{"id":167811,"date":"2019-02-25T06:28:33","date_gmt":"2019-02-24T22:28:33","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=167811"},"modified":"2019-02-23T22:56:26","modified_gmt":"2019-02-23T14:56:26","slug":"%e3%80%90%e8%80%81%e5%a4%96%e4%b8%8d%e9%9c%80%e8%a6%81%e6%a0%a1%e7%a8%bf%e3%80%91%e7%be%8e%e5%9b%bd%e5%be%b7%e5%85%8b%e8%90%a8%e6%96%afam%e5%a4%a7%e5%ad%a6acta-materialia%ef%bc%9anicomnin","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=167811","title":{"rendered":"\u7f8e\u56fd\u5fb7\u514b\u8428\u65afA&amp;M\u5927\u5b66Acta Materialia\uff1aNiCoMnIn\u78c1\u6027\u5f62\u72b6\u8bb0\u5fc6\u5408\u91d1\u4e2d\u6210\u5206\u548c\u6676\u4f53\u6392\u5e8f\u5bf9\u94c1\u78c1\u8f6c\u53d8\u7684\u5f71\u54cd"},"content":{"rendered":"<p><strong><b>\u3010\u5f15\u8a00\u3011<\/b><\/strong><\/p>\n<p>Ni-Mn\u57fa\u53d8\u78c1\u6027\u5f62\u72b6\u8bb0\u5fc6\u5408\u91d1\uff08MMSMAs\uff09\u56e0\u5176\u72ec\u7279\u7684\u6027\u8d28\u800c\u5907\u53d7\u5173\u6ce8\uff0c\u5982\u4f20\u7edf\u7684\u5f62\u72b6\u8bb0\u5fc6\u6548\u5e94\u3001\u78c1\u573a\u8bf1\u5bfc\u9a6c\u6c0f\u4f53\u76f8\u53d8\uff08MT\uff09\u3001\u5de8\u78c1\u70ed\u6548\u5e94\u548c\u5927\u78c1\u963b\u3002\u8bb8\u591a\u6027\u8d28\u6e90\u4e8e\u94c1\u78c1\u7acb\u65b9\u4f53\u5965\u6c0f\u4f53\u548c\u8d85\u987a\u78c1\u6027\u6216\u53cd\u94c1\u78c1\u6027\uff0c\u975e\u8c03\u5236\u76842M\u6216\u8c03\u5236\u7684\uff085M\uff0c7M\uff09\u56db\u65b9\u9a6c\u6c0f\u4f53\u4e4b\u95f4\u7684MT\u3002\u6362\u53e5\u8bdd\u8bf4\uff0cMMSMA\u8868\u73b0\u51fa\u8026\u5408\u94c1\u5f39\u6027\u548c\u78c1\u8f6c\u53d8\u7684\u78c1-\u7ed3\u6784\u8f6c\u53d8\uff0c\u5176\u4e2d\u7cfb\u7edf\u7684\u78c1\u72b6\u6001\u5728\u51b7\u5374\u65f6\u4ece\u5f3a\u94c1\u78c1\u6027\u53d8\u4e3a\u53cd\u94c1\u78c1\/\u8d85\u987a\u78c1\u6001\u3002\u5df2\u7ecf\u8bc1\u660e\u78c1\u6027\u6709\u5e8f\u5ea6\u5728MMSMA\u7684MT\u6e29\u5ea6\u4e2d\u8d77\u91cd\u8981\u7684\u4f5c\u7528\u3002\u66f4\u5177\u4f53\u5730\uff0c\u5728NiCoMnIn MMSMA\u4e2d\uff0c\u5965\u6c0f\u4f53\u7684\u78c1\u6709\u5e8f\u6027\u7684\u589e\u52a0\uff08\u51cf\u5c11\uff09\u4f1a\u964d\u4f4e\uff08\u589e\u52a0\uff09MT\u5904\u7684\u603b\u71b5\u53d8\u3002\u8be5\u6548\u5e94\u5bfc\u81f4MT\u6e29\u5ea6\u4e0eTC\u548cMS\u4e4b\u95f4\u7684\u5dee\u5f02\u6210\u53cd\u6bd4\u5173\u7cfb\u3002\u56e0\u6b64\uff0c\u53ef\u4ee5\u901a\u8fc7\u8c03\u6574MMSMA\u4e2d\u7684\u78c1\u6027\u6392\u5e8f\u6765\u8c03\u6574MT\u6e29\u5ea6\uff0c\u4ece\u800c\u5141\u8bb8\u4fee\u6539\u9a6c\u6c0f\u4f53\u8f6c\u6362\u7279\u6027\uff0c\u4f8b\u5982\u8f6c\u6362\u6ede\u540e\uff0c\u8f6c\u6362\u8303\u56f4\u548c\u8f6c\u6362\u6291\u5236\u7a0b\u5ea6\uff0c\u6216\u5b8c\u5168\u6291\u5236MT\uff0c\u4ece\u800c\u4ea7\u751f\u5177\u6709\u6f5c\u5728\u72ec\u7279\u6027\u8d28\u7684\u73bb\u7483\u5316\u8f6c\u53d8\u884c\u4e3a\u3002<\/p>\n<p><strong><b>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