{"id":216551,"date":"2021-01-28T06:18:37","date_gmt":"2021-01-27T22:18:37","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=216551"},"modified":"2021-01-27T22:18:51","modified_gmt":"2021-01-27T14:18:51","slug":"%e7%ba%b3%e7%b1%b3%e7%ba%a4%e7%bb%b4%e7%b4%a0%e6%9d%90%e6%96%99%e6%88%90%e4%b8%ba%e7%a0%94%e7%a9%b6%e7%83%ad%e9%97%a8-%e8%bf%91%e4%b8%80%e4%b8%aa%e6%9c%88%e8%af%a5%e6%9d%90%e6%96%99","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=216551","title":{"rendered":"\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u6750\u6599\u6210\u4e3a\u7814\u7a76\u70ed\u95e8\u2014\u2014\u8fd1\u4e00\u4e2a\u6708\u8be5\u6750\u6599\u9891\u7e41\u51fa\u73b0\u5728\u9876\u520a\u4e0a"},"content":{"rendered":"<p><strong><b>\u3010\u5f15\u8a00\u3011<\/b><\/strong><\/p>\n<p>\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u662f\u4e00\u7c7b\u5177\u6709\u9ad8\u673a\u68b0\u6027\u80fd\u7684\u53ef\u518d\u751f\u9ad8\u7eb5\u6a2a\u6bd4\u7eb3\u7c73\u7c92\u5b50\uff0c\u5176\u8868\u9762\u5177\u6709\u5316\u5b66\u53cd\u5e94\u57fa\u56e2\u53ef\u4ee5\u5b98\u80fd\u5316\u3002\u5728\u52aa\u529b\u5f00\u53d1\u53ef\u6301\u7eed\u7684\u9ad8\u7ea7\u529f\u80fd\u6750\u6599\u65f6\uff0c\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u6700\u8fd1\u5f15\u8d77\u4e86\u5e7f\u6cdb\u7684\u5173\u6ce8\u3002\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u8303\u56f4\u4ece\u68d2\u72b6\u7684\u9ad8\u7ed3\u6676\u5ea6\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u6676\u4f53\u5230\u66f4\u957f\uff0c\u66f4\u7ea0\u7f20\u7684\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u7ea4\u7ef4\uff0c\u4e4b\u524d\u4e5f\u88ab\u79f0\u4e3a\u5fae\u7ea4\u5316\u7ea4\u7ef4\u7d20\u548c\u7ec6\u83cc\u7ea4\u7ef4\u7d20\u3002\u8fd1\u5e74\u6765\uff0c\u63a8\u52a8\u4e86\u5e7f\u6cdb\u5e94\u7528\u7684\u7814\u7a76\uff0c\u4ece\u7eb3\u7c73\u590d\u5408\u6750\u6599\uff0c\u7c98\u5ea6\u8c03\u8282\u5242\uff0c\u8584\u819c\uff0c\u963b\u9694\u5c42\uff0c\u7ea4\u7ef4\uff0c\u7ed3\u6784\u8272\uff0c\u51dd\u80f6\uff0c\u6c14\u51dd\u80f6\u548c\u6ce1\u6cab\u4ee5\u53ca\u80fd\u6e90\u5e94\u7528\u5230\u8fc7\u6ee4\u819c\u7b49\u7b49\uff0c\u5728\u6750\u6599\u65b9\u9762\u5df2\u6210\u4e3a\u79d1\u5b66\u548c\u6280\u672f\u9886\u57df\u7684\u91cd\u70b9\u9886\u57df\u3002\u6211\u4eec\u5217\u4e3e\u8fd1\u4e00\u4e2a\u6708\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u5728\u9876\u520a\u53d1\u8868\u7684\u4f18\u8d28\u6587\u7ae0\uff0c\u68b3\u7406\u8be5\u6750\u6599\u8fd1\u671f\u7684\u7814\u7a76\u8fdb\u5c55\u3002<\/p>\n<p><strong style=\"line-height: 1.5;\"><b>1. \u745e\u5178\u7687\u5bb6\u7406\u5de5\u5b66\u9662Monica Ek<\/b><\/strong><strong style=\"line-height: 1.5;\"><b>\uff08ACS Sustainable Chemistry &amp; Engineering\uff09\uff1a\u901a\u8fc7\u751f\u7269\u7cbe\u70bc\u65b9\u6cd5\u4ece\u6811\u76ae\u4e2d\u5206\u79bb\u7eb3\u7c73\u7ea4\u7ef4\u7d20\uff0c\u53ef\u7528\u4f5c\u591a\u79cd\u6750\u6599<\/b><\/strong><\/p>\n<p>\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u751f\u4ea7\u5904\u4e8e\u4e0d\u65ad\u53d1\u5c55\u7684\u72b6\u6001\uff0c\u91cd\u70b9\u5728\u4e8e\u964d\u4f4e\u751f\u4ea7\u6210\u672c\u4ee5\u53ca\u5c06\u4e0d\u540c\u7684\u5b98\u80fd\u56e2\u5f15\u5165\u7ea4\u7ef4\u7d20\u7ed3\u6784\u4e2d\u3002\u8349\u9178\u7ea4\u7ef4\u7d20\uff08COX\uff09\u662f\u901a\u8fc7\u4f7f\u7ea4\u7ef4\u7d20\u7ea4\u7ef4\u4e0e\u7194\u878d\u7684\u8349\u9178\u4e8c\u6c34\u5408\u7269\u53cd\u5e94\u800c\u5236\u5f97\u7684\uff0c\u800c\u8349\u9178\u4e8c\u6c34\u5408\u7269\u5728102\u00b0C\u65f6\u76f8\u5bf9\u8f83\u4f4e\u7684\u7194\u70b9\u4f7f\u5f97\u65e0\u6eb6\u5242\u53cd\u5e94\u6210\u4e3a\u53ef\u80fd\uff0c\u5e76\u4f7f\u8be5\u65b9\u6cd5\u6210\u4e3a\u5176\u4ed6\u65b9\u6cd5\u7684\u7eff\u8272\u66ff\u4ee3\u54c1\u3002\u53ef\u4ee5\u901a\u8fc7\u8349\u9178\u7ea4\u7ef4\u7d20\u5206\u79bb\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7528\u4e8e\u4ece\u6728\u6750\u4e2d\u6f02\u767d\u7684\u725b\u76ae\u7eb8\u6d46\u548c\u6eb6\u89e3\u6d46\uff0c\u5176\u4e2d\u5927\u90e8\u5206\u6728\u8d28\u7d20\uff0c\u534a\u7ea4\u7ef4\u7d20\u548c\u6742\u8d28\u88ab\u53bb\u9664\u3002\u800c\u5728\u6797\u4ea7\u54c1\u5de5\u4e1a\u4e2d\u751f\u4ea7\u6728\u6d46\u548c\u6750\u6599\u65f6\uff0c\u4e5f\u4f1a\u4ea7\u751f\u5927\u91cf\u526f\u4ea7\u54c1\uff0c\u5c24\u5176\u662f\u6811\u76ae\u3002\u5408\u7406\u5229\u7528\u6811\u76ae\uff0c\u5c06\u53ef\u4ee5\u4f7f\u6548\u76ca\u53d8\u5f97\u66f4\u52a0\u597d\u3002<\/p>\n<p>\u745e\u5178\u7687\u5bb6\u7406\u5de5\u5b66\u9662Monica Ek\u5e94\u7528\u751f\u7269\u7cbe\u70bc\u6982\u5ff5\uff0c\u4f7f\u7528\u4e19\u916e\u548c\u52a0\u538b\u70ed\u6c34\u8403\u53d6\u65b9\u6cd5\u5b9e\u73b0\u632a\u5a01\u4e91\u6749\u6811\u76ae\u6210\u5206\u7684\u8403\u53d6\uff0c\u63a5\u7740\u901a\u8fc7\u6e29\u548c\u7684\u8fc7\u4e59\u9178\u5904\u7406\u4f7f\u6811\u76ae\u8131\u6728\u8d28\u7d20\uff0c\u7136\u540e\u5728\u65e0\u6eb6\u5242\u7684\u53cd\u5e94\u4e2d\u751f\u6210\u8349\u9178\u7ea4\u7ef4\u7d20\uff0c\u6700\u540e\u5206\u79bb\u51fa\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u3002\u5728\u8403\u53d6\u548c\u5206\u79bb\u8fc7\u7a0b\u4e2d\u5bf9\u5176\u5316\u5b66\u6210\u5206\u548c\u70ed\u6027\u80fd\u8fdb\u884c\u4e86\u76d1\u6d4b\uff0c\u7ed3\u679c\u8868\u660e\uff0c\u8349\u9178\u7ea4\u7ef4\u7d20\u7684\u6536\u7387\u4e3a82%\uff0c\u53d6\u4ee3\u5ea6\u4e3a0.3\uff0c\u8868\u9762\u7535\u8377\u4e3a1.53 mmol g<sup>&#8211;<\/sup><sup>1<\/sup>\u3002\u5206\u79bb\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u662f\u68d2\u72b6\u7eb3\u7c73\u6676\u4f53\u548c\u7eb3\u7c73\u7ea4\u7ef4\u7684\u6df7\u5408\u7269\u3002\u6700\u540e\uff0c\u5bf9\u5206\u79bb\u5f97\u5230\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u8fdb\u884c\u4e86\u521d\u6b65\u7684\u70ed\u5206\u6790\uff0c\u663e\u793a\u51fa\u4e86\u826f\u597d\u7684\u6027\u80fd\u3002\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u5f62\u6001\u548c\u70ed\u5b66\u6027\u8d28\u4f7f\u5176\u6210\u4e3a\u4e00\u79cd\u5f88\u6709\u524d\u9014\u7684\u6750\u6599\u3002\u8be5\u6750\u6599\u6765\u81ea\u53ef\u518d\u751f\u8d44\u6e90\uff0c\u662f\u5316\u77f3\u57fa\u6750\u6599\u7684\u53ef\u6301\u7eed\u66ff\u4ee3\u4ea7\u54c1\u3002\u8349\u9178\u7ea4\u7ef4\u7d20\u53ca\u5176\u884d\u751f\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u53ef\u4ee5\u7528\u4f5c\u7eb3\u7c73\u590d\u5408\u6750\u6599\uff0c\u900f\u660e\u8584\u819c\u6216\u5316\u5986\u54c1\u4e2d\u7684\u589e\u5f3a\u5242\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216553 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72471-9.png\" alt=\"\" width=\"600\" height=\"335\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72471-9.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72471-9-300x168.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u00a0\u53c2\u8003\u6587\u732e\uff1aRietzler B and Ek M. Adding Value to Spruce Bark by the Isolation of Nanocellulose in a Biorefinery Concept. ACS Sustainable Chemistry &amp; Engineering 2021.<\/p>\n<p><strong style=\"line-height: 1.5;\"><b>2. \u9a6c\u6765\u897f\u4e9a\u77f3\u6cb9\u5927\u5b66Muhammad Moniruzzaman<\/b><\/strong><strong style=\"line-height: 1.5;\"><b>\uff08ACS Sustainable Chemistry &amp; Engineering\uff09\uff1a\u7efc\u8ff0\u2014\u2014\u79bb\u5b50\u6db2\u4f53\u4f5c\u4e3a\u751f\u7269\u8d44\u6e90\u52a0\u5de5\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u53ef\u6301\u7eed\u5e73\u53f0<\/b><\/strong><\/p>\n<p>\u5728\u8fc7\u53bb\u7684\u51e0\u5341\u5e74\u4e2d\uff0c\u5bfb\u627e\u4e0e\u77f3\u6cb9\u6765\u6e90\u73af\u5883\u53cb\u597d\u548c\u53ef\u6301\u7eed\u7684\u66ff\u4ee3\u5316\u5b66\u54c1\u548c\u6750\u6599\u7684\u9700\u6c42\u8d8a\u6765\u8d8a\u663e\u5f97\u91cd\u8981\u3002\u7eb3\u7c73\u7ea4\u7ef4\u7d20\uff08NC\uff09\u662f\u5929\u7136\u7ea4\u7ef4\u7d20\u7684\u4e00\u79cd\u4ea7\u54c1\u6216\u63d0\u53d6\u7269\uff0c\u5b58\u5728\u4e8e\u591a\u79cd\u8d44\u6e90\u4e2d\uff0c\u4f8b\u5982\u690d\u7269\uff0c\u52a8\u7269\u548c\u7ec6\u83cc\u3002\u76ee\u524dNC\u53ef\u4ee5\u6839\u636e\u5176\u5927\u5c0f\u548c\u52a0\u5de5\u65b9\u6cd5\u5206\u4e3a\u4e09\u7c7b\uff1a\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u6676\u4f53\uff08CNC\uff09\uff0c\u7eb3\u7c73\u539f\u7ea4\u5316\u7ea4\u7ef4\u7d20\uff08NFC\uff09\u548c\u7ec6\u83cc\u7eb3\u7c73\u7ea4\u7ef4\u7d20\uff08BNC\uff09\u3002\u4f46\u662f\uff0c\u9ad8\u80fd\u8017\uff0c\u4f4e\u6536\u7387\u4ee5\u53ca\u4e0e\u4f7f\u7528\u9ad8\u6d53\u5ea6\u9178\u548c\u5176\u4ed6\u5316\u5b66\u54c1\u6709\u5173\u7684\u5065\u5eb7\u548c\u73af\u5883\u5371\u5bb3\u662f\u8fd9\u4e9b\u65b9\u6cd5\u7684\u4e3b\u8981\u7f3a\u70b9\u3002\u800c\u4e14\uff0c\u9178\u6c34\u89e3\u4e25\u91cd\u6076\u5316\u4e86\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u70ed\u5b8c\u6574\u6027\uff0c\u8fd9\u5bf9\u4e8e\u7eb3\u7c73\u590d\u5408\u6750\u6599\u7684\u5236\u9020\u662f\u4e0d\u5229\u7684\u3002\u4e3a\u4e86\u89e3\u51b3\u4e0a\u8ff0\u5c40\u9650\u6027\uff0c\u7814\u7a76\u4eba\u5458\u5c06\u6ce8\u610f\u529b\u96c6\u4e2d\u5728\u5229\u7528\u79bb\u5b50\u6db2\u4f53\uff08ILs\uff09\u4f5c\u4e3aNC\u751f\u4ea7\u4e2d\u6f5c\u5728\u7684\u6eb6\u5242\uff0c\u6eb6\u80c0\u5242\u548c\u50ac\u5316\u5242\u3002<\/p>\n<p>\u9a6c\u6765\u897f\u4e9a\u77f3\u6cb9\u5927\u5b66Muhammad