{"id":199004,"date":"2020-04-08T06:18:50","date_gmt":"2020-04-07T22:18:50","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=199004"},"modified":"2020-04-07T22:45:53","modified_gmt":"2020-04-07T14:45:53","slug":"%e6%a2%b3%e7%90%86%ef%bc%9a%e5%a4%a7%e7%89%9brogers%e3%80%81%e9%b2%8d%e5%93%b2%e5%8d%97%e3%80%81%e7%8e%8b%e4%b8%ad%e6%9e%97%e3%80%81%e9%bb%84%e7%bb%b4%e3%80%81%e8%b5%b5%e9%80%89%e8%b4%ba%e3%80%81josep","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=199004","title":{"rendered":"\u68b3\u7406\uff1a\u5927\u725bRogers\u3001\u9c8d\u54f2\u5357\u3001\u738b\u4e2d\u6797\u3001\u9ec4\u7ef4\u3001\u8d75\u9009\u8d3a\u3001Joseph Wang\u3001\u9ea6\u7acb\u5f3a\u7b49\u8fd1\u671f\u53ef\u7a7f\u6234\u5668\u4ef6\u7814\u7a76\u6210\u679c"},"content":{"rendered":"<p>\u53ef\u7a7f\u6234\u6280\u672f\uff0c\u662f\u7531\u9ebb\u7701\u7406\u5de5\u5b66\u9662\u5a92\u4f53\u5b9e\u9a8c\u5ba4\u6700\u65e9\u572820\u4e16\u7eaa60\u5e74\u4ee3\u63d0\u51fa\u7684\u521b\u65b0\u6280\u672f\u3002\u5229\u7528\u8be5\u6280\u672f\uff0c\u53ef\u4ee5\u628a\u591a\u5a92\u4f53\u3001\u4f20\u611f\u5668\u548c\u65e0\u7ebf\u901a\u4fe1\u7b49\u6280\u672f\u5d4c\u5165\u4eba\u4eec\u7684\u8863\u7269\u4e2d\uff0c\u53ef\u652f\u6301\u624b\u52bf\u548c\u773c\u52a8\u64cd\u4f5c\u7b49\u591a\u79cd\u4ea4\u4e92\u65b9\u5f0f\uff0c\u4e3b\u8981\u63a2\u7d22\u548c\u521b\u9020\u53ef\u76f4\u63a5\u7a7f\u6234\u7684\u667a\u80fd\u8bbe\u5907\u3002\u53ef\u7a7f\u6234\u8bbe\u5907\u591a\u4ee5\u5177\u5907\u90e8\u5206\u8ba1\u7b97\u529f\u80fd\u3001\u53ef\u8fde\u63a5\u624b\u673a\u53ca\u5404\u7c7b\u7ec8\u7aef\u7684\u4fbf\u643a\u5f0f\u914d\u4ef6\u5f62\u5f0f\u5b58\u5728\uff0c\u4e3b\u6d41\u7684\u4ea7\u54c1\u5f62\u6001\u5305\u62ec\u4ee5\u624b\u8155\u4e3a\u652f\u6491\u7684\u8868\u548c\u8155\u5e26\u7b49\u4ea7\u54c1\uff0c\u4ee5\u811a\u4e3a\u652f\u6491\u7684\u978b\u3001\u889c\u5b50\u6216\u8005\u5c06\u6765\u7684\u5176\u4ed6\u817f\u4e0a\u4f69\u6234\u4ea7\u54c1\uff0c\u4ee5\u5934\u90e8\u4e3a\u652f\u6491\u7684\u773c\u955c\u3001\u5934\u76d4\u3001\u5934\u5e26\u7b49\u4ea7\u54c1\uff0c\u4ee5\u53ca\u667a\u80fd\u670d\u88c5\u3001\u4e66\u5305\u3001\u62d0\u6756\u3001\u914d\u9970\u7b49\u5404\u7c7b\u975e\u4e3b\u6d41\u4ea7\u54c1\u5f62\u6001\u3002\u800c\u79d1\u7814\u754c\u548c\u4ea7\u4e1a\u754c\u662f\u76f8\u8f85\u76f8\u6210\u3001\u76f8\u4e92\u4ea4\u6d41\u548c\u76f8\u4e92\u4fc3\u8fdb\u7684\uff0c\u672c\u6587\u603b\u7ed3\u4e86\u79d1\u7814\u754c\u5b66\u672f\u5927\u5496\u5728\u53ef\u7a7f\u6234\u5668\u4ef6\u9886\u57df\u7684\u79d1\u7814\u65b0\u8fdb\u5c55\uff0c\u5e0c\u671b\u5bf9\u4ece\u4e8b\u53ef\u7a7f\u6234\u5668\u4ef6\u79d1\u7814\u7684\u4f60\u6709\u6240\u542f\u53d1\u3002<\/p>\n<p><strong><b>1<\/b><\/strong><strong><b>\u3001<\/b><\/strong><strong><b>Nature Medicine\uff1a<\/b><\/strong><strong><b>\u7528\u4e8e\u65b0\u751f\u513f\u548c\u513f\u79d1\u91cd\u75c7\u76d1\u62a4\u75c5\u623f\u7684\u9ad8\u7ea7\u65e0\u7ebf\u751f\u7406\u76d1\u6d4b\u7684\u76ae\u80a4\u63a5\u53e3\u751f\u7269\u4f20\u611f\u5668<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"wp-image-199613 