{"id":182952,"date":"2019-08-11T06:29:24","date_gmt":"2019-08-10T22:29:24","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=182952"},"modified":"2019-08-10T15:29:33","modified_gmt":"2019-08-10T07:29:33","slug":"%e4%b8%8d%e6%ad%a222-5%ef%bc%81%e8%b6%85%e9%ab%98%e6%95%88%e9%92%99%e9%92%9b%e7%9f%bf%e5%a4%aa%e9%98%b3%e8%83%bd%e7%94%b5%e6%b1%a0%e7%9b%98%e7%82%b9","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=182952","title":{"rendered":"\u4e0d\u6b6222.5%\uff01\u8d85\u9ad8\u6548\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u76d8\u70b9"},"content":{"rendered":"<p>\u65e5\u76ca\u67af\u7aed\u7684\u5316\u77f3\u80fd\u6e90\u5df2\u7ecf\u65e0\u6cd5\u6ee1\u8db3\u6301\u7eed\u589e\u957f\u7684\u80fd\u6e90\u9700\u6c42\uff0c\u5168\u7403\u80fd\u6e90\u5371\u673a\u6b63\u5728\u52a0\u5267\uff0c\u56e0\u800c\u5927\u529b\u5f00\u53d1\u6e05\u6d01\u518d\u751f\u80fd\u6e90\u5df2\u7ecf\u8feb\u5728\u7709\u776b\u3002\u53d6\u4e4b\u4e0d\u5c3d\u7528\u4e4b\u4e0d\u7aed\u7684\u592a\u9633\u80fd\u662f\u4f17\u591a\u53ef\u6301\u7eed\u80fd\u6e90\u4e2d\u6781\u5176\u91cd\u8981\u7684\u4e00\u73af\uff0c\u5176\u4e2d\u5229\u7528\u592a\u9633\u7684\u70ed\u8f90\u5c04\u548c\u5149\u8f90\u5c04\u662f\u6700\u5e7f\u6cdb\u7684\u3002\u592a\u9633\u80fd\u53d1\u7535\u6280\u672f\u662f\u6700\u53d7\u6b22\u8fce\u7684\u592a\u9633\u80fd\u5229\u7528\u65b9\u5f0f\u3002<\/p>\n<h2 style=\"text-align: center;\"><span style=\"color: #000080;\"><strong><b>\u8ffd\u9010\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u7684\u6548\u7387\u6781\u9650<\/b><\/strong><\/span><\/h2>\n<h4><strong>\u56fe1\u00a0\u4e0d\u540c\u79cd\u7c7b\u592a\u9633\u80fd\u7535\u6c60\u7684S-Q\u6548\u7387\u6781\u9650\uff08<\/strong><strong>\u9009\u81eaScience<\/strong><strong>\uff09<\/strong><\/h4>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182953 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72471-13.png\" alt=\"\" width=\"680\" height=\"246\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72471-13.png 680w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72471-13-300x109.png 300w\" sizes=\"(max-width: 680px) 100vw, 680px\" \/><\/p>\n<p>\u5728\u6ca1\u6709\u975e\u8f90\u5c04\u91cd\u7ec4\u7684\u60c5\u51b5\u4e0b\uff0c\u5177\u67091.1~1.4 eV\u5e26\u9699\uff08Eg\uff09\u7684\u5355\u7ed3\u592a\u9633\u80fd\u7535\u6c60Shockley-Queisser\u6548\u7387\u6781\u9650\u7ea6\u4e3a33\uff05\uff0c\u8fd9\u8868\u660e\u7ea6\u536067\uff05\u7684\u592a\u9633\u80fd\u91cf\u5bf9\u592a\u9633\u80fd\u53d1\u7535\u6ca1\u6709\u8d21\u732e\u3002\u56e0\u6b64\uff0c\u5c3d\u6700\u5927\u53ef\u80fd\u53d1\u6398\u592a\u9633\u80fd\u7535\u6c60\u7684\u6548\u7387\u6f5c\u529b\u663e\u5f97\u5c24\u4e3a\u91cd\u8981\u3002\u76ee\u524d\uff0c\u6ee1\u8db375%\u4ee5\u4e0aS-Q\u6548\u7387\u6781\u9650\u7684\u5355\u7ed3\u5149\u4f0f\u7535\u6c60\u4ec5\u6709\u56db\u79cd\uff0c\u5206\u522b\u4e3a\u5355\u6676\u7845\u7535\u6c60\u3001GaAs\u7535\u6c60\u3001GaInP\u7535\u6c60\u4ee5\u53ca\u9499\u949b\u77ff\u7535\u6c60\u3002<\/p>\n<h4><strong>\u56fe2\u00a0\u4e0d\u540c\u5e26\u9699\u548c\u7ec4\u5206\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u7684S-Q\u6548\u7387\u6781\u9650\uff08\u81ea\u5236\uff09<\/strong><\/h4>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182954 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72472-12.png\" alt=\"\" width=\"680\" height=\"362\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72472-12.png 680w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72472-12-300x160.png 300w\" sizes=\"(max-width: 680px) 100vw, 680px\" \/><\/p>\n<p>\u4e0d\u540c\u4e8e\u4f20\u7edf\u5149\u4f0f\u6280\u672f\uff0c\u9499\u949b\u77ff\u592a\u9633\u80fd\u6280\u672f\u662f\u4e00\u79cd\u65b0\u578b\u4f4e\u6210\u672c\u5149\u4f0f\u6280\u672f\uff0c\u8be5\u6280\u672f\u8fde\u7eed\u6570\u5e74\u88ab\u5168\u7403\u5404\u5927\u6743\u5a01\u6742\u5fd7\u91cd\u70b9\u62a5\u9053\u3002\u56e0\u6b64\uff0c\u9499\u949b\u77ff\u592a\u9633\u80fd\u6280\u672f\u6709\u671b\u98a0\u8986\u73b0\u6709\u7684\u592a\u9633\u80fd\u53d1\u7535\u5e02\u573a\u3002\u4f17\u6240\u5468\u77e5\uff0c\u9499\u949b\u77ff\u6750\u6599\u7684\u7ec4\u5206\u9ad8\u5ea6\u53ef\u8c03\uff0c\u5e26\u9699\u80fd\u57281.2~2.3 