{"id":162255,"date":"2018-12-21T06:30:35","date_gmt":"2018-12-20T22:30:35","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=162255"},"modified":"2018-12-21T16:40:27","modified_gmt":"2018-12-21T08:40:27","slug":"%e6%83%b3%e4%ba%86%e8%a7%a33d%e6%89%93%e5%8d%b0%ef%bc%8c%e4%bb%8e%e8%bf%99%e5%8d%81%e7%af%87%e7%bb%bc%e8%bf%b0%e5%bc%80%e5%a7%8b","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=162255","title":{"rendered":"\u60f3\u4e86\u89e33D\u6253\u5370\uff0c\u4ece\u8fd9\u5341\u7bc7\u7efc\u8ff0\u5f00\u59cb"},"content":{"rendered":"<p><strong>\u3010\u524d\u8a00\u3011<\/strong><\/p>\n<p>3D \u6253\u5370\u6280\u672f\u662f\u4e00\u79cd\u6700\u5148\u8fdb\u7684\u589e\u6750\u5236\u9020\u6280\u672f\uff0c\u7531\u4e8e\u5176\u5177\u6709\u9ad8\u7684\u751f\u4ea7\u5236\u9020\u6548\u7387\u3001\u53ef\u91cf\u4ea7\u80fd\u529b\u3001\u4f4e\u6210\u672c\u4ee5\u53ca\u590d\u6742\u6027\u7b49\u80fd\u529b\uff0c\u5728\u5148\u8fdb\u5236\u9020\u6750\u6599\u5f00\u53d1\u65b9\u9762\u5df2\u7ecf\u5f15\u8d77\u4e86\u4f01\u4e1a\u754c\u548c\u5b66\u672f\u754c\u7684\u9ad8\u5ea6\u5173\u6ce8\u3002\u8fd9\u79cd\u6280\u672f\u4e0d\u4ec5\u4ec5\u53ef\u4ee5\u52a0\u5de5\u5177\u6709\u4e09\u7ef4\u7acb\u4f53\u7ed3\u6784\u7684\u5668\u4ef6\uff0c\u800c\u4e14\u53ef\u4ee5\u7528\u4e8e\u591a\u6750\u6599\u3001\u591a\u529f\u80fd\u96c6\u6210\u5668\u4ef6\u7684\u5236\u5907\u3002\u56e0\u6b64\uff0c\u5e94\u7528 3D \u6253\u5370\u6280\u672f\u8fdb\u884c\u7814\u7a76\u5df2\u7ecf\u6210\u4e3a\u4e86\u7814\u7a76\u7684\u70ed\u70b9\u3002\u672c\u6587\u5c06\u4ece\u4ee5\u4e0b\u56db\u4e2a\u65b9\u9762\u5206\u522b\u4ecb\u7ecd\u591a\u7bc7\u7ecf\u5178\u7efc\u8ff0\uff0c\u5e0c\u671b\u80fd\u591f\u4f7f\u8bfb\u8005\u5feb\u901f\u4e86\u89e3 3D \u6253\u5370\u6280\u672f\u5728\u5404\u4e2a\u9886\u57df\u4e2d\u53d1\u6325\u7684\u4f5c\u7528\u3002<\/p>\n<p><strong>1\u30013D \u6253\u5370\u6280\u672f\u65b9\u6cd5<\/strong><\/p>\n<p>3D \u6253\u5370\u6280\u672f\u5305\u62ec\u591a\u79cd\u65b9\u6cd5\uff0c\u4f8b\u5982\u5149\u56fa\u5316\u6210\u578b\u6280\u672f\u3001\u7194\u878d\u6c89\u79ef\u6210\u578b\u6cd5\u3001\u58a8\u6c34\u76f4\u5199\u6280\u672f\u3001\u7acb\u4f53\u5e73\u7248\u5370\u5237\u6cd5\u3001\u55b7\u58a8\u6253\u5370\u3001\u9009\u62e9\u6027\u6fc0\u5149\u7194\u5316\u6280\u672f\u3001\u9009\u62e9\u6027\u6fc0\u5149\u70e7\u7ed3\u6280\u672f\u7b49\u3002\u968f\u7740 3D \u6253\u5370\u6280\u672f\u7684\u5feb\u901f\u53d1\u5c55\uff0c\u6d89\u53ca\u9886\u57df\u4e5f\u8fdb\u4e00\u6b65\u6269\u5c55\uff0c\u76ee\u524d\u5df2\u7ecf\u6210\u4e3a\u7814\u7a76\u7684\u70ed\u70b9\u65b9\u5411\u3002 Martin Pumera \u7b49\u4eba 2016 \u5e74\u5728Chem. Soc. Rev. \u6742\u5fd7\u4e0a\u53d1\u8868\u4e86\u5173\u4e8e\u5149\u56fa\u5316\u6210\u578b\u5f0f\u3001\u6324\u51fa\u5f0f\u6210\u578b\u3001\u7c89\u672b\u57fa\u5f0f\u6210\u578b\u7b49 