size-full aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/E59BBEE789872-34.png\" alt=\"\" width=\"670\" height=\"1089\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/E59BBEE789872-34.png 670w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/E59BBEE789872-34-185x300.png 185w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/E59BBEE789872-34-630x1024.png 630w\" sizes=\"(max-width: 670px) 100vw, 670px\" \/><\/p>\n<p><strong><b>\u7f8e\u56fd\u897f\u5317\u5927\u5b66John A. Rogers\u9662\u58eb\u56e2\u961f\u4e0e\u5408\u4f5c\u8005<\/b><\/strong>\u63d0\u4f9b\u4e86\u4e00\u79cd\u65e0\u7ebf\uff0c\u975e\u4fb5\u5165\u6027\u6280\u672f\uff0c\u4e0d\u4ec5\u53ef\u4ee5\u63d0\u4f9b\u4e0e\u73b0\u6709\u4e34\u5e8a\u6807\u51c6\u76f8\u5f53\u7684\u5fc3\u7387\uff0c\u547c\u5438\u9891\u7387\uff0c\u6e29\u5ea6\u548c\u8840\u6db2\u6c27\u5408\u6c34\u5e73\u7684\u6d4b\u91cf\u503c\uff0c\u800c\u4e14\u8fd8\u63d0\u4f9b\u4e86\u4e00\u7cfb\u5217\u91cd\u8981\u7684\u9644\u52a0\u529f\u80fd\uff0c\u5e76\u5728NICU\u548cPICU\u4e2d\u5f97\u5230\u4e86\u5148\u5bfc\u4e34\u5e8a\u7814\u7a76\u6570\u636e\u7684\u652f\u6301\u3002\u8fd9\u4e9b\u65b0\u65b9\u5f0f\u5305\u62ec\u8ddf\u8e2a\u8fd0\u52a8\u548c\u8eab\u4f53\u671d\u5411\uff0c\u91cf\u5316\u76ae\u80a4\u5bf9\u76ae\u80a4\u62a4\u7406\u7684\u751f\u7406\u76ca\u5904\uff0c\u6355\u83b7\u5fc3\u810f\u6d3b\u52a8\u7684\u58f0\u5b66\u7279\u5f81\uff0c\u8bb0\u5f55\u4e0e\u54ed\u58f0\u7684\u97f3\u8c03\u548c\u65f6\u95f4\u7279\u5f81\u76f8\u5173\u7684\u58f0\u97f3\u751f\u7269\u6807\u5fd7\u7269\u4ee5\u53ca\u76d1\u6d4b\u6536\u7f29\u538b\u7684\u53ef\u9760\u66ff\u4ee3\u7269\u3002\u80fd\u591f\u76d1\u6d4b\u989d\u5916\u7684\u8fd9\u4e9b\u4fe1\u606f\uff0c\u6709\u671b\u5e2e\u52a9\u53ca\u65e9\u53d1\u73b0\u4e0e\u4ea7\u4f24\u3001\u8111\u635f\u4f24\u3001\u75bc\u75db\u6216\u538b\u529b\u76f8\u5173\u7684\u5e76\u53d1\u75c7\u3002\u5728\u4e00\u9879\u5305\u62ec50\u540d\u91cd\u75c7\u5a74\u5e7c\u513f\u7684\u8bd5\u9a8c\u4e2d\uff0c\u7814\u7a76\u4eba\u5458\u53d1\u73b0\u8fd9\u79cd\u751f\u7269\u4f20\u611f\u5668\u8d34\u7247\u4e0e\u6807\u51c6\u7684\u4e34\u5e8a\u76d1\u6d4b\u7cfb\u7edf\u76f8\u6bd4\uff0c\u8868\u73b0\u51fa\u9ad8\u7ea7\u522b\u7684\u53ef\u9760\u6027\u548c\u51c6\u786e\u6027\u3002\u8fd9\u4e9b\u6280\u672f\u5e73\u53f0\u6709\u53ef\u80fd\u5927\u5927\u63d0\u9ad8\u65b0\u751f\u513f\u548c\u513f\u79d1\u91cd\u75c7\u76d1\u62a4\u7684\u8d28\u91cf\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<\/p>\n<p>https:\/\/doi.org\/10.1038\/s41591-020-0792-9<\/p>\n<p><strong><b>2\u3001Nat. Rev. Mater\uff1a\u7528\u4e8e\u690d\u5165\u5f0f\u548c\u53ef\u7a7f\u6234\u5f0f\u5149\u5b66\u4fdd\u5065\u8bbe\u5907\u7684\u591a\u529f\u80fd\u6750\u6599<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-199008 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72473-33.png\" alt=\"\" width=\"700\" height=\"600\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72473-33.