{"id":199481,"date":"2020-04-07T06:50:05","date_gmt":"2020-04-06T22:50:05","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=199481"},"modified":"2020-04-06T19:51:09","modified_gmt":"2020-04-06T11:51:09","slug":"%e6%9e%81%e7%ab%af%e5%88%b6%e9%80%a0%e5%b0%81%e9%9d%a2%e6%96%87%e7%ab%a0%e4%b8%a8%e6%97%a5%e6%9c%ac%e7%90%86%e5%8c%96%e5%ad%a6%e7%a0%94%e7%a9%b6%e6%89%80%ef%bc%9a%e6%b0%b4%e4%b8%8b%e6%8c%81%e4%b9%85","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=199481","title":{"rendered":"\u6781\u7aef\u5236\u9020\u5c01\u9762\u6587\u7ae0\u4e28\u65e5\u672c\u7406\u5316\u5b66\u7814\u7a76\u6240\uff1a\u6c34\u4e0b\u6301\u4e45\u6c14\u6ce1\u8f85\u52a9\u98de\u79d2\u6fc0\u5149\u5fae\u7eb3\u7c73\u591a\u5c3a\u5ea6\u590d\u5408\u7ec7\u6784"},"content":{"rendered":"<p><strong>\u3010\u672c\u6587\u4eae\u70b9\u3011<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199484\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f71-\u6587\u4e2d\u56fe1.jpg\" alt=\"\" width=\"944\" height=\"843\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f71-\u6587\u4e2d\u56fe1.jpg 944w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f71-\u6587\u4e2d\u56fe1-300x268.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f71-\u6587\u4e2d\u56fe1-768x686.jpg 768w\" sizes=\"(max-width: 944px) 100vw, 944px\" \/><\/p>\n<p>\u56fe1. \u6c34\u4e0b\u6301\u4e45\u6c14\u6ce1\u8f85\u52a9\u98de\u79d2\u6fc0\u5149\u52a0\u5de5\u793a\u610f\u56fe\u548c\u5178\u578b\u7ed3\u6784<\/p>\n<p><strong>\u8fd1\u65e5\uff0c\u65e5\u672c\u7406\u5316\u5b66\u7814\u7a76\u6240\uff08<\/strong><strong>RIKEN<\/strong><strong>\uff09\u6749\u5188\u5e78\u6b21\u6559\u6388\u548c\u5f20\u4e1c\u77f3\u535a\u58eb\u5728\u300a\u6781\u7aef\u5236\u9020\u300b\u671f\u520a\uff08<\/strong><strong><em>International Journal of Extreme Manufacturing<\/em><\/strong><strong>, IJEM<\/strong><strong>\uff09\u4e0a\u53d1\u8868\u4e86\u4e00\u7bc7\u9898\u4e3a\u201c<\/strong><strong>Underwater persistent bubble-assisted femtosecond laser ablation for hierarchical micro\/nanostructuring\u201d<\/strong><strong>\u7684\u8bba\u6587\u3002<\/strong>\u672c\u6587\u5c55\u73b0\u4e86\u4e00\u79cd\u6c34\u4e0b\u6301\u4e45\u6c14\u6ce1\u8f85\u52a9\u98de\u79d2\u6fc0\u5149\u52a0\u5de5\u7684\u65b0\u5de5\u827a\uff0c\u80fd\u5b9e\u73b0\u6beb\u7c73\uff0c\u5fae\u7c73\u548c\u7eb3\u7c73\u591a\u5c3a\u5ea6\u7ec7\u6784\u5316\uff0c\u6781\u5927\u5730\u4e30\u5bcc\u4e86\u6fc0\u5149\u52a0\u5de5\u5de5\u827a\u548c\u6fc0\u5149\u7ec7\u6784\u7ed3\u6784\u7684\u591a\u6837\u6027\u3002\u6b64\u79cd\u5de5\u827a\u80fd\u4ea7\u751f\u5177\u6709\u5c3e\u90e8\u540c\u5fc3\u5706\u72b6\u6beb\u7c73\u7ea7\u5b8f\u89c2\u7ed3\u6784\u3002\u52a8\u6001\u6c14\u6ce1\u6247\u5f62\u884d\u5c04\u6fc0\u5149\u52a0\u5de5\u5f62\u6210\u7684\u5c3e\u72b6\u5b8f\u89c2\u7ed3\u6784\u662f\u7531\u591a\u5c42\u6247\u5f62\uff08\u4e2d\u5fc3\u89d245-141\u00b0\uff09\u590d\u5408\u5fae\u7eb3\u7c73\u7ed3\u6784\u7ec4\u6210\u7684\u3002\u9759\u6001\u6c14\u6ce1\u8f85\u52a9\u6fc0\u5149\u52a0\u5de5\u5f62\u6210\u7684\u540c\u5fc3\u5706\u5b8f\u89c2\u7ed3\u6784\u5305\u542b\u4e86\u4f4e\/\u9ad8\/\u8d85\u9ad8\u5468\u671f\u6027\u7eb3\u7c73\u7ed3\u6784\uff0c\u5468\u671f\u5206\u522b\u4e3a550\u2013900, 100\u2013200, 40\u2013100 nm\u300240nm\u5468\u671f\uff0c\u5c0f\u4e8e1030nm\u6fc0\u5149\u6ce2\u957f\u76841\/25\uff0c\u662f\u76ee\u524d\u5728\u7845\u4e0a\u53ef\u5236\u5907\u7684\u6700\u5c0f\u8868\u9762\u6fc0\u5149\u8bf1\u5bfc\u5468\u671f\u7ed3\u6784\u3002\u72ec\u7279\u7684\u591a\u5c3a\u5ea6\u590d\u5408\u7ed3\u6784\u548c\u8d85\u9ad8\u9891\u5468\u671f\u7eb3\u7c73\u7ed3\u6784\u7684\u5236\u5907\u8bc1\u660e\u4e86\u6c14\u6ce1\u662f\u4e00\u79cd\u51e0\u4e4e\u96f6\u6210\u672c\u7684\u63a9\u6a21\u7248\uff0c\u4e3a\u591a\u5c3a\u5ea6\u590d\u6742\u7ec7\u6784\u5316\u63d0\u4f9b\u4e86\u65b0\u7684\u53ef\u8c03\u63a7\u5143\u7d20\u3002\u8be5\u5de5\u827a\u7684\u5f00\u53d1\u4e3a\u6781\u7aef\u73af\u5883\u4e0b\u7684\u591a\u5c3a\u5ea6\u5fae\u7eb3\u52a0\u5de5\u6253\u5f00\u4e86\u4e00\u9053\u65b0\u7684\u5927\u95e8\u3002<\/p>\n<p><strong>\u3010\u5185\u5bb9\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u65e5\u672c\u7406\u5316\u5b66\u7814\u7a76\u6240\uff08RIKEN\uff09\u6749\u5188\u5e78\u6b21\uff08Koji Sugioka\uff09\u6559\u6388\u548c\u5f20\u4e1c\u77f3\u535a\u58eb\u5728\u672c\u6587\u4e2d\u9996\u5148\u5c55\u793a\u4e86\u6c14\u6ce1\u7684\u52a8\u529b\u5b66\u8fc7\u7a0b\u4ee5\u53ca\u76f8\u5e94\u7684\u6beb\u7c73\u7ea7\u5b8f\u89c2\u7ec7\u6784\u5316\u7ed3\u6784\u5f62\u6001\u3002\u4f5c\u8005\u6839\u636e\u6c14\u6ce1\u4e0d\u540c\u5f62\u6001\u628a\u8be5\u5de5\u827a\u7ec6\u5316\u4e3a\u52a8\u6001\u548c\u9759\u6001\u6c34\u4e0b\u6301\u4e45\u6c14\u6ce1\u8f85\u52a9\u98de\u79d2\u6fc0\u5149\u52a0\u5de5\uff0c\u5e76\u5bf9\u4e0d\u540c\u6c14\u6ce1\u72b6\u6001\u4e0b\u751f\u6210\u7684\u8868\u9762\u7ed3\u6784\u8fdb\u884c\u4e86\u8be6\u7ec6\u5206\u6790\u3002\u901a\u8fc7\u548c\u7406\u5316\u5b66\u7814\u7a76\u6240\u5148\u8fdb\u5149\u5b66\u4e2d\u5fc3RAP\u7684\u7530\u4e2d\u62d3\u7537\uff08Takuo