{"id":205428,"date":"2020-07-17T06:46:51","date_gmt":"2020-07-16T22:46:51","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=205428"},"modified":"2020-07-16T22:47:25","modified_gmt":"2020-07-16T14:47:25","slug":"%e6%ad%a6%e5%a4%a7%e9%bb%84%e5%8d%ab%e5%8d%8eangew-chem-int-ed-%e7%bb%bc%e8%bf%b0%ef%bc%9a%e5%8f%af%e6%8b%89%e4%bc%b8%e7%94%b5%e5%8c%96%e5%ad%a6%e4%bc%a0%e6%84%9f%e5%99%a8%e7%94%a8%e4%ba%8e","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=205428","title":{"rendered":"\u6b66\u5927\u9ec4\u536b\u534eAngew. Chem. Int. Ed.\u7efc\u8ff0\uff1a\u53ef\u62c9\u4f38\u7535\u5316\u5b66\u4f20\u611f\u5668\u7528\u4e8e\u7ec6\u80de\u548c\u7ec4\u7ec7\u68c0\u6d4b"},"content":{"rendered":"<p><strong>\u3010\u80cc\u666f\u4ecb\u7ecd\u3011<\/strong><\/p>\n<p>\u4eba\u4f53\u5185\u7ec4\u7ec7\u5668\u5b98\u7684\u57fa\u672c\u751f\u7269\u5f62\u6001\u548c\u529f\u80fd\uff0c\u5982\u8840\u7ba1\u5185\u8840\u6db2\u6d41\u52a8\u3001\u80a0\u9053\u8815\u52a8\u548c\u80ba\u90e8\u547c\u5438\u8fd0\u52a8\uff0c\u90fd\u6d89\u53ca\u5230\u52a8\u6001\u673a\u68b0\u529b\u4e0e\u5e38\u9a7b\u7ec6\u80de\u4e4b\u95f4\u7684\u4e0d\u65ad\u53cd\u9988\u3002\u7ec6\u80de\u611f\u77e5\u673a\u68b0\u529b\uff08\u5982\u62c9\u4f38\u5f20\u529b\u3001\u526a\u5207\u529b\u3001\u5212\u75d5\u548c\u538b\u7f29\uff09\u5e76\u5c06\u5176\u8f6c\u5316\u4e3a\u751f\u5316\u53cd\u5e94\u7684\u590d\u6742\u8fc7\u7a0b\uff0c\u79f0\u4e3a\u673a\u68b0\u529b\u4fe1\u53f7\u8f6c\u5bfc\u3002\u5c3d\u7ba1\u673a\u68b0\u529b\u5bf9\u751f\u7269\u4f53\u529f\u80fd\u8d77\u7740\u91cd\u8981\u8c03\u8282\u4f5c\u7528\uff0c\u4f46\u76ee\u524d\u5bf9\u7ec6\u80de\u5c06\u673a\u68b0\u529b\u523a\u6fc0\u8f6c\u5316\u4e3a\u751f\u7269\u5316\u5b66\u4fe1\u606f\u7684\u673a\u5236\u4ecd\u77e5\u4e4b\u751a\u5c11\u3002\u56e0\u6b64\uff0c\u53d1\u5c55\u5b9e\u65f6\u68c0\u6d4b\u8be5\u8fc7\u7a0b\u751f\u5316\u4fe1\u53f7\u7684\u6280\u672f\uff0c\u5bf9\u63ed\u793a\u673a\u68b0\u529b\u4fe1\u53f7\u8f6c\u5bfc\u673a\u5236\u5341\u5206\u5173\u952e\u3002<\/p>\n<p>\u7535\u5316\u5b66\uff08EC\uff09\u65b9\u6cd5\u56e0\u5177\u6709\u7075\u654f\u5ea6\u9ad8\u3001\u54cd\u5e94\u901f\u5ea6\u5feb\u7b49\u4f18\u52bf\uff0c\u5df2\u6210\u4e3a\u7ec6\u80de\u548c\u7ec4\u7ec7\u4fe1\u53f7\u5206\u5b50\u5b9e\u65f6\u52a8\u6001\u76d1\u6d4b\u7684\u91cd\u8981\u6280\u672f\u4e4b\u4e00\u3002\u7136\u800c\uff0c\u4f20\u7edf\u7535\u5316\u5b66\u4f20\u611f\u5668\u4e3a\u521a\u6027\u786c\u8d28\u7535\u6781\uff0c\u7f3a\u4e4f\u5f39\u6027\uff0c\u65e0\u6cd5\u987a\u5e94\u7ec6\u80de\u548c\u7ec4\u7ec7\u5f62\u53d8\u3002\u8fd1\u5e74\u6765\uff0c\u968f\u7740\u6750\u6599\u548c\u5fae\u7eb3\u52a0\u5de5\u6280\u672f\u7684\u98de\u901f\u8fdb\u6b65\uff0c\u65b0\u5174\u67d4\u6027\u53ef\u62c9\u4f38\u7535\u5b50\u5668\u4ef6\u5f97\u5230\u4e86\u8fc5\u901f\u53d1\u5c55\uff0c\u5e76\u5728\u591a\u4e2a\u9886\u57df\uff08\u5c24\u5176\u662f\u53ef\u7a7f\u6234\u8bbe\u5907\uff09\u5c55\u793a\u4e86\u5de8\u5927\u7684\u5e94\u7528\u524d\u666f\u3002\u7136\u800c\uff0c\u6784\u5efa\u53ef\u62c9\u4f38EC\u4f20\u611f\u5668\u4ecd\u7136\u9762\u4e34\u4e25\u5cfb\u7684\u6311\u6218\uff1a\u4e00\u65b9\u9762\uff0c\u7535\u6781\u4f7f\u7528\u65f6\u76f4\u63a5\u66b4\u9732\u5728\u751f\u7269\u73af\u5883\u4e2d\uff0c\u4f20\u611f\u754c\u9762\u8981\u6c42\u5177\u5907\u826f\u597d\u7684\u751f\u7269\u76f8\u5bb9\u6027\u548c\u8010\u8