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72473-33-300x257.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p><strong><b>\u65af\u5766\u798f\u5927\u5b66\u9c8d\u54f2\u5357\u9662\u58eb\u548cSei Kwang Hahn\u6559\u6388\u7b49\u56e2\u961f<\/b><\/strong>\u5408\u4f5c\u7efc\u8ff0\u4e86\u7528\u4e8e\u5f00\u53d1\u53ef\u690d\u5165\u548c\u53ef\u7a7f\u6234\u5149\u5b50\u4fdd\u5065\u8bbe\u5907\u7684\u6700\u65b0\u591a\u529f\u80fd\u6750\u6599\uff0c\u5e76\u8ba8\u8bba\u4e86\u8fdb\u4e00\u6b65\u5e73\u79fb\u5e94\u7528\u6240\u9700\u7684\u7279\u6027\u3002\u4f20\u7edf\u4e0a\uff0c\u8fd9\u4e9b\u65b9\u6cd5\u662f\u901a\u8fc7\u4f7f\u7528\u653e\u7f6e\u5728\u8bca\u6240\u6216\u60a3\u8005\u5e8a\u65c1\u7684\u4eea\u5668\u6765\u5b9e\u73b0\u7684\u3002\u4f46\u662f\uff0c\u6750\u6599\u548c\u79fb\u52a8\u8bbe\u5907\u7684\u6700\u65b0\u8fdb\u5c55\u6b63\u5728\u52a0\u901f\u53ef\u690d\u5165\u548c\u53ef\u7a7f\u6234\u5149\u5b66\u4fdd\u5065\u8bbe\u5907\u7684\u53d1\u5c55\uff0c\u4e3a\u65e0\u521b\u5373\u65f6\u68c0\u9a8c\u548c\u4e2a\u6027\u5316\u533b\u5b66\u94fa\u5e73\u4e86\u9053\u8def\u3002\u591a\u529f\u80fd\u6750\u6599\u53ef\u4ee5\u8bf1\u5bfc\u548c\u8c03\u8282\u751f\u7269\u7ec4\u7ec7\u4e2d\u57fa\u4e8e\u5149\u7684\u53cd\u5e94\u3002\u7814\u7a76\u4eba\u5458\u8fd8\u56de\u987e\u4e86\u4ee3\u8868\u6027\u7684\u53ef\u690d\u5165\u548c\u53ef\u7a7f\u6234\u533b\u7597\u8bbe\u5907\u7684\u7279\u6027\u548c\u529f\u80fd\u3002\u6700\u540e\uff0c\u7814\u7a76\u4eba\u5458\u63d0\u51fa\u4e86\u6539\u8fdb\u6b64\u7c7b\u8bbe\u5907\u7684\u672a\u6765\u7814\u7a76\u65b9\u5411\uff0c\u5e76\u6982\u8ff0\u4e86\u5b83\u4eec\u5728\u79fb\u52a8\u533b\u7597\u548c\u4e2a\u6027\u5316\u533b\u7597\u4e2d\u7684\u4f7f\u7528\u524d\u666f\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<\/p>\n<p>https:\/\/www.nature.com\/articles\/s41578-019-0167-3<\/p>\n<p><strong><b>3\u3001AFM\uff1a\u57fa\u4e8e\u65e0\u6eb6\u5242\u79bb\u5b50\u5bfc\u7535\u5f39\u6027\u4f53\u7535\u6781\u7684\u53ef\u62c9\u4f38\u3001\u900f\u660e\u548c\u70ed\u7a33\u5b9a\u7684\u6469\u64e6\u7535\u7eb3\u7c73\u53d1\u7535\u673a<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-199009 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72474-30.png\" alt=\"\" width=\"700\" height=\"544\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72474-30.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72474-30-300x233.