{"id":161319,"date":"2019-01-13T06:55:29","date_gmt":"2019-01-12T22:55:29","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=161319"},"modified":"2019-01-12T23:57:16","modified_gmt":"2019-01-12T15:57:16","slug":"%e7%a0%94%e7%a9%b6%e8%bf%9b%e5%b1%95%e6%b1%87%e6%80%bb%ef%bc%9a%e9%bb%84%e7%bb%b4%e9%99%a2%e5%a3%ab%e4%b8%8e%e4%bb%96%e7%9a%84%e7%a0%94%e7%a9%b6%e5%9b%a2%e9%98%9f","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=161319","title":{"rendered":"\u7814\u7a76\u8fdb\u5c55\u6c47\u603b\uff1a\u9ec4\u7ef4\u9662\u58eb\u4e0e\u4ed6\u7684\u7814\u7a76\u56e2\u961f"},"content":{"rendered":"<p>\u4eba\u7269\u7b80\u4ecb<\/p>\n<div class=\"para\">\u9ec4\u7ef4\uff0c\u7537\uff0c\u6c49\u65cf\uff0c1963\u5e745\u6708\u51fa\u751f\uff0c\u4e2d\u5171\u515a\u5458\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u9662\u58eb\uff0c\u4fc4\u7f57\u65af\u79d1\u5b66\u9662\u5916\u7c4d\u9662\u58eb\uff0c\u4e2d\u56fd\u6709\u673a\u7535\u5b50\u5b66\u4e0e\u67d4\u6027\u7535\u5b50\u5b66\u7684\u4e3b\u8981\u5960\u57fa\u8005\u00a0\uff0c\u897f\u5317\u5de5\u4e1a\u5927\u5b66\u535a\u58eb\u751f\u5bfc\u5e08\u3001\u6559\u6388\uff0c\u4e2d\u56fd\u56fd\u5bb6\u6770\u51fa\u9752\u5e74\u79d1\u5b66\u57fa\u91d1\u83b7\u5f97\u8005\uff0c\u4e2d\u56fd\u201c\u5343\u4eba\u8ba1\u5212\u201d\u56fd\u5bb6\u7279\u8058\u4e13\u5bb6\uff0c\u4e2d\u56fd\u6559\u80b2\u90e8\u201c\u957f\u6c5f\u5b66\u8005\u201d\u7279\u8058\u6559\u6388\uff0c\u4e2d\u56fd\u56fd\u5bb6\u201c973\u8ba1\u5212\u201d\u9879\u76ee\u9996\u5e2d\u79d1\u5b66\u5bb6\u30021992\u5e741\u6708\uff0c\u9ec4\u7ef4\u535a\u58eb\u6bd5\u4e1a\u4e8e\u5317\u4eac\u5927\u5b66\u5e76\u7559\u6821\u4efb\u6559\uff1b1993\u5e7412\u6708\uff0c\u8d74\u65b0\u52a0\u5761\u505a\u535a\u58eb\u540e\u7814\u7a76\uff1b2006\u5e746\u6708\uff0c\u62c5\u4efb\u5357\u4eac\u90ae\u7535\u5927\u5b66\u526f\u6821\u957f\uff1b2012\u5e747\u6708\uff0c\u62c5\u4efb\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\u6821\u957f\uff1b2017\u5e746\u6708\uff0c\u62c5\u4efb\u897f\u5317\u5de5\u4e1a\u5927\u5b66\u515a\u59d4\u5e38\u59d4\u3001\u5e38\u52a1\u526f\u6821\u957f\u3002<\/div>\n<div>\u00a0<\/div>\n<div class=\"para\">\u9ec4\u7ef4\u9662\u58eb\u7684\u4e3b\u8981\u7814\u7a76\u9886\u57df\u4e3a\u7eb3\u7c73\u6750\u6599\u4e0e\u6280\u672f\u548c\u6709\u673a\u7535\u5b50\u4e0e\u5668\u4ef6\u7b49\uff0c\u4e3a\u4e86\u5927\u5bb6\u4e86\u89e3\u4ed6\u548c\u7814\u7a76\u56e2\u961f\u8fd1\u5e74\u7684\u79d1\u7814\u6210\u679c\uff0c\u6750\u6599\u4eba\u505a\u4e86\u4e00\u4e2a\u6c47\u603b\uff0c\u65b9\u4fbf\u5927\u5bb6\u9605\u8bfb\u3002<\/div>\n<p><strong>\u53d1\u8868\u7684\u7814\u7a76\u6210\u679c\uff1a<\/strong><\/p>\n<p>1.\u8bba\u6587\uff1a\u52a8\u6001\u5171\u632f\u6709\u673a\u957f\u4f59\u8f89\u6750\u6599<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-158226 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u724724.png\" alt=\"\" width=\"650\" height=\"304\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u724724.png 650w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u724724-300x140.png 300w\" sizes=\"(max-width: 650px) 100vw, 650px\" \/><\/p>\n<p><strong><b>\u5357\u4eac\u90ae\u7535\u5927\u5b66\u7684\u9ec4\u7ef4\u9662\u58eb<\/b><\/strong>\u548c<strong><b>\u9648\u6da6\u950b\u6559\u6388<\/b><\/strong>\u8bfe\u9898\u7ec4\uff08\u5171\u540c\u901a\u8baf\uff09\u7ee72015\u5e74\u9996\u6b21\u62a5\u9053\u6709\u673a\u957f\u4f59\u8f89\u6750\u6599\uff08<em><i>Nat. Mater.<\/i><\/em>\u00a0<strong><b>2015<\/b><\/strong>, <em><i>14<\/i><\/em>, 685\uff09\u4e4b\u540e\uff0c\u5229\u7528\u5171\u632f\u7ed3\u6784\u72ec\u7279\u7684\u52a8\u6001\u81ea\u9002\u5e94\u6027\uff0c\u6709\u6548\u5730\u8c03\u6574\u81ea\u8eab\u7ed3\u6784\uff0c\u4ece\u800c\u5b9e\u73b0\u5bf9\u6750\u6599\u7684\u57fa\u6001\u3001\u6fc0\u53d1\u6001\u80fd\u7ea7\u4ee5\u53ca\u8dc3\u8fc1\u6210\u4efd\u7684\u8c03\u63a7\uff0c\u5f00\u53d1\u4e86\u4e24\u79cd\u5177\u6709N-P=O\/N-P=S\u7ed3\u6784\u7684\u65b0\u578b\u957f\u4f59\u8f89\u6750\u6599\u3002\u901a\u8fc7\u7406\u8bba\u8ba1\u7b97\u7814\u7a76\u8868\u660e\uff0c\u4e0e\u5177\u6709N-P\u7ed3\u6784\u7684\u5206\u5b50\u76f8\u6bd4\uff0c\u57fa\u4e8eN-P=O\/N-P=S\u5171\u632f\u7ed3\u6784\u7684\u5206\u5b50\u5177\u6709\u53ef\u8c03\u8282\u7684\u5355\u7ebf\u6001\u2014\u4e09\u7ebf\u6001\u80fd\u7ea7\uff0c\u53ef\u6709\u6548\u5730\u51cf\u5c0f\u5b9e\u65f6\u7684\u5355\u7ebf\u6001\u2014\u4e09\u7ebf\u6001\u80fd\u7ea7\u5dee\uff08Real-time \u0394<em><i>E<\/i><\/em><sub>ST<\/sub>\uff09\u4ee5\u53ca\u52a8\u6001\u53ef\u8c03\u7684\u8dc3\u8fc1\u6210\u4efd\uff0c\u56e0\u6b64\u5177\u6709\u66f4\u591a\u7684\u7cfb\u95f4\u7a9c\u8d8a\u901a\u9053\u4ee5\u53ca\u663e\u8457\u589e\u5f3a\u7684\u81ea\u9009\u8f68\u9053\u8026\u5408\u6548\u5e94\uff0c\u53ef\u6709\u6548\u5730\u4fc3\u8fdb\u7cfb\u95f4\u7a9c\u8d8a\uff08Intersystem Crossing, ISC\uff09\u7684\u53d1\u751f\uff0c\u4ece\u800c\u83b7\u5f97\u9ad8\u7684\u4e09\u7ebf\u6001\u6fc0\u5b50\u6d53\u5ea6\u3002\u5176\u6b21\uff0c\u5229\u7528\u5206\u5b50\u4e2d\u5f15\u5165\u7684\u76f8\u5bf9\u5e73\u9762\u7684\u5171\u8f6d\u7ed3\u6784\uff0c\u6784\u7b51\u6709\u6548\u7684H\u805a\u96c6\uff08H-aggregates\uff09\uff0c\u7a33\u5b9a\u9ad8\u5ea6\u6d3b\u6cfc\u7684\u4e09\u7ebf\u6001\u6fc0\u5b50\uff0c\u7ee7\u800c\u5b9e\u73b0\u9ad8\u7684\u4f59\u8f89\u53d1\u5149\u6548\u7387\u4ee5\u53ca\u957f\u7684\u53d1\u5149\u5bff\u547d\u3002\u5f00\u53d1\u7684\u4f59\u8f89\u6750\u6599\u6700\u957f\u5bff\u547d\u4e3a0.67 s\uff0c\u7cfb\u95f4\u7a9c\u8d8a\u901f\u7387\u9ad8\u8fbe10<sup>7<\/sup>\u00a0s<sup>-1<\/sup>\uff0c\u53d1\u5149\u6548\u7387\u4e3a4.0%\uff0c\u8fd9\u4e00\u7ed3\u679c\u7a81\u7834\u4e86\u4f59\u8f89\u6750\u6599\u5bff\u547d\u548c\u6548\u7387\u4e0d\u80fd\u540c\u65f6\u63d0\u9ad8\u7684\u77db\u76fe\u95ee\u9898\u3002\u8fd9\u4e00\u6210\u679c\u8fd1\u671f\u53d1\u8868\u5728Advanced Materials (10.1002\/adma.201803856)\u4e0a\uff0c\u5e76\u88ab\u9009\u4e3a\u5f53\u671f\u7684\u5185\u5c01\u9762\uff0c\u6587\u7ae0\u7684\u7b2c\u4e00\u4f5c\u8005\u662f\u5357\u4eac\u90ae\u7535\u5927\u5b66\u535a\u58eb\u6bd5\u4e1a\u751f\u9676\u51b6\u3002<\/p>\n<p>\u6587\u7ae0\u94fe\u63a5\uff1a<a href=\"https:\/\/onlinelibrary.wiley.com\/doi\/abs\/10.1002\/adma.201803856\" target=\"_blank\" rel=\"noopener\">https:\/\/onlinelibrary.wiley.com\/doi\/abs\/10.1002\/adma.201803856<\/a><\/p>\n<p>2.