{"id":151699,"date":"2018-08-23T06:32:00","date_gmt":"2018-08-22T22:32:00","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=151699"},"modified":"2018-08-22T22:32:13","modified_gmt":"2018-08-22T14:32:13","slug":"%e6%96%af%e5%9d%a6%e7%a6%8f%e9%b2%8d%e5%93%b2%e5%8d%97%e5%9b%a2%e9%98%9fnature%e5%ad%90%e5%88%8a%e9%87%8d%e7%a3%85%e7%aa%81%e7%a0%b4%ef%bc%9a%e7%94%b5%e5%ad%90%e7%9a%ae%e8%82%a4%e4%bb%8e%e6%ad%a4","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=151699","title":{"rendered":"\u65af\u5766\u798f\u9c8d\u54f2\u5357\u56e2\u961fNature\u5b50\u520a\u91cd\u78c5\u7a81\u7834\uff1a\u7535\u5b50\u76ae\u80a4\u4ece\u6b64\u4e0d\u6015\u4f24\u5bb3"},"content":{"rendered":"<p><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/p>\n<p>\u6a21\u4eff\u4eba\u7c7b\u76ae\u80a4\u7684\u67d4\u8f6f\u4e14\u53ef\u53d8\u5f62\u7684\u7535\u5b50\u5668\u4ef6\u9002\u7528\u4e8e\u4e0b\u4e00\u4ee3\u53ef\u7a7f\u6234\u7535\u4ea7\u54c1\uff0c\u5047\u80a2\u4eba\u9020\u76ae\u80a4\u548c\u57fa\u4e8e\u9ad8\u6027\u80fd\u6750\u6599\u7684\u690d\u5165\u5f0f\u533b\u7597\u8bbe\u5907\u7b49\u9886\u57df\uff0c\u5177\u6709\u5de8\u5927\u7684\u5b9e\u7528\u4ef7\u503c\u5e76\u5c06\u6df1\u6df1\u5730\u6539\u53d8\u4eba\u4eec\u7684\u751f\u6d3b\u65b9\u5f0f\u3002\u800c\u5236\u9020\u5177\u6709\u4eba\u7c7b\u76ae\u80a4\u81ea\u6108\u5408\u7279\u6027\u7684\u67d4\u6027\u7535\u5b50\u5668\u4ef6\u6781\u5177\u6311\u6218\u6027\u3002\u4e3a\u4e86\u6a21\u4eff\u4eba\u4f53\u76ae\u80a4\u7684\u4fee\u590d\u6027\u800c\u5f00\u53d1\u7684\u53ef\u81ea\u4fee\u590d\u7684\u6750\u6599\u6709\u53ef\u80fd\u4f7f\u53ef\u62c9\u4f38\u7535\u5b50\u8bbe\u5907\u8584\u800c\u67d4\u8f6f\u7684\u7ed3\u6784\u5728\u5076\u7136\u7684\u673a\u68b0\u635f\u4f24\u4e2d\u53d8\u5f97\u975e\u5e38\u7a33\u5065\uff0c\u5e76\u4e14\u53ef\u4ee5\u9632\u6b62\u5668\u4ef6\u906d\u5230\u6c38\u4e45\u6027\u635f\u574f\u3002\u5c3d\u7ba1\u81ea\u7c98\u6750\u6599\u7684\u5f00\u53d1\u53d6\u5f97\u4e86\u91cd\u5927\u8fdb\u5c55\uff0c\u4f46\u81ea\u4e3b\u81ea\u6108\u5408\u53ef\u62c9\u4f38\u7535\u6781\u53ca\u5176\u4e0e\u591a\u529f\u80fd\u7535\u5b50\u7cfb\u7edf\u7684\u96c6\u6210\u5c1a\u672a\u5b9e\u73b0\u3002\u8fd9\u4e3b\u8981\u662f\u7531\u4e8e\u8bbe\u5907\u5236\u9020\u65b9\u9762\u7684\u6311\u6218\u4ee5\u53ca\u7f3a\u4e4f\u5c06\u5404\u4e2a\u53ef\u81ea\u884c\u4fee\u590d\u7684\u7535\u5b50\u6a21\u5757\u5927\u89c4\u6a21\u96c6\u6210\u5230\u7cfb\u7edf\u4e2d\u3002<\/p>\n<p>\u6b64\u524d\uff0cDickey\u7b49\u4eba\u901a\u8fc7\u5370\u5237\u5728\u81ea\u4fee\u590d\u805a\u5408\u7269\u4e0a\u7684\u53ef\u91cd\u65b0\u914d\u7f6e\u7684\u6db2\u6001\u91d1\u5c5e\u7535\u6781\uff0c\u8bc1\u660e\u4e86\u81ea\u4fee\u590d\u6750\u6599\u7684\u4f18\u52bf\u3002\u9c8d\u54f2\u5357\u6559\u6388\u56e2\u961f\u4e4b\u524d\u62a5\u9053\u4e86\u7531\u6db2\u6001\u91d1\u5c5e\u548c\u575a\u97e7\uff0c\u53ef\u62c9\u4f38\u548c\u53ef\u81ea\u884c\u4fee\u590d\u7684\u805a\u5408\u7269\u5236\u6210\u7684\u53ef\u62c9\u4f38\u7684\u53ef\u81ea\u4fee\u590d\u7535\u5b50\u76ae\u80a4\u3002\u7136\u800c\