{"id":207457,"date":"2020-08-14T06:30:32","date_gmt":"2020-08-13T22:30:32","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=207457"},"modified":"2020-08-13T11:50:20","modified_gmt":"2020-08-13T03:50:20","slug":"%e5%a4%a9%e6%b4%a5%e5%a4%a7%e5%ad%a6%e5%b0%81%e4%bc%9f%e5%9b%a2%e9%98%9facs-ami%e5%b0%81%e9%9d%a2%e6%96%87%e7%ab%a0%ef%bc%9a%e6%96%b0%e5%9e%8b%e4%ba%8c%e7%bb%b4%e6%9d%90%e6%96%99%e7%a2%b2","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=207457","title":{"rendered":"\u5929\u6d25\u5927\u5b66\u5c01\u4f1f\u56e2\u961fACS\u00a0AMI\u5c01\u9762\u6587\u7ae0\uff1a\u65b0\u578b\u4e8c\u7ef4\u6750\u6599\u78b2\u5316\u9517\u7814\u7a76"},"content":{"rendered":"<p>\u8fd1\u5e74\u6765\uff0c\u5177\u6709\u7c7b\u77f3\u58a8\u70ef\u7ed3\u6784\u7684\u65b0\u578b\u4e8c\u7ef4\u6750\u6599\u78b2\u5316\u9517\uff08GeTe\uff09\u56e0\u5176\u4f18\u5f02\u7684\u7535\u5b50\u548c\u5149\u5b66\u6027\u80fd\uff0c\u53d7\u5230\u4eba\u4eec\u7684\u5e7f\u6cdb\u5173\u6ce8\u30022018\u5e74\u5929\u6d25\u5927\u5b66\u5c01\u4f1f\u6559\u6388\u56e2\u961f\u6210\u529f\u7814\u7a76\u5236\u5907\u4e86\u5355\u5c42GeTe\u7eb3\u7c73\u7247\uff0c\u7814\u7a76\u4e86\u8be5\u6750\u6599\u7684Fe<sup>3+<\/sup>\u654f\u611f\u6027\uff0c\u540c\u65f6\u53d1\u73b0\u8be5\u6750\u6599\u5728\u7a7a\u6c14\u4e2d\u5b58\u5728\u7a33\u5b9a\u6027\u95ee\u9898\uff08Nanoscale, 2018, DOI: 10.1039\/C8NR03091J\uff09\u3002\u968f\u540e\uff0c\u5c01\u4f1f\u56e2\u961f\u53c8\u9488\u5bf9Ge\u7c7b\u4e8c\u7ef4\u6750\u6599\u8fdb\u884c\u4e86\u5e26\u9699\u8c03\u63a7\u548c\u5149\u50ac\u5316\u5e94\u7528\u65b9\u9762\u7684\u7814\u7a76\uff0c\u76f8\u5173\u7814\u7a76\u6210\u679c\u53d1\u8868\u5728Nature\u00a0Communications\uff08DOI: 10.1038\/s41467-020-15262-4\uff09\u3002\u540c\u65f6\uff0c\u503c\u5f97\u6ce8\u610f\u7684\u662f\uff0c\u76f8\u5173\u7406\u8bba\u7814\u7a76\u8868\u660e\u5177\u6709\u5c42\u72b6\u7ed3\u6784\u7684\u7a84\u5e26\u9699\u534a\u5bfc\u4f53GeTe\u6750\u6599\u540c\u6837\u5177\u6709\u4f18\u5f02\u7684\u5149\u50ac\u5316\u6027\u80fd\uff0c\u503c\u5f97\u8fdb\u4e00\u6b65\u7814\u7a76\u548c\u63a2\u7d22\u3002<\/p>\n<p>\u9488\u5bf9\u8fd9\u4e00\u60c5\u51b5\uff0c\u5c01\u4f1f\u6559\u6388\u56e2\u961f\u5bf9\u4e8c\u7ef4GeTe\u7684\u5149\u50ac\u5316\u6027\u80fd\u548c\u7a7a\u6c14\u7a33\u5b9a\u6027\u5c55\u5f00\u4e86\u7814\u7a76\u3002\u9996\u5148\u901a\u8fc7\u642d\u5efa\u4e86\u7a7a\u95f4\u7fa4\u4e3aR3m\uff08160\uff09\u7684\u03b1-GeTe\u6676\u4f53\u6a21\u578b\uff0c\u6a21\u62df\u8ba1\u7b97O\u4e0eGeTe\u7684\u7ed3\u5408\u8fc7\u7a0b\uff0c\u8bc1\u660e\u4e86\u6c27\uff08O\uff09\u539f\u5b50\u503e\u5411\u4e8e\u4e0e