{"id":186095,"date":"2019-10-04T06:30:26","date_gmt":"2019-10-03T22:30:26","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=186095"},"modified":"2019-10-03T17:34:11","modified_gmt":"2019-10-03T09:34:11","slug":"%e3%80%90%e5%b7%b2%e6%a0%a1%e7%a8%bf%e3%80%91%e5%8d%8e%e5%8d%97%e7%90%86%e5%b7%a5%e5%a4%a7%e5%ad%a6%e6%9b%b9%e9%95%9b%e9%99%a2%e5%a3%ab%e5%9b%a2%e9%98%9fnature-communications%ef%bc%9a-1-cm2%e5%85%a8","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=186095","title":{"rendered":"\u534e\u5357\u7406\u5de5\u66f9\u955b\u56e2\u961fNature Communications\uff1a 1 cm2\u5168\u805a\u5408\u7269\u592a\u9633\u7535\u6c60\u7684\u6548\u7387\u53d6\u5f97\u91cc\u7a0b\u7891\u7684\u7a81\u7834!"},"content":{"rendered":"<p>\u3010\u5f15\u8a00\u3011<\/p>\n<p>\u5168\u805a\u5408\u7269\u592a\u9633\u7535\u6c60(all-PSCs)\u5177\u6709\u4f18\u5f02\u7684\u5149\u3001\u70ed\u4ee5\u53ca\u673a\u68b0\u7a33\u5b9a\u6027\uff0c\u5f15\u8d77\u7814\u7a76\u4eba\u5458\u5e7f\u6cdb\u5173\u6ce8\u3002\u5168\u805a\u5408\u7269\u592a\u9633\u7684\u5149\u5438\u6536\u5c42\u7531\u805a\u5408\u7269\u7ed9\u4f53\u548c\u805a\u5408\u7269\u53d7\u4f53\u7ec4\u6210\uff0c\u5176\u4e2d\u5e94\u7528\u6700\u5e7f\u6cdb\u7684n-\u578b\u805a\u5408\u7269\u7535\u5b50\u53d7\u4f53\u662f\u57fa\u4e8e\u8418\u9170\u4e9a\u80fa\u5355\u5143\u7684N2200\u53ca\u5176\u884d\u751f\u7269\u3002\u7136\u800c\uff0c\u7531\u4e8e\u8418\u9170\u4e9a\u80fa\u7c7bn-\u578b\u805a\u5408\u7269\u5728\u8fd1\u7ea2\u5916\u533a\u57df\u7684\u5438\u6536\u8f83\u5f31\uff0c\u9650\u5236\u4e86\u592a\u9633\u5149\u5b50\u7684\u6709\u6548\u5229\u7528\u3002\u5c3d\u7ba1\u589e\u52a0\u5149\u5438\u6536\u5c42\u7684\u539a\u5ea6\u53ef\u6709\u6548\u63d0\u9ad8\u5bf9\u592a\u9633\u5149\u7684\u5438\u6536\uff0c\u4f46\u4f1a\u5bfc\u81f4\u4e25\u91cd\u7684\u7535\u8377\u590d\u5408\u800c\u65e0\u6cd5\u5b9e\u73b0\u9ad8\u80fd\u91cf\u8f6c\u6362\u6548\u7387\u3002<\/p>\n<p>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/p>\n<p>\u534e\u5357\u7406\u5de5\u5927\u5b66\u7684\u9ec4\u98de\u6559\u6388\u3001\u5e94\u78ca\u6559\u6388\u548c\u57c3\u5c14\u6717\u6839-\u7ebd\u4f26\u5821\u5927\u5b66\u7684\u674e\u5b81\u535a\u58eb\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09\u57fa\u4e8e\u81ea\u4e3b\u53d1\u5c55\u7684PTzBI-Si:PBTA-Si:N2200\u7684\u5149\u5438\u6536\u6750\u6599\u4f53\u7cfb\uff0c\u5229\u7528\u5149\u7ba1\u7406\u3001\u7cbe\u7ec6\u5f62\u8c8c\u8c03\u63a7\u65b9\u6cd5\uff0c\u5b9e\u73b0\u4e861-cm<sup>2<\/sup>\u5168\u805a\u5408\u7269\u592a\u9633\u7535\u6c60\u5668\u4ef6\u5728\u5149\u5438\u6536\u5c42\u539a\u5ea6\u7ea6350 nm\u65f6\u80fd\u91cf\u8f6c\u6362\u6548\u7387\u8d85\u8fc710%\uff0c\u8868\u660e\u4e86\u5168\u805a\u5408\u7269\u592a\u9633\u7535\u6c60\u5e7f\u9614\u7684\u5e94\u7528\u524d\u666f\u3002\u4e0a\u8ff0\u6210\u679c\u8fd1\u671f\u53d1\u8868\u4e8e\u56fd\u9645\u8457\u540d\u671f\u520a\u300aNature\u00a0 Communications\u300b\u3002<\/p>\n<p>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/p>\n<p>\u56fe1.