/b><\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c\u5728<strong><b>\u52a0\u62ff\u5927\u9ea6\u5409\u5c14\u5927\u5b66I. Karaman\u6559\u6388\u6559\u6388\u56e2\u961f\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/b><\/strong>\u5e26\u9886\u4e0b\uff0c\u4e0e<strong><b>\u4fc4\u7f57\u65af\u6258\u6728\u65af\u514b\u56fd\u7acb\u5927\u5b66<\/b><\/strong>\u548c<strong><b>\u7f8e\u56fd\u963f\u8d21\u56fd\u5bb6\u5b9e\u9a8c\u5ba4<\/b><\/strong>\u5408\u4f5c\uff0c\u7814\u7a76\u4e86\u4e0d\u540cNiCoMnIn\u5408\u91d1\u4e2d\u5965\u6c0f\u4f53\u76f8\u53d8T<em><sub><i>C<\/i><\/sub><\/em>\u548c\u8be5\u6e29\u5ea6\u4e0e\u6676\u4f53\u6709\u5e8f\u6027\u4e4b\u95f4\u7684\u5173\u7cfb\u4ee5\u53ca\u5728ODO\u8f6c\u53d8\u6e29\u5ea6\u4ee5\u4e0b\u7684\u4e8c\u6b21\u70ed\u5904\u7406\u540e\u7684\u78c1\u6027\u80fd\u3002\u7136\u540e\uff0cT<em><sub><i>C<\/i><\/sub><\/em>\u7528\u4e8e\u63a2\u6d4b\u03b7<sub>L21<\/sub>\u7684\u6f14\u53d8\u5e76\u4e0eMT\u6e29\u5ea6\u7684\u6f14\u53d8\u5efa\u7acb\u5173\u7cfb\u3002\u5de5\u4f5c\u7684\u4e3b\u8981\u76ee\u7684\u662f\u901a\u8fc7\u03b7<sub>L21<\/sub>\u4e0eT<sub>C<\/sub>\u7684\u53d8\u5316\u76f8\u5173\u8054\uff0c\u53ef\u4ee5\u9610\u660e\u4e86\u9020\u6210MT\u5bf9MMSMA\u4e2d\u4e8c\u6b21\u70ed\u5904\u7406\u7684\u9ad8\u7075\u654f\u5ea6\u7684\u673a\u5236\u3002\u76f8\u5173\u6210\u679c\u4ee5\u9898\u4e3a<strong><b>\u201c<\/b><\/strong><strong><b>Effects of composition and crystallographic ordering on the ferromagnetic transition in NiCoMnIn magnetic shape memory alloys<\/b><\/strong><strong><b>\u201d<\/b><\/strong>\u53d1\u8868\u5728\u4e86<strong><b>Acta Materialia<\/b><\/strong>\u4e0a\u3002<\/p>\n<p><strong><b>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/b><\/strong><\/p>\n<p><strong><b>\u56fe1<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><strong><b>\u591a\u6676\u6837\u54c1\u7684<\/b><\/strong><strong><b>\u4e0a\u9a6c\u6c0f\u4f53\u70b9<\/b><\/strong><strong><b>\u4e0e\u542b\u91cf\u7684\u51fd\u6570\u5173\u7cfb<\/b><\/strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-167812\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/1-25.jpg\" alt=\"\" width=\"600\" height=\"329\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/1-25.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/1-25-300x165.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u591a\u6676Ni<sub>45<\/sub>Co<sub>5<\/sub>Mn<sub>50-X<\/sub>In<sub>X<\/sub>\u00a0at.