{"id":160414,"date":"2018-11-29T06:30:33","date_gmt":"2018-11-28T22:30:33","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=160414"},"modified":"2018-11-29T12:17:37","modified_gmt":"2018-11-29T04:17:37","slug":"%e8%8a%9d%e5%8a%a0%e5%93%a5%e5%a4%a7%e5%ad%a6%e7%94%b0%e5%8d%9a%e4%b9%8bnat-rev-mater-%e7%bb%bc%e8%bf%b0-%ef%bc%9a%e6%97%a0%e6%9c%ba%e5%8d%8a%e5%af%bc%e4%bd%93%e6%9d%90%e6%96%99%e7%94%9f%e7%89%a9","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=160414","title":{"rendered":"\u829d\u52a0\u54e5\u5927\u5b66\u7530\u535a\u4e4bNat. Rev. Mater.\u7efc\u8ff0 \uff1a\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u751f\u7269\u754c\u9762"},"content":{"rendered":"<p><strong>\u3010\u524d\u8a00\u3011<\/strong><\/p>\n<p>\u968f\u7740\u534a\u5bfc\u4f53\u5de5\u4e1a\u7684\u84ec\u52c3\u53d1\u5c55\uff0c\u4eba\u4eec\u5173\u4e8e\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u7269\u7406\u5316\u5b66\u6027\u8d28\u7684\u77e5\u8bc6\u5df2\u7ecf\u76f8\u5f53\u4e30\u5bcc\uff0c\u4e5f\u56e0\u6b64\u53d1\u5c55\u51fa\u4e86\u4e00\u6574\u5957\u6210\u719f\u7684\u5668\u4ef6\u52a0\u5de5\u5de5\u827a\u3002\u9664\u4e86\u5728\u7535\u5b50\u884c\u4e1a\u7684\u5e7f\u6cdb\u5e94\u7528\u5916\uff0c\u8bb8\u591a\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u8fd8\u5177\u6709\u826f\u597d\u7684\u751f\u7269\u76f8\u5bb9\u6027\uff0c\u4ece\u800c\u62d3\u5c55\u4e86\u8fd9\u7c7b\u6750\u6599\u5668\u4ef6\u5728\u751f\u547d\u79d1\u5b66\u548c\u533b\u5b66\u9886\u57df\u7684\u5e94\u7528\u3002\u65e9\u671f\u7684\u5f00\u521b\u6027\u7814\u7a76\u5305\u62ec\u54c8\u4f5b\u5927\u5b66Charles Lieber\u7ec4\u53d1\u5c55\u7684\u5229\u7528\u7845\u7eb3\u7c73\u7ebf\u573a\u6548\u5e94\u7ba1\u6d4b\u91cf\u5c40\u90e8\u751f\u7269\u7535\u4fe1\u53f7\uff0c\u897f\u5317\u5927\u5b66John\u00a0Rogers\u7ec4\u5f00\u53d1\u7684\u57fa\u4e8e\u67d4\u6027\u7845\u819c\u7684\u8868\u76ae\u7535\u5b50\u5668\u4ef6\u548c\u53ef\u751f\u7269\u964d\u89e3\u5668\u4ef6\uff0c\u4ee5\u53ca\u52a0\u5dde\u5927\u5b66\u4f2f\u514b\u5229\u5206\u6821Paul\u00a0Alivisatos\u7ec4\u5f00\u5c55\u7684\u57fa\u4e8e\u91cf\u5b50\u70b9\u5149\u81f4\u53d1\u5149\u73b0\u8c61\u7684\u751f\u7269\u8367\u5149\u6210\u50cf\u3002\u9664\u4e86\u53ef\u4ee5\u63a5\u53d7\u751f\u7269\u4fe1\u53f7\u6765\u5b9e\u73b0\u76d1\u6d4b\u548c\u4f20\u611f\u5916\uff0c\u8fd1\u5e74\u7684\u7814\u7a76\u8868\u660e\uff0c\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u8fd8\u53ef\u4ee5\u5411\u751f\u7269\u4f53\u7cfb\u8f93\u5165\u4fe1\u53f7\uff08\u7535\u5b66\uff0c\u70ed\u5b66\uff0c\u529b\u5b66\u7b49\uff09\u6765\u8c03\u63a7\u751f\u7269\u4f53\u672c\u8eab\u7684\u884c\u4e3a\uff0c\u4f8b\u5982\u52a0\u5dde\u5927\u5b66\u4f2f\u514b\u5229\u5206\u6821\u7684\u6768\u57f9\u4e1c\u7ec4\u63d0\u51fa\u7684\u57fa\u4e8e\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\uff08\u7845\u7eb3\u7c73\u7ebf\uff0c\u91cf\u5b50\u70b9\u7b49\uff09\u7684\u4eba\u5de5\u5149\u5408\u4f5c\u7528\uff0c\u4ee5\u53ca\u829d\u52a0\u54e5\u5927\u5b66\u7530\u535a\u4e4b\u7ec4\u5f00\u5c55\u7684\u57fa\u4e8e\u7845\u57fa\u751f\u7269\u6750\u6599\uff08\u4ecb\u5b54\u7845\u9897\u7c92\uff0c\u7845\u7eb3\u7c73\u7ebf\uff0c\u67d4\u6027\u7845\u819c\u7b49\uff09\u7684\u5149\u63a7\u795e\u7ecf\u8c03\u5236\u6280\u672f\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u8be5\u9886\u57df\u524d\u671f\u7684\u7814\u7a76\u4e3b\u8981\u7740\u773c\u4e8e\u6750\u6599\u548c\u5668\u4ef6\u672c\u8eab\u7684\u6027\u80fd\u4f18\u5316\u4e0a\uff0c\u800c\u6750\u6599\u548c\u751f\u7269\u754c\u9762\u95ee\u9898\u7684\u91cd\u8981\u6027\u5219\u5f80\u5f80\u88ab\u5ffd\u89c6\u3002\u4e8b\u5b9e\u4e0a\uff0c\u8d8a\u6765\u8d8a\u591a\u7684\u7814\u7a76\u6307\u51fa\uff0c\u786e\u4fdd\u6750\u6599\u548c\u751f\u7269\u4f53\u7cfb\u5728\u529b\u5b66\u6027\u8d28\u548c\u7269\u7406\u5c3a\u5bf8\u4e0a\u7684\u5339\u914d\uff0c\u4ee5\u53ca\u5408\u7406\u8bbe\u8ba1\u8de8\u8d8a\u754c\u9762\u7684\u4fe1\u53f7\u6216\u80fd\u91cf\u6d41\u52a8\u7684\u6a21\u5f0f\u624d\u662f\u5b9e\u73b0\u9ad8\u6548\u7684\u529f\u80fd\u6027\u751f\u7269\u754c\u9762\u7684\u57fa\u7840\u3002\u8fd1\u65e5\uff0c\u5728\u56fd\u9645\u8457\u540d\u671f\u520a<strong><b>Nature<\/b><\/strong><strong><b>\u00a0Reviews Materials<\/b><\/strong>\u4e0a\uff0c<strong><b>\u829d\u52a0\u54e5\u5927\u5b66\u7530\u535a\u4e4b\u7ec4<\/b><\/strong>\u53d1\u8868\u4e86\u9898\u4e3a<strong><b>Inorganic semiconductor biointerfaces<\/b><\/strong>\u7684\u7efc\u8ff0\u6587\u7ae0\uff0c\u7cfb\u7edf\u5f97\u5f52\u7eb3\u4e86\u73b0\u6709\u7684\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u751f\u7269\u754c\u9762\u7684\u7279\u6027\uff0c\u4ee5\u53ca\u5176\u5728\u751f\u7269\u7269\u7406\u548c\u751f\u7269\u533b\u5b66\u65b9\u9762\u7684\u5e94\u7528\u3002\u5728\u672c\u6587\u4e2d\uff0c\u4f5c\u8005\u4eec\u9996\u5148\u8ba8\u8bba\u4e86\u534a\u5bfc\u4f53\u7269\u7406\u7684\u57fa\u7840\u77e5\u8bc6\u548c\u534a\u5bfc\u4f53\u5668\u4ef6\u7684\u5de5\u4f5c\u539f\u7406\uff0c\u5e76\u4e14\u7740\u91cd\u5f3a\u8c03\u4e86\u5176\u5728\u751f\u7406\u6761\u4ef6\u4e0b\u76f8\u6bd4\u4e8e\u4f20\u7edf\u56fa\u6001\u6761\u4ef6\u4e0b\u5de5\u4f5c\u7279\u70b9\u7684\u4e0d\u540c\u4e4b\u5904\u3002\u968f\u540e\uff0c\u4f5c\u8005\u4eec\u603b\u7ed3\u4e86\u5404\u79cd\u5e38\u89c1\u7684\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u7684\u5408\u6210\u548c\u5668\u4ef6\u52a0\u5de5\u5de5\u827a\uff0c\u5305\u62ec\u5404\u79cd\u53ef\u80fd\u7684\u96f6\u7ef4\uff0c\u4e8c\u7ef4\uff0c\u4e8c\u7ef4\u548c\u4e09\u7ef4\u4f53\u7cfb\u3002\u6700\u540e\uff0c\u57fa\u4e8e\u4e0d\u540c\u751f\u7269\u7535\u5b50\u5b66\u548c\u751f\u7269\u5149\u5b50\u5b66\u5668\u4ef6\u5728\u751f\u7269\u754c\u9762\u4e0a\u7684\u4fe1\u53f7\u4f20\u5bfc\u673a\u7406\uff0c\u4f5c\u8005\u4eec\u5c