eV\u8303\u56f4\u5185\u4efb\u610f\u8c03\u8282\u3002\u4e0d\u540c\u5e26\u9699\u548c\u7ec4\u5206\u7684\u9499\u949b\u77ff\u6750\u6599\u8868\u73b0\u51fa\u5929\u5dee\u5730\u522b\u7684\u5149\u4f0f\u6027\u80fd\uff0c\u8fd9\u4e5f\u51f8\u663e\u51fa\u9499\u949b\u77ff\u6750\u6599\u6781\u5176\u72ec\u7279\u7684\u5149\u7535\u6027\u80fd\u3002\u56fe2\u5217\u51fa\u4e86\u4e00\u4e9b\u4e0d\u540c\u5e26\u9699\u548c\u7ec4\u5206\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u7684S-Q\u6548\u7387\u6781\u9650\uff0c\u5176\u4e2d1.52~1.57 eV\u7684FAMA\u4f53\u7cfb\u9499\u949b\u77ff\u7535\u6c60\u6700\u9ad8\u6548\u7387\u5df2\u8d85\u8fc775%\u00a0\u7684\u76f8\u5e94S-Q\u6548\u7387\u6781\u9650\uff0c\u800c1.54 eV-MAPbI<sub>3<\/sub>\u30011.54 eV-CsPbI<sub>2<\/sub>Br\u30012.32 eV-CsPbBr<sub>3<\/sub>\u548c1.65 eV-CsFAMA\u9499\u949b\u77ff\u7535\u6c60\u6548\u7387\u4e5f\u5df2\u975e\u5e38\u63a5\u8fd175%\u7684\u76f8\u5e94\u00a0S-Q\u6548\u7387\u6781\u9650\u3002\u4e0d\u5bb9\u5ffd\u89c6\u7684\u4e00\u70b9\u662f\uff0c\u7a84\u5e26\u9699\u9499\u949b\u77ff\u7535\u6c60\u867d\u7136\u5177\u6709\u66f4\u9ad8\u7684S-Q\u6548\u7387\u6781\u9650\u503c\uff0c\u4f46\u5b9e\u9645\u6700\u9ad8\u6548\u7387\u8f83\u4e0d\u7406\u60f3\uff0c\u5b58\u5728\u660e\u663e\u7684\u5dee\u8ddd\u3002\u7efc\u4e0a\u6240\u8ff0\uff0c\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u7684\u6548\u7387\u53d1\u5c55\u6f5c\u529b\u5de8\u5927\uff0c\u8ffd\u9010\u66f4\u9ad8\u7684\u6548\u7387\u52bf\u5728\u5fc5\u7136\u3002<\/p>\n<h2 style=\"text-align: center;\"><span style=\"color: #000080;\"><strong><b>22.5%-<\/b><\/strong><strong><b>\u8d85\u9ad8\u6548\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u7684\u6548\u7387\u5206\u6c34\u5cad<\/b><\/strong><\/span><\/h2>\n<h4><strong>\u56fe3\u00a0\u6709\u673a-\u65e0\u673a\u6742\u5316\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u7684\u6548\u7387\u53d1\u5c55<\/strong><strong>\uff08\u81ea\u5236\uff09<\/strong><\/h4>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182955 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72473-13.png\" alt=\"\" width=\"680\" height=\"310\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72473-13.png 680w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72473-13-300x137.png 300w\" sizes=\"(max-width: 680px) 100vw, 680px\" \/><\/p>\n<p>2009\u5e74\uff0c\u7b2c\u4e00\u5757\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u8bde\u751f\uff0c\u6548\u7387\u4ec5\u4e3a3.8%\u30022019\u5e74\uff0c\u6700\u65b0\u7684\u9499\u949b\u77ff\u7535\u6c60\u6548\u7387\u5df2\u88ab\u5237\u65b0\u81f325.2%\u3002\u77ed\u77ed\u5341\u5e74\u5185\uff0c\u968f\u7740\u9ad8\u6548\u9499\u949b\u77ff\u7535\u6c60\u7684\u6d77\u91cf\u6d8c\u5165\uff0c\u9499\u949b\u77ff\u7535\u6c60\u7684\u5e73\u5747\u6548\u7387\u95e8\u69db\u5728\u4e0d\u65ad\u62ac\u5347\u3002\u663e\u7136\u5730\uff0c\u666e\u901a\u9ad8\u6548\u9499\u949b\u77ff\u7535\u6c60\u5df2\u7ecf\u65e0\u6cd5\u6ee1\u8db3\u5f53\u524d\u7684\u6548\u7387\u9700\u6c42\uff0c\u8fd9\u4e5f\u4fc3\u4f7f\u4e86\u8d85\u9ad8\u6548\u9499\u949b\u77ff\u7535\u6c60\u7684\u51fa\u73b0\u3002\u56e0\u6b64\uff0c\u672c\u6587\u9009\u53d6\u591a\u6676\u7845\u7535\u6c60\u548cCdTe\u8584\u819c\u7535\u6c60\u7684\u6700\u9ad8\u6548\u7387\u4f5c\u4e3a\u8bc4\u4ef7\u8d85\u9ad8\u6548\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u7684\u53c2\u6bd4\u6548\u7387\u503c\uff0c\u56e0\u4e3a\u591a\u6676\u7845\u7535\u6c60\u4ecd\u662f\u6676\u7845\u5149\u4f0f\u5e02\u573a\u5360\u6bd4\u6700\u5927\u7684\u5149\u4f0f\u6280\u672f\uff0c\u5b83\u7684\u6700\u9ad8\u6548\u7387\u4e3a22.3%\u4e14\u8be5\u6548\u7387\u8fd1\u4e24\u5e74\u672a\u88ab\u5237\u65b0\uff0c\u800cCdTe\u8584\u819c\u7535\u6c60\u5219\u662f\u8584\u819c\u5149\u4f0f\u5e02\u573a\u5360\u6bd4\u6700\u5927\u7684\u5149\u4f0f\u6280\u672f\uff0c\u5b83\u7684\u6700\u9ad8\u6548\u7387\u4e3a22.1%\u4e14\u8be5\u6548\u7387\u8fd1\u56db\u5e74\u672a\u88ab\u5237\u65b0\u3002\u56e0\u6b64\uff0c\u9009\u53d6\u8fd9\u4e24\u79cd\u53c2\u6bd4\u6548\u7387\u5c31\u518d\u5408\u9002\u4e0d\u8fc7\u4e86\u3002\u7efc\u4e0a\u6240\u8ff0\uff0c\u9009\u53d622.5%\u4f5c\u4e3a\u8d85\u9ad8\u6548\u9499\u949b\u77ff\u7535\u6c60\u7684\u6548\u7387\u5206\u5272\u70b9\u4f3c\u4e4e\u662f\u4e00\u79cd\u5b8c\u7f8e\u7684\u5e73\u8861\uff0c\u65e2\u80fd\u7a0d\u7a0d\u8d85\u8fc7\u53c2\u6bd4\u6548\u7387\u503c\uff0c\u53c8\u80fd\u8fc7\u6ee4\u6389\u5927\u591a\u6570\u9ad8\u6548\u9499\u949b\u77ff\u7535\u6c60\u6548\u7387\u503c\u3002<\/p>\n<h2 