Tanaka\uff09\u6559\u6388\u548cBikas Ranjan\u535a\u58eb\u5408\u4f5c\uff0c\u5bf9\u4e0d\u540c\u52a0\u5de5\u6761\u4ef6\u4e0b\u5236\u5907\u7684\u5c3e\u72b6\u7ed3\u6784\u5728\u8fd1\u7ea2\u5916\u5230\u4e2d\u7ea2\u5916\u7684\u5149\u5b66\u53cd\u5c04\u900f\u5c04\u7279\u6027\u8fdb\u884c\u4e86\u6bd4\u8f83\uff0c\u5e76\u63ed\u793a\u4e86\u7ed3\u6784\u7279\u6027\u5bf9\u53cd\u5c04\u548c\u900f\u5c04\u6548\u679c\u7684\u5f71\u54cd\u3002\u00a0<\/p>\n<p><strong>\u3010\u7814\u7a76\u80cc\u666f\u3011<\/strong><\/p>\n<p>\u6db2\u4f53\u8f85\u52a9\u6fc0\u5149\u52a0\u5de5\u7531\u4e8e\u53ef\u4ee5\u6709\u6548\u6291\u5236\u70ed\u6548\u5e94\uff0c\u53ca\u65f6\u53bb\u9664\u751f\u4ea7\u7c89\u672b\uff0c\u80fd\u6781\u5927\u5730\u63d0\u5347\u52a0\u5de5\u8d28\u91cf\uff0c\u5728\u65e0\u63a5\u89e6\u5207\u5272\u592a\u9633\u80fd\u7535\u6c60\u677f\u65b9\u9762\u6709\u6781\u5927\u7684\u5e94\u7528\u524d\u666f \u30101\u3011\u3002\u4f46\u662f\u6db2\u76f8\u52a0\u5de5\u4ecd\u7136\u5b58\u5728\u95ee\u9898\uff0c\u6bd4\u5982\u6fc0\u5149\u52a0\u5de5\u8fc7\u7a0b\u4e2d\u4f1a\u5bfc\u81f4\u6c34\u7684\u5206\u89e3\u5f62\u6210\u5927\u91cf\u7684\u6c14\u6ce1\uff0c\u8fd9\u4e9b\u6c14\u6ce1\u4f1a\u9ecf\u9644\u5728\u6750\u6599\u8868\u9762\uff0c\u4e25\u91cd\u5f71\u54cd\u52a0\u5de5\u8d28\u91cf\u5e76\u964d\u4f4e\u4e86\u52a0\u5de5\u6548\u7387\uff08\u56fe2a-b\uff09\u3002\u6240\u4ee5\u9ad8\u7cbe\u5bc6\u52a0\u5de5\u666e\u904d\u91c7\u7528\u52a8\u6001\u6db2\u4f53\u73af\u5883\u53ca\u65f6\u53bb\u9664\u9ecf\u9644\u7684\u6c14\u6ce1\uff0c\u907f\u514d\u6c14\u6ce1\u5f15\u8d77\u7684\u8d1f\u9762\u6548\u5e94\uff08\u56fe2c\uff09\u30102\u3011\u3002<\/p>\n<p>\u96be\u9053\u8fd9\u4e9b\u8868\u9762\u9ecf\u9644\u6c14\u6ce1\u771f\u7684\u5c31\u53ea\u662f\u718a\u5b69\u5b50\uff0c\u6c38\u8fdc\u4e0d\u53d7\u6b22\u8fce\uff0c\u627e\u4e0d\u51fa\u4efb\u4f55\u4f18\u70b9\u5417\uff1f\u6749\u5188\u5e78\u6b21\u6559\u6388\u548c\u5f20\u4e1c\u77f3\u535a\u58eb\u5e0c\u671b\u901a\u8fc7\u5b9e\u9a8c\u6253\u7834\u4eba\u4eec\u4f20\u7edf\u7684\u8ba4\u77e5\uff0c\u8ba9\u4eba\u4eec\u5bf9\u89c4\u5f8b\u6027\u7684\u4e1c\u897f\u91cd\u65b0\u8ba4\u8bc6\uff0c\u5c31\u5982\u540c\u4ed6\u4eec\u6700\u8fd1\u53d1\u8868\u5728OEA\u7684\u4e00\u7bc7\u6587\u7ae0\u62a5\u9053\u4e86\u5728\u68af\u5ea6\u7845\u5fae\u7c73\u7ed3\u6784\u4e0a\uff0c\u6fc0\u5149\u8bf1\u5bfc\u8868\u9762\u5468\u671f\u8868\u9762\u7eb3\u7c73\u7ed3\u6784\uff08LIPSS\uff09\u7684\u65b9\u5411\u4e0d\u662f\u4e25\u683c\u9075\u5faa\u4f20\u7edf\u89c4\u5f8b\u5782\u76f4\u4e8e\u6fc0\u5149\u504f\u632f\u65b9\u5411\uff0c\u800c\u662f\u4f1a\u6709\u6700\u592750\u00b0\u89d2\u5ea6\u7684\u504f\u79fb\u30103\u3011\u3002<\/p>\n<p>\u56e0\u4e3a\u4e0d\u540c\uff0c\u6240\u4ee5\u6709\u8da3\uff01\u5e0c\u671b\u60a8\u80fd\u559c\u6b22\u8fd9\u7bc7\u53d1\u8868\u5728IJEM\u4e0a\u76f8\u5bf9\u6709\u8da3\u7684\u62a5\u9053\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199485\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f72-\u6587\u4e2d\u56fe2.jpg\" alt=\"\" width=\"333\" height=\"141\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f72-\u6587\u4e2d\u56fe2.jpg 333w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f72-\u6587\u4e2d\u56fe2-300x127.jpg 300w\" sizes=\"(max-width: 333px) 100vw, 333px\" \/><\/p>\n<p>\u56fe 2 \uff08a-b\uff09\u9759\u6001\u6db2\u4f53\u6fc0\u5149\u52a0\u5de5\u8fc7\u7a0b\u4e2d\u5f62\u6210\u7684\u6301\u4e45\u9ecf\u9644\u6c14\u6ce1\u548c\u5176\u8d1f\u9762\u6548\u5e94\uff0c\uff08c\uff09\u52a8\u6001\u6db2\u4f53\u53bb\u9664\u6c14\u6ce1\u7684\u6fc0\u5149\u52a0\u5de5\u5f62\u8c8c\u5bf9\u6bd4\u56fe \u30102\u3011\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u6c14\u6ce1\u52a8\u6001\u8fc7\u7a0b\u548c\u6beb\u7c73\u5c3a\u5ea6\u7ec7\u6784\u7ed3\u6784<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199486\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f73-\u6587\u4e2d\u56fe3.jpg\" alt=\"\" width=\"1270\" height=\"897\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f73-\u6587\u4e2d\u56fe3.jpg 1270w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f73-\u6587\u4e2d\u56fe3-300x212.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f73-\u6587\u4e2d\u56fe3-768x542.