uff0c\u5373\u4f7f\u6db2\u6001\u91d1\u5c5e\u4f5c\u4e3a\u4e92\u8fde\u7535\u6781\u5de5\u4f5c\u826f\u597d\uff0c\u5b83\u4e5f\u4e0d\u9002\u7528\u4e8e\u6709\u6e90\u7535\u5b50\u5143\u4ef6\u5982\u663e\u793a\u5668\u548c\u751f\u7406\u4f20\u611f\u5668\u7684\u7535\u6781\u3002\u53e6\u4e00\u65b9\u9762\uff0c\u4e00\u7ef4\uff081D\uff09\u91d1\u5c5e\u7eb3\u7c73\u7ebf\u548c\u78b3\u7eb3\u7c73\u7ba1\uff08CNT\uff09\u5df2\u7528\u4e8e\u81ea\u6108\u5408\u7535\u6781\u3002\u7531\u4e8e\u8fd9\u79cd\u7eb3\u7c73\u7ed3\u6784\u65e0\u6cd5\u6062\u590d\u5176\u539f\u59cb\u8fde\u63a5\u6027\uff0c\u5b83\u4eec\u5728\u6108\u5408\u540e\u672a\u88ab\u8bc1\u660e\u662f\u53ef\u62c9\u4f38\u7684\u3002\u5728\u8d85\u5206\u5b50\u5316\u5b66\u9886\u57df\uff0c\u5df2\u7ecf\u786e\u5b9a\u6eb6\u6db2\u4e2d\u7684\u81ea\u7ec4\u88c5\u7ed3\u6784\u53ef\u4ee5\u52a8\u6001\u5730\u201c\u91cd\u5efa\u201d\u4e3a\u70ed\u529b\u5b66\u7a33\u5b9a\u72b6\u6001\u3002\u6b64\u5916\uff0c\u52a8\u6001\u81ea\u6108\u8fc7\u7a0b\u53d7\u6eb6\u5242\u84b8\u6c14\u548c\u6e29\u5ea6\u7684\u5f71\u54cd\u5f88\u5927\u3002\u7136\u800c\uff0c\u8fd9\u79cd\u73b0\u8c61\u5c1a\u672a\u4e0e\u5b8f\u89c2\u53d8\u5316\u8054\u7cfb\u5728\u4e00\u8d77\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>2018\u5e748\u670820\u65e5\uff0c\u7f8e\u56fd<strong>\u65af\u5766\u798f\u5927\u5b66<\/strong>\u7684<strong>\u9c8d\u54f2\u5357\u6559\u6388<\/strong>\uff08\u901a\u8baf\u4f5c\u8005\uff09\u4e0e<strong>Donghee Son<\/strong><strong>\u3001<\/strong><strong>Jiheong Kang<\/strong>\u548c<strong>Orestis Vardoulis<\/strong>\uff08\u5171\u540c\u7b2c\u4e00\u4f5c\u8005\uff09\u5728\u56fd\u9645\u9876\u7ea7\u7efc\u5408\u6027\u671f\u520a<strong><em>Nat. Nanotech.<\/em><\/strong>\u4e0a\u53d1\u8868\u4e86\u6587\u7ae0\uff1a<strong>An integrated self-healable electronic skin system fabricated via dynamic reconstruction of a nanostructured conducting network<\/strong>\u3002\u672c\u6587\u62a5\u9053\u4e86\u80fd\u591f\u76d1\u89c6\u751f\u7406\u4fe1\u53f7\u5e76\u901a\u8fc7\u7528\u6237\u548c\u7535\u5b50\u8bbe\u5907\u4e4b\u95f4\u7684\u95ed\u73af\u901a\u4fe1\u663e\u793a\u53cd\u9988\u4fe1\u606f\u7684\u7535\u5b50\u76ae\u80a4\u8bbe\u5907\u5c06\u7528\u4e8e\u4e0b\u4e00\u4ee3\u53ef\u7a7f\u6234\u8bbe\u5907\u548c\u201c\u7269\u8054\u7f51\u201d\u3002\u8fd9\u79cd\u88c5\u7f6e\u9700\u8981\u8d85\u8584\u7684\u6784\u9020\u4ee5\u5b9e\u73b0\u4e0e\u4eba\u4f53\u7684\u65e0\u7f1d\u548c\u4fdd\u5f62\u63a5\u89e6\uff0c\u4ece\u800c\u9002\u5e94\u6765\u81ea\u91cd\u590d\u8fd0\u52a8\u7684\u5e94\u53d8\u5e76\u4e14\u4f69\u6234\u8212\u9002\u3002\u6700\u8fd1\uff0c\u81ea\u4fee\u590d\u5316\u5b66\u63a8\u52a8\u4e86\u53ef\u53d8\u5f62\u548c\u53ef\u91cd\u6784\u7535\u5b50\u5668\u4ef6\u7684\u8fdb\u6b65\uff0c\u7279\u522b\u662f\u53ef\u81ea\u4fee\u590d\u7684\u7535\u6781\u7cfb\u7edf\u3002\u5728\u4e4b\u524d\u7684\u7814\u7a76\u4e2d\uff0c\u4e0e\u5177\u6709\u81ea\u4fee\u590d\u52a8\u6001\u6027\u8d28\u7684\u805a\u5408\u7269\u57fa\u6750\u4e0d\u540c\uff0c\u906d\u5230\u7834\u574f\u7684\u5bfc\u7535\u7f51\u