{"id":20657,"date":"2016-06-20T14:00:16","date_gmt":"2016-06-20T06:00:16","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=20657"},"modified":"2016-06-19T22:19:59","modified_gmt":"2016-06-19T14:19:59","slug":"%e6%8f%ad%e5%bc%80%e7%a5%9e%e7%a7%98%e7%9a%84%e9%9d%a2%e7%ba%b1%ef%bc%9a%e6%9d%a5%e8%87%aa%e5%a4%96%e5%a4%aa%e7%a9%ba%e7%9a%84%e8%b6%85%e7%a8%80%e6%9c%89%e6%99%b6%e4%bd%93%e6%9d%90%e6%96%99","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=20657","title":{"rendered":"\u63ed\u5f00\u795e\u79d8\u7684\u9762\u7eb1\uff1a\u6765\u81ea\u5916\u592a\u7a7a\u7684\u8d85\u7a00\u6709\u6676\u4f53\u6750\u6599"},"content":{"rendered":"<p><strong><b>\u6750\u6599\u725b\u6ce8<\/b><\/strong>\uff1a\u51c6\u6676\u4f53\uff0c\u4e00\u79cd\u5f02\u4e8e\u666e\u901a\u6676\u4f53\u7684\u7a00\u6709\u6750\u6599\uff0c\u7269\u7406\u5b66\u5bb6\u5df2\u53d1\u73b0\u67d0\u4e9b\u7a00\u6709\u6750\u6599\u53d7\u91cd\u9707\u80fd\u4ea7\u751f\u51c6\u6676\u4f53\u3002\u4f46\u662f\uff0c\u5929\u7136\u51c6\u6676\u4f53\u5374\u662f\u5929\u5916\u6765\u7269\u3002\u666e\u6797\u65af\u987f\u5927\u5b66\u7684\u7269\u7406\u5b66\u5bb6Paul Steinhardt\u5076\u7136\u53d1\u73b0\u4e86\u4e00\u5757\u5929\u7136\u51c6\u6676\u4f53\uff0c\u53ef\u8ffd\u6eaf\u5230\u964d\u843d\u5728\u4fc4\u7f57\u65af\u79d1\u91cc\u4e9a\u514b\u5c71\u8109\u7684\u9668\u77f3\u3002\u51c6\u6676\u4f53\u7a76\u7adf\u6709\u591a\u795e\u79d8\uff1f\u4e14\u770b\u4e0b\u6587\u5206\u89e3\u3002<\/p>\n<p><a href=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/06\/1-21-1.jpg\"><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-20899 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/06\/1-21-1.jpg\" width=\"740\" height=\"416\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/06\/1-21-1.jpg 740w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/06\/1-21-1-300x169.jpg 300w\" sizes=\"(max-width: 740px) 100vw, 740px\" \/><\/a><\/p>\n<p>\u51c6\u6676\u4f53\u662f\u4e00\u79cd\u5177\u6709\u5b8c\u5168\u6709\u5e8f\u7ed3\u6784\u7684\u7279\u6b8a\u6750\u6599\uff0c\u4f46\u6240\u8c13\u7684\u6709\u5e8f\u5e76\u4e0d\u662f\u6307\u7b80\u5355\u7684\u5468\u671f\u6027\u91cd\u590d\u6392\u5217\u3002\u5230\u76ee\u524d\u4e3a\u6b62\uff0c\u5927\u90e8\u5206\u90fd\u662f\u5728\u5b9e\u9a8c\u5ba4\u4e2d\u5236\u5f97\u7684\uff0c\u53ea\u53d1\u73b0\u4e86\u4e00\u4f8b\u7eaf\u5929\u7136\u51c6\u6676\u4f53\u3002\u73b0\u5728\uff0c\u7269\u7406\u5b66\u5bb6\u76f8\u4fe1\uff0c\u4ed6\u4eec\u5df2\u7ecf\u5f04\u6e05\u4e86\u51c6\u6676\u4f53\u7684\u4ea7\u751f\u673a\u5236\u3002<\/p>\n<p>\u52a0\u5dde\u7406\u5de5\u5b66\u9662\u7684Paul