Moniruzzaman\u91cd\u70b9\u4ecb\u7ecd\u4e86\u79bb\u5b50\u6db2\u4f53\u8f85\u52a9\u7684\u6700\u65b0\u6280\u672f\u53d1\u5c55\uff0c\u8be5\u6280\u672f\u5df2\u6210\u529f\u5730\u7528\u4e8e\u5305\u62ec\u7ea4\u7ef4\u7d20\u751f\u7269\u8d28\u5728\u5185\u7684\u751f\u7269\u8d44\u6e90\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u52a0\u5de5\u3002\u4ece\u53ef\u518d\u751f\u8d44\u6e90\u4e2d\u8fdb\u884cNC\u8403\u53d6\u65f6\uff0c\u4f7f\u7528\u79bb\u5b50\u6db2\u4f53\uff08ILs\uff09\u4f5c\u4e3a\u5177\u6709\u51fa\u8272\u7ec4\u5408\u5316\u5b66\u591a\u6837\u6027\u548c\u72ec\u7279\u6027\u80fd\u7684\u51fa\u8272\u5316\u5408\u7269\uff0c\u6db5\u76d6\u4e8612\u79cd\u7eff\u8272\u5316\u5b66\u539f\u7406\u4e2d\u7684\u81f3\u5c112\u4e2a\u5173\u952e\u5143\u7d20\u3002\u540c\u65f6\uff0cIL\u4e5f\u53ef\u4ee5\u8bf1\u5bfc\u9ad8\u7ed3\u6676\u5ea6\u548c\u9ad8\u4ea7\u91cf\u7684\u8d85\u8584\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7ea4\u7ef4\u7684\u63d0\u53d6\u3002\u540c\u65f6\uff0cIL\u4ecb\u5bfc\u7684NC\u7684\u6f5c\u5728\u53d1\u5c55\u53ef\u4ee5\u5efa\u7acb\u5728\u57fa\u4e8e\u54aa\u5511\u7684IL\u4e0a\u3002\u5728\u4f7f\u7528IL\u8d4b\u4e88NC\u7ea4\u7ef4\u4ee5\u65b0\u529f\u80fd\u5e76\u5f00\u8f9f\u65b0\u9014\u5f84\u548c\u5e02\u573a\u7684\u8fc7\u7a0b\u4e2d\uff0c\u6b63\u5728\u53d6\u5f97\u91cd\u5927\u8fdb\u5c55\u3002\u8fdb\u800c\u8fdb\u4e00\u6b65\u63a2\u7d22IL\u7684\u65b0\u5174\u65b9\u9762\uff0c\u4f8b\u5982\u6e90\u81ea\u4f4e\u6210\u672c\u53ef\u518d\u751f\u539f\u6599\u7684\u7eb3\u7c73IL\uff0c\u518d\u52a0\u4e0a\u65b0\u9896\u7684\u56de\u6536\u6280\u672f\uff0c\u5c06\u4f7f\u5f97IL\u6709\u671b\u7528\u4e8e\u5927\u89c4\u6a21NC\u5904\u7406\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216554 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72472-9.png\" alt=\"\" width=\"600\" height=\"460\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72472-9.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72472-9-300x230.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u00a0\u53c2\u8003\u6587\u732e\uff1aHaron GAS, Mahmood H, Noh MH, Alam MZ and Moniruzzaman M. Ionic Liquids as a Sustainable Platform for Nanocellulose Processing from Bioresources: Overview and Current Status. ACS Sustainable Chemistry &amp; Engineering 2021.<\/p>\n<p><strong style=\"line-height: 1.5;\"><b>3. \u5e7f\u897f\u5927\u5b66\u9ec4\u5d07\u674f\uff08Materials Today\uff09\uff1a\u7efc\u8ff0\u2014\u2014\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u6676\u4f53\u6750\u6599\u7ed3\u6784\u5f69\u8272\u663e\u793a\u7684\u6700\u65b0\u8fdb\u5c55<\/b><\/strong><\/p>\n<p>\u7ed3\u6784\u8272\uff0c\u4e5f\u79f0\u4e3a\u7269\u7406\u8272\uff0c\u662f\u7531\u6ca1\u6709\u4efb\u4f55\u989c\u6599\u7684\u7eaf\u7269\u7406\u7ed3\u6784\u4ea7\u751f\u7684\u989c\u8272\u3002\u5e38\u89c4\u5f69\u8272\u663e\u793a\u5668\u5728\u4f7f\u7528\u67d3\u6599\u6216\u989c\u6599\u901a\u8fc7\u9009\u62e9\u6027\u5730\u5438\u6536\u548c\u53cd\u5c04\u5149\u4ea7\u751f\u5178\u578b\u989c\u8272\uff0c\u800c\u7ed3\u6784\u989c\u8272\u901a\u8fc7\u5149\u6563\u5c04\uff0c\u884d\u5c04\u548c\u5e72\u6d89\u6709\u5e8f\u7684\u7ed3\u6784\u5468\u671f\u6027\u4ea7\u751f\u7684\u3002\u4e0e\u4f7f\u7528\u67d3\u6599\u6216\u989c\u6599\u7684\u65b9\u6cd5\u76f8\u6bd4\uff0c\u7ed3\u6784\u8272\u7684\u751f\u4ea7\u5177\u6709\u591a\u4e2a\u4f18\u70b9\uff0c\u5305\u62ec\u5c06\u5149\u6e90\u8f6c\u6362\u4e3a\u989c\u8272\u7684\u9ad8\u6548\u6548\u7387\uff0c\u73af\u5883\u53cb\u597d\u6027\u4ee5\u53ca\u5982\u679c\u6750\u6599\u7684\u7ed3\u6784\u6ca1\u6709\u635f\u574f\u6216\u53d8\u5f62\u7684\u60c5\u51b5\u4e0b\u4ecd\u80fd\u4fdd\u6301\u7a33\u5b9a\u7684\u957f\u671f\u989c\u8272\u3002\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u6676\u4f53\uff08CNC\uff09\u5bf9\u73af\u5883\u65e0\u5bb3\uff0c\u5e76\u4e14\u6e90\u81ea\u690d\u7269\uff0c\u7ec6\u83cc\u6216\u88ab\u819c\u3002CNC\u63a7\u5236\u5668\u662f\u7eba\u9524\u72b6\u7eb3\u7c73\u7ea7\u6750\u6599\u7684\u72ec\u7279\u6027\u8d28\uff0c\u4f8b\u5982\u9ad8\u5f3a\u5ea6\uff0c\u9ad8\u6bd4\u8868\u9762\u79ef\uff0c\u9ad8\u7684\u70ed\u7a33\u5b9a\u6027\uff0c\u5149\u900f\u8fc7\u6027\uff0c\u751f\u7269\u964d\u89e3\u6027\uff0c\u751f\u7269\u76f8\u5bb9\u6027\u548c\u81ea\u7ec4\u88c5\u80fd\u529b\u3002\u5728\u7ed3\u6784\u5f69\u8272\u663e\u793a\u6709\u826f\u597d\u7684\u524d\u666f\u3002<\/p>\n<p>\u5e7f\u897f\u5927\u5b66\u9ec4\u5d07\u674f\u603b\u7ed3\u4e86\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u819c\u7684\u5236\u5907\u4e2d\u6d89\u53ca\u7684\u5404\u79cd\u56e0\u7d20\u5bf9\u7ed3\u6784\u989c\u8272\uff0c\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u819c\u5bf9\u73af\u5883\u56e0\u7d20\u7684\u989c\u8272\u54cd\u5e94\u4ee5\u53ca\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u6750\u6599\u5728\u663e\u8272\u9886\u57df\u4e2d\u7684\u7ed3\u6784\u8bbe\u8ba1\u7684\u5f71\u54cd\u3002\u63cf\u8ff0\u4e86\u8fd1\u5e74\u6765\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u6750\u6599\u7684\u7ed3\u6784\u7740\u8272\u9886\u57df\u7684\u8fdb\u5c55\u3002\u6700\u540e\uff0c\u8ba8\u8bba\u4e86\u5728\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u6750\u6599\u7ed3\u6784\u989c\u8272\u65b9\u9762\u9884\u671f\u7684\u672a\u6765\u53d1\u5c55\u3002\u968f\u7740\u8d8a\u6765\u8d8a\u591a\u7684\u56fd\u5bb6\u5f00\u59cb\u7981\u6b62\u4f7f\u7528\u4e00\u6b21\u6027\u5851\u6599\uff0c\u4f5c\u4e3a\u53ef\u751f\u7269\u964d\u89e3\u66ff\u4ee3\u54c1\u7684\u7ea4\u7ef4\u7d20\u57fa\u6750\u6599\u5c06\u6210\u4e3a\u66f4\u5e7f\u6cdb\u7814\u7a76\u7684\u4e3b\u9898\uff0c\u800c\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u6750\u6599\u7684\u7ed3\u6784\u989c\u8272\u5c06\u6210\u4e3a\u5404\u79cd\u5e94\u7528\u4e2d\u7684\u5173\u952e\u53c2\u6570\u4e4b\u4e00\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216555 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72473-6.png\" alt=\"\" width=\"600\" height=\"428\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72473-6.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72473-6-300x214.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u53c2\u8003\u6587\u732e\uff1aXu C, Huang C and Huang H. Recent advances in structural color display of cellulose nanocrystal materials. Applied Materials Today 2021;22:100912.