\u8bba\u6587\uff1a\u53d6\u5411\u51c6\u4e8c\u7ef4\u9499\u949b\u77ff\u7528\u4e8e\u9ad8\u6027\u80fd\u5149\u7535\u5668\u4ef6<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-157623\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/10\/1-41.jpg\" alt=\"\" width=\"600\" height=\"340\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/10\/1-41.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/10\/1-41-300x170.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\u9ec4\u7ef4\u9662\u58eb\u3001\u738b\u5efa\u6d66\u6559\u6388(\u5171\u540c\u901a\u8baf\u4f5c\u8005)\u7b49<\/strong>\u5229\u75283-\u6eb4\u82ef\u7532\u80fa\u7898(3BBAI)\u5236\u5907\u4e86\u9ad8\u6548\u4e14\u6c34\u7a33\u5b9a\u7684\u51c6\u4e8c\u7ef4\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\uff0c\u5176\u529f\u7387\u8f6c\u6362\u6548\u7387(PCE)\u8fbe18.20 %\uff0c\u5e76\u5728<strong>Adv. Mater.<\/strong>\u4e0a\u53d1\u8868\u4e86\u9898\u4e3a\u201c<strong>Oriented Quasi-2D Perovskites for High Performance Optoelectronic Devices<\/strong>\u201d\u7684\u7814\u7a76\u8bba\u6587\uff0c\u535a\u58eb\u7814\u7a76\u751f\u6768\u8363\u548c\u674e\u4ec1\u5fd7\u526f\u7814\u7a76\u5458\u4e3a\u5171\u540c\u7b2c\u4e00\u4f5c\u8005\u3002\u672a\u5c01\u88c5\u5668\u4ef6\u5728\u76f8\u5bf9\u6e7f\u5ea640%\u7684\u5927\u6c14\u73af\u5883\u653e\u7f6e2400 h\u540e\uff0c\u6548\u7387\u4ecd\u4fdd\u6301\u521d\u59cb\u503c\u768482%\u4ee5\u4e0a\uff0c\u5e76\u4e14\u6d78\u5165\u6c34\u4e2d60 s\u540e\u5149\u4f0f\u53c2\u6570\u51e0\u4e4e\u4e0d\u53d8\u3002\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u7684\u4f18\u8d8a\u6027\u80fd\u5e94\u5f52\u56e0\u4e8e\u5177\u6709\u758f\u6c34\u6027\u3001\u9ad8\u5ea6\u7535\u5b50\u6709\u5e8f\u6027\u3001\u9ad8\u7ed3\u6676\u5ea6\u7684\u51c6\u4e8c\u7ef4\u9499\u949b\u77ff\u8584\u819c\u3002\u8be5\u8584\u819c\u4e0a\u5c42\u662f\u9ad8\u5ea6\u53d6\u5411\u751f\u957f\u7684\u4e09\u7ef4\u9499\u949b\u77ff\u7ec4\u5206\uff0c\u5176\u8f83\u5c0f\u7684\u5e26\u9699\u548c\u4f4e\u7684\u6fc0\u5b50\u675f\u7f1a\u80fd\u53ef\u5b9e\u73b0\u4f4e\u80fd\u592a\u9633\u5149\u5b50\u5229\u7528\u548c\u9ad8\u6548\u7535\u8377\u5206\u79bb\uff0c\u800c\u8584\u819c\u5e95\u90e8\u662f\u7ad6\u76f4\u751f\u957f\u7684\u5bbd\u5e26\u9699\u9499\u949b\u77ff\u7ec4\u5206\uff0c\u6709\u5229\u4e8e\u5b9e\u73b0\u9ad8\u6548\u7684\u7535\u8377\u4f20\u8f93\u3002\u6b64\u5916\uff0c\u7531\u4e8e\u6291\u5236\u4e86\u975e\u8f90\u5c04\u590d\u5408\uff0c\u8be5\u5668\u4ef6\u4e5f\u80fd\u4f5c\u4e3a\u53d1\u5149\u4e8c\u6781\u7ba1(LED)\u5f88\u597d\u7684\u5de5\u4f5c\uff0c\u53ef\u8fbe3.85 %\u3002\u5927\u6c14\u73af\u5883\u4e0b\uff0c\u672a\u5c01\u88c5\u5668\u4ef6\u5728200 mA\u00b7cm<sup>-2<\/sup>\u7684\u9ad8\u7535\u6d41\u5bc6\u5ea6\u4e0b\u5de5\u4f5c\u5bff\u547d\u7ea696 h\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adma.201804771\/full\" target=\"_blank\" rel=\"noopener\">Oriented Quasi-2D Perovskites for High Performance Optoelectronic Devices<\/a> <\/strong>(<strong>Adv. Mater.<\/strong>, 2018, DOI: 10.1002\/adma.201804771)<\/p>\n<p>3.\u8bba\u6587\uff1a\u57fa\u4e8e\u81ea\u53d1\u5f62\u6210\u7684\u4e9a\u5fae\u7c73\u7ea7\u7ed3\u6784\u7684\u9499\u949b\u77ff\u53d1\u5149\u4e8c\u6781\u7ba1<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-156128\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/10\/1-7.jpg\" alt=\"\" width=\"600\" height=\"734\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/10\/1-7.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/10\/1-7-245x300.jpg 245w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u5357\u4eac\u5de5\u4e1a\u5927\u5b66<\/b><\/strong><strong><b>\u9ec4\u7ef4\u9662\u58eb\uff08\u76ee\u524d\u5355\u4f4d\u897f\u5317\u5de5\u4e1a\u5927\u5b66\uff09<\/b><\/strong>\u548c<strong><b>\u738b\u5efa\u6d66<\/b><\/strong><strong><b>\u6559\u6388\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09<\/b><\/strong>\u56e2\u961f\u7684\u5e26\u9886\u4e0b\uff0c\u4e0e<strong><b>\u6d59\u6c5f\u5927\u5b66<\/b><\/strong>\u3001<strong><b>\u5357\u4eac\u90ae\u7535\u5927\u5b66<\/b><\/strong>\u548c<strong><b>\u897f\u5317\u5de5\u4e1a\u5927\u5b66<\/b><\/strong>\u5408\u4f5c\uff0c\u5c55\u793a\u4e86\u6eb6\u6db2\u52a0\u5de5\u7684\u9499\u949b\u77ff\u7684\u9ad8\u6548\u548c\u9ad8\u4eae\u5ea6\u7535\u81f4\u53d1\u5149\uff0c\u81ea\u53d1\u5f62\u6210\u4e9a\u5fae\u7c73\u7ea7\u7ed3\u6784\uff0c\u5b83\u80fd\u6709\u6548\u5730\u4ece\u5668\u4ef6\u4e2d\u63d0\u53d6\u5149\uff0c\u5e76\u4fdd\u6301\u4e0e\u6ce2\u957f\u548c\u89c6\u89d2\u65e0\u5173\u7684\u7535\u81f4\u53d1\u5149\u3002\u8fd9\u4e9b\u9499\u949b\u77ff\u662f\u901a\u8fc7\u5728\u9499\u949b\u77ff\u524d\u9a71\u4f53\u6eb6\u6db2\u4e2d\u52a0\u5165\u6c28\u57fa\u9178\u6dfb\u52a0\u5242\u800c\u5f62\u6210\u7684\u3002\u6b64\u5916\uff0c\u6dfb\u52a0\u5242\u53ef\u6709\u6548\u949d\u5316\u9499\u949b\u77ff\u8868\u9762\u7f3a\u9677\u5e76\u51cf\u5c11\u975e\u8f90\u5c04\u590d\u5408\u3002\u9499\u949b\u77ffLED\u5177\u670920.7\uff05\u7684\u5cf0\u503c\u5916\u91cf\u5b50\u6548\u7387\uff08\u7535\u6d41\u5bc6\u5ea6\u4e3a18mA\/cm<sup>2<\/sup>\uff09\uff0c\u80fd\u91cf\u8f6c\u6362\u6548\u7387\u4e3a12\uff05\uff08\u572810mA\/cm<sup>2<\/sup>\u7684\u9ad8\u7535\u6d41\u5bc6\u5ea6\u4e0b\uff09\uff0c\u63a5\u8fd1\u6027\u80fd\u6700\u4f73\u7684\u6709\u673aLED\u7684\u4ef7\u503c\u3002\u76f8\u5173\u6210\u679c\u4ee5\u9898\u4e3a\u201c<strong><b>Perovskite light-emitting diodes based on spontaneously formed submicrometre-scale structures<\/b><\/strong>\u201d\u53d1\u8868\u5728\u4e86<strong><b>Nature<\/b><\/strong>\u4e0a\u3002<\/p>\n<p><strong><b>\u6587\u732e\u94fe\u63a5<\/b><\/strong><strong><b>\uff1a<\/b><\/strong><a href=\"https:\/\/www.nature.com\/articles\/s41586-018-0576-2\" target=\"_blank\" rel=\"noopener\"><u>Perovskite<\/u><u>\u00a0<\/u><u>light-emitting<\/u><u>\u00a0<\/u><u>diodes<\/u><u>\u00a0<\/u><u>based<\/u><u>\u00a0<\/u><u>on<\/u><u>\u00a0<\/u><u>spontaneously<\/u><u>\u00a0<\/u><u>formed<\/u><u>\u00a0<\/u><u>submicrometre-scale<\/u><u>\u00a0<\/u><u>structures<\/u><\/a>\uff08Nature,2018,DOI\uff1a10.1038\/s41586-018-0576-2\uff09<\/p>\n<p>4.