{"id":151877,"date":"2018-08-27T06:30:06","date_gmt":"2018-08-26T22:30:06","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=151877"},"modified":"2018-08-24T21:45:53","modified_gmt":"2018-08-24T13:45:53","slug":"%e3%80%90%e6%8a%95%e7%a8%bf%e3%80%91%e6%96%b0%e5%8a%a0%e5%9d%a1%e5%9b%bd%e7%ab%8b%e5%a4%a7%e5%ad%a6%e8%b0%a2%e5%bb%ba%e5%b9%b3adv-mater-%e7%bb%bc%e8%bf%b0-%e5%9c%a8%e5%8e%9f%e5%ad%90%e5%b1%82","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=151877","title":{"rendered":"\u65b0\u52a0\u5761\u56fd\u7acb\u5927\u5b66\u8c22\u5efa\u5e73Adv. Mater.\u7efc\u8ff0-\u5728\u539f\u5b50\u5c42\u9762\u4e0a\u8c03\u63a7\u529f\u80fd\u5316\u91d1\u5c5e\u6750\u6599"},"content":{"rendered":"<p><strong><b>\u3010\u5f15\u8a00\u3011<\/b><\/strong><\/p>\n<p>\u4eba\u7c7b\u5236\u4f5c\u548c\u52a0\u5de5\u6750\u6599\u7684\u7cbe\u7ec6\u5ea6\u5f80\u5f80\u627f\u8f7d\u7740\u4eba\u7c7b\u6587\u660e\u548c\u5386\u53f2\u53d1\u5c55\u7684\u4e0d\u540c\u9636\u6bb5\u7684\u70d9\u5370\u3002\u800c\u5728\u8fd9\u4e9b\u529f\u80fd\u5316\u6750\u6599\u4e2d\uff0c\u91d1\u5c5e\u6750\u6599\u5360\u636e\u7740\u4e3e\u8db3\u8f7b\u91cd\u7684\u5730\u4f4d\u3002\u968f\u7740\u8fd1\u6570\u5341\u5e74\u6765\u79d1\u6280\u65e5\u65b0\u6708\u5f02\u7684\u9614\u6b65\u594b\u8fdb\uff0c\u529f\u80fd\u5316\u91d1\u5c5e\u6750\u6599\u7684\u53d1\u5c55\u6b63\u5728\u6b65\u5165\u4e00\u4e2a\u5168\u65b0\u7684\u65f6\u4ee3\uff0c\u5728\u6b64\uff0c\u4eba\u4eec\u7684\u7ec8\u6781\u76ee\u6807\u662f\u5bf9\u529f\u80fd\u5316\u91d1\u5c5e\u6750\u6599\u5b9e\u73b0\u201c\u539f\u5b50\u5230\u539f\u5b50\u201d\u7684\u7cbe\u51c6\u5b9a\u5236\u3002\u6000\u63e3\u7740\u8fd9\u4e00\u7ec8\u6781\u76ee\u6807\uff0c\u79d1\u6280\u5de5\u4f5c\u8005\u4eec\u9996\u5148\u503e\u6ce8\u4e86\u5927\u91cf\u7684\u5fc3\u8840\u5728\u7eb3\u7c73\u5c3a\u5ea6\u4e0a\u5b9e\u73b0\u5bf9\u91d1\u5c5e\u7eb3\u7c73\u6750\u6599\uff08\u542b\u6709\u7ea61000\u4e2a\u6216\u66f4\u591a\u91d1\u5c5e\u539f\u5b50\uff09\u7684\u7ed3\u6784\u548c\u76f8\u5173\u6027\u8d28\u7684\u7cbe\u51c6\u8c03\u63a7\u3002\u4e00\u7cfb\u5217\u5c3a\u5bf8\uff0c\u5f62\u8c8c\uff0c\u7ed3\u6676\u5ea6\u4ee5\u53ca\u7ed3\u6784\u5c42\u7ea7\u53ef\u63a7\u7684\u529f\u80fd\u5316\u91d1\u5c5e\u7eb3\u7c73\u6750\u6599\u5df2\u7ecf\u88ab\u6210\u529f\u7684\u5408\u6210\u51fa\u6765\u5e76\u5728\u50ac\u5316\uff0c\u80fd\u6e90\uff0c\u751f\u7269\u533b\u836f\u4ee5\u53ca\u73af\u5883\u7b49\u5e94\u7528\u9886\u57df\u5d2d\u9732\u5934\u89d2\u3002\u5c06\u7c7b\u4f3c\u7684\u7cbe\u786e\u8c03\u63a7\u5316\u5b66\u8fdb\u4e00\u6b65\u62d3\u5c55\u5230\u5206\u5b50\u751a\u81f3\u539f\u5b50\u5c42\u9762\u662f\u76ee\u524d\u91d1\u5c5e\u6750\u6599\u7814\u7a76\u7684\u70ed\u95e8\u8bdd\u9898\u3002\u56e0\u4e3a\u8fd9\u4e00\u201c\u539f\u5b50\u5230\u539f\u5b50\u201d\u7684\u7cbe\u51c6\u8c03\u63a7\u80fd\u529b\u4e0d\u4ec5\u53ef\u4ee5\u6781\u5927\u63d0\u9ad8\u529f\u80fd\u5316\u91d1\u5c5e\u7eb3\u7c73\u6750\u6599\u7684\u