06\u5df2\u6709\u7684\u7814\u7a76\u5206\u6210\u4e86\u5982\u4e0b\u51e0\u5927\u7c7b\uff0c\u5305\u62ec\u7535\u5b66\u548c\u5149\u7535\u751f\u7269\u4f20\u611f\uff0c\u5149\u7535\u548c\u5149\u70ed\u751f\u7269\u523a\u6fc0\u4ee5\u53ca\u5149\u81f4\u53d1\u5149\u751f\u7269\u6210\u50cf\uff0c\u5e76\u4e14\u5206\u522b\u7ed9\u51fa\u4e86\u5bf9\u5e94\u7684\u4e8b\u4f8b\u5206\u6790\u3002\u6700\u540e\uff0c\u4f5c\u8005\u4eec\u63d0\u8bae\u672a\u6765\u7684\u7814\u7a76\u5e94\u5f53\u5bf9\u6750\u6599\u7684\u751f\u7269\u76f8\u5bb9\u6027\u8fdb\u884c\u7cfb\u7edf\u7684\u5b9a\u91cf\u5206\u6790\uff0c\u5e76\u4e14\u6307\u51fa\u4e86\u4e00\u4e9b\u672a\u6765\u6750\u6599\u53d1\u5c55\u65b9\u5411\u4ee5\u53ca\u4e0e\u5176\u76f8\u5173\u7684\u91cd\u8981\u751f\u7269\u5b66\u95ee\u9898\u3002\u672c\u6587\u7684\u7b2c\u4e00\u4f5c\u8005\u4e3a\u539f\u829d\u52a0\u54e5\u5927\u5b66\u5316\u5b66\u7cfb\u535a\u58eb\u751f\uff0c\u73b0\u65af\u5766\u798f\u5927\u5b66\u5316\u5de5\u7cfb\u535a\u58eb\u540e<strong><b>\u848b\u5706\u95fb<\/b><\/strong>\uff0c\u901a\u8baf\u4f5c\u8005\u4e3a\u829d\u52a0\u54e5\u5927\u5b66\u5316\u5b66\u7cfb<strong><b>\u7530\u535a\u4e4b\u6559\u6388<\/b><\/strong>\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong><b>\u56fe1\uff1a\u4e00\u4e9b\u5c06\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u548c\u5668\u4ef6\u7528\u4e8e\u751f\u7269\u7814\u7a76\u7684\u91cc\u7a0b\u7891\u3002<\/b><\/strong>\u8be6\u89c1\u524d\u8a00\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-160415 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72471-17.png\" alt=\"\" width=\"600\" height=\"186\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72471-17.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72471-17-300x93.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u56fe2\uff1a\u65e0\u673a\u534a\u5bfc\u4f53\u548c\u751f\u7406\u6db2\u4f53\u754c\u9762\u7684\u6750\u6599\u7269\u7406\u603b\u7ed3\u3002<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-160416 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72472-16.png\" alt=\"\" width=\"600\" height=\"731\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72472-16.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72472-16-246x300.png 246w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08a\uff09\u76f4\u63a5\u548c\u95f4\u63a5\u5e26\u9699\u534a\u5bfc\u4f53\u7684\u80fd\u5e26\u7ed3\u6784\u533a\u522b\u3002\uff08b\uff09\u5e38\u89c1\u534a\u5bfc\u4f53\u4ef7\u5e26\u5bfc\u5e26\u76f8\u5bf9\u4e8e\u771f\u7a7a\u80fd\u7ea7\u548c\u751f\u7406\u6761\u4ef6\u4e0b\u6c27\u5316\u8fd8\u539f\u7535\u5bf9\u7684\u4f4d\u7f6e\u3002\uff08c\uff09\u534a\u5bfc\u4f53\u548c\u7535\u89e3\u8d28\u754c\u9762\u7684\u80fd\u5e26\u5f2f\u66f2\u73b0\u8c61\u4ee5\u53ca\u53d7\u5176\u5f71\u54cd\u7684\u5149\u751f\u8f7d\u6d41\u5b50\u7684\u6d41\u52a8\u3002<\/p>\n<p><strong><b>\u56fe3\uff1a\u5e38\u89c1\u65e0\u673a\u534a\u5bfc\u4f53\u5668\u4ef6\u7684\u5de5\u4f5c\u539f\u7406\u3002<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-160418 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72473-15.png\" alt=\"\" width=\"600\" height=\"352\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72473-15.