7edc\u5728\u635f\u574f\u540e\u4e0d\u80fd\u6062\u590d\u5176\u53ef\u62c9\u4f38\u6027\u3002\u5728\u8fd9\u91cc\uff0c\u672c\u6587\u62a5\u9053\u4e86\u5f53\u4e0e\u52a8\u6001\u4ea4\u8054\u7684\u805a\u5408\u7269\u7f51\u7edc\u63a5\u89e6\u65f6\u5bfc\u7535\u7eb3\u7c73\u7ed3\u6784\u7684\u81ea\u91cd\u5efa\u4e0e\u81ea\u4fee\u590d\u3002\u8fd9\u4e0e\u81ea\u4fee\u590d\u805a\u5408\u7269\u7684\u81ea\u7c98\u5408\u6027\u8d28\u76f8\u7ed3\u5408\uff0c\u5141\u8bb8\u968f\u540e\u7684\u4e92\u8fde\u3001\u4f20\u611f\u5668\u548c\u53d1\u5149\u88c5\u7f6e\u7684\u5f02\u6784\u591a\u7ec4\u4ef6\u88c5\u7f6e\u96c6\u6210\u5230\u5355\u4e2a\u591a\u529f\u80fd\u7cfb\u7edf\u4e2d\u3002\u8fd9\u4e00\u9996\u6b3e\u81ea\u4e3b\u81ea\u4fee\u590d\u548c\u53ef\u62c9\u4f38\u7684\u591a\u7ec4\u4ef6\u7535\u5b50\u76ae\u80a4\u4e3a\u672a\u6765\u5f3a\u5927\u7684\u7535\u5b50\u8bbe\u5907\u7684\u53d1\u5c55\u94fa\u5e73\u4e86\u9053\u8def\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u56fe<\/strong><strong>1. <\/strong><strong>\u5728\u575a\u97e7\u53ef\u62c9\u4f38\u7684\u81ea\u4fee\u590d\u805a\u5408\u7269\u57fa\u8d28\u4e2d\u52a8\u6001\u91cd\u5efa\u7684\u5bfc\u7535\u7eb3\u7c73\u7f51\u7edc\u7684\u793a\u610f\u56fe\u3002<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-151702\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/1600-3.png\" alt=\"\" width=\"600\" height=\"551\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/1600-3.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/1600-3-300x276.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>a. \u901a\u8fc7\u5c06CNT\u5bfc\u7535\u7f51\u7edc\u5d4c\u5165\u81ea\u4fee\u590d\u805a\u5408\u7269\u57fa\u8d28\u4e2d\u7684\u81ea\u5bc6\u5c01\u53ef\u62c9\u4f38\u7535\u6781\u7684\u5236\u9020\u8fc7\u7a0b\u7684\u793a\u610f\u56fe;<\/p>\n<p>b. \u4e0d\u540c\u7c7b\u578b\u57fa\u8d28\u7684\u987a\u5e8f\u793a\u610f\u56fe\u53ca\u5176\u5bf9\u635f\u4f24\u548c\u91cd\u5efa\u7684\u54cd\u5e94;<\/p>\n<p>c. \u5bf9\u5d4c\u5165\u81ea\u4fee\u590d\u805a\u5408\u7269\u57fa\u8d28\u4e2d\u7684CNT\u7684\u4e00\u79cd\u53ef\u80fd\u7684\u56de\u6536\u673a\u5236\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong>2.<\/strong> <strong>\u4e00\u7ef4\u5bfc\u7535\u7eb3\u7c73\u7f51\u7edc\u7684\u52a8\u6001\u91cd\u5efa\u3002<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-151703\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/2600-3.png\" alt=\"\" width=\"600\" height=\"369\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/2600-3.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/2600-3-300x185.