<\/p>\n<p><strong style=\"line-height: 1.5;\"><b>4. \u4e1c\u4eac\u5927\u5b66Tsuguyuki Saito<\/b><\/strong><strong style=\"line-height: 1.5;\"><b>\uff08ACS Nano\uff09\uff1a\u673a\u68b0\u5f3a\u5ea6\u9ad8\uff0c\u53ef\u6269\u5c55\u7684\u4e2d\u5b54\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u5e72\u51dd\u80f6\uff0c\u5177\u6709\u900f\u5149\u6027\uff0c\u9694\u70ed\u6027\u548c\u706b\u7130\u81ea\u7184\u6027<\/b><\/strong><\/p>\n<p>\u53ef\u4f38\u7f29\u6027\u662f\u7eb3\u7c73\u7ea7\u9897\u7c92\u5206\u6563\u4f53\u7ed3\u6784\u5316\u4e2d\u7684\u666e\u904d\u6311\u6218\uff0c\u7279\u522b\u662f\u5728\u5e72\u71e5\u8fd9\u4e9b\u5206\u6563\u4f53\u4ee5\u751f\u4ea7\u529f\u80fd\u6027\u591a\u5b54\u7ed3\u6784\uff08\u5982\u6c14\u51dd\u80f6\uff09\u65f6\u3002\u4f46\u662f\u6c14\u51dd\u80f6\u7684\u751f\u4ea7\u4f9d\u8d56\u4e8e\u8d85\u4e34\u754c\u5e72\u71e5\uff0c\u4f7f\u5f97\u8868\u73b0\u51fa\u8f83\u5dee\u7684\u53ef\u6269\u5c55\u6027\u3002\u89e3\u51b3\u6b64\u53ef\u6269\u5c55\u6027\u9650\u5236\u7684\u65b9\u6cd5\u662f\u5728\u73af\u5883\u538b\u529b\u4e0b\u4f7f\u7528\u84b8\u53d1\u5e72\u71e5\u3002\u7136\u800c\uff0c\u5305\u542b\u7eb3\u7c73\u7ea7\u9897\u7c92\u7684\u6e7f\u51dd\u80f6\u7684\u84b8\u53d1\u5e72\u71e5\u4f34\u968f\u7740\u5f3a\u5927\u7684\u6bdb\u7ec6\u4f5c\u7528\u529b\u3002\u56e0\u6b64\uff0c\u751f\u4ea7\u5177\u6709\u6c14\u51dd\u80f6\u7279\u5b9a\u7ed3\u6784\u7279\u5f81\uff08\u4f8b\u5982\u4e2d\u5c3a\u5ea6\u5b54\uff0c\u9ad8\u5b54\u9699\u7387\u548c\u9ad8\u6bd4\u8868\u9762\u79ef\uff08SSA\uff09\uff09\u7684\u84b8\u53d1\u5e72\u71e5\u51dd\u80f6\u6216\u201c\u5e72\u51dd\u80f6\u201d\u5177\u6709\u6311\u6218\u6027\u3002<\/p>\n<p>\u4e1c\u4eac\u5927\u5b66Tsuguyuki Saito\u62a5\u9053\u4e86\u5177\u6709\u6770\u51fa\u7684\u673a\u68b0\u5f3a\u5ea6\uff0c\u9002\u5ea6\u7684\u900f\u5149\u6027\uff0c\u9694\u70ed\u6027\u548c\u81ea\u7184\u529f\u80fd\u7684\u5355\u5757\u7eb3\u7c73\u7ea4\u7ef4\u7d20\uff08CNF\uff09\u5e72\u51dd\u80f6\u3002\u8fd9\u79cd\u5e72\u51dd\u80f6\u662f\u901a\u8fc7\u7cbe\u7ec6\u7684CNF\u7684\u7eb3\u7c73\u7ed3\u6784\u5de5\u7a0b\u83b7\u5f97\u7684\uff0c\u5176\u5bbd\u5ea6\u4e3a2-3 nm\u3002\u901a\u8fc7TEMPO-\u6c27\u5316\u5236\u5907CNF\uff0c\u4f7f\u5f97\u5355\u4e2aCNF\u7684\u8868\u9762\u4ee5\u9ad8\u5bc6\u5ea6\u4f4d\u7f6e\u9009\u62e9\u5730\u7fa7\u5316\u3002\u7ed3\u679c\u8868\u660eCNF\u5e72\u51dd\u80f6\u7684\u591a\u529f\u80fd\u6027\uff0c\u5177\u6709\u51fa\u8272\u7684\u5f3a\u5ea6\uff08\u538b\u7f29E = 170 MPa\uff0c\u03c3= 10 MPa\uff1b\u62c9\u4f38E = 290 MPa\uff0c\u03c3= 8 MPa\uff09\uff0c\u9002\u5ea6\u7684\u900f\u5149\u6027\uff0c\u9694\u70ed\u6027\uff080.06-0.07 W m<sup>\u20131 <\/sup>K<sup>\u20131<\/sup>\uff09\uff0c\u5e76\u4e14\u5177\u6709\u706b\u7130\u81ea\u7184\u6027\u80fd\u3002\u4f5c\u4e3a\u5e72\u51dd\u80f6\u5728\u91c7\u5149\u548c\u9694\u70ed\u65b9\u9762\uff0c\u5728\u5e94\u7528\u627f\u91cd\u5899\u4f53\u6784\u4ef6\u7684\u7814\u7a76\u5177\u6709\u5e7f\u9614\u7684\u524d\u666f\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216556 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72474-6.png\" alt=\"\" width=\"600\" height=\"284\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72474-6.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72474-6-300x142.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u53c2\u8003\u6587\u732e\uff1aSakuma, W., Yamasaki, S., Fujisawa, S., et al., Mechanically Strong, Scalable, Mesoporous Xerogels of Nanocellulose Featuring Light Permeability, Thermal Insulation, and Flame Self-Extinction[J]. Acs Nano, 2021.<\/p>\n<p><strong style=\"line-height: 1.5;\"><b>5. \u5df4\u897f\u7eb3\u7c73\u6280\u672f\u56fd\u5bb6\u5b9e\u9a8c\u5ba4Juliana S. Bernardes<\/b><\/strong><strong style=\"line-height: 1.5;\"><b>\uff08Carbohydrate Polymers\uff09\uff1a\u901a\u8fc7\u9759\u7535\u7edc\u5408\u6cd5\u5236\u5907\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u6d77\u7ef5\u80fd\u6539\u5584\u5176\u673a\u68b0\u6027\u80fd<\/b><\/strong><\/p>\n<p>\u5bf9\u5229\u7528\u751f\u7269\u8d28\u751f\u4ea7\u6750\u6599\u4ee5\u53d1\u5c55\u5bf9\u73af\u5883\u5f71\u54cd\u8f83\u5c0f\u7684\u53ef\u6301\u7eed\u672a\u6765\u7684\u5174\u8da3\u6b63\u5728\u8fc5\u901f\u589e\u957f\u3002\u7136\u800c\uff0c\u66f4\u73af\u4fdd\u7684\u6750\u6599\u9762\u4e34\u7740\u4e0e\u5b83\u4eec\u7684\u5185\u5728\u7279\u6027\u76f8\u5173\u7684\u6311\u6218\uff0c\u8fd9\u4e9b\u7279\u6027\u5728\u673a\u68b0\u6027\u80fd\u548c\u8010\u6c34\u6027\u65b9\u9762\u4e0e\u6cb9\u6027\u5851\u6599\u7684\u7279\u6027\u5927\u4e0d\u76f8\u540c\u3002\u800c\u5728\u6c34\u6027\u4ecb\u8d28\u4e2d\u751f\u7269\u57fa\u7ec4\u5206\u7684\u8d85\u5206\u5b50\u7ec4\u88c5\u662f\u4e00\u79cd\u6709\u524d\u9014\u7684\u7b56\u7565\uff0c\u53ef\u4ee5\u514b\u670d\u5236\u5907\u5177\u6709\u6240\u9700\u7279\u6027\u7684\u6750\u6599\u4e2d\u7684\u67d0\u4e9b\u7f3a\u70b9\u3002\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u662f\u5236\u5907\u5404\u79cd\u591a\u529f\u80fd\u751f\u7269\u57fa\u6750\u6599\u7684\u4f18\u79c0\u5019\u9009\u6750\u6599\uff0c\u5982\u819c\u3001\u6ce1\u6cab\u3001\u6c34\u51dd\u80f6\u548c\u7eb3\u7c73\u7c92\u5b50\u7b49\u7b49\u3002<\/p>\n<p>\u5df4\u897f\u7eb3\u7c73\u6280\u672f\u56fd\u5bb6\u5b9e\u9a8c\u5ba4Juliana S. Bernardes\u901a\u8fc7\u7b80\u5355\u7684\u9759\u7535\u7edc\u5408\u6cd5\u5236\u5907\u4e86\u9633\u79bb\u5b50\u548c\u9634\u79bb\u5b50\u578b\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u6d77\u7ef5\uff08CNF\uff09\u3002\u5c0f\u89d2\u5ea6x\u5c04\u7ebf\u6563\u5c04\u548c\u4f4e\u6e29\u900f\u5c04\u7535\u5b50\u663e\u5fae\u955c\u5b9e\u9a8c\u8868\u660e\uff0c\u5e26\u76f8\u53cd\u7535\u8377\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u60ac\u7f6e\u662f\u7ea0\u7f20\u7ea4\u7ef4\u56e2\u7c07\u548c\u7f51\u7edc\u7684\u6df7\u5408\u7269\u3002\u8fd9\u4e9b\u7ed3\u6784\u4e4b\u95f4\u7684\u5e73\u8861\u51b3\u5b9a\u4e86CNF\u5728\u6c34\u4e2d\u7684\u80f6\u4f53\u7a33\u5b9a\u6027\u548c\u6d41\u53d8\u6027\u80fd\u3002\u5728\u8d28\u91cf\u6210\u5206\u4e3a1:1 (\u7ea60.12 MPa)\u65f6\uff0c\u7531\u60ac\u6d6e\u4f53\u5236\u5907\u7684\u6d77\u7ef5\u7684\u538b\u7f29\u6a21\u91cf\u8fbe\u5230\u6700\u5927\u503c\uff0c\u5e76\u5728\u6750\u6599\u4e2d\u8d77\u5230\u4e86\u52a0\u5f3a\u7ed3\u6784\u7684\u4f5c\u7528\u3002\u9664\u4e86\u9759\u7535\u5438\u5f15\u5916\uff0c\u805a\u7c7b\u5185\u90e8\u8fd8\u53ef\u80fd\u53d1\u751f\u6c22\u952e\u548c\u758f\u6c34\u63a5\u89e6\uff0c\u63d0\u9ad8\u4e86\u9633\u79bb\u5b50\u6ce1\u6cab\u7684\u6c34\u7a33\u5b9a\u6027\u3002\u8fd9\u4e9b\u7ed3\u679c\u53ef\u4e3a\u5f00\u53d1\u5728\u6c34\u4e2d\u5236\u5907\u65e0\u6bd2\u5316\u5b66\u54c1\u7684\u575a\u56fa\u5168\u7ea4\u7ef4\u7d20\u6750\u6599\u63d0\u4f9b\u57fa\u7840\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216557 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72475-6.png\" alt=\"\" width=\"600\" height=\"196\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72475-6.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72475-6-300x98.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u53c2\u8003\u6587\u732e\uff1aMariano M, Souza SF, Borges AC, do Nascimento DM and Bernardes JS. Tailoring strength of nanocellulose foams by electrostatic complexation. Carbohydrate Polymers 2021;256:117547.<\/p>\n<p><strong style=\"line-height: 1.5;\"><b>6. \u4e2d\u56fd\u79d1\u5b66\u6280\u672f\u5927\u5b66\u5434\u6052\u5b89<\/b><\/strong><strong style=\"line-height: 1.5;\"><b>\uff08<\/b><\/strong><a style=\"line-height: 1.5;\" href=\"https:\/\/www.x-mol.com\/paper\/1344031783115563008?adv\"><strong><b>ACS Nano<\/b><\/strong><\/a><strong style=\"line-height: 1.5;\"><b>\uff09\uff1a\u901a\u8fc7\u6e7f\u5ea6\u4ecb\u5bfc\u7684\u754c\u9762\u5f3a\u5316\u548c\u589e\u97e7\u5206\u7ea7\u7eb3\u7c73\u7ea4\u7ef4\u7d20<\/b><\/strong><\/p>\n<p>\u5851\u6599\u5e9f\u6599\u548c\u5fae\u5851\u6599\u5bf9\u751f\u6001\u73af\u5883\u548c\u4eba\u7c7b\u5065\u5eb7\u6784\u6210\u4e86\u5de8\u5927\u5a01\u80c1\u3002 \u4ece\u53ef\u6301\u7eed\u53d1\u5c55\u7684\u89d2\u5ea6\u6765\u770b\uff0c\u7531\u4e8e\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u5177\u6709\u53ef\u518d\u751f\u548c\u53ef\u751f\u7269\u964d\u89e3\u7684\u7279\u6027\uff0c\u4ee5\u53ca\u975e\u51e1\u7684\u673a\u68b0\u6027\u80fd\u548c\u53ef\u8c03\u8282\u7684\u8868\u9762\u5316\u5b66\u6027\u8d28\uff0c\u662f\u6781\u597d\u7684\u66ff\u4ee3\u54c1\u3002\u4f46\u662f\u6e7f\u5ea6\u4f1a\u5bfc\u81f4\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u65e0\u6cd5\u63a7\u5236\u7684\u53d8\u5f62\u548c\u673a\u68b0\u4e0b\u964d\uff0c\u6240\u4ee5\u901a\u5e38\u8ba4\u4e3a\u5b83\u662f\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u57fa\u6750\u6599\u7684\u4e00\u4e2a\u7f3a\u70b9\u3002\u4f46\u662f\uff0c\u7531\u4e8e\u7f3a\u4e4f\u5bf9\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u754c\u9762\u884c\u4e3a\u7684\u6df1\u5165\u4e86\u89e3\uff0c\u7279\u522b\u662f\u5728\u53d8\u5316\u7684\u76f8\u5bf9\u6e7f\u5ea6\u4e0b\uff0c\u96be\u4ee5\u7ef4\u6301\u7ea4\u7ef4\u7d20\u57fa\u6750\u6599\u7684\u9884\u671f\u6027\u80fd\u3002<\/p>\n<p>\u4e2d\u56fd\u79d1\u5b66\u6280\u672f\u5927\u5b66\u5434\u6052\u5b89\u7ed3\u5408\u4e86\u5bc6\u5ea6\u6cdb\u51fd\u7406\u8bba\uff08DFT\uff09\u8ba1\u7b97\u548cMD\u6a21\u62df\uff0c\u7814\u7a