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p><strong><b>\u4e2d\u56fd\u79d1\u5b66\u9662\u5317\u4eac\u7eb3\u7c73\u80fd\u6e90\u4e0e\u7cfb\u7edf\u7814\u7a76\u6240\u7684\u738b\u4e2d\u6797\u9662\u58eb\u3001\u84b2\u96c4\u7814\u7a76\u5458\u7b49\u7814\u7a76\u4eba\u5458<\/b><\/strong>\u62a5\u544a\u4e86\u4e00\u79cd\u79bb\u5b50\u6469\u64e6\u7535\u7eb3\u7c73\u53d1\u7535\u673a\uff08iTENG\uff09\uff0c\u8be5\u6280\u672f\u901a\u8fc7\u4f7f\u7528\u4ecb\u7535\u5f39\u6027\u4f53\u4f5c\u4e3a\u5e26\u7535\u5c42\u548c\u79bb\u5b50\u5bfc\u7535\u5f39\u6027\u4f53\u4f5c\u4e3a\u7535\u6781\uff0c\u80fd\u591f\u5b9e\u73b0\u751f\u7269\u673a\u68b0\u80fd\u7684\u6536\u96c6\u548c\u89e6\u6478\u611f\u5e94\u3002\u540c\u65f6\u5b9e\u73b0\u4e86\u8d85\u9ad8\u62c9\u4f38\u6027\u548c\u9ad8\u900f\u660e\u6027\u3002\u50cf\u76ae\u80a4\u4e00\u6837\u67d4\u8f6f\u7684\u7eb3\u7c73\u53d1\u7535\u673a\u80fd\u591f\u8f93\u51fa\u9ad8\u8fbe95 V\u7684\u5f00\u8def\u7535\u538b\u548c55.9 mW m<sup>-2<\/sup>\u7684\u77ac\u65f6\u9762\u79ef\u529f\u7387\u5bc6\u5ea6\u3002\u66f4\u91cd\u8981\u7684\u662f\uff0c\u6d88\u9664\u4e86\u5148\u524d\u62a5\u9053\u7684\u6c34\u51dd\u80f6\u7684\u8131\u6c34\u9650\u5236\u3002ICE\u76f4\u5230335\u00b0C\u90fd\u662f\u70ed\u7a33\u5b9a\u7684\uff0c\u57fa\u4e8eICE\u7684iTENG\uff08ICE-iTENG\uff09\u5373\u4f7f\u5728100\u00b0C\u4e0b\u4fdd\u630115 h\u4e5f\u4e0d\u4f1a\u8868\u73b0\u51fa\u8f93\u51fa\u6027\u80fd\u4e0b\u964d\u3002\u6b64\u5916\uff0c\u57fa\u4e8eICE-iTENG\u7684\u4f20\u611f\u5668\u5177\u6709\u4e09\u89d2\u5f62\u91d1\u5b57\u5854\u8868\u9762\u4f5c\u4e3a\u5e26\u7535\u5c42\uff0c\u53ef\u4ee5\u611f\u5e94\u4f4e\u81f30.4 kPa\u7684\u538b\u529b\u3002\u8be5\u7814\u7a76\u63d0\u51fa\u4e86\u4e00\u79cd\u53ef\u8d85\u7ea7\u4f38\u5c55\uff0c\u751f\u7269\u76f8\u5bb9\uff0c\u900f\u660e\u4e14\u5bf9\u73af\u5883\u7a33\u5b9a\u7684\u80fd\u91cf\u6536\u96c6\u5668\u548c\u89e6\u6478\u4f20\u611f\u5668\uff0c\u8868\u660e\u5373\u4f7f\u5728\u76f8\u5bf9\u8f83\u9ad8\u7684\u6e29\u5ea6\u4e0b\uff0c\u5b83\u4eec\u4e5f\u53ef\u80fd\u5e94\u7528\u5728\u667a\u80fd\u4eba\u9020\u76ae\u80a4\uff0c\u8f6f\u673a\u5668\u4eba\uff0c\u529f\u80fd\u663e\u793a\u5668\u548c\u53ef\u7a7f\u6234\u7535\u5b50\u4ea7\u54c1\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<\/p>\n<p>https:\/\/onlinelibrary.wiley.com\/doi\/abs\/10.1002\/adfm.201909252<\/p>\n<p><strong><b>4\u3001ACS Nano\uff1a\u7528\u4e8e\u67d4\u6027\u7535\u81f4\u53d1\u5149\u5668\u4ef6\u7684\u53ef\u6301\u7eed\u900f\u660e\u9c7c\u80f6\u819c<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-199010 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72475-28.png\" alt=\"\" width=\"700\" height=\"507\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72475-28.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72475-28-300x217.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p><strong><b>\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\u9ec4\u7ef4\u9662\u58eb\u3001\u5218\u4e3e\u5e86\u6559\u6388\u548c\u4e8e\u6d77\u4e1c\u6559\u6388\u7b49\u4eba<\/b><\/strong>\u901a\u8fc7\u6eb6\u6db2\u6d47\u94f8\u6cd5\u6210\u529f\u5730\u5236\u5907\u4e86\u9ad8\u5ea6\u900f\u660e\u548c\u67d4\u6027\u7684FG\u8584\u819c\u3002\u6240\u5236\u5f97\u7684FG\u8584\u819c\u5177\u6709\u9ad8\u5ea6\u7684\u67d4\u6027\uff0c\u5e76\u4e14\u80f6\u819c\u7684\u539a\u5ea6\u548c\u67d4\u6027\u4e5f\u6613\u8c03\u8282\u3002\u5b83\u5728\u53ef\u89c1\u5149\u8c31\u4e2d\u7684\u8868\u9762\u7c97\u7cd9\u5ea6\u4e5f\u4f4e\u81f30.5 