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f73-\u6587\u4e2d\u56fe3-1024x723.jpg 1024w\" sizes=\"(max-width: 1270px) 100vw, 1270px\" \/><\/p>\n<p>\u56fe3 \u6c14\u6ce1\u52a8\u6001\u8fc7\u7a0b\uff08\u79fb\u52a8\u6027\u548c\u7d2f\u79ef\u6548\u5e94\uff09\uff0c\u52a8\u6001\u548c\u9759\u6001\u6c14\u6ce1\u884d\u5c04\u73b0\u8c61\u53ca\u76f8\u5e94\u5b8f\u89c2\u7ec7\u6784\u7ed3\u6784\u3002\uff08\u6fc0\u5149\u53c2\u6570\uff1a \u6ce2\u957f1030nm\uff0c \u91cd\u590d\u9891\u7387200kHz\uff0c\u8109\u5bbd223fs\uff0c\u6fc0\u5149\u80fd\u91cf100mW\uff0c\u8109\u51b2\u80fd\u91cf0.5\u03bcJ\uff0c\u626b\u63cf\u901f\u5ea61mm\/s\uff0c\u626b\u63cf\u7ebf\u95f4\u96945\u03bcm\uff09.\uff08a-c\uff09\u540c\u4e00\u6807\u5c3a100\u03bcm\uff0c\uff08g\uff09\u6807\u5c3a\u4e3a1mm\uff0c\uff08h-j\uff09\u540c\u4e00\u6807\u5c3a100\u03bcm\u3002<\/p>\n<p>\u5728\u672a\u542f\u52a8\u6db2\u76f8\u52a0\u5de5\u65f6\uff0c\u7845\u8868\u9762\u6ca1\u6709\u6c14\u6ce1\uff08\u56fe3a\uff09\u3002\u5f53\u542f\u52a8\u6fc0\u5149\u626b\u63cf\u540e\uff0c\u4fbf\u751f\u6210\u4e86\u5927\u91cf7-46\u5fae\u7c73\u76f4\u5f84\u7684\u5c0f\u6c14\u6ce1\uff08\u56fe3b\uff09\uff0c\u8fd9\u4e9b\u5c0f\u6c14\u6ce1\u4f1a\u7c98\u9644\u5728\u52a0\u5de5\u626b\u63cf\u8def\u5f84\u9644\u8fd1\u3002\u5f53 \u201c\u5f13\u201d\u5b57\u578b\u626b\u63cf\u7684\u7b2c\u4e8c\u6761\u7ebf\u65f6\uff0c\u6c14\u6ce1\u76f4\u5f84\u5df2\u53ef\u8fbe270\u5fae\u7c73\uff08\u56fe3c\uff09\u3002\u5c3a\u5bf8\u7684\u589e\u52a0\u662f\u7531\u4e8e\u7d2f\u79ef\u6548\u5e94\uff08\u5438\u6536\u9644\u4ef6\u7684\u6c14\u6ce1\uff09\uff08\u56fe3d-f\uff09\u5bfc\u81f4\u7684\u3002\u8fd9\u4e9b\u5927\u5c3a\u5ea6\u7684\u6c14\u6ce1\u201c\u6321\u201d\u5728\u6fc0\u5149\u52a0\u5de5\u8def\u5f84\u4e0a\uff0c\u4e0d\u53ef\u907f\u514d\u5730\u9020\u6210\u4e86\u6fc0\u5149\u7684\u884d\u5c04\u73b0\u8c61\uff08\u56fe3h\uff09\u4e5f\u4f1a\u540c\u65f6\u5f15\u8d77Marangoni\u9a6c\u5170\u6208\u5c3c\u6548\u5e94\uff0c\u63a8\u52a8\u6c14\u6ce1\u5411\u4e0b\u79fb\u52a8(\u56fe3i)\u3002\u968f\u7740\u201c\u5f13\u201d\u626b\u63cf\u4e0d\u65ad\u8fdb\u884c\uff0c\u6c14\u6ce1\u4f53\u79ef\u9010\u6e10\u589e\u5927\uff0c\u5f53\u5230\u8fbe\u4e00\u5b9a\u5c3a\u5bf8\u540e\uff08\u6570\u767e\u5fae\u7c73\uff09\uff0c\u6c14\u6ce1\u4e0d\u518d\u79fb\u52a8\uff0c\u8fd9\u65f6\u6fc0\u5149\u624d\u80fd\u8f90\u7167\u5230\u6c14\u6ce1\u7684\u4e2d\u5fc3\u548c\u524d\u9762\u90e8\u4f4d\uff08\u56fe3j\uff09\u3002\u5728\u4e2d\u5fc3\u9876\u90e8\u4f1a\u6709\u975e\u5e38\u5f3a\u7684\u6563\u5c04\u6548\u5e94\uff0c\u6240\u4ee5\u4e2d\u5fc3\u90e8\u5206\u7684\u52a0\u5de5\u6548\u7387\u975e\u5e38\u4f4e\u3002\u6c14\u6ce1\u8fd1\u8fb9\u7f18\u90e8\u5206\u4f1a\u6709\u5f3a\u70c8\u7684\u884d\u5c04\uff0c\u5bfc\u81f4\u6fc0\u5149\u7684\u52a0\u5de5\u65b9\u5411\u504f\u8f6c\u3002\u56fe3g\u56fe\u793a\u4e862mm\u00d72mm\u6c34\u4e0b\u6301\u4e45\u6c14\u6ce1\u8f85\u52a9\u98de\u79d2\u6fc0\u5149\u52a0\u5de5\u7ec7\u6784\u7684\u6beb\u5fae\u7eb3\u7c73\u591a\u5c3a\u5ea6\u7684\u590d\u5408\u7ed3\u6784\u3002\u53ef\u4ee5\u5f88\u660e\u663e\u770b\u51fa\u751f\u6210\u4e86\u4e24\u4e2a\u5177\u6709\u5c3e\u90e8\u7684\u540c\u5fc3\u5706\u72b6\u6beb\u7c73\u7ea7\u5b8f\u89c2\u7ed3\u6784\u548c\u591a\u6761\u4ec5\u6709\u5c3e\u72b6\u7684\u5b8f\u89c2\u7ed3\u6784\u3002\u5c3e\u72b6\u7ed3\u6784\u7684\u5bbd\u5ea6\u5728\u6cbf\u7740\u540c\u5fc3\u5706\u72b6\u6beb\u7c73\u7ea7\u5b8f\u89c2\u65b9\u5411\u9010\u6e10\u589e\u52a0\uff0c\u8868\u660e\u4e86\u9010\u6e10\u589e\u5927\u7684\u6c14\u6ce1\u4f53\u79ef\u3002\u540c\u5fc3\u5706\u5b8f\u89c2\u7ed3\u6784\u7684\u5c3a\u5bf8\u6bd4\u5c3e\u72b6\u7ed3\u6784\u5927\uff0c\u76f4\u5f84\u53ef\u8fbe660\u5fae\u7c73\u3002\u6709\u4e9b\u5c3e\u72b6\u7ed3\u6784\u7f3a\u5931\u540c\u5fc3\u5706\u7ed3\u6784\u662f\u7531\u4e8e\u6c14\u6ce1\u7684\u968f\u673a\u7834\u88c2\u884c\u4e3a\u3002<\/p>\n<p><strong>\u5c3e\u72b6\u5b8f\u89c2\u7ed3\u6784\u8868\u5f81<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199487\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f74-\u6587\u4e2d\u56fe4.jpg\" alt=\"\" width=\"1270\" height=\"853\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f74-\u6587\u4e2d\u56fe4.jpg 1270w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f74-\u6587\u4e2d\u56fe4-300x201.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f74-\u6587\u4e2d\u56fe4-768x516.