{"id":217393,"date":"2021-02-06T06:30:46","date_gmt":"2021-02-05T22:30:46","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=217393"},"modified":"2021-03-03T11:52:36","modified_gmt":"2021-03-03T03:52:36","slug":"ucla%e6%9d%a8%e9%98%b3%e7%ad%89science%ef%bc%9a%e5%88%a9%e7%94%a8%e5%85%b1%e8%bd%ad%e6%9c%89%e6%9c%ba%e9%98%b3%e7%a6%bb%e5%ad%90%e5%ae%9e%e7%8e%b0%e5%85%89%e4%bc%8f%e9%92%99%e9%92%9b%e7%9f%bf%e8%83%bd","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=217393","title":{"rendered":"UCLA\u6768\u9633\u7b49Science\uff1a\u5229\u7528\u5171\u8f6d\u6709\u673a\u9633\u79bb\u5b50\u5b9e\u73b0\u5149\u4f0f\u9499\u949b\u77ff\u80fd\u5e26\u8fb9\u7f18\u6001\u7684\u53ef\u91cd\u6784"},"content":{"rendered":"<p><strong>\u5f15\u8a00<\/strong><\/p>\n<p>\u4e00\u822c\u5316\u5b66\u7ed3\u6784\u4e3aABX3 \u7684\u91d1\u5c5e\u5364\u5316\u9499\u949b\u77ff\u7684\u80fd\u5e26\u8fb9\u7f18(A\uff0c\u901a\u5e38\u4e3a\u4e00\u4ef7\u6709\u673a\u9633\u79bb\u5b50;B\uff0c\u4e8c\u4ef7\u9633\u79bb\u5b50;X\u662f\u5364\u5316\u7269\u9634\u79bb\u5b50)\u4e3b\u8981\u7531B\u548cX\u7684\u8f68\u9053\u7ec4\u6210\u3002\u56e0\u6b64\uff0c\u65e0\u673aB-X\u6846\u67b6\u7684\u7ed3\u6784\u548c\u7ec4\u6210\u7c7b\u578b\u4e3b\u8981\u8d1f\u8d23\u8c03\u8282\u5176\u7535\u5b50\u6027\u8d28\uff0c\u800cA\u4f4d\u9633\u79bb\u5b50\u88ab\u8ba4\u4e3a\u53ea\u6709\u52a9\u4e8e\u7a33\u5b9a\u6676\u683c\uff0c\u800c\u4e0d\u662f\u76f4\u63a5\u5bf9\u8fd1\u8fb9\u7f18\u6001\u6709\u8d21\u732e\u3002\u76f8\u53cd\uff0c\u4e0d\u540c\u7684A\u4f4d\u9633\u79bb\u5b50\u5c3a\u5bf8\u53ef\u4ee5\u901a\u8fc7\u5f15\u8d77\u65e0\u673aB-X\u9aa8\u67b6\u7ed3\u6784\u53d8\u5f62\uff0c\u5982\u5355\u4f4d\u4f53\u79ef\u53d8\u5316\u3001\u516b\u9762\u4f53\u53d8\u5f62\u548c\u964d\u7ef4\u7b49\u95f4\u63a5\u6548\u5e94\u3002<\/p>\n<p><strong><b>UCLA\u6768\u9633<\/b><\/strong><strong><b>\u6559\u6388\uff0c<\/b><\/strong><strong><b>\u56fd\u5bb6\u53ef\u518d\u751f\u80fd\u6e90\u5b9e\u9a8c\u5ba4Matthew C. Beard<\/b><\/strong><strong><b>\u6559\u6388\u4ee5\u53ca<\/b><\/strong><strong><b>\u6258\u83b1\u591a\u5927\u5b66\u9122\u708e\u53d1<\/b><\/strong><strong><b>\u6559\u6388\uff08\u5171\u540c\u901a\u8baf\uff09<\/b><\/strong>\u7b49\u4eba\u5728<strong><b>Science<\/b><\/strong>\u4e0a\u62a5\u9053\u4e86\u4e00\u79cd\u5f71\u54cd\u9499\u949b\u77ff\u8fb9\u754c\u8f68\u9053\u7684A\u4f4d\u9633\u79bb\u5b50\u7684\u7535\u5b50\u6001\u7684\u03c0\u5171\u8f6d\u8bf1\u5bfc\u6269\u5c55\uff0c\u5e76\u76f4\u63a5\u5f71\u54cd\u6742\u5316\u9499\u949b\u77ff\u7684\u524d\u7ebf\u8f68\u9053\u3002\u5177\u6709\u8f83\u5927\u03c0\u5171\u8f6d\u7ed3\u6784\u7684\u9633\u79bb\u5b50\u53ef\u4ee5\u4e0e\u65e0\u673a\u524d\u7ebf\u5206\u5b50\u8f68\u9053\u76f8\u4e92\u4f5c\uff0c\u5177\u6709\u8f83\u5927\u03c0\u5171\u8f6d\u7ed3\u6784\u7684\u9633\u79bb\u5b50\u53ef\u4ee5\u4e0e\u65e0\u673a\u524d\u7ebf\u5206\u5b50\u8f68\u9053\u76f8\u4e92\u4f5c\u7528\u3002\u4e0e\u53c2\u8003\u65e0\u673a\u9499\u949b\u77ff\u76f8\u6bd4\uff0c\u5177\u6709\u6700\u4f73\u5d4c\u5165\u8ddd\u79bb\u7684\u8298\u4e59\u57fa\u94f5\u8868\u9762\u5c42\u63d0\u9ad8\u4e86\u7a7a\u7a74\u8fc1\u79fb\u7387\u548c\u529f\u7387\u8f6c\u6362\u6548\u7387\uff0c\u5e76\u63d0\u9ad8\u4e86\u5668\u4ef6\u7684\u7a33\u5b9a\u6027\u3002<strong><b>\u8be5\u8bba\u6587\u7b2c\u4e00\u4f5c\u8005\u4e3a\u7f8e\u56fd\u52a0\u5dde\u5927\u5b66\u6d1b\u6749\u77f6\u5206\u6821\uff08UCLA\uff09\u859b\u6676\u6676\u535a\u58eb\uff0c\u738b\u777f\u535a\u58eb\u548c\u7f8e\u56fd\u53ef\u518d\u751f\u80fd\u6e90\u56fd\u5bb6\u5b9e\u9a8c\u5ba4(NREL)\u9648\u71b9\u7ff0\u535a\u58eb\u3002<\/b><\/strong><\/p>\n<p><strong>\u56fe\u6587\u5bfc\u8bfb<\/strong><\/p>\n<p>\u56fe1\u3001\u5171\u8f6da\u4f4d\u9633\u79bb\u5b50\u7684\u7535\u5b50\u8d21\u732e\u7684\u8868\u9762\u4ee3\u8868\u7ed3\u6784<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-217397 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/\u56fe\u7247-4-9.png\" alt=\"\" width=\"600\" height=\"276\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/\u56fe\u7247-4-9.