2\u4e2a\u9517\uff08Ge\uff09\u539f\u5b50\u5f62\u6210\u66f4\u7a33\u5b9a\u7684Ge-O-Ge\u7684\u7ed3\u6784\u662f\u5bfc\u81f4\u4e8c\u7ef4GeTe\u5728\u7a7a\u6c14\u4e2d\u7a33\u5b9a\u6027\u5dee\u7684\u6839\u672c\u539f\u56e0\u3002\u968f\u540e\u5229\u7528\u8d85\u58f0\u8f85\u52a9\u6db2\u76f8\u5265\u79bb\u65b9\u6cd5\uff0c\u5206\u522b\u5728\u6c29\u6c14\u548c\u7a7a\u6c14\u4e2d\u5236\u5907\u4e86\u5c3a\u5bf8\u4e3a~10 \u00b5m\u7684Ar-GeTe\u548cO-GeTe\u7eb3\u7c73\u7247\uff0c\u5265\u79bb\u540e\u7684\u7eb3\u7c73\u7247\u5c55\u73b0\u51fa\u4f18\u5f02\u7684\u7ed3\u6676\u6027\u80fd\u548c\u5c42\u72b6\u7ed3\u6784\uff08\u56fe2\u30013\uff09\u3002\u5728N<sub>2<\/sub>\u6c1b\u56f4\u4e2d\u5bf9\u6750\u6599\u7684\u5149\u5b66\u6027\u80fd\u8868\u5f81\u7ed3\u679c\u8868\u660e\uff0cGeTe\u7eb3\u7c73\u7247\u5177\u6709\u4f18\u5f02\u7684\u5149\u50ac\u5316\u4ea7\u6c22\u6027\u80fd\uff0cAr-GeTe\u7684\u6700\u9ad8\u5149\u50ac\u5316\u4ea7\u6c22\u901f\u7387\u53ef\u8fbe\u52301.13 mmol\u2219g<sup>-1<\/sup>\u2219h<sup>-1<\/sup>\uff0c\u6bd4O-GeTe\u7eb3\u7c73\u7247\uff080.54 mmol\u2219g<sup>-1<\/sup>\u2219h<sup>-1<\/sup>\uff09\u9ad8\u51fa109%\uff08\u56fe4\uff09\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-207458 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72471-19.png\" alt=\"\" width=\"600\" height=\"655\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72471-19.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72471-19-275x300.png 275w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe1 \uff08a\uff09O\u4e0eGe\u63a5\u89e6\u540e\u6676\u4f53\u7ed3\u6784\uff1b\uff08b\uff09O\u4e0eTe\u63a5\u89e6\u540e\u6676\u4f53\u7ed3\u6784<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-207459 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72472-19.png\" alt=\"\" width=\"600\" height=\"241\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72472-19.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72472-19-300x121.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe2 \uff08a\uff09\u6837\u54c1\u5265\u79bb\u6d41\u7a0b\u56fe\uff1b\uff08b\uff09\u5265\u79bb\u524d\u540e\u6837\u54c1XRD\u6d4b\u8bd5\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-207460 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72473-20.png\" alt=\"\" width=\"600\" height=\"441\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72473-20.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72473-20-300x221.