150\u8680\u6027\uff1b\u53e6\u4e00\u65b9\u9762\uff0c\u4f53\u5185\u7ec6\u80de\u548c\u7ec4\u7ec7\u53d1\u751f\u673a\u68b0\u53d8\u5f62\u8f83\u5927\u4e14\u4ea7\u751f\u7684\u5316\u5b66\u4fe1\u53f7\u5fae\u5f31\uff0c\u76ee\u524d\u53d1\u5c55\u7684\u53ef\u7a7f\u6234\u5f0f\u4f20\u611f\u5668\u96be\u4ee5\u540c\u65f6\u6ee1\u8db3\u5927\u673a\u68b0\u53d8\u5f62\u548c\u9ad8\u7075\u654f\u5ea6\u7684\u9700\u6c42\u3002\u56e0\u6b64\uff0c\u76f4\u5230\u6700\u8fd1\u53ef\u62c9\u4f38\u7535\u5316\u5b66\u4f20\u611f\u5668\u624d\u5728\u7ec6\u80de\u548c\u7ec4\u7ec7\u5b9e\u65f6\u76d1\u6d4b\u65b9\u9762\u53d6\u5f97\u7a81\u7834\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u57fa\u4e8e\u6b64\uff0c<strong>\u6b66\u6c49\u5927\u5b66\u5218\u8273\u73b2\u535a\u58eb\u4e0e\u9ec4\u536b\u534e\u6559\u6388<\/strong>\u603b\u7ed3\u4e86\u5173\u4e8e\u53ef\u62c9\u4f38\u7535\u5316\u5b66\u4f20\u611f\u5668\u7528\u4e8e\u7ec6\u80de\u548c\u7ec4\u7ec7\u68c0\u6d4b\u65b9\u9762\u7684\u6700\u65b0\u7814\u7a76\u8fdb\u5c55\u3002\u4ee5\u201c<strong>Stretchable Electrochemical Sensors for Cell and Tissue Detection<\/strong>\u201d\u53d1\u8868\u4e8e<strong>Angew. Chem. Int. Ed.<\/strong>\u671f\u520a\u4e0a\u3002\u5728\u672c\u6587\u4e2d\uff0c\u4f5c\u8005\u9996\u5148\u603b\u7ed3\u4e86\u53ef\u62c9\u4f38\u7535\u6781\u7684\u5236\u5907\uff0c\u5e76\u7740\u91cd\u4ecb\u7ecd\u4e86\u57fa\u4e8e\u7eb3\u7c73\u6750\u6599\u7684\u7535\u6781\u5236\u5907\u7b56\u7565\u3002\u4e4b\u540e\uff0c\u4ecb\u7ecd\u4e86\u53ef\u62c9\u4f38\u4f20\u611f\u5668\u5728\u673a\u68b0\u654f\u611f\u6027\u7ec6\u80de\u548c\u7ec4\u7ec7\u5b9e\u65f6\u76d1\u6d4b\u4e2d\u7684\u4ee3\u8868\u6027\u5e94\u7528\u3002\u6700\u540e\uff0c\u4f5c\u8005\u5c55\u671b\u4e86\u53ef\u62c9\u4f38\u7535\u5316\u5b66\u4f20\u611f\u5728\u7ec6\u80de\u3001\u7ec4\u7ec7\u53ca\u6d3b\u4f53\u68c0\u6d4b\u4e2d\u7684\u5e94\u7528\u53ef\u80fd\u6027\u548c\u9762\u4e34\u7684\u6311\u6218\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u89e3\u8bfb\u3011<\/strong><\/p>\n<p><strong>1<\/strong><strong>\u3001\u5f15\u8a00<\/strong><\/p>\n<p><strong>2<\/strong><strong>\u3001\u53ef\u62c9\u4f38\u7535\u6781\u5236\u5907<\/strong><\/p>\n<p>\u5230\u76ee\u524d\u4e3a\u6b62\uff0c\u5df2\u7ecf\u53d1\u5c55\u4e86\u4e24\u79cd\u57fa\u672c\u7b56\u7565\u5236\u5907\u53ef\u62c9\u4f38\u7535\u6781\uff1a\u57fa\u4e8e\u7279\u6b8a\u51e0\u4f55\u7ed3\u6784\u57fa\u5e95\u548c\u57fa\u4e8e\u5bfc\u7535\u7eb3\u7c73\u6750\u6599\u81ea\u8eab\u6027\u8d28\u7684\u53ef\u62c9\u4f38\u6027\u3002<\/p>\n<p><strong>2.1<\/strong><strong>\u3001\u57fa\u4e8e\u7ed3\u6784\u7684\u53ef\u62c9\u4f38\u7535\u6781<\/strong><\/p>\n<p>\u4f20\u7edf\u7684\u5bfc\u7535\u6750\u6599\uff0c\u5982Au\u548cPt\uff0c\u7531\u4e8e\u5176\u56fa\u6709\u7684\u8106\u6027\u548c\u521a\u6027\uff0c\u4e0d\u9002\u5408\u7528\u4f5c\u53ef\u62c9\u4f38\u7535\u6781\u3002\u5c3d\u7ba1\u8db3\u591f\u8584\u7684\u8584\u819c\u7535\u6781\u56e0\u5176\u5f2f\u66f2\u521a\u5ea6\u964d\u4f4e\uff0c\u5177\u6709\u8f83\u597d\u7684\u67d4\u97e7\u6027\uff0c\u4f46\u5b83\u4eec\u7684\u65ad\u88c2\u5e94\u53d8\u6781\u9650\u901a\u5e38\u4f4e\u4e8e1%\uff0c\u8fdc\u8fdc\u4e0d\u80fd\u6ee1\u8db3\u751f\u7269\u8f6f\u7ec4\u7ec7\u7684\u8f83\u5927\u673a\u68b0\u5e94\u53d8\u3002\u4e3a\u4e86\u89e3\u51b3\u8fd9\u4e00\u95ee\u9898\uff0c\u4eba\u4eec\u5229\u7528\u5177\u6709\u7279\u5b9a\u51e0\u4f55\u7ed3\u6784\u7684\u57fa\u5e95\u5236\u4f5c\u4e86\u53ef\u62c9\u4f38\u7535\u6781\u3002<\/p>\n<p><strong>\u56fe\u4e00\u3001\u7528\u4e8e\u5236\u5907\u53ef\u62c9\u4f38\u7535\u6781\u7684\u5178\u578b\u51e0\u4f55\u7ed3\u6784<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-205429\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie1.jpg\" alt=\"\" width=\"600\" height=\"424\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie1-300x212.