u8981\u6c42\u65e5\u8d8b\u4e25\u683c\uff0c\u6c7d\u8f66\u8f7b\u91cf\u5316\u5df2\u6210\u4e3a\u4e16\u754c\u6c7d\u8f66\u53d1\u5c55\u7684\u52bf\u4e0d\u53ef\u6321\u7684\u8d8b\u52bf\u3002\u636e\u6b27\u6d32\u94dd\u4e1a\u534f\u4f1a\u62a5\u544a\uff0c\u6c7d\u8f66\u8d28\u91cf\u6bcf\u964d\u4f4e 100kg\uff0c\u6bcf\u767e\u516c\u91cc\u53ef\u8282\u7ea6 0.6L\u71c3\u6cb9\uff0c\u51cf\u6392CO<sub>2<\/sub>800-900g\u3002\u94dd\u7684\u5bc6\u5ea6\u4ec5\u6709\u94a2\u76841\/3\uff0c\u4e14\u5177\u6709\u826f\u597d\u7684\u53ef\u5851\u6027\u548c\u56de\u6536\u6027\uff0c\u662f\u7406\u60f3\u7684\u6c7d\u8f66\u8f7b\u91cf\u5316\u6750\u6599\u3002\u4e0a\u4e16\u7eaa70\u5e74\u4ee3\u7b2c\u4e00\u6b21\u7b2c\u4e8c\u6b21\u77f3\u6cb9\u5371\u673a\u671f\u95f4\uff0c\u9762\u5bf9\u65e5\u76ca\u9ad8\u6da8\u7684\u77f3\u6cb9\u4ef7\u683c\uff0c\u4e16\u754c\u8303\u56f4\u5185\u7684\u6c7d\u8f66\u5236\u9020\u5546\u5c1d\u8bd5\u7528\u94dd\u5408\u91d1\u5236\u9020\u4e4b\u524d\u94a2\u5236\u7684\u6563\u70ed\u5668\u3001\u6c14\u7f38\u76d6\u4e0e\u4fdd\u9669\u6760\u7b49\u90e8\u4ef6\u4ee5\u63d0\u9ad8\u71c3\u6cb9\u6548\u7387\u3002\u4ece\u6b64\uff0c\u94dd\u5408\u91d1\u5728\u6c7d\u8f66\u4e2d\u7684\u6bd4\u4f8b\u4e0d\u65ad\u63d0\u9ad8\u3002\u8457\u540d\u54a8\u8be2\u516c\u53f8\u8fbe\u79d1\u56fd\u9645\uff08Ducker Worldwide\uff09\u516c\u5e03\u7684\u7814\u7a76\u6570\u636e\u8868\u660e\uff0c\u6b27\u6d32\u6c7d\u8f66\u5e73\u5747\u7528\u94dd\u91cf\u81ea1990\u5e74\u5df2\u7ecf\u7ffb\u4e86\u4e09\u500d\uff0c\u753150kg\u589e\u957f\u5230\u76ee\u524d\u7684151kg\uff0c\u5e76\u5c06\u57282025\u5e74\u589e\u957f\u81f3196kg.<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-151082 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/2-32.png\" alt=\"\" width=\"600\" height=\"348\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/2-32.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/2-32-300x174.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe2. \u6b27\u6d32\u6c7d\u8f66\u7528\u94dd\uff08140kg\uff09\u5206\u5e03\u6bd4\u4f8b\uff082012\u5e74\u6570\u636e\uff09<\/p>\n<p>\u76ee\u524d\uff0c\u6c7d\u8f66\u8f7b\u91cf\u5316\u8d8b\u52bf\u8d8a\u6765\u8d8a\u731b\u70c8\uff0c\u94dd\u5408\u91d1\u5728\u8f6e\u6bc2\u3001\u53d1\u52a8\u673a\u3001\u6563\u70ed\u5668\u3001 \u6cb9\u7ba1\u7b49\u65b9\u9762\u7684\u5e94\u7528\u975e\u5e38\u5e7f\u6cdb\u3002\u8f66\u8eab\u8d28\u91cf\u5360\u6c7d\u8f66\u603b\u8d28\u91cf\u768440%\u5de6\u53f3\uff0c\u5bf9\u4e8e\u6574\u8f66\u7684\u8f7b\u91cf\u5316\u800c\u8a00\uff0c\u8f66\u8eab\u7684\u8f7b\u91cf\u5316\u8d77\u7740\u4e3e\u8db3\u8f7b\u91cd\u7684\u4f5c\u7528\u3002\u636e2016\u5e74\u6b27\u6d32\u8f66\u8eab\u4f1a\u8bae\uff08EuroCarBody 2016\uff09\u8d44\u6599\u663e\u793a\uff0c\u94dd\u5408\u91d1\u5e94\u7528\u7387\u5df2\u7ecf\u8fbe\u90e8\u5206\u9ad8\u7aef\u8f66\u578b\u767d\u8f66\u8eab\uff08\u5373\u5b8c\u6210\u710a\u63a5\u4f46\u672a\u6d82\u88c5\u7684\u8f66\u8eab\uff09\u8d28\u91cf\u7684\u4e00\u534a\u4ee5\u4e0a\u3002\u5982\u963f\u65af\u987f\u00b7\u9a6c\u4e01\uff08Aston Martin\uff09DB11\u94dd\u5408\u91d1\u5e94\u7528\u7387\u9ad8\u8fbe86.1%\uff0c\u00a0\u7b2c2\u4ee3\u672c\u7530NSX\uff08Acura NSX\uff09\u8fbe79.0%\uff0c \u7b2c5\u4ee3\u8def\u864e\u53d1\u73b0\uff08Land Rover Discovery\uff09\u8fbe62.9%\u3002\u7136\u800c\uff0c\u94dd\u5408\u91d1\u5728\u666e\u901a\u8f66\u578b\u8f66\u8eab\u4e0a\u7684\u5e94\u7528\u8fd8\u504f\u5c11\u3002\u8457\u540d\u54a8\u8be2\u516c\u53f8\u8fbe\u79d1\u56fd\u9645\uff08Ducker Worldwide\uff09\u7684\u6570\u636e\u663e\u793a\uff0c\u94dd\u5408\u91d1\u677f\u5728\u6c7d\u8f66\u8f66\u8eab\u7684\u6e17\u900f\u7387 2015 \u5e74\u65f6\u4ec5\u4e3a 4%\u3002\u65f6\u81f3\u4eca\u65e5\uff0c\u5168\u94dd\u8f66\u8eab\u5236\u9020\u4f9d\u7136\u662f\u4e00\u9879\u5904\u4e8e\u91d1\u5b57\u5854\u5c16\u7684\u6280\u672f\uff0c\u53ea\u5728\u90e8\u5206\u9ad8\u7aef\u8f66\u578b\u4e0a\u5f97\u4ee5\u5e94\u7528\u3002\u8f66\u8eab\u8f7b\u91cf\u5316\u662f\u76ee\u524d\u6c7d\u8f66\u5236\u9020\u5546\u8f7b\u91cf\u5316\u53d1\u5c55\u65b9\u9762\u7684\u91cd\u8981\u653b\u5173\u8bfe\u9898\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-151083 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/3-33.png\" alt=\"\" width=\"600\" height=\"507\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/3-33.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/3-33-300x254.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe3.\u00a0Aston Martin DB11\u94dd\u5408\u91d1\u5e94\u7528\u5206\u5e03<\/p>\n<p>2.