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72473-15-300x176.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08a\uff09\u573a\u6548\u5e94\u7ba1\uff08b\uff09pn\u7ed3\uff08c\uff09\u5149\u4f0f\u5668\u4ef6\uff08d\uff09\u53d1\u5149\u4e8c\u6781\u7ba1\u3002<\/p>\n<p><strong><b>\u56fe4\uff1a\u5404\u79cd\u7ef4\u5ea6\u7684\u534a\u5bfc\u4f53\u6750\u6599\u548c\u5668\u4ef6\u4ee5\u53ca\u5176\u53ef\u80fd\u5f62\u6210\u751f\u7269\u754c\u9762\u7c7b\u578b\u3002<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-160420 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72474-16.png\" alt=\"\" width=\"600\" height=\"324\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72474-16.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72474-16-300x162.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08a\uff09\u96f6\u7ef4\u91cf\u5b50\u70b9\u53ef\u4ee5\u7528\u4e8e\u4eba\u5de5\u5149\u5408\u4f5c\u7528\u548c\u6807\u8bb0\u7ec6\u80de\u5185\u4e3b\u52a8\u8fd0\u8f93\u8fc7\u7a0b\u3002\uff08b\uff09\u4e00\u7ef4\u7eb3\u7c73\u7ebf\u53ef\u4ee5\u7528\u4e8e\u7ec6\u80de\u5185\u7535\u751f\u7406\u8bb0\u5f55\u548c\u4fc3\u8fdb\u5fae\u751f\u7269\u71c3\u6599\u7535\u6c60\u3002\uff08c\uff09\u4e8c\u7ef4\u8584\u819c\u53ef\u4ee5\u7528\u4e8e\u52a0\u5de5\u77ac\u6001\u7535\u5b50\u5b66\u5668\u4ef6\u548c\u975e\u9057\u4f20\u5149\u7535\u795e\u7ecf\u523a\u6fc0\u3002\uff08d\uff09\u4e09\u7ef4\u4ecb\u89c2\u7ed3\u6784\u53ef\u4ee5\u7528\u6765\u5b9e\u73b0\u591a\u529f\u80fd\u7ec6\u80de\u63a2\u9488\u548c\u7c7b\u7ec4\u7ec7\u68c0\u6d4b\u7f51\u7edc\u3002\uff08e\uff09\u751f\u7269\u7535\u5b50\u5b66\u548c\u751f\u7269\u5149\u5b50\u5b66\u754c\u9762\u5305\u62ec\u7535\u5b66\u68c0\u6d4b\uff0c\u5149\u7535\u68c0\u6d4b\uff0c\u5149\u7535\u523a\u6fc0\uff0c\u5149\u70ed\u523a\u6fc0\u548c\u5149\u81f4\u53d1\u5149\u6210\u50cf\u7b49\u3002<\/p>\n<p><strong><b>\u56fe5\uff1a\u5404\u79cd\u8de8\u8d8a\u751f\u7269\u754c\u9762\u7684\u4fe1\u53f7\u4f20\u5bfc\u6a21\u5f0f\u3002<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-160421 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72475-13.png\" alt=\"\" width=\"600\" height=\"536\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72475-13.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72475-13-300x268.