Asimow\u548c\u4ed6\u7684\u5408\u4f5c\u4f19\u4f34\u4eca\u5929\u5728\u7f8e\u56fd\u56fd\u5bb6\u79d1\u5b66\u5b66\u9662\u9662\u520a\u53d1\u8868\u7684\u4e00\u7bc7\u8bba\u6587\uff0c\u00a0\u4ecb\u7ecd\u4e86\u5982\u4f55\u4f7f\u67d0\u4e9b\u7a00\u6709\u6750\u6599\u53d7\u91cd\u9707\u4ea7\u751f\u51c6\u6676\u4f53\u3002\u00a0\u4ed6\u4eec\u7684\u7814\u7a76\u7ed3\u679c\u8868\u660e\uff0c\u51c6\u6676\u4f53\u53ef\u80fd\u5728\u5ca9\u77f3\u964d\u843d\u5230\u5730\u9762\u5f62\u6210\u9668\u77f3\u4e4b\u524d\uff0c\u5728\u5c0f\u884c\u661f\u5e26\u78b0\u649e\u671f\u95f4\u5f62\u6210\u3002<\/p>\n<p>\u90a3\u4e48\u662f\u4ec0\u4e48\u8ba9\u51c6\u6676\u4f53\u5982\u6b64\u7279\u6b8a\uff1f\u6676\u4f53\u901a\u5e38\u7531\u7cbe\u786e\u6709\u5e8f\u7684\u539f\u5b50\u6392\u5217\u800c\u7ec4\u6210\uff0c\u5176\u70b9\u9635\uff08\u8702\u7a9d\u72b6\uff09\u7ed3\u6784\u4e0d\u65ad\u91cd\u590d\u8fdb\u800c\u5f62\u6210\u5468\u671f\u6027\u7684\u56fe\u6848\u3002\u4f46\u662f\uff0c\u51c6\u6676\u4f53\u7684\u70b9\u9635\u5e76\u4e0d\u662f\u5b8c\u5168\u91cd\u590d\u6392\u5217\uff0c\u800c\u662f\u5728\u76f8\u90bb\u6676\u80de\u5185\u6709\u5fae\u5c0f\u7684\u53d8\u5316\u3002\u7136\u800c\uff0c\u4ed6\u4eec\u5374\u9075\u5faa\u786e\u5207\u7684\u6570\u5b66\u89c4\u5219\uff0c\u7c7b\u4f3c\u4e8e\u8457\u540d\u7684Fibonacci\u5e8f\u5217\uff0c\u5176\u4e2d\u6bcf\u4e00\u4e2a\u6570\u5b57\u662f\u5b83\u4e4b\u524d\u7684\u4e24\u4e2a\u6570\u7684\u548c\uff081\uff0c1\uff0c2\uff0c3\uff0c5\uff0c8\uff0c13\uff0c21\uff0c\u7b49\u7b49\uff09\u3002<\/p>\n<p>\u4f8b\u5982\uff0c\u4f60\u53ef\u4ee5\u5728\u534e\u4e3d\u7684\u897f\u73ed\u7259\u963f\u7f55\u5e03\u62c9\u5bab\u7684\u9a6c\u8d5b\u514b\u4e0a\u770b\u5230\u8fd9\u79cd\u6392\u5217\u65b9\u5f0f\u3002\u60f3\u60f3\u6d74\u5ba4\u5730\u677f\uff0c\u53ea\u7528\u4e09\u89d2\u5f62\u3001\u6b63\u65b9\u5f62\u6216\u516d\u8fb9\u5f62\u7684\u74f7\u7816\u8fdb\u884c\u5e73\u94fa\u3002\u5982\u679c\u4e0d\u80fd\u6709\u4efb\u4f55\u7f1d\u9699\u6216\u91cd\u53e0\uff0c\u90a3\u4e48\u8fd9\u610f\u5473\u7740\u4e00\u4e2a\u4e94\u8fb9\u5f62\u7684\u4e94\u70b9\u5bf9\u79f0\u662f\u884c\u4e0d\u901a\u7684\u3002\u5982\u679c\u6709\u4e00\u79cd\u65b9\u6cd5\u7528\u5176\u5b83\u5f62\u72b6\u539f\u5b50\u6765\u586b\u8865\u7f1d\u9699\uff0c\u4f7f\u6240\u6709\u539f\u5b50\u7d27\u5bc6\u6392\u5217\uff0c\u8fd9\u663e\u7136\u4e5f\u662f\u53ef\u4ee5\u7684\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-20661\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/06\/\u56fe\u72472-10.png\" alt=\"\u56fe\u72472\" width=\"390\" height=\"195\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/06\/\u56fe\u72472-10.png 390w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/06\/\u56fe\u72472-10-300x150.png 300w\" sizes=\"(max-width: 390px) 100vw, 390px\" \/>\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a0\u00a01982\u5e744\u6708\uff0cDaniel Schechtman\u7b14\u8bb0\u672c\u7684\u4e00\u9875\uff08\u56fe\u7247\uff1a\u8bfa\u8d1d\u5c14\u5956\u57fa\u91d1\u4f1a\uff09<\/p>\n<p>1982\u5e74\uff0c\u51c6\u6676\u4f53\u9996\u6b21\u7531\u4ee5\u8272\u5217\u7269\u7406\u5b66\u5bb6Daniel Schechtman\uff08\u968f\u540e\u5728\u4ee5\u8272\u5217\u7406\u5de5\u5b66\u9662\u4efb\u6559\uff09\u53d1\u73b0\uff0c\u4ed6\u5728\u7535\u5b50\u663e\u5fae\u955c\u4e0b\u89c2\u5bdf\u94dd\u2014\u9530\u5408\u91d1\u6837\u54c1\u65f6\u53d1\u73b0\u4e86\u4e00\u79cd\u5947\u602a\u7684\u975e\u5468\u671f\u6027\u56fe\u6848\u3002\u201cEyn chaya kao\uff08\u201c\u4e0d\u53ef\u80fd\u6709\u8fd9\u6837\u7684\u4e8b\u7269\u201d\uff09\u201d\u4ed6\u7528\u5e0c\u4f2f\u6765\u8bed\u5583\u5583\u81ea\u8bed\u9053\u3002\u7136\u800c\uff0c\u4e8b\u5b9e\u5c31\u662f\u5982\u6b64\u3002<\/p>\n<p>\u53ef\u601c\u7684Schechtman\u5fcd\u53d7\u4e86\u5f88\u591a\u540c\u884c\u4eec\u7684\u5632\u7b11\uff0c\u5b9e\u9a8c\u5ba4\u8d1f\u8d23\u4eba\u8bbd\u523a\u5730\u529d\u4ed6\u91cd\u65b0\u9605\u8bfb\u4ed6\u7684\u6676\u4f53\u6559\u79d1\u4e66\uff0c\u751a\u81f3\u4e00\u5ea6\u8981\u6c42\u4ed6\u79bb\u5f00\u7814\u7a76\u5c0f\u7ec4\uff0c\u4f46\u4ed6\u7b11\u5230\u4e86\u6700\u540e\u3002Schechtman\u7684\u53d1\u73b0\u5f15\u53d1\u4e86\u4e00\u573a\u6676\u4f53\u9769\u547d\uff0c\u5e76\u83b7\u5f97\u4e862011\u5e74\u8bfa\u8d1d\u5c14\u5316\u5b66\u5956\u3002\u81f3\u4eca\u4e3a\u6b62\uff0c\u5728\u5168\u7403\u8303\u56f4\u5185\u7