\u8bba\u6587\uff1a\u901a\u8fc7\u5206\u5b50\u81ea\u7ec4\u88c5\u589e\u5f3a\u8d85\u957f\u6709\u673a\u78f7\u5149\u6750\u6599\u7684\u53d1\u5149\u6548\u7387\u548c\u78f7\u5149\u5bff\u547d<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-149694\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/revised1-1.jpg\" alt=\"\" width=\"600\" height=\"250\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/revised1-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/revised1-1-300x125.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\u9ec4\u7ef4\u9662\u58eb<\/b><\/strong>\u548c<strong><b>\u5b89\u4f17\u798f\u6559\u6388\uff08\u5171\u540c\u901a\u8baf\uff09<\/b><\/strong>\u901a\u8fc7\u4e09\u805a\u6c30\u80fa\u548c\u82b3\u9999\u7fa7\u57fa\u5728\u6c34\u6eb6\u6db2\u4e2d\u7684\u81ea\u7ec4\u88c5\u5236\u5907\u4e86\u8d85\u957f\u6709\u673a\u78f7\u5149\u6750\u6599\u3002\u901a\u8fc7\u591a\u79cd\u5206\u5b50\u95f4\u76f8\u4e92\u4f5c\u7528\u5f62\u6210\u7684\u8d85\u5206\u5b50\u6846\u67b6\uff0c\u53ef\u4ee5\u6784\u5efa\u521a\u6027\u5f88\u5f3a\u7684\u4e09\u7ef4\u7f51\u7edc\u5c06\u539f\u5b50\u56fa\u5b9a\u5728\u5176\u4e2d\uff0c\u5728\u6709\u6548\u51cf\u5c11\u4e09\u7ebf\u6001\u7535\u5b50\u975e\u8f90\u5c04\u8dc3\u8fc1\u7684\u540c\u65f6\uff0c\u4fc3\u8fdb\u7cfb\u95f4\u7a9c\u8d8a\u3002\u6240\u83b7\u5f97\u8d85\u5206\u5b50\u6709\u673a\u6846\u67b6\u53ef\u5b9e\u73b0\u957f\u8fbe1.91\u79d2\u7684\u53d1\u5149\u5bff\u547d\u548c24.3%\u7684\u78f7\u5149\u91cf\u5b50\u6548\u7387\u3002\u8be5\u6210\u679c\u4ee5\u9898\u4e3a&#8221;<strong><b>Simultaneously Enhancing Efficiency and Lifetime of Ultralong Organic Phosphorescence Materials by Molecular Self-assembly<\/b><\/strong>&#8220;\u53d1\u8868\u5728<strong><b>J. Am. Chem. Soc.<\/b><\/strong>\u4e0a\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><\/p>\n<p><a href=\"https:\/\/pubs.acs.org\/doi\/pdf\/10.1021\/jacs.8b03867\" target=\"_blank\" rel=\"noopener\">Simultaneously Enhancing Efficiency and Lifetime of Ultralong Organic Phosphorescence Materials by Molecular Self-assembly<\/a><\/p>\n<p>\u00a0(J. Am. Chem. Soc., 2018, DOI: 10. 1021\/jacs.8b03867)<\/p>\n<p>5.\u8bba\u6587\uff1a\u94c5\u5364\u5316\u7269\u9499\u949b\u77ff\u5728\u7535\u81f4\u53d1\u5149\u7684\u65b0\u8fdb\u5c55<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-69382 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/03\/1-6.jpg\" width=\"600\" height=\"468\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/03\/1-6.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/03\/1-6-300x234.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u65b0\u52a0\u5761\u5357\u6d0b\u7406\u5de5\u5927\u5b66\u7684\u5c91\u5b50\u5065\u6559\u6388<\/strong>\u548c<strong>\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\u7684\u9ec4\u7ef4\u6559\u6388\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u8fd1\u65e5\u5728NATURE COMMUNICATIONS\u4e0a\u53d1\u8868\u4e86\u9898\u4e3aTranscending the slow bimolecular recombination in lead-halide perovskites for electroluminescence\u7684\u6587\u7ae0\uff0c\u62a5\u5230\u4e86\u4ed6\u4eec\u5728\u94c5\u5364\u5316\u7269\u9499\u949b\u77ff\u4e0a\u7684\u6700\u65b0\u8fdb\u5c55\u3002\u4ece\u5fae\u89c2\u8f7d\u6d41\u5b50\u52a8\u529b\u5b66\u89d2\u5ea6\u6e05\u6670\u9610\u660e\u4e86\u5e38\u89c4\u91d1\u5c5e\u5364\u5316\u7269\u9499\u949b\u77ff\u6750\u6599\u8fd0\u7528\u5728\u53d1\u5149\u4e8c\u6781\u7ba1\u4e2d\u5b58\u5728\u7684\u53d1\u5149\u6548\u7387\u74f6\u9888\u3002\u901a\u8fc7\u98de\u79d2\u8d85\u5feb\u5149\u8c31\u7814\u7a76\uff0c\u63d0\u51fa\u5982\u4f55\u901a\u8fc7\u8c03\u63a7\u9499\u949b\u77ff\u7684\u7ef4\u5ea6\u6765\u514b\u670d\u8fd9\u4e2a\u673a\u7406\u4e0a\u7684\u74f6\u9888\uff0c\u4ece\u800c\u5b9e\u73b0\u9ad8\u6548\u7387\u7684\u9499\u949b\u77ff\u53d1\u5149\u4e8c\u6781\u7ba1\u3002\u8be5\u7814\u7a76\u6210\u679c\u4e3a\u5b9e\u73b0\u9ad8\u6548\u4f4e\u6210\u672c\u7684\u65b0\u578b\u9499\u949b\u77ff\u53d1\u5149\u4e8c\u6781\u7ba1\u5960\u5b9a\u4e86\u7406\u8bba\u57fa\u7840\u3002<\/p>\n<p><strong>\u539f\u6587\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/www.nature.com\/articles\/ncomms14558\" target=\"_blank\" rel=\"noopener\">Transcending the slow bimolecular recombination in lead-halide perovskites for electroluminescence<\/a>(Nat. Commun., 2017\uff0cDoi:10.1038\/ncomms14558)<\/p>\n<p>6.\u8bba\u6587\uff1a\u901a\u8fc7\u5206\u5b50\u5c42\u5185\u03c0-\u03c0\u76f8\u4e92\u4f5c\u7528\u6784\u5efa\u6c22\u952e\u6709\u673a\u82b3\u9999\u9aa8\u67b6\u7528\u4e8e\u83b7\u5f97\u8d85\u957f\u78f7\u5149<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-130113\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/revised-1-2.jpg\" alt=\"\" width=\"600\" height=\"600\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/revised-1-2.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/revised-1-2-150x150.jpg 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/03\/revised-1-2-300x300.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u5357\u4eac\u5de5\u4e1a\u5927\u5b66<\/b><\/strong><strong><b>\u9ec4\u7ef4\u9662\u58eb<\/b><\/strong>\u548c<strong><b>\u5b89\u4f17\u798f<\/b><\/strong>\u8bfe\u9898\u7ec4\uff0c\u901a\u8fc7\u5206\u5185\u5b50\u5c42\u03c0-\u03c0\u76f8\u4e92\u4f5c\u7528\u6210\u529f\u6784\u5efa\u51fa\u5177\u6709\u4e0d\u540c\u5b54\u5f84\u7684\u6c22\u952e\u6709\u673a\u82b3\u9999\u9aa8\u67b6\uff08HOAFs\uff09\u3002\u6240\u5236\u5907\u7684HOAFs\u9996\u6b21\u5728\u5ba4\u6e29\u7a7a\u6c14\u4e2d\u5b9e\u73b0\u4e86\u8d85\u957f\u6709\u673a\u78f7\u5149\u53d1\u5149\uff0c\u4e5f\u5c31\u662f\u6709\u673a\u957f\u4f59\u8f89\u53d1\u5149\u3002\u5176\u4e2d\uff0cPhTCz-1\u7684\u9ec4\u8272\u8367\u5149\u5bff\u547d\u8fbe79.8\u00a0ms\uff0c\u5728\u505c\u6b62\u6fc0\u53d1\u540e\u53ef\u89c2\u5bdf\u5230\u6301\u7eed\u51e0\u79d2\u957f\u4f59\u8f89\u53d1\u5149\u3002\u800cPhTCz-2\u548cPhTCz-3\uff0c\u7531\u4e8e\u6c27\u6c14\u7684\u731d\u706d\u4f5c\u7528\uff0c\u5176\u957f\u4f59\u8f89\u73b0\u8c61\u53ea\u80fd\u5728\u6c2e\u6c14\u4e2d\u89c2\u5bdf\u5230\uff0c\u9274\u4e8e\u6b64\u7279\u6027\u53ef\u88ab\u7528\u6765\u68c0\u6d4b\u6c27\u6c14\u3002\u8be5\u5de5\u4f5c\u62d3\u5c55\u4e86\u65e0\u91d1\u5c5e\u6709\u673a\u78f7\u5149\u6750\u6599\u7684\u4f53\u7cfb\u3002\u540c\u65f6\uff0c\u8be5\u7c7b\u65b0\u578b\u7684HOAFS\u6750\u6599\u8fd8\u6709\u9ad8\u7684\u70ed\u5206\u89e3\u6e29\u5ea6\uff0c\u8fd9\u4e5f\u4e3a\u8bbe\u8ba1\u65b0\u578b\u9ad8\u6e29\u7a33\u5b9a\u7684HOFs\u63d0\u4f9b\u4e86\u65b0\u7684\u601d\u8def\u3002\u8be5\u6210\u679c\u4ee5\u9898\u4e3a&#8221;<strong><b>Hydrogen-Bonded Organic Aromatic Frameworks for Ultralong Phosphorescence by Intralayer <\/b><\/strong><strong><b>\u03c0-\u03c0<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><strong><b>Interactions<\/b><\/strong>&#8220;\u53d1\u8868\u5728<strong><b>Angew. Chem. Int. Ed.