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08a\uff09\u2460\u573a\u6548\u5e94\u7ba1\u53ef\u4ee5\u7528\u6765\u68c0\u6d4b\u5c40\u90e8\u5206\u6790\u7269\u6d53\u5ea6\u548c\u7ec6\u80de\u819c\u7535\u4f4d\u2461\u5149\u7535\u4e8c\u6781\u7ba1\u53ef\u4ee5\u7528\u6765\u68c0\u6d4b\u751f\u7269\u53d1\u5149\u8fc7\u7a0b\u2462\u5149\u4f0f\u5668\u4ef6\u53ef\u4ee5\u901a\u8fc7\u5149\u7535\u5bb9\u6216\u5149\u7535\u5316\u5b66\u8fc7\u7a0b\u6765\u523a\u6fc0\u7ec6\u80de\u884c\u4e3a\u2463\u53d1\u5149\u4e8c\u6781\u7ba1\u7ed3\u5408\u5149\u9057\u4f20\u6280\u672f\u53ef\u4ee5\u7528\u6765\u76f4\u63a5\u523a\u6fc0\u7ec6\u80de\u2464\u8f7d\u6d41\u5b50\u7b26\u5408\u4ea7\u751f\u7684\u70ed\u80fd\u53ef\u4ee5\u7528\u4e8e\u6539\u53d8\u7ec6\u80de\u819c\u7535\u5bb9\u4ee5\u5b9e\u73b0\u7ec6\u80de\u523a\u6fc0\u2465\u7eb3\u7c73\u5c3a\u5ea6\u7684\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u53ef\u4ee5\u88ab\u7ec6\u80de\u5185\u541e\uff0c\u4ece\u800c\u5b9e\u73b0\u7ec6\u80de\u5185\u529f\u80fd\u754c\u9762\u3002\uff08b\uff09\u5149\u7535\u5bb9\uff08\u53ea\u6d89\u53ca\u53cc\u7535\u5bb9\u5145\u653e\u7535\uff09\u548c\u5149\u7535\u5316\u5b66\uff08\u5305\u62ec\u754c\u9762\u6c27\u5316\u8fd8\u539f\u53cd\u5e94\uff09\u8fc7\u7a0b\u7684\u533a\u522b\u3002<\/p>\n<p><strong>\u3010\u5c0f\u7ed3\u548c\u5c55\u671b\u3011<\/strong><\/p>\n<p>\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u548c\u5668\u4ef6\u7531\u4e8e\u5176\u591a\u6837\u7684\u7269\u7406\u5316\u5b66\u6027\u8d28\uff0c\u826f\u597d\u7684\u53ef\u52a0\u5de5\u6027\u548c\u751f\u7269\u76f8\u5bb9\u6027\uff0c\u5df2\u7ecf\u88ab\u5e7f\u6cdb\u5f97\u7528\u4e8e\u751f\u7269\u7269\u7406\u5b66\u7814\u7a76\u548c\u751f\u7269\u533b\u5b66\u5e94\u7528\u4e2d\u3002\u672c\u6587\u8be6\u7ec6\u5f97\u8ba8\u8bba\u4e86\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u5668\u4ef6\u7684\u5408\u6210\u52a0\u5de5\u548c\u5de5\u4f5c\u539f\u7406\uff0c\u6df1\u5165\u5f97\u603b\u7ed3\u4e86\u8de8\u8d8a\u751f\u7269\u754c\u9762\u7684\u5404\u79cd\u4fe1\u53f7\u4f20\u9012\u673a\u7406\uff0c\u4e3a\u6b64\u540e\u7684\u7814\u7a76\u6253\u4e0b\u4e86\u575a\u5b9e\u7684\u57fa\u7840\u3002\u5c3d\u7ba1\u5982\u6b64\uff0c\u5728\u6750\u6599\u751f\u7269\u7684\u754c\u9762\u4e0a\u4ecd\u7136\u6709\u8bb8\u591a\u5c1a\u672a\u5b8c\u5168\u56de\u7b54\u7684\u95ee\u9898\u9700\u8981\u65b0\u7684\u624b\u6bb5\u6765\u8fdb\u884c\u6df1\u5165\u7684\u7814\u7a76\u3002\u65b0\u8fd1\u5f00\u53d1\u7684\u8868\u5f81\u6280\u672f\u5305\u62ec\u9ad8\u901f\u539f\u5b50\u529b\u663e\u5fae\u5b66\uff0c\u77ac\u6001\u5149\u8c31\uff0c\u51b7\u51bb\u79bb\u5b50\u675f\u523b\u8680\uff0c\u9ad8\u901f\u8d85\u5206\u8fa8\u663e\u5fae\u5b66\u7b49\u624b\u6bb5\u90fd\u53ef\u80fd\u5f97\u5230\u524d\u6240\u672a\u6709\u7684\u5173\u4e8e\u751f\u7269\u754c\u9762\u7684\u9ad8\u7cbe\u5ea6\u7ed3\u6784\u548c\u529f\u80fd\u4fe1\u606f\u3002\u9664\u6b64\u4e4b\u5916\uff0c\u65b0\u578b\u7684\u6750\u6599\u5408\u6210\u624b\u6bb5\u4e5f\u53ef\u80fd\u4e3a\u751f\u7269\u754c\u9762\u63d0\u4f9b\u65b0\u7684\u673a\u9047\u3002\u4e3e\u4f8b\u6765\u8bf4\uff0c\u7ed3\u5408\u57fa\u