{"id":168421,"date":"2019-02-28T07:51:41","date_gmt":"2019-02-27T23:51:41","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=168421"},"modified":"2019-03-01T00:14:15","modified_gmt":"2019-02-28T16:14:15","slug":"%e4%b8%ad%e7%a7%91%e9%99%a2%e7%89%a9%e7%90%86%e6%89%80%e6%9c%80%e6%96%b0nature%e4%b8%ba%e6%8b%93%e6%89%91%e7%94%b5%e5%ad%90%e6%9d%90%e6%96%99%e7%bc%96%e7%9b%ae","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=168421","title":{"rendered":"\u4e2d\u79d1\u9662\u7269\u7406\u6240\u6700\u65b0Nature:\u4e3a\u62d3\u6251\u7535\u5b50\u6750\u6599\u7f16\u76ee"},"content":{"rendered":"<p><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/p>\n<p>\u7852\u5316\u94cb\u7b49\u62d3\u6251\u7535\u5b50\u6750\u6599\u5728\u5757\u4f53\u7b49\u72b6\u6001\u4e2d\u5e38\u5e38\u5448\u73b0\u51fa\u8d85\u5e38\u89c4\u7ebf\u6027\u54cd\u5e94\u6027\u80fd\uff0c\u8fd9\u7c7b\u72ec\u7279\u73b0\u8c61\u56e0\u5176\u5728\u9ad8\u6027\u80fd\u7535\u5b50\u5668\u4ef6\u548c\u91cf\u5b50\u8ba1\u7b97\u7b49\u9886\u57df\u7684\u6f5c\u5728\u5e94\u7528\u800c\u53d7\u5230\u57fa\u7840\u7814\u7a76\u548c\u5e94\u7528\u63a2\u7d22\u9886\u57df\u7684\u70ed\u5207\u5173\u6ce8\u3002\u7136\u800c\uff0c\u7531\u4e8e\u96be\u4ee5\u540c\u65f6\u5177\u5907\u4e30\u5bcc\u7684\u6750\u6599\u7ecf\u9a8c\u548c\u5148\u8fdb\u7684\u7406\u8bba\u5de5\u5177\uff0c\u76ee\u524d\u7684\u7814\u7a76\u5de5\u4f5c\u5e38\u5e38\u53d7\u9650\u4e8e\u62d3\u6251\u4e0d\u53d8\u91cf\u7684\u8ba1\u7b97\u96be\u5ea6\u800c\u65e0\u6cd5\u6df1\u5165\u5f00\u5c55\u3002<\/p>\n<p>\u3010<strong>\u6210\u679c\u7b80\u4ecb<\/strong>\u3011<\/p>\n<p>\u65e5\u524d\uff0c<strong>\u4e2d\u56fd\u79d1\u5b66\u9662\u7269\u7406\u7814\u7a76\u6240\u5317\u4eac\u51dd\u805a\u6001\u7269\u7406\u56fd\u5bb6\u7814\u7a76\u4e2d\u5fc3\u7684<\/strong><strong>\u7fc1\u7ea2\u660e\u526f\u7814\u7a76\u5458\u4ee5\u53ca<\/strong><strong>\u65b9\u8fb0\u7814\u7a76\u5458<\/strong>\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba\u53d1\u8868\u6587\u7ae0\u4ecb\u7ecd\u4e86\u4e00\u79cd\u80fd\u591f\u9ad8\u6548\u5206\u6790\u975e\u78c1\u6027\u6750\u6599\u4e2d\u975e\u5e73\u51e1\u80fd\u5e26\u62d3\u6251\u5b66\uff08Nontrivial band algorithm\uff09\u7684\u81ea\u52a8\u5316\u7b97\u6cd5\u3002\u8fd9\u4e00\u7b97\u6cd5\u662f\u901a\u8fc7\u7814\u7a76\u5360\u636e\u6001\u5bf9\u79f0\u6027\u4e0e\u62d3\u6251\u4e0d\u53d8\u91cf\u4e4b\u95f4\u7684\u5173\u7cfb\u800c\u5efa\u7acb\u7684\u3002\u57fa\u4e8e\u8be5\u7b97\u6cd5\uff0c\u7814\u7a76\u4eba\u5458\u572839519\u4e2d\u6750\u6599\u4e2d\u53d1\u73b0\u67098056\u79cd\u6750\u6599\u662f\u62d3\u6251\u975e\u5e73\u51e1\u7684\uff0c\u4e0d\u4ec5\u5982\u6b64\uff0c\u901a\u8fc7\u4ea4\u4e92\u5f0f\u7f51\u9875\u754c\u9762\uff0c\u8fd9\u4e9b\u88ab\u53d1\u73b0\u7684\u6750\u6599\u5747\u53ef\u88ab\u67e5\u8be2\u7814\u7a76\u3002\u8fd9\u4e00\u5de5\u4f5c\u5927\u5927\u62d3\u5bbd\u4e86\u4eba\u4eec\u5bf9\u4e8e\u975e\u5e73\u51e1\u62d3\u6251\u5b66\u7684\u8ba4\u8bc6\u30022019\u5e7402\u670827\u65e5\uff0c\u76f8\u5173\u6210\u679c\u4ee5\u9898\u4e3a\u201c<strong>Catalogue of topological electronic