\u8f66\u7528\u94dd\u5408\u91d1\u7684\u4e3b\u8981\u79cd\u7c7b<\/p>\n<p>\u76ee\u524d\u6c7d\u8f66\u7528\u94dd\u5408\u91d1\u57fa\u672c\u53ef\u5206\u4e3a\u538b\u94f8\u94dd\u5408\u91d1\u548c\u53d8\u5f62\u94dd\u5408\u91d1\uff0c\u5176\u4e2d\u4ee5\u538b\u94f8\u94dd\u5408\u91d1\u4e3a\u4e3b,\u7ea6\u536066%\u5de6\u53f3\u3002 \u53d8\u5f62\u94dd\u5408\u91d1\u53c8\u53ef\u4ee5\u5206\u4e3a\u8f67\u5236\u677f\u6750\uff0818%\uff09\uff0c\u6324\u538b\u578b\u6750\uff0811%\uff09\u53ca\u5c11\u91cf\u953b\u538b\u4ef6\uff085%\uff09\u3002\u503c\u5f97\u6ce8\u610f\u7684\u662f\uff0c2016\u5e74\u94f8\u9020\u94dd\u5408\u91d1\u867d\u7136\u4ecd\u662f\u8f66\u7528\u94dd\u5408\u91d1\u7684\u4e3b\u8981\u5f62\u5f0f\uff0c\u4f46\u5176\u4efd\u989d\u8f832012\u5e74\u4e0b\u964d\u4e868\u4e2a\u767e\u5206\u6bd4\u3002\u76f8\u53cd\uff0c\u7531\u4e8e\u8f66\u8eab\u8f7b\u91cf\u5316\u7684\u53d1\u5c55\uff0c\u8f67\u5236\u677f\u6750\u7684\u4efd\u989d\u75312012\u5e74\u768413%\u663e\u8457\u589e\u957f\u4e3a2016\u5e74\u768418%\u3002\u4e0e\u6b64\u540c\u65f6\uff0c\u6324\u538b\u578b\u6750\u4e0e\u953b\u538b\u4ef6\u7684\u4efd\u989d\u53d8\u5316\u4e0d\u5927\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-151084 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/4-26.png\" alt=\"\" width=\"600\" height=\"441\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/4-26.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/4-26-300x221.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe4. 2016\u5e74\u4e0e2012\u5e74\u6b27\u6d32\u6c7d\u8f66\u7528\u94dd\u79cd\u7c7b\u5bf9\u6bd4<\/p>\n<p>\uff081\uff09\u94f8\u9020\u94dd\u5408\u91d1<\/p>\n<p>\u94f8\u9020\u94dd\u5408\u91d1\u662f\u76ee\u524d\u5927\u90e8\u5206\u6c7d\u8f66\u4e0a\u7528\u91cf\u6700\u5927\u7684\u94dd\u5408\u91d1\u79cd\u7c7b\uff0c\u5e7f\u6cdb\u7528\u4e8e\u8f66\u8f6e\u3001\u53d1\u52a8\u673a\u90e8\u4ef6\u3001\u5e95\u67b6\u3001\u51cf\u9707\u5668\u652f\u67b6\u4ee5\u53ca\u7a7a\u95f4\u6846\u67b6\u7b49\u7ed3\u6784\u4ef6\u3002\u5728\u6c7d\u8f66\u5de5\u4e1a\u4e2d\uff0c\u94f8\u9020\u94dd\u5408\u91d1\u8f6e\u6bc2\u662f\u666e\u53ca\u6700\u5feb\u3001\u94dd\u5316\u7387\u8f83\u9ad8\u7684\u96f6\u90e8\u4ef6\u3002\u76ee\u524d\uff0c\u7edd\u5927\u591a\u6570\u94dd\u5408\u91d1\u8f66\u8f6e\u91c7\u7528A356\u5408\u91d1\u901a\u8fc7\u4f4e\u538b\u94f8\u9020\u6cd5\u5236\u9020\uff0c\u90e8\u5206\u9ad8\u6863\u8f66\u8f6e\u5219\u91c7\u7528\u6324\u538b\u94f8\u9020\uff08\u4e1a\u6001\u6a21\u953b\uff09\u3001\u953b\u9020\u6216\u65cb\u538b\u6280\u672f\u5236\u9020\u3002\u53d1\u52a8\u673a\u7684\u7f38\u4f53\u548c\u7f38\u76d6\u5747\u8981\u6c42\u6750\u6599\u5bfc\u70ed\u6027\u