56e0\u5de5\u7a0b\u548c\u751f\u7269\u77ff\u5316\u8fc7\u7a0b\u6216\u8bb8\u80fd\u591f\u5b9a\u70b9\u5b9a\u5411\u5f97\u5728\u7279\u5b9a\u7ec6\u80de\u5185\u8154\u5ba4\u5904\u5408\u6210\u5177\u6709\u7279\u5b9a\u5f62\u8c8c\u7684\u7eb3\u7c73\u534a\u5bfc\u4f53\u6750\u6599\u7528\u4e8e\u9ad8\u7cbe\u5ea6\u751f\u7269\u68c0\u6d4b\u6216\u8005\u9ad8\u6548\u80fd\u751f\u7269\u8c03\u63a7\u3002\u6700\u540e\uff0c\u9664\u4e86\u4f20\u7edf\u7684\u7535\u5b66\u6d3b\u6027\u7684\u751f\u7269\u4f53\u7cfb\u5916\uff0c\u8fd8\u6709\u8bb8\u591a\u65b0\u7684\u5bf9\u8c61\u53ef\u4ee5\u7528\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u548c\u5668\u4ef6\u6765\u8fdb\u884c\u7814\u7a76\uff0c\u5305\u62ec\u7ec6\u80de\u9aa8\u67b6\u7684\u7ed3\u6784\u548c\u57fa\u4e8e\u8fd0\u52a8\u86cb\u767d\u7684\u4e3b\u52a8\u8fd0\u8f93\u8fc7\u7a0b\uff0c\u5fae\u751f\u7269\u7fa4\u843d\u5185\u901a\u8baf\uff0c\u4ee5\u53ca\u80da\u80ce\u53d1\u80b2\u8fc7\u7a0b\u7b49\u3002<\/p>\n<p><strong><b>\u6587\u732e\u94fe\u63a5\uff1a<\/b><\/strong>Inorganic semiconductor biointerfaces\uff08Nat. Rev. Mater., 2018, DOI:\u00a010.1038\/\u00a0s41578-018-0062-3\uff09<\/p>\n<p><a href=\"https:\/\/www.nature.com\/articles\/s41578-018-0062-3\">https:\/\/www.nature.com\/articles\/s41578-018-0062-3<\/a><\/p>\n<p>\u7845\u57fa\u751f\u7269\u754c\u9762\u6750\u6599\u65b9\u5411\u6700\u8fd1\u53d1\u8868\u6587\u7ae0\uff08\u8282\u9009\uff09\uff1a<\/p>\n<p>1) Jiang, Y. W.,* Li, X. J.,* Liu, B.,* Yi, J., Fang, Y., Shi, F. Y., Gao, X., Sudzilovsky, E., Parameswaran, R., Koehler, K., Nair, V., Yue, J. P., Guo, K. H., Fang, Y., Tsai, H.-M., Freyermuth, G., Wong, R. C. S., Kao, C.-M., Chen, C.-T., Nicholls, A. W., Wu, X. Y., Shepherd, G. M. G., &amp; Tian, B. Z., Rational design of silicon structures for optically controlled multiscale biointerfaces, <em><i>Nature Biomedical Engineering<\/i><\/em>\u00a0<strong><b>2<\/b><\/strong>, 508-521 (*These authors contributed equally to this work.)<\/p>\n<p>2) Jiang, Y. W.,* Carvalho-de-Souza, J. L.,* Wong, R. C. S.,* Luo, Z. Q., Isheim, D., Zuo, X. B., Nicholls, A. W., Jung, I. W., Yue, J. P., Liu, D.-J., Wang, Y. C., De Andrade, V., Xiao, X. H., Navrazhnykh, L. Weiss, D. E., Wu, X. Y., Seidman, D. N., Bezanilla, F. &amp; Tian, B. Z. Heterogeneous silicon-based mesostructures for phospholipid-supported transient bioelectric systems. <em><i>Nature Materials<\/i><\/em>\u00a0<strong><b>15<\/b><\/strong>, 1023-1030 (2016). (*These authors contributed equally to this work.)