{"id":184987,"date":"2019-09-05T06:30:31","date_gmt":"2019-09-04T22:30:31","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=184987"},"modified":"2019-09-04T10:43:46","modified_gmt":"2019-09-04T02:43:46","slug":"%e3%80%90%e5%ae%a1%e7%a8%bf%e5%b7%b2%e5%9b%9e%e5%a4%8d%e3%80%91%e5%8c%97%e4%ba%ac%e8%88%aa%e7%a9%ba%e8%88%aa%e5%a4%a9%e5%a4%a7%e5%ad%a6%e6%9d%8e%e5%ae%87%e8%88%aa%e5%92%8c%e6%b5%99%e6%b1%9f%e5%a4%a7","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=184987","title":{"rendered":"\u5317\u4eac\u822a\u7a7a\u822a\u5929\u5927\u5b66\u674e\u5b87\u822a\u548c\u6d59\u6c5f\u5927\u5b66\u5b8b\u5409\u821fAdv. Funct. Mater.: \u529f\u80fd\u6027\u8f6f\u590d\u5408\u6750\u6599\u4f5c\u4e3a\u53ef\u7a7f\u6234\u7535\u5b50\u4ea7\u54c1\u7684\u70ed\u4fdd\u62a4\u57fa\u5e95"},"content":{"rendered":"<p>\u3010<strong>\u5f15\u8a00<\/strong>\u3011<\/p>\n<p>\u529b\u5b66\u8bbe\u8ba1\u548c\u6750\u6599\u7684\u6700\u65b0\u8fdb\u5c55\u4f7f\u9ad8\u6027\u80fd\u53ef\u7a7f\u6234\u7535\u5b50\u8bbe\u5907\u80fd\u591f\u4e0e\u4eba\u4f53\u76ae\u80a4\u4fdd\u5f62\u63a5\u89e6\uff0c\u4ee5\u4fbf\u4e3b\u52a8\u548c\u51c6\u786e\u5730\u6d4b\u91cf\u751f\u7406\u4fe1\u53f7\uff08\u4f8b\u5982\uff0c\u4f53\u6e29\u3001\u8840\u6c27\u3001\u8840\u7cd6\u7b49\uff09\uff0c\u7528\u4e8e\u5177\u6709\u9884\u5148\u8bca\u65ad\u529f\u80fd\u7684\u5065\u5eb7\u7ba1\u7406\u3002\u5c3d\u7ba1\u8fd9\u4e9b\u53ef\u7a7f\u6234\u7535\u5b50\u8bbe\u5907\u7684\u4fdd\u5f62\u63a5\u89e6\u53ca\u5e94\u7528\u5728\u5b9e\u9a8c\u4e2d\u5f97\u5230\u4e86\u6210\u529f\u7684\u9a8c\u8bc1\uff0c\u4f46\u529f\u80fd\u90e8\u4ef6\uff08\u4f8b\u5982\uff0c\u53d1\u5149\u4e8c\u6781\u7ba1\uff09\u7684\u53d1\u70ed\u6709\u53ef\u80fd\u4f1a\u5bfc\u81f4\u4eba\u4f53\u4e0d\u9002\uff0c\u751a\u81f3\u5bf9\u76ae\u80a4\u9020\u6210\u635f\u4f24\u3002\u7531\u805a\u5408\u7269\u5236\u6210\u7684\u67d4\u6027\u57fa\u5e95\u6563\u70ed\u80fd\u529b\u8f83\u5dee\uff0c\u4e3a\u4e86\u51cf\u5c11\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6\u7684\u4e0d\u5229\u70ed\u6548\u5e94\uff0c\u6587\u732e\u5df2\u62a5\u9053\u591a\u79cd\u57fa\u5e95\u8bbe\u8ba1\uff0c\u5305\u62ec\u6db2\u6001\u91d1\u5c5e\/\u805a\u5408\u7269\u590d\u5408\u6750\u6599\u57fa\u5e95\u3001\u7eb3\u7c73\u7ebf\u6216\u7eb3\u7c73\u9897\u7c92\/\u805a\u5408\u7269\u590d\u5408\u6750\u6599\u57fa\u5e95\u548c\u91d1\u5c5e\u6563\u70ed\u7247\u57fa\u5e95\u7b49\uff0c\u901a\u8fc7\u63d0\u9ad8\u57fa\u5e95\u7684\u70ed\u5bfc\u7387\u4ee5\u589e\u5f3a\u53ef\u7a7f\u6234\u7535\u5b50\u4f20\u70ed\u7cfb\u7edf\u7684\u6563\u70ed\u3002\u70ed\u5bfc\u7387\u7684\u63d0\u9ad8\u964d\u4f4e\u4e86\u7535\u5b50\u5668\u4ef6\u7684\u6e29\u5ea6\uff0c\u4f46\u662f\u6709\u53ef\u80fd\u4f7f\u66f4\u591a\u7684\u70ed\u91cf\u5411\u76ae\u80a4\u6269\u6563\uff0c\u5bfc\u81f4\u76ae\u80a4\u7684\u6e29\u5ea6\u5347\u9ad8\uff0c\u8fd9\u5c31\u7ed9\u76ae\u80a4\u6e29\u5ea6\u7684\u7ba1\u7406\u5e26\u6765\u56f0\u96be\u3002\u6709\u5b66\u8005\u901a\u8fc7\u5f15\u5165