80fd\u597d\uff0c\u6297\u8150\u8680\u80fd\u529b\u5f3a\uff0c\u8fd9\u6b63\u662f\u94dd\u5408\u91d1\u7684\u4f18\u52bf\u6240\u5728\u3002\u76ee\u524d\u5927\u91cf\u56fd\u5185\u5916\u6c7d\u8f66\u91c7\u7528\u4e86\u94dd\u5236\u7f38\u4f53\u548c\u7f38\u76d6\uff0c\u4f46\u94f8\u94c1\u4ecd\u5728\u90e8\u5206\u8981\u6c42\u9ad8\u5f3a\u9ad8\u8010\u6027\u7684\u573a\u5408\u4f7f\u7528\u3002\u8fd1\u5e74\u6765\uff0c\u65b0\u578bAl-Si-Cu-Mg-Fe\u7cfb\u5408\u91d1\u7684\u5f00\u53d1\u53ca\u76f8\u5e94\u94f8\u9020\u6280\u672f\u7684\u53d1\u5c55\uff0c\u4f7f\u94dd\u5408\u91d1\u94f8\u4ef6\u8fbe\u5230\u66f4\u9ad8\u6027\u80fd\uff0c\u8fdb\u4e00\u6b65\u63a8\u52a8\u4e86\u94dd\u5408\u91d1\u5728\u53d1\u52a8\u673a\u90e8\u4ef6\uff08\u5305\u62ec\u67f4\u6cb9\u53d1\u52a8\u673a\uff09\u4e0a\u7684\u5e94\u7528\u3002\u7f38\u4f53\u7f38\u76d6\u7684\u94f8\u9020\u65b9\u6cd5\u4e5f\u8f83\u4e3a\u591a\u6837\uff0c\u5e38\u89c1\u7684\u6709\u91cd\u529b\u94f8\u9020\u3001\u4f4e\u538b\u94f8\u9020\u7b49\u3002\u6b64\u5916\uff0c\u94f8\u9020\u94dd\u5408\u91d1\u5728\u51cf\u9707\u5668\u652f\u67b6\u3001\u7535\u52a8\u8f66\u7535\u6c60\u5305\u3001\u7ed3\u6784\u7bb1\u4f53\u7b49\u7ed3\u6784\u4ef6\u5f97\u5230\u5927\u91cf\u5e94\u7528\u3002\u7531\u4e8e\u8fd9\u4e9b\u90e8\u4ef6\u591a\u4e3a\u5f62\u72b6\u590d\u6742\u7684\u8584\u58c1\u4ef6\uff0c\u6545\u591a\u91c7\u7528Al-Si\u5408\u91d1\u7531\u9ad8\u538b\u94f8\u9020\u65b9\u6cd5\u5236\u9020\u3002<\/p>\n<p>\uff082\uff09\u53d8\u5f62\u94dd\u5408\u91d1<\/p>\n<p>\u76f8\u8f83\u4e8e\u94f8\u9020\u94dd\u5408\u91d1\uff0c\u53d8\u5f62\u94dd\u5408\u91d1\u5728\u6c7d\u8f66\u4e0a\u7684\u5e73\u5747\u5e94\u7528\u4efd\u989d\u8fd8\u8f83\u5c11\u3002\u8fbe\u79d1\u56fd\u9645\uff08Ducker Worldwide\uff09\u7684\u8c03\u67e5\u8868\u660e\uff0c2016\u5e74\u53d8\u5f62\u94dd\u5408\u91d1\u4ec5\u5360\u8f66\u7528\u94dd\u5408\u91d1\u768434%\uff08\u8f67\u5236\u677f\u675018%\uff0c\u6324\u538b\u578b\u675011%\uff0c\u953b\u538b\u4ef65%\uff09\u3002\u7136\u800c\u5728\u90e8\u5206\u91c7\u7528\u5168\u94dd\u8f66\u8eab\u7684\u9ad8\u7aef\u8f66\u578b\u4e0a\uff0c\u53d8\u5f62\u94dd\u5408\u91d1\u7684\u4efd\u989d\u8fdc\u8fdc\u9ad8\u4e8e\u94f8\u9020\u94dd\u5408\u91d1\u3002\u76ee\u524d\u4e1a\u5185\u5bf9\u5305\u62ec\u5168\u94dd\u8f66\u8eab\u6280\u672f\u5728\u5185\u7684\u53d8\u5f62\u94dd\u5408\u91d1\u7684\u7814\u53d1\u4e0e\u5e94\u7528\u6280\u672f\u6295\u5165\u8f83\u5927\uff0c\u5176\u6240\u5360\u6bd4\u4f8b\u8fc5\u901f\u589e\u5927\u3002\u8fbe\u79d1\u56fd\u9645\uff08Ducker