76\u4e86\u5206\u7ea7\u7eb3\u7c73\u7ea4\u7ef4\u7d20\uff08CNC\uff09\u4e2d\u6e7f\u5ea6\u4ecb\u5bfc\u7684\u754c\u9762\u4ee5\u53ca\u76f8\u5173\u7684\u591a\u5c3a\u5ea6\u53d8\u5f62\u884c\u4e3a\u3002\u5728CNC\u754c\u9762\u5904\u6355\u83b7\u7684\u6c34\u5206\u5b50\u548c\u76f8\u5173\u7684\u6c22\u952e\u7ade\u4e89\u89e6\u53d1\u4e86\u6ed1\u52a8\u754c\u9762\u7684\u5f62\u6210\u4ee5\u53ca\u5206\u5c42\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u975e\u5f39\u6027\u53d8\u5f62\u3002\u5728\u5206\u5b50\u6c34\u5e73\u4e0a\u8be6\u7ec6\u8ba8\u8bba\u4e86\u5e94\u53d8\u786c\u5316\u9636\u6bb5\u548c\u53d8\u5f62\u673a\u7406\u3002\u6700\u540e\uff0c\u5728\u4e0d\u540c\u7684\u76f8\u5bf9\u6e7f\u5ea6\u4e0b\u8fdb\u884c\u4e86CNC\u8584\u819c\u7684\u529b\u5b66\u5b9e\u9a8c\uff0c\u4ee5\u9a8c\u8bc1\u5b8f\u89c2\u5c3a\u5ea6\u4e0a\u7684\u975e\u5f39\u6027\u53d8\u5f62\u884c\u4e3a\u3002\u901a\u8fc7\u4eff\u771f\u548c\u5b9e\u9a8c\u8868\u660e\uff0c\u6e7f\u5ea6\u4ecb\u5bfc\u7684\u754c\u9762\u53ef\u4ee5\u4fc3\u8fdb\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u673a\u68b0\u589e\u5f3a\u3002\u6a21\u62df\u548c\u5b9e\u9a8c\u4e3a\u8003\u8651\u4e0d\u540c\u6e7f\u5ea6\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u673a\u68b0\u54cd\u5e94\u63d0\u4f9b\u4e86\u53c2\u8003\uff0c\u8fd9\u5bf9\u4e8e\u901a\u8fc7\u754c\u9762\u8bbe\u8ba1\u83b7\u5f97\u9ad8\u6027\u80fd\u7ea4\u7ef4\u7d20\u57fa\u6750\u6599\u5177\u6709\u91cd\u8981\u610f\u4e49\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216558 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72476-5.png\" alt=\"\" width=\"600\" height=\"291\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72476-5.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72476-5-300x146.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u53c2\u8003\u6587\u732e\uff1aHou Y, Guan Q-F, Xia J, Ling Z-C, He Z, Han Z-M, et al. Strengthening and Toughening Hierarchical Nanocellulose via Humidity-Mediated Interface. ACS Nano 2020.<\/p>\n<p><strong style=\"line-height: 1.5;\"><b>7. \u5c71\u4e1c\u5927\u5b66\u5218\u5b8f<\/b><\/strong><strong style=\"line-height: 1.5;\"><b>\uff08Advanced Healthcare Materials\uff09\uff1a\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u589e\u5f3a\u7f9f\u57fa\u78f7\u7070\u77f3\u7eb3\u7c73\u5e26\u819c\u4f5c\u4e3a\u5e72\u7ec6\u80de\u591a\u7cfb\u5206\u5316\u5e73\u53f0\uff0c\u7528\u4e8e\u4f53\u5916\u4eff\u751f\u6784\u5efa\u751f\u7269\u6d3b\u60273D\u7c7b\u56fa\u9187\u7ec4\u7ec7\u3002<\/b><\/strong><\/p>\n<p>\u4e25\u91cd\u9aa8\u7f3a\u635f\u7684\u4e34\u5e8a\u6cbb\u7597\uff0c\u5c24\u5176\u662f\u8840\u7ba1\u548c\u5468\u56f4\u795e\u7ecf\u635f\u4f24\u5f15\u8d77\u7684\u7ec4\u7ec7\u635f\u4f24\uff0c\u4ecd\u7136\u662f\u4e00\u4e2a\u5de8\u5927\u7684\u6311\u6218\uff0c\u5e38\u5e38\u5bfc\u81f4\u9aa8\u4e0d\u6108\u5408\u548c\u5176\u4ed6\u540e\u9057\u75c7\u3002\u56e0\u6b64\uff0c\u652f\u67b6\u88ab\u8bbe\u8ba1\u6210\u6a21\u62df\u5929\u7136\u7ec4\u7ec7\uff0c\u53ef\u5728\u4e0b\u4e00\u4ee3\u7ec4\u7ec7\u5de5\u7a0b\u4e2d\u4f7f\u7528\u3002\u540c\u65f6\u4e0e\u9aa8\u9abc\u7ec4\u7ec7\u5de5\u7a0b\u652f\u67b6\u76f8\u5173\u7684\u5927\u591a\u6570\u7814\u7a76\u90fd\u96c6\u4e2d\u5728\u6210\u9aa8\u7ec6\u80de\u7684\u5206\u5316\u4e0a\uff0c\u56e0\u4e3a\u4fc3\u8fdb\u65b0\u7684\u9aa8\u9abc\u751f\u957f\u662f\u9aa8\u9abc\u518d\u751f\u7684\u4e3b\u8981\u76ee\u6807\u3002\u7f9f\u57fa\u78f7\u7070\u77f3\uff08HAp\uff09\u662f\u9aa8\u9abc\u7ec4\u7ec7\u7684\u91cd\u8981\u65e0\u673a\u6210\u5206\uff0c\u5df2\u5e7f\u6cdb\u5e94\u7528\u4e8e\u9aa8\u9abc\u518d\u751f\uff0c\u836f\u7269\u8f7d\u4f53\u7cfb\u7edf\uff0c\u80bf\u7624\u6cbb\u7597\u548c\u7ec6\u80de\u6210\u50cf\u7b49\u9886\u57df\u3002\u7ec6\u83cc\u7eb3\u7c73\u7ea4\u7ef4\u7d20\uff08BNC\uff09\uff0c\u53ef\u751f\u7269\u964d\u89e3\u7684\u6750\u6599\u7684\u4eb2\u6c34\u6027\u548c\u4f18\u5f02\u7684\u8f7d\u836f\u91cf\u548c\u673a\u68b0\u6027\u80fd\uff0c\u5df2\u5728\u4f53\u5916\u5728\u4f24\u53e3\u6108\u5408\uff0c\u836f\u7269\u9012\u9001\uff0c\u4ee5\u53ca\u4eff\u751f\u7ec4\u7ec7\u6a21\u578b\u7684\u91cd\u6784\u5e94\u7528\u3002\u8003\u8651\u7684BNC\u548c\u6709\u6548\u6210\u9aa8\u80fd\u529b\u548cHAP\u7684\u5f3a\u5ea6\u7684\u663e\u7740\u7684\u7279\u6027\uff0c\u4e24\u8005\u96c6\u6210\u7528\u4e8e\u9aa8\u9abc\u518d\u751f\u652f\u67b6\u662f\u4e00\u79cd\u5f88\u6709\u524d\u9014\u7684\u7b56\u7565\u3002<\/p>\n<p>\u5c71\u4e1c\u5927\u5b66\u5218\u5b8f\u6210\u529f\u5730\u6784\u5efa\u4e86\u6210\u9aa8\/\u795e\u7ecf\u5206\u5316\u548c\u8840\u7ba1\u751f\u6210\u591a\u5206\u5316\u589e\u5f3a\u5e73\u53f0\uff0c\u7528\u4e8e\u5728HApNB-BNC\u6df7\u5408\u819c\u4e0a\u4fee\u590d\u548c\u91cd\u5efa\u4eff\u751f\u7c7b\u9aa8\u7ec4\u7ec7\u7684\u9aa8\u3002\u5728\u5408\u6210\u8d85\u8fc7100 \u00b5m\u7684HApNB\u540e\uff0c\u5c06HApNB\u7ec4\u88c5\u5230\u7ea4\u7ef4\u7d20\u6c34\u51dd\u80f6\u4e2d\u6784\u5efa\u7684\u6742\u5316\u819c\u663e\u7740\u6539\u5584\u4e86\u5176\u673a\u68b0\u6027\u80fd\uff0c\u4eb2\u6c34\u6027\u548c\u8f7d\u836f\u6027\u80fd\uff0c\u4e3a\u6742\u5316\u819c\u5728\u7ec4\u7ec7\u5de5\u7a0b\u4e2d\u7684\u5e94\u7528\u5960\u5b9a\u4e86\u575a\u5b9e\u7684\u57fa\u7840\u3002\u800c\u4e14\u52a8\u7269\u5b9e\u9a8c\u7ed3\u679c\u8868\u660e\uff0cHApNB-BNC\u751f\u7269\u819c\u5177\u6709\u51fa\u8272\u7684\u4fee\u590d\u80fd\u529b\uff0c\u6709\u8da3\u7684\u662f\uff0c\u88c5\u6709\u751f\u957f\u56e0\u5b50\u7684\u5e73\u53f0\u53ef\u901a\u8fc7\u4f53\u5185\u9aa8\u9abc\uff0c\u8840\u7ba1\u548c\u795e\u7ecf\u7684\u5feb\u901f\u751f\u957f\u8fdb\u4e00\u6b65\u6539\u5584\u9aa8\u9abc\u4fee\u590d\u548c\u518d\u751f\u3002\u8fd9\u79cd\u589e\u5f3a\u5206\u5316\u7684\u5e73\u53f0\u7b56\u7565\u4e3a\u7c7b\u9aa8\u7ec4\u7ec7\u63d0\u4f9b\u4e86\u4e00\u79cd\u6613\u4e8e\u64cd\u4f5c\u7684\u65b0\u9896\u6784\u9020\u65b9\u6cd5\uff0c\u4e3a\u9aa8\u518d\u751f\u7684\u4e34\u5e8a\u6cbb\u7597\u65b9\u6cd5\u94fa\u5e73\u4e86\u9053\u8def\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216559 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72477-4.png\" alt=\"\" width=\"600\" height=\"333\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72477-4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72477-4-300x167.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u53c2\u8003\u6587\u732e\uff1aLiu, F., Wei, B., Xu, X., Ma, B., Zhang, S., Duan, J., Kong, Y., Yang, H., Sang, Y., Wang, S., Tang, W., Liu, C., Liu, H., Nanocellulose\u2010Reinforced Hydroxyapatite Nanobelt Membrane as a Stem Cell Multi\u2010Lineage Differentiation Platform for Biomimetic Construction of Bioactive 3D Osteoid Tissue In Vitro. Adv. Healthcare Mater. 2020, 2001851.<\/p>\n<p><strong style=\"line-height: 1.5;\"><b>8. \u7f8e\u56fd\u5317\u5361\u7f57\u6765\u7eb3\u5927\u5b66Saad A.Khan\uff08Journal of Colloid and Interface Science \uff09\uff1a\u7531\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u548c\u7eb3\u7c73\u7532\u58f3\u8d28\u5f62\u6210\u7684\u7f14\u5408\u7ed3\u6784\u5177\u6709pH\u54cd\u5e94\u80fd\u529b\uff0c\u5e76\u5177\u6709\u53ef\u8c03\u8282\u7684\u6d41\u53d8\u6027<\/b><\/strong><\/p>\n<p>\u751f\u7269\u57fa\u7eb3\u7c73\u6750\u6599\u662f\u4e00\u4e2a\u6d3b\u8dc3\u4e14\u4e0d\u65ad\u53d1\u5c55\u7684\u7814\u7a76\u8bfe\u9898\uff0c\u7279\u522b\u662f\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u548c\u5176\u7c7b\u4f3c\u548c\u4e92\u8865\u7684\u7279\u6027\u7684\u7eb3\u7c73\u7532\u58f3\u7d20\u3002\u5bf9\u8fd9\u4e9b\u6750\u6599\u7684\u5174\u8da3\u4e3b\u8981\u7531\u4e24\u4e2a\u56e0\u7d20\u9a71\u52a8\u3002\u9996\u5148\uff0c\u6709\u53ef\u4ee5\u589e\u52a0\u751f\u7269\u57fa\u7ec4\u4ef6\u7684\u5229\u7528\uff0c\u4ece\u800c\u51cf\u5c11\u5bf9\u73af\u5883\u7684\u8d1f\u9762\u5f71\u54cd\uff0c\u5982\u5bf9\u4e00\u6b21\u6027\u5851\u6599\u7684\u4f9d\u8d56\u3001\u5bf9\u5316\u77f3\u71c3\u6599\u7684\u4f9d\u8d56\u4ee5\u53ca\u4f7f\u7528\u82db\u523b\u7684\u6eb6\u5242\u548c\u8bd5\u5242\u3002\u7b2c\u4e8c\uff0c\u8fd9\u7c7b\u6750\u6599\u7531\u4e8e\u5176\u53ef\u8c03\u7684\u8868\u9762\u5316\u5b66\u548c\u5f62\u8c8c\u800c\u5448\u73b0\u51fa\u8bb8\u591a\u4f18\u70b9\uff0c\u4f7f\u5b83\u4eec\u6210\u4e3a\u8bb8\u591a\u4e0d\u540c\u5e94\u7528\u7684\u8bf1\u4eba\u5019\u9009\u6750\u6599\u3002\u56e0\u6b64\uff0c\u5b83\u4eec\u88ab\u5e94\u7528\u4e8e\u533b\u7597\u7528\u9014\u3001\u51c0\u6c34\u3001\u4e73\u6db2\u7a33\u5b9a\u7b49\u8bb8\u591a\u9886\u57df\uff0c\u5e76\u53d6\u5f97\u4e86\u5de8\u5927\u7684\u6210\u529f\u3002\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u548c\u7eb3\u7c73\u7532\u58f3\u8d28\u90fd\u662f\u5177\u6709\u4e92\u8865\u7ed3\u6784\u548c\u7279\u6027\u7684\u751f\u7269\u57fa\u6750\u6599\u3002\u4e24\u8005\u5747\u663e\u793a\u51fa\u4e0epH\u6709\u5173\u7684\u8868\u9762\u7535\u8377\uff0c\u5176\u7b26\u53f7\u76f8\u53cd\u3002\u56e0\u6b64\uff0c\u5e94\u8be5\u6709\u53ef\u80fd\u5728\u89c4\u5b9a\u7684pH\u6761\u4ef6\u4e0b\u901a\u8fc7\u79bb\u5b50\u952e\u5f62\u6210\u6765\u64cd\u7eb5\u5b83\u4eec\u4ee5\u5f62\u6210\u590d\u6742\u7684\u7ed3\u6784\u3002<\/p>\n<p>\u7f8e\u56fd\u5317\u5361\u7f57\u6765\u7eb3\u5927\u5b66Saad