{"id":205643,"date":"2020-07-24T06:50:37","date_gmt":"2020-07-23T22:50:37","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=205643"},"modified":"2020-07-23T21:51:00","modified_gmt":"2020-07-23T13:51:00","slug":"%e5%9b%9b%e5%b7%9d%e5%a4%a7%e5%ad%a6%e6%9f%af%e5%87%af%e5%89%af%e7%a0%94%e7%a9%b6%e5%91%98%e3%80%81%e6%9d%a8%e4%bc%9f%e6%95%99%e6%8e%88%e7%ad%89acs-nano%e5%a4%9a%e5%8a%9f%e8%83%bdmxene%e7%bb%87","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=205643","title":{"rendered":"\u56db\u5ddd\u5927\u5b66\u67ef\u51ef\u526f\u7814\u7a76\u5458\u3001\u6768\u4f1f\u6559\u6388\u7b49ACS Nano:\u591a\u529f\u80fdMXene\u7ec7\u7269\u7528\u4e8e\u5065\u5eb7\u7ba1\u7406\u4ee5\u53ca\u751f\u7269\u533b\u7597"},"content":{"rendered":"<p><strong>\u3010\u80cc\u666f\u4ecb\u7ecd\u3011<\/strong><\/p>\n<p>\u8fd1\u5e74\u6765\uff0c\u591a\u529f\u80fd\u67d4\u6027\u7535\u5b50\u5668\u4ef6\u56e0\u5176\u5728\u667a\u80fd\u663e\u793a\u3001\u53ef\u6301\u7eed\u80fd\u6e90\u3001\u53ef\u7a7f\u6234\u4f20\u611f\u5668\u3001\u533b\u7597\u76d1\u6d4b\u3001\u4eba\u673a\u4ea4\u4e92\u3001\u4eba\u9020\u76ae\u80a4\u3001\u8f6f\u673a\u5668\u4eba\u7b49\u9886\u57df\u7684\u6f5c\u5728\u5e94\u7528\u800c\u5907\u53d7\u5173\u6ce8\u3002\u6b64\u5916\uff0c\u76f8\u5e94\u7684\u6cbb\u7597\u7528\u7535\u5b50\u5668\u4ef6\uff0c\u5982\u8584\u819c\u52a0\u70ed\u5668\u3001\u5fc3\u810f\u8d77\u640f\u5668\u3001\u523a\u6fc0\u54cd\u5e94\u578b\u836f\u7269\u91ca\u653e\u5e73\u53f0\u7b49\uff0c\u4e5f\u5f15\u8d77\u4e86\u4eba\u4eec\u5bf9\u5404\u79cd\u7269\u7406\u6cbb\u7597\u548c\u5316\u5b66\u6cbb\u7597\u7684\u6781\u5927\u5174\u8da3\u3002\u968f\u7740\u4eba\u4eec\u5bf9\u4fbf\u643a\u6027\u548c\u53ef\u53ca\u6027\u7684\u67d4\u6027\u7535\u5b50\u5668\u4ef6\u9700\u6c42\u4e0d\u65ad\u589e\u52a0\uff0c\u8feb\u5207\u9700\u8981\u5177\u6709\u96c6\u6210\u533b\u7597\u76d1\u6d4b\u548c\u533b\u7597\u6cbb\u7597\u529f\u80fd\u7684\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6\u3002\u7136\u800c\uff0c\u7531\u4e8e\u5668\u4ef6\u96c6\u6210\u8fc7\u7a0b\u590d\u6742\uff0c\u4ee5\u53ca\u7f3a\u5c11\u591a\u529f\u80fd\u7eb3\u7c73\u6750\u6599\uff0c\u5bf9\u8fd9\u7c7b\u5668\u4ef6\u7684\u7814\u7a76\u5f88\u5c11\u3002<\/p>\n<p>\u7531\u67d4\u6027\u886c\u5e95\u548c\u5bfc\u7535\u7eb3\u7c73\u6750\u6599\u7ec4\u6210\u7684\u5404\u79cd\u5bfc\u7535\u590d\u5408\u6750\u6599\u5728\u591a\u529f\u80fd\u67d4\u6027\u7535\u5b50\u5668\u4ef6\u5236\u9020\u4e2d\u5177\u6709\u5e7f\u9614\u7684\u5e94\u7528\u524d\u666f\u3002\u7136\u800c\u7531\u4e8e\u4f20\u7edf\u5851\u6599\u57fa\u6750\u4e0e\u4eba\u4f53\u76ae\u80a4\u5b58\u5728\u673a\u68b0\u4e0d\u5339\u914d\u4ee5\u53ca\u4e0d\u826f\u7684\u900f\u6c14\u6027\uff0c\u5b83\u4eec\u901a\u5e38\u4e0d\u9002\u5408\u7528\u4e8e\u5236\u9020\u9488\u5bf9\u4e2a\u4eba\u5065\u5eb7\u76d1\u6d4b\u548c\u6cbb\u7597\u5e94\u7528\u7684