style=\"text-align: center;\"><span style=\"color: #000080;\"><strong><b>\u8d85\u9ad8\u6548\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u6c47\u603b<\/b><\/strong><\/span><\/h2>\n<h4>\u56fe4 \u8d85\u9ad8\u6548\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u6c47\u603b<strong>\uff08\u81ea\u5236\uff09<\/strong><\/h4>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182956 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72474-13.png\" alt=\"\" width=\"680\" height=\"446\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72474-13.png 680w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72474-13-300x197.png 300w\" sizes=\"(max-width: 680px) 100vw, 680px\" \/><\/p>\n<p>\u4ece\u4e0a\u8868\u6765\u770b\uff0c\u8d85\u9ad8\u6548\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u7684\u6700\u4f4e\u6548\u7387\u503c\u4e3a22.5%\uff0c\u6700\u9ad8\u6548\u7387\u503c\u4e3a25.2%\uff0c\u4e24\u8005\u5747\u4e3aNewport\u8ba4\u8bc1\u6548\u7387\uff0c\u6548\u7387\u76f8\u5dee2.7\u4e2a\u767e\u5206\u70b9\u3002\u4e03\u5bb6\u7814\u7a76\u673a\u6784\u5148\u540e\u62a5\u9053\u51fa\u8d85\u9ad8\u6548\u9499\u949b\u77ff\u7535\u6c60\u6548\u7387\uff0c\u5176\u4e2d\u97e9\u56fd\u7814\u7a76\u673a\u6784\u6700\u591a\uff0c\u663e\u793a\u51fa\u5341\u5206\u5f3a\u52b2\u7684\u9499\u949b\u77ff\u7535\u6c60\u7814\u53d1\u5b9e\u529b\u3002\u8d85\u9ad8\u6548\u9499\u949b\u77ff\u7535\u6c60\u57fa\u672c\u662f\u5728\u8fd1\u4e09\u5e74\u624d\u6e10\u6e10\u51fa\u73b0\uff0c\u5c1a\u6709\u5f88\u5927\u7684\u53d1\u5c55\u7a7a\u95f4\uff0c\u672a\u6765\u4f1a\u6709\u66f4\u591a\u65b0\u7684\u7814\u7a76\u673a\u6784\u52a0\u5165\u5230\u8be5\u884c\u5217\u4e2d\u3002<\/p>\n<h2 style=\"text-align: center;\"><span style=\"color: #000080;\"><strong><b>\u4e03\u5927\u7814\u7a76\u673a\u6784\u7684\u9ad8\u6548\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u6587\u732e\u63a8\u8350<\/b><\/strong><\/span><\/h2>\n<h3>\u673a\u6784\u4e00\u3001\u9ebb\u7701\u7406\u5de5\u5b66\u9662&amp;\u97e9\u56fd\u5316\u5b66\u6280\u672f\u7814\u7a76\u6240 \u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0<\/h3>\n<p>An Interface Stabilized Perovskite Solar Cell with High Stabilized Efficiency\u00a0and Low Voltage Loss\u00a0(Energy Environmental Science, 2019, DOI: 10.1039\/C9EE00751B)\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0<strong><b>22.6%(<\/b><\/strong><strong><b>\u8ba4\u8bc1<\/b><\/strong><strong><b>)<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182960 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72475-10.png\" alt=\"\" width=\"520\" height=\"419\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72475-10.png 520w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72475-10-300x242.png 300w\" sizes=\"(max-width: 520px) 100vw, 520px\" \/><\/p>\n<p>\u4f17\u6240\u5468\u77e5\uff0c\u4f7f\u7528\u6781\u6027\u8d28\u5b50\u6eb6\u5242\uff08\u4e3b\u8981\u662f\u5f02\u4e19\u9187\uff09\u7684\u5e38\u89c4\u6c89\u79ef\u65b9\u6cd5\u5bfc\u81f4\u4e0b\u90e8\u9499\u949b\u77ff\u5c42\u7684\u4e0d\u7a33\u5b9a\u548c\u5668\u4ef6\u6027\u80fd\u7684\u964d\u4f4e\u3002\u672c\u6587\u62a5\u9053\u4e86\u4e00\u79cd\u72ec\u7279\u7684\u9009\u62e9\u6027\u524d\u4f53\u6eb6\u89e3\uff08SPD\uff09\u7b56\u7565\uff0c\u5373\u4f7f\u7528\u524d\u4f53\/\u6eb6\u5242\u7ec4\u5408\uff08\u76f4\u94fe\u70f7\u57fa\u6eb4\u5316\u94f5\/\u6c2f\u4eff\uff09\u5728\u9499\u949b\u77ff\u8584\u819c\u4e0a\u539f\u4f4d\u5408\u6210\u5c42\u72b6\u9499\u949b\u77ff\uff08LP\uff09\u3002\u503c\u5f97\u6ce8\u610f\u7684\u662f\uff0cLP\u524d\u4f53\u65e0\u6cd5\u6eb6\u4e8e\u6c2f\u82ef\u6216\u82ef\u6eb6\u5242\u3002\u8fd9\u79cdLP\u949d\u5316\u5c42\uff083D\/LP\u5f02\u8d28\u7ed3\uff09\u53ef\u4ee5\u6709\u6548\u5730\u949d\u5316\u754c\u9762\u548c\u6676\u754c\u7f3a\u9677\uff0c\u6700\u5c0f\u5316\u975e\u8f90\u5c04\u590d\u5408\u4f4d\u70b9\uff0c\u5e76\u9632\u6b62\u9499\u949b\u77ff\u754c\u9762\u5904\u7684\u8f7d\u6d41\u5b50\u731d\u706d\uff0c\u5e76\u589e\u52a0\u5176\u9632\u6f6e\u6027\u3002\u76f8\u6bd4\u4e8e\u4f20\u7edf\u65b9\u6cd5\uff0cSPD\u7b56\u7565\u80fd\u591f\u6700\u6709\u6548\u5730\u5c06\u5404\u79cd\u949d\u5316\u5c42