{"id":211313,"date":"2020-10-23T12:00:35","date_gmt":"2020-10-23T04:00:35","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=211313"},"modified":"2020-10-23T18:06:33","modified_gmt":"2020-10-23T10:06:33","slug":"%e3%80%90%e5%b7%b2%e5%9b%9e%e5%a4%8d%e3%80%91joule%ef%bc%9a%e9%9d%9e%e5%af%8c%e5%8b%92%e7%83%af%e6%9c%89%e6%9c%ba%e4%bd%93%e7%9b%b8%e5%bc%82%e8%b4%a8%e7%bb%93%e5%a4%aa%e9%98%b3%e8%83%bd%e7%94%b5","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=211313","title":{"rendered":"Joule\uff1a\u975e\u5bcc\u52d2\u70ef\u6709\u673a\u4f53\u76f8\u5f02\u8d28\u7ed3\u592a\u9633\u80fd\u7535\u6c60\u4e2d\u7684\u81ea\u6fc0\u89e3\u79bb"},"content":{"rendered":"<p><strong>\u3010\u5f15\u8a00\u3011<\/strong><\/p>\n<p>\u6709\u673a\u592a\u9633\u80fd\u7535\u6c60\u662f\u5bcc\u52d2\u70ef\u5206\u5b50\u4e0e\u4f9b\u4f53\u7535\u5b50(D):\u53d7\u4f53\u7535\u5b50(A)\u754c\u9762\u5f62\u6210\u4f53\u76f8\u5f02\u8d28\u7ed3\uff0c\u89e3\u79bb\u5149\u751f\u6210\u7684\u9ad8\u7ed3\u5408\u80fd\u7684Frenkel\u6fc0\u5b50\u3002\u8fd1\u5e74\u6765\uff0c\u975e\u5bcc\u52d2\u70ef\u5206\u5b50\u4f5c\u4e3a\u7535\u5b50\u53d7\u4f53\u4ea7\u751f\u6709\u6548\u7684D:A\u754c\u9762\uff0c\u80fd\u591f\u6709\u6548\u5730\u89e3\u79bb\u6fc0\u5b50\u3002\u5728\u975e\u5bcc\u52d2\u70ef\u592a\u9633\u80fd\u7535\u6c60\u4e2d\uff0cD:A\u754c\u9762\u5fc5\u987b\u63d0\u4f9b\u4e00\u79cd\u89e3\u79bbFrenkel\u6fc0\u5b50\u7684\u5f3a\u5927\u5e93\u4ed1\u5f15\u529b\uff0c\u624d\u80fd\u4ea7\u751f\u5149\u7535\u6d41\u3002\u5149\u6fc0\u53d1\u4f1a\u5f15\u8d77\u975e\u5bcc\u52d2\u70ef\u5206\u5b50\u5185\u4f9b\u4f53\u7535\u5b50\u548c\u53d7\u4f53\u7535\u5b50\u4e4b\u95f4\u7684\u5206\u5b50\u5185\u7535\u8377\u8f6c\u79fb\uff0c\u5bfc\u81f4\u6709\u673a\u592a\u9633\u80fd\u7535\u6c60\u4e2dD<sup>+<\/sup>\u548cA<sup>&#8211;<\/sup>\u63d0\u4f9b\u7535\u80fd\u5206\u89e3\u7684\u9ad8\u7ed3\u5408\u80fdFrenkel\u6fc0\u5b50\u3002\u7814\u7a76\u8868\u660e\uff0c\u5728\u975e\u5bcc\u52d2\u70ef\u672c\u4f53\u76f8\u5f02\u8d28\u7ed3\u4e2d\uff0c\u5f53D\u548cA\u4e4b\u95f4\u7684\u80fd\u91cf\u504f\u79fb\u51cf\u5c0f\u65f6\uff0c\u6fc0\u5b50\u89e3\u79bb\u4ecd\u7136\u53ef\u4ee5\u6709\u6548\u5730\u53d1\u751f\u3002\u5728\u975e\u5bcc\u52d2\u70ef\uff08PM6:Y6\uff09\u4f53\u5f02\u8d28\u7ed3\u4e2d\uff0c\u5149\u7535\u6d41\u4e0e\u5916\u90e8\u504f\u538b\u65e0\u5173\u3002\u6b64\u5916\uff0c\u5728D:A\u754c\u9762\u4e0a\uff0c\u53ef\u4ee5\u8fc5\u901f\u53d1\u751f\u7535\u8377\u8f6c\u79fb\u3002\u5728\u975e\u5bcc\u52d2\u70ef\u592a\u9633\u80fd\u7535\u6c60\u4e2d\uff0cD:A\u672c\u4f53\u76f8\u5f02\u8d28\u7ed3\u5f62\u6210\u65f6\