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\uff08a\uff09\u4e0d\u540c\u7ed3\u6784\u7684\u53ef\u62c9\u4f38\u539f\u7406\u793a\u610f\u56fe\uff1b<\/p>\n<p>\uff08b\uff09\u86c7\u7eb9\u72b6\u91d1\u7ed3\u6784\u7684\u5149\u5b66\u663e\u5fae\u7167\u7247\uff1b<\/p>\n<p>\uff08c\uff09\u91d1\u7eb3\u7c73\u7f51\uff08\u539a\u5ea650nm\uff09\u7535\u6781\u7684SEM\u56fe\uff1b<\/p>\n<p>\uff08d\uff09\u6b63\u5f26\u6ce2\u7ed3\u6784PDMS\u6761\u7eb9\u4e0a\u91d1\u5fae\u5e26\uff08\u539a\u5ea660nm\uff09\u7684\u5149\u5b66\u663e\u5fae\u955c\u56fe\u50cf\u3002<\/p>\n<p><strong>2.2<\/strong><strong>\u3001\u57fa\u4e8e\u7eb3\u7c73\u6750\u6599\u7684\u53ef\u62c9\u4f38\u7535\u6781<\/strong><\/p>\n<p>\u5728\u8fc7\u53bb\u7684\u51e0\u5341\u5e74\u91cc\uff0c\u5927\u91cf\u7eb3\u7c73\u6750\u6599\u7684\u6d8c\u73b0\u4f7f\u5f97\u53ef\u62c9\u4f38\u7535\u6781\u5236\u5907\u66f4\u4fbf\u5229\uff0c\u5982\u76f4\u63a5\u65cb\u6d82\u3001\u9010\u5c42\u7ec4\u88c5\u3001\u771f\u7a7a\u8fc7\u6ee4\u548c\u5728\u5f39\u6027\u805a\u5408\u7269\u8868\u9762\u539f\u4f4d\u5408\u6210\u7eb3\u7c73\u6750\u6599\u7b49\u3002\u66f4\u4e3a\u91cd\u8981\u7684\u662f\uff0c\u673a\u68b0\u529b\u4fe1\u53f7\u8f6c\u5bfc\u8fc7\u7a0b\u4e2d\u7684\u65e9\u671f\u4fe1\u53f7\u4e8b\u4ef6\u901a\u5e38\u5f15\u53d1\u6781\u5c11\u91cf\uff08\u5982nM\u7ea7\u522b\u6216\u66f4\u4f4e\u6c34\u5e73\uff09\u7684\u751f\u5316\u5206\u5b50\uff0c\u800c\u7eb3\u7c73\u6750\u6599\u8d4b\u4e88\u4e86EC\u4f20\u611f\u5668\u4f18\u826f\u7684\u50ac\u5316\u6548\u7387\uff0c\u8fdb\u800c\u6781\u5927\u5730\u63d0\u9ad8\u4e86\u5176\u68c0\u6d4b\u7075\u654f\u5ea6\u3002<\/p>\n<p><strong>\u56fe\u4e8c\u3001\u7528\u4e8e\u5236\u5907\u53ef\u62c9\u4f38\u7535\u6781\u7684\u7eb3\u7c73\u6750\u6599<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-205430\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie2.jpg\" alt=\"\" width=\"600\" height=\"358\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie2.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie2-300x179.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\uff08a\uff09\u7eb3\u7c73\u9897\u7c92\u62c9\u4f38\u65b9\u6848\uff1b<\/p>\n<p>\uff08b\uff09PDMS\u8584\u819c\u8868\u9762\u751f\u957f\u91d1\u7eb3\u7c73\u7ed3\u6784\u7684SEM\u56fe\uff1b<\/p>\n<p>\uff08c\uff09\u805a\u6c28\u916f-AuNPs\u590d\u5408\u6750\u6599\u57280%\uff08\u5de6\uff09\u548c50%\uff08\u53f3\uff09\u62c9\u4f38\u5e94\u53d8\u4e0b\u7684TEM\u56fe\uff1b<\/p>\n<p>\uff08d\uff09\u4e00\u7ef4\u7eb3\u7c73\u6750\u6599\u62c9\u4f38\u8fc7\u7a0b\u793a\u610f\u56fe\uff1b<\/p>\n<p>\uff08e\uff09PDMS\u57fa\u5e95\u8868\u9762AuNTs\u7f51\u7edc\u7684SEM\u56fe\uff1b<\/p>\n<p>\uff08f\uff09PDMS\u57fa\u5e95\u8868\u9762PEDOT\u5305\u88f9CNT\u8584\u819c\u7684\u793a\u610f\u56fe\uff1b<\/p>\n<p>\uff08g\uff09\u7c7b\u91d1\u9488\u83c7\u7ed3\u6784AuNWs\u7684\u4fa7\u89c6SEM\u56fe\uff1b<\/p>\n<