\u5408\u6210\u52303D\u9499\u949b\u77ff\u5c42\u4e0a\uff0c\u800c\u4e0d\u4f1a\u7834\u574f\u4e0b\u9762\u76843D\u9499\u949b\u77ff\u5c42\uff0c\u5e76\u6291\u5236\u9499\u949b\u77ff\u03b4\u76f8\u548c\u975e\u6676\u76f8\u7684\u5f62\u6210\u6765\u6700\u5927\u5316\u8bbe\u5907\u6027\u80fd\u548c\u7a33\u5b9a\u6027\u3002\u4f7f\u7528SPD\u7b56\u7565\u5bfc\u81f4\u51a0\u519b\u5668\u4ef6\u7684\u529f\u7387\u8f6c\u6362\u6548\u7387\u9ad8\u8fbe23.4\uff05\uff0c\u5e76\u83b7\u5f9722.6\uff05\u7684\u8ba4\u8bc1\u7a33\u6001PCE\uff0c\u8fd9\u662f\u8fc4\u4eca\u4e3a\u6b62\u4e3a\u5df2\u62a5\u9053\u7684\u6700\u9ad8\u8ba4\u8bc1\u7a33\u6001PCE\uff0cV<sub>oc<\/sub>\u635f\u5931\u4e3a\u4ec5\u4e3a~340 mV\uff0c\u8fd9\u4e5f\u662f\u8fc4\u4eca\u4e3a\u6b62\u5df2\u62a5\u9053\u7684\u6700\u4f4eV<sub>oc<\/sub>\u635f\u5931\uff0c\u4e14\u5177\u6709\u589e\u5f3a\u7684\u64cd\u4f5c\u7a33\u5b9a\u6027\u3002\u6b64\u5916\uff0cPSC\u663e\u793a\u51fa\u7535\u81f4\u53d1\u5149\uff08EL\uff09\u5916\u90e8\u91cf\u5b50\u6548\u7387\uff08EQE\uff09\u9ad8\u8fbe8.9\uff05\uff0c\u8fd9\u662f\u5df2\u62a5\u9053PSC\u7684\u6700\u9ad8\u503c\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182962 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72476-7.png\" alt=\"\" width=\"680\" height=\"137\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72476-7.png 680w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72476-7-300x60.png 300w\" sizes=\"(max-width: 680px) 100vw, 680px\" \/><\/p>\n<h3>\u673a\u6784\u4e8c\u3001\u97e9\u56fd\u80fd\u6e90\u7814\u7a76\u6240<\/h3>\n<p>Methylammonium Chloride Induces Intermediate Phase Stabilization for Efficient Perovskite Solar Cells\u00a0(Joule, 2019, DOI: 10.1016\/j.joule.2019.06.014)\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0<strong><b>23.5%(<\/b><\/strong><strong><b>\u8ba4\u8bc1<\/b><\/strong><strong><b>)<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182963 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72477-7.png\" alt=\"\" width=\"520\" height=\"520\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72477-7.png 520w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72477-7-150x150.png 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72477-7-300x300.png 300w\" sizes=\"(max-width: 520px) 100vw, 520px\" \/><\/p>\n<p>\u672c\u6587\u7cfb\u7edf\u5730\u7814\u7a76\u4e86\u7532\u57fa\u6c2f\u5316\u94f5\uff08MACl\uff09\u6dfb\u52a0\u5242\u5728\u7532\u8112\u7898\u5316\u94c5\uff08FAPbI<sub>3<\/sub>\uff09\u9499\u949b\u77ff\u4e2d\u7684\u4f5c\u7528\u3002\u6dfb\u52a0MACl\u5236\u5907\u7684\u8584\u819c\u6676\u7c92\u5c3a\u5bf8\u589e\u5927\u4e866\u500d\u3002\u6709\u8da3\u7684\u662f\uff0c\u5728\u6ca1\u6709\u9000\u706b\u7684\u60c5\u51b5\u4e0b\uff0cMACl\u4ec5\u901a\u8fc7\u9633\u79bb\u5b50\u4f4d\u70b9\u53d6\u4ee3\u5c31\u80fd\u6709\u6548\u5730\u7a33\u5b9aFAPbI<sub>3<\/sub>\u4e2d\u95f4\u4f53\u7684\u03b1\u76f8\uff0c\u4ece\u800c\u5236\u9020\u51fa\u5177\u6709\u8d85\u7eaf\u03b1\u76f8\u7684\u9ad8\u7ed3\u6676\u5ea6FAPbI<sub>3<\/sub>\u9499\u949b\u77ff\uff0c\u5149\u81f4\u53d1\u5149\u5bff\u547d\u589e\u52a0\u4e864.3\u500d\u3002\u5bc6\u5ea6\u6cdb\u51fd\u7406\u8bba\uff08DFT\uff09\u5f97\u51fa\u9499\u949b\u77ff\u7ed3\u6784\u7684\u5f62\u6210\u4e0eMACl\u7684\u63ba\u5165\u91cf\u6709\u5173\u3002\u5f53\u6dfb\u52a040\u6469\u5c14\uff05MACl\u65f6\u4f18\u5316\u7684\u592a\u9633\u80fd\u7535\u6c60\u83b7\u5f97\u4e8624.02\uff05\u7684\u6700\u9ad8\u6548\u7387\uff0c\u8ba4\u8bc1\u6548\u7387\u4e3a23.48\uff05\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182964 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72478-5.png\" alt=\"\" width=\"680\" height=\"137\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72478-5.png 680w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72478-5-300x60.png 300w\" sizes=\"(max-width: 680px) 100vw, 680px\" \/><\/p>\n<h3>\u673a\u6784\u4e09\u3001\u97e9\u56fd\u5316\u5b66\u6280\u672f\u7814\u7a76\u6240<\/h3>\n<p>A fluorene-terminated hole-transporting material for highly efficient and stable perovskite solar cells\u00a0(Nature Energy, 2018, DOI: 10.1038\/s41560-018-0200-6)\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0<strong><b>22.6%(<\/b><\/strong><strong><b>\u8ba4\u8bc1<\/b><\/strong><strong><b>)<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182965 