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe3 \uff08a\uff0cc\uff09\u5206\u522b\u662fAr-GeTe\u548cO-GeTe\u7c89\u672b\u7684SEM\u56fe\u50cf\uff1b\uff08b\uff0cd\uff09\u7845\u6676\u7247\u4e0a\u7684Ar-GeTe\u548cO-GeTe\u7eb3\u7c73\u7247\u7684EDS\u56fe\u6848\u548c\uff08e\uff0ci\uff09\u7684AFM\u56fe\u50cf\uff1b\uff08f\uff0cj\uff09\u4f4e\u500d\u7387TEM\u7167\u7247\uff0c\uff08g\uff0ck\uff09\u9ad8\u5206\u8fa8\u7387TEM\u663e\u5fae\u7167\u7247\u548c\uff08h\uff0cl\uff09Ar-GeTe\u548cO-GeTe\u8584\u7247\u7684SAED\u56fe\u6848\uff1b\uff08a\uff0cb\uff0ce\u2013h\uff09Ar-GeTe\uff0c\uff08c\uff0cd\uff0ci\u2013l\uff09O-GeTe\u3002<\/p>\n<p style=\"text-align: center;\">\uff08\u6bd4\u4f8b\u5c3a\uff1a10\u03bcm\u3002\u7ea2\u8272\u7ebf\u6846\uff1aSAED\u6d4b\u8bd5\u533a\u57df\uff09<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-207461 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72474-16.png\" alt=\"\" width=\"600\" height=\"490\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72474-16.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72474-16-300x245.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe4 \uff08a\uff09\u6837\u54c1\u5149\u50ac\u5316\u4ea7\u6c22\u91cf\u968f\u65f6\u95f4\u53d8\u5316\u56fe\u50cf\uff1b\uff08b\uff09\u6837\u54c1\u7684\u5149\u50ac\u5316\u4ea7\u6c22\u901f\u7387\uff08HERs\uff09\u56fe\u50cf\uff1bAr-GeTe\uff08c\uff09\u548cO-GeTe\uff08d\uff09\u7eb3\u7c73\u7247\u5149\u50ac\u5316\u5faa\u73af\u7a33\u5b9a\u6027\u6d4b\u8bd5\u56fe<\/p>\n<p>\u6587\u7ae0\u4ece2\u4e2a\u89d2\u5ea6\u5bf9\u7eb3\u7c73\u7247\u6c27\u5316\u540e\u5149\u50ac\u5316\u6027\u80fd\u7684\u4e0b\u964d\u8fd9\u4e00\u7ed3\u679c\u8fdb\u884c\u4e86\u89e3\u91ca\uff0c\u9996\u5148\u901a\u8fc7\u7b2c\u4e00\u6027\u539f\u7406\u8ba1\u7b97\u4e86\u5355\u5c42GeTe\u548cO-GeTe\u7684\u5e26\u9699\u5bbd\u5ea6\u548c\u6001\u5bc6\u5ea6\uff08\u56fe5\uff09\uff0c\u53ef\u4ee5\u770b\u51fa\u6c27\u5316\u540e\u6837\u54c1\u7684\u5e26\u9699\u589e\u5927\uff0c\u4f46\u662f\u5728GeTe\u4e2d\uff0c\u4ef7\u5e26\u548c\u5bfc\u5e26\u5206\u522b\u7531Te\u7684p\u8f68\u9053\u548cGe\u7684p\u8f68\u9053\u8d21\u732e\uff0c\u800c\u5728O-GeTe\u4e2d\uff0c\u4ef7\u5e26\u548c\u5bfc\u5e26\u4e3b\u8981\u7531Te\u7684p\u8f68\u9053\u63d0\u4f9b\u7684\uff0c\u8fd9\u4f1a\u4f7f\u6837\u54c1\u5728\u6c27\u5316\u540e\u66f4\u6613\u4e8e\u91cd\u7ec4\u5149\u751f\u8f7d\u6d41\u5b50\uff0c\u5e76\u964d\u4f4e\u5149\u50ac\u5316\u6027\u80fd\u3002<\/p>\n<p>\u6b64\u5916\uff0c\u7814\u7a76\u901a\u8fc7\u56fa\u4f53\u7d2b\u5916\u548cXPS-\u4ef7\u5e26\u8c31\u6d4b\u5b9a\u4e86\u7eb3\u7c73\u7247\u7684\u5b9e\u9645\u5e26\u9699\uff0c\u5e76\u8ba1\u7b97\u5f97\u5230\u5177\u4f53\u4ef7\u5e26\u548c\u5bfc\u5e26\u4f4d\u7f6e\uff08\u56fe6\uff09\u3002\u6c27\u5316\u540