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>a. \u4e0a\u56fe\uff1a\u663e\u793a\u4e86\u7ecf\u8fc720\u6b212N\u5207\u5272\u540eCNT\/PDMS-MPU<sub>4<\/sub>-IU<sub>0.6<\/sub>\u590d\u5408\u7535\u6781\u7684\u81ea\u6108\u6027\u80fd\uff1b\u4e0b\u56fe\uff1a\u53ef\u81ea\u4fee\u590d\u7684CNT\/PDMS-MPU<sub>0.4<\/sub>-IU<sub>0.6<\/sub>\u590d\u5408\u7535\u6781\u7684\u7535\u7279\u6027\u66f2\u7ebf\u968f\u65f6\u95f4\u7684\u53d8\u5316\uff0c\u540c\u65f6\u7ecf\u53d7\u4e0d\u540c\u673a\u68b0\u5f3a\u5ea6\uff080.5-4N\uff09\u7684\u635f\u574f\uff1b<\/p>\n<p>b. \u53ef\u81ea\u4fee\u590d\u7684CNT\/PDMS-MPU<sub>4<\/sub>-IU<sub>0.6<\/sub>\u590d\u5408\u7535\u6781\u81ea\u6108\u5408\uff0812\u5c0f\u65f6\uff09\u4e4b\u524d\u548c\u4e4b\u540e\u7684\u5149\u5b66\u663e\u5fae\u955c\u56fe\u50cf\u3002\u5373\u4f7f\u5728\u9ad8\u8fbe100\uff05\u7684\u5e94\u53d8\u62c9\u4f38\u540e\uff0c\u81ea\u6108\u7684CNT\u7f51\u7edc\u4e5f\u5f88\u7a33\u5065\uff08\u5e95\u90e8\u56fe\u50cf\uff09\uff1b<\/p>\n<p>c. \u81ea\u5bc6\u5c01CNT\/PDMS-MPU<sub>4<\/sub>-IU<sub>0.6<\/sub>\u590d\u5408\u7535\u6781\u7684\u7535\u963b\u4f5c\u4e3a\u5e94\u53d8\u7684\u51fd\u6570\uff0c\u57282N\u5207\u5272\u540e\u4e0d\u540c\u7684\u81ea\u6108\u65f6\u95f4\u7684\u7535\u963b\u503c\u53d8\u5316\u66f2\u7ebf\uff1b<\/p>\n<p>d. \u539f\u59cb\uff08\u7ea2\u8272\uff09\u548c\u81ea\u610812\u5c0f\u65f6\u540e\uff08\u84dd\u8272\uff09CNT\/PDMS-MPU<sub>4<\/sub>-IU<sub>0.6<\/sub>\u590d\u5408\u7535\u6781\u7684\u7535\u963b\u56fe\uff1b<\/p>\n<p>e. \u5207\u5272\u548c\u91cd\u65b0\u8fde\u63a5\u540eCNT\/PDMS-MPU<sub>4<\/sub>-IU<sub>0.6<\/sub>\uff08\u9876\u90e8\uff0c\u7ea2\u8272\uff09\u548cAgNW\/PDMS-MPU<sub>0.4<\/sub>-IU<sub>0.6<\/sub>\uff08\u5e95\u90e8\uff0c\u84dd\u8272\uff09\u91cd\u5efa\u7684\u5b9e\u65f6\u7535\u6c14\u76d1\u63a7\uff1b<\/p>\n<p>f. \u53ef\u81ea\u4fee\u590d\u7684CNT\/PDMS-MPU<sub>4<\/sub>-IU<sub>0.6<\/sub>\uff08\u9876\u90e8\uff0c\u7ea2\u8272\uff09\u548cAgNW\/PDMS-MPU<sub>0.4<\/sub>-IU<sub>0.6<\/sub>\uff08\u5e95\u90e8\uff0c\u84dd\u8272\uff09\u590d\u5408\u7535\u6781\u81ea\u6108\u540e\uff0812\u5c0f\u65f6\uff09\u7684\u626b\u63cf\u7535\u5b50\u663e\u5fae\u955c\uff08SEM\uff09\u56fe\u50cf\uff1b<\/p>\n<p>g. \u4e09\u79cd\u590d\u5408\u7535\u6781\uff08\u7ea2\u8272\uff0cCNT\/PDMS-MPU<sub>4<\/sub>-IU<sub>0.6<\/sub>;\u7eff\u8272\uff0cCNT\/SEBS;\u84dd\u8272\uff0cCNT\/PDMS\uff09\u7684\u5f52\u4e00\u5316\u7535\u963b\u53d8\u5316\u968f\u65f6\u95f4\u7684\u53d8\u5316\u3002\u6d4b\u91cf\u65f6\u5728\u6bcf\u4e2a\u7535\u6781\u7684\u8868\u9762\u4e0a\u8fdb\u884c\u5207\u5272\uff1b<\/p>\n<p>h. \u62c9\u4f38\u4e09\u79cd\u590d\u5408\u7535\u6781\u4e4b\u540e\u7528\u9ad8\u8fbe100\uff05\u7684\u62c9\u4f38\u5e94\u53d8\u7ef4\u6301\u57282\u5929\uff0c\u4e4b\u540e\u8fdb\u884c\u6d4b\u8bd5\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong>3. <\/strong><strong>\u5177\u6709\u81ea\u4e3b\u53ef\u4fee\u590d\u6027\u7684\u4e92\u8fde\u548c\u4f20\u611f\u5668\u3002<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-151704\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/3600-4.png\" alt=\"\" width=\"600\" height=\"548\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/3600-4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/3600-4-300x274.