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72479-5.png\" alt=\"\" width=\"520\" height=\"432\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72479-5.png 520w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u72479-5-300x249.png 300w\" sizes=\"(max-width: 520px) 100vw, 520px\" \/><\/p>\n<p>\u672c\u6587\u5408\u6210\u4e86\u4e00\u79cd\u82b4\u5c01\u7aef\u7684HTM\u00a0(N2,N2\u2019,N7,N7\u2019-tetrakis(9,9-dimethyl-9H-fluoren-2-yl)-N2,N2\u2019,N7,N7\u2019-tetrakis(4-methoxyphenyl)-9,9\u2019-spirobi[fluorene]-2,2\u2019,7,7\u2019-tetraamine, \u7b80\u5199DM\uff0c\u5177\u6709\u5fae\u8c03\u7684HOMO\u6c34\u5e73\u548c\u9ad8\u73bb\u7483\u5316\u8f6c\u53d8\u6e29\u5ea6T<sub>g<\/sub>\uff08~160\u2103\uff09\uff0c\u8fdb\u800c\u63d0\u9ad8PCS\u7684VOC\u503c\u548c\u70ed\u7a33\u5b9a\u6027\u3002\u57fa\u4e8eDM HTM\u7684\u5149\u4f0f\u5668\u4ef6\u83b7\u5f9723.2\uff05\u7684\u51a0\u519b\u6548\u7387\uff0c\u8ba4\u8bc1\u6548\u7387\u8fbe\u5230\u4e8622.6\uff05\u3002\u6b64\u5916\uff0c\u5177\u6709DM\u7684\u5668\u4ef6\u663e\u793a\u51fa\u6bd4Spiro-OMeTAD\u88c5\u7f6e\u66f4\u597d\u7684\u70ed\u7a33\u5b9a\u6027\uff0c\u572860\u00a0\u2103\u70ed\u9000\u706b\u8d85\u8fc7500\u5c0f\u540e\u4fdd\u6301\u5176\u521d\u59cb\u6027\u80fd\u7684\u7ea695%\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182966 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724710-5.png\" alt=\"\" width=\"680\" height=\"137\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724710-5.png 680w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724710-5-300x60.png 300w\" sizes=\"(max-width: 680px) 100vw, 680px\" \/><\/p>\n<p>Efficient, stable and scalable perovskite solar cells using poly(3-hexylthiophene)\u00a0(Nature, 2019, DOI: 10.1038\/s41586-019-1036-3)\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0<strong><b>22.7%(<\/b><\/strong><strong><b>\u8ba4\u8bc1<\/b><\/strong><strong><b>)<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182967 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724711-4.png\" alt=\"\" width=\"520\" height=\"481\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724711-4.png 520w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724711-4-300x278.png 300w\" sizes=\"(max-width: 520px) 100vw, 520px\" \/><\/p>\n<p>\u672c\u6587\u63d0\u51fa\u4e86\u4e00\u79cd\u4f7f\u7528\u65e0\u63ba\u6742P3HT\u4f5c\u4e3a\u7a7a\u7a74\u4f20\u8f93\u6750\u6599\u7684\u9ad8\u6548\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\uff0c\u5e76\u91c7\u7528\u6b63\u5df1\u57fa\u4e09\u7532\u57fa\u6eb4\u5316\u94f5\u5728\u7a84\u5e26\u9699\u9499\u949b\u77ff\u5149\u5438\u6536\u5c42\u7684\u9876\u90e8\u8868\u9762\u539f\u4f4d\u53cd\u5e94\u5f62\u6210\u4e00\u5c42\u8584\u7684\u5bbd\u5e26\u9699\u5364\u5316\u7269\u9499\u949b\u77ff\u3002\u4f18\u5316\u8bbe\u5907\u5b9e\u73b0\u4e8623.3%\u7684\u51a0\u519bPCE\uff0c\u8ba4\u8bc1\u6548\u7387\u4e3a22.7\uff05\uff0c\u4e14\u5728\u6ca1\u6709\u5c01\u88c5\u7684\u60c5\u51b5\u4e0b\uff0c\u8868\u73b0\u51fa85\uff05\u76f8\u5bf9\u6e7f\u5ea6\u4e0b\u7684\u4f18\u5f02\u7a33\u5b9a\u6027\uff0c\u5c01\u88c5\u5668\u4ef6\u5728\u5ba4\u6e291-Sun\u7167\u5c041,370\u5c0f\u65f6\u540e\u4fdd\u630195\uff05\u7684\u521d\u59cb\u6548\u7387\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182968 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724712-3.png\" alt=\"\" width=\"680\" height=\"137\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724712-3.png 680w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724712-3-300x60.png 300w\" sizes=\"(max-width: 680px) 100vw, 680px\" \/><\/p>\n<h3>\u673a\u6784\u56db\u3001\u4e2d\u56fd\u79d1\u5b66\u9662\u534a\u5bfc\u4f53\u7814\u7a76\u6240<\/h3>\n<p>Surface passivation of perovskite film for efficient\u00a0solar cells\u00a0(Nature Photonics, 2019, DOI: 10.1038\/s41566-019-0398-2)\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0<strong><b>23.3%(<\/b><\/strong><strong><b>\u8ba4\u8bc1<\/b><\/strong><strong><b>)<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182969 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724713-2.png\" alt=\"\" width=\"520\" height=\"386\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724713-2.png 