nm\uff0c\u900f\u5149\u7387\u9ad8\u8fbe91.1\uff05\u3002\u901a\u8fc7\u4f7f\u7528\u5d4c\u5165Ag NWs\u7684FG\u8584\u819c\u4f5c\u4e3a\u5bfc\u7535\u7535\u6781\uff0c\u5236\u9020\u4e86\u4e00\u79cd\u67d4\u6027\uff0c\u53ef\u56de\u6536\u548c\u53ef\u751f\u7269\u964d\u89e3\u7684ACEL\u5668\u4ef6\u3002\u5f53\u5728300 V\u7684\u7535\u538b\u548c400 Hz\u7684\u9891\u7387\u4e0b\u5de5\u4f5c\u65f6\uff0c\u8be5\u8bbe\u5907\u663e\u793a\u7684\u4eae\u5ea6\u9ad8\u8fbe56 cd m<sup>-2<\/sup>\u3002\u6b64\u5916\uff0c\u8be5\u88c5\u7f6e\u5177\u6709\u9ad8\u5ea6\u7684\u67d4\u6027\uff0c\u5e76\u4e14\u57281000\u6b21\u5f2f\u66f2\u5faa\u73af\u540e\u4eae\u5ea6\u4ecd\u662f\u7a33\u5b9a\u7684\u3002\u8fd9\u9879\u5de5\u4f5c\u8868\u660e\uff0cFG\u819c\u662f\u67d4\u6027\u7535\u5b50\u4ea7\u54c1\uff0c\u7279\u522b\u662fACEL\u5668\u4ef6\u7684\u6709\u6f5c\u529b\u7684\u5019\u9009\u8005\u3002FG\u8584\u819c\u5728\u67d4\u6027\u7535\u5b50\u9886\u57df\u7684\u5176\u4ed6\u5e94\u7528\u53ef\u80fd\u5728\u4e0d\u4e45\u7684\u5c06\u6765\u5f97\u5230\u6269\u5c55\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<\/p>\n<p>https:\/\/pubs.acs.org\/doi\/abs\/10.1021\/acsnano.9b09880<\/p>\n<p><strong><b>5\u3001Small\uff1a<\/b><\/strong><strong><b>\u5177\u6709\u9ad8\u80fd\u91cf\u5bc6\u5ea6\u548c\u51fa\u8272\u53ef\u9760\u6027\u7684\u53ef\u7a7f\u6234\u7eba\u7ec7\u57fa<\/b><\/strong><strong><b>Co-Zn\u78b1\u6027\u5fae\u7535\u6c60<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-199011 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72476-28.png\" alt=\"\" width=\"700\" height=\"364\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72476-28.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72476-28-300x156.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p><strong><b>\u6b66\u6c49\u7406\u5de5\u5927\u5b66\u9ea6\u7acb\u5f3a\u6559\u6388\u3001\u4f55\u4eae\u7b49\u7814\u7a76\u4eba\u5458<\/b><\/strong>\u63d0\u51fa\u4e86\u4e00\u79cd\u7b80\u4fbf\u53ef\u884c\u7684\u65b9\u6cd5\uff0c\u5e76\u91c7\u7528\u65b0\u9896\u7684\u5668\u4ef6\u8bbe\u8ba1\u6765\u5236\u9020\u9ad8\u6027\u80fd\u7684\u5e73\u9762\u5185Co-Zn\u78b1\u6027\u5fae\u7535\u6c60\u3002CH @ NC-LDH @ NT\u6838\u58f3\u7535\u6781\u662f\u901a\u8fc7\u5316\u5b66\u9540\u7ed3\u5408\u6c34\u70ed\u6cd5\u548c\u7535\u6c89\u79ef\u6cd5\u5236\u5907\u7684\u3002\u7531\u4e8e3D\u9ad8\u901f\u7535\u5b50\u4f20\u8f93\u7f51\u7edc\u548c\u5206\u5c42\u6838\u58f3\u7ed3\u6784\u7684\u534f\u540c\u6548\u5e94\uff0cCo-Zn\u5fae\u7535\u6c60\u53ef\u63d0\u4f9b\u9ad8\u6027\u80fd\u3002\u6b64\u5916\uff0c\u7814\u7a76\u4eba\u5458\u901a\u8fc7\u91c7\u7528\u6fc0\u5149\u96d5\u523b\u65b9\u6cd5\u548c\u4f20\u9012\u6a21\u5851\u5de5\u827a\uff0c\u5206\u522b\u5236\u9020\u4e86\u96c6\u6210\u7684\u5fae\u7535\u6781\u548c\u67d4\u6027\u56fe\u6848\u5316\u7684\u5bb9\u5668\u3002\u5408\u7406\u7684\u6c9f\u69fd\u578b\u914d\u7f6e\u53ef\u4ee5\u6709\u6548\u5730\u9632\u6b62\u7531\u4e8e\u7535\u6781\u63a5\u89e6\u5f15\u8d77\u7684\u77ed\u8def\u3002\u7ec4\u88c5\u597d\u7684Co-Zn\u78b1\u6027\u5fae\u7535\u6c60\u53ef\u63d0\u4f9b\u51fa\u8272\u7684\u80fd\u91cf\/\u529f\u7387\u5bc6\u5ea6\uff080.17 