<\/b><\/strong>\u4e0a\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/anie.201800697\/epdf\" target=\"_blank\" rel=\"noopener\">Hydrogen-Bonded Organic Aromatic Frameworks for Ultralong Phosphorescence by Intralayer \u03c0-\u03c0\u00a0Interactions.<\/a> (Angew. Chem. Int. Ed., 2018,\u00a0DOI: 10.1002\/anie.201800697)<\/p>\n<p>7.\u8bba\u6587\uff1a\u7528\u4e8e\u591a\u8272\u55b7\u58a8\u53ef\u590d\u7528\u7eb8\u4e2d\u7684\u6d3b\u6027\u91d1\u5c5e\u914d\u4f53\u914d\u5408\u7269\u7684\u7814\u7a76<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-121479\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/1-23.jpg\" alt=\"\" width=\"600\" height=\"386\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/1-23.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/1-23-300x193.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u897f\u5317\u5de5\u4e1a\u5927\u5b66\u9ec4\u7ef4\u9662\u58eb<\/strong>\uff0c<strong>\u5357\u4eac\u90ae\u7535\u5927\u5b66\u8d75\u5f3a\u6559\u6388<\/strong>(<strong>\u5171\u540c\u901a\u8baf\u4f5c\u8005<\/strong>)\u5728<strong>Nat. Commun.<\/strong>\u4e0a\u53d1\u8868\u4e86\u9898\u4e3a\u201c<strong>Dynamic metal-ligand coordination for multicolour and water-jet rewritable pape<\/strong>r\u201d\u7684\u6587\u7ae0\u3002\u7814\u7a76\u5e76\u63a2\u8ba8\u4e86\u5982\u4f55\u5229\u7528\u52a8\u6001\u91d1\u5c5e\u914d\u4f53\u76f8\u4e92\u4f5c\u7528\u7684\u53ef\u9006\u6027\u6765\u5b9e\u73b0\u53ef\u64e6\u5199\u7eb8\u7684\u5236\u5907\uff0c\u5e76\u7a81\u7834\u4e86\u76ee\u524d\u7684\u9650\u5236\u3002\u7814\u7a76\u4e86\u542b\u6709\u4e09\u8054\u5421\u5576\u914d\u4f53\u7684\u805a\u5408\u7269\u8584\u819c\u5728\u6ee4\u7eb8\u4e0a\u7684\u6d82\u5c42\uff0c\u5176\u4e0a\u53ef\u4ee5\u4f7f\u7528\u4e0d\u540c\u7684\u91d1\u5c5e\u76d0\u6c34\u6eb6\u6db2\uff08MSAS\uff09\u4f5c\u4e3a\u53ef\u4e0e\u914d\u4f53\u914d\u4f4d\u7684\u6cb9\u58a8\u91cd\u590d\u6d82\u8986\u591a\u8272\u56fe\u50cf\uff0c\u7ed3\u679c\u53d1\u73b0\u6253\u5370\u7684\u56fe\u7247\u53ef\u4ee5\u4fdd\u75596\u4e2a\u6708\u4ee5\u4e0a\uff0c\u7528\u56db\u4e01\u57fa\u6c1f\u5316\u94f5\uff08TBAF\uff09\u53ef\u4ee5\u65b9\u4fbf\u5730\u64e6\u9664\u91d1\u5c5e &#8211; \u914d\u4f53\u914d\u4f4d\u952e\u3002\u901a\u8fc7\u5c06\u6c34\u54cd\u5e94\u578b\u53d1\u5149\u950c\u7edc\u5408\u7269\u5f15\u5165\u6210\u50cf\u5c42\u4e2d\uff0c\u5236\u9020\u4e86\u53e6\u4e00\u79cd\u53ef\u4ee5\u901a\u8fc7\u4f7f\u7528\u7eaf\u6c34\u4f5c\u4e3a\u58a8\u6c34\u6765\u8bb0\u5f55\u4fe1\u606f\u7684\u53ef\u590d\u5199\u7eb8\u5f20\uff0c\u6c34\u662f\u4e00\u79cd\u7eff\u8272\u8d44\u6e90\uff0c\u56e0\u6b64\u5f00\u53d1\u6c34\u55b7\u5370\u53ef\u64e6\u5199\u7eb8\u5177\u6709\u91cd\u8981\u610f\u4e49\uff0c\u6b64\u5e94\u7528\u5c06\u662f\u5b9e\u73b0\u5177\u6709\u957f\u4fdd\u7559\u65f6\u95f4\u7684\u591a\u8272\u6c34\u55b7\u5370\u7684\u6709\u5e0c\u671b\u7684\u65b9\u6cd5\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/www.nature.com\/articles\/s41467-017-02452-w\" target=\"_blank\" rel=\"noopener\">Dynamic metal-ligand coordination for multicolour and water-jet rewritable paper<\/a><\/strong>\uff08Nat. Commun., 2017,DOI: 10.1038\/s41467-017-02452-w\uff09<\/p>\n<p>8.\u8bba\u6587\uff1a\u65e0\u540e\u5904\u7406\u3001\u65e0\u63ba\u6742\u4e8c\u82b3\u57fa\u82b4\u7c7b\u7eb3\u7c73\u5206\u5b50\u4f5c\u4e3a\u67d4\u6027p-i-n\u578b\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u7684\u7a7a\u7a74\u4f20\u8f93\u6750\u6599<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-121212\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/10.1016@j.nanoen.2018-02.png\" alt=\"\" width=\"600\" height=\"424\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/10.1016@j.nanoen.2018-02.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/01\/10.1016@j.nanoen.2018-02-300x212.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\u9ec4\u7ef4\u6559\u6388<\/strong><strong>(<\/strong><strong>\u901a\u8baf\u4f5c\u8005<\/strong><strong>)<\/strong>\u7b49\u4eba\u5728<strong>Nano Energy<\/strong> \u4e0a\u53d1\u8868\u9898\u4e3a\u201c<strong>Diarylfluorene-based Nano-molecules as Dopant-Free Hole-transporting Materials without Post-treatment Process for Flexible p-i-n Type Perovskite Solar Cells<\/strong>\u201d\u7684\u6587\u7ae0\u3002\u7814\u7a76\u56e2\u961f\u8bbe\u8ba1\u4e86\u4e24\u7ec4\u4e8c\u82b3\u57fa\u82b4\u7c7bHTM\uff0cTPA\u6216\u80059-NPC\u4f5c\u4e3a\u94fe\u81c2\uff0cC8\u6216\u8005C6Cz\u4e3a\u4fa7\u94fe\uff0c\u5206\u522b\u547d\u540d\u4e3aMC8-TPA, MC8-9-NPC\uff0cMC6Cz-TPA\u548cMC6Cz-9-NPC\u3002\u8fd9\u4e9b\u6750\u6599\u5728\u666e\u901a\u6709\u673a\u6eb6\u5242\u4e2d\u6709\u5f88\u597d\u7684\u6eb6\u89e3\u6027\uff0c\u65cb\u6d82\u800c\u6210\u7684\u8584\u819c\u754c\u9762\u5149\u6ed1\uff0c\u758f\u6c34\u6027\u597d\uff0c\u5728ITO\u4e0a\u4e0d\u9700\u540e\u7eed\u70ed\u5904\u7406\u5373\u8868\u73b0\u5b8c\u5168\u7ed3\u6676\u6001\u3002\u5728\u4e8c\u82b3\u57fa\u82b4\u7c7bHTM\u4e0a\u5236\u5907\u7684\u9499\u949b\u77ff\u8584\u819c\u6bd4\u5728PEDOT:PSS\u4e0a\u7684\u6676\u7c92\u66f4\u5927\uff0c\u7ea6\u4e3a300nm\u3002\u5668\u4ef6\u7684\u6700\u9ad8\u6548\u7387\u8fbe\u523013.85%\uff0c\u67d4\u6027\u9499\u949b\u77ff\u7535\u6c60\u6700\u9ad8\u6548\u7387\u4e3a9.09%\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/www.sciencedirect.com\/science\/article\/pii\/S2211285518300065\" target=\"_blank\" rel=\"noopener\">Diarylfluorene-based Nano-molecules as Dopant-Free Hole-transporting Materials without Post-treatment Process for Flexible p-i-n Type Perovskite Solar Cells<\/a>\uff08Nano Energy,2017,DIO:10.1016\/j.nanoen.2018.01.005)<\/p>\n<p>9.