520w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724713-2-300x223.png 300w\" sizes=\"(max-width: 520px) 100vw, 520px\" \/><\/p>\n<p>\u672c\u6587\u5f00\u53d1\u4e86\u4e00\u79cd\u6709\u673a\u5364\u5316\u7269\u76d0\u82ef\u4e59\u57fa\u7898\u5316\u94f5\uff08PEAI\uff09\u540e\u5904\u7406\u6df7\u5408\u9499\u949b\u77ffFA<sub>1-x<\/sub>MA<sub>x<\/sub>PbI<sub>3<\/sub>\u7684\u5de5\u827a\u7528\u4e8e\u949d\u5316\u8584\u819c\u8868\u9762\u7f3a\u9677\u3002\u4ee4\u4eba\u60ca\u8bb6\u7684\u662f\uff0c\u53ea\u6709\u6709\u673a\u5364\u5316\u7269\u76d0PEAI\u4f5c\u4e3a3D\u9499\u949b\u77ff\u7684\u66f4\u6709\u6548\u949d\u5316\u6dfb\u52a0\u5242\uff0c\u800c\u4e0d\u662f\u5728\u6700\u8fd1\u8bb8\u591a\u7814\u7a76\u4e2d\u63d0\u5230\u76842D\u5c42\u72b6\u9499\u949b\u77ffPEA<sub>2<\/sub>PbI<sub>4<\/sub>\u3002PEAI\u7684\u5b58\u5728\u51cf\u5c11\u8868\u9762\u7f3a\u9677\u548c\u6291\u5236\u975e\u8f90\u5c04\u590d\u5408\uff0c\u8fdb\u800c\u4ea7\u751f\u66f4\u9ad8\u6548\u7684\u7535\u6c60\u3002\u51a0\u519b\u5e73\u9762\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u5668\u4ef6\u53d6\u5f97\u4e8623.6%\u7684\u9ad8\u6548\u7387\uff0c\u8ba4\u8bc1\u7a33\u6001\u6548\u7387\u8fbe\u5230\u4e8623.32\uff05\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182970 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724714-2.png\" alt=\"\" width=\"680\" height=\"137\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724714-2.png 680w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724714-2-300x60.png 300w\" sizes=\"(max-width: 680px) 100vw, 680px\" \/><\/p>\n<h3>\u673a\u6784\u4e94\u3001\u6d1b\u6851\u8054\u90a6\u7406\u5de5\u5b66\u9662<\/h3>\n<p>Ultrahydrophobic 3D\/2D fluoroarene bilayer-based water-resistant perovskite solar cells with efficiencies exceeding 22%\u00a0(Science Advances, 2019, DOI: 10.1126\/sciadv.aaw2543)\u00a0\u00a0<strong><b>22.1%(<\/b><\/strong><strong><b>\u7a33\u6001<\/b><\/strong><strong><b>)<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182971 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724715-2.png\" alt=\"\" width=\"520\" height=\"501\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724715-2.png 520w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724715-2-300x289.png 300w\" sizes=\"(max-width: 520px) 100vw, 520px\" \/><\/p>\n<p>\u672c\u6587\u5c55\u793a\u4e86\u5c06\u4e94\u6c1f\u82ef\u57fa\u4e59\u57fa\u94f5\uff08FEA\uff09\u7898\u5316\u94c5[(FEA)<sub>2<\/sub>PbI<sub>4<\/sub>]\uff08\u8d85\u758f\u6c34\u60272D\u9499\u949b\u77ff\uff09\u6c89\u79ef\u52303D\u9499\u949b\u77ff\u8584\u819c\u8868\u9762\u5f62\u6210\u9ad8\u6548\u53cc\u5c423D\/2D\u67b6\u6784\u3002\u5168\u6c1f\u5316\u82ef\u5355\u5143\u8d4b\u4e88\u95f4\u9694\u5c42\u8d85\u758f\u6c34\u7279\u6027\uff0c\u4fdd\u62a4\u9499\u949b\u77ff\u5149\u6355\u83b7\u6750\u6599\u514d\u53d7\u73af\u5883\u6e7f\u6c14\u7684\u5f71\u54cd\u3002\u9664\u6b64\u4e4b\u5916\uff0c\u5168\u6c1f\u82ef\u5355\u5143\u7684\u5f15\u5165\u8d4b\u4e88\u82b3\u9999\u6838\u7535\u5b50\u6027\u8d28\uff0c\u4fc3\u8fdb\u7a7a\u7a74\u7684\u63d0\u53d6\u548c\u6291\u5236\u5c42\u95f4\u79bb\u5b50\u8fc1\u79fb\u3002\u503c\u5f97\u6ce8\u610f\u7684\u662f\uff0c\u5c42\u72b62D\u9499\u949b\u77ff(FEA)<sub>2<\/sub>PbI<sub>4<\/sub>\u7684\u5f62\u6210\u4ec5\u4ec5\u6d88\u8017\u7684\u662f\u5b58\u5728\u4e8e3D\u9499\u949b\u77ff\u5c42\u8868\u9762\u7684\u975e\u9499\u949b\u77ff\u76f8FAPbI<sub>3<\/sub>\u3002\u5b9e\u9a8c\u8bc1\u660e\u901a\u8fc7\u826f\u597d\u7684\u63a7\u5236\u5c31\u80fd\u6210\u529f\u5730\u57283D\u9499\u949b\u77ff\u5c42\u8868\u9762\u6c89\u79ef\u8d85\u758f\u6c34\u3001\u8d85\u8584\u548c\u9ad8\u5ea6\u5747\u5300\u76842D\u00a0(FEA)<sub>2<\/sub>PbI<sub>4<\/sub>\u5c42\u3002\u57fa\u4e8e\u4e94\u6c1f\u82ef\u57fa\u4e59\u57fa\u94f5\uff08FEA\uff09\u6539\u6027\u7684\u5149\u4f0f\u5668\u4ef6\u5b9e\u73b0\u4e8622.2%\u7684\u6548\u7387\uff0c\u8fd9\u662f\u5df2\u62a5\u9053\u76843D\/2D\u6df7\u5408\u7ef4\u5668\u4ef6\u7684\u6700\u9ad8\u6548\u7387\u3002\u6b64\u5916\uff0c\u672a\u5bc6\u5c01\u76843D\/2D PSC\u5728\u6f6e\u6e7f\u7a7a\u6c14\u4e2d\u8fde\u7eed\u5149\u71671000\u5c0f\u65f6\u540e\u4fdd\u630190\uff05\u7684\u521d\u59cb\u6548\u7387\uff0c\u663e\u793a\u51fa\u4f18\u5f02\u7684\u8010\u6e7f\u6027\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182972 