u5177\u6709\u6709\u6548\u7684\u5185\u529b\uff0c\u4f7f\u6fc0\u5b50\u89e3\u79bb\uff0c\u89e3\u79bb\u540e\u7684\u8f7d\u6d41\u5b50\u6d41\u5411\u5404\u4e2a\u7535\u6781\uff0c\u4ea7\u751f\u5149\u7535\u6d41\u3002\u4e0e\u6b64\u540c\u65f6\uff0c\u975e\u5bcc\u52d2\u70ef-\u5f02\u8d28\u7ed3\u4e2d\u7684\u9ad8\u80fd\u7d0a\u4e71\u4e5f\u5f97\u5230\u4e86\u6291\u5236\uff0c\u964d\u4f4e\u4e86\u5149\u4f0f\u635f\u8017\u3002\u5728\u975e\u5bcc\u52d2\u70ef\u592a\u9633\u80fd\u7535\u6c60\u4e2d\uff0c\u5149\u6fc0\u53d1\u7684D:A\u672c\u4f53\u76f8\u5f02\u8d28\u7ed3\u662f\u76f8\u4e92\u4f5c\u7528\u7684\uff0c\u4ee5\u51cf\u5c11\u7531\u4e0d\u5747\u5300\u5f15\u8d77\u7684\u9ad8\u80fd\u7d0a\u4e71\uff0c\u5b9e\u73b0\u9ad8\u6548\u7535\u8377\u4f20\u8f93\uff0c\u83b7\u5f97\u9ad8\u6548\u7684\u5149\u4f0f\u6548\u7387\u4ee5\u53ca\u8d85\u8fc716\uff05\u529f\u7387\u8f6c\u6362\u6548\u7387\u7684\u6709\u673a\u592a\u9633\u80fd\u7535\u6c60\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c<strong>\u4e2d\u56fd\u534e\u5357\u7406\u5de5\u5927\u5b66<\/strong>\u7684<strong>\u53f6\u8f69\u7acb\u6559\u6388<\/strong>\u4ee5\u53ca<strong>\u7f8e\u56fd\u7530\u7eb3\u897f\u5927\u5b66<\/strong>\u7684<strong>Bin Hu<\/strong><strong>\u6559\u6388\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba<\/strong>\u53d1\u73b0\u975e\u5bcc\u52d2\u70ef\u592a\u9633\u80fd\u7535\u6c60\u4e2d\u7684\u65bd\u4e3b\uff1a\u53d7\u4e3b\u754c\u9762\u53d1\u751f\u7684\u81ea\u6fc0\u89e3\u79bb\uff0c\u4ee5\u5b8c\u5168\u5206\u79bb\u7535\u5b50-\u7a7a\u7a74\u5bf9\uff0c\u5b9e\u73b0\u9ad8\u6548\u7684\u5149\u4f0f\u4f5c\u7528\u3002\u901a\u8fc7\u539f\u4f4d\u76d1\u6d4b\uff0cD:A\uff08PM6:Y6\uff09\u5904\u7684\u89e3\u79bb\u4e0e\u5149\u7535\u6d41\u7684\u78c1\u573a\u4f5c\u7528\u76f8\u4ea4\uff0c\u968f\u5149\u6fc0\u53d1\u5f3a\u5ea6\u7684\u9010\u6e10\u589e\u52a0\u800c\u589e\u52a0\uff0c\u4e00\u65e6\u975e\u5bcc\u52d2\u70efY6\u5206\u5b50\u88ab\u5149\u6fc0\u53d1\uff0cD:A\u754c\u9762\u7684\u89e3\u79bb\u53d8\u5f97\u5bb9\u6613\u3002\u8fd9\u662f\u4e00\u79cd\u589e\u52a0\u5149\u7167\u6765\u8bc6\u522b\u7684\u81ea\u6fc0\u89e3\u79bb\u73b0\u8c61\uff0c\u7528\u5149\u7535\u6d41\u7684\u78c1\u573a\u6548\u5e94\u76d1\u6d4b\u8be5\u89e3\u79bb\u3002\u7814\u7a76\u53d1\u73b0\uff0c\u57281 