\u5438\u6536\u5149\u8c31\u548c\u5149\u5b66\u6a21\u62df<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-186098\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/41467_2019_12132_Fig1_HTML.webp_.jpg\" alt=\"\" width=\"600\" height=\"502\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/41467_2019_12132_Fig1_HTML.webp_.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/41467_2019_12132_Fig1_HTML.webp_-300x251.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>a.\u6d3b\u6027\u5c42\u7ec4\u5206\u548c\u6eb6\u5242\u7684\u7ed3\u6784\u5f0f<\/p>\n<p>b.\u6d3b\u6027\u5c42\u539a\u5ea6\u5206\u522b\u4e3a130nm\u548c320nm\u7684PBTA-Si:PTzBISi:N2200(1.3:0.7:1)\u6df7\u5408\u819c\u7684\u5438\u6536\u5149\u8c31<\/p>\n<p>c.\u6d3b\u6027\u5c42\u539a\u5ea6\u4e0d\u540c\u7684\u57fa\u4e8ePBTA-Si:PTzBISi:N2200(1.3:0.7:1)\u7684all-PSCs\u5438\u6536\u7684\u5149\u5b50\u4e0e\u6ce2\u957f\u7684\u5173\u7cfb<\/p>\n<p>d.\u77ed\u8def\u7535\u6d41\u5bc6\u5ea6\uff08J<sub>SC<\/sub>\uff09\u6a21\u62df\u503c\u4e0e\u6d3b\u6027\u5c42\u539a\u5ea6\u7684\u5173\u7cfb<\/p>\n<p>\u56fe2.\u57fa\u4e8ePBTA-Si:PTzBISi:N2200(1.3:0.7:1)\u7684\u539a\u819call-PSCs\u7684\u5149\u4f0f\u6027\u80fd<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-186097\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/41467_2019_12132_Fig2_HTML.webp_.jpg\" alt=\"\" width=\"600\" height=\"473\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/41467_2019_12132_Fig2_HTML.webp_.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/41467_2019_12132_Fig2_HTML.webp_-300x237.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>a.\u6d3b\u6027\u5c42\u539a\u5ea6\u5927\u7ea6\u4e3a320nm\u7684all-PSCs\u7684\u586b\u5145\u56e0\u5b50(FF)\u548cJ<sub>SC<\/sub>\u4e0e\u4e8c\u82c4\u919a\u542b\u91cf\u7684\u5173\u7cfb<\/p>\n<p>b.\u4e8c\u82c4\u919a\u4f53\u79ef\u5206\u6570\u4e3a0.1%\u7684all-PSCs\u7684FF\u4e0e\u6d3b\u6027\u5c42\u539a\u5ea6\u7684\u5173\u7cfb<\/p>\n<p>c.\u4e8c\u82c4\u919a\u4f53\u79ef\u5206\u6570\u4e3a0.1%\u7684all-PSCs\u7684\u5916\u91cf\u5b50\u6548\u7387<\/p>\n<p>d.\u5185\u91cf\u5b50\u6548\u7387\u4e3a80%\u65f6\u7684J<sub>SC<\/sub>\u6a21\u62df\u503c\u548c\u5b9e\u9a8c\u503c\uff0c\u63d2\u56fe\u4e3a\u6d3b\u6027\u5c42\u539a\u5ea6\u5206\u522b\u4e3a130nm\u548c380nm\u76840.05cm<sup>2<\/sup>\u7684all-PSCs\u7684\u7167\u7247<\/p>\n<p>\u56fe3.PBTA-Si:PTzBISi:N2200(1.3:0.7:1)\u6df7\u5408\u7269\u819c\u7684\u5f62\u8c8c<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-186100\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/41467_2019_12132_Fig3_HTML.webp_.jpg\" alt=\"\" width=\"600\" height=\"525\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/41467_2019_12132_Fig3_HTML.webp_.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/41467_2019_12132_Fig3_HTML.webp_-300x263.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>a.