{"id":192137,"date":"2019-12-11T06:30:39","date_gmt":"2019-12-10T22:30:39","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=192137"},"modified":"2019-12-10T17:04:20","modified_gmt":"2019-12-10T09:04:20","slug":"%e3%80%90%e6%8a%95%e7%a8%bf%e3%80%91%e4%b8%ad%e7%a7%91%e9%99%a2%e5%8c%96%e5%ad%a6%e6%89%80%e9%83%ad%e7%8e%89%e5%9b%bd%e7%a0%94%e7%a9%b6%e5%91%98%e9%a9%ac%e6%99%ae%e6%89%80joachim-maier%e6%95%99","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=192137","title":{"rendered":"\u4e2d\u79d1\u9662\u5316\u5b66\u6240\u90ed\u7389\u56fd\u7814\u7a76\u5458&#038;\u9a6c\u666e\u6240Joachim Maier\u6559\u6388Materials Today: \u8fc8\u5411\u66f4\u597d\u7684\u9502\u91d1\u5c5e\u7535\u6c60\uff1a\u6311\u6218\u4e0e\u7b56\u7565"},"content":{"rendered":"<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192138\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72471-20.png\" alt=\"\" width=\"600\" height=\"276\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72471-20.png 698w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72471-20-300x138.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/> \u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0<\/p>\n<p>\u6587\u7ae0\u94fe\u63a5\uff1ahttps:\/\/doi.org\/10.1016\/j.mattod.2019.09.018<\/p>\n<p><strong><b>\u3010\u6838\u5fc3\u5185\u5bb9\u3011<\/b><\/strong><\/p>\n<p>1) \u4ece\u70ed\u529b\u5b66\u89d2\u5ea6\u89e3\u6790\u4e86\u9502\u91d1\u5c5e\u8d1f\u6781\u4e2d\u7684SEI\u819c\u548c\u679d\u6676\u751f\u957f\u673a\u5236\u3002<\/p>\n<p>2) \u8be6\u7ec6\u4ecb\u7ecd\u4e86\u9502\u91d1\u5c5e\u8d1f\u6781\u5728\u6db2\u6001\u3001\u805a\u5408\u7269\u3001\u65e0\u673a\u56fa\u6001\u7535\u89e3\u8d28\u4f53\u7cfb\u4e2d\u9047\u5230\u7684\u6311\u6218\u548c\u6700\u65b0\u7814\u7a76\u6210\u679c\u3002<\/p>\n<p>3) \u5bf9\u9502\u91d1\u5c5e\u8d1f\u6781\u5728\u4e0d\u540c\u7535\u89e3\u8d28\u4f53\u7cfb\u4e2d\u5c06\u6765\u7684\u7814\u7a76\u91cd\u70b9\u548c\u6311\u6218\u8fdb\u884c\u4e86\u5c55\u671b\u3002<\/p>\n<p><strong><b>\u3010\u7efc\u8ff0\u80cc\u666f\u4e0e\u7b80\u4ecb\u3011<\/b><\/strong><\/p>\n<p>\u8d1f\u6781\u6750\u6599\u662f\u5f71\u54cd\u7535\u6c60\u80fd\u91cf\u5bc6\u5ea6\u7684\u5173\u952e\u90e8\u5206\u3002\u7531\u4e8e\u5177\u6709\u9ad8\u7406\u8bba\u5bb9\u91cf(~3860 mAh\/g)\u548c\u4f4e\u6c27\u5316\u8fd8\u539f\u7535\u52bf(-3.04 V vs. SHE)\uff0c\u91d1\u5c5e\u9502\u4e00\u76f4\u4ee5\u6765\u88ab\u8ba4\u4e3a\u662f\u6700\u7406\u60f3\u7684\u8d1f\u6781\u6750\u6599\u3002\u5982\u679c\u5c06\u4f20\u7edf\u8d1f\u6781\u66ff\u6362\u6210\u9502\u91d1\u5c5e\u8d1f\u6781\uff0c\u7535\u6c60\u7684\u80fd\u91cf\u5bc6\u5ea6\u6709\u671b\u8d85\u8d8a\u76ee\u524d\u7684\u9502\u79bb\u5b50\u7535\u6c60\u3002\u7136\u800c\uff0c\u4e0d\u53ef\u907f\u514d\u7684\u9502\u679d\u6676\u751f\u957f\u3001\u7535\u89e3\u8d28\u7684\u6d88\u8017\u3001\u5faa\u73af\u8fc7\u7a0b\u4e2d\u4e25\u91cd\u7684\u4f53\u79ef\u53d8\u5316\u4ee5\u53ca\u4e0e\u4e4b\u76f8\u5173\u7684\u6f5c\u5728\u5b89\u5168\u98ce\u9669\u9650\u5236\u4e86\u9502\u91d1\u5c5e\u8d1f\u6781\u7684\u5b9e\u9645\u5e94\u7528\u3002\u636e\u62a5\u9053\uff0c\u7535\u89e3\u8d28\u5316\u5b66\u8c03\u63a7\u3001\u8d1f\u6781\u754c\u9762\u5de5\u7a0b\u548c\u7ed3\u6784\u6784\u7b51\u7684\u7b56\u7565\u5728\u589e\u5f3a\u9502\u91d1\u5c5e\u7a33\u5b9a\u6027\u65b9\u9762\u5df2\u7ecf\u53d6\u5f97\u4e86\u8fdb\u5c55\u3002\u4f46\u662f\uff0c\u5728\u91d1\u5c5e\u9502\u8d1f\u6781\u4ece\u6db2\u6001\u5411\u56fa\u6001\u4f53\u7cfb\u8f6c\u53d8\u65f6\uff0c\u4ecd\u7136\u9762\u4e34\u79bb\u5b50\u7535\u5bfc\u7387\u4f4e\u3001\u754c\u9762\u63a5\u89e6\u5dee\u3001\u52a8\u529b\u5b66\u7f13\u6162\u7b49\u65b9\u9762\u7684\u4e25\u5cfb\u6311\u6218\u3002<strong><b>\u4e2d\u79d1\u9662\u5316\u5b66\u6240\u5f20\u83b9\u535a\u58eb\uff08\u7b2c\u4e00\u4f5c\u8005\uff09\u3001\u90ed\u7389\u56fd\u7814\u7a76\u5458\u548c\u9a6c\u666e\u6240<\/b><\/strong><strong><b>Joachim <\/b><\/strong><strong><b>Maier\u6559\u6388\u603b\u7ed3\u4e86\u5e76\u4e14\u5f3a\u8c03\u4e86\u9502\u91d1\u5c5e\u8d1f\u6781\u5728\u6db2\u6001\u3001\u805a\u5408\u7269\u3001\u65e0\u673a\u56fa\u6001\u7535\u89e3\u8d28\u4f53\u7cfb\u4e2d\u9762\u4e34\u7684\u95ee\u9898\uff0c\u7efc\u8ff0\u4e86\u9488\u5bf9\u4e0d\u540c\u4f53\u7cfb\u91c7\u53d6\u7684<\/b><\/strong><strong><b>\u5148\u8fdb\u7b56\u7565<\/b><\/strong><strong><b>\u7528\u4e8e\u63d0\u9ad8\u91d1\u5c5e\u9502\u8d1f\u6781\u7684\u7a33\u5b9a\u6027\u3002\u8be5\u5de5\u4f5c\u4e5f\u5bf9\u9502\u91d1\u5c5e\u8d1f\u6781\u5c06\u6765\u7684\u7814\u7a76\u91cd\u70b9\u548c\u65b9\u5411\u8fdb\u884c\u4e86\u5c55\u671b\uff0c\u4e3a\u672a\u6765\u9ad8\u6bd4\u80fd\u50a8\u80fd\u7cfb\u7edf\u7684\u53d1\u5c55\u63d0\u4f9b\u65b0\u601d\u8def\u3002<\/b><\/strong><\/p>\n<p><strong><b>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/b><\/strong><\/p>\n<p><strong><b>1<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><strong><b>\u9502\u91d1\u5c5e\u7535\u6c60\u5728\u4e0d\u540c\u7535\u89e3\u8d28\u4f53\u7cfb\u4e2d\u7684\u80fd\u91cf\u5bc6\u5ea6<\/b><\/strong><\/p>\n<p>\u672c\u6587\u6bd4\u8f83\u4e86\u4ee5\u77f3\u58a8\u548c\u91d1\u5c5e\u9502\u4f5c\u4e3a\u8d1f\u6781\u6750\u6599\u7684\u6db2\u6001\u4e8c\u6b21\u7535\u6c60\u7684\u80fd\u91cf\u5bc6\u5ea6\u3002\u91c7\u7528\u4f20\u7edf\u7684\u77f3\u58a8\u8d1f\u6781\uff0c\u9502\u79bb\u5b50\u7535\u6c60\u7684\u80fd\u91cf\u5bc6\u5ea6\u6781\u9650\u4e3a300 Wh\/kg\uff0c\u5bf9\u5e94\u7684\u7535\u52a8\u6c7d\u8f66\u7eed\u822a\u91cc\u7a0b&lt;300 km\u3002\u5982\u679c\u91c7\u7528\u91d1\u5c5e\u9502\u4f5c\u4e3a\u8d1f\u6781\uff0c\u7535\u6c60\u7684\u80fd\u91cf\u5bc6\u5ea6\u6709\u671b\u7a81\u7834400 Wh\/kg\uff0c\u5bf9\u5e94\u7684\u7535\u52a8\u6c7d\u8f66\u7eed\u822a\u91cc\u7a0b\u6709\u671b\u8fbe\u5230500 km\u53ca\u4ee5\u4e0a\u3002\u5728\u805a\u5408\u7269\u7535\u89e3\u8d28\u548c\u65e0\u673a\u56fa\u6001\u7535\u89e3\u8d28\u7b49\u4f53\u79ef\u66ff\u6362\u6db2\u6001\u7535\u89e3\u8d28\u7684\u524d\u63d0\u4e0b\uff0c\u672c\u6587\u5206\u522b\u8ba1\u7b97\u4e86\u805a\u5408\u7269\u548c\u65e0\u673a\u56fa\u6001\u4f53\u7cfb\u4e2d\u9502\u91d1\u5c5e\u7535\u6c60\u7684\u80fd\u91cf\u5bc6\u5ea6\uff0c\u53d1\u73b0\u805a\u5408\u7269\u9502\u91d1\u5c5e\u7535\u6c60\u8868\u73b0\u51fa\u66f4\u9ad8\u7684\u80fd\u91cf\u5bc6\u5ea6\u3002\u4e0e\u6db2\u6001\u548c\u805a\u5408\u7269\u7535\u89e3\u8d28\u76f8\u6bd4\uff0c\u65e0\u673a\u56fa\u6001\u7535\u89e3\u8d28\u7531\u4e8e\u81ea\u8eab\u5bc6\u5ea6\u5927\uff0c\u5bf9\u63d0\u5347\u7535\u6c60\u7684\u80fd\u91cf\u5bc6\u5ea6\u5e76\u65e0\u4f18\u52bf\uff1b\u4f46\u662f\u901a\u8fc7\u51cf\u8584\u539a\u5ea6\uff08\u4f8b\u598220\u5fae\u7c73\uff09\uff0c\u6709\u671b\u83b7\u5f97\u8f83\u9ad8\u7684\u80fd\u91cf\u5bc6\u5ea6\uff0c\u4f46\u6709\u53ef\u80fd\u524a\u5f31\u4e86\u65e0\u673a\u56fa\u4f53\u9502\u91d1\u5c5e\u7535\u6c60\u7684\u7684\u5b89\u5168\u6027\u3002\u8be6\u7ec6\u7684\u8ba1\u7b97\u53c2\u6570\u8bf7\u53c2\u89c1\u652f\u6301\u6750\u6599\u3002<\/p>\n<p>\u56fe1. Li-LiNi<sub>0.8<\/sub>Co<sub>0.1<\/sub>Mn<sub>0.1<\/sub>O<sub>2<\/sub>\u548cLi-S\u7535\u6c60\u5728\u6db2\u6001\u3001\u805a\u5408\u7269\u3001\u65e0\u673a\u56fa\u6001\u7535\u89e3\u8d28\u4f53\u7cfb\u4e2d\u7684\u80fd\u91cf\u5bc6\u5ea6\u56fe\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192139\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72472-18.png\" alt=\"\" width=\"600\" height=\"374\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72472-18.png 1161w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72472-18-300x187.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72472-18-768x478.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72472-18-1024x638.png 