MHz\u4e0b\uff0c\u5149\u6fc0\u53d1Y6\u5206\u5b50\u4f1a\u4ea7\u751f\u4e00\u4e2a\u5076\u6781\u6781\u5316\u4fe1\u53f7\uff0c\u5728PM6:Y6\u7cfb\u7edf\u4e2d\u4ea7\u751f\u5149\u6fc0\u53d1\u4f53\u6781\u5316\u3002\u4ece\u672c\u8d28\u4e0a\u8bb2\uff0c\u5177\u6709\u5149\u8bf1\u5bfc\u5076\u6781\u6781\u5316\u7684\u5149\u6fc0\u53d1\u975e\u5bcc\u52d2\u70efY6\u5206\u5b50\u80fd\u591f\u5728D:A\u754c\u9762\u5b8c\u5168\u5206\u79bb\u7535\u5b50-\u7a7a\u7a74\u5bf9\uff0c\u5728\u975e\u5bcc\u52d2\u70ef\u6709\u673a\u592a\u9633\u80fd\u7535\u6c60\u4e2d\u5f00\u53d1\u9ad8\u6548\u5149\u4f0f\u7535\u6c60\uff0c\u4ece\u800c\u5b9e\u73b0\u81ea\u6fc0\u89e3\u79bb\u3002\u76f8\u5173\u6210\u679c\u4ee5<strong>\u201c<\/strong><strong>Self-Stimulated Dissociation in Non-Fullerene Organic Bulk-Heterojunction Solar Cells<\/strong>\u201d\u53d1\u8868\u5728<strong>Joule<\/strong>\u4e0a\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p><strong>\u56fe<\/strong><strong> 1 PM6<\/strong><strong>\uff1a<\/strong><strong>Y6<\/strong><strong>\u4f53\u76f8\u5f02\u8d28\u7ed3\u592a\u9633\u80fd\u7535\u6c60\u7684\u7279\u6027<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-211321\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/1-16.jpg\" alt=\"\" width=\"600\" height=\"447\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/1-16.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/1-16-300x224.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08A\uff09\u5728\u4f53\u76f8\u5f02\u8d28\u7ed3ITO\/ZnO\/C60-SAM\/PM6:Y6\/MoO<sub>3<\/sub>\/Ag\u5668\u4ef6\u4e2d\uff0c\u91c7\u7528532 nm\u548c785 nm\u53cc\u5149\u675f\u5206\u522b\u6fc0\u53d1\u4f9b\u4f53-PM6\u548c\u53d7\u4f53-Y6\u5f97\u5230\u7684\u78c1\u5149\u7535\u6d41\uff08Magneto-J<sub>sc<\/sub>\uff09\u56fe\uff1b<\/p>\n<p>\uff08B\uff09\u539f\u59cbPM6\u548cY6\u819c\u7684\u7d2b\u5916-\u53ef\u89c1\u5438\u6536\u5149\u8c31\uff1b<\/p>\n<p>\uff08C\uff09\u5728ITO\/ZnO\/C60-SAM\/PM6:Y6\/MoO<sub>3<\/sub>\/Ag\u5668\u4ef6\u4e2d\uff0c\u6a21\u62df\u7684\u592a\u9633\u5149\u6fc0\u53d1\uff0c\u6d4b\u91cf\u7684I-V\u7279\u6027\u56fe\uff1b<\/p>\n<p>\uff08D\uff09\u5728D:A\u5904\u7531\u5149\u5b66\u4ea7\u751f\u7684\u7535\u5b50-\u7a7a\u7a74\u5bf9\u5f15\u8d77\u7684Magneto-J<sub>sc<\/sub>\u4fe1\u53f7\u7684\u793a\u610f\u56fe\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong> 2 <\/strong><strong>\u81ea\u6fc0\u89e3\u79bb\u7684\u5b8c\u5168\u6dec\u706d<\/strong><strong>Magneto-J<sub>sc<\/sub><\/strong><strong>\u4fe1\u53f7\u7684\u5173\u952e\u504f\u7f6e\u76d1\u63a7<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-211320\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/2-17.jpg\" alt=\"\" width=\"600\" height=\"163\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/2-17.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/2-17-300x82.