\u67d4\u6027\u7535\u5b50\u5668\u4ef6\u3002\u76f8\u53cd\uff0c\u5546\u7528\u7ec7\u7269\u5177\u6709\u56fa\u6709\u7684\u67d4\u97e7\u6027\u3001\u8212\u9002\u6027\u548c\u900f\u6c14\u6027\uff0c\u662f\u67d4\u6027\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6\u7684\u6f5c\u5728\u5019\u9009\u6750\u6599\u3002\u7136\u800c\uff0c\u5982\u4f55\u5728\u4e0d\u4e27\u5931\u5176\u56fa\u6709\u7684\u67d4\u6027\u3001\u9002\u5e94\u6027\u3001\u8212\u9002\u6027\u548c\u900f\u6c14\u6027\u7684\u524d\u63d0\u4e0b\u5f15\u5165\u591a\u529f\u80fd\u6027\u4ecd\u7136\u662f\u4e00\u4e2a\u6311\u6218\u3002\u4e0e\u4f20\u7edf\u7684\u5bfc\u7535\u91d1\u5c5e\u4e0d\u540c\uff0c\u5177\u6709\u66f4\u597d\u67d4\u97e7\u6027\u7684\u65b0\u578b\u5bfc\u7535\u6750\u6599\uff0c\u5982\u91d1\u5c5e\u7eb3\u7c73\u7ebf\u3001\u672c\u5f81\u5bfc\u7535\u805a\u5408\u7269\u548c\u78b3\u7eb3\u7c73\u586b\u6599\uff0c\u53ef\u901a\u8fc7\u6eb6\u6db2\u6cd5\uff0c\u5982\u6d78\u6d82\u6cd5\u3001\u55b7\u6d82\u6cd5\u548c\u4e1d\u7f51\u5370\u5237\u5728\u67d4\u6027\u57fa\u5e95\u4e0a\u6784\u5efa\u5bfc\u7535\u5c42\u3002\u91d1\u5c5e\u7eb3\u7c73\u7ebf\u7531\u4e8e\u5176\u826f\u597d\u7684\u5bfc\u7535\u6027\u548c\u673a\u68b0\u67d4\u97e7\u6027\u800c\u5177\u6709\u5f88\u5927\u7684\u5e94\u7528\u524d\u666f\uff0c\u4f46\u540c\u65f6\u4e5f\u5b58\u5728\u7eb3\u7c73\u7ebf\u805a\u96c6\u3001\u7ed3\u70b9\u7535\u963b\u9ad8\u3001\u6210\u672c\u9ad8\u7b49\u7f3a\u70b9\u3002\u78b3\u7eb3\u7c73\u7ba1\u548c\u77f3\u58a8\u70ef\u7b49\u5177\u6709\u4f18\u826f\u5bfc\u7535\u6027\u80fd\u7684\u78b3\u7eb3\u7c73\u586b\u6599\u5df2\u6210\u4e3a\u5236\u5907\u67d4\u6027\u7535\u5b50\u5668\u4ef6\u7684\u91cd\u8981\u7814\u7a76\u65b9\u5411\uff0c\u4f46\u5176\u5728\u6c34\u4ecb\u8d28\u4e2d\u7684\u52a0\u5de5\u6027\u80fd\u5dee\uff0c\u4e0e\u666e\u901a\u67d4\u6027\u886c\u5e95\u7684\u5f31\u76f8\u4e92\u4f5c\u7528\u963b\u788d\u4e86\u5176\u5e7f\u6cdb\u5e94\u7528\u3002\u6b64\u5916\uff0c\u8fd9\u4e9b\u7eb3\u7c73\u6750\u6599\u6700\u5e38\u7528\u4e8e\u6d4b\u91cf\u673a\u68b0\u523a\u6fc0\u4e0b\u7535\u963b\u53d8\u5316\u7684\u53ef\u7a7f\u6234\u4f20\u611f\u5668\uff0c\u7136\u800c\u5b83\u4eec\u65e0\u6cd5\u5c06\u9ad8\u5bfc\u7535\u6027\u4e0e\u673a\u68b0\u8010\u4e45\u6027\u8026\u5408\u7528\u4e8e\u70ed\u7597\u5e94\u7528\u3002\u56e0\u6b64\uff0c\u5982\u4f55\u540c\u65f6\u83b7\u5f97\u53ef\u9760\u7684\u529b\u5b66\u5b8c\u6574\u6027\u548c\u826f\u597d\u7684\u7535\u5b66\u6027\u80fd\uff0c\u4ee5\u5236\u5907\u7528\u4e8e\u533b\u7597\u4fdd\u5065\u548c\u6cbb\u7597\u7684\u591a\u529f\u80fd\u667a\u80fd\u7ec7\u7269\u4ecd\u7136\u662f\u4e00\u4e2a\u5de8\u5927\u7684\u6311\u6218\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u6700\u8fd1\uff0c<strong>\u56db\u5ddd\u5927\u5b66\u67ef\u51ef\u526f\u7814\u7a76\u5458\u3001\u6768\u4f1f\u6559\u6388\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09\u4