684\u5b9e\u9a8c\u5ba4\u91cc\uff0c\u5df2\u7ecf\u5236\u5907\u51fa\u8d85\u8fc7100\u79cd\u4e0d\u540c\u79cd\u7c7b\u7684\u51c6\u6676\u4f53\u3002\u51c6\u6676\u4f53\u6750\u6599\u53ef\u7528\u4e8e\u5236\u4f5c\u4e0d\u7c98\u9505\uff0cLED\u706f\u548c\u624b\u672f\u5668\u68b0\u7b49\u5176\u4ed6\u5e94\u7528\u4e2d\u3002<\/p>\n<p>2007\u5e74\uff0c\u666e\u6797\u65af\u987f\u5927\u5b66\u7684\u7269\u7406\u5b66\u5bb6Paul Steinhardt\u5728\u68b3\u7406\u535a\u7269\u9986\u6536\u85cf\u7684\u5ca9\u77f3\u65f6\u5076\u7136\u53d1\u73b0\u4e86\u4e00\u5757\u51c6\u6676\u4f53\uff0c\u5728\u6b64\u4e4b\u524d\u8fd8\u6ca1\u6709\u4eba\u53d1\u73b0\u5929\u7136\u51c6\u6676\u4f53\u3002\u4e4b\u540e\u4ed6\u4ee5\u6b64\u4e3a\u57fa\u7840\uff0c\u8ffd\u6eaf\u5230\u4e00\u5757\u964d\u843d\u5728\u4fc4\u7f57\u65af\u79d1\u91cc\u4e9a\u514b\u5c71\u8109\u7684\u9668\u77f3\uff0c\u751a\u81f3\u7ec4\u7ec7\u4e00\u652f\u63a2\u9669\u961f\u5230\u90a3\u91cc\u5bfb\u627e\u66f4\u591a\u7684\u51c6\u6676\u4f53\u6837\u54c1\u3002\u4ed6\u63a8\u65ad\u5929\u7136\u51c6\u6676\u4f53\u6765\u81ea\u4e8e\u5916\u592a\u7a7a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-20662\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/06\/\u56fe\u72473-10.png\" alt=\"\u56fe\u72473\" width=\"390\" height=\"410\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/06\/\u56fe\u72473-10.png 390w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2016\/06\/\u56fe\u72473-10-285x300.png 285w\" sizes=\"(max-width: 390px) 100vw, 390px\" \/><\/p>\n<p>Asimow\u5bf9\u4e8e\u8fd9\u4e2a\u60ca\u4eba\u7684\u53d1\u73b0\u63d0\u51fa\u4e86\u4e24\u4e2a\u5173\u952e\u6027\u7684\u95ee\u9898\u3002\u7b2c\u4e00\uff0c\u5982\u4f55\u624d\u80fd\u5728\u81ea\u7136\u754c\u4e2d\u5f62\u6210\u51c6\u6676\u4f53\uff1f\u7b2c\u4e8c\uff0c\u4ed6\u4eec\u4e3a\u4ec0\u4e48\u5982\u6b64\u7f55\u89c1\uff1f\u4ed6\u5f97\u5230\u4e86\u7b2c\u4e00\u4e2a\u7ebf\u7d22\uff1aSteinhardt\u5728Khatyrka\u9668\u77f3\u6676\u7c92\u4e2d\u53d1\u73b0\u4e86\u4e00\u4e9b\u5947\u602a\u7684\u7eb9\u7406\uff08\u5728\u94c1\u6676\u7c92\u5f62\u6210\u65f6\uff09\uff0cAsimow\u8ba4\u4e3a\u8fd9\u4e9b\u7eb9\u7406\u4e0e\u7ecf\u8fc7\u538b\u7f29\u51b2\u51fb\u8bd5\u9a8c\u7684\u6750\u6599\u6240\u5f62\u6210\u7684\u7eb9\u7406\u975e\u5e38\u76f8\u4f3c\u3002<\/p>\n<p>\u51b2\u51fb\u538b\u7f