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f74-\u6587\u4e2d\u56fe4-1024x688.jpg 1024w\" sizes=\"(max-width: 1270px) 100vw, 1270px\" \/><\/p>\n<p>\u56fe4 \u5c3e\u72b6\u7ed3\u6784\u7684\u8be6\u7ec6SEM\u8868\u5f81\uff0c\uff08a-l\uff0990\u00b0\u5782\u76f4\u4fef\u89c6\u56fe\uff08m-o\uff0940\u00b0\u503e\u659c\u89c2\u6d4b\u3002\uff08a-o\uff09\u6807\u5c3a\u4e3a50, 20, 4, 0.5, 0.5, 0.5, 20, 20, 4, 0.5, 4, 0.5, 50, 20 \u548c20 \u03bcm\u3002<\/p>\n<p>\u56fe4\u5bf9\u5c3e\u72b6\u7ed3\u6784\u8fdb\u884c\u4e86\u7ec6\u5316\u8868\u5f81\uff0c\u53ef\u89c1\u5c3e\u72b6\u5b8f\u89c2\u7ed3\u6784\u662f\u7531\u5c42\u72b6\u6247\u5f62\u5fae\u7c73\u7ed3\u6784\u6784\u6210\uff08\u56fe4a\uff09\uff0c\u6247\u5f62\u4e2d\u5fc3\u89d2\u4e3a45-141\u00b0\u3002\u5728\u5fae\u7ed3\u6784\u4e0a\u8fd8\u9576\u5d4c\u7740\u9ad8\u9891\u5468\u671f\u7eb3\u7c73\u7ed3\u6784\uff08\u5468\u671f100-200nm\uff09\uff08\u56fe4b-l\uff09\u3002\u5c42\u72b6\u6247\u5f62\u5fae\u7ed3\u6784\u662f\u7531\u4e8e\u5728\u201c\u5f13\u201d\u5b57\u578b\u626b\u63cf\u8fc7\u7a0b\u4e2d\u52a8\u6001\u6c14\u6ce1\u6240\u5f15\u8d77\u7684\u6247\u5f62\u884d\u5c04\u5bfc\u81f4\u7684\uff0c\u6bcf\u4e00\u5c42\u5bf9\u5e94\u4e00\u6b21\u626b\u63cf\u3002\u5728\u5782\u76f4\u89c2\u6d4b\u6837\u54c1\u65f6\uff0c\u53ef\u4ee5\u770b\u5230\u6bcf\u5c42\u6247\u5f62\u7ed3\u6784\u5b9e\u9645\u4e0a\u662f\u8bb8\u591a\u7684\u6761\u72b6\u6c9f\u69fd\u75d5\u8ff9\uff0c\u6c9f\u69fd\u7684\u7ec8\u7aef\u88ab\u4e0a\u5c42\u7ed3\u6784\u906e\u853d\u3002\u4ece\u800c\u53ef\u4ee5\u786e\u5b9a\u6fc0\u5149\u4e0d\u518d\u662f\u5782\u76f4\u5165\u5c04\u800c\u662f\u503e\u659c\u5165\u5c04\u3002\u901a\u8fc7\u65cb\u8f6c\u89c2\u6d4b\u89d2\u5ea6\u4f7f\u6247\u5f62\u7ed3\u6784\u5e73\u884c\u4e8e\u89c2\u6d4b\u89d2\u5ea6\uff08\u56fe4m-o\uff09\uff0c\u4ece\u800c\u786e\u5b9a\u4e86\u884d\u5c04\u5bfc\u81f4\u4e86\u5165\u5c04\u5149\u226550\u00b0\u65b9\u5411\u504f\u8f6c\u3002\u56fe5\u4ece\u4e0d\u540c\u89c6\u89d2\u5c55\u793a\u4e86\u52a8\u6001\u6c14\u6ce1\u6247\u5f62\u884d\u5c04\u52a0\u5de5\u539f\u7406\u793a\u610f\u56fe\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199488\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f75-\u6587\u4e2d\u56fe5.jpg\" alt=\"\" width=\"1087\" height=\"419\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f75-\u6587\u4e2d\u56fe5.jpg 1087w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f75-\u6587\u4e2d\u56fe5-300x116.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f75-\u6587\u4e2d\u56fe5-768x296.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f75-\u6587\u4e2d\u56fe5-1024x395.jpg 1024w\" sizes=\"(max-width: 1087px) 100vw, 1087px\" \/><\/p>\n<p>\u56fe5 \u52a8\u6001\u6c14\u6ce1\u6247\u5f62\u884d\u5c04\u52a0\u5de5\u7684\u793a\u610f\u56fe<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199489\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f76-\u6587\u4e2d\u56fe6.jpg\" alt=\"\" width=\"1270\" height=\"636\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f76-\u6587\u4e2d\u56fe6.jpg 1270w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f76-\u6587\u4e2d\u56fe6-300x150.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f76-\u6587\u4e2d\u56fe6-768x385.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f76-\u6587\u4e2d\u56fe6-1024x513.jpg 1024w\" sizes=\"(max-width: 1270px) 100vw, 1270px\" \/><\/p>\n<p>\u56fe6 \u9759\u6001\u6c14\u6ce1\u8f85\u52a9\u52a0\u5de5\u5f62\u6210\u7684\u540c\u5fc3\u5706\u5b8f\u89c2\u7ed3\u6784\u7684\u5fae\u89c2\u8868\u5f81\u3002\uff08\u6fc0\u5149\u53c2\u6570\uff1a \u6ce2\u957f1030nm\uff0c \u91cd\u590d\u9891\u7387200kHz\uff0c\u8109\u5bbd223fs\uff0c\u6fc0\u5149\u80fd\u91cf100mW\uff0c\u8109\u51b2\u80fd\u91cf0.5\u03bcJ\uff0c\u626b\u63cf\u901f\u5ea61mm\/s\uff0c\u626b\u63cf\u7ebf\u95f4\u96945\u03bcm\uff09\u3002(a-l) \u6807\u5c3a\u4e3a50, 1 (\u5185\u90e8\u865a\u7ebf\u533a\u57df)\/10, 3, 0.5, 5, 0.5, 10, 1, 0.4, 1, 0.4, \u548c0.4 \u03bcm\u3002<\/p>\n<p>\u56fe6\u548c\u56fe7\u5bf9\u540c\u5fc3\u5706\u5b8f\u89c2\u7ed3\u6784\u7684\u4e0d\u540c\u4f4d\u7f6e\u8fdb\u884c\u4e86\u8be6\u7ec6SEM\u8868\u5f81\uff0c\u53ef\u4ee5\u786e\u5b9a\u4f4e\u9891\uff08LSFL\uff09\/\u9ad8\u9891(HSFL)\u548c\u8d85\u9ad8\u9891(UHSFL)\u5468\u671f\u6027\u7ed3\u6784\u7684\u5f62\u6210\uff0c\u660e\u663e\u4e0d\u540c\u4e8e\u5c3e\u72b6\u5b8f\u89c2\u7ed3\u6784\u3002\u4f4e\u9891\uff0c\u9ad8\u9891\u548c\u8d85\u9ad8\u9891\u5468\u671f\u7eb3\u7c73\u7ed3\u6784\u7684\u5468\u671f\u5206\u522b\u4e3a550\u2013900, 100\u2013200, 40\u2013100 nm\u300240nm\u5468\u671f\uff0c\u5c0f\u4e8e1030nm\u6fc0\u5149\u6ce2\u957f\u76841\/25\uff0c\u662f\u76ee\u524d\u5728\u7845\u4e0a\u53ef\u5236\u5907\u7684\u6700\u5c0f\u8868\u9762\u6fc0\u5149\u8bf1\u5bfc\u5468\u671f\u7ed3\u6784\u3002\u884d\u5c04\u52a0\u5de5\u5728\u9759\u6001\u5927\u6c14\u6ce1\u7684\u4e0b\u9762\u4f1a\u5f62\u6210\u8bb8\u591a\u5c0f\u7684\u6301\u4e45\u6c14\u6ce1\uff0c\u8fd9\u4e9b\u5c0f\u6c14\u6ce1\u4f1a\u5bf9\u5927\u6c14\u6ce1\u884d\u5c04\u6fc0\u5149\u5f62\u6210\u4e8c\u6b21\u8c03\u5236\uff0c\u5728\u5c0f\u6c14\u6ce1\u7684\u8fb9\u7f18\u4f1a\u5f62\u6210\u8d85\u9ad8\u5468\u671f\u7eb3\u7c73\u7ed3\u6784\u3002\u76f8\u90bb\u5c0f\u6c14\u6ce1\u5bf9\u6fc0\u5149\u7684\u5927\u9762\u79ef\u8c03\u5236\u6216\u5c0f\u6c14\u6ce1\u7684\u79fb\u52a8\u548c\u7834\u88c2\u5bfc\u81f4\u4e86\u