e0e\u534e\u897f\u533b\u9662\u82cf\u767d\u6d77\u56e2\u961f\u5408\u4f5c<\/strong>\u62a5\u9053\u4e86\u4ece\u65b0\u578b\u529f\u80fd\u578b\u7eb3\u7c73\u6750\u6599\uff08MXene\uff09\u4e0e\u4f20\u7edf\u67d4\u6027\u7ec7\u7269\uff08\u7ea4\u7ef4\u7d20\uff09\u590d\u5408\u7684\u89d2\u5ea6\u5236\u5907\u4e86\u4e00\u79cd\u591a\u529f\u80fd\u667a\u80fd\u7ec7\u7269\uff0c\u5e76\u5c06\u5176\u5e94\u7528\u4e8e\u4fdd\u5065\u548c\u751f\u7269\u533b\u7528\u3002\u4f5c\u8005\u5229\u7528MXene\u72ec\u7279\u7684\u8868\u9762\u5316\u5b66\u4ee5\u53ca\u7ea4\u7ef4\u7d20\u8868\u9762\u4e30\u5bcc\u7684\u5b98\u80fd\u56e2\uff0c\u901a\u8fc7MXene\u7eb3\u7c73\u7247\u7684\u5f3a\u6c22\u952e\u4f5c\u7528\u6c89\u79ef\u5728\u7ea4\u7ef4\u7d20\u7ea4\u7ef4\u8868\u9762\uff0c\u5236\u5907\u51fa\u5177\u6709\u4f18\u5f02\u7684\u5bfc\u7535\u6027\u4ee5\u53ca\u7126\u8033\u70ed\u529f\u80fd\u7684\u590d\u5408\u7ec7\u7269\u3002\u540c\u65f6\uff0c\u4f5c\u8005\u8fd8\u5229\u7528MXene\u5728\u8131\/\u5438\u9644\u6c34\u5206\u5b50\u8fc7\u7a0b\u4e2d\u7684\u7535\u963b\u54cd\u5e94\uff0c\u5229\u7528\u7ec7\u7269\u5347\u6e29\u8fc7\u7a0b\u4e2d\u8131\u6c34\u5f15\u8d77\u7684\u7535\u963b\u964d\u4f4e\u8fdb\u800c\u95f4\u63a5\u53cd\u9988\u7126\u8033\u70ed\u7684\u5347\u6e29\u6548\u5e94\uff0c\u5c06\u5176\u5236\u5907\u6210\u7684\u7535\u70ed\u6577\u6599\u53ef\u4ee5\u5b9e\u65f6\u76d1\u6d4b\u6e29\u5ea6\u7684\u53d8\u5316\uff0c\u907f\u514d\u4e86\u957f\u671f\u4f4e\u6e29\u70e7\u4f24\u7684\u5371\u9669\u3002\u6b64\u5916\uff0c\u4f5c\u8005\u8fd8\u5229\u7528\u590d\u5408\u7ec7\u7269\u7684\u7535\u70ed\u6548\u679c\u6765\u6d88\u9664\u7ec6\u83cc\u611f\u67d3\u6027\u4f24\u53e3\u5904\u7684\u8010\u836f\u83cc\uff0c\u5e76\u80fd\u4fc3\u8fdb\u4f24\u53e3\u4fee\u590d\u3002\u4f5c\u8005\u8ba4\u4e3a\uff0c\u8fd9\u4e9b\u591a\u79cd\u4f18\u5f02\u7684\u6027\u80fd\u4f7f\u5f97\u6b64MXene\u57fa\u591a\u529f\u80fd\u590d\u5408\u7ec7\u7269\u6709\u671b\u89e3\u51b3\u4e0b\u4e00\u4ee3\u4e2a\u6027\u5316\u533b\u7597\u7535\u5b50\u8bbe\u5907\u7684\u969c\u788d\u3002\u76f8\u5173\u6210\u679c\u4ee5<strong>\u201cSmart Ti<sub>3<\/sub>C<sub>2<\/sub>T<sub>x<\/sub> MXene Fabric with Fast Humidity Response and Joule Heating for Healthcare and Medical Therapy Applications\u201d<\/strong>\u53d1\u8868\u4e8e<strong>ACS<\/strong><strong>Nano<\/strong>\u4e0a<strong>\u3002<\/strong><\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u56fe\u4e00\u3001<\/strong><strong>MXene<\/strong><strong>\u7ec7\u7269\u7684\u5236\u5907\u4e0e\u8868\u5f81<\/strong><\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-205644\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano1.jpg\" alt=\"\" width=\"600\" height=\"569\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano1-300x285.