29\u8bd5\u9a8c\u662f\uff0c\u79d1\u5b66\u5bb6\u628a\u6750\u6599\u6837\u54c1\u653e\u7f6e\u5728\u4e00\u4e2a\u7279\u6b8a\u94a2\u8154\u5185\u5e76\u5411\u5b83\u53d1\u5c04\u5f39\u4e38\uff0c\u4f7f\u5176\u627f\u53d7\u96be\u4ee5\u7f6e\u4fe1\u7684\u9ad8\u538b\u3002\u8fd9\u662f\u7528\u6765\u63a2\u7d22\u6750\u6599\u5728\u6781\u7aef\u73af\u5883\u4e0b\u8868\u73b0\u7684\u8bd5\u9a8c\u624b\u6bb5\u3002<\/p>\n<p>Steinhardt\u7684\u5047\u8bbe\u4f3c\u4e4e\u662f\u5408\u7406\u7684\uff0c\u56e0\u4e3a\u79d1\u5b66\u5bb6\u4eec\u5df2\u7ecf\u8bc1\u5b9eKhatyrka\u9668\u77f3\u5728\u5760\u843d\u5230\u5730\u7403\u4e4b\u524d\u7ecf\u5386\u4e86\u67d0\u79cd\u9707\u52a8\uff0c\u6700\u6709\u53ef\u80fd\u7684\u662f\u5728\u592a\u9633\u7cfb\u521d\u671f\u7684\u5c0f\u884c\u661f\u5e26\u4e2d\u4e0e\u53e6\u4e00\u4e2a\u7269\u4f53\u53d1\u751f\u78b0\u649e\u800c\u4ea7\u751f\u7684\u3002\u6240\u4ee5Asimow\u9009\u7528\u94dc\u2014\u94dd\u5408\u91d1\u8bd5\u6837\uff08\u6210\u5206\u7c7b\u4f3c\u4e8e\u9668\u77f3\u4e2d\u7684\u67d0\u79cd\u7269\u8d28\uff09\u653e\u5165\u8be5\u5ba4\uff0c\u5e76\u7528\u94bd\u80f6\u56ca\u51b2\u51fb\u5b83\u6765\u4ea7\u751f\u7b49\u6548\u4e8e20\u4e07\u4e2a\u5927\u6c14\u538b\u7684\u73af\u5883\u3002<\/p>\n<p>\u77a7\uff01\u73b0\u5728\u4ed6\u548c\u540c\u4e8b\u4eec\u4f7f\u7528\u94c1\u542b\u91cf\u8d85\u6807\u7684\u94dc\u2014\u94dd\u5408\u91d1\u4f5c\u4e3a\u6837\u54c1\uff0c\u8fdb\u884c\u5206\u6790\u540e\u4fbf\u89c2\u5bdf\u5230\u4e86\u51c6\u6676\u7684\u72ec\u7279\u56fe\u6848\u3002<\/p>\n<p>\u201c\u6211\u4eec\u77e5\u9053\uff0c\u9668\u77f3\u5df2\u7ecf\u7ecf\u5386\u8fc7\u9707\u8361\u4e86\uff0c\u6211\u4eec\u63a8\u6d4b\uff0c\u9707\u8361\u53ef\u80fd\u662f\u5fc5\u8981\u7684\u7684\u8fc7\u7a0b\uff0c\u5f53\u6211\u4eec\u7b2c\u4e00\u6b21\u5c1d\u8bd5\u65f6\uff0c\u5b83\u4fbf\u8d77\u4f5c\u7528\u4e86\u3002\u201d\u00a0Asimow\u8bf4\u9053\u3002\u201c\u8fd9\u544a\u8bc9\u6211\u4eec\uff0c\u5982\u679c\u6709\u5408\u9002\u7684\u539f\u6599\u53ca\u51b2\u51fb\u5f3a\u5ea6\uff0c\u4ea7\u751f\u5929\u7136\u51c6\u6676\u4f53\u4e5f\u4e0d\u662f\u90a3\u4e48\u96be\u3002\u201d<\/p>\n<p>\u4ed6\u7684\u7814\u7a76\u7ed3\u679c\u63d0\u4f9b\u4e86\u4e00\u4e2a\u57fa\u672c\u7684\u673a\u5236\uff0c\u5c3d\u7ba1\u5728\u51b2\u51fb\u538b\u7f29\u8fc7\u7a0b\u4e2d\u5f62\u6210\u51c6\u6676\u7684\u7cbe\u786e\u