<\/p>\n<p>3) Parameswaran. R., Carvalho-de-Souza, J. L., Jiang, Y. W., Burke, M., Zimmerman, J., Koehler, K., Phillips, A. W., Yi, J., Adams, E., Bezanilla, F., &amp; Tian, B. Z. Photoelectrochemical modulation of neuronal activity with freestanding coaxial silicon nanowires <em><i>Nature Nanotechnology<\/i><\/em>, <strong><b>13<\/b><\/strong>, 260\u2013266 (2018)<\/p>\n<p>4) Fang, Y.,* Jiang, Y. W.,* Ledesma, H. A.,* Yi, J., Gao, X., Weiss, D. E., Shi, F. Y., &amp; Tian., B. Z. Texturing Silicon Nanowires for Highly Localized Optical Modulation of Cellular Dynamics, <em><i>Nano Letters<\/i><\/em>\u00a0<strong><b>18<\/b><\/strong>, 4487-4492 (2018). (*These authors contributed equally to this work.)<\/p>\n<p>5) Luo, Z. Q.,* Jiang, Y. W.,* Myers, B. D., Isheim, D., Wu, J. S., Zimmerman, J. F., Wang, Z. A., Li, Q. Q., Wang, Y. C., Chen, X. Q., Seidman, D. N. &amp; Tian, B. Z. Atomic gold-enabled three-dimensional lithography for silicon mesostructures. <em><i>Science<\/i><\/em>\u00a0<strong><b>348<\/b><\/strong>, 1451-1455 (2015). (*These authors contributed equally to this work.)<\/p>\n<p>6) Fang, Y.,* Jiang, Y. W.,* Cherukara, M. J.* Shi, F. Y., Koehler, K., Freyermuth, G., Isheim, D., Narayanan, B., Nicholls, A. W., Seidman, D. N., Sankaranarayanan, S. K. R. S., &amp; Tian, B. Z. Alloy-assisted deposition of three-dimensional arrays of atomic gold catalyst for crystal growth studies, <em><i>Nature Communications<\/i><\/em>\u00a0<strong><b>8<\/b><\/strong>, 2014 (2017). (*These authors contributed equally to this work.)<\/p>\n<p>\u672c\u6587\u7531<strong><b>\u829d\u52a0\u54e5\u5927\u5b66\u7530\u535a\u4e4b\u7ec4<\/b><\/strong>\u4f9b\u7a3f\uff0c\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u7f16\u8f91\u3002<\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaorenvip\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n<p>&nbsp;<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u524d\u8a00\u3011 \u968f\u7740\u534a\u5bfc\u4f53\u5de5\u4e1a\u7684\u84ec\u52c3\u53d1\u5c55\uff0c\u4eba\u4eec\u5173\u4e8e\u65e0\u673a\u534a\u5bfc\u4f53\u6750\u6599\u7269\u7406\u5316\u5b66\u6027\u8d28\u7684\u77e5\u8bc6\u5df2\u7ecf\u76f8\u5f53\u4e30\u5bcc\uff0c\u4e5f\u56e0\u6b64\u53d1\u5c55\u51fa\u4e86\u4e00\u6574\u5957\u6210\u719f\u7684\u5668\u4ef6\u52a0\u5de5\u5de5\u827a\u3002\u9664\u4e86\u5728\u7535\u5b50\u884c\u4e1a\u7684\u5e7f\u6cdb\u5e94\u7528\u5916\uff0c\u8bb8&#8230;<\/p>\n","protected":false},"author":10213,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-160414","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/160414"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/10213"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=160414"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/160414\/revisions"}],"predecessor-version":[{"id":160445,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/160414\/revisions\/160445"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=160414"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=160414"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=160414"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}