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\u56fe\u4e8c\u3001<\/strong><strong>MXene<\/strong><strong>\u7ec7\u7269\u7684\u900f\u6c14\u6027\u548c\u6e7f\u5ea6\u54cd\u5e94<\/strong><\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-205645\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano2.jpg\" alt=\"\" width=\"600\" height=\"480\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano2.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano2-300x240.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\u56fe\u4e09\u3001\u7126\u8033\u70ed\u6027\u80fd\u548c\u53ef\u7a7f\u6234\u70ed\u7597\u5e94\u7528<\/strong><\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-205646\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano3.jpg\" alt=\"\" width=\"600\" height=\"772\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano3.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano3-233x300.jpg 233w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\u56fe\u56db\u3001\u53ef\u6e29\u5ea6\u9884\u8b66\u7684<\/strong><strong>MXene<\/strong><strong>\u7ec7\u7269\u7528\u4e8e\u667a\u80fd\u70ed\u7597<\/strong><\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-205647\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano4.jpg\" alt=\"\" width=\"600\" height=\"535\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano4.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano4-300x268.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\u56fe\u4e94\u3001<\/strong><strong>MXene<\/strong><strong>\u7ec7\u7269\u4f24\u53e3\u6108\u5408\u6027\u80fd\u7684\u4f53\u5185\u8bc4\u4f30<\/strong><\/p>\n<p><strong><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-205648\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano5.jpg\" alt=\"\" width=\"600\" height=\"589\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano5.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/07\/acsnano5-300x295.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/>\u3010\u5c0f\u7ed3\u3011<\/strong><\/p>\n<p>\u7efc\u4e0a\u6240\u8ff0\uff0c\u4f5c\u8005\u5229\u7528MXene\u7247\u4e0e\u7ea4\u7ef4\u7d20\u7ea4\u7ef4\u4e4b\u95f4\u7684\u5f3a\u76f8\u4e92\u4f5c\u7528\uff0c\u5c06MXene\u7247\u6d78\u6d82\u5728\u7ea4\u7ef4\u7d20\u7ea4\u7ef4\u8868\u9762\uff0c\u5f00\u53d1\u4e86\u4e00\u79cd\u591a\u529f\u80fd\u96c6\u6210MXene\u57fa\u667a\u80fd\u7ec7\u7269\u3002\u4f5c\u8005\u6240\u5236\u5907\u7684\u591a\u529f\u80fdMXene\u7ec7\u7269\u5177\u6709\u9ad8\u7075\u654f\u5ea6\u7684\u6e7f\u5ea6\u54cd\u5e94\u3001\u4f18\u826f\u7684\u7126\u8033\u52a0\u70ed\u6027\u80fd\u3001\u4f18\u5f02\u7684\u70ed\u6d88\u9664\u7ec6\u83cc\u6027\u80fd\u4ee5\u53ca\u4ee4\u4eba\u6ee1\u610f\u7684\u7ed3\u6784\u548c\u6027\u80fd\u53ef\u9760\u6027\uff0c\u5728\u4e2a\u4eba\u4fdd\u5065\u548c\u6cbb\u7597\u4e2d\u5177\u6709\u5e7f\u9614\u7684\u5e94\u7528\u524d\u666f\u3002\u6b64\u5916\uff0c\u4f