p>\uff08h\uff09\u5de6\u56fe\uff1aAuNSs\u8584\u819c\u7684SEM\u56fe\u3002\u53f3\u56fe\uff1a\u5149\u5b66\u56fe\u50cf\u663e\u793a\u4e86\u62c9\u4f38\u8fc7\u7a0b\u4e2dAuNSs\u8584\u819c\u4e2d\u7684\u8936\u76b1\u53d8\u5f62\uff1b<\/p>\n<p>\uff08i\uff09\u5de6\u56fe\uff1a\u4e1d\u7f51\u5370\u5237\u6280\u672f\u4ee5\u7279\u5236\u58a8\u6c34\u5236\u5907\u53ef\u62c9\u4f38\u5668\u4ef6\u7684\u793a\u610f\u56fe\u3002\u53f3\u56fe\uff1a\u6253\u5370\u7684\u53ef\u62c9\u4f38\u56fe\u6848\u53ca\u76f8\u5e94PEDOT\uff1aPSS\u58a8\u6c34\u5fae\u89c2\u7ed3\u6784\u793a\u610f\u56fe\u3002<\/p>\n<p><strong>3<\/strong><strong>\u3001\u7ec6\u80de\u68c0\u6d4b<\/strong><\/p>\n<p>\u6240\u6709\u7ec6\u80de\u90fd\u53d7\u5230\u5fae\u73af\u5883\u4e2d\u7684\u673a\u68b0\u529b\u4fe1\u53f7\u523a\u6fc0\uff0c\u800c\u5b83\u4eec\u7684\u751f\u7269\u5316\u5b66\u53cd\u5e94\u4e0e\u8fd9\u4e9b\u673a\u68b0\u529b\u5bc6\u5207\u76f8\u5173\u3002\u957f\u671f\u4ee5\u6765\uff0c\u7531\u4e8e\u521a\u6027\u786c\u8d28\u7535\u6781\u7f3a\u4e4f\u5f39\u6027\uff0c\u96be\u4ee5\u5b9e\u73b0\u7ec6\u80de\u52a8\u6001\u62c9\u4f38\u72b6\u6001\u4e0b\u91ca\u653e\u4fe1\u53f7\u5206\u5b50\u7684\u68c0\u6d4b\u3002\u5982\u4eca\uff0c\u5c06\u673a\u68b0\u529b\u654f\u611f\u6027\u7ec6\u80de\u57f9\u517b\u5728\u53ef\u62c9\u4f38EC\u4f20\u611f\u5668\u8868\u9762\uff0c\u901a\u8fc7\u4f20\u611f\u5668\u53d8\u5f62\u5373\u53ef\u5b9e\u73b0\u7ec6\u80de\u7684\u52a8\u6001\u62c9\u4f38\uff0c\u540c\u65f6\u5b9e\u65f6\u76d1\u6d4b\u7ec6\u80de\u91ca\u653e\u7684\u4fe1\u53f7\u5206\u5b50\u3002<\/p>\n<p><strong>\u56fe\u4e09\u3001\u62c9\u4f38\u7ec6\u80de\u91ca\u653e\u4fe1\u53f7\u5206\u5b50\u7684\u5b9e\u65f6\u76d1\u6d4b<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-205431\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie3.jpg\" alt=\"\" width=\"600\" height=\"255\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie3.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie3-300x128.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\uff08a\uff09\u53ef\u62c9\u4f38EC\u4f20\u611f\u5668\u68c0\u6d4b\u52a8\u6001\u62c9\u4f38\u7ec6\u80de\u7684\u793a\u610f\u56fe\uff1b<\/p>\n<p>\uff08b\uff09\u5728AuNTs\/PDMS\u819c\u4e0a\u57f9\u517b\u7684HUVECs\u7684\u626b\u63cf\u7535\u955c\u548c\u663e\u5fae\u56fe\u50cf\uff1b<\/p>\n<p>\uff08c\uff09\u62c9\u4f38\u5e94\u53d8\u9012\u589e\u65f6\uff0cCNTs@PEDOT\/PDMS\u8868\u9762\u7684HUVECs\u5f62\u72b6\u53d8\u5316\u53ca\u5176\u91ca\u653eNO\u7684\u5b9e\u65f6\u52a8\u6001\u76d1\u6d4b\uff1b<\/p>\n<p>\uff08d\uff09v-AuNWs\u7535\u6781\u76d1\u6d4b\u4e73\u817a\u764c\u7ec6\u80deH<sub>2<\/sub>O<sub>2<\/sub>\u91ca\u653e\u7684\u793a\u610f\u56fe\u548c\u7535\u6d41\u54cd\u5e94\uff1b<\/p>\n<p>\uff08e\uff09\u5149\u81f4\u66f4\u65b0AuNTs\/TiO<sub>2<\/sub>NWs\/AuNTs\/PDMS\u4f20\u611f\u5668\u5faa\u73af\u68c0\u6d4b\u7ec6\u80de\u7684\u793a\u610f\u56fe\u3002<\/p>\n<p><strong>\u56fe\u56db\u3001\u7ec6\u80de\u673a\u68b0\u529b\u4fe1\u53f7\u8f6c\u5bfc\u7684\u5b9e\u65f6\u76d1\u6d4b<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-205432\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie4.jpg\" alt=\"\" width=\"600\" height=\"290\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie4.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie4-300x145.