{"id":157335,"date":"2018-10-27T06:30:15","date_gmt":"2018-10-26T22:30:15","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=157335"},"modified":"2018-10-28T23:40:39","modified_gmt":"2018-10-28T15:40:39","slug":"%e3%80%8anano-letters%e3%80%8b%e6%8a%a5%e9%81%93%e7%94%b5%e5%ad%90%e5%ad%a6%e9%99%a2%e4%bd%99%e6%9e%97%e8%94%9a%e6%95%99%e6%8e%88%e8%af%be%e9%a2%98%e7%bb%84%e5%8a%a8%e6%80%81%e8%b7%b3%e8%b7%83","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=157335","title":{"rendered":"\u300aNano Letters\u300b\u62a5\u9053\u7535\u5b50\u5b66\u9662\u4f59\u6797\u851a\u6559\u6388\u8bfe\u9898\u7ec4\u52a8\u6001\u8df3\u8dc3\u6db2\u6ef4\u8bf1\u5bfc\u751f\u957f\u5f02\u8d28\u9517\u7845\u8d85\u6676\u683c\u5c9b\u94fe\u7eb3\u7c73\u7ebf\u7ed3\u6784\u6700\u65b0\u8fdb\u5c55"},"content":{"rendered":"<p><strong>\u00a0\u3010\u524d\u8a00\u3011<\/strong><\/p>\n<p>\u901a\u8fc7\u4eba\u5de5\u7ec4\u5206\u8c03\u63a7\u548c\u8bbe\u8ba1\uff0c\u5b9e\u73b0\u5f02\u8d28\u9517\u7845\u8d85\u6676\u683c\u7ed3\u6784\u662f\u63a2\u7d22\u65b0\u4e00\u4ee3\u5149\u7535\u5668\u4ef6\u5e94\u7528\u7684\u57fa\u7840\u3002\u800c\u5728\u51c6\u4e00\u7ef4\u7684\u7eb3\u7c73\u7ebf\u6c9f\u9053\u4e2d\uff0c\u80fd\u540c\u65f6\u53e0\u52a0\u7ec4\u5206\uff08Compositional\uff09\u548c\u5f62\u8c8c\uff08Geometric\uff09\u53d8\u5316\u5bf9\u80fd\u5e26\u7684\u8c03\u63a7\u80fd\u529b\uff0c\u6709\u671b\u5efa\u7acb\u66f4\u4e3a\u9ad8\u6548\u7684\u7269\u6027\u8c03\u63a7\u65b0\u6280\u672f\u548c\u65b0\u601d\u8def\u3002\u4f20\u7edf\u9517\u7845\u5f02\u8d28\uff08\u8f74\u5411\uff09\u8d85\u6676\u683c\u7eb3\u7c73\u7ebf\u5236\u5907\u4f9d\u8d56\u4e8e\u4ea4\u66ff\u6c14\u6c1b\u4f9b\u7ed9\u7684VLS\u751f\u957f\u6a21\u5f0f\uff0c\u7531\u4e8e\u80cc\u666f\u73af\u5883\u4e2d\u7684\u7ec4\u5206\u5207\u6362\u8fdf\u6ede\uff08reservoir\uff09\u6548\u5e94\uff0c\u96be\u4ee5\u83b7\u5f97\u975e\u5e38\u201c\u9510\u5229\u201d\u7684\u7ec4\u5206\u8c03\u63a7\u3002\u6bcf\u4e2a\u7ec4\u5206\u5468\u671f\u81f3\u5c11\u9700\u8981\u4e24\u6b21\u751f\u957f\u73af\u5883\u5207\u53d8\uff08switching\uff09\u548c\u6e05\u6d17\uff08purging\uff09\u8fc7\u7a0b\uff0c\u6545\u800c\u751f\u957f\u5236\u5907\u6210\u672c\u9ad8\u4e14\u975e\u5e38\u7f13\u6162\u3002\u6b64\u5916\uff0c\u7ad6\u76f4\u751f\u957f\u8d85\u6676\u683c\u7eb3\u7c73\u7ebf\u96be\u4ee5\u5b9e\u73b0\u89c4\u6a21\u5