\u65e0\u4e8c\u82c4\u919a\u548c\u4e8c\u82c4\u919a\u4f53\u79ef\u5206\u6570\u4e3a0.1%\u7684\u6df7\u5408\u819c\u7684\u63a0\u5165\u5c04\u5e7f\u89d2X\u5c04\u7ebf\u6563\u5c04(GIWAXS)\u66f2\u7ebf<\/p>\n<p>b. (010)\u548c(100)\u6563\u5c04\u5cf0\u7684\u6676\u4f53\u76f8\u5e72\u957f\u5ea6<\/p>\n<p>c.\u4e0d\u540c\u6df7\u5408\u7269\u819c\u7684\u540c\u6b65\u8f90\u5c04\u5171\u632f\u8f6f X \u5c04\u7ebf\u6563\u5c04(RSoXS)\u66f2\u7ebf<\/p>\n<p>\u56fe4.\u5927\u9762\u79ef\u7684all-PSCs\u7684\u5149\u4f0f\u6027\u80fd<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-186099\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/41467_2019_12132_Fig4_HTML.webp_.jpg\" alt=\"\" width=\"600\" height=\"488\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/41467_2019_12132_Fig4_HTML.webp_.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/09\/41467_2019_12132_Fig4_HTML.webp_-300x244.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>a.\u57fa\u5e95\u548c\u6d3b\u6027\u5c42\u539a\u5ea6\u4e0d\u540c\u76841cm<sup>2<\/sup>\u7684all-PSCs\u7684J-V\u66f2\u7ebf\uff0c\u63d2\u56fe\u4e3a\u57fa\u5e95\u4e3acustom-ITO\u3001\u6d3b\u6027\u5c42\u539a\u5ea6\u4e3a350nm\u7684all-PSCs\u7684\u7167\u7247<\/p>\n<p>b.\u00a0\u57fa\u5e95\u4e3acustom-ITO\u30011cm<sup>2<\/sup>\u7684all-PSCs\u7684\u5916\u91cf\u5b50\u6548\u7387\u548c\u7535\u6d41\u5bc6\u5ea6<\/p>\n<p>c.0.05cm<sup>2<\/sup>\u548c1cm<sup>2\u00a0<\/sup>\u7684\u539a\u819call-PSCs\u7684\u6697\u6001J-V\u66f2\u7ebf<\/p>\n<p>d.J<sup>1\/2<\/sup>-V\u66f2\u7ebf<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/www.nature.com\/articles\/s41467-019-12132-6.pdf\">Surpassing the 10% efficiency milestone for 1-cm2 all-polymer solar cells<\/a>\uff08Nat. Commun., 2019,DOI:10.1038\/s41467-019-12132-6\uff09<\/p>\n<p>\u672c\u6587\u7531kv1004\u4f9b\u7a3f\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u5168\u805a\u5408\u7269\u592a\u9633\u7535\u6c60(all-PSCs)\u5177\u6709\u4f18\u5f02\u7684\u5149\u3001\u70ed\u4ee5\u53ca\u673a\u68b0\u7a33\u5b9a\u6027\uff0c\u5f15\u8d77\u7814\u7a76\u4eba\u5458\u5e7f\u6cdb\u5173\u6ce8\u3002\u5168\u805a\u5408\u7269\u592a\u9633\u7684\u5149\u5438\u6536\u5c42\u7531\u805a\u5408\u7269\u7ed9\u4f53\u548c\u805a\u5408\u7269\u53d7\u4f53\u7ec4\u6210\uff0c\u5176\u4e2d\u5e94\u7528&#8230;<\/p>\n","protected":false},"author":1592,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-186095","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/186095"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/1592"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=186095"}],"version-history":[{"count":14,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/186095\/revisions"}],"predecessor-version":[{"id":186979,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/186095\/revisions\/186979"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=186095"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=186095"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=186095"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}