539f\u5b50\u6548\u7387\uff0c\u800c\u4e14\u53ef\u4ee5\u4e3a\u5efa\u7acb\u91d1\u5c5e\u6750\u6599\u7684\u7ed3\u6784-\u6027\u8d28\u5173\u7cfb\u63d0\u4f9b\u575a\u5b9e\u7684\u57fa\u7840\u3002\u7136\u800c\uff0c\u6570\u5341\u5e74\u4e43\u81f3\u4e0a\u767e\u5e74\u7684\u5408\u6210\u5b9e\u8df5\u8868\u660e\u5728\u539f\u5b50\u5c42\u9762\u4e0a\u5b9e\u73b0\u5bf9\u91d1\u5c5e\u7eb3\u7c73\u6750\u6599\u7684\u7cbe\u51c6\u8c03\u63a7\u5e76\u975e\u6613\u4e8b\uff1a\u5728\u4f20\u7edf\u91d1\u5c5e\u7eb3\u7c73\u9897\u7c92\uff08Nanoparticle, &gt;\u00a03 nm\uff09\u4f53\u7cfb\u5185\u96be\u4ee5\u5b9e\u73b0\u7cbe\u786e\u5230\u539f\u5b50\u7684\u5408\u6210\u548c\u4fee\u9970\u3002<\/p>\n<p>\u8fd1\u4e8c\u5341\u4f59\u5e74\u6765\u786b\u9187\u4fdd\u62a4\u7684\u91d1\u5c5e\u7eb3\u7c73\u56e2\u7c07\uff08Nanocluster, NC\uff09\u7684\u8fc5\u901f\u5d1b\u8d77\u4e3a\u5728\u539f\u5b50\u5c42\u9762\u4e0a\u5b9e\u73b0\u91d1\u5c5e\u6750\u6599\u7684\u7cbe\u51c6\u8c03\u63a7\u63d0\u4f9b\u4e86\u7406\u60f3\u7684\u7814\u7a76\u5e73\u53f0\u3002\u786b\u9187\u4fdd\u62a4\u7684\u91d1\u5c5eNC\u662f\u4e00\u7c7b\u5c3a\u5bf8\u8d85\u5c0f\uff08&lt; 3 nm\uff09\u7684\u7eb3\u7c73\u9897\u7c92\u3002\u5f97\u76ca\u4e8e\u5176\u65e5\u81fb\u6210\u719f\u7684\u7cbe\u786e\u5230\u539f\u5b50\u7684\u5408\u6210\uff08\u901a\u8fc7\u5316\u5b66\u624b\u6bb5\u7b49\uff09\u548c\u8868\u5f81\uff08\u901a\u8fc7\u5148\u8fdb\u7684\u8d28\u8c31\u548cX-\u5c04\u7ebf\u6280\u672f\u7b49\uff09\u624b\u6bb5\uff0c\u786b\u9187\u4fdd\u62a4\u7684\u91d1\u5c5eNC\u901a\u5e38\u53ef\u4ee5\u7528\u7c7b\u4f3c\u4e8e\u5206\u5b50\u7684\u201c\u5206\u5b50\u5f0f\u201d\u8868\u793a\uff1a\u5982[M<em><sub><i>n<\/i><\/sub><\/em>(SR)<em><sub><i>m<\/i><\/sub><\/em>]<em><sup><i>q<\/i><\/sup><\/em>, \u5176\u4e2d<em><i>n<\/i><\/em>, <em><i>m<\/i><\/em>\u00a0\u548c<em><i>q<\/i><\/em>\u5206\u522b\u8868\u793a\u5355\u4e2a\u56e2\u7c07\u4e2d\u91d1\u5c5e\u539f\u5b50\uff08M\uff09\uff0c\u786b\u9187\u914d\u4f53\uff08SR\uff09\u4ee5\u53ca\u51c0\u7535\u8377\u7684\u6570\u76ee\u3002\u57fa\u4e8e\u5728\u6b64\u8d85\u5c0f\u5c3a\u5ea6\u4e0b\u7684\u5f3a\u91cf\u5b50\u9650\u57df\u6548\u5e94\u4ee5\u53ca\u72ec\u7279\u7684\u91d1\u5c5e-\u786b\u9187\u952e\uff08M-SR\uff09\uff0c\u91d1\u5c5eNC\u5448\u73b0\u51fa\u65b0\u9896\u7684\u7c7b\u5206\u5b50\u6027\u8d28\uff08\u5982HOMO-LUMO\u8dc3\u8fc1\uff0c\u91cf\u5b50\u5316\u7535\u8377\u884c\u4e3a\uff0c\u672c\u5f81\u65cb\u5149\u6027\uff0c\u5f3a\u8367\u5149\uff0c\u4ee5\u53ca\u4f18\u5f02\u7684\u50ac\u5316\u6d3b\u6027\u548c\u9009\u62e9\u6027\u7b49\uff09\uff0c\u4f7f\u5176\u5728\u50ac\u5316\uff0c\u751f\u7269\u533b\u836f\u548c\u6e05\u6d01\u80fd\u6e90\u7b49\u9886\u57df\u5177\u6709\u5e7f\u6cdb\u7684\u5e94\u7528\u524d\u666f\u3002\u9664\u6b64\u4e4b\u5916\uff0c\u4e0a\u8ff0\u7c7b\u5206\u5b50\u6027\u8d28\u8fd8\u8868\u73b0\u51fa\u5f3a\u70c8\u7684\u5c3a\u5bf8\/\u7ed3\u6784\u76f8\u5173\u6027\uff0c\u4e3a\u5728\u539f\u5b50\u5c3a\u5ea6\u4e