b9a\u4f4d\u96c6\u6210\uff0c\u8fd9\u4e5f\u4e3a\u5e73\u9762\u5de5\u827a\u5e94\u7528\u5e26\u6765\u5de8\u5927\u56f0\u96be\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u5357\u4eac\u5927\u5b66\u7535\u5b50\u79d1\u5b66\u4e0e\u5de5\u7a0b\u5b66\u9662\u4f59\u6797\u851a\u6559\u6388\u8bfe\u9898\u7ec4\uff0c\u9996\u6b21\u63d0\u51fa\u5e76\u5c1d\u8bd5\u4e86\u4e00\u79cd\u5168\u65b0\u7684\u601d\u8def\uff1a\u5c06\u9517\u7845\u7eb3\u7c73\u7ebf\u7ec4\u5206\u8c03\u63a7\u7684\u5207\u6362\u4efb\u52a1\uff0c\u4ea4\u4ed8\u7ed9\u5728\u5e73\u9762\u4e0a\u6eda\u52a8\u524d\u8fdb\u7684\u7eb3\u7c73\u91d1\u5c5e\u6db2\u6ef4\u6765\u5b8c\u6210\u3002\u4f8b\u5982\uff0c\u5229\u7528\u4f4e\u7194\u70b9\u91d1\u5c5e\u94df\u4f5c\u4e3a\u50ac\u5316\u9897\u7c92\uff0c\u4ee5\u975e\u6676a-Si\/a-Ge\u53e0\u5c42\u4f5c\u4e3a\u524d\u9a71\u4f53\uff0c\u94df\u9897\u7c92\u5728\u5e73\u9762\u8fd0\u52a8\u4e2d\u5728\u524d\u7aef\u5438\u6536\u975e\u6676\u5c42\u5e76\u5728\u540e\u7aef\u6dc0\u79ef\u51fa\u6676\u6001\u7684\u7eb3\u7c73\u7ebf\u7ed3\u6784\u3002\u5f53\u6db2\u6ef4\u8fd0\u52a8\u901f\u5ea6\u8db3\u591f\u9ad8\u7684\u65f6\u5019\uff0c\u7531\u4e8e\u672c\u8eab\u201c\u6eda\u52a8\u201d\u5bfc\u81f4\u7684\u5185\u90e8\u8f93\u8fd0\u6da1\u65cb\u4f5c\u7528\uff0c\u53ef\u81ea\u53d1\u5730\u8c03\u5236\u5bf9\u5e95\u5c42a-Si\/a-Ge\u53e0\u5c42\u7684\u5438\u6536\u6df1\u5ea6\uff0c\u5728\u5e73\u9762\u201c\u52a8\u6001\u8df3\u8dc3\u201d\u8fc7\u7a0b\u4e2d\uff0c\u5b9e\u73b0\u5468\u671f\u6027\u3001\u5f62\u8c8c\u548c\u7ec4\u5206\u540c\u6b65\u8c03\u5236\u7684\u5d4c\u5957\u5f02\u8d28\u9517-\u7845\u8d85\u6676\u683c\u5c9b\u94fe\u7eb3\u7c73\u7ebf\uff08Ge\/Si hetero island-chain\u00a0nanowires, hiNWs\uff09\u7ed3\u6784\u3002\u5b9e\u9a8c\u53d1\u73b0\uff0c\u5176\u5f02\u8d28\u9517\u7845\u7eb3\u7c73\u7ebf\u7ed3\u6784\u7684\u7ec4\u5206\u3001\u5468\u671f\u548c\u76f4\u5f84\u7b49\u5173\u952e\u53c2\u6570\u5747\u53ef\u901a\u8fc7\u975e\u6676\u53e0\u5c42\u8bbe\u8ba1\u548c\u6db2\u6ef4\u5927\u5c0f\u63a7\u5236\u6709\u6548\u8c03\u8282\u3002\u5176\u4e2dGe\u6210\u5206\u5728Ge\/Si\u5f02\u8d28\u754c\u9762\u4e0a\u53ef\u5728\u51e0\u4e2a\u7eb3\u7c73\u5185\u5b8c\u621075%Ge\u7684\u81ea\u53d1\u8f6c\u53d8\uff0c\u4e0d\u9700\u8981\u4efb\u4f55\u5916\u754c\u4eba\u5de5\u8c03\u63a7\u5e72\u9884\u3002\u540c\u65f6\uff0c\u9517\u7845\u8d85\u6676\u683c\u7eb3\u7c73\u7ebf