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724716-2.png\" alt=\"\" width=\"680\" height=\"136\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724716-2.png 680w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724716-2-300x60.png 300w\" sizes=\"(max-width: 680px) 100vw, 680px\" \/><\/p>\n<h3>\u673a\u6784\u516d\u3001\u5317\u5361\u7f57\u6765\u7eb3\u5927\u5b66<\/h3>\n<p>Defect passivation in hybrid perovskite solar cells using quaternary ammonium halide anions and cations\u00a0(Nature Energy, 2017, DOI: 10.1038\/nenergy.2017.102)\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0<strong><b>20.6%(<\/b><\/strong><strong><b>\u8ba4\u8bc1<\/b><\/strong><strong><b>)<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182973 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724717-1.png\" alt=\"\" width=\"520\" height=\"390\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724717-1.png 520w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724717-1-300x225.png 300w\" sizes=\"(max-width: 520px) 100vw, 520px\" \/><\/p>\n<p>\u672c\u6587\u5c55\u793a\u4e86\u4e00\u7cfb\u5217\u5b63\u94f5\u5364\u5316\u7269\uff08QAHs\uff09\uff08NR<sub>4<\/sub><sup>+<\/sup>X<sup>&#8211;<\/sup>\u7ed3\u6784\uff0c\u5176\u4e2dR\u662f\u70f7\u57fa\u6216\u82b3\u57fa\uff0cX\u662f\u5364\u5316\u7269\uff09\u4e2d\u5e26\u8d1f\u7535\u548c\u6b63\u7535\u7684\u7ec4\u5206\u53ef\u4ee5\u6709\u6548\u5730\u949d\u5316\u4e0d\u540c\u7c7b\u578b\u6df7\u5408\u9499\u949b\u77ffOIHP\u7684\u5e26\u7535\u7f3a\u9677\uff0c\u8bc1\u660e\u4e86QAHs\u949d\u5316OIHP\u5e26\u7535\u79bb\u5b50\u7f3a\u9677\u662f\u4e00\u79cd\u666e\u9002\u6027\u7684\u949d\u5316\u65b9\u6cd5\u3002\u9ad8\u6548\u7684\u7f3a\u9677\u949d\u5316\u663e\u8457\u964d\u4f4e\u4e86\u7535\u8377\u9677\u9631\u5bc6\u5ea6\u5e76\u5ef6\u957f\u4e86\u8f7d\u6d41\u5b50\u590d\u5408\u5bff\u547d\u3002QAHs\u7f3a\u9677\u949d\u5316\u6700\u5c0f\u5316\u5668\u4ef6V<sub>oc<\/sub>\u635f\u5931\u4ec5\u4e3a0.39 V\uff0c\u5e76\u5c06\u6548\u7387\u63d0\u5347\u81f3\u6700\u9ad8\u768421.0%\uff0c\u8ba4\u8bc1\u6548\u7387\u4e3a20.6\uff05\u3002\u6b64\u5916\uff0c\u7f3a\u9677\u6108\u5408\u4e5f\u663e\u8457\u589e\u5f3a\u9499\u949b\u77ff\u8584\u819c\u7684\u73af\u5883\u7a33\u5b9a\u6027\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182974 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724718-1.png\" alt=\"\" width=\"680\" height=\"137\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724718-1.png 680w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724718-1-300x60.png 300w\" sizes=\"(max-width: 680px) 100vw, 680px\" \/><\/p>\n<h3>\u673a\u6784\u4e03\u3001\u6210\u5747\u9986\u5927\u5b66<\/h3>\n<p>CH<sub>3<\/sub>NH<sub>3<\/sub>PbI<sub>3<\/sub> and HC(NH<sub>2<\/sub>)<sub>2<\/sub>PbI<sub>3<\/sub> Powders Synthesized from Low\u2010Grade PbI<sub>2<\/sub>: Single Precursor for High-Efficiency Perovskite Solar Cells (ChemSusChem, 2018, DOI: 10.1002\/cssc.201800610)<strong><b>\u00a018.4%<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182975 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724719-1.png\" alt=\"\" width=\"520\" height=\"357\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724719-1.png 520w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724719-1-300x206.png 300w\" sizes=\"(max-width: 520px) 100vw, 520px\" \/><\/p>\n<p>\u672c\u6587\u62a5\u9053\u4e86\u4f7f\u7528\u5ec9\u4ef7\u4f4e\u54c1\u4f4d\uff0899\uff05\uff09PbI<sub>2<\/sub>\u5408\u6210\u9499\u949b\u77ff\u7c89\u672b\u4ee5\u53ca\u57fa\u4e8e\u5355\u4e00\u524d\u4f53\u7c89\u672b\u5236\u5907\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u3002FAPbI<sub>3<\/sub>\u9499\u949b\u77ff\u7c89\u672b\u662f\u7528FAI\u4e0e\u4f4e\u54c1\u4f4dPbI<sub>2<\/sub>\u5728\u4e59\u8148\u4e2d\u5408\u6210\u7684\uff0c\u5b9e\u9a8c\u53d1\u73b0\u5ba4\u6e29\u4e0b\u5408\u6210\u7684\u975e\u9499\u949b\u77ff\u03b4-FAPbI<sub>3<\/sub>\u7c89\u672b\u7684\u6eb6\u6db2\u80fd\u591f\u5bfc\u81f4\u9ed1\u8272\u9499\u949b\u77ff\u819c\uff0c\u800c\u5728150\u2103\u4e0b\u5408\u6210\u7684\u9ed1\u8272\u9499\u949b\u77ff\u03b1- FAPbI<sub>3<\/sub>\u7c89\u672b\u7684\u6eb6\u6db2\u5219\u65e0\u6cd5\u8f6c\u53d8\u6210\u9ed1\u8272\u9499\u949b\u77ff\u819c\u3002\u4f7f\u7528\u03b4- FAPbI<sub>3<\/sub>\u7c89\u672b\u5236\u5907\u7684\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u83b7\u5f97\u4e8618.4%\u7684\u51a0\u519bPCE\uff0c\u4e14\u5177\u6709\u8f83\u5c0f\u7684\u56de\u6ede\uff0c\u8868\u660e\u4f7f\u7528\u03b4- FAPbI<sub>3<\/sub>\u7c89\u672b\u5236\u5907\u7684FAPbI<sub>3<\/sub>\u819c\u4e2d\u7684\u7f3a\u9677\u8f83\u5c11\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-182976 