0a\u76d1\u6d4b\u91d1\u5c5e\u7eb3\u7c73\u56e2\u7c07\u7684\u5c3a\u5bf8\u548c\u7ed3\u6784\u6f14\u5316\u8fc7\u7a0b\u63d0\u4f9b\u4e86\u4fbf\u6377\u7684\u624b\u6bb5\u3002<\/p>\n<p><strong><b>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/b><\/strong><\/p>\n<p>\u9274\u4e8e\u6b64\uff0c<strong><b>\u65b0\u52a0\u5761\u56fd\u7acb\u5927\u5b66\u8c22\u5efa\u5e73\u6559\u6388\u8bfe\u9898\u7ec4<\/b><\/strong>\u548c<strong><b>\u9752\u5c9b\u79d1\u6280\u5927\u5b66\u8881\u52cb\u6559\u6388\u8bfe\u9898\u7ec4<\/b><\/strong>\u4e8e\u8fd1\u671f\u5728Advanced\u00a0Materials\u4e0a\u53d1\u8868\u9898\u4e3a \u201cEngineering Functional Metal Materials at the Atomic Level\u201d\u7684\u53d7\u9080\u7814\u7a76\u8fdb\u5c55\u62a5\u544a\uff08Progress\u00a0Report\uff09\u3002\u8be5\u62a5\u544a\u63d0\u51fa\u786b\u9187\u4fdd\u62a4\u7684\u91d1\u5c5eNC\u5177\u6709\u7c7b\u4f3c\u4e8e\u5929\u7136\u86cb\u767d\u8d28\u7684\u591a\u7ea7\u7ed3\u6784\u7279\u5f81\uff0c\u5e76\u57fa\u4e8e\u6b64\u591a\u7ea7\u7ed3\u6784\u7279\u5f81\uff0c\u7cfb\u7edf\u603b\u7ed3\u4e86\u5728\u539f\u5b50\u7cbe\u5ea6\u4e0a\u8c03\u63a7\u91d1\u5c5eNC\u7684\u5c3a\u5bf8\u4ee5\u53ca\u7ed3\u6784\u7279\u8d28\u7684\u7b56\u7565\u3002\u4f17\u6240\u5468\u77e5\uff0c\u5929\u7136\u86cb\u767d\u8d28\u5206\u5b50\u5177\u6709\u591a\u7ea7\u7ed3\u6784\u7279\u5f81\uff1a\u4e00\u7ea7\u7ed3\u6784\uff08Primary\u00a0Structure\uff09\u63cf\u8ff0\u7684\u662f\u591a\u80bd\u94fe\u7684\u6c28\u57fa\u9178\u5e8f\u5217\uff0c\u4e8c\u7ea7\u7ed3\u6784\uff08Secondary\u00a0Structure\uff09\u8868\u8ff0\u7684\u662f\u591a\u80bd\u94fe\u7684\u533a\u57df\u7ed3\u6784\u57fa\u5143\uff08\u5982\u03b1\u87ba\u65cb\u548c\u03b2\u6298\u53e0\u7b49\uff09\uff0c\u4e09\u7ea7\u7ed3\u6784\uff08Tertiary\u00a0Structure\uff09\u5219\u662f\u7531\u4e8c\u7ea7\u7ed3\u6784\u5806\u53e0\u800c\u6210\u7684\u591a\u80bd\u5206\u5b50\u7684\u4e09\u7ef4\u7ed3\u6784\u3002\u7c7b\u4f3c\u7684\uff08\u89c1\u56fe1\uff09\uff0c\u786b\u9187\u4fdd\u62a4\u7684\u91d1\u5c5eNC\u7684\u4e00\u7ea7\u7ed3\u6784\u63cf\u8ff0\u7684\u662f\u5176\u7ec4\u5206\u91d1\u5c5e\u539f\u5b50\u548c\u786b\u9187\u914d\u4f53\u7684\u79cd\u7c7b\uff0c\u4e8c\u7ea7\u7ed3\u6784\u8868\u8ff0\u7684\u662f\u7531\u8fd9\u4e9b\u91d1\u5c5e\u539f\u5b50\u548c\u786b\u9187\u914d\u4f53\u7ec4\u6210\u7684\u57fa\u672c\u7ed3\u6784\u57fa\u5143\uff08\u5982\u591a\u9762\u4f53\u91d1\u5c5e\u6838\u4ee5\u53ca\u91d1\u5c5e-\u786b\u9187\u8868\u9762\u4fdd\u62a4\u6a21\u4f53\uff08Surface\u00a0Protecting\u00a0Motif\uff09\u7b49\uff09\uff0c\u800c\u4e09\u7ea7\u7ed3\u6784\u5219\u662f\u8fd9\u4e9b\u7ed3\u6784\u57fa\u5143\u7684\u7a7a\u95f4\u5806\u79ef\u65b9\u5f0f\u3002\u57fa\u4e8e\u6b64\u591a\u7ea7\u7ed3\u6784\u6a21\u578b\uff0c\u8be5\u62a5\u544a\u8be6\u7ec6\u603b\u7ed3\u4e86\u901a\u8fc7\u91d1\u5c5e-\u786b\u9187\uff08M(I)-SR\uff09\u914d\u5408\u7269\u7684\u8fd8\u539f\u751f\u957f\uff08\u56fe1\u4e2d\u7a7a\u5fc3\u5706\u6240\u793a\uff09