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\uff08a\uff09I\uff1aCNT\/AuNT\/PDMS\u7535\u6781\u8bf1\u5bfc\u548c\u76d1\u6d4b\u7ec6\u80de\u673a\u68b0\u529b\u4fe1\u53f7\u8f6c\u5bfc\u7684\u793a\u610f\u56fe\uff1bII\uff1a\u62c9\u4f38\u72b6\u6001\u4e0bHUVECs\u7684\u663e\u5fae\u6210\u50cf\u56fe\uff1aAlexa-fluor488-phalloidin\uff08\u7eff\u8272\uff1a\u808c\u52a8\u86cb\u767d\uff09\u548choechst33342\uff08\u84dd\u8272\uff1a\u7ec6\u80de\u6838\uff09\u67d3\u8272\uff1bIII\uff1a\u4e0d\u540c\u62c9\u4f38\u6a21\u91cf\u4e0bHUVECs\u7684\u5b89\u57f9\u76d1\u6d4b\uff1b<\/p>\n<p>\uff08b\uff09I\uff1aCNTs@PEDOT\/PDMS\u4f20\u611f\u5668\u5468\u5411\u62c9\u4f38HUVEC\u793a\u610f\u56fe\u3002II\uff1a\u5728\u4f20\u611f\u5668\u96c6\u6210\u8840\u7ba1\u82af\u7247\u4e2d\uff0c\u5468\u5411\u62c9\u4f38\u524d\u540eHUVECs\u7684\u793a\u610f\u56fe\u548c\u76f8\u5e94\u663e\u5fae\u56fe\u50cf\uff1bIII\uff1a\u5468\u5411\u62c9\u4f38HUVECs\u65f6\u7684\u5b89\u57f9\u76d1\u6d4b\u3002<\/p>\n<p><strong>4<\/strong><strong>\u3001\u7ec4\u7ec7\u68c0\u6d4b<\/strong><\/p>\n<p>\u4f53\u5185\u7684\u7ec4\u7ec7\u975e\u5e38\u67d4\u8f6f\uff0c\u5176\u5f39\u6027\u6a21\u91cf\u6bd4\u4f20\u7edf\u521a\u6027\u7535\u6781\uff08\u5982Pt\u548cAu\u7535\u6781\uff09\u4f4e\u51e0\u4e2a\u6570\u91cf\u7ea7\u3002\u53e6\u5916\uff0c\u52a8\u6001\u8840\u6d41\u3001\u80a0\u8815\u52a8\u3001\u547c\u5438\u7b49\u8fd0\u52a8\u4f7f\u7ec4\u7ec7\u53d1\u751f\u4f53\u79ef\u53d8\u5316\uff0c\u800c\u786c\u8d28\u6750\u6599\u4e0d\u80fd\u53d8\u5f62\uff0c\u5f80\u5f80\u4f1a\u9020\u6210\u7ec4\u7ec7\u635f\u4f24\u7684\u9ad8\u98ce\u9669\uff0c\u751a\u81f3\u5f71\u54cd\u5668\u5b98\u7684\u6b63\u5e38\u529f\u80fd\u3002\u53ef\u62c9\u4f38\u7535\u6781\u4e3a\u53d1\u5c55\u751f\u7269\u76f8\u5bb9\u6027\u7535\u5b50-\u8f6f\u7ec4\u7ec7\u4f20\u611f\u63a5\u53e3\u5e26\u6765\u4e86\u65b0\u7684\u673a\u9047\uff1a\u4e00\u65b9\u9762\uff0c\u53ef\u4f38\u7f29\u7535\u6781\u4e3a\u8f6f\/\u66f2\u7ebf\u751f\u7269\u7ec4\u7ec7\u63d0\u4f9b\u4fdd\u5f62\u63a5\u89e6\uff0c\u4ece\u800c\u7f13\u89e3\u4e86\u4f20\u611f\u5668\u548c\u7ec4\u7ec7\u7684\u673a\u68b0\u9519\u914d\uff1b\u53e6\u4e00\u65b9\u9762\uff0c\u53ef\u62c9\u4f38\u4f20\u611f\u5668\u53ef\u4ee5\u53d8\u5f62\u4ee5\u9002\u5e94\u7ec4\u7ec7\u6216\u5668\u5b98\u4f53\u79ef\u7684\u53d8\u5316\u3002<\/p>\n<p><strong>\u56fe\u4e94\u3001\u7ec4\u7ec7\u68c0\u6d4b<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-205433\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie5.jpg\" alt=\"\" width=\"600\" height=\"223\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie5.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/anie5-300x112.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\uff08a\uff09AuNTs\/PDMS\u7535\u6781\u63d2\u5165\u4eba\u8110\u9759\u8109\u8fc7\u7a0b\u7684\u793a\u610f\u56fe\uff08I\uff09\u548cNO\u91ca\u653e\u7684\u5b89\u57f9\u54cd\u5e94\uff08II\uff09\uff1b<\/p>\n<p>\uff08b\uff09CNTs\/TiO<sub>2\/<\/sub>AuNTs\u7535\u6781\u8bf1\u5bfc\u80a0\u6bb5\u6269\u5f20\u7684\u793a\u610f\u56fe\uff08I\uff09\u548c\u5b9e\u65f6\u76d1\u6d4b5-HT\u91ca\u653e\u7684\u5b89\u57f9\u54cd\u5e94\uff08II\uff09\uff1b<\/p>\n<p>\uff08c\uff09I\uff1a\u4e00\u4e2a\u5904\u4e8e\u8f6f\u72b6\u6001\u7684\u786c\u5ea6\u53ef\u8c03\u8282\u63a2\u9488\uff1bII\uff1a\u63a2\u9488\u63d2\u5165\u5927\u9f20\u7eb9\u72b6\u4f53\u5b9e\u65f6\u76d1\u6d4b\u91cd\u590d\u9ad8\u94