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u5728785 nm\u5149\u675f\u7684\u4e0d\u540c\u6fc0\u53d1\u5f3a\u5ea6\u4e0b\u4e0e\u504f\u538b\u6709\u5173\u7684Magneto-J<sub>sc<\/sub>\uff1a<\/p>\n<p>\uff08A\uff092.9 mW\/cm<sup>2<\/sup>\uff1b<\/p>\n<p>\uff08B\uff098.8 mW\/cm<sup>2<\/sup>\uff1b<\/p>\n<p>\uff08C\uff0917.5 mW\/cm<sup>2<\/sup>\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong> 3 <\/strong><strong>\u81ea\u6fc0\u89e3\u79bb\u7684\u5b8c\u5168\u6dec\u706d<\/strong><strong>Magneto-J<sub>sc<\/sub><\/strong><strong>\u4fe1\u53f7\u6240\u9700\u7684\u4e34\u754c\u504f\u7f6e<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-211319\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/3-17.jpg\" alt=\"\" width=\"600\" height=\"239\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/3-17.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/3-17-300x120.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08A\uff09Magneto-J<sub>sc<\/sub>\u786e\u5b9a\u7684\u4e34\u754c\u504f\u538bV<sub>c<\/sub>\u4e0e\u6fc0\u53d1Y6\u5206\u5b50\u5f3a\u5ea6\u7684\u5916\u504f\u538b\u7684\u5173\u7cfb\uff1b<\/p>\n<p>\uff08B\uff09\u5728\u6052\u5b9a532nm\u7684\u6fc0\u53d1\u5f3a\u5ea6\u4e0b\u6fc0\u53d1\u4f9b\u4f53-PM6\uff0c\u5728\u4e0d\u540c785nm\u5149\u675f\u5f3a\u5ea6\u4e0b\u6fc0\u53d1Y6\u5206\u5b50\u7684I-V\u7279\u6027\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong> 4 <\/strong><strong>\u4f53\u76f8\u5f02\u8d28\u7ed3\uff08<\/strong><strong>ITO\/ZnO\/C60-SAM\/PM6:Y6\/MoO<sub>3<\/sub>\/Ag<\/strong><strong>\uff09\u4e2d\u7684\u592a\u9633\u5149\u611f\u5e94<\/strong><strong>Magneto-J<sub>sc<\/sub><\/strong><strong>\u4fe1\u53f7<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-211318\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/4-17.jpg\" alt=\"\" width=\"600\" height=\"232\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/4-17.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/4-17-300x116.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08A\uff09\u91c7\u7528\u77ed\u901a\u548c\u957f\u901a\u6ee4\u5149\u7247\u6fc0\u53d1\u4f9b\u4f53-PM6\u548c\u53d7\u4f53-Y6\u5206\u5b50\uff0c\u5c06\u592a\u9633\u5149\u7167\u5c04\u5149\u8c31\u5206\u4e3a\u5149\u8c31\u533a-I\u548c\u5149\u8c31\u533a-II\uff1b<\/p>\n<p>\uff08B\uff09\u5728\u5149\u8c31\u533a-I\u548c\u5149\u8c31\u533aI+II\u6fc0\u53d1\u7684Magneto-J<sub>sc<\/sub>\u56fe\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong> 5<\/strong> <strong>\u51c6<\/strong><strong>2D<\/strong><strong>\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60<\/strong><strong>[ITO\/PEDOT:PSS\/(PEA)<sub>2<\/sub>MA<sub>4<\/sub>Pb<sub>5<\/sub>I<sub>16 <\/sub>\/PC<sub>61<\/sub>BM\/PEI\/Ag]<\/strong><strong>\u7684\u81ea\u6fc0\u89e3\u79bb<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-211317\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/5-13.jpg\" alt=\"\" width=\"600\" height=\"163\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/5-13.