7ec6\u8282\u8fd8\u6ca1\u6709\u88ab\u63a2\u7d22\u51fa\u6765\u3002\u81f3\u4e8e\u4e3a\u4ec0\u4e48\u51c6\u6676\u4f53\u5728\u91ce\u5916\u5982\u6b64\u7f55\u89c1\uff0cAsimow\u8ba4\u4e3a\uff0c\u5176\u90e8\u5206\u539f\u56e0\u662f\u94dc\u2014\u94dd\u5408\u91d1\u592a\u7a00\u6709\u3002\u8fd9\u5728\u8fc4\u4eca\u4e3a\u6b62\u7814\u7a76\u7684\u5176\u5b83\u4efb\u4f55\u9668\u77f3\u4e2d\u90fd\u4e0d\u5b58\u5728\uff0c\u8fd9\u662f\u5177\u6709\u5b8c\u5168\u4e0d\u540c\u5316\u5b66\u884c\u4e3a\u7684\u4e24\u79cd\u91d1\u5c5e\uff0c\u901a\u5e38\u4e0d\u4f1a\u5171\u5b58\u3002<\/p>\n<p>\u4f46\u662f\uff0c\u8fd9\u5e76\u4e0d\u610f\u5473\u7740\u5176\u4ed6\u7c7b\u4f3c\u9668\u77f3\u4e0d\u5b58\u5728\u51c6\u6676\u4f53\u3002\u76f4\u523020\u4e16\u7eaa70\u5e74\u4ee3\u9668\u77f3\u90fd\u662f\u76f8\u5f53\u7f55\u89c1\u7684\uff0c\u4f46\u662f\uff0c\u73b0\u5728\u6570\u4ee5\u5343\u8ba1\u7684\u9668\u77f3\u65e0\u65f6\u4e0d\u523b\u7684\u88ab\u6536\u96c6\u3002\u641c\u5bfb\u9668\u77f3\u6700\u597d\u7684\u5730\u65b9\u662f\u5357\u6781\u6d32\u548c\u6492\u54c8\u62c9\u6c99\u6f20\uff0c\u5728\u90a3\u91cc\uff0c\u9ed1\u8272\u7684\u5ca9\u77f3\u5f88\u5bb9\u6613\u5728\u767d\u96ea\u548c\u6c99\u5b50\u91cc\u627e\u5230\u3002<\/p>\n<p>Asimow\u5982\u4eca\u5bf9\u5b9e\u9a8c\u8fdb\u884c\u5fae\u8c03\uff0c\u90e8\u5206\u662f\u4e3a\u4e86\u786e\u5b9a\u5176\u4e2d\u94c1\u7684\u6765\u6e90\u3002\u00a0\u4ed6\u8bbe\u7f6e\u4e86\u4e24\u4e2a\u4ee5\u4e0a\u7684\u5bf9\u7167\u5b9e\u9a8c\uff0c\u4ee5\u6d88\u9664\u4ed6\u7b2c\u4e00\u4e2a\u5b9e\u9a8c\u4e2d\u6f5c\u5728\u7684\u94c1\u6e90\u2014\u2014\u6700\u6709\u53ef\u80fd\u7684\u94bd\u80f6\u56ca\u3002\u867d\u7136\u4ed6\u8fd8\u6ca1\u6709\u5206\u6790\u6570\u636e\uff0c\u4f46\u5b8c\u5168\u4e0d\u5e0c\u671b\u5176\u5f62\u6210\u51c6\u6676\u4f53\u3002\u968f\u540e\u4ed6\u5bf9\u6700\u521d\u7684\u5b9e\u9a8c\u8fdb\u884c\u6539\u8fdb\uff0c\u8fdb\u4e00\u6b65\u63a2\u7a76\u5728\u7cbe\u786e\u6761\u4ef6\u4e0b\u51c6\u6676\u4f53\u5982\u4f55\u81ea\u53d1\u5f62\u6210\u3002<\/p>\n<p>\u73b0\u5728\uff0c\u4ed6\u5f88\u9ad8\u5174\u4ed6\u7684\u7b2c\u4e00\u6b21\u5c1d\u8bd5\u4fbf\u89e3\u7b54\u4e86\u6700\u521d\u7684\u95ee\u9898\u3002\u201c\u8fd9\u89e3\u91ca\u4e86\u5929\u7136\u51c6\u6676\u4f53\u5f62\u6210\u7684\u673a\u5236\uff0c\u4ee5\u53ca\u4e3a\u4ec0\u4e48\u6211\u4eec\u5c1a\u672a\u