\u8bba\u6587\uff1a\u6cbe\u4e0a\u6c34\u80fd\u53d1\u5149\u7684\u4e8c\u7ef4\u67d4\u6027\u663e\u793a\u5668<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-102594\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/09\/\u99761.jpg\" alt=\"\" width=\"600\" height=\"490\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/09\/\u99761.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/09\/\u99761-300x245.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u5357\u4eac\u5de5\u4e1a\u5927\u5b66<\/strong><strong>\u9ec4\u7ef4<\/strong><strong>\u9662\u58eb<\/strong><strong>\uff0c\u5317\u4eac\u5927\u5b66\u6df1\u5733\u7814\u7a76\u9662\u5b5f\u9e3f\u6559\u6388\u548c\u5fb7\u514b\u8428\u65af\u5927\u5b66\u8fbe\u62c9\u65af\u5206\u6821<\/strong><strong>Ray H. Baughman<\/strong><strong>\u6559\u6388\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\u4e0d\u533a\u5206\u987a\u5e8f\uff09<\/strong>\u7b49\u4eba\u7814\u7a76\u4e86\u4e00\u79cd\u57fa\u4e8e\u6781\u5316\u7535\u6781\u6865\u63a5\u7684\u67d4\u6027\u663e\u793a\u5668\uff0c\u6784\u5efa\u4e86\u5229\u7528\u5149\u4fe1\u53f7\u7684\u8fdc\u8ddd\u79bb\u611f\u5e94\u5668\u3002\u8be5\u7814\u7a76\u53d1\u8868\u4e8e <strong>Advanced Materials<\/strong>, \u9898\u4e3a <strong>\u201cPolar-Electrode-Bridged Electroluminescent Displays: 2D Sensors Remotely Communicating Optically\u201d<\/strong>\u3002\u7814\u7a76\u4eba\u5458\u8bbe\u8ba1\u4e86\u4e00\u79cd\u65b0\u578b\u7ed3\u6784\u7684\u53d1\u5149\u5668\u4ef6\uff0c\u8fd9\u79cd\u5668\u4ef6\u4e3b\u8981\u7531\u56db\u4e2a\u90e8\u5206\u6784\u6210\uff0c\u5206\u522b\u662f\uff0c\u4e00\u5bf9\u5e73\u884c\u53e0\u52a0\u6216\u8005\u5e76\u6392\u5206\u5e03\u7684\u7535\u6781\uff0c\u53d1\u5149\u5c42\uff0c\u4ecb\u7535\u5c42\u4ee5\u53ca\u4e00\u4e2a\u53ef\u8c03\u63a7\u7684\u7535\u6781\u5c42\u3002\u901a\u8fc7\u9009\u62e9\u4e0d\u540c\u7684\u6781\u5316\u6750\u6599\u6216\u8005\u5bfc\u7535\u8584\u819c\uff0c\u5b9e\u73b0\u4e86\u8be5\u7535\u6781\u5c42\u7684\u53ef\u63a7\u3002\u8fd9\u79cd\u65b0\u578b\u7ed3\u6784\u4e0d\u4ec5\u7b80\u5355\uff0c\u5229\u4e8e\u5927\u89c4\u6a21\u5236\u9020\uff0c\u66f4\u4e3a\u91cd\u8981\u7684\u662f\uff0c\u4e0e\u4f20\u7edf\u610f\u4e49\u4e0a\u7684\u53d1\u5149\u5668\u4ef6\u76f8\u6bd4\uff0c\u4e00\u5bf9\u76f8\u53cd\u7684\u7535\u6781\u4e0d\u518d\u662f\u4e92\u76f8\u5806\u53e0\uff0c\u800c\u662f\u5e76\u6392\u5206\u5e03\u3002\u6b63\u662f\u7531\u4e8e\u8fd9\u79cd\u7ed3\u6784\u4e0a\u7684\u4f18\u52bf\uff0c\u7814\u7a76\u8005\u4eec\u8bbe\u8ba1\u51fa\u4e86\u4e0d\u540c\u79cd\u7c7b\u7684\u5668\u4ef6\u3002\u4f8b\u5982\uff0c\u5c06\u8fd9\u79cd\u67d4\u6027\u6750\u6599\u5b89\u88c5\u5728\u96e8\u4f1e\u4e0a\uff0c\u5f53\u6c34\u843d\u5728\u96e8\u4f1e\u4e0a\uff0c\u96e8\u4f1e\u5c31\u4f1a\u53d1\u5149\uff0c\u8fd9\u4e5f\u4e3a\u6784\u5efa\u5229\u7528\u5149\u4fe1\u53f7\u53d8\u5316\u7684\u8fdc\u7a0b\u63a2\u6d4b\u5668\u63d0\u4f9b\u4e86\u53ef\u80fd\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adma.201703552\/full\" target=\"_blank\" rel=\"noopener\">Polar-Electrode-Bridged Electroluminescent Displays: 2D Sensors Remotely Communicating Optically<\/a>\uff08Adv. Mater., 2017, DOI: 10.1002\/adma.201703552\uff09<\/p>\n<p>10.\u8bba\u6587\uff1a\u901a\u8fc7\u8c03\u8282\u5206\u5b50\u95f4\u76f8\u4e92\u4f5c\u7528\u5b9e\u73b0\u53ef\u89c1\u5149\u6fc0\u53d1\u7684\u8d85\u957f\u6709\u673a\u78f7\u5149<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-93018\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/2-15.png\" alt=\"\" width=\"600\" height=\"437\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/2-15.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/07\/2-15-300x219.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\u9ec4\u7ef4\u9662\u58eb\u548c\u5b89\u4f17\u798f\u7814\u7a76\u5458\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u4f7f\u7528\u7b80\u660e\u7684\u5316\u5b66\u65b9\u6cd5\uff0c\u5728\u53ef\u89c1\u5149\u7167\u5c04\u4e0b\u7684\u56fa\u4f53\u4e2d\uff0c\u901a\u8fc7\u8c03\u8282\u5206\u5b50\u5e8f\u5217\u6765\u83b7\u5f97\u660e\u4eae\u7684UOP\uff0c\u4f8b\u5982\u624b\u673a\u624b\u7535\u7b52\u3002\u901a\u8fc7\u63ba\u5165\u5364\u7d20\u539f\u5b50\u8c03\u8282\u5206\u5b50\u95f4\u76f8\u4e92\u4f5c\u7528\uff0c\u6fc0\u53d1\u5149\u8c31\u8868\u73b0\u51fa\u660e\u663e\u7684\u7ea2\u79fb\u3002\u7ecf\u8fc7H\u805a\u96c6\u7684UOP\uff0c\u5177\u67098.3\uff05\u7684\u9ad8\u78f7\u5149\u6548\u7387\u548c0.84s\u7684\u5bff\u547d\u3002\u5728\u8089\u773c\u53ef\u4ee5\u8bc6\u522b\u76840.32 mcd m -2\u7684\u4eae\u5ea6\u5185\uff0cUOP\u603b\u5171\u53ef\u6301\u7eed104\u79d2\u3002\u9274\u4e8e\u8fd9\u4e9b\u7279\u70b9\uff0c\u8d85\u957f\u7684\u6709\u673a\u78f7\u5149\u6750\u6599\u53ef\u88ab\u7528\u4e8e\u53cc\u91cd\u6570\u636e\u7684\u52a0\u5bc6\u548c\u89e3\u5bc6\u3002\u6b64\u5916\uff0c\u901a\u8fc7\u805a\u5408\u7269\u57fa\u8d28\u5c01\u88c5\u5728\u6c34\u6eb6\u6db2\u4e2d\u5206\u6563\u7684UOP\u7eb3\u7c73\u9897\u7c92\uff0c\u5e76\u4e14\u7814\u7a76\u4e86\u5b83\u4eec\u5728\u751f\u7269\u6210\u50cf\u4e2d\u7684\u5e94\u7528\u3002\u8fd9\u4e00\u7ed3\u679c\u5c06\u4e3a\u65e0\u91d1\u5c5e\u6709\u673a\u78f7\u5149\u6750\u6599\u53ca\u5176\u5e94\u7528\u94fa\u8def\u3002\u8be5\u6210\u679c\u4ee5<strong>\u201cVisible-Light-Excited Ultralong Organic Phosphorescence by Manipulating Intermolecular Interactions\u201d<\/strong>\u4e3a\u9898\u4e8e2017\u5e747\u670817\u65e5\u53d1\u8868\u5728\u671f\u520a<strong>Advanced Materials<\/strong>\u4e0a\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong>Cai S, Shi H, Li J, et al. Visible\u2010Light\u2010Excited Ultralong Organic Phosphorescence by Manipulating Intermolecular Interactions[J]. Advanced Materials, 2017.<\/p>\n<p>11.