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/5-13-300x82.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08A\uff09\u5728\u4e0d\u540c\u6a21\u62df\u592a\u9633\u5149\u4e0b\u7684Magneto-J<sub>sc<\/sub>\u56fe\uff1b<\/p>\n<p>\uff08B\uff09\u6bcf\u4e2a\u6fc0\u53d1\u5f3a\u5ea6\u4e0b\u7684Magento-J<sub>sc<\/sub>\u4e0e\u5916\u90e8\u53cd\u5411\u504f\u7f6e\u4e4b\u95f4\u7684\u5173\u7cfb\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong> 6 <\/strong><strong>\u5728<\/strong><strong>ITO\/ZnO\/C60-SAM\/PM6:Y6\/MoO<sub>3<\/sub>\/Ag<\/strong><strong>\u5668\u4ef6\u4e2d\u7684\u6fc0\u53d1\u975e\u5bcc\u52d2\u70ef\u53d7\u4f53<\/strong><strong>-Y6<\/strong><strong>\u5206\u5b50\u548c\u4f9b\u4f53<\/strong><strong>-PM6<\/strong><strong>\u5206\u5b50<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-211316\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/6-7.jpg\" alt=\"\" width=\"600\" height=\"163\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/6-7.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/6-7-300x82.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08A\uff09Magneto-J<sub>sc<\/sub>\uff1b<\/p>\n<p>\uff08B\uff09Magneto-J<sub>sc <\/sub>\u4e0e\u5916\u90e8\u53cd\u5411\u504f\u7f6e\uff1b<\/p>\n<p>\uff08C\uff09I-V\u7279\u6027\u3002<\/p>\n<p><strong>\u56fe<\/strong><strong> 7 <\/strong><strong>Y6<\/strong><strong>\u5206\u5b50\u4e2d\u7684\u5149\u8bf1\u5bfc\u4f53\u6781\u5316<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-211315\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/7-3.jpg\" alt=\"\" width=\"600\" height=\"164\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/7-3.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/7-3-300x82.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\uff08A\uff09\u975e\u5bcc\u52d2\u70ef\u53d7\u4f53-Y6\u5206\u5b50\u4e2d\u7684\u53d7\u7535\u5b50\u548c\u4f9b\u7535\u5b50\u7684\u793a\u610f\u56fe\uff1b<\/p>\n<p>\uff08B\uff09\u5728\u53d7\u4f53-Y6\u6d3b\u6027\u5c42\u5668\u4ef6[ITO\/ZnO\/C60-SAM\/Y6\/MoO<sub>3<\/sub>\/Ag]\u4e2d\u6a21\u62df\u592a\u9633\u5149\u4e0b\u4e0d\u540c\u5149\u6fc0\u53d1\u5f3a\u5ea6\u4e0b\u7684\u7535\u5bb9\u9891\u7387\u7279\u6027\uff1b<\/p>\n<p>\uff08C\uff09\u5728\u6a21\u62df\u592a\u9633\u5149\u4e0b\uff0c\u91c7\u7528\u4e0d\u540c\u6fc0\u53d1\u5f3a\u5ea6\u4e0b\uff0c\u57281\u00d710<sup>6 <\/sup>Hz\u65f6\uff0c\u78c1\u7535\u5bb9\u663e\u793a\u4f53\u6781\u5316\u3002<\/p>\n<p><strong>\u3010\u5c0f\u7ed3\u3011<\/strong><\/p>\n<p>\u8fd9\u9879\u5de5\u4f5c\u4e2d\u53d1\u73b0\u4e86\u4e00\u4e2a\u6709\u8da3\u7684\u73b0\u8c61\uff1a\u589e\u52a0\u5149\u6fc0\u53d1\u5f3a\u5ea6\uff0c\u4f1a\u5bfc\u81f4\u5b8c\u5168\u89e3\u79bb\u975e\u5bcc\u52d2\u70efPM6:Y6\u672c\u4f53\u76f8\u5f02\u8d28\u7ed3\u592a\u9633\u80fd\u7535\u6c60[ITO\/ZnO\/C60-SAM\/PM6\uff1aY6\/MoO<sub>3<\/sub>\/Ag]\u4e2dD:A\u754c\u9762\u4e0a\u7684\u7535\u5b50-\u7a7a\u7a74\u5bf9\u6240\u9700\u7684\u4e34\u754c\u504f\u538b\u964d\u4f4e\u3002\u4ece\u672c\u8d28\u4e0a\u8bb2\uff0c\u8fd9\u79cd\u73b0\u8c61\u63d0\u51fa\u4e86\u4e00\u79cd\u72ec\u7279\u7684\u673a\u5236\uff0c\u5373\u5728\u975e\u5bcc\u52d2\u70ef\u592a\u9633\u80fd\u7535\u6c60\u4e2d\u53d1\u751f\u81ea\u6fc0\u89e3\u79bb\u3002\u8fd9\u79cd\u81ea\u6fc0\u89e3\u79bb\u662f\u901a\u8fc7\u5668\u4ef6\u5de5\u4f5c\u6761\u4ef6\u4e0b\u7528Magneto-J<sub>sc<\/sub>\u4fe1\u53f7\u76d1\u6d4b\uff0c\u4ee5\u53ca\u786e\u5b9a\u5b8c\u5168\u89e3\u79bb\u7535\u5b50-\u7a7a\u7a74\u5bf9\uff0c\u540c\u65f6\u5206\u522b\u6fc0\u53d1\u4f9b\u4f53-PM6\u548c\u53d7\u4f53-Y6\u5206\u5b50\u3002\u672c\u8d28\u4e0a\uff0c\u968f\u7740\u5149\u6fc0\u53d1\u7684Y6\u5206\u5b50\u7684\u589e\u52a0\uff0c\u964d\u4f4e\u5728D:A\u754c\u9762\u4e0a\u5b8c\u5168\u89e3\u79bb\u7535\u5b50-\u7a7a\u7a74\u5bf9\u6240\u9700\u7684\u4e34\u754c\u504f\u538b\uff0c\u5728\u975e\u5bcc\u52d2\u70efPM6:Y6\u672c\u4f53\u76f8\u5f02\u8d28\u7ed3\u592a\u9633\u80fd\u7535\u6c60\u7684D:A\u754c\u9762\u5904\u53d1\u751f\u81ea\u6fc0\u89e3\u79bb\u3002\u9ad8\u6548\u7684\u51c62D\u9499\u949b\u77ff\u592a\u9633\u80fd\u7535\u6c60\u7f3a\u4e4f\u81ea\u6fc0\u89e3\u79bb\u4f5c\u7528\uff0c\u5176\u4e2d\u5149\u6fc0\u53d1\u5f3a\u5ea6\u7684\u589e\u52a0\u5bfc\u81f4\u5b8c\u5168\u89e3\u79bb\u7535\u5b50-\u7a7a\u7a74\u5bf9\u6240\u9700\u7684\u4e34\u754c\u504f\u538b\u589e\u52a0\u3002\u901a\u8fc7\u5149\u6fc0\u53d1\u4f9d\u8d56\u6027\u78c1\u7535\u5bb9\u6d4b\u91cf\uff0c\u6765\u6392\u9664\u5149\u751f\u8f7d\u6d41\u5b50\u548c\u79bb\u5b50\u7684\u53c2\u4e0e\uff0c\u5149\u6fc0\u53d1\u53d7\u4f53-Y6\u5206\u5b50\u53ef\u4ee5\u5728\u53cc\u6781\u6781\u5316\u72b6\u6001\u4e0b\u589e\u52a0\u4f53\u6781\u5316\uff0c\u4ece\u800c\u5bfc\u81f4\u7a7a\u95f4\u5206\u5e03\u7684\u5206\u5b50\u5185\u5076\u6781\u5b50\u5f15\u8d77\u5149\u6fc0\u53d1\u589e\u52a0\u7684\u4f53\u6781\u5316\u3002\u56e0\u6b64\uff0c\u5728\u975e\u5bcc\u52d2\u70efPM6:Y6\u4f53\u5f02\u8d28\u7ed3\u592a\u9633\u80fd\u7535\u6c60\u4e2d\uff0c\u81ea\u6fc0\u89e3\u79bb\u662f\u7531\u5149\u6fc0\u53d1Y6\u5206\u5b50\u7684\u5149\u6fc0\u53d1\u589e\u52a0\u7684\u4f53\u6781\u5316\u5f15\u8d77\u7684\uff0c\u4ece\u800c\u83b7\u5f97\u9ad8\u6548\u7387\u7684\u5149\u4f0f\u4f5c\u7528\u3002<\/p>\n<p><strong>\u6587\u732e\u94fe\u63a5<\/strong><strong><a