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>2<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><strong><b>\u9502\u91d1\u5c5e\u8d1f\u6781\u9762\u4e34\u7684\u6311\u6218<\/b><\/strong><\/p>\n<p><strong><b>\u9502\u91d1\u5c5e\u8d1f\u6781\u9762\u4e34\u7684\u4e3b\u8981\u6311\u6218\u4e3a\u4ee5\u4e0b\u4e09\u4e2a\u65b9\u9762\uff1a\uff081\uff09\u9502\u679d\u6676\u7684\u751f\u6210\uff1b\uff082\uff09\u9502\u91d1\u5c5e\u4e0e\u7535\u89e3\u6db2\u7684\u6301\u7eed\u53cd\u5e94\u9020\u6210\u7535\u89e3\u6db2\u7684\u6d88\u8017\uff1b\uff083\uff09S<\/b><\/strong><strong><b>EI<\/b><\/strong><strong><b>\u754c\u9762\u5c42\u7684\u673a\u68b0\u6027\u7834\u88c2\u4ee5\u53ca\u7531\u5176\u9020\u6210\u7684\u4f4e\u5e93\u4f26\u6548\u7387\u3002<\/b><\/strong>\u8fd9\u4e9b\u95ee\u9898\u6700\u7ec8\u5f71\u54cd\u7535\u6c60\u7684\u5faa\u73af\u5bff\u547d\u548c\u5b89\u5168\u6027\u80fd\u3002\u672c\u6587\u4ece\u70ed\u529b\u5b66\u89d2\u5ea6\uff0c\u4ee5\u7ecf\u5178\u7684Li-I<sub>2<\/sub>\u7535\u6c60\u5165\u624b\uff0c\u901a\u8fc7\u5206\u6790SEI\u5c42\u754c\u9762\u7684\u539a\u5ea6\u3001\u79bb\u5b50\u7535\u5bfc\u3001\u7535\u5b50\u7535\u5bfc\u3001\u5316\u5b66\u52bf\u5206\u5e03\u3001\u7535\u5316\u5b66\u7535\u4f4d\u7b49\u65b9\u9762\u5bf9\u754c\u9762\u70ed\u529b\u5b66\u7a33\u5b9a\u6027\u7684\u5f71\u54cd\u3002<strong><b>\u5bfc\u81f4\u9502\u679d\u6676\u751f\u6210\u7684\u539f\u56e0\u6709\u5f88\u591a\uff0c\u4e3b\u8981\u53ef\u5206\u4e3a\u4e24\u7c7b\uff1a\uff081\uff09\u754c\u9762\u5f62\u8c8c\u5728\u6a2a\u5411\u4e0a\u7684\u4e0d\u5747\u5300\u6027\uff0c\u9020\u6210\u539f\u56e0\uff1a\u6bdb\u7ec6\u6548\u5e94\u3001\u5c16\u7aef\u6548\u5e94\u3001\u8868\u9762\u5f20\u529b\u548c\u573a\u6548\u5e94\u5f15\u8d77\u7684\u6210\u6838\u51cf\u5f31\u6216\u7535\u8377\u8f6c\u79fb\u969c\u788d\u3001\u6d53\u5dee\u6781\u5316\uff1b\uff082\uff09\u5faa\u73af\u8fc7\u7a0b\u4e2d\u4e0d\u5747\u5300\u7684\u70ed\u6216\u5316\u5b66\u5206\u5e03\u3002<\/b><\/strong><\/p>\n<p>\u56fe2. (a-b) LiI\u70ed\u529b\u5b66\u7a97\u53e3\u548c\u5e26\u9699\uff1b(c) SEI\u548c\u56fa\u6001\u7535\u89e3\u8d28\u7684\u5316\u5b66\u52bf\u5206\u5e03\u56fe\uff1b(d) SEI\u76f8\u754c\u9762\u5904\u7684\u7a7a\u95f4\u7535\u8377\u6548\u5e94\uff1b(e)\u5728\u500d\u7387\u5f71\u54cd\u3001\u6d53\u5dee\u6781\u5316\u548c\u5c16\u7aef\u6548\u5e94\u7684\u5f71\u54cd\u4e0b\u7684\u9502\u679d\u6676\u751f\u957f\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192140\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72473-15.png\" alt=\"\" width=\"600\" height=\"278\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72473-15.png 1270w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72473-15-300x139.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72473-15-768x356.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72473-15-1024x475.png 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u88681. Li\u5728(001)\u548c(111)\u9762\u548cMg\u5728(0001)\u9762\u8ba1\u7b97\u7684\u8868\u9762\u80fd\u3001\u76f8\u4e92\u4f5c\u7528\u80fd\u548c\u6269\u6563\u52bf\u5792<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192159\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/360\u622a\u56fe17020802100102141.jpg\" alt=\"\" width=\"600\" height=\"100\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/360\u622a\u56fe17020802100102141.jpg 1099w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/360\u622a\u56fe17020802100102141-300x50.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/360\u622a\u56fe17020802100102141-768x128.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/360\u622a\u56fe17020802100102141-1024x171.jpg 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><b><\/b><strong><b>3 \u6db2\u6001\u4f53\u7cfb\u4e2d\u7684\u9502\u91d1\u5c5e<\/b><\/strong><\/p>\n<p>\u9488\u5bf9\u9502\u91d1\u5c5e\u8d1f\u6781\u5728\u6db2\u6001\u4f53\u7cfb\u4e2d\u679d\u6676\u7684\u751f\u957f\u3001SEI\u754c\u9762\u7684\u4e0d\u7a33\u5b9a\u6027\uff0c\u4e3b\u8981\u7684\u8c03\u63a7\u624b\u6bb5\u4e3b\u8981\u4ece\u6db2\u6001\u7535\u89e3\u6db2\u5316\u5b66\u6210\u5206\u7684\u8c03\u63a7\u3001SEI\u754c\u9762\u5de5\u7a0b\u4ee5\u53ca\u5bf9\u7535\u6781\u5408\u7406\u7684\u7ed3\u6784\u5316\u8bbe\u8ba1\u51e0\u65b9\u9762\u5165\u624b\u3002\u6b64\u5916\uff0c\u672c\u7ae0\u8fd8\u8be6\u7ec6\u9610\u8ff0\u4e86\u9502\u5bf9\u79f0\u7535\u6c60\u4e2d\u5e38\u89c1\u7684\u7535\u538b\u53d8\u5316\u4e0e\u9502\u91d1\u5c5e\u8868\u9762\u5f62\u8c8c\u6f14\u53d8\u4e2d\u95f4\u7684\u8054\u7cfb\u3002<\/p>\n<p>\u56fe3. (a) Li\u5bf9\u79f0\u7535\u6c60\u7684\u5178\u578b\u7535\u538b\u54cd\u5e94\u66f2\u7ebf\u56fe. (b-d)\u9996\u5708\u6c89\u79ef\u3001\u6eb6\u89e3\u3001\u591a\u5708\u540e\u6c89\u79ef\u7535\u538b\u7684\u53d8\u5316\u4ee5\u53ca\u5bf9\u5e94\u7684\u9502\u8d1f\u6781\u8868\u9762\u5f62\u8c8c\u6f14\u53d8\u793a\u610f\u56fe\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192141\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72474-14.png\" alt=\"\" width=\"600\" height=\"309\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72474-14.png 1904w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72474-14-300x154.