{"id":210502,"date":"2020-10-04T06:30:38","date_gmt":"2020-10-03T22:30:38","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=210502"},"modified":"2020-10-03T21:38:37","modified_gmt":"2020-10-03T13:38:37","slug":"%e3%80%90%e6%8a%95%e7%a8%bf%e3%80%91progress-in-materials-science%ef%bc%9a%e7%a2%b3%e5%8c%96%e7%a1%bc%e9%99%b6%e7%93%b7%e6%91%a9%e6%93%a6%e5%ad%a6%e6%80%a7%e8%83%bd","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=210502","title":{"rendered":"Progress in Materials Science\uff1a\u78b3\u5316\u787c\u9676\u74f7\u6469\u64e6\u5b66\u6027\u80fd"},"content":{"rendered":"<p>\u8fd1\u65e5\uff0c\u56fd\u9645\u6750\u6599\u9886\u57df\u9876\u7ea7\u7efc\u8ff0\u671f\u520a\u300aProgress in Materials Science\u300b\uff08IF=31.56\uff09\u4ee5\u9898\u4e3a\u201cA review of tribological properties for boron carbide ceramics\u201d\u5728\u7ebf\u53d1\u8868\u4e86\u540d\u53e4\u5c4b\u5927\u5b66\u5f20\u5dcd\u535a\u58eb\u7684\u7efc\u8ff0\u8bba\u6587\uff0c\u9610\u8ff0\u4e86\u78b3\u5316\u787c\u9676\u74f7\u6469\u64e6\u5b66\u6027\u80fd\u7684\u6700\u65b0\u8fdb\u5c55\u3002<\/p>\n<p>\u8bba\u6587\u94fe\u63a5\uff1a<a href=\"https:\/\/doi.org\/10.1016\/j.pmatsci.2020.100718\">https:\/\/doi.org\/10.1016\/j.pmatsci.2020.100718<\/a><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-210503 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/1-2.png\" alt=\"\" width=\"600\" height=\"320\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/1-2.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/1-2-300x160.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u78b3\u5316\u787c\u5177\u6709\u6781\u9ad8\u7684\u786c\u5ea6\uff0c\u662f\u5df2\u77e5\u7269\u8d28\u4e2d\u7b2c\u4e09\u786c\u7684\u6750\u6599\u3002\u78b3\u5316\u787c\u9676\u74f7\u88ab\u8ba4\u4e3a\u662f\u6469\u64e6\u5b66\u5e94\u7528\u9886\u57df\u7684\u6f5c\u5728\u5019\u9009\u6750\u6599\u3002\u4e0e\u5176\u5b83\u9676\u74f7\u6750\u6599\u76f8\u6bd4\uff0c\u78b3\u5316\u787c\u5177\u6709\u66f4\u4f4e\u7684\u5bc6\u5ea6\uff0c\u56e0\u6b64\u78b3\u5316\u787c\u9676\u74f7\u66f4\u9002\u5408\u4f5c\u4e3a\u79fb\u52a8\u6216\u65cb\u8f6c\u7684\u6469\u64e6\u5143\u4ef6\u5e94\u7528\u4e8e\u6469\u64e6\u5b66\u9886\u57df\u3002\u8fd1\u5e74\u6765\uff0c\u78b3\u5316\u787c\u9676\u74f7\u7684\u6469\u64e6\u5b66\u6027\u80fd\u9010\u6e10\u53d7\u5230\u79d1\u7814\u5de5\u4f5c\u8005\u7684\u6301\u7eed\u5173\u6ce8\uff0c\u5df2\u53d6\u5f97\u4e00\u5b9a\u7684\u8fdb\u5c55\uff0c\u4f46\u662f\u5c1a\u65e0\u6709\u5173\u78b3\u5316\u787c\u9676\u74f7\u6469\u64e6\u5b66\u6027\u80fd\u7684\u7cfb\u7edf\u6027\u63cf\u8ff0\u3002\u56e0\u6b64\uff0c\u672c\u6587\u7cfb\u7edf\u5730\u4ecb\u7ecd\u4e86\u78b3\u5316\u787c\u9676\u74f7\u5728\u6469\u64e6\u5b66\u6027\u80fd\u65b9\u9762\u7684\u6700\u65b0\u7814\