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724720-1.png\" alt=\"\" width=\"680\" height=\"92\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724720-1.png 680w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/08\/\u56fe\u724720-1-300x41.png 300w\" sizes=\"(max-width: 680px) 100vw, 680px\" \/><\/p>\n<h3><strong><b>\u8d85\u9ad8\u6548\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u57fa\u672c\u7279\u5f81\u603b\u7ed3<\/b><\/strong><\/h3>\n<p>\uff081\uff09\u6240\u6709\u7814\u7a76\u673a\u6784\u91c7\u7528\u7684\u9499\u949b\u77ff\u5438\u5149\u5242\u5e26\u9699\u4e3a1.52~1.57 eV\uff1b<\/p>\n<p>\uff082\uff09\u9664\u5317\u5361\u7f57\u6765\u7eb3\u5927\u5b66\u548c\u4e2d\u56fd\u79d1\u5b66\u9662\u534a\u5bfc\u4f53\u7814\u7a76\u6240\u91c7\u7528\u7684\u662f\u987a\u5f0f\u5e73\u9762n-i-p\u7ed3\u6784\uff08SnO<sub>2<\/sub>\uff09\u5916\uff0c\u5176\u4f59\u7814\u7a76\u673a\u6784\u5747\u662f\u987a\u5f0f\u4ecb\u5b54n-i-p\u7ed3\u6784\uff08TiO<sub>2<\/sub>\uff09\uff1b<\/p>\n<p>\uff083\uff09\u9664\u97e9\u56fd\u5316\u5b66\u6280\u672f\u7814\u7a76\u6240\u91c7\u7528\u7684\u7a7a\u7a74\u4f20\u8f93\u6750\u6599\u4e3a\u63ba\u6742\u7684DM\u548c\u975e\u63ba\u6742\u7684P3HT\u5916\uff0c\u5176\u4f59\u7814\u7a76\u673a\u6784\u5747\u662f\u63ba\u6742\u7684Spiro-OMeTAD\uff1b<\/p>\n<p>\uff084\uff09\u9664\u5317\u5361\u7f57\u6765\u7eb3\u5927\u5b66\u548c\u4e2d\u56fd\u79d1\u5b66\u9662\u534a\u5bfc\u4f53\u7814\u7a76\u6240\u91c7\u7528\u7684\u662f\u4e24\u6b65\u65cb\u6d82\u8f6c\u5316\u5236\u5907\u9499\u949b\u77ff\u8584\u819c\u5916, \u5176\u4f59\u7814\u7a76\u673a\u6784\u5747\u662f\u4e00\u6b65\u65cb\u6d82\u53cd\u6eb6\u5242\u6ef4\u52a0\u5236\u5907\uff1b<\/p>\n<p>\uff085\uff09\u6240\u6709\u9499\u949b\u77ff\u524d\u4f53\u4e2d\u5747\u52a0\u5165\u4e86\u9002\u91cfMACl\u3002\u03b1-FAPbI<sub>3<\/sub>\u7684\u76f8\u7a33\u5b9a\u548c\u7f3a\u9677\u949d\u5316\u662f\u6700\u91cd\u8981\u7684\u4e24\u4e2a\u5143\u7d20\uff0c\u6d89\u53ca2D\/3D\u6df7\u5408\u7ef4\u3001\u529f\u80fd\u6027\u6709\u673a\u5206\u5b50\u6216\u79bb\u5b50\u7684\u8868\u9762\u5904\u7406\u4ee5\u53ca\u68af\u5ea6\u5e26\u9699\u7684\u6982\u5ff5\u3002<\/p>\n<p>\u672c\u6587\u7531<strong>bbbbbbioy<\/strong>\u4f9b\u7a3f\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1: tougao@cailiaoren.com.<\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaorenVIP.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u65e5\u76ca\u67af\u7aed\u7684\u5316\u77f3\u80fd\u6e90\u5df2\u7ecf\u65e0\u6cd5\u6ee1\u8db3\u6301\u7eed\u589e\u957f\u7684\u80fd\u6e90\u9700\u6c42\uff0c\u5168\u7403\u80fd\u6e90\u5371\u673a\u6b63\u5728\u52a0\u5267\uff0c\u56e0\u800c\u5927\u529b\u5f00\u53d1\u6e05\u6d01\u518d\u751f\u80fd\u6e90\u5df2\u7ecf\u8feb\u5728\u7709\u776b\u3002\u53d6\u4e4b\u4e0d\u5c3d\u7528\u4e4b\u4e0d\u7aed\u7684\u592a\u9633\u80fd\u662f\u4f17\u591a\u53ef\u6301\u7eed\u80fd\u6e90\u4e2d\u6781\u5176\u91cd\u8981&#8230;<\/p>\n","protected":false},"author":10213,"featured_media":182978,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1187],"tags":[],"class_list":["post-182952","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-zhuanlan"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/182952"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/10213"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=182952"}],"version-history":[{"count":8,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/182952\/revisions"}],"predecessor-version":[{"id":182988,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/182952\/revisions\/182988"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/182978"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=182952"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=182952"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=182952"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}