3D \u6253\u5370\u65b9\u6cd5\u7684\u7814\u7a76\u8fdb\u5c55\u3002<sup>1<\/sup>\u00a02017 \u5e74 Rolf Mu\u0308lhaupt \u5728 Chem. Rev. \u6742\u5fd7\u4e0a\u53d1\u8868\u4e86\u5173\u4e8e\u5e73\u7248\u5370\u5237\u3001\u6570\u5b57\u5149\u5904\u7406\u3001\u591a\u5149\u5b50\u805a\u5408\u7b49 3D \u6253\u5370\u65b9\u6cd5\u7684\u53d1\u5c55\u8d8b\u52bf\u3002<sup>2<\/sup><\/p>\n<p>\u56fe1.3D \u6253\u5370\u6280\u672f\u65b9\u6cd5<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-162265 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72471-13.png\" alt=\"\" width=\"600\" height=\"267\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72471-13.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72471-13-300x134.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>2\u30013D \u6253\u5370\u6750\u6599<\/strong><\/p>\n<p>2017\u5e74\uff0cTomaso Zambelli \u7b49\u4eba\u5728 Adv. Mater. \u6742\u5fd7\u4e0a\u53d1\u8868\u4e86\u5173\u4e8e 3D \u6253\u5370\u6280\u672f\u5236\u5907\u91d1\u5c5e\u7684\u7efc\u8ff0\uff0c\u603b\u7ed3\u51fa\u5404\u79cd 3D \u6253\u5370\u6280\u672f\u5236\u5907\u5fae\u7c73\u5c3a\u5ea6\u4e0a\u7684\u91d1\u5c5e\u7ed3\u6784\uff0c\u5e76\u4e14\u7ed3\u5408\u4e86\u591a\u79cd 3D \u6253\u5370\u65b9\u6cd5\u5236\u5907\u91d1\u5c5e\u5316\u8fc7\u7a0b\uff0c\u591a\u6b65\u9aa4\u7684\u65b9\u6cd5\u975e\u5e38\u9002\u7528\u4e8e\u5404\u79cd\u5e94\u7528\u7a0b\u5e8f\u3002\u4e00\u65e6\u5fae\u91d1\u5c5e\u589e\u6750\u5236\u9020\u6210\u529f\uff0c\u5b83\u4eec\u5c06\u80fd\u591f\u5236\u5907\u51fa\u66f4\u590d\u6742\u7684\u51e0\u4f55\u5f62\u72b6\u548c\u6750\u6599\u7ed3\u6784\u3002<sup>3<\/sup>\u00a0Shlomo Magdassi\u00a0\u7b49\u4eba 2018 \u5e74\u5728 Adv. Mater. \u6742\u5fd7\u4e0a\u53d1\u8868\u4e86\u5173\u4e8e 3D \u6253\u5370 3D \u6c34\u51dd\u80f6\u3001\u54cd\u5e94\u5149\u805a\u5316\u5408\u7269\u6750\u6599\u548c\u9676\u74f7\u6750\u6599\u7684\u8fdb\u5c55\u3002<sup>4<\/sup>\u00a0\u540c\u5e74\uff0c Tawfique Hasan \u7b49\u4eba\u5728 Chem. Soc. Rev. \u6742\u5fd7\u4e0a\u53d1\u8868\u4e86\u5173\u4e8e\u4e8c\u7ef4\u6750\u6599\u7684 3D \u6253\u5370\uff0c\u5177\u4f53\u9610\u8ff0\u4e86 3D \u6253\u5370\u77f3\u58a8\u70ef\u3001\u77f3\u58a8\u7094\u7b49\u4e8c\u7ef4\u6750\u6599\u7684\u5177\u4f53\u6253\u5370\u8fc7\u7a0b\u548c\u5e94\u7528\u524d\u666f\u3002<sup>5<\/sup><\/p>\n<p>\u56fe2.3D \u6253\u5370\u91d1\u5c5e\u6750\u6599<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-162266 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72472-14.png\" alt=\"\" width=\"600\" height=\"237\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72472-14.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72472-14-300x119.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe3 . 