53d1\u73b0\u5176\u4ed6\u673a\u5236\u3002\u201dAsimow\u8bf4\u3002\u201c\u56e0\u4e3a\u6211\u4eec\u6709\u72ec\u7279\u7684\u539f\u6599\u548c\u73af\u5883\u3002\u73b0\u5728\u6700\u5927\u7684\u8c1c\u56e2\u5c31\u662f\u4e3a\u4ec0\u4e48\u94dc\u94dd\u5408\u91d1\u4f1a\u5927\u91cf\u5b58\u5728\u4e8e\u8fd9\u79cd\u9668\u77f3\u5f53\u4e2d\u3002\u201d\u8fd9\u503c\u5f97\u6211\u4eec\u8fdb\u4e00\u6b65\u7684\u63a2\u7d22\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5<a href=\"http:\/\/gizmodo.com\/we-finally-know-how-these-mysterious-ultra-rare-crystal-1781821181\">These Mysterious Ultra-Rare Crystals Probably Formed in Outer Space<\/a><\/p>\n<p>\u672c\u6587\u7531\u7f16\u8f91\u90e8\u7cef\u7c73\u63d0\u4f9b\u7d20\u6750\uff0c\u674e\u5168\u7ffb\u8bd1\uff0c\u725b\u857e\u5ba1\u6838\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u6750\u6599\u725b\u6ce8\uff1a\u51c6\u6676\u4f53\uff0c\u4e00\u79cd\u5f02\u4e8e\u666e\u901a\u6676\u4f53\u7684\u7a00\u6709\u6750\u6599\uff0c\u7269\u7406\u5b66\u5bb6\u5df2\u53d1\u73b0\u67d0\u4e9b\u7a00\u6709\u6750\u6599\u53d7\u91cd\u9707\u80fd\u4ea7\u751f\u51c6\u6676\u4f53\u3002\u4f46\u662f\uff0c\u5929\u7136\u51c6\u6676\u4f53\u5374\u662f\u5929\u5916\u6765\u7269\u3002\u666e\u6797\u65af\u987f\u5927\u5b66\u7684\u7269\u7406\u5b66\u5bb6Paul Ste&#8230;<\/p>\n","protected":false},"author":230,"featured_media":20668,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[4],"tags":[34,56,48],"class_list":["post-20657","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-ganhuo","tag-history","tag-crsytal","tag-liquidmetal"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/20657"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/230"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=20657"}],"version-history":[{"count":7,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/20657\/revisions"}],"predecessor-version":[{"id":20900,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/20657\/revisions\/20900"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/20668"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=20657"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=20657"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=20657"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}