\u6216\u8005\u9884\u5f62\u6210\u7684\u91d1\u5c5eNC\u7684\u8f6c\u5316\u53cd\u5e94\uff08\u56fe1\u4e2d\u5b9e\u5fc3\u5706\u6240\u793a\uff09\u5bf9\u56e2\u7c07\u7684\u5c3a\u5bf8\u548c\u5404\u7ea7\u7ed3\u6784\u7684\u7cbe\u51c6\u8c03\u63a7\u7b56\u7565\u3002\u9700\u8981\u7279\u522b\u6307\u51fa\u7684\u662f\uff0c\u8be5\u62a5\u544a\u7740\u91cd\u4ecb\u7ecd\u4e86\u8fd9\u4e9b\u7cbe\u51c6\u8c03\u63a7\u7b56\u7565\u80cc\u540e\u7684\u5316\u5b66\u539f\u7406\u548c\u53cd\u5e94\u673a\u7406\uff0c\u4ee5\u671f\u4e3a\u5c06\u6765\u7684\u57fa\u7840\u548c\u65b9\u6cd5\u8bba\u7814\u7a76\u63d0\u4f9b\u6709\u6548\u7684\u53c2\u8003\u548c\u6307\u5bfc\u3002\u5f97\u76ca\u4e8e\u4ee5\u4e0a\u603b\u7ed3\u7684\u4e00\u7cfb\u5217\u7cbe\u51c6\u8c03\u63a7\u7b56\u7565\uff0c\u91d1\u5c5eNC\u8fd8\u5728\u4e0d\u540c\u7ed3\u6784\u5c42\u7ea7\u4e0a\u8868\u73b0\u51fa\u4e86\u7279\u5f02\u7684\u6750\u6599\u6027\u80fd\u3002\u4f5c\u4e3a\u8fd9\u4e9b\u7279\u5f02\u6750\u6599\u6027\u80fd\u7684\u4ee3\u8868\uff0c\u91d1\u5c5eNC\u6e90\u4e8e\u4e0d\u540c\u7ed3\u6784\u5c42\u7ea7\u7684\u50ac\u5316\u548c\u751f\u7269\u533b\u836f\u6027\u80fd\u4e5f\u5728\u8be5\u62a5\u544a\u4e2d\u5f97\u5230\u4e86\u6df1\u5165\u8ba8\u8bba\u3002<\/p>\n<p>\uff08\u4ee5\u4e0b\u56fe\u7247\u6765\u81ea\u4f5c\u8005\uff0c\u66f4\u591a\u56fe\u6587\u53c2\u89c1\u539f\u6587\u732e\uff09<\/p>\n<p><strong><b>\u56fe1. \u786b\u9187\u4fdd\u62a4\u7684\u91d1\u5c5e\u7eb3\u7c73\u56e2\u7c07\u7684\u591a\u7ea7\u7ed3\u6784\u4ee5\u53ca\u9488\u5bf9\u5404\u7ea7\u7ed3\u6784\u7684\u7cbe\u51c6\u8c03\u63a7\u7b56\u7565\u793a\u610f\u56fe\u3002\u4ee5[<\/b><\/strong><strong><b>Au<\/b><\/strong><strong><sub><b>25<\/b><\/sub><\/strong><strong><b>(S(CH<\/b><\/strong><strong><sub><b>2<\/b><\/sub><\/strong><strong><b>)<\/b><\/strong><strong><sub><b>2<\/b><\/sub><\/strong><strong><b>Ph)<\/b><\/strong><strong><sub><b>18<\/b><\/sub><\/strong><strong><b>]<\/b><\/strong><strong><sup><b>&#8211;<\/b><\/sup><\/strong><strong><b>\u7ed3\u6784\u4e3a\u4f8b\u3002<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-151879 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/1-41.png\" alt=\"\" width=\"600\" height=\"426\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/1-41.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/1-41-300x213.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u56fe2. <\/b><\/strong><strong><b>M(I)-SR<\/b><\/strong><strong><b>\u914d\u5408\u7269\u8fd8\u539f\u751f\u957f\u6cd5\u7cbe\u51c6\u5408\u6210\u91d1\u5c5e\u7eb3\u7c73\u56e2\u7c07\u7684\u673a\u7406\u793a\u610f\u56fe\u53ca\u751f\u957f\u8fc7\u7a0b\u8d28\u8c31\u8ddf\u8e2a\u56fe\u3002<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-151880 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/2-39.png\" alt=\"\" width=\"600\" height=\"442\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/2-39.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/2-39-300x221.