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72474-14-768x395.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72474-14-1024x527.png 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe4.\u00a0\u529f\u80fd\u578b\u7535\u89e3\u8d28\u6dfb\u52a0\u5242\u4f7fSEI\u66f4\u5747\u5300\u5730\u751f\u6210\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192142\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72475-13.png\" alt=\"\" width=\"600\" height=\"417\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72475-13.png 1268w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72475-13-300x209.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72475-13-768x534.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72475-13-1024x712.png 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe5. \u4eba\u5de5SEI\u754c\u9762\u5c42\u4fee\u9970\u540e\u9502\u91d1\u5c5e\u8868\u9762\u65e0\u679d\u6676\u6c89\u79ef\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192143\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72476-12.png\" alt=\"\" width=\"600\" height=\"349\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72476-12.png 1240w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72476-12-300x174.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72476-12-768x447.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72476-12-1024x595.png 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe6. \u4e0d\u540c3D\u96c6\u6d41\u4f53\u5f15\u5bfc\u5747\u5300\u9502\u6c89\u79ef\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192144\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72477-11.png\" alt=\"\" width=\"600\" height=\"482\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72477-11.png 1240w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72477-11-300x241.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72477-11-768x617.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72477-11-1024x823.png 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe7. 3D\u9aa8\u67b6\u4e0e\u9502\u91d1\u5c5e\u590d\u5408\u5236\u5907\u66f4\u7a33\u5b9a\u7684\u9502\u91d1\u5c5e\u590d\u5408\u7535\u6781\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192145\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72478-7.png\" alt=\"\" width=\"600\" height=\"295\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72478-7.png 1269w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72478-7-300x148.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72478-7-768x378.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72478-7-1024x504.png 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>4<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><strong><b>\u805a\u5408\u7269\u4f53\u7cfb\u4e2d\u7684\u9502\u91d1\u5c5e<\/b><\/strong><\/p>\n<p>\u805a\u5408\u7269\u9502\u7535\u6c60\u5177\u6709\u4f4e\u5bc6\u5ea6\u3001\u6297\u6cc4\u6f0f\u3001\u6613\u52a0\u5de5\u7b49\u4f18\u70b9\uff0c\u5728\u63d0\u9ad8\u7535\u6c60\u80fd\u91cf\u5bc6\u5ea6\u548c\u5b89\u5168\u6027\u65b9\u9762\u6709\u5f88\u5927\u7684\u6f5c\u529b\uff0c\u6709\u671b\u8d85\u8d8a\u4f20\u7edf\u9502\u79bb\u5b50\u7535\u6c60\u3002\u805a\u5408\u7269\u7535\u89e3\u8d28\u5206\u4e3a\u51dd\u80f6\u7535\u89e3\u8d28\u548c\u56fa\u4f53\u9ad8\u5206\u5b50\u7535\u89e3\u8d28\u4e24\u79cd\u3002\u51dd\u80f6\u7535\u89e3\u8d28\u542b\u6db2\u4f53\u7535\u89e3\u6db2\u4f46\u514d\u4e8e\u6cc4\u6f0f\u7684\u98ce\u9669\uff0c\u5e76\u4e14\u5177\u6709\u8f83\u9ad8\u7684\u79bb\u5b50\u7535\u5bfc\u7387\uff0c\u4f46\u662f\u673a\u68b0\u5f3a\u5ea6\u4f4e\uff0c\u65e0\u