3D \u6253\u5370\u805a\u5408\u7269\u57fa\u9676\u74f7\u6750\u6599<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-162267 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72473-13.png\" alt=\"\" width=\"448\" height=\"315\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72473-13.png 448w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72473-13-300x211.png 300w\" sizes=\"(max-width: 448px) 100vw, 448px\" \/><\/p>\n<p>\u56fe4 . 3D \u6253\u5370\u4e8c\u7ef4\u6750\u6599<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-162268 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72474-13.png\" alt=\"\" width=\"600\" height=\"212\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72474-13.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72474-13-300x106.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>3\u30013D \u6253\u5370\u7ed3\u6784<\/strong><\/p>\n<p>William B. Carter \u7b49\u4eba 2016 \u5e74 \u5728 Annu. Rev. Mater. Res. \u6742\u5fd7\u4e0a\u53d1\u8868\u4e86\u5173\u4e8e3D \u6253\u5370\u5404\u79cd\u7ed3\u6784\u7684\u7efc\u8ff0\uff0c\u5176\u5177\u4f53\u7684\u9610\u8ff0\u4e86\u7ed3\u6784\u6750\u6599\u9886\u57df\u7684\u73b0\u72b6\uff0c\u590d\u6742\u7ed3\u6784\u7684\u83b7\u5f97\u53ef\u4ee5\u5e94\u7528\u5728\u4f17\u591a\u9886\u57df\u3002<\/p>\n<p>\u56fe5 . 3D \u6253\u5370\u7ed3\u6784<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-162269 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72475-13.png\" alt=\"\" width=\"611\" height=\"371\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72475-13.png 611w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72475-13-300x182.png 300w\" sizes=\"(max-width: 611px) 100vw, 611px\" \/><\/p>\n<p><strong>4\u30013D \u6253\u5370\u7684\u5e94\u7528<\/strong><\/p>\n<p>3D \u6253\u5370\u6280\u672f\u5df2\u7ecf\u5e94\u7528\u5728\u793e\u4f1a\u4e2d\u5404\u4e2a\u9886\u57df\uff0c\u4f8b\u5982\u5728\u5316\u5b66\u5de5\u7a0b\u548c\u50ac\u5316\u6280\u672f\u9886\u57df\u53ef\u4ee5\u7528\u4f5c\u7ed3\u6784\u5316\u50ac\u5316\u5242\u3001\u6405\u62cc\u673a\u548c\u53cd\u5e94\u5806\uff0c\u7ec4\u7ec7\u5de5\u7a0b\u548c\u836f\u7269\u8f93\u9001\uff0c\u751f\u7269\u5e94\u7528\u4ee5\u53ca\u80fd\u6e90\u9886\u57df\u7b49\u3002<sup>7-10<\/sup>\u00a0Rob Ameloot\u00a0\u53ca\u5176\u5408\u4f5c\u8005\u5728 2018 \u5e74 Chem. Soc. Rev. \u6742\u5fd7\u4e0a\u8bba\u8ff0\u4e86\u8ba1\u7b97\u673a\u8f85\u52a9\u6280\u672f\u7ed3\u5408 3D \u6253\u5370\u6280\u672f\u5728\u5316\u5b66\u5de5\u7a0b\u4ee5\u53ca\u50ac\u5316\u9886\u57df\u7684\u5e94\u7528\u3002\u901a\u8fc7\u7ed8\u5236\u8ba1\u7b97\u673a\u6a21\u578b\u8bbe\u8ba1\u5316\u5b66\u53cd\u5e94\u5668\u4ee5\u53ca\u7ed3\u6784\u50ac\u5316\u5242\uff0c\u5e94\u7528 3D \u6253\u5370\u65b9\u6cd5\u5236\u5907\u51fa\u6765<sup>7<\/sup><\/p>\n<p>Xuan-Ming Duan\u00a0\u8bfe\u9898\u7ec4\u57282015\u5e74 Chem. Soc. Rev. \u6742\u5fd7\u4e0a\u53d1\u8868\u4e86\u9898\u4e3a\u201cTwo-photon polymerization microfabrication of\u00a0hydrogels: an advanced 3D printing technology\u00a0for tissue engineering and drug delivery\u201d\u7684\u7efc\u8ff0\uff0c\u5176\u4e3b\u8981\u8bba\u8ff0\u4e86\u901a\u8fc7 3D \u6253\u5370\u7b56\u7565\u5236\u5907\u7684\u6c34\u51dd\u80f6\uff0c\u5e76\u5c06\u5176\u7528\u4e8e\u7ec4\u7ec7\u5de5\u7a0b\u548c\u836f\u7269\u8f93\u9001\u3002 3D \u6253\u5370\u6280\u672f\u4e0d\u4ec5\u53ef\u4ee5\u5236\u5907\u5177\u6709\u4e09\u7ef4\u7ed3\u6784\u7684\u6c34\u51dd\u80f6\uff0c\u800c\u4e14\u53ef\u9002\u7528\u4e8e\u591a\u6750\u6599\u7684\u5fae\u5236\u5907\uff0c\u56e0\u6b64\u5176\u5728\u533b\u5b66\u4e0a\u5177\u6709\u5e7f\u53d1\u7684\u5e94\u7528\u524d\u666f\u3002<sup>8<\/sup>\u00a02018\u5e74\uff0cSteven\u00a0D.\u00a0R.\u00a0Christie\u00a0\u7b49\u4eba\u5728 Nat. Rev. Chem. \u4e0a\u7efc\u8ff0\u4e86 3D \u6253\u5370\u6280\u672f(\u5149\u523b\u6280\u672f\u548c\u55b7\u58a8\u6253\u5370\u6280\u672f)\u5728\u751f\u7269\u9886\u57df\u7684\u5e94\u7528\uff0c\u5217\u4e3e\u4e86 3D \u6253\u5370\u7684\u8bf8\u591a\u65b9\u6cd5\uff0c\u5e76\u8fdb\u884c\u4e86\u5c55\u671b\u3002<sup>9<\/sup>\u00a0Liangbing Hu\u00a0\u7b49\u4eba 2017\u00a0\u5e74\u5728 Adv. Mater. \u6742\u5fd7\u4e0a\u53d1\u8868\u4e86\u5173\u4e8e3D \u6253\u5370\u78b3\u57fa\u6750\u6599\u5728\u80fd\u6e90\u5b58\u50a8\u9886\u57df\u7684\u5e94\u7528\u3002\u91cd\u70b9\u9610\u8ff0\u4e86\u4ee5\u77f3\u58a8\u70ef\u4ee5\u53ca\u6c27\u5316\u77f3\u58a8\u70ef\u4f5c\u4e3a\u7535\u6781\u6d3b\u6027\u58a8\u6c34\u6750\u6599\uff0c\u901a\u8fc7 3D \u6253\u5370\u58a8\u6c34\u76f4\u5199\u6280\u672f\u6784\u9020\u5fae\u7eb3\u7ed3\u6784\uff0c\u5e76\u4e14\u5c06\u5176\u5e94\u7528\u5728\u7535\u6c60\u4ee5\u53ca\u8d85\u7ea7\u7535\u5bb9\u5668\u50a8\u80fd\u5668\u4ef6\u4e0a\u3002\u9664\u6b64\u4e4b\u5916\uff0c\u7814\u7a76\u8005\u8fd8\u5bf9 3D \u6253\u5370\u6280\u672f\u5728\u5176\u4ed6\u9886\u57df\u7684\u53d1\u5c55\u8fdb\u884c\u4e86\u5c55\u671b\u3002<sup>10<\/sup><\/p>\n<p>\u56fe6.3D \u6253\u5370\u6280\u672f\u5728\u50ac\u5316\u9886\u57df\u7684\u5e94\u7528<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-162270 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72476-11.png\" alt=\"\" width=\"600\" height=\"441\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72476-11.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72476-11-300x221.