Worldwide\uff09\u9884\u6d4b\uff0c\u7531\u4e8e\u94dd\u5408\u91d1\u8f66\u8eab\u6280\u672f\u7684\u5feb\u901f\u53d1\u5c55\uff0c\u53d8\u5f62\u94dd\u5408\u91d1\uff08\u7279\u522b\u662f\u8f67\u5236\u677f\u6750\uff09\u5728\u6c7d\u8f66\u4e0a\u7684\u5e94\u7528\u5c06\u8fce\u6765\u8fc5\u901f\u589e\u957f\uff08\u5982\u56fe1\u6240\u793a\uff09\u3002<\/p>\n<p>\u8f66\u7528\u53d8\u5f62\u94dd\u5408\u91d1\u4e3b\u8981\u5305\u62ec5xxx\u7cfb\uff08Al-Mg\u7cfb\uff09\u30016xxx\u7cfb\uff08Al-Mg-Si\u7cfb\uff09\uff0c\u4ee5\u53ca\u5c11\u91cf2xxx\u7cfb\uff08Al-Cg\u7cfb\uff09\u30017xxx\u7cfb\uff08Al-Zn-Mg\u7cfb\uff09\u3002\u5176\u4e2d\uff0c5xxx\u7cfb\u5408\u91d1\u4e0d\u53ef\u70ed\u5904\u7406\u5f3a\u5316\uff0c\u6210\u578b\u6027\u80fd\u4f18\u826f\uff0c\u4f46\u6210\u578b\u540e\u6613\u51fa\u73b0\u5c48\u670d\u70b9\u5ef6\u957f\u800c\u8868\u9762\u8d77\u76b1\uff0c\u5f71\u54cd\u4ea7\u54c1\u5916\u89c2\u8d28\u91cf\uff0c\u56e0\u6b64\u4e3b\u8981\u7528\u4e8e\u5185\u677f\u7b49\u5f62\u72b6\u590d\u6742\u7684\u90e8\u4f4d\u30026xxx\u7cfb\u5408\u91d1\u5219\u53ef\u901a\u8fc7Mg\u3001Si\u7684\u56fa\u6eb6\u53caMg<sub>2<\/sub>Si\u76f8\u7684\u65f6\u6548\u6790\u51fa\u8fdb\u884c\u70ed\u5904\u7406\u5f3a\u5316\uff0c\u5176\u6d82\u88c5\u70d8\u5e72\u540e\u5f3a\u5ea6\u63d0\u9ad8\uff0c\u4e14\u6709\u8f83\u9ad8\u7684\u6297\u51f9\u75d5\u6027\uff0c\u9002\u7528\u4e8e\u5916\u677f\u3001\u8f66\u8eab\u6846\u67b6\u7b49\u8981\u6c42\u5f3a\u5ea6\u3001\u521a\u6027\u7684\u90e8\u4f4d\u3002\u9664\u8f67\u5236\u677f\u6750\uff0c\u6324\u538b\u578b\u6750\u4e5f\u662f\u91cd\u8981\u8f66\u7528\u53d8\u5f62\u94dd\u5408\u91d1\uff0c\u4e00\u822c\u9002\u7528\u4e8e\u7b49\u622a\u9762\u7684\u7ed3\u6784\u4ef6\uff0c\u5982\u4fdd\u9669\u6760\u3001\u5438\u80fd\u76d2\u3001\u524d\u7eb5\u6881\u524d\u6bb5\u3001\u95e8\u69db\u3001\u540e\u7eb5\u6881\u540e\u6bb5\u3002\u4e2d\u7b49\u5f3a\u5ea6\u76846xxx\u56e0\u5176\u8f83\u9ad8\u7684\u6324\u51fa\u901f\u7387\u548c\u8868\u9762\u8d28\u91cf\uff0c\u4ee5\u53ca\u6324\u538b\u8fc7\u7a0b\u4e2d\u7684\u65f6\u6548\u786c\u5316\u7279\u6027\uff0c\u662f\u6324\u538b\u578b\u6750\u7684\u4e3b\u8981\u6750\u6599\u3002\u5728\u90e8\u5206\u5f3a\u5ea6\u8981\u6c42\u8f83\u9ad8\u7684\u573a\u5408\uff0c\u9ad8\u5f3a7xxx \u7cfb\u94dd\u5408\u91d1\u4e5f\u7528\u6765\u751f\u4ea7\u6324\u538b\u578b\u6750\u3002\u540c\u65f6\uff0c\u4e3a\u63d0\u9ad8\u6297\u51b2\u51fb\u5f3a\u5ea6\uff0c \u578b\u6750\u65ad\u9762\u591a\u91c7\u7528\u201c\u53e3\u201d\u3001\u201c\u65e5\u201d\u3001\u201c\u76ee\u201d\u5b57\u5f62\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-151085 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/5-21.png\" alt=\"\" width=\"600\" height=\"605\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/5-21.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/5-21-150x150.png 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/5-21-298x300.png 298w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe5. \u6324\u538b\u578b\u6750\u5236\u9020\u7684\u201c\u65e5\u201d\u5b57\u578b\u5438\u80fd\u76d2\uff08\u5de6\u4fa7\u4e3a\u78b0\u649e\u524d\uff0c\u53f3\u4fa7\u4e3a\u78b0\u649e\u5438\u80fd\u540e\uff09<\/p>\n<p>3.\u8f66\u7528\u94dd\u5408\u91d1\u7684\u6311\u6218\u4e0e\u53d1\u5c55\u65b9\u5411<\/p>\n<p>\u94dd\u5408\u91d1\u5728\u6c7d\u8f66\u8f7b\u91cf\u5316\u6d6a\u6f6e\u4e2d\u53d1\u6325\u4e86\u91cd\u8981\u4f5c\u7528\uff0c\u7136\u800c\u4e5f\u9762\u4e34\u7740\u91cd\u8981\u6311\u6218\u3002\u5b9e\u9645\u4e0a\uff0c\u8f7b\u91cf\u5316\u5e76\u4e0d\u4ec5\u4ec5\u662f\u8981\u6c42\u51cf\u91cd\uff0c\u800c\u662f\u8981\u505a\u5230\u8f66\u8f86\u7684\u6027\u80fd\u3001\u5b89\u5168\u3001\u6210\u672c\u548c\u91cd\u91cf\u56db\u8005\u4e4b\u95f4\u7684\u5e73\u8861\u3002\u76ee\u524d\uff0c\u8f66\u7528\u94dd\u5408\u91d1\u9762\u4e34\u7684\u6838\u5fc3\u963b\u529b\u4ecd\u7136\u662f\u9ad8\u6602\u7684\u6210\u672c\uff0c\u8fd9\u4f7f\u5f97\u5168\u94dd\u8f66\u8eab\u7684\u5e94\u7528\u53ea\u80fd\u5c40\u9650\u4e8e\u9ad8\u7aef\u8f66\u578b\u800c\u6682\u65f6\u65e0\u6cd5\u5411\u6570\u91cf\u5e9e\u5927\u7684\u7ecf\u6d4e\u8f66\u578b\u62d3\u5c55\u3002\u94dd\u5408\u91d1\u7684\u6027\u80fd\u9650\u5236\uff0c\u4e5f\u662f\u5236\u7ea6\u5176\u53d1\u5c55\u7684\u91cd\u8981\u56e0\u7d20\u3002\u5728\u67d0\u4e9b\u90e8\u4ef6\u4e0a\uff0c\u5b83\u4ecd\u7136\u65e0\u6cd5\u53d6\u4ee3\u94a2\u94c1\u3002\u540c\u65f6\uff0c\u94dd\u5408\u91d1\u7684\u8fde\u63a5\u6280\u672f\uff0c\u5c24\u5176\u662f\u94f8\u94c1-\u94dd\u3001\u94a2-\u94dd\u3001\u9541-\u94dd\u7b49\u591a\u6750\u6599\u8fde\u63a5\u6280\u672f\u4e5f\u662f\u94dd\u5408\u91d1\u5728\u6c7d\u8f66\u4e0a\u5e94\u7528\u53d7\u963b\u7684\u4e00\u5927\u56e0\u7d20