5927\u9762\u79ef\u7684\u8d85\u9ad8\u9891\u5468\u671f\u7ed3\u6784\u7684\u5f62\u6210\u3002\u6240\u4ee5\u8d85\u9ad8\u9891\u548c\u9ad8\u9891\u7ed3\u6784\u6761\u5e26\u72b6\u4f1a\u4ea4\u66ff\u51fa\u73b0\u3002\u6709\u4e9b\u5c0f\u6c14\u6ce1\u4e00\u76f4\u6ca1\u6709\u7834\u88c2\uff0c\u5176\u4e2d\u88f9\u7740\u7684\u7eb3\u7c73\u6750\u6599\u4f1a\u6c89\u79ef\u5230\u6c14\u6ce1\u5e95\u90e8\uff0c\u5305\u62ec\u5927\u91cf\u7684\u76f4\u5f84\u51e0\u7eb3\u7c73\u7684\u7eb3\u7c73\u5c0f\u9897\u7c92\u548c\u5c11\u91cf\u5c3a\u5bf8\u4e3a\u51e0\u767e\u7eb3\u7c73\u7684\u7403\u5f62\u5927\u9897\u7c92\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199490\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f77-\u6587\u4e2d\u56fe7.jpg\" alt=\"\" width=\"1270\" height=\"1420\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f77-\u6587\u4e2d\u56fe7.jpg 1270w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f77-\u6587\u4e2d\u56fe7-268x300.jpg 268w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f77-\u6587\u4e2d\u56fe7-768x859.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f77-\u6587\u4e2d\u56fe7-916x1024.jpg 916w\" sizes=\"(max-width: 1270px) 100vw, 1270px\" \/><\/p>\n<p>\u56fe7\u9759\u6001\u6c14\u6ce1\u5f62\u6210\u7684\u540c\u5fc3\u5706\u5b8f\u89c2\u7ed3\u6784\u7684\u5fae\u7eb3\u7ed3\u6784\u8868\u5f81\uff08\u6fc0\u5149\u53c2\u6570\uff1a \u6ce2\u957f1030nm\uff0c \u91cd\u590d\u9891\u7387200kHz\uff0c\u8109\u5bbd223fs\uff0c\u6fc0\u5149\u80fd\u91cf100mW\uff0c\u8109\u51b2\u80fd\u91cf0.5\u03bcJ\uff0c\u626b\u63cf\u901f\u5ea61mm\/s\uff0c\u626b\u63cf\u7ebf\u95f4\u96945\u03bcm\uff09\u3002\uff08a-m\uff09\u6807\u5c3a\u4e3a20, 5, 1, 1, 0.4, 0.4, 2, 10, 1, 0.4, 0.4, 1\u548c0.3 \u03bcm\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199491\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f78-\u6587\u4e2d\u56fe8.jpg\" alt=\"\" width=\"1268\" height=\"404\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f78-\u6587\u4e2d\u56fe8.jpg 1268w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f78-\u6587\u4e2d\u56fe8-300x96.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f78-\u6587\u4e2d\u56fe8-768x245.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f78-\u6587\u4e2d\u56fe8-1024x326.jpg 1024w\" sizes=\"(max-width: 1268px) 100vw, 1268px\" \/><\/p>\n<p>\u56fe8\u4e0d\u540c\u626b\u63cf\u901f\u5ea6\u4e0b\u6c34\u4e0b\u6c14\u6ce1\u8f85\u52a9\u98de\u79d2\u6fc0\u5149\u52a0\u5de5\u7684\u5b8f\u89c2\u7ed3\u6784\u3002\uff08a-c\uff09\u626b\u63cf\u901f\u5ea6\u5206\u522b\u4e3a1\uff0c0.5\u548c0.1mm\/s\u3002\uff08\u6fc0\u5149\u53c2\u6570\uff1a \u6ce2\u957f1030nm\uff0c \u91cd\u590d\u9891\u7387200kHz\uff0c\u8109\u5bbd223fs\uff0c\u6fc0\u5149\u80fd\u91cf100mW\uff0c\u8109\u51b2\u80fd\u91cf0.5\u03bcJ\uff0c\u626b\u63cf\u901f\u5ea61mm\/s\uff0c\u626b\u63cf\u7ebf\u95f4\u969410\u03bcm\uff09\u3002\uff08a-c\uff09\u6807\u5c3a\u4e3a1mm\u3002<\/p>\n<p>\u5728\u8bbe\u5b9a\u626b\u63cf\u7ebf\u95f4\u8ddd\u4e3a10\u5fae\u7c73\u7684\u60c5\u51b5\u4e0b\uff0c\u6539\u53d8\u626b\u63cf\u901f\u5ea6\u53ef\u4ee5\u8c03\u63a7\u5c3e\u90e8\u5b8f\u89c2\u7ed3\u6784\u7684\u5c3a\u5bf8\uff0c1mm\/s\u5feb\u901f\u626b\u63cf\u80fd\u4ea7\u751f\u8fd12mm\u957f\u7684\u5c3e\u72b6\u5b8f\u89c2\u7ed3\u6784\uff0c\u800c0.1mm\/s\u7684\u626b\u63cf\u51e0\u4e4e\u4e0d\u80fd\u4ea7\u751f\u5c3e\u72b6\u5b8f\u89c2\u7ed3\u6784\uff0c\u8fd9\u8bf4\u660e\u6c14\u6ce1\u7684\u63a5\u89e6\u7ebf\u79fb\u52a8\u901f\u5ea6\u548c\u957f\u5ea6\u51b3\u5b9a\u4e86\u6c14\u6ce1\u7684\u79fb\u52a8\u6027\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199492\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f79-\u6587\u4e2d\u56fe9.jpg\" alt=\"\" width=\"1270\" height=\"847\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f79-\u6587\u4e2d\u56fe9.jpg 1270w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f79-\u6587\u4e2d\u56fe9-300x200.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f79-\u6587\u4e2d\u56fe9-768x512.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f79-\u6587\u4e2d\u56fe9-1024x683.jpg 1024w\" sizes=\"(max-width: 1270px) 100vw, 1270px\" \/><\/p>\n<p>\u56fe9\u4e0d\u540c\u6761\u4ef6\u4e0b\u751f\u6210\u7684\u5c42\u72b6\u6247\u5f62\u7ed3\u6784\u8868\u5f81\u3002\uff08\u6fc0\u5149\u53c2\u6570\uff1a \u6ce2\u957f1030nm\uff0c \u91cd\u590d\u9891\u7387200kHz\uff0c\u8109\u5bbd223fs\uff0c\u6fc0\u5149\u80fd\u91cf100mW\uff0c\u8109\u51b2\u80fd\u91cf0.5\u03bcJ\uff0c\u626b\u63cf\u901f\u5ea61mm\/s\uff0c\u626b\u63cf\u7ebf\u95f4\u969410\u03bcm\uff09\u3002\uff08a-o\uff09\u6807\u5c3a\u4e3a50, 10, 10, 0.5, 10, 10, 0.5, 10, 10, 0.5, 4, 0.5, 50, 20\u548c 