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe7.3D \u6253\u5370\u53cd\u5e94\u5668<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-162271 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72477-12.png\" alt=\"\" width=\"335\" height=\"421\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72477-12.png 335w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72477-12-239x300.png 239w\" sizes=\"(max-width: 335px) 100vw, 335px\" \/><\/p>\n<p>\u56fe8.3D \u6253\u5370\u6280\u672f\u5728\u80fd\u6e90\u9886\u57df\u5e94\u7528<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-162272 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72478-10.png\" alt=\"\" width=\"319\" height=\"318\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72478-10.png 319w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72478-10-150x150.png 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2018\/12\/\u56fe\u72478-10-300x300.png 300w\" sizes=\"(max-width: 319px) 100vw, 319px\" \/><\/p>\n<p>3D \u6253\u5370\u6280\u672f\u9010\u6e10\u7684\u8fdb\u5165\u5230\u4e86\u793e\u4f1a\u7684\u5404\u4e2a\u9886\u57df\uff0c\u5176\u5728\u6784\u9020\u590d\u6742\u7ed3\u6784\u4ee5\u53ca\u53ef\u89c4\u6a21\u5316\u7b49\u65b9\u9762\u5177\u6709\u7edd\u5bf9\u4f18\u52bf\u3002\u7bc7\u5e45\u6240\u9650\u4e0d\u8be6\u7ec6\u8ba8\u8bba\u3002\u7efc\u4e0a\uff0c\u672c\u6587\u7b80\u5355\u4ecb\u7ecd\u4e86\u6570\u7bc73D \u6253\u5370\u6280\u672f\u5728\u5404\u4e2a\u9886\u57df\u7684\u91cd\u8981\u7efc\u8ff0\uff0c\u5e0c\u671b\u8bfb\u8005\u670b\u53cb\u80fd\u4ece\u4e2d\u83b7\u5f97\u4e00\u4e9b\u5e2e\u52a9\uff0c\u5bf93D \u6253\u5370\u6280\u672f\u6709\u4e00\u4e2a\u7b80\u5355\u7684\u8ba4\u8bc6\u4e86\u89e3\u3002<\/p>\n<p><strong><b>\u3010\u53c2\u8003\u6587\u732e\u3011<\/b><\/strong><\/p>\n<p>1 Ambrosi, A., Pumera, M. 3D-printing technologies for electrochemical\u00a0applications. Chem. Soc. Rev., 45, 2740-2755, DOI: 10.1039\/c5cs00714c\u00a0(2016).<\/p>\n<p>2.Ligon, S. C., Liska, R., Stampfl, J., Gurr, M., Mulhaupt, R. Polymers for 3D Printing and Customized Additive Manufacturing. Chem. Rev. 2017, 117, 10212-10290, DOI: 10.1021\/acs.chemrev.7b00074 (2017). \u00a0<br \/>\n 3 Hirt, L., Reiser, A., Spolenak, R., Zambelli, T. Additive Manufacturing of Metal Structures at theMicrometer Scale. Mater. 29, 1604211-1604240, DOI: 10.1002\/adma.201604211\u00a0(2017).<\/p>\n<p>4 Layani, M., Wang, X. F., Magdassi, S. Novel Materials for 3D Printing by Photopolymerization. Adv. Mater. 30, 1706344-1706350, DOI: 10.1002\/adma.201706344\u00a0(2018).<\/p>\n<p>5 Schaedler, T A., Carter, W. B. Architected Cellular Materials. Annu. Rev. Mater. Res. 2016. 46:187\u2013210, DOI: 10.1146\/annurev-matsci-070115-031624 (2016).<\/p>\n<p>6 Hu, G. H., Kang, J., Leonard, W. T. N., Zhu, X. X., Howe, R. C. T., Jones, C. G., Hersam, M. C., Hasan, T. Functional inks and printing of\u00a0two-dimensional\u00a0materials. Chem. Soc. Rev. 47, 3265-3300, DOI: 10.1039\/c8cs00084k (2018).