A.Khan\u901a\u8fc7\u5728\u66b4\u9732\u4e8e\u9178\u6027\u6216\u4e2d\u6027\u6761\u4ef6\u540e\uff0c\u5c06\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u548c\u7eb3\u7c73\u7532\u58f3\u8d28\u6df7\u5408\uff0c\u4ee5\u5f71\u54cd\u5176\u7535\u79bb\u72b6\u6001\u3002\u5982\u4f55\u901a\u8fc7\u7b49\u6e29\u6ef4\u5b9a\u91cf\u70ed\u6cd5\u76d1\u6d4b\u5c06\u7eb3\u7c73\u58f3\u591a\u7cd6\u5f15\u5165\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u8fc7\u7a0b\u4e2d\u7684\u76f8\u4e92\u4f5c\u7528\u70ed\u3002\u6700\u540e\u901a\u8fc7\u6d41\u53d8\u5b66\u6d4b\u91cf\u8868\u5f81\u6240\u5f97\u7ed3\u6784\u7684\u5f3a\u5ea6\u548c\u51dd\u80f6\u6027\u8d28\u3002\u53d1\u73b0\u5728\u8bbe\u8ba1\u7684\u6742\u5316\u7cfb\u7edf\u4e2d\u5f97\u5230\u7684\u51dd\u80f6\u6027\u8d28\u76f4\u63a5\u53d6\u51b3\u4e8e\u8d77\u59cb\u6750\u6599\u7684\u7535\u8377\u72b6\u6001\uff0c\u800c\u8fd9\u53ef\u4ee5\u7531pH\u8c03\u8282\u6765\u51b3\u5b9a\u3002\u5728\u4e0d\u540c\u6761\u4ef6\u4e0b\uff08pH\uff0c\u6d53\u5ea6\uff0c\u7eb3\u7c73\u7532\u58f3\u7d20\u4e0e\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u6bd4\u4f8b\uff09\u4f1a\u5f71\u54cd\u4e0d\u540c\u7684\u7c92\u5b50\u95f4\u76f8\u4e92\u4f5c\u7528\uff0c\u5305\u62ec\u79bb\u5b50\u5438\u5f15\uff0c\u758f\u6c34\u7f14\u5408\u548c\u7269\u7406\u7f20\u7ed3\u3002\u800c\u4e14\u4e2d\u548c\u7684\u7532\u58f3\u7d20\u4e0e\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u4e4b\u95f4\u7684\u758f\u6c34\u7f14\u5408\u5f3a\u70c8\u5730\u6709\u52a9\u4e8e\u589e\u52a0\u5f39\u6027\u6a21\u91cf\u503c\u3002\u79bb\u5b50\u7edc\u5408\u7269\u5728\u66f4\u5bbd\u7684pH\u6761\u4ef6\u4e0b\u63d0\u4f9b\u4e86\u589e\u5f3a\u7684\u7a33\u5b9a\u6027\uff0c\u800c\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u7269\u7406\u7f20\u7ed3\u662f\u6240\u6709\u7cfb\u7edf\u4e2d\u7684\u91cd\u8981\u589e\u7a20\u673a\u7406\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216560 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72478-4.png\" alt=\"\" width=\"600\" height=\"332\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72478-4.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72478-4-300x166.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u53c2\u8003\u6587\u732e\uff1aFacchine EG, Bai L, Rojas OJ and Khan SA. Associative structures formed from cellulose nanofibrils and nanochitins are pH-responsive and exhibit tunable rheology. Journal of Colloid and Interface Science 2021;588:232-241.<\/p>\n<p><strong style=\"line-height: 1.5;\"><b>9. \u6b66\u6c49\u5927\u5b66\u5e38\u6625\u96e8\uff08ACS Nano\uff09\uff1a\u7efc\u8ff0\u2014\u2014\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u5728\u805a\u5408\u7269\u57fa\u8d28\u4e2d\u53ef\u63a7\u6392\u5217\u7684\u6700\u65b0\u8fdb\u5c55<\/b><\/strong><\/p>\n<p>\u4e3a\u4e86\u5e94\u5bf9\u5168\u7403\u6c14\u5019\u53d8\u5316\u548c\u5851\u6599\u6c61\u67d3\uff0c\u800c\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7531\u4e8e\u5177\u6709\u4e8c\u6c27\u5316\u78b3\u79ef\u7d2f\u7684\u7279\u6027\uff0c\u9884\u8ba1\u672c\u4e16\u7eaa\u5c06\u88ab\u7528\u4e8e\u5236\u9020\u9ad8\u79d1\u6280\u6750\u6599\u548c\u4ea7\u54c1\u3002\u800c\u4e14\u53ef\u4ee5\u4f7f\u7528\u5404\u79cd\u7c7b\u578b\u7684\u6765\u6e90\uff0c\u4f8b\u5982\u690d\u7269\uff0c\u6d77\u6d0b\u52a8\u7269\uff08\u88ab\u819c\uff09\u548c\u7ec6\u83cc\uff0c\u901a\u8fc7\u5404\u79cd\u63d0\u53d6\u8fc7\u7a0b\uff08\u4f8b\u5982\u9178\u6c34\u89e3\uff0c\u673a\u68b0\u5904\u7406\uff0c\u9176\u6c34\u89e3\uff0c\u6c27\u5316\u65b9\u6cd5\u548c\u79bb\u5b50\u6db2\u4f53\u5904\u7406\uff09\u6765\u884d\u751f\u5177\u6709\u4e0d\u540c\u5f62\u6001\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u3002\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u4f4e\u5bc6\u5ea6\u548c\u9ad8\u5f39\u6027\u6a21\u91cf\u4f7f\u5176\u6210\u4e3a\u66ff\u4ee3\u4f20\u7edf\u589e\u5f3a\u5242\u4ee5\u5236\u5907\u575a\u56fa\uff0c\u8f7b\u5de7\u7684\u7eb3\u7c73\u590d\u5408\u6750\u6599\u7684\u7406\u60f3\u9009\u62e9\u3002\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u5177\u6709\u5f88\u5f3a\u7684\u81ea\u805a\u96c6\u503e\u5411\uff0c\u5176\u586b\u6599\u4e0e\u805a\u5408\u7269\u57fa\u4f53\u7684\u754c\u9762\u76f8\u5bb9\u6027\u662f\u83b7\u5f97\u9ad8\u6027\u80fd\u7eb3\u7c73\u590d\u5408\u6750\u6599\u7684\u4e3b\u8981\u6311\u6218\u3002<\/p>\n<p>\u6b66\u6c49\u5927\u5b66\u5e38\u6625\u96e8\u6982\u8ff0\u4e86\u5305\u542b\u9ad8\u5ea6\u6709\u5e8f\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u7eb3\u7c73\u590d\u5408\u6750\u6599\u7684\u6700\u65b0\u8fdb\u5c55\uff0c\u4ece\u5176\u6709\u5229\u7684\u7ed3\u6784-\u6027\u8d28\u5173\u7cfb\u8f6c\u53d8\u4e3a\u6f5c\u5728\u7684\u5e94\u7528\u3002\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u5728\u805a\u5408\u7269\u57fa\u4f53\u4e2d\u7684\u6392\u5217\u51b3\u5b9a\u4e86\u7eb3\u7c73\u590d\u5408\u6750\u6599\u7684\u6574\u4f53\u6027\u80fd\u3002\u672c\u6587\u7efc\u8ff0\u4e86\u4e09\u79cd\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u6392\u5217\u53ef\u63a7\u7684\u7eb3\u7c73\u590d\u5408\u6750\u6599(\u53d6\u5411\u3001\u87ba\u65cb\u548c\u68af\u5ea6)\uff0c\u4e3a\u65b0\u4e00\u4ee3\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u57fa\u529f\u80fd\u590d\u5408\u6750\u6599\u7684\u53d1\u5c55\u63d0\u4f9b\u601d\u8def\u3002\u5c3d\u7ba1\u9ad8\u53d6\u5411\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u590d\u5408\u6750\u6599\u7684\u5236\u5907\u65b9\u6cd5\u591a\u79cd\u591a\u6837(\u7535\u573a\/\u78c1\u573a\u3001\u62c9\u4f38\/\u526a\u5207\u529b\u548c\u6a21\u677f)\uff0c\u4f46\u8fd9\u4e9b\u5404\u5411\u5f02\u6027\u6750\u6599\u7684\u5b9e\u9645\u5e94\u7528\u4ecd\u5177\u6709\u6311\u6218\u6027\u3002\u6b64\u5916\uff0c\u5c06\u87ba\u65cb\u72b6\u5206\u5e03\u7684cnc\u6574\u5408\u5230\u805a\u5408\u7269\u57fa\u4f53\u4e2d\uff0c\u4f7f\u5f97\u7eb3\u7c73\u590d\u5408\u6750\u6599\u80fd\u591f\u901a\u8fc7\u663e\u793a\u53ef\u9006\u7684\u989c\u8272\u53d8\u5316\uff0c\u5728\u6f6e\u6e7f\u73af\u5883\u6216\u5e94\u53d8\u4f20\u611f\u5668\u4e2d\u5177\u6709\u6f5c\u5728\u7684\u5e94\u7528\u524d\u666f\u3002\u6700\u540e\uff0c\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u68af\u5ea6\u5206\u5e03\u7eb3\u7c73\u590d\u5408\u6750\u6599\u7684\u8bbe\u8ba1\u548c\u5236\u5907\u4e3a\u5f00\u53d1\u65b0\u578b\u8f6f\u81f4\u52a8\u5668\u63d0\u4f9b\u4e86\u673a\u4f1a\u3002\u5f53\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u4e0d\u5bf9\u79f0\u5730\u5f15\u5165\u73af\u5883\u54cd\u5e94\u6027\u805a\u5408\u7269\u57fa\u4f53\u4e2d\u65f6\uff0c\u7eb3\u7c73\u590d\u5408\u6750\u6599\u7684\u81a8\u80c0\u548c\u6eb6\u80c0\u5728\u73af\u5883\u523a\u6fc0\u4e0b\u53ef\u4ee5\u8f6c\u5316\u4e3a\u62c9\u4f38\/\u6536\u7f29\u3001\u5f2f\u66f2\u548c\u65cb\u8f6c\u7b49\u5404\u79cd\u53d8\u5f62\u3002\u7531\u6b64\uff0c\u4f5c\u8005\u7ed9\u51fa\u4e86\u4e09\u4e2a\u5efa\u8bae\uff1a1.\u5408\u7406\u5b89\u6392\u5de5\u4e1a\u751f\u4ea7\u529f\u80fd\u826f\u597d\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u662f\u672a\u6765\u53d1\u5c55\u7684\u5173\u952e\u30022.\u5728\u8003\u8651\u6269\u5927\u751f\u4ea7\u89c4\u6a21\u65f6\uff0c\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u6210\u672c\u548c\u8d28\u91cf\u4e5f\u662f\u91cd\u8981\u56e0\u7d20\u30023.