20\u03bcm\u3002<\/p>\n<p>\u56fe9\u5c55\u793a\u4e86\u4e0d\u540c\u52a0\u5de5\u6761\u4ef6\u4e0b\u5f62\u6210\u7684\u5c42\u72b6\u6247\u5f62\u5fae\u7eb3\u7c73\u7ed3\u6784\uff08\u626b\u63cf\u95f4\u9694\u4e3a10\u5fae\u7c73\u626b\u63cf\u901f\u5ea6\u4e3a1mm\/s\uff09\uff0c\u53ef\u4ee5\u770b\u51fa\u6b64\u7ed3\u6784\u548c\u56fe4\uff08\u626b\u63cf\u95f4\u9694\u4e3a5\u5fae\u7c73\u626b\u63cf\u901f\u5ea6\u4e3a1mm\/s\uff09\u7ed3\u6784\u660e\u663e\u4e0d\u540c\uff0c\u8868\u660e\u901a\u8fc7\u8c03\u8282\u626b\u63cf\u95f4\u9694\u53ef\u4ee5\u8c03\u8282\u5c42\u72b6\u6247\u5f62\u7ed3\u6784\uff08\u5c3e\u72b6\u5b8f\u89c2\u7ed3\u6784\uff09\u7684\u5f62\u8c8c\u3002\u56fe10\u5bf9\u6bd4\u4e86\u4e24\u79cd\u7ed3\u6784\u5728\u7279\u5b9a\u533a\u57df\u7684\u5149\u5b66\u7279\u6027\uff0c\u53ef\u4ee5\u770b\u51fa\u4e24\u79cd\u7ed3\u6784\u5728\u5149\u5b66\u663e\u5fae\u955c\u4e0b\u90fd\u5448\u73b0\u9ed1\u8272\uff08\u56fe10a\uff0cd\uff09\uff0c\u8868\u660e\u5c42\u72b6\u6247\u5f62\u7ed3\u6784\u53ef\u4ee5\u7eb3\u5165\u9ed1\u7845\u7684\u8303\u7574\u3002\u9ed1\u7845\u901a\u5e38\u90fd\u5177\u6709\u5f88\u597d\u7684\u6297\u53cd\u5c04\u7279\u6027\u3002\u6240\u4ee5\u4f5c\u8005\u5229\u7528FITR\u5149\u8c31\u4eea\u5bf9\u4e24\u79cd\u5c42\u72b6\u6247\u5f62\u7ed3\u6784\u5728\u8fd1\u7ea2\u5916\u548c\u4e2d\u7ea2\u5916\u533a\u57df\u7684\u900f\u5c04\u548c\u53cd\u5c04\u7279\u6027\u8fdb\u884c\u4e86\u6bd4\u8f83\u5206\u6790\u3002\u53ef\u4ee5\u770b\u51fa5\u5fae\u7c73\u626b\u63cf\u95f4\u9694\u7684\u6761\u4ef6\u4e0b\u5f62\u6210\u7684\u5c42\u72b6\u6247\u5f62\u7ed3\u6784\u8868\u9762\u7684\u9ad8\u9891\u7eb3\u7c73\u5468\u671f\u7ed3\u6784\u66f4\u7d27\u5bc6\uff0c\u800c\u4e14\u5c42\u72b6\u6247\u5f62\u7ed3\u6784\u5bc6\u5ea6\u66f4\u9ad8\uff085\u5fae\u7c73\u626b\u63cf\u95f4\u9694\uff0c\u56fe10b-c\uff0c10j-k vs \u56fe10e-f\uff0c10l-m, 10\u5fae\u7c73\u626b\u63cf\u95f4\u9694\uff09\uff0c\u6240\u4ee5\u65e0\u8bba\u662f\u900f\u5c04\u7387\u8fd8\u662f\u53cd\u5c04\u7387\u90fd\u6bd410\u5fae\u7c73\u626b\u63cf\u95f4\u9694\u6761\u4ef6\u4e0b\u7684\u5f62\u6210\u7684\u7ed3\u6784\u66f4\u4f4e\uff08\u56fe10g\uff09\u3002\u7531\u4e8e\u5c42\u72b6\u6247\u5f62\u7ed3\u5728\u6b63\u4ea4\u65b9\u5411\u7684\u7ed3\u6784\u5dee\u5f02\u6027\uff0c\u6b64\u79cd\u7ed3\u6784\u5728X\u548cY\u65b9\u5411\u8fd8\u5c55\u73b0\u4e86\u504f\u632f\u5149\u5149\u5b66\u53cd\u5c04\uff08\u56fe10h\uff09\u548c\u900f\u5c04\uff08\u56fe10i\uff09\u5404\u5f02\u6027\u3002\u5728\u9759\u6001\u6c14\u6ce1\u8f85\u52a9\u6fc0\u5149\u52a0\u5de5\u7684\u533a\u57df\u53c8\u9996\u6b21\u53d1\u73b0\u4e86\u65b0\u9896\u7684\u4f4e\/\u9ad8\/\u8d85\u9ad8\u4ea4\u53e0\u7684\u590d\u5408\u7ed3\u6784\uff08\u56fe11\uff09\uff0c\u8fd9\u79cd\u7ed3\u6784\u7684\u5f62\u6210\u662f\u7531\u4e8e\u6c14\u6ce1\u5185\u58c1\u7684\u591a\u6b21\u53cd\u5c04\u7684\u5149\u548c\u6298\u5c04\u5149\u91cd\u590d\u4f5c\u7528\u5728\u540c\u4e00\u4e2a\u533a\u57df\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199493\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f710-\u6587\u4e2d\u56fe10.jpg\" alt=\"\" width=\"1220\" height=\"944\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f710-\u6587\u4e2d\u56fe10.jpg 1220w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f710-\u6587\u4e2d\u56fe10-300x232.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f710-\u6587\u4e2d\u56fe10-768x594.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f710-\u6587\u4e2d\u56fe10-1024x792.jpg 1024w\" sizes=\"(max-width: 1220px) 100vw, 1220px\" \/><\/p>\n<p>\u56fe10 \u4e0d\u540c\u5c42\u72b6\u6247\u5f62\u7ed3\u6784\u7684\u5149\u5b66\u7279\u6027\u5bf9\u6bd4\u548c\u7ed3\u6784\u5206\u6790\u3002\uff08a-c\uff0cj-k\uff09\u626b\u63cf\u95f4\u9694\u4e3a5\u03bcm\u3002\uff08d-f\uff0cl-m\uff09\u626b\u63cf\u95f4\u9694\u4e3a10\u03bcm\u3002\u6807\u5c3a\uff1a\uff08a\uff0cb\uff0cd\uff0ce\uff09\u6807\u5c3a\u76f8\u540c\u4e3a500\u03bcm, (c\uff0cf) 50\u03bcm, (j\uff0cl) 5\u03bcm and (k\uff0cm) 1\u03bcm\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199494\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f711-\u6587\u4e2d\u56fe11.jpg\" alt=\"\" width=\"761\" height=\"508\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f711-\u6587\u4e2d\u56fe11.jpg 761w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f711-\u6587\u4e2d\u56fe11-300x200.jpg 300w\" sizes=\"(max-width: 761px) 100vw, 761px\" \/><\/p>\n<p>\u56fe11 \u590d\u5408\u4f4e\/\u9ad8\/\u8d85\u9ad8\u5468\u671f\u6027\u7eb3\u7c73\u7ed3\u6784\u3002\uff08a-d\uff09\u6807\u5c3a5, 1, 3 and 1 \u03bcm\u3002<\/p>\n<p><strong>\u3010\u5e94\u7528\u4e0e\u5c55\u671b\u3011<\/strong><\/p>\n<p>\u6b64\u5de5\u4f5c\u8868\u660e\u6c14\u6ce1\u662f\u4e00\u79cd\u5b8c\u7f8e\u7684\u63a9\u6a21\u7248\uff0c\u53ef\u4ee5\u8f85\u52a9\u6fc0\u5149\u52a0\u5de5\u5f62\u6210\u72ec\u7279\u7684\u6beb\u7c73\u5fae\u7c73\u7eb3\u7c73\u591a\u5c3a\u5ea6\u590d\u5408\u7ed3\u6784\u3002\u5927\u9762\u79ef40-100nm\u8d85\u9ad8\u5468\u671f\u7eb3\u7c73\u5468\u671f\u7ed3\u6784\u5236\u5907\u8868\u660e\u6c14\u6ce1\u53ef\u4ee5\u8c03\u8282\u6fc0\u5149\u7684\u591a\u79cd\u7279\u6027\u5982\u5165\u5c04\u89d2\u5ea6\uff0c\u6fc0\u5149\u80fd\u91cf\uff0c\u6fc0\u5149\u91cd\u590d\u9891\u7387\u548c\u5149\u6591\u5c3a\u5bf8\uff0c\u5c55\u73b0\u51fa\u4e86\u4f20\u7edf\u5149\u5b66\u5668\u4ef6\u96be\u4ee5\u8fbe\u5230\u7684\u8c03\u63a7\u80fd\u529b\u3002\u4f46\u662f\u5149\u4e0e\u6c14\u6ce1\u4f5c\u7528\u8fc7\u7a0b\u6781\u5176\u590d\u6742\uff0c\u4e9f\u9700\u540e\u7eed\u7814\u7a76\u9610\u91ca\u8fc7\u7a0b\u548c\u673a\u7406\u3002\u6c14\u6ce1\u7684\u6301\u4e45\u6027\uff0c\u8010\u7834\u574f\u6027\u548c\u79fb\u52a8\u7279\u6027\u4e5f\u51b3\u5b9a\u4e86\u6700\u540e\u7684\u7ed3\u6784\u7279\u6027\u3002\u867d\u7136\u52a0\u5de5\u8fc7\u7a0b\u5f88\u96be\u63a7\u5236\uff0c\u8fd9\u79cd\u5de5\u827a\u65e0\u8bba\u5728\u5236\u9020\u65b9\u6cd5\u5b66\u8fd8\u662f\u7ed3\u6784\u591a\u6837\u6027\u90fd\u5c55\u73b0\u4e86\u72ec\u7279\u7684\u4f18\u52bf\uff0c\u4e3a\u6781\u7aef\u6761\u4ef6\u4e0b\u7684\u52a0\u5de5\u63d0\u4f9b\u4e86\u66f4\u591a\u53ef\u80fd\u6027\u3002<\/p>\n<p><strong>\u539f\u6587\u94fe\u63a5<\/strong>\uff1a<a href=\"https:\/\/doi.org\/10.1088\/2631-7990\/ab729f\">https:\/\/doi.org\/10.1088\/2631-7990\/ab729f<\/a>. Zhang D S, Ranjan B, Tanaka T, Sugioka K. Underwater persistent bubble-assisted femtosecond laser ablation for hierarchical micro\/nanostructuring. <em>Int. J. Extrem. Manuf<\/em>. <strong>2<\/strong>, 015001 (2020).<\/p>\n<p><strong>\u3010\u4f5c\u8005\u7b80\u4ecb\u3011<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199495\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f712-\u4f5c\u8005-Koji-Sugioka.jpg\" alt=\"\" width=\"195\" height=\"260\" \/><\/p>\n<p>\u6749\u5188\u5e78\u6b21 (Koji Sugioka)\u6559\u6388\u4e3a\u65e5\u672c\u7406\u5316\u5b66\u7814\u7a76\u6240\u5148\u8fdb\u5149\u5b50\u4e2d\u5fc3\u8054\u5408\u7814\u7a76\u90e8\u95e8\u7684\u8d1f\u8d23\u4eba\uff0c\u5148\u540e\u62c5\u4efb\u4e1c\u4eac\u7535\u673a\u5927\u5b66\u3001\u4e1c\u4eac\u7406\u79d1\u5927\u5b66\u3001\u4eac\u90fd\u5927\u5b66\u5ba2\u5ea7\u6559\u6388\uff1b\u4f5c\u4e3a\u521b\u59cb\u4eba\uff0c\u53d1\u8d77\u6fc0\u5149\u7cbe\u5bc6\u5fae\u7ec6\u52a0\u5de5\u56fd\u9645\u7814\u8ba8\u4f1a(International Symposium on Laser Precision Microfabrication, LPM)\uff0c\u5e76\u62c5\u4efb\u7f8e\u56fd\u6fc0\u5149\u5b66\u4f1a\uff08LIA\uff09\u3001\u65e5\u672c\u6fc0\u5149\u52a0\u5de5\u5b66\u4f1a(JLPS)\u548c\u65e5\u672c\u6fc0\u5149\u6280\u672f\u5b66\u4f1a\uff08JLST\uff09\u7406\u4e8b\u4f1a\u6210\u5458\uff0c\u56fd\u9645\u5149\u7535\u5b50\u4e0e\u6fc0\u5149\u5de5\u7a0b\u5b66\u4f1a\uff08IAPLE\uff09\u7406\u4e8b\u4f1a\u59d4\u5458\uff0cSPIE\u3001OSA\u548cIAPLE\u4f1a\u5458\u3002Koji Sugioka\u6559\u6388\u4f5c\u4e3a\u8d85\u5feb\u6fc0\u5149\u52a0\u5de5\u6280\u672f\u7684\u9886\u519b\u4eba\u7269\uff0c\u5728\u6fc0\u5149\u63ba\u6742\u3001\u6fc0\u5149\u523b\u8680\u3001\u6fc0\u5149\u8868\u9762\u6539\u6027\u3001\u6fc0\u5149\u8bf1\u5bfc\u9009\u62e9\u6027\u91d1\u5c5e\u5316\u3001\u900f\u660e\u6750\u6599\u5fae\u7ec6\u52a0\u5de5\u3001\u771f\u7a7a\u7d2b\u5916\u6fc0\u5149\u52a0\u5de5\u3001\u6fc0\u5149\u8868\u9762\u7eb3\u7c73\u7ed3\u6784\u548c\u4e09\u7ef4\u5fae\/\u7eb3\u52a0\u5de5\u7b49\u9886\u57df\u4eab\u8a89\u56fd\u9645\u3002\u8fd1\u5e74\u6765\uff0c\u5728Light: Science &amp; Applications, Applied physics reviews\u7b49\u56fd\u9645\u77e5\u540d\u671f\u520a\u4e0a\uff0c\u53d1\u8868\u8bba\u6587200\u591a\u7bc7\uff0c\u5176\u4e2d20\u7bc7\u4e3a\u7279\u9080\u8bba\u6587\uff1b\u62c5\u4efbJournal of the Laser Micro\/Nanoengineering (JLMN)\u4e3b\u7f16\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199496\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f713-\u4f5c\u8005-\u5f20\u4e1c\u77f3.jpg\" alt=\"\" width=\"223\" height=\"298\" \/><\/p>\n<p>\u5f20\u4e1c\u77f3\u535a\u58eb\u4e8e2014\u5e74\u4e8e\u897f\u5b89\u4ea4\u901a\u5927\u5b66\u83b7\u5f97\u535a\u58eb\u5b66\u4f4d\uff0c\u968f\u540e\u52a0\u5165\u5fb7\u56fd\u57c3\u68ee-\u675c\u4f0a\u65af\u5821\u5927\u5b66\u5de5\u4e1a\u5316\u5b66\u7cfbProf. Stephan Barcikowski\u8bfe\u9898\u7ec4\u8fdb\u884c\u535a\u58eb\u540e\u7814\u7a76\uff0c\u4e4b\u540e\u5728\u5408\u80a5\u4e2d\u79d1\u9662\u56fa\u4f53\u7269\u7406\u6240\u6881\u957f\u6d69\u6559\u6388\u8bfe\u9898\u7ec4\u505a\u6570\u6708\u8bbf\u95ee\u7814\u7a76\uff0c\u5e76\u4e8e2017\u5e74\u52a0\u5165\u65e5\u672c\u7406\u5316\u5b66\u7814\u7a76\u6240Prof. Koji