{"id":214736,"date":"2020-12-18T08:41:20","date_gmt":"2020-12-18T00:41:20","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=214736"},"modified":"2020-12-18T08:41:20","modified_gmt":"2020-12-18T00:41:20","slug":"%e6%9c%80%e6%96%b0science%ef%bc%9a%e9%86%8c%e4%bd%9c%e4%b8%ba%e5%85%b1%e5%82%ac%e5%8c%96%e5%89%82%e5%8a%a9%e5%8a%9b%e9%ab%98%e6%95%88pd%e5%82%ac%e5%8c%96","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=214736","title":{"rendered":"\u6700\u65b0Science\uff1a\u918c\u4f5c\u4e3a\u5171\u50ac\u5316\u5242\u52a9\u529b\u9ad8\u6548Pd\u50ac\u5316"},"content":{"rendered":"<p><strong><b>\u3010\u5f15\u8a00\u3011<\/b><\/strong><\/p>\n<p>\u94af\u50ac\u5316\u7684\u6709\u673a\u5206\u5b50\u6c27\u5316\u53cd\u5e94\u8d77\u6e90\u4e8e1959\u5e74\uff0c\u5f53\u65f6\u7528\u4e8e\u4e59\u70ef\u548c\u6c34\u7684\u6c27\u5316\u5076\u8054\u3002\u6b64\u540e\u4e0d\u4e45\u5c31\u62a5\u9053\u4e86\u94af\u50ac\u5316\u7684\u82b3\u70c3\u4e0e\u8054\u82b3\u57fa\u7684\u6c27\u5316\u3002\u8fd9\u4e9b\u65b9\u6cd5\u7684\u8f83\u5dee\u7684\u50ac\u5316\u6548\u7387\u548c\u8f83\u4f4e\u7684\u9009\u62e9\u6027\u4fc3\u8fdb\u4e86\u4ee5\u9884\u6c27\u5316\u5e95\u7269\uff08\u5982\u82b3\u57fa\u5364\u5316\u7269\uff09\u4e3a\u5076\u5408\u7684Pd\u50ac\u5316\u7684\u53d1\u5c55\u3002Pd\u50ac\u5316\u7684\u53cd\u5e94\u53d6\u5f97\u4e86\u975e\u51e1\u7684\u6210\u529f\uff0c\u5bf9\u4e8eC-H\u952e\u7684\u76f4\u63a5\u6c27\u5316\u5b98\u80fd\u7684\u65b9\u6cd5\u53ef\u4ee5\u57fa\u672c\u4e0a\u7b80\u5316\u5230\u4e0d\u540c\u7684\u5316\u5b66\u7ed3\u6784\u3002Pd\u50ac\u5316C-H\u952e\u6c27\u5316\u53cd\u5e94\u80fd\u591f\u4f7f\u836f\u7269\u3001\u519c\u836f\u4ee5\u53ca\u5176\u4ed6\u9886\u57df\u4e2d\u7684\u5404\u79cd\u590d\u6742\u6709\u673a\u5206\u5b50\u5408\u6210\u66f4\u52a0\u7b80\u5355\uff0c\u4f46\u662f\u76ee\u524d\u7684\u65b9\u6cd5\u4e2dPd\u50ac\u5316\u5242\u7684\u8d1f\u8f7d\u91cf\u91cf\u6709\u65f6\u9700\u8981\u975e\u5e38\u9ad8\uff0c\u800c\u4e14\u53cd\u5e94\u4e2d\u9700\u8981\u52a0\u5165\u5927\u91cf\u6c27\u5316\u5242\uff0c\u4e25\u91cd\u5f71\u54cd\u4e86Pd(II)\u50ac\u5316\u5728\u6709\u673a\u5408\u6210\u53cd\u5e94\u4e2d\u7684\u5e94\u7528\u3002\u5c3d\u7ba1\u5f15\u5165\u6c27\u6c14\u4f5c\u4e3a\u6c27\u5316\u5242\u51cf\u5c11\u4e86\u5bf9\u9884\u6d3b\u5316\u7684\u9700\u6c42\uff0c\u4f46\u662f\u50ac\u5316\u5374\u5f80\u5f80\u6548\u7387\u8f83\u4f4e\uff0c\u7279\u522b\u662f\u5728\u82b3\u70c3\u5076\u8054\u7684\u60c5\u51b5\u4e0b\uff0c\u73b0\u6709\u7684\u65b9\u6cd5\u901a\u5e38\u8868\u73b0\u51fa\u8f83\u5dee\u7684\u50ac\u5316\u5242\u6027\u80fd\u3002<\/p>\n<p>\u8fd1\u65e5\uff0c<strong><b>\u7f8e\u56fd<\/b><\/strong><strong><b>\u5a01\u65af\u5eb7\u661f\u5927\u5b66\u9ea6\u8fea\u900a\u5206\u6821Shannon