\u5728\u672a\u6765\u7684\u7814\u7a76\u4e2d\u9700\u8981\u4ed4\u7ec6\u7814\u7a76\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u547d\u8fd0\u548c\u98ce\u9669\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216561 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72479-3.png\" alt=\"\" width=\"561\" height=\"562\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72479-3.png 561w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72479-3-150x150.png 150w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u72479-3-300x300.png 300w\" sizes=\"(max-width: 561px) 100vw, 561px\" \/><\/p>\n<p>\u53c2\u8003\u6587\u732e\uff1aPeng N, Huang D, Gong C, Wang Y, Zhou J and Chang C. Controlled Arrangement of Nanocellulose in Polymeric Matrix: From Reinforcement to Functionality. ACS Nano 2020;14:16169-16179.<\/p>\n<p><strong>10.\u00a0<\/strong><strong style=\"line-height: 1.5;\"><b>\u82ac\u5170\u963f\u5c14\u6258\u5927\u5b66Stina Gr\u00f6nqvist\uff08ACS Sustainable Chemistry &amp; Engineering\uff09\uff1a\u9176\u4fc3\u539f\u7ea4\u5316\u4e0e\u6e29\u548c\u673a\u68b0\u5904\u7406\u76f8\u7ed3\u5408\u751f\u4ea7\u9ad8\u56fa\u4f53\u542b\u91cf\u7eb3\u7c73\u7ea4\u7ef4\u7d20<\/b><\/strong><\/p>\n<p>\u4eba\u4eec\u5bf9\u751f\u7269\u57fa\uff08\u5c24\u5176\u662f\u690d\u7269\u6765\u6e90\u7684\uff09\u7eb3\u7c73\u7ea7\u6750\u6599\u7684\u5174\u8da3\u4e0e\u65e5\u4ff1\u589e\uff0c\u8fd9\u4e0d\u4ec5\u662f\u56e0\u4e3a\u5b83\u4eec\u5177\u6709\u53ef\u66ff\u4ee3\u66ff\u4ee3\u5316\u77f3\u7684\u540c\u7c7b\u6750\u6599\u7684\u53ef\u518d\u751f\uff0c\u53ef\u6301\u7eed\u53d1\u5c55\u7684\u7279\u6027\uff0c\u800c\u4e14\u8fd8\u56e0\u4e3a\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u539f\u7ea4\u7ef4\u5177\u6709\u72ec\u7279\u7684\u7279\u6027\uff0c\u4f8b\u5982\u751f\u7269\u76f8\u5bb9\u6027\u548c\u5177\u6709\u9ad8\u5f3a\u5ea6\u548c\u5438\u6e7f\u6027\u7684\u7279\u6027\uff0c\u4f7f\u5176\u6210\u4e3a\u5728\u8bb8\u591a\u6280\u672f\u5e94\u7528\u4e2d\u5f97\u4ee5\u5229\u7528\u7684\u6709\u5229\u5019\u9009\u8005\uff0c\u4ee5\u53ca\u5148\u8fdb\u6750\u6599\u7684\u57fa\u7840\u3002\u57fa\u4e8e\u690d\u7269\u7684\u7ea4\u7ef4\u7d20\u6750\u6599\u662f\u529f\u80fd\u6750\u6599\u7684\u91cd\u8981\u7ec4\u6210\u90e8\u5206\uff0c\u5e76\u4e14\u5df2\u7ecf\u5bf9\u53ef\u6301\u7eed\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u751f\u4ea7\u7b56\u7565\u8fdb\u884c\u4e86\u6df1\u5165\u7814\u7a76\u3002<\/p>\n<p>\u82ac\u5170\u963f\u5c14\u6258\u5927\u5b66Stina Gr\u00f6nqvist\u4ecb\u7ecd\u4e86\u5728\u6e29\u548c\u7684\u673a\u68b0\u6405\u62cc\u4e0b\u901a\u8fc7\u9176\u7684\u4f5c\u7528\u4ea7\u751f\u4e00\u79cd\u65b0\u578b\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u3002\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u4ea7\u7269\u53ca\u76f8\u5e94\u7684\u5de5\u827a\u79f0\u4e3a\u7ea4\u7ef4\u7d20\u7684\u9ad8\u6d53\u5ea6\u9176\u7ea4\u98a4\uff0c\u7b80\u79f0HefCel\u3002\u7ea4\u7ef4\u5728\u4f4e\u542b\u6c34\u91cf\u7684\u7ea4\u7ef4\u6469\u64e6\u4ea7\u751f\u526a\u5207\u529b\uff0c\u7ed3\u5408CBH\u7684\u6301\u7eed\u4f5c\u7528\uff0c\u901a\u8fc7\u4e00\u79cd\u5265\u843d\u578b\u53cd\u5e94\u8bf1\u5bfc\u8868\u9762\u7ea4\u7ef4\u6027\u98a4\u52a8\uff0c\u5f62\u6210\u7cca\u72b6\u7ea4\u7ef4\u7f51\u7edc\uff0c\u6536\u7387\u9ad8\u8fbe85%\u3002\u901a\u8fc7\u9ad8\u5206\u8fa8\u7387\u663e\u5fae\u955c\u6210\u50cf\uff0c\u539f\u7ea4\u7ef4\u7684\u5c3a\u5bf8\u548c\u5927\u5c0f\u5206\u5e03\u8868\u660eHefCel\u5206\u7ea7\u5c5e\u4e8e\u5fae\u7ea4\u98a4\u7ea4\u7ef4\u7d20\u6216\u7ea4\u7ef4\u7d20\u5fae\u539f\u7ea4\u7ef4(CMFs)\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7c7b\u3002\u800c\u4e14\u539f\u7ea4\u7ef4\u7684\u6a2a\u5411\u5bbd\u5ea6\u901a\u5e38\u572815\u81f320 nm\u4e4b\u95f4\u3002\u603b\u7684\u6765\u8bf4\u4ee5\u66f4\u4f4e\u80fd\u6e90\u6d88\u8017\u7684\u65b9\u5f0f\u751f\u4ea7\u9ad8\u56fa\u4f53\u542b\u91cf\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u65b9\u6cd5\uff0c\u4e3a\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u53ef\u6301\u7eed\u751f\u4ea7\u63d0\u4f9b\u4e86\u65b0\u7684\u5e94\u7528\u9886\u57df\uff0c\u6bd4\u5982\u5728\u7eba\u7ec7\u3001\u5305\u88c5\u548c\u9020\u7eb8\u4e0a\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216562 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724710-2.png\" alt=\"\" width=\"600\" height=\"327\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724710-2.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724710-2-300x164.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u53c2\u8003\u6587\u732e\uff1aPere J, Tammelin T, Niemi P, Lille M, Virtanen T, Penttil\u00e4 PA, et al. Production of High Solid Nanocellulose by Enzyme-Aided Fibrillation Coupled with Mild Mechanical Treatment. ACS Sustainable Chemistry &amp; Engineering 2020;8:18853-18863.<\/p>\n<p><strong style=\"line-height: 1.5;\"><b>11. \u4e1c\u534e\u5927\u5b66\u6d2a\u67ab<\/b><\/strong><strong style=\"line-height: 1.5;\"><b>\uff08Biomacromolecules\uff09\uff1a\u901a\u8fc7\u5f15\u5165\u4e1d\u7d20\u86cb\u767d\u7eb3\u7c73\u9897\u7c92\u548c\u809d\u7d20\u7528\u4e8e\u5c0f\u53e3\u5f84\u8840\u7ba1\u79fb\u690d\u5e94\u7528\uff0c\u6539\u5584\u7ec6\u83cc\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u5bfc\u7ba1\u7684\u6027\u80fd<\/b><\/strong><\/p>\n<p>\u6839\u636e\u4e16\u754c\u536b\u751f\u7ec4\u7ec7\u7684\u5e74\u5ea6\u62a5\u544a\uff0c\u5fc3\u8840\u7ba1\u75be\u75c5\uff08CVD\uff09\u4ecd\u7136\u662f\u9020\u6210\u4eba\u7c7b\u6b7b\u4ea1\u7684\u4e3b\u8981\u539f\u56e0\u3002\u8840\u7ba1\u91cd\u5efa\u5728CVD\u7684\u4e34\u5e8a\u624b\u672f\u4e2d\u5360\u6709\u91cd\u8981\u5730\u4f4d\u7279\u522b\u662f\u5bf9\u4e8e\u52a8\u8109\u548c\u9759\u8109\u75c5\u53d8\uff0c\u4f8b\u5982\u4e25\u91cd\u7684\u521b\u4f24\uff0c\u5148\u5929\u6027\u7578\u5f62\uff0c\u8840\u7ba1\u80bf\u7624\u548c\u652f\u67b6\u690d\u5165\u540e\u7ee7\u53d1\u7684\u8840\u7ba1\u95ed\u585e\u3002\u7528\u4e8e\u8840\u7ba1\u91cd\u5efa\u7684\u8840\u7ba1\u79fb\u690d\u7269\u53ef\u4ee5\u5206\u4e3a\u751f\u7269\u8840\u7ba1\u79fb\u690d\u7269\u6216\u5408\u6210\u6750\u6599\u79fb\u690d\u7269\u3002\u7ba1\u72b6\u7ec6\u83cc\u7eb3\u7c73\u7ea4\u7ef4\u7d20\uff08BNC\uff09\u7531\u4e8e\u5176\u72ec\u7279\u7684\u7279\u6027\uff08\u5982\u7ec6\u80de\u5916\u57fa\u8d28\u68373D\u7eb3\u7c73\u539f\u7ea4\u7ef4\u7f51\u7edc\u7ed3\u6784\uff0c\u9ad8\u7eaf\u5ea6\u548c\u4fdd\u6c34\u6027\uff0c\u826f\u597d\u7684\u53ef\u5851\u6027\u548c\u72ec\u7279\u6027\uff09\uff0c\u5df2\u88ab\u8bc1\u660e\u662f\u7528\u4e8e\u5c0f\u53e3\u5f84\u8840\u7ba1\u79fb\u690d\u7684\u6709\u524d\u9014\u7684\u5929\u7136\u751f\u7269\u6750\u6599\u3002\u4e1d\u7d20\u86cb\u767d\uff08SF\uff09\u662f\u4e00\u79cd\u53ef\u4ee5\u4ece\u5bb6\u8695\u8327\u548c\u8718\u86db\u4e1d\u4e2d\u63d0\u53d6\u7684\u5929\u7136\u7ea4\u7ef4\u86cb\u767d\uff0c\u7531\u4e8e\u5176\u76f8\u5f53\u7684\u751f\u7269\u76f8\u5bb9\u6027\u548c\u53ef\u751f\u7269\u964d\u89e3\u6027\uff0c\u5df2\u88ab\u5e7f\u6cdb\u7528\u4f5c\u751f\u7269\u6750\u6599\u3002\u809d\u7d20\u5df2\u5728\u4e34\u5e8a\u4e0a\u5e7f\u6cdb\u7528\u4f5c\u6297\u51dd\u5242\uff0c\u800c\u4f7f\u7528EDC \/ NHS\u4ea4\u8054\u7684\u809d\u7d20\u8fdb\u884c\u8868\u9762\u4fee\u9970\u53ef\u4ee5\u5728\u5f88\u957f\u4e00\u6bb5\u65f6\u95f4\u5185\u663e\u7740\u6539\u5584\u8840\u7ba1\u79fb\u690d\u7269\u7684\u8840\u6db2\u76f8\u5bb9\u6027\u3002<\/p>\n<p>\u4e1c\u534e\u5927\u5b66\u6d2a\u67ab\u901a\u8fc7\u5c06SF\u7eb3\u7c73\u9897\u7c92\uff08SFNP\uff09\u548c\u809d\u7d20\u5305\u57cb\u7684SFNP\uff08SF-HepNP\uff09\u4e73\u5242\u4ece\u5185\u90e8\u9644\u7740\u5230BNC\u58c1\u4e0a\uff0c\u5236\u9020\u4e86\u4e24\u79cd\u5f62\u5f0f\u7684\u5c0f\u53e3\u5f84\u8840\u7ba1\u79fb\u690d\u7269\uff08BNC-SFNP\u548cBNC-SF-HepNP\uff09\u3002\u7ed3\u679c\u8868\u660e\uff0c\u809d\u7d20\u5316\u7684BNC-Hep\u548cBNC-SFNP-Hep\u5bfc\u7ba1\u6539\u5584\u4e86\u6297\u51dd\u6027\u80fd\uff0cBNC-SFNP-Hep\u5728\u4fc3\u8fdb\u4eba\u8110\u9759\u8109\u5185\u76ae\u7ec6\u80de\u589e\u6b96\u7684\u540c\u65f6\uff0c\u4e5f\u63a7\u5236\u4e86\u4eba\u52a8\u8109\u5e73\u6ed1\u808c\u7ec6\u80de\u8fc7\u5ea6\u589e\u6b96\uff0c\u534f\u52a9\u5feb\u901f\u5185\u76ae\u5316\uff0c\u6539\u5584\u7ba1\u8154\u901a\u7545\u3002\u5728\u76ae\u4e0b\u690d\u51654\u5468\u540e\u672a\u89c1\u660e\u663e\u708e\u75c7\u53cd\u5e94\u548c\u7269\u8d28\u964d\u89e3\uff0c\u5e76\u4e14\u5bfc\u7ba1\u5468\u56f4\u53ef\u89c1\u81ea\u4f53\u7ec4\u7ec7\uff0c\u7ec6\u80de\u6d78\u6da6\u81f3\u6240\u6709\u6837\u672c\u8fb9\u7f18\uff0cBNC-SFNP\u5bfc\u7ba1\u6d78\u6da6\u6700\u6df1\uff0c\u4e3a\u5c0f\u53e3\u5f84\u8840\u7ba1\u5e94\u7528\u63d0\u4f9b\u9002\u5b9c\u7684\u8840\u7ba1\u751f\u6210\u5fae\u73af\u5883\u3002BNC-Hep\u548cBNC-SFNP-Hep\u5bfc\u7ba1\u5468\u56f4\u708e\u75c7\u7ec6\u80de\u8f83\u5c11\u3002\u56e0\u6b64\uff0cBNC-SFNP-Hep\u5bfc\u7ba1\u7684\u6297\u51dd\u7279\u6027\u53ca\u5176\u5bf9\u5185\u76ae\u5316\u7684\u523a\u6fc0\u63d0\u793a\u5176\u4f5c\u4e3a\u5c0f\u53e3\u5f84\u4eba\u5de5\u8840\u7ba1\u5728\u4e34\u5e8a\u5e94\u7528\u4e2d\u5177\u6709\u5f88\u5927\u7684\u6f5c\u529b\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216563 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724711-2.png\" alt=\"\" width=\"600\" height=\"324\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724711-2.