<\/p>\n<p>7 Cabrera, C. P., Achille, C., Kuhn, S., Ameloot, R. 3D printing in chemical engineering and catalytic\u00a0technology: structured catalysts, mixers\u00a0and reactors. Chem. Soc. Rev. 47, 209-230, DOI: 10.1039\/c7cs00631d (2017).<\/p>\n<p>8 Xing, J. F., Zheng, M. L., Duan, X. M.\u00a0Two-photon polymerization\u00a0microfabrication of\u00a0hydrogels: an advanced 3D printing technology\u00a0or tissue engineering and drug delivery. Chem. Soc. Rev. 44, 5031-5039, DOI: 10.1039\/c5cs00278h (2015).<\/p>\n<p>9 Capel, A. J., Rimington, R. P., Lewis, M. P., Christie, S. D. R. 3D printing for chemical,\u00a0pharmaceutical and biological\u00a0applications. Nat. Rev. Chem. 2, 422-436, DOI: 10.1038\/s41570-018-0058-y (2018).<\/p>\n<p>10 Fu, K., Yao, Y. G., Dai, J. Q., Hu, L. B. Progress in 3D Printing of Carbon Materials for Energy-Related Applications. Adv. Mater. 29, 1603486-1603505, DOI: 10.1002\/adma.201603486 (2017).<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba<strong>\u79d1\u6280\u987e\u95eeJingxin Zhao<\/strong>\u4f9b\u7a3f\uff0c\u7f16\u8f91\u90e8\u7f16\u8f91\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1: tougao@cailiaoren.com.<\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaokefu.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u524d\u8a00\u3011 3D \u6253\u5370\u6280\u672f\u662f\u4e00\u79cd\u6700\u5148\u8fdb\u7684\u589e\u6750\u5236\u9020\u6280\u672f\uff0c\u7531\u4e8e\u5176\u5177\u6709\u9ad8\u7684\u751f\u4ea7\u5236\u9020\u6548\u7387\u3001\u53ef\u91cf\u4ea7\u80fd\u529b\u3001\u4f4e\u6210\u672c\u4ee5\u53ca\u590d\u6742\u6027\u7b49\u80fd\u529b\uff0c\u5728\u5148\u8fdb\u5236\u9020\u6750\u6599\u5f00\u53d1\u65b9\u9762\u5df2\u7ecf\u5f15\u8d77\u4e86\u4f01\u4e1a\u754c\u548c\u5b66\u672f&#8230;<\/p>\n","protected":false},"author":10213,"featured_media":162593,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2810],"tags":[],"class_list":["post-162255","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-huizong"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/162255"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/10213"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=162255"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/162255\/revisions"}],"predecessor-version":[{"id":162277,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/162255\/revisions\/162277"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/162593"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=162255"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=162255"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=162255"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}