\uff05\u56fa\u6eb6\u70ed\u5904\u7406\u7684\u6837\u54c1\uff0c\u4e0a\u9a6c\u6c0f\u4f53\u70b9M<sub>S<\/sub>\u4e0e\u542b\u91cf\u7684\u76f8\u5173\u6027\u3002Plot\u5c06\u5f53\u524d\u5de5\u4f5c\u6750\u6599\uff08\u7ea2\u8272\uff09\u83b7\u5f97\u7684\u6570\u636e\u4e0e\u6587\u732e\u4e2d\u53d1\u8868\u7684\u6570\u636e\u8fdb\u884c\u6bd4\u8f83\uff08\u84dd\u8272\u548c\u7eff\u8272\uff09\u3002<\/p>\n<p><strong><b>\u56fe2<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><strong><b>\u591a\u6676\u6837\u54c1\u7684<\/b><\/strong><strong><b>\u70ed\u5904\u7406<\/b><\/strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-167813\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/2-22.jpg\" alt=\"\" width=\"600\" height=\"573\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/2-22.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/2-22-300x287.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08a\uff09\u901a\u8fc7\u6837\u54c1\u8d28\u91cf\u548c\u6e29\u5ea6\u901f\u7387\u5f52\u4e00\u5316\u7684\u91cf\u70ed\u54cd\u5e94\u03c6\u4e0e\u6e29\u5ea6\u4e4b\u95f4\u7684\u5173\u7cfb\uff1b<\/p>\n<p>\uff08b\uff09\u5728\u4e24\u4e2a\u70ed\u5faa\u73af\u8fc7\u7a0b\u4e2d\u6e29\u5ea6\u5bfc\u6570\u2202\u03c6\/\u2202T\u4e0e\u6e29\u5ea6\u4e4b\u95f4\u7684\u5173\u7cfb\uff1b<\/p>\n<p>\uff08c\uff09\u57280.05T\u7684\u6052\u5b9a\u78c1\u573a\u4e0b\uff0c\u5728\u5355\u4e2a\u51b7\u5374\/\u52a0\u70ed\u5faa\u73af\u671f\u95f4\u603b\u78c1\u5316\u5f3a\u5ea6\u7684\u5bfc\u6570\u2202M\/\u2202T\u4e0e\u6e29\u5ea6\u4e4b\u95f4\u7684\u5173\u7cfb\u3002\u5bf9\u4e8e\u76f8\u540c\u7684\u591a\u6676\uff08PC\uff09NiCoMnIn<sub>13.71<\/sub>\u78c1\u6027\u5f62\u72b6\u8bb0\u5fc6\u5408\u91d1\u6837\u54c1\uff08MMSMA\uff09\uff0c\u57281173K\u4e0b\u56fa\u6eb624\u5c0f\u65f6\uff08WQ\uff09\uff0c\u5728773K\u4e0b\u8fdb\u884c\u4e8c\u6b21\u9000\u706b0.5\u5c0f\u65f6\uff0c\u7136\u540e\u6c34\u6dec\u3002\u7bad\u5934\u8868\u793a\u6e29\u5ea6\u5faa\u73af\u7684\u51b7\u5374\/\u52a0\u70ed\u65b9\u5411\u3002\uff08b\uff09\u4e2d\u7684\u7a7a\u5fc3\u5706\u5708\u8868\u793a\u8ba1\u7b97\u5c45\u91cc\u6e29\u5ea6\u7684\u5cf0\u503c\u6e29\u5ea6\uff0c\u5c45\u91cc\u6e29\u5ea6\u662f\u4ece\u8fd9\u56db\u6761\u66f2\u7ebf\u7684\u5e73\u5747\u503c\u8ba1\u7b97\u51fa\u6765\u7684\uff08\u663e\u793a\u5728\u4e2d\u95f4\uff09\u3002\u5c06\u8be5\u503c\u4e0e\u4ece\uff08c\uff09\u4e2d\u7684\u70ed\u78c1\u5316\u66f2\u7ebf\u6d4b\u91cf\u7684\u5c45\u91cc\u6e29\u5ea6\u8fdb\u884c\u6bd4\u8f83\u3002<\/p>\n<p><strong><b>\u56fe3<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><strong><b>\u591a\u6676NiCoMnInx<\/b><\/strong><strong><b>\u53d8\u78c1\u6027<\/b><\/strong><strong><b>\u5f62\u72b6\u8bb0\u5fc6\u5408\u91d1\u4e2d\u5965\u6c0f\u4f53T<\/b><\/strong><strong><sub><b>C<\/b><\/sub><\/strong><strong><b>\u7684\u6f14\u53d8<\/b><\/strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-167814\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/3-21.jpg\" alt=\"\" width=\"600\" height=\"945\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/3-21.