mWh cm<sup>-2 <\/sup>\/ 14.4 mW cm<sup>-2<\/sup>\uff09\u548c\u51fa\u8272\u7684\u5faa\u73af\u7a33\u5b9a\u6027\uff08800\u4e2a\u5faa\u73af\u4e2d\u7684\u5bb9\u91cf\u4fdd\u6301\u7387\u8fbe71\uff05\uff09\u3002\u8be5\u7814\u7a76\u5de5\u4f5c\u6f14\u793a\u4e86\u5fae\u7535\u6c60\u7684\u5de7\u5999\u5236\u9020\u5de5\u827a\u4ee5\u53ca\u5408\u7406\u7684\u8bbe\u5907\u8bbe\u8ba1\uff0c\u4ece\u800c\u4e3a\u5728\u67d4\u6027\u548c\u4fbf\u643a\u5f0f\u7535\u5b50\u4ea7\u54c1\u4e2d\u5f00\u53d1\u5fae\u5668\u4ef6\u63d0\u4f9b\u4e86\u65b0\u7684\u7b56\u7565\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<\/p>\n<p>https:\/\/onlinelibrary.wiley.com\/doi\/abs\/10.1002\/smll.202000293<\/p>\n<p><strong><b>6\u3001Science Advances\uff1a\u6e7f\u5bfc\u7535\u805a\u5408\u7269\u5728\u5404\u79cd\u57fa\u6750\u4e0a\u7684\u5f3a\u7c98\u5408\u529b<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-199013 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72477-23.png\" alt=\"\" width=\"700\" height=\"823\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72477-23.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72477-23-255x300.png 255w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p><strong><b>\u7f8e\u56fd\u9ebb\u7701\u7406\u5de5\u5b66\u9662\u8d75\u9009\u8d3a\u6559\u6388\u7b49\u4eba<\/b><\/strong>\u63d0\u51fa\u4e86\u4e00\u79cd\u901a\u7528\u800c\u53c8\u7b80\u5355\u7684\u65b9\u6cd5\uff0c\u5373\u901a\u8fc7\u4e2d\u95f4\u7684\u4eb2\u6c34\u6027\u805a\u5408\u7269\u7c98\u5408\u5242\u5c42\u6765\u5b9e\u73b0\u5404\u79cd\u6e7f\u5bfc\u7535\u805a\u5408\u7269\u5728\u4e0d\u540c\u57fa\u6750\u4e0a\u7684\u7262\u56fa\u7c98\u5408\u3002\u7814\u7a76\u4eba\u5458\u63d0\u51fa\u7684\u65b9\u6cd5\u53ef\u4ee5\u5728\u5404\u79cd\u7edd\u7f18\u548c\u5bfc\u7535\u886c\u5e95\uff08\u5305\u62ec\u73bb\u7483\uff0cPDMS\uff0c\u805a\u9170\u4e9a\u80fa\uff0cITO\u548c\u91d1\uff09\u4ee5\u53ca\u5177\u6709\u4ee3\u8868\u6027\u7684\u751f\u7269\u7535\u5b50\u8bbe\u5907\u4e0a\uff0c\u5c06\u5404\u79cd\u6e7f\u5bfc\u7535\u805a\u5408\u7269\uff08\u5982PEDOT\uff1aPSS\uff0cPPy\u548cPAni\uff09\u7262\u56fa\u5730\u96c6\u6210\u5230\u754c\u9762\u4e0a\u3002\u7c98\u9644\u5728\u57fa\u6750\u4e0a\u7684\u6240\u5f97\u5bfc\u7535\u805a\u5408\u7269\u5728\u4e0d\u5f71\u54cd\u5bfc\u7535\u805a\u5408\u7269\u7684\u7535\u5b66\u6216\u673a\u68b0\u6027\u80fd\u7684\u60c5\u51b5\u4e0b\uff0c\u5177\u6709\u51fa\u8272\u7684\u7c98\u5408\u6027\u80fd\uff08\u8d85\u8fc7120 