\u5206\u5c42\u6b63\u4ea4\u5f02\u6027\u57fa\u5e95\u8bbe\u8ba1\u8fdb\u800c\u63a7\u5236\u70ed\u6d41\u65b9\u5411\u4ee5\u964d\u4f4e\u6700\u5927\u76ae\u80a4\u6e29\u5ea6\uff0c\u4f46\u5236\u9020\u590d\u6742\u6027\u6781\u5927\u5730\u9650\u5236\u4e86\u5176\u5e7f\u6cdb\u7684\u5e94\u7528,\u540c\u65f6\u8fd9\u79cd\u5404\u5411\u5f02\u6027\u57fa\u5e95\u56e0\u6dfb\u52a0\u786c\u7ec4\u5206\u800c\u964d\u4f4e\u4e86\u57fa\u5e95\u7684\u67d4\u6027\u3002\u5c3d\u7ba1\u4e0a\u8ff0\u9488\u5bf9\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6\u4f20\u70ed\u7cfb\u7edf\u57fa\u5e95\u7684\u8bbe\u8ba1\u5177\u6709\u4e00\u5b9a\u7684\u70ed\u7ba1\u7406\u529f\u80fd\uff0c\u4f46\u5728\u5668\u4ef6\u8fd0\u884c\u671f\u95f4\u5bf9\u76ae\u80a4\u7684\u70ed\u9632\u62a4\u7684\u7814\u7a76\u5374\u5f88\u5c11\uff0c\u8fd9\u4ecd\u7136\u662f\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6\u9762\u4e34\u7684\u5173\u952e\u6311\u6218\u4e4b\u4e00\u3002<\/p>\n<p>\u3010<strong>\u6210\u679c\u7b80\u4ecb<\/strong>\u3011<\/p>\n<p>\u5728\u8fd9\u4e2a\u5de5\u4f5c\u4e2d\uff0c\u4f5c\u8005\u62a5\u9053\u4e86\u4e00\u79cd\u529f\u80fd\u6027\u8f6f\u590d\u5408\u6750\u6599\u4f5c\u4e3a\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6\u7684\u70ed\u9632\u62a4\u57fa\u5e95\uff0c\u80fd\u591f\u5728\u4fdd\u6301\u57fa\u5e95\u67d4\u6027\u7684\u524d\u63d0\u4e0b\u63a7\u5236\u70ed\u6d41\u548c\u6709\u6548\u5730\u5438\u6536\u70ed\u80fd\u3002\u8be5\u529f\u80fd\u6027\u8f6f\u590d\u5408\u6750\u6599\u662f\u5c06\u91d1\u5c5e\u8584\u819c\u4e0e\u76f8\u53d8\u6750\u6599\u5d4c\u5165\u67d4\u6027\u9ad8\u5206\u5b50\u805a\u5408\u7269\u4e2d\uff0c\u8fd9\u6837\u8f83\u591a\u70ed\u6d41\u80fd\u6cbf\u7740\u9762\u5185\u65b9\u5411\u4f20\u64ad\uff0c\u5e76\u4e14\u5f53\u6e29\u5ea6\u9ad8\u4e8e\u76f8\u53d8\u6750\u6599\u7684\u8f6c\u53d8\u6e29\u5ea6\u65f6\uff0c\u70ed\u91cf\u80fd\u88ab\u5438\u6536\u3002\u4e00\u4e9b\u76f8\u53d8\u6750\u6599\u5177\u6709\u901a\u8fc7\u56fa-\u6db2\u76f8\u53d8\u5438\u6536\u5927\u91cf\u70ed\u80fd\u7684\u80fd\u529b\uff0c\u540c\u65f6\u4fdd\u6301\u76f8\u5bf9\u7a33\u5b9a\u7684\u6e29\u5ea6\u3002\u76f8\u53d8\u6750\u6599\u7684\u8fd9\u4e00\u7279\u6b8a\u70ed\u5b66\u6027\u80fd\u4e3a\u751f\u7269\u96c6\u6210\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6\u7cfb\u7edf\u7684\u70ed\u9632\u62a4\u63d0\u4f9b\u4e86\u4e00\u6761\u5408\u9002\u7684\u9014\u5f84\u3002\u8be5\u529f\u80fd\u6027\u67d4\u6027\u590d\u5408\u6750\u6599\u7684\u5b9e\u9a8c\u4e0e\u6570\u503c\u7814\u7a76\u63ed\u793a\u4e86\u8bbe\u8ba1\u4e0e\u5e94\u7528\u7684\u57fa\u672c\u539f\u7406\u3002\u4e0e\u65b0\u9c9c\u732a\u76ae\u96c6\u6210\u7684\u57fa\u4e8e\u70ed\u9632\u62a4\u57fa\u5e95\u7684\u53ef\u7a7f\u6234\u5f0f\u52a0\u70ed\u5668\u7684\u6f14\u793a\uff0c\u8bf4\u660e\u4e86\u5176\u53ef\u6709\u6548\u5730\u964d\u4f4e\u6700\u9ad8\u76ae\u80a4\u6e29\u5ea6\u7684\u80fd\u529b\uff0c\u4ece\u800c\u5c55\u793a\u4e86\u4e0e\u53ef\u7a7f\u6234\u7535\u5b50\u4ea7\u54c1\u76f8\u7ed3\u5408\u7684\u5b9e\u9645\u5e94\u7528\u53ef\u80fd\uff0c\u5e76\u4e3a\u9700\u8981\u751f\u7269\u70ed\u4fdd\u62a4\u7684\u751f\u7269\u96c6\u6210\u5e94\u7528\u521b\u9020\u4e86\u5de5\u7a0b\u5e94\u7528\u7684\u673a\u4f1a\u3002<strong>\u8be5\u6210\u679c\u4ee5\u9898\u4e3a\u201cFunctional Soft Composites As Thermal Protecting Substrates for Wearable Electronics\u201d\u53d1\u8868\u5728Adv. Funct. Mater.