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>a. \u5177\u6709\u4e09\u79cd\u4e0d\u540c\u539a\u5ea6\u7684AgNW\u76f8\u5bf9\u7535\u963b\u968f\u62c9\u529b\u7684\u53d8\u5316\u56fe\uff08\u7ea2\u8272\uff0cAgNW 114nm;\u84dd\u8272\uff0c317nm;\u7eff\u8272\uff0c702nm\uff09\u3002\u63d2\u56fe\uff1a\u6bcf\u4e2a\u7535\u6781\u7684\u7167\u7247\uff1b<\/p>\n<p>b. \u9876\u90e8\uff0c\u5177\u6709\u4e0d\u540cAgNW\u539a\u5ea6\u7684\u6297\u635f\u4f24\u7535\u6781\u7684\u7535\u963b\u4e0e\u65f6\u95f4\u7684\u5173\u7cfb(\u540c\u8fdb\u884c\u4e09\u6b21\u8fde\u7eed\u5207\u5272\uff0c\u6bcf\u4e2a2N\uff09\u3002\u5e95\u90e8\uff0c\u4f4e\u963b\u8303\u56f4\u653e\u5927\u56fe\uff1b<\/p>\n<p>c. \u5728\u4eba\u5de5\u6c57\u6db2\u4e0b\uff0c\u81ea\u6108\u5408AgNW\/PDMS-MPU<sub>4<\/sub>-IU<sub>0.6<\/sub>\u590d\u5408\u7535\u6781\u7684\u8fde\u7eed\u81ea\u6108\u5408\u8fc7\u7a0b\u7684\u56fe\u50cf\uff08\u9876\u90e8\u6846\u67b6\uff09\u3002\u5728\u81ea\u4e3b\u6108\u5408\u8fc7\u7a0b\u4e4b\u540e\uff0c\u6108\u5408\u7684\u7535\u6781\u88ab\u62c9\u4f38\u81f3\u9ad8\u8fbe50\uff05\u7684\u5e94\u53d8\uff08\u5e95\u90e8\u6846\u67b6\uff09\uff1b<\/p>\n<p>d. \u4e0e\u805a\u9170\u4e9a\u80fa\u57fa\u677f\u4e0a\u7684\u5546\u7528\u53d1\u5149\u4e8c\u6781\u7ba1\uff08LED\uff09\u548c\u65e0\u6e90\u6a21\u5757\u8fde\u63a5\u7684\u53ef\u81ea\u4fee\u590d\u4e92\u8fde\u7684\u7167\u7247\uff08\u9876\u90e8\u548c\u5de6\u90e8\uff0c\u90e8\u5206\u5207\u5272;\u9876\u90e8\u548c\u53f3\u90e8\uff0c\u5b8c\u5168\u5207\u5272;\u5e95\u90e8\uff0c\u81ea\u6108\uff09\u3002\u81ea\u52a8\u6108\u5408\u7684\u7b2c\u4e00\u4e92\u8fde\u88ab\u5f88\u597d\u5730\u62c9\u4f38\u4ee5\u5411\u7b2c\u4e8cLED\u5355\u5143\uff08\u5e95\u90e8\uff09\u63d0\u4f9b\u7535\u529b\uff1b<\/p>\n<p>e. \u56fe\u50cf\u548c\u81ea\u6108\u5f0fECG\u4f20\u611f\u5668\u7684\u76f8\u5e94\u793a\u610f\u56fe\uff1b<\/p>\n<p>f. \u4ece\u53ef\u81ea\u4fee\u590d\u7684ECG\u4f20\u611f\u5668\uff08\u7ea2\u8272\uff09\u548c\u5546\u7528\u4f20\u611f\u5668\uff08\u9ed1\u8272\uff09\u6d4b\u91cf\u7684\u5fc3\u810f\u4fe1\u53f7\u3002\u84dd\u8272\u9634\u5f71\u90e8\u5206\u663e\u793a\u7535\u6781\u710a\u76d8\u5df2\u635f\u574f\uff0c\u968f\u540e\u5728\u51e0\u79d2\u949f\u5185\u6062\u590d\uff1b<\/p>\n<p>g. \u5e94\u53d8\u7075\u654f\u5ea6\u6bd4\u8f83\uff1b<\/p>\n<p>h. \u62c9\u4f38\u5faa\u73af\uff0830\uff05\u5e94\u53d8\uff09\u6d4b\u8bd5\uff1b<\/p>\n<p>i.\u5177\u6709\u51f9\u53e3\uff08\u5d4c\u5165\u7269\uff09\u7684\u5e94\u53d8\u4f20\u611f\u5668\uff0c\u7531\u4e8e\u805a\u5408\u7269\u57fa\u677f\u7684\u9ad8\u97e7\u6027\uff0c\u4ecd\u7136\u663e\u793a\u51fa\u826f\u597d\u7684\u53ef\u62c9\u4f38\u6027\u800c\u6ca1\u6709\u7535\u635f\u5931\uff0c\u8fd9\u80fd\u591f\u4f7f\u88c2\u7f1d\u4f20\u64ad\u6700\u5c0f\u5316\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong>4. <\/strong><strong>\u5177\u6709\u81ea\u4e3b\u53ef\u4fee\u590d\u6027\u7684\u9ad8\u5ea6\u53ef\u62c9\u4f38\u7684\u7535\u81f4\u53d1\u5149\u76ae\u80a4\u3002<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-151706\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/4600-4.png\" alt=\"\" width=\"600\" height=\"569\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/4600-4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/4600-4-300x285.