6cd5\u963b\u6321\u9502\u679d\u6676\u7684\u7a7f\u523a\uff0c\u5b58\u5728\u5b89\u5168\u9690\u60a3\u3002\u4f17\u591a\u56fa\u4f53\u9ad8\u5206\u5b50\u7535\u89e3\u8d28\u4e2d\uff0c\u805a\u73af\u6c27\u4e59\u70f7PEO\u7531\u4e8e\u5176\u826f\u597d\u7684\u7684\u9502\u76d0\u6eb6\u89e3\u5ea6\u548c\u5bf9\u9502\u5316\u5b66\u7535\u5316\u5b66\u7a33\u5b9a\u6027\uff0c\u88ab\u8ba4\u4e3a\u662f\u6700\u6709\u524d\u666f\u7684\u56fa\u4f53\u9ad8\u5206\u5b50\u7535\u89e3\u8d28\uff0c\u4f46\u662f\u5ba4\u6e29\u4e0b\u79bb\u5b50\u7535\u5bfc\u7387\u4f4e\u9650\u5236\u4e86\u5176\u5e94\u7528\u3002<strong><b>\u56e0\u6b64\uff0c\u805a\u5408\u7269\u4f53\u7cfb\u4e2d\u9700\u8981\u6709\u9488\u5bf9\u6027\u5730\u63d0\u9ad8\u7535\u89e3\u8d28\u672c\u8eab\u7684\u79bb\u5b50\u7535\u5bfc\u7387\u3001\u673a\u68b0\u5f3a\u5ea6\u4ee5\u53ca\u591a\u529f\u80fd\u6027\u62d3\u5c55\uff0c\u4f8b\u5982\uff1a\u6ee1\u8db3\u6b63\u8d1f\u6781\u4e0d\u540c\u9700\u6c42\u3001\u589e\u5f3a\u805a\u5408\u7269\u7535\u89e3\u8d28\u7684\u963b\u71c3\u6027\u7b49\u3002\u91c7\u53d6\u7684\u7b56\u7565\u6709\uff1a\u56fa\u5b9a\u9634\u79bb\u5b50\u3001\u5f15\u5165\u521a\u6027\u9ad8\u5206\u5b50\u9aa8\u67b6\u3001\u8bbe\u8ba1\u53cc\u5c42\u5f02\u8d28\u7ed3\u6784\u7684\u805a\u5408\u7269\u548c\u6dfb\u52a0\u963b\u71c3\u6dfb\u52a0\u5242\u7b49\u3002<\/b><\/strong><\/p>\n<p>\u56fe8. \u56fa\u5b9a\u9634\u79bb\u5b50\u5bf9\u805a\u5408\u7269\u7535\u89e3\u8d28\u79bb\u5b50\u8fc1\u79fb\u6570\u548c\u79bb\u5b50\u7535\u5bfc\u7387\u7684\u5f71\u54cd\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192146\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72479-6.png\" alt=\"\" width=\"600\" height=\"540\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72479-6.png 1270w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72479-6-300x270.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72479-6-768x691.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u72479-6-1024x921.png 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe9. \u805a\u5408\u7269\u7535\u89e3\u8d28\u5728\u9502\u91d1\u5c5e\u7535\u6c60\u4e2d\u7684\u591a\u529f\u80fd\u62d3\u5c55\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192147\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724710-6.png\" alt=\"\" width=\"600\" height=\"452\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724710-6.png 1271w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724710-6-300x226.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724710-6-768x579.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724710-6-1024x772.png 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>5<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><strong><b>\u65e0\u673a\u56fa\u6001\u4f53\u7cfb\u4e2d\u7684\u9502\u91d1\u5c5e<\/b><\/strong><\/p>\n<p>\u4e0e\u6db2\u6001\u548c\u805a\u5408\u7269\u7535\u89e3\u8d28\u76f8\u6bd4\uff0c\u65e0\u673a\u56fa\u6001\u7535\u89e3\u8d28\u7531\u4e8e\u4e0d\u7136\u6027\u3001\u6297\u6f0f\u6db2\u3001\u9ad8\u673a\u68b0\u5f3a\u5ea6\u3001\u9ad8\u70ed\u7a33\u5b9a\u6027\uff0c\u53ef\u4ee5\u663e\u8457\u5730\u63d0\u9ad8\u7535\u6c60\u7684\u5b89\u5168\u6027\u3002<strong><b>\u4f46\u662f\uff0c\u4f4e\u79bb\u5b50\u7535\u5bfc\u5f15\u8d77\u7684\u5185\u90e8\u6b27\u59c6\u635f\u8017\uff0c\u4e0e\u9502\u7684\u70ed\u529b\u5b66\u517c\u5bb9\u6027\u3001\u754c\u9762\u7a33\u5b9a\u6027\u95ee\u9898\u4ee5\u53ca\u7f3a\u4e4f\u67d4\u6027\u7684\u56fa\u6709\u7279\u6027\u9650\u5236\u4e86\u65e0\u673a\u56fa\u6001\u7535\u89e3\u8d28\u7684\u5b9e\u9645\u5e94\u7528\u3002<\/b><\/strong>\u56e0\u6b64\uff0c\u672c\u8282\u5185\u5bb9\u4ece\u70ed\u529b\u5b66\u5bf9\u754c\u9762\u7a33\u5b9a\u6027\u7684\u5206\u6790\u5165\u624b\uff0c\u7efc\u8ff0\u4e86\u964d\u4f4e\u754c\u9762\u963b\u6297\u3001\u589e\u5f3a\u7535\u89e3\u8d28\u67d4\u6027\u7684\u8bf8\u591a\u7b56\u7565\u3002<\/p>\n<p>\u88682. \u56fa\u6001\u7535\u89e3\u8d28\u80b2\u91d1\u5c5e\u9502\u7684\u8fd8\u539f\u53cd\u5e94<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192158\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/360\u622a\u56fe16520820085448.jpg\" alt=\"\" width=\"600\" height=\"397\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/360\u622a\u56fe16520820085448.jpg 1077w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/360\u622a\u56fe16520820085448-300x198.