href=\"https:\/\/www.cell.com\/joule\/fulltext\/S2542-4351(20)30441-4#%20\" target=\"_blank\" rel=\"noopener\">Self-Stimulated Dissociation in Non-Fullerene Organic Bulk-Heterojunction Solar Cells<\/a><\/strong>\uff08Joule DOI: 10.1016\/j.joule.2020.09.005\uff09\u3002<\/p>\n<p>\u3010<strong>\u63a8\u8350\u9605\u8bfb\u76f8\u5173\u7684\u6587\u732e\u53ca\u8bfe\u9898\u7ec4\u7b80\u4ecb<\/strong>\u3011\uff1aY6\u5206\u5b50\u7ed3\u6784\u7684\u8bbe\u8ba1\u5f00\u53d1\uff08Single-Junction Organic Solar Cell with over 15% Efficiency Using Fused-Ring Acceptor with Electron-Deficient Core, Joule DOI: 10.1016\/j.joule.2019.01.004\uff09\uff1bY6\u4f53\u7cfb\u7684\u7ed3\u6784\u4e0e\u6027\u80fd\u7684\u5173\u7cfb\uff08Delocalization of exciton and electron wavefunction in non-fullerene acceptor molecules enables efficient organic solar cells, Nature Communications DOI: 10.1038\/s41467-020-17867-1\uff09<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-211314\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/8-2.jpg\" alt=\"\" width=\"658\" height=\"512\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/8-2.jpg 658w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/10\/8-2-300x233.jpg 300w\" sizes=\"(max-width: 658px) 100vw, 658px\" \/><\/p>\n<p>\u53f6\u8f69\u7acb\uff0c\u534e\u5357\u7406\u5de5\u5927\u5b66\u53d1\u5149\u6750\u6599\u4e0e\u5668\u4ef6\u56fd\u5bb6\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u6559\u6388\uff0c\u517c\u4efb\u534e\u5357\u534f\u540c\u521b\u65b0\u7814\u7a76\u9662\u5370\u5237\u6709\u673a\u592a\u9633\u7535\u6c60\u521b\u65b0\u4e2d\u5fc3\u4e3b\u4efb\u3002\u76ee\u524d\u7684\u7814\u7a76\u65b9\u5411\u4e3b\u8981\u96c6\u4e2d\u4e8e\u534f\u540c\u5229\u7528\u6750\u6599\u3001\u754c\u9762\u548c\u5668\u4ef6\u5de5\u827a\u7b49\u7b56\u7565\u63d0\u9ad8\u805a\u5408\u7269\u53ca\u9499\u949b\u77ff\u5149\u7535\u5668\u4ef6\u7684\u6027\u80fd\u3002\u5728Nature, Science, Nature Photonics, Nature Commun., Joule, Adv. Mater., Adv. Energy Mater., Energy