e\u6837\u54c1\u5e26\u9699\u589e\u5927\uff0c\u4e0e\u8ba1\u7b97\u7ed3\u679c\u4e00\u81f4\uff0c\u4f46\u662fO\u539f\u5b50\u7684\u63ba\u6742\u4f7f\u5f97GeTe\u6676\u4f53\u7ed3\u6784\u5185\u90e8\u51fa\u73b0Ge\u7a7a\u4f4d\uff0c\u4f7f\u5f97\u8d39\u7c73\u80fd\u7ea7\u548c\u4ef7\u5e26\u3001\u5bfc\u5e26\u4f4d\u7f6e\u53d1\u751f\u504f\u79fb\uff0c\u5149\u50ac\u5316\u4ea7\u6c22\u6027\u80fd\u53d7\u5230\u5f71\u54cd\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-207462 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72475-13.png\" alt=\"\" width=\"600\" height=\"466\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72475-13.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72475-13-300x233.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe5 \u5355\u5c42GeTe\uff08a\uff0cc\uff09\u548cO-GeTe\uff08b\uff0cd\uff09\u7684\u7535\u5b50\u80fd\u5e26\u7ed3\u6784\u548c\u72b6\u6001\u5bc6\u5ea6<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-207463 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72476-11.png\" alt=\"\" width=\"600\" height=\"495\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72476-11.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72476-11-300x248.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe6 Ar-GeTe\u548cO-GeTe\u7eb3\u7c73\u7247\u7684\uff08a\uff09\u7d2b\u5916-\u56fa\u6001\u6f2b\u53cd\u5c04\u5149\u8c31\uff08UV-DRS\uff09\uff1b\uff08b\uff09XPS\u4ef7\u5e26\u5149\u8c31\uff1b\uff08c\uff09\u80fd\u5e26\u7ed3\u6784\u548c\u5149\u50ac\u5316\u53cd\u5e94\u793a\u610f\u56fe<\/p>\n<p>\u7efc\u4e0a\u6240\u8ff0\uff0c\u901a\u8fc7\u8d85\u58f0\u8f85\u52a9\u6db2\u76f8\u5265\u79bb\u6cd5\u53ef\u4ee5\u6709\u6548\u5730\u5265\u79bb\u5236\u5907\u5927\u5c3a\u5bf8\u3001\u9ad8\u7ed3\u6676\u6027\u7684\u4e8c\u7ef4GeTe\u7eb3\u7c73\u7247\uff0c\u5c3d\u7ba1\u7406\u8bba\u548c\u5b9e\u9a8c\u4e24\u4e2a\u65b9\u9762\u5747\u8868\u660e\u8be5\u7eb3\u7c73\u7247\u5728\u7a7a\u6c14\u4e2d\u4e0d\u7a33\u5b9a\uff0c\u5bb9\u6613\u4e0eO\u539f\u5b50\u7ed3\u5408\uff0c\u4f46\u662f\u8be5\u7eb3\u7c73\u7247\u4f9d\u65e7\u5c55\u73b0\u51fa\u4f18\u5f02\u7684\u5149\u50ac\u5316\u4ea7\u6c22\u6027\u80fd\uff0c\u800c\u8fd9\u79cd\u201c\u5149\u9700\u6c42\u201d\u548c\u201c\u6c27\u907f\u514d\u201d\u7684\u7279\u6027\u5c06\u4f7f\u5f97\u8be5\u6750\u6599\u5728\u592a\u7a7a\u4f9b\u80fd\u9886\u57df\u5177\u6709\u8d85\u9ad8\u7684\u5e94\u7528\u524d\u666f\u548c\u4ef7\u503c\uff0c\u4e3a\u9ad8\u6027\u80fd\u4e8c\u7ef4\u6750\u6599\u7684\u7814\u7a76\u63d0\u4f9b\u4e86\u501f\u9274\u4e0e\u6307\u5bfc\u610f\u4e49\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-207464 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72477-10.png\" alt=\"\" width=\"600\" height=\"796\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72477-10.