S. Stahl<\/b><\/strong><strong><b>\uff08\u901a\u8baf\u4f5c\u8005\uff09<\/b><\/strong>\u63a2\u8ba8\u4e86\u5177\u6709\u4ee3\u8868\u6027\u7684Pd\u50ac\u5316\u6c27\u5316C-H\u82b3\u57fa\u5316\u53cd\u5e94\u7684\u673a\u7406\uff0c\u5e76\u9610\u660e\u4e86\u7834\u574f\u50ac\u5316\u5242\u6027\u80fd\u7684\u673a\u7406\u7279\u5f81\uff0c\u5305\u62ec\u5e95\u7269\u6d88\u8017\u7684\u526f\u53cd\u5e94\u548c\u50ac\u5316\u5242\u4f5c\u4e3a\u975e\u6d3b\u6027\u7269\u8d28\u7684\u5b58\u5728\u3002\u540c\u65f6\u63ed\u793a\u4e86\u5728\u53cd\u5e94\u4e2d\u52a0\u5165\u918c\u4f5c\u4e3a\u5171\u50ac\u5316\u5242\uff0c\u80fd\u591f\u89e3\u51b3\u4ee5\u4e0a\u7f3a\u70b9\u3002\u4f7f\u75282,5-\u4e8c\u53d4\u4e01\u57fa\u90bb\u82ef\u918c\u4f7fPd\u50ac\u5316\u5242\u80fd\u591f\u6709\u6548\u5730\u5229\u7528\u5206\u5b50\u6c27\u4f5c\u4e3a\u6c27\u5316\u5242\uff0c\u53cd\u5e94\u4ea7\u7387\u9ad8\uff0c\u5e76\u4f7fPd\u50ac\u5316\u5242\u7684TON\u5927\u4e8e1900\uff08\u4ee5\u5f80\u7684Pd\u50ac\u5316\u53cd\u5e94TON\u4e3a13\uff09\uff0c\u540c\u65f6\u5728\u5bf9\u82ef\u4e59\u9178\u90bb\u4f4dC(sp<sup>2<\/sup>)-H\u7684\u6d3b\u5316\u53cd\u5e94\u4e2d\uff0c\u5b9e\u73b0\u4e86\u4e2d\u7b49\u5230\u4f18\u5f02\u7684C-H\u952e\u82b3\u57fa\u5316\u7ed3\u679c\u3002\u76f8\u5173\u7814\u7a76\u6210\u679c\u4ee5\u201c<strong><b>Tailored quinones support high-turnover Pd catalysts for oxidative C<\/b><\/strong><strong><b>&#8211;<\/b><\/strong><strong><b>H arylation with O<\/b><\/strong><strong><sub><b>2<\/b><\/sub><\/strong>\u201d\u4e3a\u9898\u53d1\u8868\u5728<strong><b>Science<\/b><\/strong>\u4e0a\u3002<\/p>\n<p><strong><b>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/b><\/strong><\/p>\n<p><strong><b>\u56fe\u4e00<\/b><\/strong><strong><b>\u3001\u00a0Pd\u50ac\u5316C-H\u6c27\u5316\u53cd\u5e94\uff0c\u7a81\u51fa\u4e86\u50ac\u5316\u5242\u6027\u80fd<\/b><\/strong><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-214737\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/12\/\u56fe1-2.jpg\" alt=\"\" width=\"600\" height=\"657\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/12\/\u56fe1-2.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/12\/\u56fe1-2-274x300.jpg 274w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p><strong><b>\u56fe\u4e8c<\/b><\/strong><strong><b>\u3001Pd\u50ac\u5316C-H\u82b3\u57fa\u5316\u53cd\u5e94\u7684\u52a8\u529b\u5b66\u548c\u5149\u8c31\u5206\u6790<\/b><\/strong><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-214738\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/12\/\u56fe2-2.jpg\" alt=\"\" width=\"600\" height=\"745\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/12\/\u56fe2-2.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/12\/\u56fe2-2-242x300.jpg 242w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p><strong><b>\u56fe\u4e09<\/b><\/strong><strong><b>\u3001\u5b9e\u9a8c\u6570\u636e\u548c\u8ba1\u7b97\u5206\u6790\u4e00\u81f4<\/b><\/strong><strong><b>\u6027<\/b><\/strong><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-214739\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/12\/\u56fe3-2.jpg\" alt=\"\" width=\"600\" height=\"625\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/12\/\u56fe3-2.