5c\u8005\u8fd8\u5c55\u793a\u4e86\u4e00\u79cd\u4e00\u4f53\u5f0f\u53ef\u7a7f\u6234\u7535\u5b50\u5668\u4ef6\uff0c\u5728\u547c\u5438\u76d1\u6d4b\u3001\u667a\u80fd\u70ed\u7597\u548c\u4f24\u53e3\u6108\u5408\u65b9\u9762\u663e\u793a\u51fa\u5de8\u5927\u7684\u6f5c\u529b\u3002\u4f5c\u8005\u8ba4\u4e3a\uff0c\u8fd9\u79cd\u67d4\u6027\u3001\u591a\u529f\u80fd\u7684MXene\u7ec7\u7269\u5728\u672a\u6765\u4fbf\u643a\u5f0f\u667a\u80fd\u533b\u7597\u548c\u7535\u6cbb\u7597\u9886\u57df\u5177\u6709\u5f88\u9ad8\u7684\u5e94\u7528\u6f5c\u529b\u3002<\/p>\n<p>&nbsp;<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/pubs.acs.org\/doi\/10.1021\/acsnano.0c03391\" target=\"_blank\" rel=\"noopener\">Smart Ti3C2Tx MXene Fabric with Fast Humidity Response and Joule Heating for Healthcare and Medical Therapy Applications<\/a>\uff08<em>ACS Nano<\/em>,\u00a0<strong>2020<\/strong>, DOI:10.1021\/acsnano.0c03391\uff09<\/p>\n<p>&nbsp;<\/p>\n<p>\u3010<strong>\u56e2\u961f\u7f51\u9875<\/strong>\u3011\uff1a<a href=\"http:\/\/www.polymeryangscu.com\/\" target=\"_blank\" rel=\"noopener\">http:\/\/www.polymeryangscu.com\/<\/a><\/p>\n<p>\n \u672c\u6587\u7531\u6211\u4ea6\u662f\u884c\u4eba\u7f16\u8bd1\u6574\u7406\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1\uff1a<a href=\"mailto:tougao@cailiaoren.com.\" target=\"_blank\" rel=\"noopener\">tougao@cailiaoren.com.<\/a><\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaorenvip.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u80cc\u666f\u4ecb\u7ecd\u3011 \u8fd1\u5e74\u6765\uff0c\u591a\u529f\u80fd\u67d4\u6027\u7535\u5b50\u5668\u4ef6\u56e0\u5176\u5728\u667a\u80fd\u663e\u793a\u3001\u53ef\u6301\u7eed\u80fd\u6e90\u3001\u53ef\u7a7f\u6234\u4f20\u611f\u5668\u3001\u533b\u7597\u76d1\u6d4b\u3001\u4eba\u673a\u4ea4\u4e92\u3001\u4eba\u9020\u76ae\u80a4\u3001\u8f6f\u673a\u5668\u4eba\u7b49\u9886\u57df\u7684\u6f5c\u5728\u5e94\u7528\u800c\u5907\u53d7\u5173\u6ce8\u3002\u6b64\u5916\uff0c\u76f8\u5e94\u7684&#8230;<\/p>\n","protected":false},"author":11455,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[4419],"class_list":["post-205643","post","type-post","status-publish","format-standard","hentry","category-jiedu","tag-mxene"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/205643"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/11455"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=205643"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/205643\/revisions"}],"predecessor-version":[{"id":205996,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/205643\/revisions\/205996"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=205643"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=205643"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=205643"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}