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/08\/\u56fe\u72477-10-226x300.png 226w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u56fe7 \u6587\u7ae0\u5c01\u9762<\/p>\n<p>\u76f8\u5173\u7814\u7a76\u5de5\u4f5c\u4ee5\u201cTwo-Dimensional\u00a0GeTe: Air\u00a0Stability\u00a0and\u00a0Photocatalytic\u00a0Performance\u00a0for\u00a0Hydrogen\u00a0Evolution\u201d \u4e3a\u9898\u4f5c\u4e3a\u5c01\u9762\u6587\u7ae0\u5728\u7ebf\u53d1\u8868\u5728ACS Applied Materials &amp; Interfaces\uff08DOI: 10.1021\/acsami.0c08699\uff09\u4e0a\u3002\u8bba\u6587\u7684\u7b2c\u4e00\u4f5c\u8005\u4e3a\u5929\u6d25\u5927\u5b66\u6750\u6599\u5b66\u9662\u7855\u58eb\u7814\u7a76\u751f\u5f20\u946b\uff0c\u901a\u8baf\u4f5c\u8005\u4e3a\u5929\u6d25\u5927\u5b66\u5c01\u4f1f\u6559\u6388\u548c\u5510\u6797\u535a\u58eb\u3002<\/p>\n<p>\u8be5\u9879\u5de5\u4f5c\u5f97\u5230\u4e86\u56fd\u5bb6\u91cd\u70b9\u7814\u53d1\u8ba1\u5212\u9879\u76ee\u3001\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u9879\u76ee\u7684\u8d44\u52a9\u3002<\/p>\n<p>\u539f\u6587\u94fe\u63a5\uff1ahttps:\/\/pubs.acs.org\/doi\/10.1021\/acsami.0c08699<\/p>\n<p>\u672c\u6587\u7531\u4f5c\u8005\u56e2\u961f\u4f9b\u7a3f\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u8fd1\u5e74\u6765\uff0c\u5177\u6709\u7c7b\u77f3\u58a8\u70ef\u7ed3\u6784\u7684\u65b0\u578b\u4e8c\u7ef4\u6750\u6599\u78b2\u5316\u9517\uff08GeTe\uff09\u56e0\u5176\u4f18\u5f02\u7684\u7535\u5b50\u548c\u5149\u5b66\u6027\u80fd\uff0c\u53d7\u5230\u4eba\u4eec\u7684\u5e7f\u6cdb\u5173\u6ce8\u30022018\u5e74\u5929\u6d25\u5927\u5b66\u5c01\u4f1f\u6559\u6388\u56e2\u961f\u6210\u529f\u7814\u7a76\u5236\u5907\u4e86\u5355\u5c42GeTe\u7eb3&#8230;<\/p>\n","protected":false},"author":11454,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-207457","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/207457"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/11454"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=207457"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/207457\/revisions"}],"predecessor-version":[{"id":207465,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/207457\/revisions\/207465"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=207457"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=207457"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=207457"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}