Environ. Sci. \u7b49\u671f\u520a\u53d1\u8868SCI\u7814\u7a76\u8bba\u6587220\u4f59\u7bc7\uff0c\u8bba\u6587\u88ab\u5f15\u752823000\u4f59\u6b21\uff0cH-\u6307\u6570\u4e3a79\uff0c\u5e76\u8fde\u7eed\u4e8e2014\u81f32019\u5e74\u5ea6\u5165\u9009\u5168\u7403\u201c\u9ad8\u88ab\u5f15\u79d1\u5b66\u5bb6\u201d\u3002\u53f6\u8f69\u7acb\u6559\u6388\u8bfe\u9898\u7ec4\u4e3b\u8981\u6709\u4e09\u4e2a\u5927\u7814\u7a76\u65b9\u5411\uff0c\u5206\u522b\u662f\uff1a\u6709\u673a\u5149\u4f0f\u3001\u9499\u949b\u77ff\u5149\u4f0f\u3001\u9499\u949b\u77ff\u53d1\u5149\u3002\u5176\u4e2d\u6709\u673a\u5149\u4f0f\u4e3b\u8981\u96c6\u4e2d\u7814\u7a76\u5f53\u4eca\u9ad8\u6027\u80fd\u4f53\u7cfb\u7684\u7ed3\u6784\u4e0e\u6027\u80fd\u5173\u7cfb\u8fdb\u4e00\u6b65\u53d1\u5c55\u66f4\u9ad8\u6027\u80fd\u7684\u4f53\u7cfb\u3001\u5668\u4ef6\u7a33\u5b9a\u6027\u7814\u7a76\u3001\u5927\u9762\u79ef\u6a21\u7ec4\u5668\u4ef6\u7684\u5f00\u53d1\u3001\u534a\u900f\u660e\u5668\u4ef6\u53ca\u5176\u5e94\u7528\u63a2\u7d22\u7b49\u65b9\u5411\u3002<\/p>\n<p><strong>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1a<\/strong><strong>cailiaokefu<\/strong><strong>\uff0c\u6211\u4eec\u4f1a\u9080\u8bf7\u5404\u4f4d\u8001\u5e08\u52a0\u5165\u4e13\u5bb6\u7fa4\u3002<\/strong><\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c<a href=\"mailto:\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\" target=\"_blank\" rel=\"noopener\">\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com<\/a>\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u6709\u673a\u592a\u9633\u80fd\u7535\u6c60\u662f\u5bcc\u52d2\u70ef\u5206\u5b50\u4e0e\u4f9b\u4f53\u7535\u5b50(D):\u53d7\u4f53\u7535\u5b50(A)\u754c\u9762\u5f62\u6210\u4f53\u76f8\u5f02\u8d28\u7ed3\uff0c\u89e3\u79bb\u5149\u751f\u6210\u7684\u9ad8\u7ed3\u5408\u80fd\u7684Frenkel\u6fc0\u5b50\u3002\u8fd1\u5e74\u6765\uff0c\u975e\u5bcc\u52d2\u70ef\u5206\u5b50\u4f5c\u4e3a\u7535\u5b50\u53d7&#8230;<\/p>\n","protected":false},"author":7035,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[4504,2640,2983],"class_list":["post-211313","post","type-post","status-publish","format-standard","hentry","category-jiedu","tag-y6","tag-2640","tag-2983"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/211313"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/7035"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=211313"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/211313\/revisions"}],"predecessor-version":[{"id":211746,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/211313\/revisions\/211746"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=211313"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=211313"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=211313"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}