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u00a0<\/b><\/strong>\uff08a\uff09\u751f\u957f\u673a\u7406\u793a\u610f\u56fe\uff1b<\/p>\n<p>\uff08b\uff09\u8fd8\u539f\u751f\u957f\u6cd5\u5236\u5907[Au<sub>25<\/sub>(SR)<sub>18<\/sub>]<sup>&#8211;<\/sup>\u7684\u56e2\u7c07\u751f\u957f\u8fc7\u7a0b\u7535\u55b7\u96fe\u7535\u79bb\u8d28\u8c31\u8ddf\u8e2a\u56fe\u3002<\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>3<\/b><\/strong><strong><b>.<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><strong><b>\u901a\u8fc7NaOH\u534f\u52a9\u7684NaBH<\/b><\/strong><strong><sub><b>4<\/b><\/sub><\/strong><strong><b>\u8fd8\u539f\u6cd5\u5236\u5907\u4e0d\u540c\u786b\u9187\u914d\u4f53\u4fdd\u62a4\u7684[<\/b><\/strong><strong><b>Au<\/b><\/strong><strong><sub><b>25<\/b><\/sub><\/strong><strong><b>(SR)<\/b><\/strong><strong><sub><b>18<\/b><\/sub><\/strong><strong><b>]<\/b><\/strong><strong><sup><b>&#8211;<\/b><\/sup><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-151881 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/3-40.png\" alt=\"\" width=\"600\" height=\"610\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/3-40.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/3-40-295x300.png 295w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u00a0<\/b><\/strong>\uff08a\uff09\u5408\u6210\u65b9\u6cd5\u793a\u610f\u56fe\uff1b<\/p>\n<p>\uff08b,c\uff09\u4ea7\u54c1\u7684\u7d2b\u5916-\u53ef\u89c1\u5149\u8c31\uff08b\uff09\u548c\u7535\u55b7\u96fe\u7535\u79bb\u8d28\u8c31\uff08c\uff09\u56fe\u3002<\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>4<\/b><\/strong><strong><b>. <\/b><\/strong><strong><b>[Au<\/b><\/strong><strong><sub><b>38<\/b><\/sub><\/strong><strong><b>(SR)<\/b><\/strong><strong><sub><b>24<\/b><\/sub><\/strong><strong><b>]<\/b><\/strong><strong><sup><b>0<\/b><\/sup><\/strong><strong><b>\u7684\u4e24\u4e2a\u7ed3\u6784\u5f02\u6784\u4f53\uff1aAu<\/b><\/strong><strong><sub><b>38Q<\/b><\/sub><\/strong><strong><b>\u548cAu<\/b><\/strong><strong><sub><b>38<\/b><\/sub><\/strong><strong><sub><b>T<\/b><\/sub><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-151882 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/4-32.png\" alt=\"\" width=\"600\" height=\"493\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/4-32.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/4-32-300x247.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08a,b\uff09Au<sub>38<\/sub><sub>Q<\/sub>\uff08a\uff09\u548cAu<sub>38<\/sub><sub>T<\/sub>\uff08b\uff09\u7684Au<sub>23<\/sub>\u6838\uff0cAu(I)-SR\u4fdd\u62a4\u6a21\u4f53\u4ee5\u53ca\u5b8c\u6574\u7ed3\u6784\u793a\u610f\u56fe\u3002<\/p>\n<p>\uff08c\uff09Au<sub>38T<\/sub>\uff08\u84dd\u7ebf\uff09\u548cAu<sub>38Q<\/sub>\uff08\u9ed1\u7ebf\uff09\u7684\u7d2b\u5916-\u53ef\u89c1\u5149\u8c31\u4ee5\u53ca\u8584\u5c42\u8272\u8c31\u8868\u5f81\u7ed3\u679c\u3002<\/p>\n<p><strong><b>\u56fe5<\/b><\/strong><strong><b>.