materials<\/strong>\u201d\u7684\u6587\u7ae0\u5728\u7ebf\u53d1\u8868\u5728<strong>Nature<\/strong>\u4e0a\u3002<\/p>\n<p>\u3010<strong>\u56fe\u6587\u5bfc\u8bfb<\/strong>\u3011<\/p>\n<p><strong>\u56fe1 <\/strong><strong>\u81ea\u52a8\u8bca\u65ad\u7b97\u6cd5\u6d41\u7a0b\u56fe<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-168422\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/1-30.jpg\" alt=\"\" width=\"600\" height=\"250\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/1-30.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/1-30-300x125.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u56fe2 <\/strong><strong>\u5bf9\u5bfc\u5e26\u548c\u4ef7\u5e26\u7684\u89e3\u91ca\u548c\u5b9a\u4e49<\/strong> <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-168423\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/2-29.jpg\" alt=\"\" width=\"600\" height=\"132\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/2-29.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/2-29-300x66.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u56fe3 \u4e94\u79cd\u7c7b\u578b\u7684\u62d3\u6251\u6750\u6599<\/strong> <img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-168424\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/3-28.jpg\" alt=\"\" width=\"600\" height=\"341\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/3-28.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/02\/3-28-300x171.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/www.nature.com\/articles\/s41586-019-0944-6\">Catalogue of topological electronic materials<\/a>\uff08Nature, 2018, DOI: 10.1038\/s41586-019-0944-6\uff09<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4eba\u5b66\u672f\u7ec4NanoCJ\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u7f16\u8f91\u6574\u7406\u3002<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u7852\u5316\u94cb\u7b49\u62d3\u6251\u7535\u5b50\u6750\u6599\u5728\u5757\u4f53\u7b49\u72b6\u6001\u4e2d\u5e38\u5e38\u5448\u73b0\u51fa\u8d85\u5e38\u89c4\u7ebf\u6027\u54cd\u5e94\u6027\u80fd\uff0c\u8fd9\u7c7b\u72ec\u7279\u73b0\u8c61\u56e0\u5176\u5728\u9ad8\u6027\u80fd\u7535\u5b50\u5668\u4ef6\u548c\u91cf\u5b50\u8ba1\u7b97\u7b49\u9886\u57df\u7684\u6f5c\u5728\u5e94\u7528\u800c\u53d7\u5230\u57fa\u7840\u7814\u7a76\u548c\u5e94\u7528\u63a2\u7d22\u9886\u57df&#8230;<\/p>\n","protected":false},"author":1076,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-168421","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/168421"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/1076"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=168421"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/168421\/revisions"}],"predecessor-version":[{"id":168425,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/168421\/revisions\/168425"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=168421"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=168421"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=168421"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}