kPa\u7684\u526a\u5207\u5f3a\u5ea6\uff09\u4ee5\u53ca\u51fa\u8272\u7684\u673a\u68b0\u548c\u7535\u5316\u5b66\u7a33\u5b9a\u6027\u3002\u8be5\u65b9\u6cd5\u4e0e\u7528\u4e8e\u5bfc\u7535\u805a\u5408\u7269\u7684\u5404\u79cd\u5236\u9020\u65b9\u6cd5\u517c\u5bb9\uff0c\u5305\u62ec\u6eb6\u5242\u6d47\u94f8\u548c\u7535\u6c89\u79ef\uff0c\u5e76\u5141\u8bb8\u4f7f\u7528\u53ef\u5546\u8d2d\u7684\u6750\u6599\uff08\u4f8b\u5982\u4eb2\u6c34\u6027PU\u548c\u5bfc\u7535\u805a\u5408\u7269\uff09\uff0c\u4ece\u800c\u5728\u751f\u7269\u7535\u5b50\u8bbe\u5907\u4e2d\u5e7f\u6cdb\u5e94\u7528\u3002\u8fd9\u9879\u7814\u7a76\u4e0d\u4ec5\u63d0\u4f9b\u4e86\u4e00\u79cd\u7b80\u5355\u800c\u6709\u6548\u7684\u65b9\u6cd5\u6765\u89e3\u51b3\u751f\u7269\u805a\u5408\u7269\u4e2d\u5bfc\u7535\u805a\u5408\u7269\u96c6\u6210\u7684\u95ee\u9898\uff0c\u800c\u4e14\u8fd8\u63d0\u4f9b\u4e86\u5728\u5404\u79cd\u6c34\u51dd\u80f6\u4e0e\u57fa\u6750\u4e4b\u95f4\u5b9e\u73b0\u7262\u56fa\u7c98\u5408\u7684\u901a\u7528\u7b56\u7565\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<\/p>\n<p>https:\/\/doi.org\/10.1126\/sciadv.aay5394<\/p>\n<p><strong><b>7\u3001JACS\uff1a\u53ef\u7a7f\u6234\u5f0f\u5fae\u9488\u4f20\u611f\u5668\u9635\u5217\u4e0a\u963f\u7247\u7c7b\u836f\u7269\u4e0e\u795e\u7ecf\u7c7b\u836f\u7269\u7684\u8fde\u7eed\u76d1\u6d4b<\/b><\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"size-full wp-image-199015 aligncenter\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72478-21.png\" alt=\"\" width=\"700\" height=\"633\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72478-21.png 700w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/03\/\u56fe\u72478-21-300x271.png 300w\" sizes=\"(max-width: 700px) 100vw, 700px\" \/><\/p>\n<p><strong><b>\u7f8e\u56fd\u52a0\u5229\u798f\u5c3c\u4e9a\u5927\u5b66Joseph Wang\u9662\u58eb\u7b49\u7814\u7a76\u4eba\u5458<\/b><\/strong>\u63d0\u51fa\u4e86\u5728\u5355\u4e2a\u53ef\u7a7f\u6234\u5e73\u53f0\u4e0a\u540c\u65f6\u5fae\u521b\u68c0\u6d4b\u82ac\u592a\u5c3c\u548cOP\u795e\u7ecf\u5236\u5242\u7684\u5fae\u9488\u4f20\u611f\u5668\u9635\u5217\u3002\u6700\u7ec8\u7684\u5fae\u9488\u4f20\u611f\u5668\u9635\u5217\u80fd\u591f\u533a\u5206\u51fa\u8fc7\u91cf\u963f\u7247\u7c7b\u836f\u7269\u548c\u795e\u7ecf\u6bd2\u7269\u4e2d\u6bd2\u7684\u53d1\u751f\uff0c\u5373\u80fd\u591f\u8fc5\u901f\u5730\u8bc6\u522b\u51fa\u8fd9\u79cd\u672a\u77e5\u7684\u66b4\u9732\uff0c\u5e76\u7acb\u5373\u8fdb\u884c\u6cbb\u7597\u3002\u65b0\u7684\u5fae\u9488\u4f20\u611f\u5668\u9635\u5217\u5e73\u53f0\u5728\u6a21\u62df\u743c\u8102\u7cd6\u51dd\u80f6\u4e2d\u5bf9OPi\u548cOP\u76ee\u6807\u663e\u793a\u51fa\u4f18\u5f02\u7684\u5206\u6790\u6027\u80fd\uff0c\u5305\u62ec\u9ad8\u7075\u654f\u5ea6\uff0c\u9009\u62e9\u6027\u548c\u7a33\u5b9a\u6027\u3002\u6b64\u5916\uff0c\u5c3d\u7ba1\u963f\u7247\u7c7b\u836f\u7269\u5fae\u9488\u4f20\u611f\u5668\u53ef\u4ee5\u6839\u636e\u5176\u72ec\u7279\u7684\u6c27\u5316\u8fd8\u539f\u7279\u5f81\u68c0\u6d4b\u82ac\u592a\u5c3c\uff0c\u5e76\u6839\u636e\u4e0d\u540c\u7684\u7535\u4f4d\u6d4b\u91cf\u5417\