\u4e0a\u3002<\/strong><\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>Figure 1.<\/strong><strong>\u76ae\u80a4\u96c6\u6210\u53ef\u7a7f\u6234\u8bbe\u5907\u7684\u6a2a\u622a\u9762\u56fe<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-184988\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/r1-2.jpg\" alt=\"\" width=\"600\" height=\"199\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/r1-2.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/r1-2-300x100.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>a\uff09\u67d4\u6027\u805a\u5408\u7269\u7684\u4f20\u7edf\u57fa\u5e95<\/p>\n<p>b\uff09\u529f\u80fd\u6027\u67d4\u6027\u590d\u5408\u6750\u6599\u7684\u70ed\u9632\u62a4\u57fa\u5e95\uff0c\u7531\u5d4c\u5165\u67d4\u6027\u805a\u5408\u7269\u7684\u76f8\u53d8\u6750\u6599\u4e0e\u5176\u4e0a\u90e8\u7684\u91d1\u5c5e\u8584\u819c\u6784\u6210<\/p>\n<p><strong>Figure 2.<\/strong><strong>\u5177\u6709\u70ed\u9632\u62a4\u57fa\u5e95\u7684\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-184989\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/r2-2.jpg\" alt=\"\" width=\"600\" height=\"429\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/r2-2.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/r2-2-300x215.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>a\uff09\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6\u793a\u610f\u56fe\uff0c\u5305\u62ec\u529f\u80fd\u6027\u67d4\u6027\u590d\u5408\u6750\u6599\u4e0a\u7684\u70ed\u6e90\uff08\u67d4\u6027\u8d85\u8584\u52a0\u70ed\u5668\uff09\u3002\u5f53\u4e0e\u76ae\u80a4\u76f8\u7ed3\u5408\u65f6\uff0c\u76ae\u80a4\u4e0a\u7684\u6700\u9ad8\u6e29\u5ea6\u51fa\u73b0\u5728\u70ed\u9632\u62a4\u57fa\u5e95\u4e0e\u76ae\u80a4\u4e4b\u95f4\u754c\u9762\u4e0a\u7684\u84dd\u70b9\u6807\u8bb0\u7684\u4e2d\u5fc3<\/p>\n<p>b\uff09\u5e26\u6709ACF\u8fde\u7ebf\u7684\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6<\/p>\n<p>c\uff09\u8d85\u8584\u67d4\u6027\u52a0\u70ed\u5668<\/p>\n<p>d\uff09\u5f2f\u6298\u72b6\u6001\u4e0b\u7684\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6<\/p>\n<p>e\uff09\u96c6\u6210\u5728\u4eba\u4f53\u76ae\u80a4\u4e0a\u7684\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6<\/p>\n<p><strong>Figure 3.<\/strong><strong>\u529f\u80fd\u6027\u67d4\u6027\u590d\u5408\u6750\u6599\u4f5c\u4e3a\u70ed\u9632\u62a4\u57fa\u5e95\u7684\u70ed\u9632\u62a4\u6548\u679c<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-184990\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/r3-2.jpg\" alt=\"\" width=\"600\" height=\"766\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/r3-2.