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>a. \u539f\u59cb\u548c\u53ef\u81ea\u884c\u4fee\u590d\u7684LEC\u8bbe\u5907\u7684\u5e94\u53d8\u611f\u5e94\u80fd\u529b\u3002 \u63d2\u56fe\uff1a\u663e\u793a\u4e8c\u7b49\u5206\u548c\u81ea\u4e3b\u6108\u5408\u7535\u5bb9LEC\u8bbe\u5907\u7684\u56fe\u50cf;<\/p>\n<p>b. \u5e26\u51f9\u53e3\u7684LEC\u62c9\u4f38\u800c\u4e0d\u65ad\u88c2\u3002 \u56fe\u50cf\u663e\u793a\uff0c\u7531\u4e8e\u81ea\u4fee\u590d\u805a\u5408\u7269\u57fa\u8d28\u7684\u9ad8\u65ad\u88c2\u97e7\u6027\uff0c\u5728\u7f3a\u53e3\u5b58\u5728\u4e0b\u6ca1\u6709\u88c2\u7eb9\u6269\u5c55;<\/p>\n<p>c. \u6211\u4eec\u5e94\u7528200 V\u548c250 Hz a.c. \u7535\u573a\u4ee5CNT\u4e3a\u57fa\u7840\u7684LEC\uff0c\u540c\u65f6\u5c06\u5176\u62c9\u4f38\u81f3250\uff05\u62c9\u4f38\u5e94\u53d8\uff0c\u4ee5\u786e\u8ba4\u5176\u9ad8\u62c9\u4f38\u6027;<\/p>\n<p>d. \u5207\u5272\u548c\u81ea\u6108\uff08\u4e00\u5929\u540e\uff09\u53ef\u81ea\u884c\u4fee\u590d\u7684\u57fa\u4e8eCNT\u7684LEC\u8bbe\u5907\u7684\u7167\u7247;<\/p>\n<p>e. \u7ecf\u8fc7\u4e00\u5929\u540e\uff0c\u81ea\u6108CNT\uff08e\uff09\u663e\u793a\u51fa\u53ef\u9760\u7684\u62c9\u4f38\u6027\uff0c\u540c\u65f6\u63d0\u4f9b\u7a33\u5b9a\u7684\u5149;<\/p>\n<p>f. \u7ecf\u8fc7\u4e00\u5929\u540e\uff0c\u81ea\u6108AgNWLEC\u88c5\u7f6e\u663e\u793a\u51fa\u53ef\u9760\u7684\u62c9\u4f38\u6027\u540c\u65f6\u63d0\u4f9b\u7a33\u5b9a\u7684\u5149;<\/p>\n<p>g. \u5728\u6c34\u4e0b\u6d78\u6e0d\/\u62c9\u4f38\u5faa\u73af\u540e\u7528\u81ea\u4fee\u590d\u805a\u5408\u7269\u5c42\u5c01\u88c5\u7684AgNW LEC\u7684\u56fe\u50cf;<\/p>\n<p>h. \u539f\u59cbLEC\u88c5\u7f6e\u5728\u6c34\u4e0b\u7684\u56fe\u50cf;<\/p>\n<p>i. \u62c9\u4f38LEC\u88c5\u7f6e\u5728\u6c34\u4e0b\u7684\u56fe\u50cf\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong>5. <\/strong><strong>\u96c6\u6210\u7684\u53ef\u81ea\u4fee\u7535\u5b50\u76ae\u80a4\u7cfb\u7edf\u7684\u793a\u610f\u56fe\u548c\u76f8\u5e94\u56fe\u50cf\u3002<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-151705\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/560.png\" alt=\"\" width=\"600\" height=\"457\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/560.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/560-300x229.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>a. \u591a\u529f\u80fd\u53ef\u81ea\u4fee\u590d\u7684\u7535\u5b50\u76ae\u80a4\u7cfb\u7edf\u7684\u793a\u610f\u56fe\uff0c\u5305\u62ec\u5177\u6709\u7535\u5bb9\u7ed3\u6784\u7684\u5e94\u53d8\u4f20\u611f\u5668\uff08\u9876\u90e8\u4e2d\u5fc3\u548c\u5de6\u4fa7\u63d2\u56fe\u663e\u793a\u5c42\u4fe1\u606f;\u7ea2\u8272\u7bad\u5934\u8868\u793a\u6bcf\u4e2a\u7535\u6781\u7ec4\u88c5\u5728\u6240\u9700\u8868\u9762\u4e0a\uff09\uff0cECG\u4f20\u611f\u5668\uff08\u5e95\u90e8\u4e2d\u5fc3\uff09\u5de6\u4fa7\u63d2\u56fe\u663e\u793a\u5176\u7ec4\u88c5\u8fc7\u7a0b\uff09\u548cLEC\u9635\u5217\uff08\u53f3\u4fa7\u548c\u5e95\u90e8\u63d2\u56fe\u8868\u793a\u5176\u901a\u8fc7\u6c22\u952e\u9a71\u52a8\u7684\u8f7b\u4fbf\u7ec4\u4ef6\u5236\u9020\uff09;<\/p>\n<