\u8bba\u6587\uff1a\u5229\u7528\u76f8\u4e92\u6269\u6563\u8f85\u52a9\u590d\u5408\u4e8c\u7ef4MOF\u548cTi3C2Tx\u7eb3\u7c73\u8584\u7247\u7528\u4e8e\u7535\u50ac\u5316\u6790\u6c27\u53cd\u5e94<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-84246 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/nn-2017-014093_0001.jpeg\" alt=\"\" width=\"600\" height=\"288\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/nn-2017-014093_0001.jpeg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/05\/nn-2017-014093_0001-300x144.jpeg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>ACS Nano<\/strong><strong>\u00a0<\/strong>\u520a\u767b\u4e86\u4e00\u7bc7\u9898\u4e3a<strong>\u201cInterdiffusion Reaction-Assisted Hybridization of Two-Dimensional Metal\u2212Organic Frameworks and Ti<sub>3<\/sub>C<sub>2<\/sub>T<sub>x<\/sub><\/strong><strong>\u00a0<\/strong><strong>Nanosheets for Electrocatalytic Oxygen Evolution\u201d<\/strong>\u7684\u6587\u7ae0\uff0c\u62a5\u9053\u4e86<strong>\u5357\u4eac\u90ae\u7535\u5927\u5b66\u674e\u7ecd\u5468\u6559\u6388\u3001\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\u9ec4\u7ef4\u6559\u6388\u3001\u9ec4\u6653\u6559\u6388\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba<\/strong>\uff0c\u8fd0\u7528\u5185\u90e8\u6269\u6563\u76f8\u8f85\u52a9\u7684\u8fc7\u7a0b\u539f\u4f4d\u5408\u6210CoBDC\uff0c\u5e76\u5c06Ti3C2Tx \u7eb3\u7c73\u7247\u4e0e\u4e4b\u590d\u5408\u3002\u5c06\u5f97\u5230\u7684\u590d\u5408\u6750\u6599\u5e94\u7528\u4e8e\u7535\u5316\u5b66\u6790\u6c27\u53cd\u5e94(OER)\u4e2d\uff0c\u57280.1M KOH\u7684\u7535\u89e3\u6db2\u4e0b\uff0c\u76f8\u5bf9\u4e8e\u53ef\u9006\u6c22\u7535\u6781\u57281.64V\u7535\u52bf\u4e0b\u80fd\u8fbe\u5230\u7535\u6d41\u5bc6\u5ea6\u4e3a10mA cm<sup>\u2212<\/sup><sup>2<\/sup> \u53ca\u5854\u83f2\u5c14\u659c\u7387\u4e3a48.2mV dec<sup>&#8211;<\/sup><sup>1<\/sup>\u3002\u8fd9\u4e9b\u6027\u80fd\u8d85\u51fa\u90a3\u4e9b\u57fa\u4e8e IrO<sub>2<\/sub>\u7684\u50ac\u5316\u5242\u751a\u81f3\u6bd4\u6b64\u524d\u62a5\u9053\u7684\u66f4\u5148\u8fdb\u7684\u57fa\u4e8e\u8fc7\u6e21\u91d1\u5c5e\u7684\u50ac\u5316\u5242\u3002\u7531\u4e8eCoBDC\u5c42\u63d0\u4f9b\u591a\u5b54\u7ed3\u6784\u548c\u8f83\u5927\u7684\u6d3b\u6027\u8868\u9762\u79ef\u4e14Ti3C2Tx\u7eb3\u7c73\u7247\u7684\u4f18\u826f\u7684\u7535\u5bfc\u6027\u548c\u4eb2\u6c34\u6027\u4f7f\u5f97\u7535\u8377\u548c\u79bb\u5b50\u5728\u590d\u5408\u5f97\u5230\u7684Ti<sub>3<\/sub>C<sub>2<\/sub>T<sub>x<\/sub>\u2212CoBDC\u754c\u9762\u4e0a\u5feb\u901f\u4f20\u9012\u3002\u540c\u65f6\u4e5f\u4fbf\u4e8e\u6c34\u6027\u7535\u89e3\u6db2\u63a5\u8fd1\u50ac\u5316\u7684\u6d3b\u6027CoBDC\u8868\u9762\u3002\u8fd9\u79cd\u7eb3\u7c73\u8584\u7247\u8fdb\u4e00\u6b65\u7ec4\u88c5\u5230\u7a7a\u6c14\u9634\u6781\u5f62\u6210\u53ef\u5145\u7535\u7684\u950c-\u7a7a\u6c14\u7535\u6c60\uff0c\u5e76\u6210\u529f\u5e26\u52a8LED\u53d1\u5149\u3002<\/p>\n<p><span style=\"color: #000000;\"><strong>\u6587\u732e\u94fe\u63a5\uff1a<\/strong><span style=\"color: #0000ff;\"><a style=\"color: #0000ff;\" href=\"http:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acsnano.7b01409\" target=\"_blank\" rel=\"noopener noreferrer\">Interdiffusion Reaction-Assisted Hybridization of Two-Dimensional Metal\u2212Organic Frameworks and Ti3C2Tx Nanosheets for Electrocatalytic Oxygen Evolution<\/a><\/span>\uff08ACS Nano, \u00a02017, DOI: 10.1021\/acsnano.7b01409\uff09<\/span><\/p>\n<p>12.\u8bba\u6587\uff1a\u4e00\u79cd\u9ad8\u6548\u7684\u7ea2\u5149LED-\u57fa\u4e8e\u6e7f\u6cd5\u52a0\u5de5\u7684\u591a\u91cf\u5b50\u9631\u9499\u949b\u77ff\u6750\u6599<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-77167\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/adma201606600-fig-0001.png\" alt=\"\" width=\"500\" height=\"154\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/adma201606600-fig-0001.png 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/04\/adma201606600-fig-0001-300x92.png 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p>\u6765\u81ea<strong>\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\u7684\u9ec4\u7ef4\u548c<\/strong><strong>\u738b\u5efa\u6d66\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u7528\u4e00\u79cd\u7b80\u5355\u53ef\u6269\u5c55\u7684\u65b9\u6cd5\u6210\u529f\u5236\u5907\u51fa\u4e86\u7eaf\u7ea2\u5149\u9ad8\u6548\u9499\u949b\u77ff\u53d1\u5149\u5668\u4ef6\uff0c\u5927\u5927\u63a8\u52a8\u4e86\u6709\u673a\u91d1\u5c5e\u5364\u5316\u7269\u9499\u949b\u77ff\u53d1\u5149\u4e8c\u6781\u7ba1\u7684\u5e94\u7528\u3002<\/p>\n<p>\u7814\u7a76\u4eba\u5458\u628a\u65e0\u673a\u5c0f\u9633\u79bb\u5b50Cs\u5f15\u5165\u5230\u591a\u91cf\u5b50\u9631\u7ed3\u6784\u7684\u9499\u949b\u77ff\u8584\u819c\u4e2d\uff0c\u4ece\u800c\u5236\u5907\u51fa\u7eaf\u7ea2\u5149\u9ad8\u6548\u9499\u949b\u77ff\u53d1\u5149\u5668\u4ef6\u3002\u591a\u91cf\u5b50\u52bf\u9631\u7ed3\u6784\u4e0d\u4ec5\u6709\u5229\u4e8e\u7acb\u65b9CsPbBr<sub>3<\/sub>\u9499\u949b\u77ff\u7ed3\u6784\u5728\u4f4e\u6e29\u4e0b\u7684\u5efa\u7acb\uff0c\u8fd8\u80fd\u591f\u8ba9Cs\u57fa\u591a\u91cf\u5b50\u52bf\u9631\u63d0\u4f9b\u7eaf\u51c0\u7a33\u5b9a\u7684\u7ea2\u8272\u7535\u81f4\u53d1\u5149\u3002\u8fd9\u79cd\u901a\u7528\u7684\u5236\u5907\u591a\u91cf\u5b50\u52bf\u9631\u9499\u949b\u77ff\u6750\u6599\u7684\u65b9\u6cd5\uff0c\u80fd\u591f\u8ba9\u63a7\u5236\u53d1\u5c04\u5c42\u7684\u7ed3\u6676\u5ea6\u548c\u5f62\u8c8c\u6709\u5f88\u9ad8\u7684\u81ea\u7531\u5ea6\u3002\u5668\u4ef6\u4e2d\u5305\u542b\u7684\u6c2f\u5316\u7269\u80fd\u8fdb\u4e00\u6b65\u63d0\u9ad8Cs\u57fa\u9499\u949b\u77ff\u591a\u91cf\u5b50\u52bf\u9631\u7684\u7ed3\u6676\u5ea6\u548c\u5149\u5b66\u6027\u80fd\uff0c\u8ba9\u5668\u4ef6\u5177\u6709\u4f4e\u7684\u5f00\u5173\u7535\u538b\uff082v\uff09, \u9ad8\u7684\u5916\u91cf\u5b50\u6548\u7387\uff08\u6700\u59273.7%\uff09\uff0c\u9ad8\u7684\u4eae\u5ea6\uff084v\u7535\u538b\u4e0b\u7ea6\u4e3a440 cd m<strong><sup>\u2212<\/sup><\/strong><sup>2<\/sup>\uff09\u3002\u8fd9\u4e9b\u6027\u80fd\u6d4b\u8bd5\u7ed3\u679c\u663e\u793aCs\u57fa\u9499\u949b\u77ff\u591a\u91cf\u5b50\u52bf\u9631LED\u662f\u6027\u80fd\u6700\u4f18\u7684\u7ea2\u5149\u9499\u949b\u77ffLED\u3002\u800c\u4e14\u8be5\u9499\u949b\u77ffLED\u5177\u6709\u521b\u7eaa\u5f55\u7684\u7a33\u5b9a\u6027\uff0c\u572810 mA cm<strong><sup>\u2212<\/sup><\/strong><sup>2<\/sup>\u6052\u5b9a\u7535\u6d41\u5bc6\u5ea6\u4e0b\u5668\u4ef6\u7684\u5bff\u547d\u8d85\u8fc75\u4e2a\u5c0f\u65f6\u3002\u7814\u7a76\u4eba\u5458\u7684\u76f8\u5173\u5de5\u4f5c\u663e\u793a\u591a\u91cf\u5b50\u52bf\u9631\u9499\u949b\u77ff\u6750\u6599\u5728\u7528\u5927\u89c4\u6a21\u751f\u4ea7\u5236\u5907\u51fa\u53ef\u89c1\u5149\u8303\u56f4\u9ad8\u6027\u80fdLED\u4e0a\u5177\u6709\u5de8\u5927\u6f5c\u529b\uff0c\u8fd9\u5bf9\u4f4e\u6210\u672c\u7167\u660e\u548c\u663e\u793a\u9886\u57df\u6709\u5de8\u5927\u5438\u5f15\u529b\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong><strong>\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adma.201606600\/full\" target=\"_blank\" rel=\"noopener\">Efficient Red Perovskite Light-Emitting Diodes Based on Solution-Processed Multiple Quantum Wells<\/a><\/strong>\uff08Advanced\u00a0 Materials,2017, Doi\/10.1002\/adma.201606600\/full\uff09<\/p>\n<p>13.