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/r3-2-235x300.jpg 235w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>a,b\uff09\u52a0\u70ed40s\u65f6PDMS\u57fa\u5e95\u4e0e\u70ed\u9632\u62a4\u57fa\u5e95\u5e95\u90e8\u7684\u5b9e\u9a8c\u548c\u6709\u9650\u5143\u6e29\u5ea6\u5206\u5e03<\/p>\n<p>c\uff09\u57fa\u5e95\u5e95\u90e8\u7684\u6700\u9ad8\u6e29\u5ea6\u968f\u65f6\u95f4\u7684\u53d8\u5316\uff08\u52a0\u70ed40s\uff09<\/p>\n<p>d\uff09\u57fa\u5e95\u5e95\u90e8\u7684\u6700\u9ad8\u6e29\u5ea6\u968f\u7740\u52a0\u70ed\u65f6\u95f4\u7684\u51fd\u6570\u5173\u7cfb\u3002\u70ed\u9632\u62a4\u57fa\u5e95\u5728\u52a0\u70ed\u8fc7\u7a0b\u4e2d\u7684\u70ed\u54cd\u5e94\u5206\u4e3aI\u3001II\u3001III\u548cIV\u56db\u4e2a\u9636\u6bb5\uff1a<\/p>\n<p>e\uff09\u52a0\u70ed\u65f6\u95f4\u5bf9\u964d\u6e29\u6548\u7387\u7684\u5f71\u54cd\uff1b<\/p>\n<p>f\uff09\u77f3\u8721\u5c42\u539a\u5ea6\u5bf9\u964d\u6e29\u6548\u7387\u7684\u5f71\u54cd\uff1b<\/p>\n<p>g\uff09\u590d\u5408\u6750\u6599\u57fa\u5e95\u539a\u5ea6\u5bf9\u964d\u6e29\u6548\u7387\u7684\u5f71\u54cd\uff1b<\/p>\n<p>h\uff09\u77f3\u8721\u5c42\u4f4d\u7f6e\u5bf9\u964d\u6e29\u6548\u7387\u7684\u5f71\u54cd\u3002f\uff09-h\uff09\u8fd8\u8003\u8651\u4e86\u94dc\u819c\u539a\u5ea6\u5bf9\u964d\u6e29\u6548\u7387\u7684\u5f71\u54cd\u3002<\/p>\n<p><strong>Figure 4.<\/strong> <strong>\u529f\u80fd\u6027\u67d4\u6027\u590d\u5408\u6750\u6599\u57fa\u5e95\u5bf9\u751f\u7269\u7ec4\u7ec7\u7684\u70ed\u9632\u62a4\u4f5c\u7528<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-184991\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/r4-2.jpg\" alt=\"\" width=\"600\" height=\"459\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/r4-2.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/r4-2-300x230.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u3010\u5c0f\u7ed3\u3011<\/strong><\/p>\n<p>\u5728\u8fd9\u9879\u7814\u7a76\u4e2d\uff0c\u4f5c\u8005\u4e3a\u53ef\u7a7f\u6234\u7535\u5b50\u8bbe\u5907\u63d0\u51fa\u4e86\u4e00\u79cd\u65b0\u9896\u7684\u70ed\u9632\u62a4\u57fa\u5e95\u8bbe\u8ba1\u3002\u6784\u6210\u70ed\u9632\u62a4\u57fa\u5e95\u7684\u529f\u80fd\u6027\u8f6f\u590d\u5408\u6750\u6599\uff0c\u7531\u5d4c\u5165\u67d4\u6027\u805a\u5408\u7269\u4e2d\u7684\u76f8\u53d8\u6750\u6599\u53ca\u5176\u4e0a\u90e8\u7684\u8584\u91d1\u5c5e\u819c\u7ec4\u6210\u3002\u7ed3\u679c\u8868\u660e\uff0c\u4e0e\u4f20\u7edf\u67d4\u6027\u57fa\u5e95\u76f8\u6bd4\uff0c\u6240\u63d0\u51fa\u7684\u70ed\u9632\u62a4\u57fa\u5e95\u53ef\u4ee5\u5728\u9002\u5f53\u7684\u53c2\u6570\u4e0b\u5c06\u76ae\u80a4\u6e29\u5347\u5cf0\u503c\u964d\u4f4e\u8d85\u8fc785\uff05\u3002\u5b9e\u9a8c\u548c\u6570\u503c\u7814\u7a76\u63ed\u793a\u4e86\u70ed\u9632\u62a4\u673a\u7406\uff1a\u901a\u8fc7\u91d1\u5c5e\u5c42\u8c03\u63a7\u70ed\u6d41\uff0c\u5229\u7528\u76f8\u53d8\u6750\u6599\u5438\u6536\u70ed\u80fd\u3002\u5145\u5206\u7814\u7a76\u4e86\u51e0\u4f55\u53c2\u6570\u5bf9\u964d\u6e29\u6027\u80fd\u7684\u5f71\u54cd\u3002\u4e0e\u65b0\u9c9c\u732a\u76ae\u96c6\u6210\u7684\u53ef\u7a7f\u6234\u5f0f\u52a0\u70ed\u5668\/\u70ed\u9632\u62a4\u57fa\u5e95\u7684\u964d\u6e29\u6548\u679c\uff0c\u5c55\u793a\u4e86\u70ed\u9632\u62a4\u57fa\u5e95\u964d\u4f4e\u76ae\u80a4\u6e29\u5ea6\u7684\u4f18\u5f02\u6027\u80fd\u3002<\/p>\n<p><a