\u53ef\u4ee5\u88ab\u7cbe\u786e\u5b9a\u4f4d\u5728\u6307\u5b9a\u533a\u57df\uff0c\u4e3a\u540e\u7eed\u7535\u5b66\u63a5\u89e6\u548c\u5668\u4ef6\u63a2\u7d22\u5e26\u6765\u5de8\u5927\u65b9\u4fbf\u3002\u6b64\u9879\u7814\u7a76\u4e3a\u63a2\u7d22\u65b0\u578b\u7eb3\u7c73\u6db2\u6ef4\u52a8\u6001\u7269\u6027\u8c03\u63a7\u624b\u6bb5\uff0c\u5b9e\u73b0\u9ad8\u6548\u5149\u7535\u529f\u80fd\u7ed3\u6784\u548c\u5668\u4ef6\u5e94\u7528\u5960\u5b9a\u4e86\u5173\u952e\u57fa\u7840\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p>\u56fe1.\u00a0\u52a8\u6001\u8df3\u8dc3\u6db2\u6ef4\u8bf1\u5bfc\u751f\u957f\u5f02\u8d28\u9517-\u7845\u8d85\u6676\u683c\u5c9b\u94fe\u7eb3\u7c73\u7ebf\u7ed3\u6784\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-157353 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/10\/\u56fe\u724720.png\" alt=\"\" width=\"650\" height=\"313\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/10\/\u56fe\u724720.png 650w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/10\/\u56fe\u724720-300x144.png 300w\" sizes=\"(max-width: 650px) 100vw, 650px\" \/><\/p>\n<p>\u672c\u9879\u7814\u7a76\u6210\u679c\u8bba\u6587\u8fd1\u671f\u53d1\u8868\u5728\u300a<strong><b>Nano<\/b><\/strong><strong><b>\u00a0Letters<\/b><\/strong>\u300b\u4e0a\uff0cNanodroplet Hydrodynamic Transformation of Uniform Amorphous Bilayer into Highly Modulated Ge\/Si Island-Chains, Nano Letters, DOI: 10.1021\/acs.nanolett.8b02847 (2018)\u3002\u8bba\u6587\u7b2c\u4e00\u4f5c\u8005\u4e3a\u535a\u58eb\u751f\u8d75\u8000\u9f99\u540c\u5b66\uff0c\u901a\u8baf\u4f5c\u8005\u662f\u5357\u4eac\u5927\u5b66\u4f59\u6797\u851a\u6559\u6388\u3002\u76f8\u5173\u5de5\u4f5c\u5f97\u5230\u4e86\u7535\u5b50\u79d1\u5b66\u4e0e\u5de5\u7a0b\u5b66\u9662\u7684\u5f90\u9a8f\u6559\u6388\u3001\u65bd\u6bc5\u6559\u6388\u4ee5\u53ca\u6cd5\u56fd\u5df4\u9ece\u7efc\u5408\u7406\u5de5Pere Roca i Cabarrocas\u6559\u6388\u7684\u5927\u529b\u652f\u6301\u3002\u8be5\u9879\u7814\u7a76\u5de5\u4f5c\u53d7\u5230\u201c\u9752\u5e74\u5343\u4eba\u8ba1\u5212\u201d\uff0c\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\uff0c\u6c5f\u82cf\u7701\u6770\u51fa\u9752\u5e74\u57fa\u91d1\u548c\u201c\u53cc\u521b\u4eba\u624d\u201d\u8ba1\u5212\u7684\u8d44\u52a9\u3002<\/p>\n<p>\u76f8\u5173\u6587\u7ae0\u94fe\u63a5\uff1a<a