p>b. \u76ae\u80a4\u4e0a\u7684\u591a\u529f\u80fd\u81ea\u6108\u7535\u5b50\u76ae\u80a4\u88c5\u7f6e\uff0c\u540c\u65f6\u8fdb\u884cLEC\u64cd\u4f5c\uff0c\u53d1\u51fa\u84dd\u7eff\u8272\u5149\u3002\u63d2\u56fe\uff1a\u521a\u6027\u57fa\u677f\u4e0a\u7684\u7535\u5b50\u76ae\u80a4\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong>6. <\/strong><strong>\u96c6\u6210\u7684\u81ea\u4fee\u590d\u7535\u5b50\u76ae\u80a4\u7cfb\u7edf\u3002<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-151707\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/6600-2.png\" alt=\"\" width=\"600\" height=\"590\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/6600-2.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/6600-2-300x295.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>a. \u7cfb\u7edf\u6982\u8ff0\uff0c\u4f20\u611f\u5668\u5c06\u503c\u65e0\u7ebf\u4f20\u9001\u5230\u663e\u793a\u5668\uff1b<\/p>\n<p>b. \u7531\u81ea\u6108\u88c5\u7f6e\u6d4b\u91cf\u7684\u4ee5500Hz\u91c7\u6837\u7684ECG\u6ce2\u5f62;<\/p>\n<p>c. \u81ea\u68c0LEC\u5fc3\u5f62\u50cf\u7d20\uff0c\u5f53\u68c0\u6d4b\u5230\u5fc3\u8df3\u65f6\u95ea\u70c1;<\/p>\n<p>d. \u5fc3\u7387\u7531\u53ef\u81ea\u6211\u4fee\u590d\u7684ECG\u4f20\u611f\u5668\u76d1\u6d4b;<\/p>\n<p>e. \u5e94\u53d8\u4f20\u611f\u5668\u5bf930\uff05\u62c9\u4f38\u8f7d\u8377\u548c\u5378\u8f7d\u7684\u54cd\u5e94;<\/p>\n<p>f. \u53ef\u81ea\u884c\u4fee\u590d\u7684LEC\u6761\u5f62\u50cf\u7d20\u6839\u636e\u5fc3\u7387\u503c\u6253\u5f00\u548c\u5173\u95ed\u3002<\/p>\n<p><strong>\u3010\u5c0f\u7ed3\u3011<\/strong><\/p>\n<p>\u9c8d\u54f2\u5357\u6559\u6388\u56e2\u961f\u8bc1\u660e\u4e86\u5bfc\u75351D\u7eb3\u7c73\u7ed3\u6784\u7f51\u7edc\u5728\u4e0e\u52a8\u6001\u8d85\u5206\u5b50\u4ea4\u8054\u805a\u5408\u7269\u7f51\u7edc\u63a5\u89e6\u65f6\u53ef\u4ee5\u91cd\u5efa\u5e76\u91cd\u65b0\u83b7\u5f97\u5bfc\u7535\u6027\u548c\u673a\u68b0\u6027\u80fd\u3002\u4e0e\u5176\u4ed6\u81ea\u4fee\u590d\u7535\u6781\u76f8\u6bd4\uff0c\u672c\u7814\u7a76\u4e2d\u7684\u7eb3\u7c73\u6750\u6599\/\u805a\u5408\u7269\u590d\u5408\u7535\u6781\u975e\u5e38\u6709\u4f18\u52bf\uff0c\u539f\u56e0\u5982\u4e0b\uff1a\uff081\uff09\u5b83\u4eec\u53ef\u7528\u4f5c\u5668\u4ef6\u4e2d\u7684\u6709\u6e90\u5143\u4ef6\uff08\u5305\u62ec\u4e92\u8fde\uff09;\uff082\uff09\u5373\u4f7f\u5728\u635f\u574f\u540e\uff0c\u5b83\u4eec\u4e5f\u5177\u6709\u5f88\u9ad8\u7684\u62c9\u4f38\u6027;\uff083\uff09\u5b83\u4eec\u53ef\u4ee5\u81ea\u4fee\u590d\uff0c\u5177\u6709\u5f88\u5f3a\u7684\u8010\u53d7\u6027;\uff084\uff09\u5b83\u4eec\u5728\u5ba4\u6e29\u4e0b\u8868\u73b0\u51fa\u81ea\u4e3b\u7684\u81ea\u4fee\u590d\u6027\u3002\u51ed\u501f\u8fd9\u4e9b\u7279\u6027\uff0c\u7814\u7a76\u8005\u4eec\u5236\u9020\u4e86\u4e00\u4e2a\u5168\u96c6\u6210\u7684\u7535\u5b50\/\u5149\u7535\u591a\u529f\u80fd\u81ea\u6108\u7535\u5b50\u7cfb\u7edf\uff0c\u5177\u6709\u4eba\u7c7b\u76ae\u80a4\u822c\u7684\u5185\u5728\u62c9\u4f38\u6027\u548c\u81ea\u6211\u6062\u590d\u80fd\u529b\uff0c\u800c\u8fd9\u4e00\u5207\u57fa\u4e8e\u7b80\u5355\u7684\u81ea