href=\"https:\/\/onlinelibrary.wiley.com\/journal\/16163028\" target=\"_blank\" rel=\"noopener\">Functional Soft Composites As Thermal Protecting Substrates for Wearable Electronics<\/a><\/p>\n<p>(Adv. Funct. Mater., 2019, DOI: 10.1002\/adfm.201905470)<\/p>\n<p>\u672c\u6587\u7531tt\u4f9b\u7a3f\uff0c\u6750\u6599\u725b\u6574\u7406\u7f16\u8f91\u3002\u00a0<\/p>\n<p>\u6750\u6599\u725b\u7f51\u4e13\u6ce8\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u53ca\u884c\u4e1a\u8fdb\u5c55\uff0c\u8fd9\u91cc\u6c47\u96c6\u4e86\u5404\u5927\u9ad8\u6821\u7855\u535a\u751f\u3001\u4e00\u7ebf\u79d1\u7814\u4eba\u5458\u4ee5\u53ca\u884c\u4e1a\u4ece\u4e1a\u8005\uff0c\u5982\u679c\u60a8\u5bf9\u4e8e\u8ddf\u8e2a\u6750\u6599\u9886\u57df\u79d1\u6280\u8fdb\u5c55\uff0c\u89e3\u8bfb\u9ad8\u6c34\u5e73\u6587\u7ae0\u6216\u662f\u8bc4\u8ff0\u884c\u4e1a\u6709\u5174\u8da3\uff0c\u70b9\u6211\u52a0\u5165\u7f16\u8f91\u90e8\u5927\u5bb6\u5ead\u3002\u00a0<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaokefu\uff0c\u6211\u4eec\u4f1a\u9080\u8bf7\u5404\u4f4d\u8001\u5e08\u52a0\u5165\u4e13\u5bb6\u7fa4\u3002\u00a0<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u529b\u5b66\u8bbe\u8ba1\u548c\u6750\u6599\u7684\u6700\u65b0\u8fdb\u5c55\u4f7f\u9ad8\u6027\u80fd\u53ef\u7a7f\u6234\u7535\u5b50\u8bbe\u5907\u80fd\u591f\u4e0e\u4eba\u4f53\u76ae\u80a4\u4fdd\u5f62\u63a5\u89e6\uff0c\u4ee5\u4fbf\u4e3b\u52a8\u548c\u51c6\u786e\u5730\u6d4b\u91cf\u751f\u7406\u4fe1\u53f7\uff08\u4f8b\u5982\uff0c\u4f53\u6e29\u3001\u8840\u6c27\u3001\u8840\u7cd6\u7b49\uff09\uff0c\u7528\u4e8e\u5177\u6709\u9884\u5148\u8bca\u65ad\u529f\u80fd\u7684&#8230;<\/p>\n","protected":false},"author":7336,"featured_media":184988,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[4087],"class_list":["post-184987","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","tag-4087"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/184987"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/7336"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=184987"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/184987\/revisions"}],"predecessor-version":[{"id":185025,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/184987\/revisions\/185025"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/184988"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=184987"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=184987"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=184987"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}