href=\"https:\/\/pubs.acs.org\/doi\/10.1021\/acs.nanolett.8b02847\"><u>https:\/\/pubs.acs.org\/doi\/10.1021\/acs.nanolett.8b02847<\/u><\/a>\u00a0\u00a0<\/p>\n<p><strong>\u4eba\u7269\u7b80\u4ecb\uff1a<\/strong><\/p>\n<p>\u4f59\u6797\u851a \u535a\u58eb\/\u6559\u6388<\/p>\n<p>1997\u5e74\u8fdb\u5165\u5357\u4eac\u5927\u5b66\u7269\u7406\u7cfb\uff0c\u83b7\u534a\u5bfc\u4f53\u4e13\u4e1a\u5b66\u58eb\u5b66\u4f4d\uff1b2001-02\u5e74\u53c2\u52a0\u56e2\u4e2d\u592e\u7b2c\u4e09\u5c4a\u7814\u7a76\u751f\u9752\u5e74\u5fd7\u613f\u8005\u652f\u6559\u56e2\uff08\u5b81\u590f\u9686\u5fb7\u53bf\u8054\u624d\u4e61\u4e2d\u5b66\u6559\u5e08\uff09\uff1b2002\u5e74\u8fd4\u56de\u5357\u4eac\u5927\u5b66\u653b\u8bfb\u56fa\u4f53\u7535\u5b50\u4e0e\u5fae\u7535\u5b50\u5b66\uff0c\u83b7\u5de5\u5b66\u535a\u58eb\u5b66\u4f4d\uff1b2007\u5e74\u8d74\u6cd5\u56fd\u5df4\u9ece\u7efc\u5408\u7406\u5de5\u754c\u9762\u4e0e\u8584\u819c\u7269\u7406\u5b9e\u9a8c\u5ba4\uff08LPICM\uff09\u5f00\u5c55\u535a\u58eb\u540e\u7814\u7a76\u5de5\u4f5c\uff1b2009\u5e74\u5165\u804c\u6cd5\u56fd\u56fd\u5bb6\u79d1\u5b66\u7814\u7a76\u4e2d\u5fc3(CNRS)\uff0c\u7ec8\u8eab\u804c\u4f4d\u7814\u7a76\u5458\uff08CR2\uff09\uff1b2013\u5e74\u81f3\u4eca\uff0c\u5165\u9009\u4e2d\u7ec4\u90e8\u9752\u5e74\u5343\u4eba\u8ba1\u5212\u52a0\u5165\u5357\u4eac\u5927\u5b66\u7535\u5b50\u79d1\u5b66\u4e0e\u5de5\u7a0b\u5b66\u9662\u3002 \u73b0\u4efb\u5357\u4eac\u5927\u5b66\u6559\u6388\uff0c\u535a\u58eb\u751f\u5bfc\u5e08\uff0c\u56fd\u5bb6\u201c\u9752\u5e74\u5343\u4eba\u8ba1\u5212\u201d\uff0c\u6c5f\u82cf\u7701\u53cc\u521b\u8ba1\u5212\u53ca\u6c5f\u82cf\u7701\u6770\u51fa\u9752\u5e74\u57fa\u91d1\uff0c\u62c5\u4efb\u300a\u534a\u5bfc\u4f53\u5b66\u62a5\u300b\u7f16\u59d4\u4f1a\u59d4\u5458\u3002\u4e3b\u8981\u7814\u7a76\u65b9\u5411\u5305\u62ec\uff1a1)\u00a0\u7845\u57fa\u7eb3\u7c73\u7ed3\u6784\u751f\u957f\u673a\u7406\u548c\u7269\u6027\u8c03\u63a7\uff1b2)\u00a0\u67d4\u6027\u53ef\u62c9\u4f38\u6676\u7845\u7535\u5b50\u548c\u4f20\u611f\u5e94\u7528\uff1b3)\u00a0\u5f84\u5411\u7ed3\u592a\u9633\u80fd\u7535\u6c60\u548c\u80fd\u6e90\u5e94\u7528\u3002\u5728\u7eb3\u7c73\u7ebf\u751f\u957f\u63a7\u5236\u9886\u57df\u7684\u4e00\u7cfb\u5217\u539f\u521b\u6027\u5de5\u4f5c\u591a\u6b21\u88ab\u5b66\u672f\u65b0\u95fb\u5a92\u4f53Nature Materials Highlights\uff0cSPIE Newsroom, APS Physics Focus\u548cPhys.org\u62a5\u9053\u3002\u76f8\u5173\u5de5\u4f5c\u5df2\u53d1\u8868\u5b66\u672f\u8bba\u6587100\u4f59\u7bc7\uff0c\u5176\u4e2d\u4ee5\u7b2c\u4e00\u6216\u901a\u8baf\u4f5c\u8005\u5728Phys.Rev.Lett.