<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><strong><b>[Au<\/b><\/strong><strong><sub><b>38<\/b><\/sub><\/strong><strong><b>(SR)<\/b><\/strong><strong><sub><b>24<\/b><\/sub><\/strong><strong><b>]<\/b><\/strong><strong><sup><b>0<\/b><\/sup><\/strong><strong><b>\uff08Au<\/b><\/strong><strong><sub><b>38Q<\/b><\/sub><\/strong><strong><b>\uff09\u7684\u4e00\u5bf9\u65cb\u5149\u5f02\u6784\u4f53<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-151883 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/5-24.png\" alt=\"\" width=\"600\" height=\"658\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/5-24.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/5-24-274x300.png 274w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08a\uff09\u6cbf<em><i>C<\/i><\/em><em><sub><i>3<\/i><\/sub><\/em>\u8f74\u89c6\u89d2\uff1b<\/p>\n<p>\uff08b\uff09\u5782\u76f4\u4e8e<em><i>C<\/i><\/em><em><sub><i>3<\/i><\/sub><\/em>\u8f74\u89c6\u89d2\uff1bSR-[Au(I)-SR]<sub>2<\/sub>\u4fdd\u62a4\u6a21\u4f53\u5747\u7528\u84dd\u8272\u9ad8\u4eae\u663e\u793a\u3002<\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>6.<\/b><\/strong><strong><b>\u57fa\u4e8e\u56e2\u7c07\u8f6c\u5316\u53cd\u5e94\u7684\u56e2\u7c07\u5c3a\u5bf8\uff0c\u4e00\u7ea7\uff0c\u4e8c\u7ea7\u548c\u4e09\u7ea7\u7ed3\u6784\u7684\u7cbe\u51c6\u8c03\u63a7\u7b56\u7565\u793a\u610f\u56fe<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-151884 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/6-16.png\" alt=\"\" width=\"600\" height=\"556\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/6-16.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/6-16-300x278.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u56fe7<\/b><\/strong><strong><b>.<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><strong><b>\u79cd\u5b50\u751f\u957f\u6cd5\u4ece[<\/b><\/strong><strong><b>Au<\/b><\/strong><strong><sub><b>25<\/b><\/sub><\/strong><strong><b>(SR)<\/b><\/strong><strong><sub><b>18<\/b><\/sub><\/strong><strong><b>]<\/b><\/strong><strong><sup><b>&#8211;<\/b><\/sup><\/strong><strong><b>\u5236\u5907[<\/b><\/strong><strong><b>Au<\/b><\/strong><strong><sub><b>44<\/b><\/sub><\/strong><strong><b>(SR)<\/b><\/strong><strong><sub><b>26<\/b><\/sub><\/strong><strong><b>]<\/b><\/strong><strong><sup><b>2-<\/b><\/sup><\/strong><strong><b>\u793a\u610f\u56fe\u53ca\u751f\u957f\u8fc7\u7a0b\u8d28\u8c31\u8ddf\u8e2a\u56fe<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-151885 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/7-12.png\" alt=\"\" width=\"600\" height=\"895\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/7-12.