be\u6db2\u8bf1\u5bfc\u7684\u8c37\u6c28\u9178\u91ca\u653e\uff1b<\/p>\n<p>\uff08d\uff09PtNWs\u4fee\u9970\u53ef\u62c9\u4f38MEA\u7528\u4e8e\u5927\u9f20\u8111\u90e8\u5916\u5468\u795e\u7ecf\u523a\u6fc0\u7684\u5149\u5b66\u56fe\u50cf\uff1b<\/p>\n<p>\uff08e\uff09\u4e09\u7ef4\u96c6\u6210\u578b\u591a\u529f\u80fd\u67d4\u6027\u4f20\u611f\u5668\u8d34\u9644\u5728\u5154\u5fc3\u810f\u5916\u8868\u9762\u7684\u5149\u5b66\u7167\u7247\u3002<\/p>\n<p><strong>5<\/strong><strong>\u3001\u603b\u7ed3\u4e0e\u5c55\u671b<\/strong><\/p>\n<p><strong>\u3010\u5c0f\u7ed3\u3011<\/strong><\/p>\n<p>\u7efc\u4e0a\u6240\u8ff0\uff0c\u4f5c\u8005\u603b\u7ed3\u4e86\u8fd1\u4e9b\u5e74\u53ef\u62c9\u4f38EC\u4f20\u611f\u5668\u7528\u4e8e\u7ec6\u80de\u548c\u7ec4\u7ec7\u68c0\u6d4b\u7684\u6700\u65b0\u8fdb\u5c55\u3002\u9996\u5148\uff0c\u4f5c\u8005\u4ecb\u7ecd\u57fa\u4e8e\u72ec\u7279\u7ed3\u6784\u8bbe\u8ba1\u548c\u65b0\u578b\u7eb3\u7c73\u6750\u6599\u7ec4\u88c5\u7684\u7535\u6781\u5236\u5907\u7b56\u7565\u3002\u4e4b\u540e\uff0c\u91cd\u70b9\u4ecb\u7ecd\u4e86\u8fd9\u4e9b\u4f20\u611f\u5668\u5728\u673a\u68b0\u654f\u611f\u6027\u7ec6\u80de\u548c\u7ec4\u7ec7\u5b9e\u65f6\u76d1\u6d4b\u4e2d\u7684\u5e94\u7528\u3002\u6700\u540e\uff0c\u4f5c\u8005\u63d0\u51fa\u53ef\u62c9\u4f38EC\u4f20\u611f\u5668\u5728\u7ec6\u80de\u3001\u7ec4\u7ec7\u53ca\u6d3b\u4f53\u6c34\u5e73\u68c0\u6d4b\u65b9\u9762\u7684\u53d1\u5c55\u65b9\u5411\uff1a\uff081\uff09\u63d0\u9ad8\u53ef\u62c9\u4f38\u7535\u6781\u7684\u7efc\u5408\u6027\u80fd\uff08\u5982\u7075\u654f\u5ea6\u3001\u9009\u62e9\u6027\u3001\u6297\u6c61\u67d3\uff09\u4ecd\u7136\u662f\u51c6\u786e\u6d4b\u91cf\u7684\u524d\u63d0\uff1b\uff082\uff09\u53d1\u5c55\u591a\u529f\u80fd\u96c6\u6210\u578b\uff08\u5982\u7269\u7406\u548c\u5316\u5b66\u4f20\u611f\u7ed3\u5408\uff09\u53ef\u62c9\u4f38\u4f20\u611f\u5668\uff0c\u83b7\u53d6\u673a\u68b0\u529b\u4fe1\u53f7\u8f6c\u5bfc\u7684\u591a\u53c2\u6570\u4fe1\u606f\uff1b\uff083\uff09\u7814\u53d1\u53ef\u62c9\u4f38\u5fae\u4f20\u611f\u754c\u9762\uff0c\u7ed3\u5408\u5355\u7ec6\u80de\u53ca\u4e9a\u7ec6\u80de\u5fae\u64cd\u63a7\u6280\u672f\uff0c\u63a2\u7a76\u673a\u68b0\u529b\u4fe1\u53f7\u8f6c\u5bfc\u673a\u5236\u3002\u9274\u4e8e\u53ef\u62c9\u4f38EC\u4f20\u611f\u9886\u57df\u5c1a\u5904\u4e8e\u8d77\u6b65\u9636\u6bb5\uff0c\u4f5c\u8005\u5728\u8be5\u7efc\u8ff0\u603b\u7ed3\u4e86\u4f20\u611f\u5668\u8bbe\u8ba1\u548c\u5236\u5907\u7684\u57fa\u672c\u539f\u5219\uff0c\u5e76\u6307\u51fa\u4e86\u672a\u6765\u7684\u53d1\u5c55\u65b9\u5411\uff0c\u6709\u52a9\u4e8e\u63a8\u52a8\u53ef\u62c9\u4f38EC\u4f20\u611f\u6280\u672f\u5728\u751f\u7269\u533b\u5b66\u9886\u57df\u7684\u5e7f\u6cdb\u53ca\u6df1\u5165\u5e94\u7528\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/anie.202007754\" target=\"_blank\" rel=\"noopener\">Stretchable Electrochemical Sensors for Cell and Tissue Detection<\/a> \uff08<em>Angew. Chem. Int. Ed.\u00a0<\/em><strong>2020<\/strong>, DOI:10.1002\/anie.202007754\uff09<\/p>\n<p>&nbsp;<\/p>\n<p>\u3010<strong>\u56e2\u961f\u4ecb\u7ecd<\/strong>\u3011<\/p>\n<p><strong>\u9ec4\u536b\u534e\u6559\u6388<\/strong>\uff0c\u6b66\u6c49\u5927\u5b66\u73de\u73c8\u7279\u8058\u6559\u6388\uff0c\u535a\u58eb\u751f\u5bfc\u5e08\uff0c\u56fd\u5bb6\u6770\u51fa\u9752\u5e74\u79d1\u5b66\u57fa\u91d1\u83b7\u5f97\u8005\uff0c\u56fd\u5bb6\u201c\u4e07\u4eba\u8ba1\u5212\u201d\u79d1\u6280\u521b\u65b0\u9886\u519b\u4eba\u624d\u3002\u4ece\u4e8b\u751f\u547d\u5206\u6790\u5316\u5b66\u7814\u7a76\uff0c\u4e3b\u8981\u7814\u7a76\u65b9\u5411\u4e3a\u5355\u7ec6\u80de\u5206\u6790\u3001\u751f\u7269\u7535\u5206\u6790\u5316\u5b66\u4ee5\u53ca\u5fae\u6d41\u63a7\u82af\u7247\u3002\u8fc4\u4eca\u5df2\u5728<em>Angew. Chem. Int. Ed.