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724711-2-300x162.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u53c2\u8003\u6587\u732e\uff1aBao L, Hong FF, Li G, Hu G and Chen L. Improved Performance of Bacterial Nanocellulose Conduits by the Introduction of Silk Fibroin Nanoparticles and Heparin for Small-Caliber Vascular Graft Applications. Biomacromolecules 2020.<\/p>\n<p><strong style=\"line-height: 1.5;\"><b>12. \u7f8e\u56fd\u52a0\u5229\u798f\u5c3c\u4e9a\u5927\u5b66Anand Bala Subramaniam\uff08ACS Applied Materials &amp; Interfaces\uff09\uff1a\u4f7f\u7528\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7eb8\u6765\u4fc3\u8fdb\u5de8\u578b\u5355\u5c42\u56ca\u6ce1\u7684\u4fbf\u6377\u548c\u9ad8\u4ea7\u91cf\u7ec4\u88c5<\/b><\/strong><\/p>\n<p>\u5de8\u5927\u7684\u5355\u819c\u56ca\u6ce1(GUVs)\u662f\u76f4\u5f84\u5927\u4e8e1\u03bcm\u7684\u5355\u58c1\u5c01\u95ed\u78f7\u8102\u53cc\u5c42\u819c\u3002GUV\u7c7b\u4f3c\u4e8e\u6700\u5c0f\u7684\u751f\u7269\u7ec6\u80de\u3002\u8fd9\u79cd\u76f8\u4f3c\u4f7fGUV\u6709\u52a9\u4e8e\u589e\u8fdb\u5bf9\u819c\u7ec4\u7ec7\uff0c\u7ec6\u80de\u9aa8\u67b6\u529b\u5b66\uff0c\u751f\u6b96\uff0c\u5206\u88c2\uff0c\u8fd0\u8f93\u548c\u7535\u4fe1\u53f7\u4f20\u5bfc\u7b49\u65b9\u9762\u7684\u7406\u89e3\u3002 \u6b64\u5916\uff0c\u81ea\u4e0b\u800c\u4e0a\u7684\u5408\u6210\u751f\u7269\u5b66\uff0c\u4eba\u9020\u7ec4\u7ec7\u5de5\u7a0b\u548c\u836f\u7269\u8f93\u9001\u65b9\u9762\u7684\u521b\u65b0\u4e3a\u5728\u4eff\u751f\u5e94\u7528\u4e2d\u4f7f\u7528GUV\u5f00\u8f9f\u4e86\u65b0\u9014\u5f84\u3002<\/p>\n<p>\u7f8e\u56fd\u52a0\u5229\u798f\u5c3c\u4e9a\u5927\u5b66Anand Bala Subramaniam\u63d0\u51fa\u4e86\u5229\u7528\u8868\u9762\u7531\u7ea0\u7f20\u7684\u5706\u67f1\u7eb3\u7c73\u7ea4\u7ef4\u7ec4\u6210\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7eb8\uff0c\u6765\u4fc3\u8fdb\u7ec4\u88c5GUVs\u7684\u7b80\u4fbf\u548c\u9ad8\u4ea7\u91cf\u3002\u4e0e\u73b0\u6709\u7684\u8868\u9762\u8f85\u52a9\u7ec4\u88c5\u6280\u672f\u76f8\u6bd4\uff0c\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7eb8\u7684\u4f7f\u7528\u53ef\u4f7f\u6210\u672c\u964d\u4f4e10\u4e07\u500d\uff0c\u540c\u65f6\u63d0\u9ad8\u4ea7\u91cf\u3002\u4f7f\u7528\u5927\u6570\u636e\u96c6\u5171\u805a\u7126\u663e\u5fae\u955c\u5bf9\u4ea7\u91cf\u548c\u5c3a\u5bf8\u5206\u5e03\u7684\u5b9a\u91cf\u6d4b\u91cf\u9610\u660e\u4e86\u7ec4\u88c5\u7684\u673a\u7406\u3002\u540c\u65f6\u63d0\u51fa\u4e86\u4e00\u4e2a\u70ed\u529b\u5b66\u53d1\u82bd\u548c\u5408\u5e76\u7684BNM\u6a21\u578b\uff0c\u4e3a\u4ece\u4e0d\u540c\u51e0\u4f55\u548c\u5316\u5b66\u8868\u9762\u83b7\u5f97\u7684GUVs\u7684\u4ea7\u7387\u548c\u5c3a\u5bf8\u7684\u5dee\u5f02\u63d0\u4f9b\u4e86\u7edf\u4e00\u7684\u89e3\u91ca\u3002BNM\u6a21\u578b\u901a\u8fc7\u5e73\u8861\u8868\u9762\u9644\u7740\u819c\u8f6c\u53d8\u4e3a\u8868\u9762\u9644\u7740\u7403\u82bd\u7684\u90e8\u5206\u7684\u5f39\u6027\u3001\u9644\u7740\u529b\u548c\u8fb9\u7f18\u80fd\u91cf\uff0c\u8003\u8651\u4e86\u82bd\u51fa\u5f15\u8d77\u7684\u81ea\u7531\u80fd\u7684\u53d8\u5316\u3002\u8be5\u6a21\u578b\u8868\u660e\uff0c\u5728\u4e0e\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7ea4\u7ef4\u5c3a\u5bf8\u76f8\u4f3c\u7684\u7ea0\u7f20\u67f1\u72b6\u7eb3\u7c73\u7ea4\u7ef4\u7684\u4eb2\u6c34\u6027\u8868\u9762\u4e0a\uff0cGUVs\u7684\u5f62\u6210\u662f\u81ea\u53d1\u7684\u3002\u8fd9\u9879\u5de5\u4f5c\u4fc3\u8fdb\u4e86\u5bf9\u8868\u9762\u6027\u8d28\u5bf9\u805a\u82ef\u4e59\u70ef\u7ec4\u88c5\u7684\u5f71\u54cd\u7684\u7406\u89e3\u3002\u5b83\u8fd8\u89e3\u51b3\u4e86\u76ee\u524d\u963b\u788dGUVs\u4f5c\u4e3a\u836f\u7269\u8fd0\u8f7d\u5de5\u5177\u3001\u5408\u6210\u7ec6\u80de\u5236\u9020\u548c\u4eba\u5de5\u7ec4\u7ec7\u5927\u89c4\u6a21\u7ec4\u88c5\u7684\u5b9e\u9645\u969c\u788d\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216564 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724712-1.png\" alt=\"\" width=\"600\" height=\"322\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724712-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724712-1-300x161.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u53c2\u8003\u6587\u732e\uff1aPazzi J and Subramaniam AB. Nanoscale Curvature Promotes High Yield Spontaneous Formation of Cell-Mimetic Giant Vesicles on Nanocellulose Paper. ACS Applied Materials &amp; Interfaces 2020;12:56549-56561.<\/p>\n<p><strong style=\"line-height: 1.5;\"><b>13. \u626c\u5dde\u5927\u5b66\u5434\u5fb7\u5cf0\uff08Carbohydrate Polymers\uff09\uff1a<\/b><\/strong><strong style=\"line-height: 1.5;\"><b>\u901a\u8fc7\u8c03\u8282\u7ea4\u7ef4\u7684\u67d4\u97e7\u6027\u6765\u8c03\u6574\u76ae\u6c0f\u4e73\u5242\u7684\u5f62\u6001\u548c\u7c98\u5f39\u6027<\/b><\/strong><\/p>\n<p>\u968f\u7740\u4eba\u4eec\u5bf9\u73af\u5883\u95ee\u9898\u7684\u65e5\u76ca\u5173\u6ce8\uff0c\u751f\u7269\u8d28\u6750\u6599\u4f5c\u4e3a\u4f20\u7edf\u6750\u6599\u6216\u5408\u6210\u6750\u6599\u7684\u66ff\u4ee3\u6750\u6599\u5728\u8bb8\u591a\u9886\u57df\u53d7\u5230\u4e86\u4eba\u4eec\u7684\u5e7f\u6cdb\u5173\u6ce8\u3002\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u56e0\u5176\u4e30\u5bcc\u7684\u53ef\u518d\u751f\u8d44\u6e90\u548c\u4f18\u5f02\u7684\u529b\u5b66\u6027\u80fd\u800c\u6210\u4e3a\u6700\u5177\u4ee3\u8868\u6027\u7684\u6750\u6599\u3002\u56e0\u6b64\uff0c\u8fd9\u7c7b\u6750\u6599\u5728\u7eff\u8272\u590d\u5408\u6750\u6599\u548c\u529f\u80fd\u6750\u6599\u9886\u57df\u5f15\u8d77\u4e86\u5e7f\u6cdb\u7684\u5173\u6ce8\u3002\u53e6\u4e00\u4e2a\u6f5c\u5728\u7684\u5e94\u7528\u662f\u5236\u5907\u76ae\u514b\u6797\u4e73\u6db2\uff0c\u56e0\u4e3a\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u53ef\u4ee5\u6ee1\u8db3\u53ef\u6301\u7eed\u548c\u73af\u5883\u53cb\u597d\u578b\u7c92\u5b50\u4e73\u5316\u5242\u7684\u8981\u6c42\u3002\u8fd9\u4e9b\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u66f4\u5438\u5f15\u4eba\u7684\u5730\u65b9\u662f\u5176\u5404\u5411\u5f02\u6027\u7684\u7ea4\u7ef4\u7ed3\u6784\uff0c\u5b83\u6709\u5229\u4e8e\u5728\u6781\u4f4e\u7684\u8d1f\u8f7d\u6c34\u5e73\u7a33\u5b9a\u6cb9\/\u6c34(O\/W)\u754c\u9762\u3002\u6b64\u5916\uff0c\u5b83\u4eec\u7684\u8868\u9762\u6027\u8d28\u5f88\u5bb9\u6613\u901a\u8fc7\u5316\u5b66\u4fee\u9970\u6765\u8c03\u8282\uff0c\u8fd9\u4e3a\u8c03\u63a7\u4e73\u6db2\u7684\u5f62\u6001\u548c\u6700\u7ec8\u6027\u8d28\u63d0\u4f9b\u4e86\u66f4\u591a\u7684\u53ef\u80fd\u6027\u3002\u56e0\u6b64\uff0c\u5230\u76ee\u524d\u4e3a\u6b62\uff0c\u56f4\u7ed5\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7a33\u5b9a\u4e73\u5242\u7684\u5236\u5907\u548c\u5e94\u7528\u8fdb\u884c\u4e86\u5927\u91cf\u7684\u7814\u7a76\u3002<\/p>\n<p>\u626c\u5dde\u5927\u5b66\u5434\u5fb7\u5cf0\u4ee5\u7ec6\u83cc\u7ea4\u7ef4\u7d20(BC)\u3001\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u7ea4\u7ef4(CNF)\u548c\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u6676(CNC)\u4e09\u79cd\u7c7b\u578b\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u4e3a\u539f\u6599\uff0c\u5236\u5907\u4e86\u6c34\u5305\u6cb9\u578b\u76ae\u6c0f\u4e73\u5242\uff0c\u63a2\u8ba8\u4e86\u7ea4\u7ef4\u67d4\u97e7\u6027\u5bf9\u4e73\u5316\u6548\u679c\u7684\u5f71\u54cd\u3002\u5728\u6c34\u76f8\u60ac\u6d6e\u6db2\u4e2d\uff0c\u6700\u77ed\u7684CNC\u662f\u521a\u6027\u7684\uff0c\u800c\u6700\u957f\u7684BC\u662f\u5b8c\u5168\u67d4\u6027\u7684\uff0c\u8fd9\u5bfc\u81f4\u4e86\u5b83\u4eec\u5728\u7a00\u91ca\u5230\u534a\u7a00\u91ca\u6d53\u5ea6\u548c\u6d41\u53d8\u6e17\u6ee4\u6db2\u4e2d\u7684\u5dee\u5f02\u5f88\u5927\u3002\u56e0\u6b64\uff0c\u8fd9\u4e9b\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u7ea4\u7ef4\u5728\u4e73\u5316\u8fc7\u7a0b\u4e2d\u53d1\u6325\u7740\u4e0d\u540c\u7684\u4f5c\u7528\u3002\u67d4\u6027BC\u51e0\u4e4e\u6ca1\u6709\u4e73\u5316\u80fd\u529b\uff0c\u800c\u534a\u67d4\u6027CNF\u548c\u521a\u6027CNC\u53ef\u4ee5\u5f88\u597d\u5730\u7528\u4e8e\u7a33\u5b9a\u4e73\u6db2\u3002\u5bf9\u4e8eCNF\u7a33\u5b9a\u7684\u7cfb\u7edf\u6765\u8bf4\uff0c\u6d88\u8017\u6548\u5e94\u5360\u4e3b\u5bfc\u5730\u4f4d\uff0c\u5bb9\u6613\u5bfc\u81f4\u6db2\u6ef4\u56e2\u7c07\u7684\u5f62\u6210\uff0c\u800c\u5bf9\u4e8eCNF\u7a33\u5b9a\u7684\u7cfb\u7edf\u6765\u8bf4\uff0c\u6392\u65a5\u529b\u4f5c\u7528\u66f4\u4e3a\u91cd\u8981\u3002\u52a8\u6001\u6d41\u53d8\u5b66\u8fdb\u4e00\u6b65\u63ed\u793a\u4e86\u6db2\u6ef4\u957f\u671f\u7ed3\u6784\u5f1b\u8c6b\u7684\u53ef\u89c1\u8bc1\u636e\u3002\u8fd9\u9879\u5de5\u4f5c\u63d0\u51fa\u4e86\u4e00\u4e9b\u6709\u8da3\u7684\u89c2\u70b9\uff0c\u53ef\u4ee5\u901a\u8fc7\u8c03\u8282\u7ea4\u7ef4\u7684\u67d4\u97e7\u6027\u6765\u8c03\u6574\u76ae\u6c0f\u4e73\u5242\u7684\u5f62\u6001\u548c\u7c98\u5f39\u6027\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216565 