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/360\u622a\u56fe16520820085448-768x508.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/360\u622a\u56fe16520820085448-1024x677.jpg 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe10. \u4e0d\u540c\u56fa\u6001\u7535\u89e3\u8d28\u7684(a-b)\u5206\u89e3\u7535\u538b\u548c\u5206\u89e3\u80fd\u91cf\uff0c(c)\u7535\u5316\u5b66\u7a97\u53e3\u4ee5\u53ca\u6c27\u5316\u7535\u4f4d<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192148\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724711-6.png\" alt=\"\" width=\"600\" height=\"173\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724711-6.png 1268w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724711-6-300x87.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724711-6-768x222.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724711-6-1024x296.png 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe11. \u964d\u4f4e\u9502\u91d1\u5c5e\u4e0e\u56fa\u6001\u7535\u89e3\u8d28\u754c\u9762\u63a5\u89e6\u963b\u6297\u7684\u6700\u65b0\u7b56\u7565\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192149\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724712-3.png\" alt=\"\" width=\"600\" height=\"275\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724712-3.png 1269w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724712-3-300x138.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724712-3-768x352.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724712-3-1024x470.png 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe12.\u00a0\u589e\u5f3aLLZO\u9676\u74f7\u67d4\u6027\u7684\u7b56\u7565\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192150\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724713-1.png\" alt=\"\" width=\"600\" height=\"323\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724713-1.png 1370w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724713-1-300x161.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724713-1-768x413.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724713-1-1024x551.png 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>6<\/b><\/strong><strong><b>\u00a0<\/b><\/strong><strong><b>\u56fa\u6db2\u6df7\u5408\u4f53\u7cfb\u4e2d\u7684\u9502\u91d1\u5c5e<\/b><\/strong><\/p>\n<p>\u56fa\u6db2\u6df7\u5408\u4f53\u7cfb\u7684\u4f18\u52bf\uff1a(1)\u964d\u4f4e\u6db2\u542b\u91cf\u7684\u540c\u65f6\u4fdd\u6301\u754c\u9762\u63a5\u89e6\uff1b(2)\u5177\u6709\u826f\u597d\u7684\u673a\u68b0\u6027\u80fd(\u6210\u578b\u6027\u3001\u6da6\u6e7f\u6027)\u4ee5\u53ca\u5b89\u5168\u6027\uff1b(3)\u7531\u4e8e\u9634\u79bb\u5b50\u88ab\u5438\u9644\uff0c\u589e\u52a0\u4e86\u7535\u89e3\u8d28\u7684\u79bb\u5b50\u7535\u5bfc\u548c\u9502\u79bb\u5b50\u8fc1\u79fb\u6570\uff0c\u964d\u4f4e\u4e86\u6d53\u5dee\u6781\u5316\uff0c\u4fc3\u8fdb\u4e86\u9502\u79bb\u5b50\u7684\u8fd0\u8f93\u3002<\/p>\n<p>\u56fe13. \u56fa\u6db2\u6df7\u5408\u7535\u89e3\u8d28\u7684\u7814\u7a76\u8fdb\u5c55\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192151\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724714-1.png\" alt=\"\" width=\"600\" height=\"332\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724714-1.png 1236w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724714-1-300x166.