\u3002\u5965\u8fea\u5168\u65b0A8\u00a0D5\u5c31\u201c\u629b\u5f03\u201d\u4e86\u575a\u6301\u4e86\u4e8c\u5341\u4f59\u5e74\u7684\u5168\u94dd\u8f66\u8eab\uff0c\u800c\u91c7\u7528\u4e86\u91cd\u91cf\u53ef\u89c2\u7684\u9ad8\u5f3a\u94a2\u3002\u53d7\u6b64\u5f71\u54cd\uff0cD5\u8f66\u578b\u6bd4\u4e0a\u4e00\u4ee3\u8f66\u578b\u589e\u91cd51KG\uff0c\u4f46\u8f66\u8eab\u6297\u626d\u521a\u6027\u5927\u5e45\u63d0\u534724%\uff0c\u5b89\u5168\u6027\u5927\u5e45\u589e\u5f3a\uff0c\u540c\u65f6\u4e5f\u5927\u5e45\u964d\u4f4e\u4e86\u6210\u672c\u3002<\/p>\n<p>\u6b27\u76df\u66fe\u5728\u7b2c\u516d\u6846\u67b6\u8ba1\u5212\u4e0b\u4e8e2004-2009\u5e74\u7ec4\u7ec79\u4e2a\u56fd\u5bb6\u548c\u5730\u533a\u768438\u5bb6\u5355\u4f4d\u5408\u4f5c\u5b9e\u65bd\u4e86\u8d85\u8f7b\u8f66\u8eab\u8054\u5408\u7814\u53d1\u9879\u76ee\uff08SuperLight-Car\uff09\u3002\u8be5\u9879\u76ee\u7ecf\u9a8c\u8868\u660e\uff0c\u8f66\u7528\u94dd\u5408\u91d1\u7684\u8fdb\u4e00\u6b65\u53d1\u5c55\uff0c\u5e94\u540c\u65f6\u81f4\u529b\u4e8e\u65b0\u578b\u9ad8\u6027\u80fd\u5408\u91d1\u548c\u65b0\u578b\u751f\u4ea7\u6280\u672f\u7684\u7814\u53d1\u3002\u7814\u53d1\u5de5\u4f5c\u8fd8\u9700\u8981\u6574\u5408\u8d44\u6e90\uff0c\u7531\u6c7d\u8f66\u5236\u9020\u5546\u7275\u5934\uff0c\u8054\u5408\u539f\u6750\u6599\u3001\u96f6\u90e8\u4ef6\u4f9b\u5e94\u5546\u53ca\u76f8\u5173\u79d1\u7814\u673a\u6784\uff0c\u5171\u540c\u63a2\u7d22\u5148\u8fdb\u7684\u8f7b\u91cf\u5316\u6280\u672f\uff0c\u63a8\u52a8\u8f66\u8eab\u8f7b\u91cf\u5316\u76f8\u5173\u4ea7\u4e1a\u94fe\u7684\u5efa\u7acb\u3002<\/p>\n<p><strong>\u4e3b\u8981\u53c2\u8003\u8d44\u6599\uff1a<\/strong><\/p>\n<p>1.Hirsch, J. (2014). Recent development in aluminium for automotive applications.\u00a0Transactions of Nonferrous Metals Society of China,\u00a024(7), 1995-2002.<\/p>\n<p>2.Hirsch, J. (2011). Aluminium in innovative light-weight car design.\u00a0Materials Transactions,\u00a052(5), 818-824.<\/p>\n<p>3.Lahaye, C., Hirsch, J., Bassan, D., Criqui, B., Sahr, C., Goede, M., &amp; Volkswagen, A. G. (2008). Contribution of aluminium to the multi-material light-weight BIW design of superlight-car [C]. In\u00a0HIRSCH J, SKROTZKI B, GOTTSTEIN G. Proceedings of the 11th International Conference on Aluminium Alloys. Weinheim: WILEY-VCH Verlag GmbH &amp; Co. KGaA\u00a0(pp. 2363-2373).