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/7-12-201x300.png 201w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08a\uff09\u79cd\u5b50\u751f\u957f\u6cd5\u793a\u610f\u56fe\uff1b<\/p>\n<p>\uff08b\uff09\u79cd\u5b50\u751f\u957f\u6cd5\u5236\u5907[Au<sub>44<\/sub>(SR)<sub>26<\/sub>]<sup>2-<\/sup>\u7684\u56e2\u7c07\u751f\u957f\u8fc7\u7a0b\u7535\u55b7\u96fe\u7535\u79bb\u8d28\u8c31\u8ddf\u8e2a\u56fe\u3002<\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>8<\/b><\/strong><strong><b>.<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><strong><b>[<\/b><\/strong><strong><b>Au<\/b><\/strong><strong><sub><b>25<\/b><\/sub><\/strong><strong><b>(SR)<\/b><\/strong><strong><sub><b>18<\/b><\/sub><\/strong><strong><b>]<\/b><\/strong><strong><sup><b>&#8211;<\/b><\/sup><\/strong><strong><b>\u50ac\u53164-\u785d\u57fa\u82ef\u915a\u52a0\u6c22\u53cd\u5e94\u793a\u610f\u56fe<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-151886 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/8-7.png\" alt=\"\" width=\"600\" height=\"819\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/8-7.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/8-7-220x300.png 220w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08a\uff094-\u785d\u57fa\u82ef\u915a\u52a0\u6c22\u53cd\u5e94\u8def\u5f84\u793a\u610f\u56fe\uff1b<\/p>\n<p>\uff08b\uff09[Au<sub>25<\/sub>(SR)<sub>18<\/sub>]<sup>&#8211;<\/sup>\u50ac\u5316\u6d3b\u6027\u4f4d\u70b9\u793a\u610f\u56fe\u3002<\/p>\n<p><strong><b>\u3010\u5c0f\u7ed3\u3011<\/b><\/strong><\/p>\n<p>\u603b\u800c\u8a00\u4e4b\uff0c\u5728\u8fc7\u53bb\u7684\u4e8c\u5341\u4f59\u5e74\u91cc\uff0c\u5bf9\u529f\u80fd\u5316\u91d1\u5c5e\u6750\u6599\u7684\u201c\u539f\u5b50\u5230\u539f\u5b50\u201d\u5b9a\u5236\u7814\u7a76\u53d6\u5f97\u4e86\u957f\u8db3\u7684\u8fdb\u6b65\uff0c\u5b9e\u73b0\u4e86\u5bf9\u786b\u9187\u4fdd\u62a4\u7684\u91d1\u5c5eNC\u7684\u5c3a\u5bf8\uff0c\u4e00\u7ea7\uff0c\u4e8c\u7ea7\u548c\u4e09\u7ea7\u7ed3\u6784\u7684\u7cbe\u786e\u5230\u539f\u5b50\u7684\u8c03\u63a7\u3002\u4e3b\u8981\u7684\u8c03\u63a7\u7b56\u7565\u5305\u62ec\u5728\u8fd8\u539f\u751f\u957f\u6cd5\u4e2d\u8c03\u63a7\u8fd8\u539f\u53cd\u5e94\u52a8\u529b\u5b66\u548c\u5c3a\u5bf8\u805a\u7126\u53cd\u5e94\uff08Size-Focusing\uff09\u70ed\u529b\u5b66\uff1b\u4ee5\u53ca\u5728\u56e2\u7c07\u8f6c\u5316\u53cd\u5e94\u4e2d\u5f15\u5165\u5fc5\u8981\u7684\u70ed\u5904\u7406\uff0c\u5916\u6e90\u91d1\u5c5e\u79bb\u5b50\uff0c\u786b\u9187\u914d\u4f53\uff0cM(I)-SR\u4fdd\u62a4\u6a21\u4f53\uff0c\u6c27\u5316\u8fd8\u539f\u5242\u548c\u91d1\u5c5eNC\u3002\u503c\u5f97\u6307\u51fa\u7684\u662f\uff0c\u76f8\u8f83\u4e8e\u56e2\u7c07\u7684\u5c3a\u5bf8\u548c\u4e00\u7ea7\u7ed3\u6784\uff0c\u56e2\u7c07\u4e8c\u7ea7\u7ed3\u6784\uff08\u7ed3\u6784\u5f02\u6784\u4f53\uff09\u548c\u4e09\u7ea7\u7ed3\u6784\uff08\u65cb\u5149\u5f02\u6784\u4f53\uff09\u7684\u8c03\u63a7\u7814\u7a76\u8d77\u6b65\u8f83\u665a\uff0c\u6545\u6025\u9700\u5b66\u672f\u754c\u7684\u66f4\u591a\u5173\u6ce8\u3002\u9664\u4e86\u5728\u56e2\u7c07\u5185\u5bf9\u56e2\u7c07\u7684\u4e00\u7ea7\uff0c\u4e8c\u7ea7\u548c\u4e09\u7ea7\u7ed3\u6784\u8fdb\u884c\u8c03\u63a7\u5916\uff0c\u53e6\u5916\u4e00\u4e2a\u540c\u7b49\u91cd\u8981\u7684\u7814\u7a76\u65b9\u5411\u662f\u5728\u56e2\u7c07\u95f4\u5bf9\u56e2\u7c07\u7684\u56db\u7ea7\u7ed3\u6784\uff08Quaternary