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724714-1-768x425.png 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724714-1-1024x567.png 1024w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u3010\u603b\u7ed3\u4e0e\u5c55\u671b\u3011<\/b><\/strong><\/p>\n<p>\u9502\u91d1\u5c5e\u88ab\u8ba4\u4e3a\u662f\u63a8\u52a8\u5148\u8fdb\u7535\u6c60\u6280\u672f\u5411\u9ad8\u80fd\u65b9\u5411\u53d1\u5c55\u7684\u7ec8\u6781\u8d1f\u6781\u6750\u6599\u3002\u7136\u800c\uff0c\u9502\u679d\u6676\u751f\u957f\u4ee5\u53ca\u4e0e\u5176\u5bc6\u5207\u76f8\u5173\u7684\u5b89\u5168\u98ce\u9669\u9650\u5236\u4e86\u5176\u5b9e\u9645\u5e94\u7528\u3002\u672c\u6587\u4f5c\u8005\u9488\u5bf9\u9502\u91d1\u5c5e\u8d1f\u6781\u5728\u6db2\u6001\u3001\u805a\u5408\u7269\u548c\u65e0\u673a\u56fa\u4f53\u7535\u89e3\u8d28\u4f53\u7cfb\u4e2d\u6240\u9762\u4e34\u7684\u6311\u6218\u548c\u76f8\u5e94\u7684\u7b56\u7565\u603b\u7ed3\u5982\u56fe14\u6240\u793a\uff0c\u5e76\u6307\u51fa\u4e86\u9502\u91d1\u5c5e\u8d1f\u6781\u5728\u5c06\u6765\u53d1\u5c55\u8fc7\u7a0b\u4e2d\u7684\u7814\u7a76\u91cd\u70b9\uff1a<\/p>\n<p>1\uff09<strong><b>\u5e93\u4f26\u6548\u7387<\/b><\/strong>&#8211;\u5e93\u4f26\u6548\u7387\u662f\u68c0\u9a8c\u9502\u91d1\u5c5e\u8d1f\u6781\u7a33\u5b9a\u6027\u7684\u91cd\u8981\u6307\u6807\u3002\u7814\u7a76\u8868\u660e\uff0c\u572880%\u9502\u8fc7\u91cf\u7684\u60c5\u51b5\u4e0b\uff0c\u9502\u91d1\u5c5e\u7535\u6c60\u7684\u5e93\u4f26\u6548\u7387\u9700\u8981\u8fbe\u523099.9%\u4ee5\u4e0a\uff0c\u624d\u53ef\u4ee5\u4fdd\u8bc1\u7535\u6c60\u5faa\u73af1000\u6b21\u5bb9\u91cf\u8870\u51cf\u7387\u4e3a20%\u3002\u7531\u4e8e\u5e93\u4f26\u6548\u7387\u53d7\u679d\u6676\u751f\u957f\u3001\u6b7b\u9502\u751f\u6210\u3001\u7535\u89e3\u6db2\u6d88\u8017\u7b49\u539f\u56e0\u7684\u5171\u540c\u5f71\u54cd\uff0c\u56e0\u6b64\uff0c\u5728\u957f\u671f\u5faa\u73af\u8fc7\u7a0b\u4e2d\uff0c\u4fdd\u6301\u9ad8\u5e93\u4f26\u6548\u7387\u662f\u975e\u5e38\u6709\u6311\u6218\u6027\u7684\u3002<\/p>\n<p>2\uff09<strong><b>\u5148\u8fdb\u7684\u8868\u5f81\u6280\u672f<\/b><\/strong>\u2014\u7531\u4e8e\u9502\u662f\u8f7b\u8d28\u5143\u7d20\u3001\u6027\u8d28\u6d3b\u6cfc\uff0c\u5bf9\u5316\u5b66\u73af\u5883\u9ad8\u5ea6\u654f\u611f\uff0c\u7814\u7a76Li\u548cSEI\u7684\u521d\u59cb\u7eb3\u7c73\u7ed3\u6784\u548c\u52a8\u6001\u6c89\u79ef\/\u5265\u79bb\u8fc7\u7a0b\u4e2d\u7684\u6676\u4f53\u5b66\u53d8\u5f97\u975e\u5e38\u6709\u6311\u6218\u6027\uff0c\u4e5f\u5bf9\u9502\u91d1\u5c5e\u8d1f\u6781\u6df1\u5165\u7814\u7a76\u610f\u4e49\u975e\u51e1\u3002<\/p>\n<p>3\uff09<strong><b>\u9502\u91d1\u5c5e\u9aa8\u67b6\u8bbe\u8ba1<\/b><\/strong>\u2014\u76ee\u524d\u4e0e\u9502\u91d1\u5c5e\u590d\u5408\u7684\u9aa8\u67b6\u5927\u591a\u5177\u6709\u7535\u5b50\u7535\u5bfc\u7279\u6027\uff0c\u7136\u800c\u79bb\u5b50\u7535\u5bfc\u9aa8\u67b6\u3001\u6216\u8005\u6df7\u5408\u7535\u5b50-\u79bb\u5b50\u7535\u5bfc\u9aa8\u67b6\u7684\u7814\u7a76\u76ee\u524d\u5e76\u4e0d\u591a\u89c1\u3002\u8be5\u9879\u7814\u7a76\u8fd9\u5bf9\u63a2\u7d22\u9502\u6c89\u79ef\u884c\u4e3a\u5177\u6709\u91cd\u8981\u610f\u4e49\u3002<\/p>\n<p>4\uff09<strong><b>\u56fa\u6001\u7535\u89e3\u8d28\u4f53\u7cfb<\/b><\/strong>\u2014\u56fa\u6001\u7535\u89e3\u8d28\u4f53\u7cfb\u4e0d\u5177\u6709\u6d41\u52a8\u6027\uff0c\u56e0\u4e3a\u7535\u6c60\u6613\u53d7\u754c\u9762\u7684\u6301\u7eed\u6076\u5316\u800c\u9020\u6210\u6027\u80fd\u4e0b\u964d\u3002\u754c\u9762\u5de5\u7a0b\u7684\u7814\u7a76\u5bf9\u4e8e\u6539\u5584\u9502\u6c89\u79ef\u884c\u4e3a\u548c\u589e\u5f3a\u754c\u9762\u7a33\u5b9a\u6027\u662f\u6709\u5fc5\u8981\u7684\u3002\u6b64\u5916\uff0c\u901a\u8fc7\u5c06\u56fa\u6001\u7535\u89e3\u8d28\u4e0e\u6db2\u6001\/\u805a\u5408\u7269\u7535\u89e3\u8d28\u590d\u5408\u7684\u65b9\u6cd5\u6709\u671b\u5728\u673a\u68b0\u6027\u80fd\u3001\u79bb\u5b50\u7535\u5bfc\u3001\u89c4\u6a21\u5316\u751f\u4ea7\u65b9\u9762\u540c\u65f6\u83b7\u5f97\u63d0\u5347\u3002<\/p>\n<p>\u603b\u4e4b\uff0c\u6b32\u5b9e\u73b0\u9ad8\u5b89\u5168\u6027\u548c\u9ad8\u80fd\u91cf\u5bc6\u5ea6\u7684\u9502\u91d1\u5c5e\u7535\u6c60\uff0c\u987b\u5bf9\u754c\u9762\u53cd\u5e94\u548c\u52a8\u529b\u5b66\u6709\u66f4\u6df1\u5165\u7684\u4e86\u89e3\uff0c\u5e76\u5728\u7535\u6781\/\u7535\u89e3\u8d28\u4f53\u7cfb\u7ed3\u6784\u3001\u7535\u6c60\u5de5\u7a0b\u548c\u6280\u672f\u6027\u80fd\u8bc4\u4f30\u65b9\u9762\u4ed8\u51fa\u66f4\u5927\u7684\u52aa\u529b\u3002<\/p>\n<p>\u56fe14. \u9502\u91d1\u5c5e\u7535\u6c60\u5728\u4e0d\u540c\u7535\u89e3\u8d28\u4f53\u7cfb\u4e2d\u9762\u4e34\u7684\u6311\u6218\u548c\u76f8\u5e94\u7684\u7b56\u7565\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192152\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724715-1.png\" alt=\"\" width=\"600\" height=\"335\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724715-1.png 