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/3-21-190x300.jpg 190w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>4 <\/b><\/strong><strong><b>\u591a\u6676NiCoMnInx<\/b><\/strong><strong><b>\u53d8\u78c1\u6027<\/b><\/strong><strong><b>\u5f62\u72b6\u8bb0\u5fc6\u5408\u91d1\u4e2d\u5965\u6c0f\u4f53T<\/b><\/strong><strong><sub><b>C<\/b><\/sub><\/strong><strong><b>\u4e0e\u4e8c\u6b21HT\u6e29\u5ea6<\/b><\/strong><strong><b>\u7684<\/b><\/strong><strong><b>\u5173\u7cfb<\/b><\/strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-167815\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/4-22.jpg\" alt=\"\" width=\"600\" height=\"392\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/4-22.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/4-22-300x196.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>5 <\/b><\/strong><strong><b>\u56db\u79cd\u4e0d\u540cSHT\u5355\u6676Ni<\/b><\/strong><strong><sub><b>45<\/b><\/sub><\/strong><strong><b>Co<\/b><\/strong><strong><sub><b>5<\/b><\/sub><\/strong><strong><b>Mn<\/b><\/strong><strong><sub><b>36.6<\/b><\/sub><\/strong><strong><b>In<\/b><\/strong><strong><sub><b>13.4<\/b><\/sub><\/strong><strong><b>\u6837\u54c1\u7684<\/b><\/strong><strong><b>XRD<\/b><\/strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-167816\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/5-16.jpg\" alt=\"\" width=\"600\" height=\"333\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/5-16.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/5-16-300x167.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>6 <\/b><\/strong><strong><b>\u8ba1\u7b97\u7684\u603b\u6709\u6548\u78c1\u4ea4\u6362\u53c2\u6570<\/b><\/strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-167817\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/6-11.jpg\" alt=\"\" width=\"600\" height=\"653\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/6-11.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/6-11-276x300.jpg 276w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u56fe<\/b><\/strong><strong><b>7 <\/b><\/strong><strong><b>\u4e09\u79cd\u4e0d\u540c\u7ec4\u5408\u7269\u7684T<\/b><\/strong><strong><sub><b>C<\/b><\/sub><\/strong><strong><b>\u968f<\/b><\/strong>\u03b7<sub>L21<\/sub><strong><b>\u51fd\u6570\u7684\u53d8\u5316<\/b><\/strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-167818\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/7-8.jpg\" alt=\"\" width=\"600\" height=\"393\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/7-8.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/7-8-300x197.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u3010<strong><b>\u5c0f\u7ed3<\/b><\/strong>\u3011<\/p>\n<p>\u603b\u4e4b\uff0c\u5965\u6c0f\u4f53\u7684\u5c45\u91cc\u6e29\u5ea6\u8868\u73b0\u51fa\u5bf9L<sub>21<\/sub>\u6709\u5e8f\u5ea6\u7684\u76f8\u5173\u6027\u3002\u901a\u8fc7\u4ece\u5934\u7b97DFT\u8ba1\u7b97\u9a8c\u8bc1\u4e86\u8fd9\u79cd\u5173\u7cfb\u3002T<em><sub><i>C<\/i><\/sub><\/em>\u548c\u03b7<sub>L21<\/sub>\u4e4b\u95f4\u7