Sugioka\u56e2\u961f\u7ee7\u7eed\u6df1\u9020\uff0c\u76ee\u524d\u7684\u7814\u7a76\u8bfe\u9898\u4e3a\u7eb3\u7c73\u6750\u6599\u548c\u7eb3\u7c73\u7ed3\u6784\u7684\u5236\u5907\uff0c\u8c03\u63a7\u548c\u5e94\u7528\u3002\u8fd1\u5e74\u6765\u5728Chemical Reviews \uff08\u9ad8\u88ab\u5f15\u6587\u7ae0\uff09\uff0cACS Applied Nano Materials\uff0cNanomaterials\u53d1\u8868\u591a\u7bc7\u6587\u7ae0\uff0c\u603b\u5f15\u7528\u4e00\u5343\u4f59\u6b21\uff0cH-index\u662f21\u3002<\/p>\n<p><strong>\u3010\u53c2\u8003\u6587\u732e\u3011<\/strong><\/p>\n<p>\u30101\u3011Zhang D, G\u00f6kce B, Sommer S, Streubel R, Barcikowski S. Debris-free rear-side picosecond laser ablation of thin germanium wafers in water with ethanol. Appl. Surf. Sci. 367, 222-230 (2016)<\/p>\n<p>\u30102\u3011Barcikowski S, Men\u00e9ndez-Manj\u00f3n A, Chichkov B, Brikas M, Ra\u010diukaitis G. Generation of nanoparticle colloids by picosecond and femtosecond laser ablations in liquid flow. Appl. Phys. Lett. 91, 083113 (2007)<\/p>\n<p>\u30103\u3011Zhang D, Koji S. Hierarchical microstructures with high spatial frequency laser induced periodic surface structures possessing different orientations created by femtosecond laser ablation of silicon in liquids. Opto-Electron. Adv. 2, 190002 (2019).<\/p>\n<p><strong>\u300a\u6781\u7aef\u5236\u9020\u300b\u671f\u520a\u7b80\u4ecb<\/strong><\/p>\n<p>\u300a<strong>\u6781\u7aef\u5236\u9020<\/strong>\u300b\u671f\u520a\uff08<strong><em>International Journal of Extreme Manufacturing<\/em><\/strong><strong>, IJEM<\/strong><strong>\uff09\uff0c<\/strong>\u83b7\u4e2d\u56fd\u79d1\u6280\u671f\u520a\u56fd\u9645\u5f71\u54cd\u529b\u63d0\u5347\u8ba1\u5212D\u7c7b\u9879\u76ee\u8d44\u52a9\uff0c\u81f4\u529b\u4e8e\u53d1\u8868\u6781\u7aef\u6761\u4ef6\u4e0b\u5236\u9020\u53ca\u76f8\u5173\u9886\u57df\u7684\u9ad8\u8d28\u91cf\u6700\u65b0\u7814\u7a76\u6210\u679c\uff0c\u6587\u7ae0\u5f62\u5f0f\u4e3b\u8981\u4e3a\u539f\u521b\u6027\u548c\u7efc\u8ff0\u6027\u6587\u7ae0\u3002\u76ee\u524d\u8be5\u520a\u5171\u8bbe\u4e94\u5927\u680f\u76ee\uff1a\u6781\u7aef\u5236\u9020\u80fd\u573a\u4e0e\u6750\u6599\u76f8\u4e92\u4f5c\u7528\u3001\u6781\u7aef\u5236\u9020\u52a0\u5de5\u6280\u672f\u4e0e\u7406\u8bba\u3001\u6781\u7aef\u5236\u9020\u6d4b\u91cf\u4e0e\u8868\u5f81\u3001\u6781\u7aef\u6027\u80fd\u88c5\u5907\u53ca\u7cfb\u7edf\u7684\u8bbe\u8ba1\u53ca\u7814\u53d1\u3001\u6781\u7aef\u7269\u7406\u6761\u4ef6\u4ea7\u751f\u88c5\u7f6e\u7684\u5236\u9020\u3002IJEM\u73b0\u5df2\u88abCNKI\u3001INSPEC\u3001DOAJ\u7b49\u6570\u636e\u5e93\u6536\u5f55\u3002<\/p>\n<ul>\n<li><strong>\u5f00\u6e90\uff08<\/strong><strong>OA<\/strong><strong>\uff09\u671f\u520a\uff0c\u514d\u8d39\u83b7\u53d6<\/strong><\/li>\n<li><strong>\u514d\u8d39\u4e13\u4e1a\u5316\u8bed\u8a00\u6da6\u8272<\/strong><\/li>\n<li><strong>\u514d\u8d39\u9ad8\u8d28\u91cf\u56fe\u7247\u7f16\u8f91<\/strong><\/li>\n<li><strong>\u514d\u8d39\u5168\u7403\u5316\u5ba3\u4f20\u63a8\u5e7f<img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-199497\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f714-\u6587\u4e2d\u6781\u7aef\u5236\u9020\u671f\u520a\u4e8c\u7ef4\u7801.jpg\" alt=\"\" width=\"405\" height=\"406\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f714-\u6587\u4e2d\u6781\u7aef\u5236\u9020\u671f\u520a\u4e8c\u7ef4\u7801.jpg 405w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f714-\u6587\u4e2d\u6781\u7aef\u5236\u9020\u671f\u520a\u4e8c\u7ef4\u7801-150x150.jpg 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/04\/IJEM\u5e8f\u53f714-\u6587\u4e2d\u6781\u7aef\u5236\u9020\u671f\u520a\u4e8c\u7ef4\u7801-300x300.jpg 300w\" sizes=\"(max-width: 405px) 100vw, 405px\" \/><\/strong><\/li>\n<\/ul>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u672c\u6587\u4eae\u70b9\u3011 \u56fe1. \u6c34\u4e0b\u6301\u4e45\u6c14\u6ce1\u8f85\u52a9\u98de\u79d2\u6fc0\u5149\u52a0\u5de5\u793a\u610f\u56fe\u548c\u5178\u578b\u7ed3\u6784 \u8fd1\u65e5\uff0c\u65e5\u672c\u7406\u5316\u5b66\u7814\u7a76\u6240\uff08RIKEN\uff09\u6749\u5188\u5e78\u6b21\u6559\u6388\u548c\u5f20\u4e1c\u77f3\u535a\u58eb\u5728\u300a\u6781\u7aef\u5236\u9020\u300b\u671f\u520a\uff08Intern&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-199481","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/199481"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=199481"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/199481\/revisions"}],"predecessor-version":[{"id":199542,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/199481\/revisions\/199542"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=199481"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=199481"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=199481"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}