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/\u56fe\u7247-4-9-300x138.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe2\u3001\u5171\u8f6d\u94f5\u4e0e\u9499\u949b\u77ff\u9aa8\u67b6\u4e4b\u95f4\u7684\u76f8\u4e92\u4f5c\u7528\u6a21\u5f0f<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-217396 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/\u56fe\u7247-3-9.png\" alt=\"\" width=\"600\" height=\"310\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/\u56fe\u7247-3-9.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/\u56fe\u7247-3-9-300x155.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe3\u3001\u5171\u8f6d\u94f5\u7684\u63d2\u5c42\u6784\u578b<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-217395 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/\u56fe\u7247-2-9.png\" alt=\"\" width=\"600\" height=\"387\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/\u56fe\u7247-2-9.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/\u56fe\u7247-2-9-300x194.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u56fe4\u3001\u8f7d\u6d41\u5b50\u52a8\u529b\u5b66\u53d8\u5316\u4e0e\u5149\u4f0f\u54cd\u5e94\u7684\u7814\u7a76<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-217394 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/\u56fe\u7247-1-10.png\" alt=\"\" width=\"600\" height=\"405\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/\u56fe\u7247-1-10.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/\u56fe\u7247-1-10-300x203.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a\u201c<a href=\"https:\/\/science.sciencemag.org\/content\/371\/6529\/636\"><u>Reconfiguring the band-edge states of photovoltaic perovskites by conjugated organic cations<\/u><\/a>\u201d\uff08Science\uff0c2021\uff0cDOI\uff1a10.1126\/science.abd4860\uff09<\/p>\n<p>\u672c\u6587\u7531talent\u4f9b\u7a3f\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u5f15\u8a00 \u4e00\u822c\u5316\u5b66\u7ed3\u6784\u4e3aABX3 \u7684\u91d1\u5c5e\u5364\u5316\u9499\u949b\u77ff\u7684\u80fd\u5e26\u8fb9\u7f18(A\uff0c\u901a\u5e38\u4e3a\u4e00\u4ef7\u6709\u673a\u9633\u79bb\u5b50;B\uff0c\u4e8c\u4ef7\u9633\u79bb\u5b50;X\u662f\u5364\u5316\u7269\u9634\u79bb\u5b50)\u4e3b\u8981\u7531B\u548cX\u7684\u8f68\u9053\u7ec4\u6210\u3002\u56e0\u6b64\uff0c\u65e0\u673aB-X\u6846&#8230;<\/p>\n","protected":false},"author":11454,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-217393","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/217393"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/11454"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=217393"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/217393\/revisions"}],"predecessor-version":[{"id":217398,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/217393\/revisions\/217398"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=217393"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=217393"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=217393"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}