u7a76\u73b0\u72b6\uff0c\u6587\u7ae0\u5171\u4e03\u4e2a\u90e8\u5206\uff1a<\/p>\n<p>\u7b2c\u4e00\u90e8\u5206\u89e3\u91ca\u4e86\u78b3\u5316\u787c\u9676\u74f7\u7684\u5fae\u89c2\u7ed3\u6784\u3001\u529b\u5b66\u6027\u80fd\u548c\u8868\u9762\u7279\u6027\u5bf9\u6469\u64e6\u5b66\u6027\u80fd\u7684\u5f71\u54cd\u3002<\/p>\n<p>\u7b2c\u4e8c\u90e8\u5206\u4ecb\u7ecd\u4e86\u78b3\u5316\u787c\u9676\u74f7\u81ea\u6da6\u6ed1\u6469\u64e6\u5b66\u6027\u80fd\u7814\u7a76\u8fdb\u5c55\u3002<\/p>\n<p>\u7b2c\u4e09\u90e8\u5206\u8bc4\u4ef7\u4e86\u78b3\u5316\u787c\u5728\u6da6\u6ed1\u6761\u4ef6\u4e0b\u7684\u6469\u64e6\u5b66\u6027\u80fd\u3002<\/p>\n<p>\u7b2c\u56db\u90e8\u5206\u8be6\u7ec6\u8003\u5bdf\u4e86\u8f7d\u8377\u3001\u6ed1\u52a8\u901f\u5ea6\u3001\u6e7f\u5ea6\u3001\u6e29\u5ea6\u3001\u6c14\u6c1b\u7b49\u5916\u90e8\u56e0\u7d20\u5bf9\u78b3\u5316\u787c\u9676\u74f7\u6469\u64e6\u5b66\u6027\u80fd\u7684\u5f71\u54cd\u3002<\/p>\n<p>\u7b2c\u4e94\u90e8\u5206\u5206\u6790\u4e86\u78b3\u5316\u787c\u9676\u74f7\u5728\u6ed1\u52a8\u8fc7\u7a0b\u4e2d\u7684\u6469\u64e6\u5316\u5b66\u53cd\u5e94\u3002<\/p>\n<p>\u7b2c\u516d\u90e8\u5206\u9610\u8ff0\u4e86\u78b3\u5316\u787c\u4f5c\u4e3a\u9676\u74f7\u6d82\u5c42\u7684\u6469\u64e6\u5b66\u6027\u80fd\u3002<\/p>\n<p>\u6700\u540e\uff0c\u63d0\u51fa\u4e86\u4f4e\u6469\u64e6\u3001\u4f4e\u78e8\u635f\u78b3\u5316\u787c\u9676\u74f7\u7684\u672a\u6765\u7814\u7a76\u65b9\u5411\u3002<\/p>\n<p><strong>\u4f5c\u8005\u7b80\u4ecb<\/strong><\/p>\n<p>\u5f20\u5dcd\uff0c\u65e0\u673a\u975e\u91d1\u5c5e\u6750\u6599\u4e13\u4e1a\uff0c\u76ee\u524d\u5728\u540d\u53e4\u5c4b\u5927\u5b66\u653b\u8bfb\u535a\u58eb\u5b66\u4f4d\u30022010.12-2018.3\u5c31\u804c\u4e8e\u4e2d\u56fd\u79d1\u5b66\u9662\u5927\u8fde\u5316\u5b66\u7269\u7406\u7814\u7a76\u6240\uff0c\u4e3b\u8981\u4ece\u4e8b\u70ed\u9632\u62a4\u6d82\u5c42\u7684\u7814\u5236\uff0c\u671f\u95f4\u7814\u5236\u7684\u70ed\u9632\u62a4\u6d82\u5c42\u5e94\u7528\u4e8e\u897f\u660c\u3001\u6587\u660c\u3001\u9152\u6cc9\u3001\u592a\u539f\u7b49\u536b\u661f\u53d1\u5c04\u57fa\u5730\u7684\u706b\u7bad\u53d1\u5c04\u53f0\uff0c\u5728\u957f\u5f81\u516d\u53f7\u9996\u98de\u4efb\u52a1\u3001\u957f\u5f81\u4e94\u53f7\u9996\u98de\u4efb\u52a1\u3001\u957f\u5f81\u4e03\u53f7\u9996\u98de\u4efb\u52a1\u7b49\u53d1\u5c04\u5de5\u4f5c\u4e2d\uff0c\u4ea7\u54c1\u6027\u80fd\u7a33\u5b9a\u53ef\u9760\uff0c\u6ee1\u8db3\u4e86\u53d1\u5c04\u4efb\u52a1\u9632\u62a4\u6280\u672f\u6307\u6807\u7684\u5404\u9879\u8981\u6c42\uff0c\u4e3a\u987a\u5229\u6267\u884c\u56fd\u5bb6\u91cd\u70b9\u536b\u661f\u4efb\u52a1\u4fdd\u9a7e\u62a4\u822a\u3002\u62c5\u4efb\u5168\u56fd\u8010\u706b\u6750\u6599\u6807\u51c6\u5316\u6280\u672f\u59d4\u5458\u4f1a\u7b2c\u4e94\u5c4a\u59d4\u5458\u4f1a\u59d4\u5458\u3001\u5168\u56fd\u8010\u706b\u6750\u6599\u6807\u