684\u5173\u7cfb\u5df2\u88ab\u7528\u4e8e\u5b9a\u6027\u5730\u4f30\u8ba1\u5728ODO\u8f6c\u53d8\u6e29\u5ea6\u4ee5\u4e0b\u8fdb\u884c\u4e8c\u6b21\u70ed\u5904\u7406\u7684\u6709\u5e8f\u5ea6\u7684\u6f14\u53d8\u3002\u7ed3\u679c\u8868\u660e\uff0c\u6709\u5e8f\u52a8\u529b\u5b66\u5f88\u5feb\uff0c\u603b\u7684\u6709\u5e8f\u5ea6\u4e3b\u8981\u53d6\u51b3\u4e8e\u4e8c\u6b21\u70ed\u5904\u7406\u6e29\u5ea6\u548c\u51b7\u5374\u901f\u5ea6\uff0c\u5bf9\u4e8e\u5904\u7406\u65f6\u95f4\u591f\u957f\u800c\u8a00\uff0c\u6392\u5e8f\u53d7\u5230\u4f4e\u6e29\u4e0b\u539f\u5b50\u6269\u6563\u53ef\u7528\u7684\u4f4e\u70ed\u80fd\u7684\u9650\u5236\u3002\u6700\u540e\uff0c\u6210\u5206\u7684\u7ec6\u5fae\u53d8\u5316\u5bf9MT\u6e29\u5ea6\u5177\u6709\u5f3a\u70c8\u5f71\u54cd\uff0c\u5e76\u4e14\u5bf9\u94c1\u78c1\u8f6c\u53d8\u5177\u6709\u663e\u7740\u4f46\u8f83\u5c0f\u7684\u5f71\u54cd\u3002<\/p>\n<p><strong><b>\u00a0<\/b><\/strong><strong><b>\u6587\u732e\u94fe\u63a5\uff1a<\/b><\/strong><a href=\"https:\/\/www.sciencedirect.com\/science\/article\/pii\/S1359645419300114\"><u>Effects of composition and crystallographic ordering on the ferromagnetic transition in NiCoMnIn magnetic shape memory alloys<\/u><\/a>\uff08Acta Materialia, 2019, DOI:10.1016\/j.actamat.2019.01.008\uff09<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u7f16\u8f91\u90e8\u5b66\u672f\u7ec4<strong><b>\u6728\u6587\u97ec<\/b><\/strong>\u7ffb\u8bd1\uff0c\u6750\u6599\u725b\u6574\u7406\u7f16\u8f91\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 Ni-Mn\u57fa\u53d8\u78c1\u6027\u5f62\u72b6\u8bb0\u5fc6\u5408\u91d1\uff08MMSMAs\uff09\u56e0\u5176\u72ec\u7279\u7684\u6027\u8d28\u800c\u5907\u53d7\u5173\u6ce8\uff0c\u5982\u4f20\u7edf\u7684\u5f62\u72b6\u8bb0\u5fc6\u6548\u5e94\u3001\u78c1\u573a\u8bf1\u5bfc\u9a6c\u6c0f\u4f53\u76f8\u53d8\uff08MT\uff09\u3001\u5de8\u78c1\u70ed\u6548\u5e94\u548c\u5927\u78c1\u963b\u3002\u8bb8\u591a\u6027\u8d28&#8230;<\/p>\n","protected":false},"author":2109,"featured_media":167816,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[2829,2534,875],"class_list":["post-167811","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","tag-2829","tag-2534","tag-magnet"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/167811"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2109"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=167811"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/167811\/revisions"}],"predecessor-version":[{"id":168127,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/167811\/revisions\/168127"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/167816"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=167811"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=167811"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=167811"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}