\u8bba\u6587\uff1a\u8fd8\u539f\u578b\u67d3\u6599\/\u77f3\u58a8\u70ef\u590d\u5408\u6750\u6599\u53ef\u7528\u4f5c\u9ad8\u80fd\u91cf\u9502\u79bb\u5b50\u7535\u6c60\u7684\u6709\u673a\u6b63\u6781\u6750\u6599<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-44150 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72471-30.jpg\" alt=\"\u56fe\u72471\" width=\"500\" height=\"115\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72471-30.jpg 500w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/09\/\u56fe\u72471-30-300x69.jpg 300w\" sizes=\"(max-width: 500px) 100vw, 500px\" \/><\/p>\n<p><strong>\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\u9ec4\u7ef4\u9662\u58eb<\/strong>\u548c<strong>\u5357\u6d0b\u7406\u5de5\u5927\u5b66Ting Yu\u6559\u6388\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09\u7b49<\/strong>\u63d0\u4f9b\u4e86\u4e00\u79cd\u7b80\u5355\u901a\u7528\u7684\u8fd8\u539f\u67d3\u6599\/\u77f3\u58a8\u590d\u5408\u6750\u6599\u5236\u5907\u65b9\u6cd5\u3002\u5c06\u8d85\u58f0\u5904\u7406\u548c\u6c34\u70ed\u6cd5\u76f8\u7ed3\u5408\u53ef\u5236\u5907\u51fa\u591a\u79cd\u8fd8\u539f\u67d3\u6599\/\u77f3\u58a8\u590d\u5408\u6750\u6599\uff0c\u7528\u6765\u505a\u9ad8\u6027\u80fd\u9502\u79bb\u5b50\u7535\u6c60\u6b63\u6781\u6750\u6599\u3002\u4f8b\u5982\uff0c\u901a\u8fc7\u8fd8\u539f\u7eff8\u548c\u77f3\u58a8\u70ef\u7247\u4e4b\u95f4\u7684\u03c0-\u03c0\u76f8\u4e92\u4f5c\u7528\u7814\u7a76\u4eba\u5458\u5f97\u5230\u4e86\u7a33\u5b9a\u7684\u590d\u5408\u7ed3\u6784\uff0c\u5b83\u4e0d\u4ec5\u53ef\u4ee5\u6709\u6548\u5730\u6291\u5236\u6d3b\u6027\u7269\u8d28\u7684\u6eb6\u89e3\u73b0\u8c61\uff0c\u5728\u7535\u5316\u5b66\u53cd\u5e94\u671f\u95f4\u8fd8\u53ef\u4ee5\u4fdd\u8bc1\u7535\u5b50\u7684\u5feb\u901f\u4f20\u8f93\u3002\u56e0\u6b64\uff0c\u8fd8\u539f\u7eff8 \/\u77f3\u58a8\u70ef\uff08VG8 \/ G\uff09\u7684\u590d\u5408\u6750\u6599\u8868\u73b0\u51fa\u826f\u597d\u7684\u5faa\u73af\u7a33\u5b9a\u6027\u548c\u4f18\u5f02\u7684\u9ad8\u500d\u7387\u6027\u80fd\u3002\u8fd9\u79cd\u7b80\u5355\u901a\u7528\u7684\u65b9\u6cd5\u8fd8\u53ef\u4ee5\u7528\u6765\u5236\u5907\u8fd8\u539f\u68d5BR\/\u77f3\u58a8\u70ef\uff08VB BR\/ G\uff09\u548c\u8fd8\u539f\u6a44\u6984T \/\u77f3\u58a8\u70ef\uff08VO T \/ G\uff09\u590d\u5408\u6750\u6599\uff0c\u90fd\u8868\u73b0\u51fa\u4f18\u5f02\u7684\u7535\u5316\u5b66\u6027\u80fd\uff0c\u4e3a\u9ad8\u6027\u80fd\u9502\u79bb\u5b50\u7535\u6c60\u6b63\u6781\u6750\u6599\u7684\u5f00\u53d1\u63d0\u4f9b\u4e86\u65b0\u7684\u65b9\u5411\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>\uff1a<a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adfm.201603603\/full\" target=\"_blank\" rel=\"noopener\">Toward High Energy Organic Cathodes for Li-Ion Batteries:A Case Study of Vat Dye\/Graphene Composites<\/a>\u00a0\uff08Adv. Funct. Mater.\uff0c2016\uff0cDOI: 10.1002\/adfm.201603603\uff09<\/p>\n<p><strong>\u53d1\u8868\u7684\u7efc\u8ff0\uff1a<\/strong><\/p>\n<p>1.\u7efc\u8ff0\uff1a\u9762\u5411\u5927\u9762\u79ef\u9499\u949b\u77ff\u7535\u6c60\u7684\u6750\u6599<\/p>\n<p><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-159894 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72472-14.png\" alt=\"\" width=\"600\" height=\"203\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72472-14.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72472-14-300x102.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-159895 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72473-13.png\" alt=\"\" width=\"600\" height=\"165\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72473-13.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/11\/\u56fe\u72473-13-300x83.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\uff08\u5148\u8fdb\u6750\u6599\u7814\u7a76\u9662\uff09\u9ec4\u7ef4\u9662\u58eb\u3001\u79e6\u5929\u77f3\u6559\u6388\u56e2\u961f<\/b><\/strong>\u5728<strong><em><b><i>Advanced Functional Materials<\/i><\/b><\/em><\/strong>\u6742\u5fd7\u4e0a\u53d1\u8868\u4e86\u9898\u4e3a\u201c<strong><em><b><i>Materials toward the Up-scaling of Perovskite Solar Cells: Progress, Challenges and Strategies<\/i><\/b><\/em><\/strong>\u201d\u7684\u7efc\u8ff0\u6027\u6587\u7ae0\uff0c<strong><b>\u7b2c\u4e00\u4f5c\u8005\u4e3a\u738b\u82b3\u82b3\u526f\u6559\u6388<\/b><\/strong>\u3002\u5728\u8fd9\u7bc7\u7efc\u8ff0\u4e2d\uff0c\u4f5c\u8005\u9996\u5148\u4ecb\u7ecd\u4e86\u9499\u949b\u77ff\u5149\u4f0f\u5668\u4ef6\u548c\u7ec4\u4ef6\u7684\u7ed3\u6784\uff0c\u7136\u540e\u4ece\u5404\u4e2a\u529f\u80fd\u5c42\u6750\u6599\u7684\u89d2\u5ea6\u8be6\u7ec6\u63a2\u8ba8\u4e86\u8fd1\u5e74\u6765\u5927\u9762\u79ef\u9499\u949b\u77ff\u5149\u4f0f\u5668\u4ef6\u7684\u7814\u7a76\u8fdb\u5c55\u3001\u76ee\u524d\u7684\u95ee\u9898\u548c\u89e3\u51b3\u7b56\u7565\uff0c\u5305\u62ec\u9499\u949b\u77ff\u6750\u6599\uff0c\u7a7a\u7a74\u4f20\u8f93\u6750\u6599\uff0c\u7535\u5b50\u4f20\u8f93\u6750\u6599\u548c\u7535\u6781\u6750\u6599\u3002\u6b64\u5916\u8fd8\u5206\u6790\u4e86\u5f71\u54cd\u9499\u949b\u77ff\u5149\u4f0f\u5668\u4ef6\u7a33\u5b9a\u6027\u7684\u51e0\u70b9\u5173\u952e\u56e0\u7d20\u3002\u6700\u540e\u5bf9\u5927\u9762\u79ef\u9499\u949b\u77ff\u5149\u4f0f\u5668\u4ef6\u7684\u53d1\u5c55\u548c\u7b56\u7565\u8fdb\u884c\u4e86\u603b\u7ed3\u548c\u5c55\u671b\u3002\u6587\u4e2d\u5173\u4e8e\u5927\u9762\u79ef\u9499\u949b\u77ff\u7535\u6c60\u4ea7\u4e1a\u5316\u65b9\u9762\u5f97\u5230\u4e86<strong><b>\u5408\u4f5c\u5355\u4f4d\u4eac\u4e1c\u65b9\u79d1\u6280\u96c6\u56e2\u674e\u65b0\u56fd\u3001\u5434\u6653\u535a\u58eb<\/b><\/strong>\u7684\u5efa\u8bae\u3002\u8be5\u8bba\u6587\u4f5c\u8005\u4e3a<strong><b>Fangfang Wang<\/b><\/strong>, Yezhou Cao, Cheng Chen, Qing Chen, Xiao Wu, Xinguo Li, <strong><b>Tianshi Qin<\/b><\/strong>,*and <strong><b>Wei Huang<\/b><\/strong>*<\/p>\n<p>\u6587\u7ae0\u94fe\u63a5\uff1a<a href=\"https:\/\/onlinelibrary.wiley.com\/doi\/full\/10.1002\/adfm.201803753\"><u>https:\/\/onlinelibrary.wiley.com\/doi\/full\/10.1002\/adfm.201803753<\/u><\/a><\/p>\n<p>2.