Structure\uff0c\u5373\u5176\u81ea\u7ec4\u88c5\u7ed3\u6784\uff0c\u5bf9\u5e94\u4e8e\u5929\u7136\u86cb\u767d\u8d28\u5206\u5b50\u95f4\u7684\u7a7a\u95f4\u6392\u5217\uff09\u8fdb\u884c\u7cbe\u51c6\u8c03\u63a7\u3002\u6b64\u5916\uff0c\u57fa\u4e8e\u91d1\u5c5eNC\u7684\u7c7b\u86cb\u767d\u8d28\u7684\u591a\u7ea7\u7ed3\u6784\u7684\u5e94\u7528\u7814\u7a76\u5c1a\u5904\u4e8e\u8d77\u6b65\u9636\u6bb5\uff0c\u540c\u6837\u9700\u8981\u5b66\u672f\u754c\u503e\u6ce8\u66f4\u591a\u52aa\u529b\u3002<\/p>\n<p><strong><b>\u81f4\u8c22\uff1a<\/b><\/strong>\u4e0a\u8ff0\u76f8\u5173\u7814\u7a76\u5f97\u5230\u4e86\u65b0\u52a0\u5761\u6559\u80b2\u90e8(Grant No. R-279-000-481-112\uff1bR-279-000-538-114)\u7684\u8d44\u52a9\u3002<\/p>\n<p><strong><b>\u6587\u732e\u94fe\u63a5\uff1a<\/b><\/strong><\/p>\n<p>Yao, Q.; Yuan, X.; Chen, T.; Xie, J. Engineering Functional Metal Materials at the Atomic Level. Adv.\u00a0Mater. <strong><b>2018<\/b><\/strong>, <em><i>30<\/i><\/em>, 1802751.<\/p>\n<p>\u672c\u6587\u7531\u65b0\u52a0\u5761\u56fd\u7acb\u5927\u5b66\u7684\u8c22\u5efa\u5e73\u6559\u6388\u8bfe\u9898\u7ec4\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c<strong><b>\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com<\/b><\/strong>\u3002<\/p>\n<p>\u6750\u6599\u4eba\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1a<strong><b>cailiaokefu<\/b><\/strong>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u4eba\u7c7b\u5236\u4f5c\u548c\u52a0\u5de5\u6750\u6599\u7684\u7cbe\u7ec6\u5ea6\u5f80\u5f80\u627f\u8f7d\u7740\u4eba\u7c7b\u6587\u660e\u548c\u5386\u53f2\u53d1\u5c55\u7684\u4e0d\u540c\u9636\u6bb5\u7684\u70d9\u5370\u3002\u800c\u5728\u8fd9\u4e9b\u529f\u80fd\u5316\u6750\u6599\u4e2d\uff0c\u91d1\u5c5e\u6750\u6599\u5360\u636e\u7740\u4e3e\u8db3\u8f7b\u91cd\u7684\u5730\u4f4d\u3002\u968f\u7740\u8fd1\u6570\u5341\u5e74\u6765\u79d1\u6280\u65e5\u65b0\u6708\u5f02&#8230;<\/p>\n","protected":false},"author":9133,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-151877","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/151877"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/9133"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=151877"}],"version-history":[{"count":6,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/151877\/revisions"}],"predecessor-version":[{"id":151909,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/151877\/revisions\/151909"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=151877"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=151877"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=151877"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}