\/B, Nature Commun.,\u00a0Nano Lett., Adv. Mater., Adv.\u00a0Funct.\u00a0Mater., Nano Energ.\uff0cAppl. Phys. Lett.\u7b49\u56fd\u9645\u671f\u520a\u4e0a\u53d1\u8868\u8bba\u658750\u4f59\u7bc7\u3002\u627f\u62c5\u548c\u53c2\u4e0e\u591a\u9879973\u91cd\u5927\u7814\u7a76\u3001\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u548c\u6c5f\u82cf\u7701\u79d1\u6280\u652f\u6491\u91cd\u70b9\u7814\u53d1\u8ba1\u5212\u7b49\u3002\u7533\u8bf7\u548c\u83b7\u5f97\u56fd\u9645PCT\u53d1\u660e\u6388\u6743\u4e13\u52292\u9879\u548c\u56fd\u5185\u53d1\u660e\u4e13\u52297\u9879\uff0c\u7533\u8bf7\u53d7\u7406\u56fd\u9645\u548c\u56fd\u5185\u4e13\u522912\u9879\u3002<\/p>\n<p>\u672c\u6587\u7531\u5357\u4eac\u5927\u5b66\u4f59\u6797\u851a\u8bfe\u9898\u7ec4\u4f9b\u7a3f\uff0c\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u7f16\u8f91\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com.<\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaorenvip.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u00a0\u3010\u524d\u8a00\u3011 \u901a\u8fc7\u4eba\u5de5\u7ec4\u5206\u8c03\u63a7\u548c\u8bbe\u8ba1\uff0c\u5b9e\u73b0\u5f02\u8d28\u9517\u7845\u8d85\u6676\u683c\u7ed3\u6784\u662f\u63a2\u7d22\u65b0\u4e00\u4ee3\u5149\u7535\u5668\u4ef6\u5e94\u7528\u7684\u57fa\u7840\u3002\u800c\u5728\u51c6\u4e00\u7ef4\u7684\u7eb3\u7c73\u7ebf\u6c9f\u9053\u4e2d\uff0c\u80fd\u540c\u65f6\u53e0\u52a0\u7ec4\u5206\uff08Compositional\uff09&#8230;<\/p>\n","protected":false},"author":10213,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-157335","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/157335"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/10213"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=157335"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/157335\/revisions"}],"predecessor-version":[{"id":157509,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/157335\/revisions\/157509"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=157335"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=157335"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=157335"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}