\u7efc\u8ff0\uff1a\u4e8c\u7ef4\u53d1\u5149\u6750\u6599\u7684\u5236\u5907\u3001\u6027\u80fd\u548c\u5e94\u7528<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-149006\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/1-9.jpg\" alt=\"\" width=\"600\" height=\"359\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/1-9.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/08\/1-9-300x180.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u897f\u5317\u5de5\u4e1a\u5927\u5b66\u7684\u9ec4\u7ef4\u9662\u58eb\u4e0e\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\u7684\u9ec4\u6653\u6559\u6388\u3001\u9648\u6c38\u534e\u6559\u6388\uff08\u5171\u540c\u901a\u8baf\uff09<\/strong>\u8054\u5408\u5728Chem. Soc. Rev.\u4e0a\u53d1\u8868\u7efc\u8ff0\u6587\u7ae0\uff0c\u9898\u4e3a\uff1aTwo-dimensional light-emitting materials: preparation, properties and applications\u3002<strong>\u7b2c\u4e00\u4f5c\u8005\u4e3a\u738b\u5fd7\u4f1f\u535a\u58eb\u548c\u4ec7\u6676\u6676\u7855\u58eb\u3002<\/strong>\u4f5c\u8005\u5c06\u4e8c\u7ef4\u53d1\u5149\u6750\u6599\u5f52\u7eb3\u4e3a\u4e09\u5927\u7c7b\uff0c\u5373\u4e8c\u7ef4\u65e0\u673a\u53d1\u5149\u6750\u6599\u3001\u4e8c\u7ef4\u6709\u673a\u53d1\u5149\u6750\u6599\u548c\u4e8c\u7ef4\u6709\u673a-\u65e0\u673a\u6742\u5316\u53d1\u5149\u6750\u6599\uff0c\u5e76\u5bf9\u5176\u5236\u5907\u3001\u6027\u8d28\u53ca\u5e94\u7528\u8fdb\u884c\u4e86\u70b9\u8bc4\u3002\u4f5c\u8005\u9610\u8ff0\u4e86\u6bcf\u4e00\u7c7b\u6750\u6599\u7684\u5236\u5907\u65b9\u6cd5\u5e76\u8ba8\u8bba\u5b83\u4eec\u7684\u7ed3\u6784\u548c\u5316\u5b66\u6027\u8d28\uff0c\u7279\u522b\u5bf9\u7ed3\u6784\u4e0e\u53d1\u5149\u7279\u6027\u4e4b\u95f4\u7684\u5173\u7cfb\u8fdb\u884c\u4e86\u91cd\u70b9\u8ba8\u8bba\u3002\u6700\u540e\uff0c\u4f5c\u8005\u5bf9\u4e8c\u7ef4\u53d1\u5149\u6750\u6599\u76ee\u524d\u7684\u6f5c\u5728\u5e94\u7528\u4ee5\u53ca\u53d1\u5c55\u4e2d\u7684\u6311\u6218\u548c\u672a\u6765\u673a\u9047\u8fdb\u884c\u4e86\u5c55\u671b\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong>\uff1a<a href=\"http:\/\/pubs.rsc.org\/en\/content\/articlelanding\/2018\/cs\/c8cs00332g#!divAbstract\" target=\"_blank\" rel=\"noopener\">Two-dimensional light-emitting materials: preparation, properties and applications<\/a>, (Chem. Soc. Rev., 2018, DOI: 10.1039\/c8cs00332g)<\/p>\n<p>3.\u7efc\u8ff0\uff1a\u65e0\u94c5\u6709\u673a\u65e0\u673a\u6742\u5316\u9499\u949b\u77ff\u5728\u5149\u4f0f\u4e0a\u7684\u8fd0\u7528<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-66599\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/0-4.png\" alt=\"\" width=\"700\" height=\"328\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/0-4.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2017\/02\/0-4-300x141.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p>\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\u7684<strong>\u9ec4\u7ef4\u9662\u58eb\u3001\u9648\u6c38\u534e\u6559\u6388\u548c\u590f\u82f1\u4e1c\u526f\u7814\u7a76\u5458\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09<\/strong>\u5728<strong>Advanced Materials<\/strong>\u53d1\u8868\u4e86\u9898\u4e3a<strong>\u201cLead-free Organic\u2013Inorganic Hybrid Perovskites for Photovoltaic Applications: Recent Advances and Perspectives\u201d<\/strong>\u7684\u7efc\u8ff0\u3002\u5728\u8fd9\u7bc7\u7efc\u8ff0\u4e2d\uff0c\u4f5c\u8005\u4e3b\u8981\u4ece\u65e0\u94c5\u9499\u949b\u77ff\u6676\u4f53\u7ed3\u6784\u3001\u8584\u819c\u6c89\u79ef\u548c\u5668\u4ef6\u6027\u80fd\u65b9\u9762\u7684\u7406\u8bba\u5206\u6790\u548c\u5b9e\u9a8c\u89e3\u91ca\uff0c\u56de\u987e\u4e86\u65e0\u94c5\u9499\u949b\u77ff\u7684\u6700\u65b0\u7814\u7a76\u8fdb\u5c55\u3002\u540c\u65f6\u8fd8\u8ba8\u8bba\u4e86\u8fdb\u4e00\u6b65\u4e86\u89e3\u65e0\u94c5\u6742\u5316\u9499\u949b\u77ff\u57fa\u672c\u6027\u8d28\u7684\u91cd\u8981\u6027\uff0c\u7279\u522b\u662f\u4e0e\u5149\u6709\u5173\u7684\u6027\u8d28\u3002<\/p>\n<p><strong>\u539f\u6587\u94fe\u63a5\uff1a<\/strong><a href=\"http:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/adma.201605005\/full\" target=\"_blank\" rel=\"noopener\">Lead-free Organic\u2013Inorganic Hybrid Perovskites for Photovoltaic Applications: Recent Advances and Perspectives <\/a>\uff08 <span class=\"fontstyle0\">Adv. Mater.,\u00a0<\/span><span class=\"fontstyle2\">2017<\/span><span class=\"fontstyle3\">, <\/span><span class=\"fontstyle0\">DOI: 10.1002\/adma.201605005<\/span>\u00a0\uff09<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u7f16\u8f91\uff0c\u6750\u6599\u725b\u6574\u7406\u3002<\/p>\n<p><strong><b>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaorenVIP<\/b><\/strong><\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u4eba\u7269\u7b80\u4ecb \u9ec4\u7ef4\uff0c\u7537\uff0c\u6c49\u65cf\uff0c1963\u5e745\u6708\u51fa\u751f\uff0c\u4e2d\u5171\u515a\u5458\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u9662\u58eb\uff0c\u4fc4\u7f57\u65af\u79d1\u5b66\u9662\u5916\u7c4d\u9662\u58eb\uff0c\u4e2d\u56fd\u6709\u673a\u7535\u5b50\u5b66\u4e0e\u67d4\u6027\u7535\u5b50\u5b66\u7684\u4e3b\u8981\u5960\u57fa\u8005\u00a0\uff0c\u897f\u5317\u5de5\u4e1a\u5927\u5b66\u535a\u58eb\u751f\u5bfc\u5e08\u3001&#8230;<\/p>\n","protected":false},"author":10213,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2810],"tags":[],"class_list":["post-161319","post","type-post","status-publish","format-standard","hentry","category-huizong"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/161319"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/10213"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=161319"}],"version-history":[{"count":10,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/161319\/revisions"}],"predecessor-version":[{"id":164687,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/161319\/revisions\/164687"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=161319"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=161319"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=161319"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}