u5561\u548c\u53bb\u7532\u82ac\u592a\u5c3c\uff0c\u4f46\u5b83\u5e76\u4e0d\u662f\u901a\u7528\u7684\u963f\u7247\u7c7b\u836f\u7269\u68c0\u6d4b\u5668\u3002\u8fd9\u79cd\u591a\u6a21\u5f0f\u53ef\u7a7f\u6234\u4f20\u611f\u5e73\u53f0\u5728\u73b0\u573a\u73af\u5883\u4e2d\u5bf9\u836f\u7269\u548c\u795e\u7ecf\u5236\u5242\u7684\u66b4\u9732\u63d0\u4f9b\u53ca\u65f6\u7684\u53cd\u9988\u548c\u9002\u5f53\u7684\u5bf9\u7b56\u5177\u6709\u5f88\u5927\u7684\u6f5c\u529b\u3002\u5728\u6982\u5ff5\u9a8c\u8bc1\u6f14\u793a\u4e2d\u83b7\u5f97\u7684\u4ee4\u4eba\u9f13\u821e\u7684\u5206\u6790\u7ed3\u679c\u4e3a\u5feb\u901f\u201c\u611f\u77e5\u5e76\u91c7\u53d6\u884c\u52a8\u201d\u7684\u95ed\u73af\u53ef\u7a7f\u6234\u7cfb\u7edf\u4ee5\u53ca\u53ca\u65f6\u91c7\u53d6\u5bf9\u7b56\uff08\u4ece\u540c\u4e00\u5fae\u9488\u8d34\u7247\u91ca\u653e\u89e3\u6bd2\u5242\uff09\u63d0\u4f9b\u4e86\u65b0\u7684\u53ef\u80fd\u6027\u3002\u56e0\u6b64\uff0c\u672a\u6765\u7684\u5de5\u4f5c\u5c06\u5305\u62ec\u5bf9\u65b0\u7684\u5fae\u9488\u8d34\u7247\u8fdb\u884c\u8be6\u7ec6\u7684\u52a8\u7269\u7814\u7a76\uff0c\u5e76\u5c06\u5176\u4e0e\u53ca\u65f6\u7684\u6cbb\u7597\u4f53\u7cfb\u7ed3\u5408\u8d77\u6765\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<\/p>\n<p>https:\/\/pubs.acs.org\/doi\/abs\/10.1021\/jacs.0c01883<\/p>\n<p>\u672c\u6587\u7531eric\u4f9b\u7a3f\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1: tougao@cailiaoren.com.<\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaorenVIP\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u53ef\u7a7f\u6234\u6280\u672f\uff0c\u662f\u7531\u9ebb\u7701\u7406\u5de5\u5b66\u9662\u5a92\u4f53\u5b9e\u9a8c\u5ba4\u6700\u65e9\u572820\u4e16\u7eaa60\u5e74\u4ee3\u63d0\u51fa\u7684\u521b\u65b0\u6280\u672f\u3002\u5229\u7528\u8be5\u6280\u672f\uff0c\u53ef\u4ee5\u628a\u591a\u5a92\u4f53\u3001\u4f20\u611f\u5668\u548c\u65e0\u7ebf\u901a\u4fe1\u7b49\u6280\u672f\u5d4c\u5165\u4eba\u4eec\u7684\u8863\u7269\u4e2d\uff0c\u53ef\u652f\u6301\u624b\u52bf\u548c\u773c\u52a8\u64cd&#8230;<\/p>\n","protected":false},"author":10213,"featured_media":199006,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1187],"tags":[],"class_list":["post-199004","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-zhuanlan"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/199004"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/10213"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=199004"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/199004\/revisions"}],"predecessor-version":[{"id":199615,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/199004\/revisions\/199615"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/199006"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=199004"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=199004"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=199004"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}