\u7c98\u5408\u88c5\u914d\u5de5\u827a\u3002\u5728\u81ea\u4fee\u590d\u7684\u673a\u8f7d\u7cfb\u7edf\u4e2d\uff0c\u9ad8\u6027\u80fd\u4e92\u8fde\u7684ECG\/\u5e94\u53d8\u4f20\u611f\u5668\u548cLEC\u5355\u5143\u73b0\u5728\u53ef\u4ee5\u901a\u8fc7\u5229\u7528\u81ea\u4fee\u590d\u805a\u5408\u7269\u7684\u81ea\u7c98\u7279\u6027\u65e0\u7f1d\u96c6\u6210\u5230\u5355\u4e2a\u5e73\u53f0\u4e2d\uff0c\u4f7f\u5176\u9ad8\u5ea6\u9002\u7528\u4e8e\u5148\u8fdb\u7684\u673a\u5668\u4eba\u6216\u5047\u80a2\u7535\u5b50\u76ae\u80a4\u3002\u6b64\u5916\uff0c\u6bcf\u4e2a\u4f20\u611f\u5668\u8bb0\u5f55\u7684\u751f\u7406\u6570\u636e\u53ef\u4ee5\u65e0\u7ebf\u4f20\u8f93\u5230LEC\u9635\u5217\uff0c\u4ee5\u5b9e\u65f6\u63d0\u4f9b\u8fde\u7eed\u76d1\u6d4b\u3002\u9c8d\u54f2\u5357\u6559\u6388\u56e2\u961f\u7684\u7cfb\u7edf\u7ea7\u591a\u529f\u80fd\u53ef\u81ea\u4fee\u590d\u7535\u5b50\u76ae\u80a4\u4e3a\u53d1\u5c55\u5f3a\u5065\uff0c\u751a\u81f3\u7262\u4e0d\u53ef\u7834\u7684\u672a\u6765\u7535\u5b50\u4ea7\u54c1\u8d21\u732e\u51fa\u4e86\u4e00\u4efd\u529b\u91cf\u3002<\/p>\n<p><strong>\u6587\u7ae0\u94fe\u63a5\uff1a<\/strong><a href=\"https:\/\/doi.org\/10.1038\/s41565-018-0244-6\"><strong>An integrated self-healable electronic skin system fabricated via dynamic reconstruction of a nanostructured conducting network.<\/strong><\/a> (<strong><em>Nat. Nanotech.<\/em><\/strong><em>,<\/em> DOI: 10.1038\/s41565-018-0244-6)<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u7eb3\u7c73\u6750\u6599\u5b66\u672f\u7ec4\u827e\u8d8a\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u6a21\u4eff\u4eba\u7c7b\u76ae\u80a4\u7684\u67d4\u8f6f\u4e14\u53ef\u53d8\u5f62\u7684\u7535\u5b50\u5668\u4ef6\u9002\u7528\u4e8e\u4e0b\u4e00\u4ee3\u53ef\u7a7f\u6234\u7535\u4ea7\u54c1\uff0c\u5047\u80a2\u4eba\u9020\u76ae\u80a4\u548c\u57fa\u4e8e\u9ad8\u6027\u80fd\u6750\u6599\u7684\u690d\u5165\u5f0f\u533b\u7597\u8bbe\u5907\u7b49\u9886\u57df\uff0c\u5177\u6709\u5de8\u5927\u7684\u5b9e\u7528\u4ef7\u503c\u5e76\u5c06\u6df1\u6df1\u5730\u6539\u53d8\u4eba\u4eec&#8230;<\/p>\n","protected":false},"author":9703,"featured_media":151707,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[3532,2677,2754,2854,3533],"class_list":["post-151699","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","tag-3532","tag-2677","tag-2754","tag-2854","tag-3533"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/151699"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/9703"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=151699"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/151699\/revisions"}],"predecessor-version":[{"id":151743,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/151699\/revisions\/151743"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/151707"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=151699"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=151699"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=151699"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}