<\/em>,<em> J.Am.Chem. Soc.<\/em>,<em> ACS Nano<\/em>,<em> Chem. Sci.<\/em>,<em> Anal. Chem.<\/em>, <em>Small<\/em>\u7b49\u5b66\u672f\u520a\u7269\u53d1\u8868SCI\u8bba\u6587100\u4f59\u7bc7\uff0c\u53c2\u4e0e\u4e3b\u7f16\u4e13\u84571\u90e8\u3002<\/p>\n<p>\u8bfe\u9898\u7ec4\u4e3b\u9875\uff1a<a href=\"http:\/\/www.huanglab.whu.edu.cn\/\" target=\"_blank\" rel=\"noopener\">http:\/\/www.huanglab.whu.edu.cn\/<\/a><\/p>\n<p>\u3010<strong>\u56e2\u961f\u5728\u8be5\u9886\u57df\u7684\u5de5\u4f5c\u6c47\u603b<\/strong>\u3011<\/p>\n<p>\u8fd1\u51e0\u5e74\uff0c\u9ec4\u536b\u534e\u6559\u6388\u56e2\u961f\u5728\u53ef\u62c9\u4f38\u7535\u5316\u5b66\u4f20\u611f\u5668\u7684\u7814\u53d1\u53ca\u5176\u751f\u7269\u533b\u5b66\u5e94\u7528\u65b9\u9762\u5f00\u5c55\u4e86\u7cfb\u7edf\u7814\u7a76\u3002\u9996\u5148\uff0c\u5236\u5907\u4e86\u5927\u957f\u5f84\u6bd4\u7684\u91d1\u7eb3\u7c73\u7ba1\u548c\u805a\u5408\u7269PEDOT\u5305\u8986\u7684\u78b3\u7eb3\u7c73\u7ba1\uff0c\u7387\u5148\u6784\u5efa\u4e86\u6297\u673a\u68b0\u5f62\u53d8\u6027\u9ad8\u3001\u7535\u5316\u5b66\u6027\u80fd\u4f18\u5f02\u548c\u751f\u7269\u76f8\u5bb9\u6027\u826f\u597d\u7684\u53ef\u62c9\u4f38\u7535\u5316\u5b66\u4f20\u611f\u5668\uff0c\u5b9e\u73b0\u4e86\u5185\u76ae\u7ec6\u80de\u548c\u8840\u7ba1\u7ec4\u7ec7\u91ca\u653eNO\u7684\u5b9e\u65f6\u76d1\u6d4b\uff08<em>Angew. Chem. Int. Ed.<\/em> <strong>2016<\/strong>, 55, 4537-4541\uff1b<em>Anal. Chem.<\/em> <strong>2017<\/strong>, 89, 2032\uff09\u3002\u4e3a\u4e86\u8fdb\u4e00\u6b65\u8003\u5bdf\u5355\u7eaf\u673a\u68b0\u529b\u523a\u6fc0\u5bf9\u5185\u76ae\u7ec6\u80de\u91ca\u653eNO\u7684\u5f71\u54cd\uff0c\u6784\u5efa\u4e86\u57fa\u4e8e\u91d1\u7eb3\u7c73\u7ba1\u548c\u78b3\u7eb3\u7c73\u7ba1\u590d\u5408\u7ed3\u6784\u7684\u4f20\u611f\u5668\uff0c\u63d0\u5347\u4e86\u5176\u7075\u654f\u5ea6\u548c\u673a\u68b0\u6027\u80fd\uff0c\u6210\u529f\u76d1\u6d4b\u4e86\u5185\u76ae\u7ec6\u80de\u88ab\u62c9\u4f38\u65f6\u5f15\u8d77NO\u5feb\u901f\u91ca\u653e\u7684\u529b\u5b66\u4fe1\u53f7\u8f6c\u5bfc\u8fc7\u7a0b\uff08<em>Angew. Chem. Int. Ed.<\/em> <strong>2017<\/strong>, 56, 9454-9458\uff09\u3002\u6b64\u5916\uff0c\u5c06\u67d4\u6027\u4f20\u611f\u5668\u4e0e\u5fae\u6d41\u63a7\u82af\u7247\u96c6\u6210\uff0c\u6210\u529f\u6a21\u62df\u4e86\u4f4e\u8840\u538b\u3001\u6b63\u5e38\u8840\u538b\u53ca\u9ad8\u8840\u538b\u72b6\u6001\u8840\u7ba1\u5bf9\u5185\u76ae\u7ec6\u80de\u4ea7\u751f\u7684\u73af\u5f62\u62c9\u4f38\u5e94\u529b\uff0c\u5e76\u5b9e\u65f6\u76d1\u6d4b\u4e86\u8fd9\u4e9b\u5e94\u529b\u8bf1\u5bfc\u7684\u4fe1\u53f7\u5206\u5b50\u91ca\u653e\uff08<em>Small<\/em> <strong>2019<\/strong>, 1903204\uff09\u3002<\/p>\n<p>\u4e3a\u4e86\u89e3\u51b3\u67d4\u6027\u53ef\u62c9\u4f38\u7535\u6781\u754c\u9762\u6c61\u67d3\u95ee\u9898\uff0c\u8be5\u56e2\u961f\u7ed3\u5408\u524d\u671f\u53d1\u5c55\u7684\u5149\u50ac\u5316\u964d\u89e3\u7b56\u7565\uff08<em>Angew. Chem. Int. Ed.