51c6\u5316\u6280\u672f\u59d4\u5458\u4f1a\u7b2c\u56db\u5c4a\u8bd5\u9a8c\u65b9\u6cd5\u5206\u6280\u672f\u59d4\u5458\u4f1a\u59d4\u5458\u3001\u5165\u9009\u5927\u8fde\u5e02\u6807\u51c6\u5316\u4e13\u5bb6\u5e93\u3001\u5927\u8fde\u5e02\u9ad8\u5c42\u6b21\u4eba\u624d\u521b\u65b0\u652f\u6301\u8ba1\u5212\u4e2d\u7684\u5927\u8fde\u5e02\u9752\u5e74\u79d1\u6280\u4e4b\u661f\u3002\u81f3\u4eca\u4ee5\u7b2c\u4e00\u4f5c\u8005\u53d1\u8868\u5b66\u672f\u8bba\u6587100\u4f59\u7bc7\u3002\u653b\u8bfb\u535a\u58eb\u671f\u95f4\uff0c\u4ee5\u7b2c\u4e00\u4f5c\u8005\u5728Progress in Materials Science, Materials and Design, Journal of the European Ceramic Society, Ceramics International, Wear, Tribology Transactions\u7b49SCI\u671f\u520a\u4e0a\u53d1\u8868\u8bba\u658712\u7bc7\uff0c\u7d2f\u8ba1\u5f71\u54cd\u56e0\u5b5067.1\u3002\u7533\u8bf7\u4e2d\u56fd\u4e13\u522929\u9879\uff0c\u5df2\u83b7\u5f97\u6388\u674315\u9879\uff0c\u5236\u5b9a\u4f01\u4e1a\u6807\u51c61\u9879\uff0c\u53c2\u7f16\u56fd\u5bb6\u6807\u51c61\u9879\u3002\u62c5\u4efb\u300aAsia-Pacific Journal of Materials Science\u300b\u300a\u5de5\u4e1a\u6c34\u5904\u7406\u300b\u300a\u94f8\u9020\u300b\u7b49\u671f\u520a\u5ba1\u7a3f\u4eba\uff0c\u300a\u5de5\u4e1a\u6c34\u5904\u7406\u300b\u7b2c\u4e00\u5c4a\u9752\u5e74\u7f16\u59d4\u3002<\/p>\n<p>\u4e3b\u8981\u7814\u7a76\u65b9\u5411\uff1a\u8010\u78e8\u9676\u74f7\u5236\u5907\u53ca\u6469\u64e6\u3001\u78e8\u635f\u673a\u7406\u7814\u7a76\uff0c\u6297\u70ed\u9707\u9676\u74f7\u5236\u5907\u53ca\u673a\u7406\u5206\u6790\uff0c\u4e0d\u5b9a\u5f62\u8010\u706b\u6750\u6599\u53ca\u70ed\u9632\u62a4\u6d82\u5c42\u7814\u5236\uff0c\u77ff\u7269\u6750\u6599\u7684\u5e94\u7528\u7b49\u9886\u57df\u3002<\/p>\n<p>\u672c\u6587\u7531\u4f5c\u8005\u6295\u7a3f\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u8fd1\u65e5\uff0c\u56fd\u9645\u6750\u6599\u9886\u57df\u9876\u7ea7\u7efc\u8ff0\u671f\u520a\u300aProgress in Materials Science\u300b\uff08IF=31.56\uff09\u4ee5\u9898\u4e3a\u201cA review of tribolog&#8230;<\/p>\n","protected":false},"author":11454,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-210502","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/210502"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/11454"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=210502"}],"version-history":[{"count":5,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/210502\/revisions"}],"predecessor-version":[{"id":210555,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/210502\/revisions\/210555"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=210502"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=210502"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=210502"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}