975w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724715-1-300x167.png 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724715-1-768x429.png 768w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong><b>\u3010\u4f5c\u8005\u7b80\u4ecb\u3011<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192153\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724716-1-261x300.png\" alt=\"\" width=\"200\" height=\"230\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724716-1-261x300.png 261w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724716-1.png 337w\" sizes=\"(max-width: 200px) 100vw, 200px\" \/><\/p>\n<p><strong><b>\u5f20\u83b9<\/b><\/strong>\uff0c\u4e2d\u56fd\u79d1\u5b66\u9662\u5316\u5b66\u7814\u7a76\u6240\u535a\u58eb\u540e\uff0c\u54c8\u5c14\u6ee8\u5de5\u7a0b\u5927\u5b66\u548c\u7f8e\u56fd\u9a6c\u91cc\u5170\u5927\u5b66\u8054\u5408\u57f9\u517b\u535a\u58eb\u6bd5\u4e1a\u751f\uff0c\u7814\u7a76\u65b9\u5411\u4e3a\uff1a\u9ad8\u6bd4\u80fd\u548c\u9ad8\u5b89\u5168\u6027\u50a8\u80fd\u7535\u6c60\u53ca\u5173\u952e\u6750\u6599\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192154\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724717.png\" alt=\"\" width=\"200\" height=\"244\" \/><\/p>\n<p><strong><b>Joachim Maier<\/b><\/strong>\uff0c\u73b0\u4efb\u65af\u56fe\u52a0\u7279\u9a6c\u666e\u56fa\u6001\u7814\u7a76\u6240\u7269\u7406\u5316\u5b66\u7cfb\u4e3b\u4efb\uff0c\u7814\u7a76\u65b9\u5411\u4e3a\uff1a\u56fa\u6001\u7535\u89e3\u8d28\u7684\u754c\u9762\u53ca\u754c\u9762\u5904\u7684\u79bb\u5b50\u8f93\u8fd0\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-192155\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724718.png\" alt=\"\" width=\"200\" height=\"252\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724718.png 256w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2019\/12\/\u56fe\u724718-239x300.png 239w\" sizes=\"(max-width: 200px) 100vw, 200px\" \/><\/p>\n<p><strong><b>\u90ed\u7389\u56fd<\/b><\/strong>\uff0c\u73b0\u4efb\u4e2d\u56fd\u79d1\u5b66\u9662\u5316\u5b66\u7814\u7a76\u6240\u7814\u7a76\u5458\uff0c\u535a\u58eb\u751f\u5bfc\u5e08\uff0c\u201c\u6770\u9752\u201d\uff0c\u4e2d\u7ec4\u90e8\u201c\u4e07\u4eba\u8ba1\u5212\u201d\u9996\u6279\u9752\u5e74\u62d4\u5c16\u4eba\u624d\uff0c\u8bfe\u9898\u7ec4\u957f\uff0c\u4e2d\u56fd\u7845\u9178\u76d0\u5b66\u4f1a\u56fa\u6001\u79bb\u5b50\u5b66\u5206\u4f1a\u7406\u4e8b\u3002\u7814\u7a76\u65b9\u5411\u4e3a\uff1a\u7535\u5316\u5b66\u50a8\u80fd\u5668\u4ef6\u53ca\u5176\u5173\u952e\u6750\u6599\uff0c\u9ad8\u6bd4\u80fd\u7535\u6c60\uff0c\u52a8\u529b\u7535\u6c60\u53ca\u50a8\u80fd\u7535\u6c60\u6280\u672f\uff0c\u7535\u5b50\u5b58\u50a8\u4e0e\u8f93\u8fd0\u3002<\/p>\n<p>\u672c\u6587\u4f5c\u8005\u4f9b\u7a3f\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1: tougao@cailiaoren.com.<\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaorenVIP.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0 \u6587\u7ae0\u94fe\u63a5\uff1ahttps:\/\/doi.org\/10.1016\/j.mattod.2019.09.018 \u3010\u6838\u5fc3\u5185\u5bb9\u3011 1) \u4ece\u70ed\u529b&#8230;<\/p>\n","protected":false},"author":11454,"featured_media":192138,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-192137","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/192137"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/11454"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=192137"}],"version-history":[{"count":6,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/192137\/revisions"}],"predecessor-version":[{"id":192205,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/192137\/revisions\/192205"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/192138"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=192137"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=192137"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=192137"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}