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/12\/\u56fe3-2-288x300.jpg 288w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p>&nbsp;<\/p>\n<p><strong><b>\u56fe\u56db<\/b><\/strong><strong><b>\u3001<\/b><\/strong><strong><b>\u4f4e<\/b><\/strong><strong><b>\u8f7d\u91cf\u50ac\u5316\u5242\u7684\u50ac\u5316\u6027\u80fd<\/b><\/strong><strong><b><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-214740\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/12\/\u56fe4-2.jpg\" alt=\"\" width=\"600\" height=\"733\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/12\/\u56fe4-2.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2020\/12\/\u56fe4-2-246x300.jpg 246w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/b><\/strong><\/p>\n<p><strong><b>\u00a0<\/b><\/strong><strong><b>\u6587\u732e\u94fe\u63a5<\/b><\/strong>\uff1a\u201c<a href=\"https:\/\/science.sciencemag.org\/content\/370\/6523\/1454\"><strong><u><b>Tailored quinones support high-turnover Pd catalysts for oxidative C<\/b><\/u><\/strong><strong><u><b>&#8211;<\/b><\/u><\/strong><strong><u><b>H arylation with O<\/b><\/u><\/strong><strong><u><sub><b>2<\/b><\/sub><\/u><\/strong><\/a>\u201d(<strong><b>Science<\/b><\/strong>\uff0c<strong><b>2020<\/b><\/strong>\uff0c<strong><b>10.1126\/science.abd1085<\/b><\/strong>)<\/p>\n<p>\u672c\u6587\u7531\u6750\u6599\u4ebaCYM\u7f16\u8bd1\u4f9b\u7a3f\u3002\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1tougao@cailiaoren.com\u3002<\/p>\n<p>\u6750\u6599\u4eba\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaokefu \u3002<\/p>\n<p>&nbsp;<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u94af\u50ac\u5316\u7684\u6709\u673a\u5206\u5b50\u6c27\u5316\u53cd\u5e94\u8d77\u6e90\u4e8e1959\u5e74\uff0c\u5f53\u65f6\u7528\u4e8e\u4e59\u70ef\u548c\u6c34\u7684\u6c27\u5316\u5076\u8054\u3002\u6b64\u540e\u4e0d\u4e45\u5c31\u62a5\u9053\u4e86\u94af\u50ac\u5316\u7684\u82b3\u70c3\u4e0e\u8054\u82b3\u57fa\u7684\u6c27\u5316\u3002\u8fd9\u4e9b\u65b9\u6cd5\u7684\u8f83\u5dee\u7684\u50ac\u5316\u6548\u7387\u548c\u8f83\u4f4e\u7684\u9009\u62e9&#8230;<\/p>\n","protected":false},"author":9629,"featured_media":214737,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[155,116],"class_list":["post-214736","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-jiedu","tag-science","tag-catalyst"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/214736"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/9629"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=214736"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/214736\/revisions"}],"predecessor-version":[{"id":214741,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/214736\/revisions\/214741"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/214737"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=214736"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=214736"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=214736"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}