<\/em> <strong>2015<\/strong>, 54, 14402-14406\uff09\uff0c\u5728\u91d1\u7eb3\u7c73\u7ba1\u7f51\u7edc\u7ed3\u6784\u4e2d\u5f15\u5165\u5149\u50ac\u5316\u5242\u4e8c\u6c27\u5316\u949b\u7eb3\u7c73\u7ebf\uff0c\u5b9e\u73b0\u53ef\u62c9\u4f38\u7535\u5316\u5b66\u4f20\u611f\u754c\u9762\u7684\u65e0\u635f\u9ad8\u6548\u66f4\u65b0\uff08<em>Anal. Chem.<\/em> <strong>2018<\/strong>, 90, 5977-5981\uff09\u3002\u5728\u6b64\u57fa\u7840\u4e0a\uff0c\u5229\u7528\u78b3\u7eb3\u7c73\u7ba1\u7684\u6297\u751f\u7269\u5206\u5b50\u5438\u9644\u7279\u6027\uff0c\u6784\u5efa\u4e86\u517c\u5177\u6297\u751f\u7269\u6c61\u67d3\u548c\u9ad8\u6548\u964d\u89e3\u6c61\u67d3\u7269\u6027\u80fd\u7684\u53ef\u62c9\u4f38\u7535\u5316\u5b66\u4f20\u611f\u754c\u9762\u3002\u5229\u7528\u4f20\u611f\u5668\u81a8\u80c0\u6a21\u62df\u80a0\u9053\u8815\u52a8\u7684\u6269\u5f20\u8fc7\u7a0b\uff0c\u540c\u65f6\u5b9e\u65f6\u76d1\u6d4b\u4e86\u6269\u5f20\u523a\u6fc0\u5f15\u8d77\u76845-HT\u91ca\u653e\uff0c\u4e3a\u63ed\u793a5-HT\u5728\u80a0\u9053\u8fd0\u52a8\u4e2d\u7684\u4f5c\u7528\u673a\u5236\u63d0\u4f9b\u4e86\u65b0\u89c6\u89d2\uff08<em>Angew. Chem. Int. Ed.<\/em> <strong>2020<\/strong>, 59, 4075-4081\uff09\u3002\u6700\u8fd1\uff0c\u8be5\u56e2\u961f\u603b\u7ed3\u4e86\u56fd\u9645\u4e0a\u8be5\u9886\u57df\u7684\u6700\u65b0\u7814\u7a76\u8fdb\u5c55\uff0c\u64b0\u5199\u7efc\u8ff0<strong>\u201c<\/strong><strong>Stretchable Electrochemical Sensors for Cell and Tissue Detection<\/strong><strong>\u201d<\/strong><strong>\uff0c<\/strong>\u53d1\u8868\u5728<strong>Angew. Chem. Int. Ed.<\/strong>\u4e0a\uff08<em>Angew. Chem. Int. Ed.<\/em>\u00a0<strong>2020<\/strong>, DOI:10.1002\/anie.202007754\uff09\u3002<\/p>\n<p>\u672c\u6587\u7531\u6211\u4ea6\u662f\u884c\u4eba\u7f16\u8bd1\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1\uff1a<a href=\"mailto:tougao@cailiaoren.com.\" target=\"_blank\" rel=\"noopener\">tougao@cailiaoren.com.<\/a><\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaokefu.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u80cc\u666f\u4ecb\u7ecd\u3011 \u4eba\u4f53\u5185\u7ec4\u7ec7\u5668\u5b98\u7684\u57fa\u672c\u751f\u7269\u5f62\u6001\u548c\u529f\u80fd\uff0c\u5982\u8840\u7ba1\u5185\u8840\u6db2\u6d41\u52a8\u3001\u80a0\u9053\u8815\u52a8\u548c\u80ba\u90e8\u547c\u5438\u8fd0\u52a8\uff0c\u90fd\u6d89\u53ca\u5230\u52a8\u6001\u673a\u68b0\u529b\u4e0e\u5e38\u9a7b\u7ec6\u80de\u4e4b\u95f4\u7684\u4e0d\u65ad\u53cd\u9988\u3002\u7ec6\u80de\u611f\u77e5\u673a\u68b0\u529b\uff08\u5982\u62c9\u4f38\u5f20&#8230;<\/p>\n","protected":false},"author":11455,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[533],"tags":[4412],"class_list":["post-205428","post","type-post","status-publish","format-standard","hentry","category-zongshu","tag-4412"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/205428"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/11455"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=205428"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/205428\/revisions"}],"predecessor-version":[{"id":205520,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/205428\/revisions\/205520"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=205428"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=205428"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=205428"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}