<\/p>\n<p>4.Aluminum Content in Cars. Ducker Worldwide, <a href=\"https:\/\/www.ducker.com\/\"><u>https:\/\/www.ducker.com\/<\/u><\/a><\/p>\n<p>5.Aluminium in cars, unlocking the light-weighting potential. European Aluminium Association,<a href=\"https:\/\/www.european-aluminium.eu\/\"><u>https:\/\/www.european-aluminium.eu\/<\/u><\/a><\/p>\n<p>6.Goede, M., Stehlin, M., Rafflenbeul, L., Kopp, G., &amp; Beeh, E. (2009). Super Light Car\u2013lightweight construction thanks to a multi-material design and function integration, European Transport Research Review, 1: 5-10.<\/p>\n<p>7.2016\u6b27\u6d32\u8f66\u8eab\u4f1a\u8bae(EuroCarBody\uff09\u8d44\u6599\u3002<\/p>\n<p>\u6750\u6599\u4eba\u4e13\u680f\u79d1\u6280\u987e\u95ee\u6731\u8001\u5e08\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c<strong><b>\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com<\/b><\/strong>\u3002<\/p>\n<p>\u6750\u6599\u4eba\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1a<strong><b>cailiaokefu<\/b><\/strong>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>1.\u7531\u94dd\u5408\u91d1\u76f8\u4f34\u7684\u6c7d\u8f66\u8f7b\u91cf\u5316\u6f6e\u6d41 \u56fe1. \u6b27\u6d32\u6c7d\u8f66\u5e73\u5747\u7528\u94dd\u91cf\u53d8\u5316 \u5982\u4eca\uff0c\u201c\u8f7b\u91cf\u5316\u201d\u8fd9\u4e2a\u8bcd\u5df2\u7ecf\u7531\u6c7d\u8f66\u884c\u4e1a\u7684\u672f\u8bed\u53d1\u5c55\u4e3a\u5a92\u4f53\u65b0\u95fb\u91cc\u7684\u9ad8\u9891\u8bcd\u6c47\u3002\u300a\u4e2d\u56fd\u5236\u90202025\u300b\u4e2d\uff0c&#8230;<\/p>\n","protected":false},"author":9133,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[4],"tags":[],"class_list":["post-151080","post","type-post","status-publish","format-standard","hentry","category-ganhuo"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/151080"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/9133"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=151080"}],"version-history":[{"count":6,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/151080\/revisions"}],"predecessor-version":[{"id":151210,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/151080\/revisions\/151210"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=151080"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=151080"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=151080"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}