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724713-1.png\" alt=\"\" width=\"600\" height=\"287\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724713-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724713-1-300x144.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u53c2\u8003\u6587\u732e\uff1aLu Y, Li J, Ge L, Xie W and Wu D. Pickering emulsion stabilized with fibrous nanocelluloses: Insight into fiber flexibility-emulsifying capacity relations. Carbohydrate Polymers 2021;255:117483.<\/p>\n<p><strong><b>\u00a014.\u00a0<\/b><\/strong><strong style=\"line-height: 1.5;\"><b>\u6fb3\u5927\u5229\u4e9a\u8499\u7eb3\u58eb\u5927\u5b66Gil Garnier\uff08Biomacromolecules\uff09\uff1a\u9633\u79bb\u5b50\u4ea4\u8054\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u57fa\u8d28\u7528\u4e8e\u80a0\u9053\u7c7b\u5668\u5b98\u7684\u751f\u957f\u548c\u6062\u590d<\/b><\/strong><\/p>\n<p>\u6c34\u51dd\u80f6\u662f\u591a\u5b54\u7684\u4e09\u7ef4\u7ed3\u6784\uff0c\u53ef\u4ee5\u5bb9\u7eb3\u5927\u91cf\u7684\u6c34\uff0c\u540c\u65f6\u5177\u6709\u4e00\u5b9a\u7684\u673a\u68b0\u5b8c\u6574\u6027\u3002\u8fd9\u7c7b\u8f6f\u6750\u6599\u4f9d\u8d56\u4e8e\u7269\u7406\u6216\u5316\u5b66\u4ea4\u8054\u7684\u7ea4\u7ef4\u7f51\u7edc\uff0c\u53ef\u4ee5\u54cd\u5e94\u6e29\u5ea6\u53d8\u5316\uff0c pH\u548c\u8f90\u5c04\u3002\u6c34\u51dd\u80f6\u7684\u80f6\u4f53\u7a33\u5b9a\u6027\u4f9d\u8d56\u4e8e\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u7684\u7f20\u7ed3\u7f51\u7edc\uff0c\u53ef\u4ee5\u901a\u8fc7\u5171\u4ef7\u6216\u79bb\u5b50\u4ea4\u8054\u8fdb\u4e00\u6b65\u6539\u6027\u3002\u4e5f\u53ef\u4ee5\u5c06\u6dfb\u52a0\u5242\uff08\u4f8b\u5982\u6c28\u57fa\u9178\u548c\u7cd6\uff09\u6eb6\u89e3\u5728\u8fd9\u4e9b\u6c34\u51dd\u80f6\u4e2d\uff0c\u4ee5\u8bbe\u8ba1\u5176\u751f\u5316\u7279\u6027\uff0c\u4ee5\u5b9e\u73b0\u7279\u5b9a\u6c34\u5e73\u7684\u91cd\u91cf\u514b\u5206\u5b50\u6e17\u900f\u538b\u6d53\u5ea6\u548c\u79bb\u5b50\u5f3a\u5ea6\u3002\u7531\u4e8e\u5176\u5177\u6709\u5f88\u5927\u7684\u53ef\u8c03\u6027\uff0c\u4e0e\u5176\u751f\u7269\u76f8\u5bb9\u6027\u76f8\u5173\uff0c\u56e0\u6b64\u690d\u7269\u57fa\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u6c34\u51dd\u80f6\u662f\u751f\u7269\u533b\u5b66\u5e94\u7528\u7684\u7406\u60f3\u9009\u62e9\u3002\u529f\u80fd\u5316\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u6c34\u51dd\u80f6\u88ab\u7528\u4e8e\u80a0\u9053\u7c7b\u5668\u5b98\u7684\u751f\u957f\u3002\u4f46\u662f\uff0c\u8fd9\u4e9b\u51dd\u80f6\u7684\u521a\u5ea6\u4e0e\u56fa\u4f53\u542b\u91cf\u6210\u6b63\u6bd4\uff0c\u5e76\u4e14\u672a\u8bc4\u4f30\u591a\u79cd\u4ea4\u8054\u5242\u7684\u4f5c\u7528\u53ca\u5176\u6d53\u5ea6\u3002\u6700\u540e\uff0c\u5373\u4f7f\u5728\u77ed\u671f\u5185\uff0c\u5728\u7ea4\u7ef4\u7d20\u57fa\u8d28\u4e2d\u751f\u957f\u7684\u7403\u4f53\u548c\u7c7b\u5668\u5b98\u7684\u6062\u590d\u4f20\u4ee3\uff0c\u5c1a\u672a\u6df1\u5165\u8c03\u67e5\u3002<\/p>\n<p>\u6fb3\u5927\u5229\u4e9a\u8499\u7eb3\u58eb\u5927\u5b66Gil Garnier\u7814\u7a76\u9633\u79bb\u5b50\u4ea4\u8054\uff0c\u4ee5\u63a7\u5236\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u6c34\u51dd\u80f6\u7684\u673a\u68b0\u6027\u80fd\uff0c\u4ee5\u4fc3\u8fdb\u80a0\u9053\u7c7b\u5668\u5b98\u7684\u751f\u957f\u548c\u6062\u590d\u3002\u63d0\u51fa\u4e00\u4e2a\u5047\u8bbe\uff0c\u5373\u9ad8\u5ea6\u7fa7\u5316\u7684\u7ea4\u7ef4\u7d20\u7eb3\u7c73\u7ea4\u7ef4\u53ef\u4ee5\u5f62\u6210\u529f\u80fd\u5316\u7684\u57fa\u8d28\uff0c\u4e3a\u7c7b\u5668\u5b98\u751f\u957f\u63d0\u4f9b\u7406\u60f3\u7684\u751f\u5316\u548c\u7269\u7406\u7279\u6027\u3002 \u5e76\u8bc4\u4f30\u4e86\u5176\u5bf9\u6c34\u51dd\u80f6\u4ee5\u53ca\u7c7b\u5668\u5b98\u5f62\u6210\u7684\u5f71\u54cd\u3002\u4ece\u6d41\u53d8\u5b66\u89d2\u5ea6\u8868\u5f81\u4e86\u4e0eCa<sup>2 +<\/sup>\u548cMg<sup>2 +<\/sup>\u4ea4\u8054\u7684TPON\u6c34\u51dd\u80f6\u7684\u673a\u68b0\u6027\u80fd\u3002\u5728\u8fd9\u4e9b\u7ea4\u7ef4\u7d20\u57fa\u8d28\u4e2d\u57f9\u517b\u7c7b\u5668\u5b984\u5929\uff0c\u5e76\u56de\u6536\u4f20\u4ee3\u548cRNA\u63d0\u53d6\u3002\u4ece\u9541\u4ea4\u8054\u7684\u6c34\u51dd\u80f6\u4e2d\u56de\u6536\u7684\u7ec6\u80de\u7c07\u53ef\u4ee5\u901a\u8fc7\uff0c\u5176\u63d0\u53d6\u7684RNA\u5b8c\u597d\u65e0\u635f\u3002\u9633\u79bb\u5b50\u4ea4\u8054\u7684\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u6c34\u51dd\u80f6\u6709\u671b\u6210\u4e3a3D\u7ec6\u80de\u57f9\u517b\u7cfb\u7edf\u7684\u66ff\u4ee3\u690d\u7269\u57fa\u57fa\u8d28\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-216566 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724714-1.png\" alt=\"\" width=\"600\" height=\"161\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724714-1.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/01\/\u56fe\u724714-1-300x81.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u53c2\u8003\u6587\u732e\uff1aCurvello R and Garnier G. Cationic Cross-Linked Nanocellulose-Based Matrices for the Growth and Recovery of Intestinal Organoids. Biomacromolecules 2020.<\/p>\n<p>\u672c\u6587\u7531\u6625\u56fd\u4f9b\u7a3f\u3002<\/p>\n<p>\u672c\u5185\u5bb9\u4e3a\u4f5c\u8005\u72ec\u7acb\u89c2\u70b9\uff0c\u4e0d\u4ee3\u8868\u6750\u6599\u4eba\u7f51\u7acb\u573a\u3002<\/p>\n<p>\u672a\u7ecf\u5141\u8bb8\u4e0d\u5f97\u8f6c\u8f7d\uff0c\u6388\u6743\u4e8b\u5b9c\u8bf7\u8054\u7cfbkefu@cailiaoren.com\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1: tougao@cailiaoren.com.<\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaorenVIP\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u5f15\u8a00\u3011 \u7eb3\u7c73\u7ea4\u7ef4\u7d20\u662f\u4e00\u7c7b\u5177\u6709\u9ad8\u673a\u68b0\u6027\u80fd\u7684\u53ef\u518d\u751f\u9ad8\u7eb5\u6a2a\u6bd4\u7eb3\u7c73\u7c92\u5b50\uff0c\u5176\u8868\u9762\u5177\u6709\u5316\u5b66\u53cd\u5e94\u57fa\u56e2\u53ef\u4ee5\u5b98\u80fd\u5316\u3002\u5728\u52aa\u529b\u5f00\u53d1\u53ef\u6301\u7eed\u7684\u9ad8\u7ea7\u529f\u80fd\u6750\u6599\u65f6\uff0c\u7eb3\u7c73\u7ea4\u7ef4\u7d20\u6700\u8fd1\u5f15\u8d77\u4e86\u5e7f\u6cdb\u7684&#8230;<\/p>\n","protected":false},"author":11454,"featured_media":216552,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[1187],"tags":[],"class_list":["post-216551","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-zhuanlan"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/216551"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/11454"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=216551"}],"version-history":[{"count":2,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/216551\/revisions"}],"predecessor-version":[{"id":216580,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/216551\/revisions\/216580"}],"wp:featuredmedia":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/media\/216552"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=216551"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=216551"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=216551"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}