{"id":217984,"date":"2021-02-20T06:30:29","date_gmt":"2021-02-19T22:30:29","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=217984"},"modified":"2021-02-19T09:45:42","modified_gmt":"2021-02-19T01:45:42","slug":"angew-chem-int-ed%ef%bc%9a%e7%9f%b3%e5%a2%a8%e7%83%af-%e7%94%b5%e8%a7%a3%e6%b6%b2%e7%95%8c%e9%9d%a2%e7%94%b5%e5%ae%b9%e4%b8%ad%e7%9a%84%e6%ba%b6%e5%89%82%e5%8c%96%e6%95%88%e5%ba%94","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=217984","title":{"rendered":"Angew Chem Int Ed\uff1a\u77f3\u58a8\u70ef-\u7535\u89e3\u6db2\u754c\u9762\u7535\u5bb9\u4e2d\u7684\u6eb6\u5242\u5316\u6548\u5e94"},"content":{"rendered":"<p>\u7535\u5316\u5b66\u53cc\u5c42\u7535\u5bb9\u5668\uff08EDLC\uff09\uff0c\u4e5f\u79f0\u4e3a\u8d85\u7ea7\u7535\u5bb9\u5668\uff0c\u662f\u9ad8\u529f\u7387\u80fd\u91cf\u5b58\u50a8\u7684\u6700\u4f73\u9009\u62e9\u4e4b\u4e00\u3002 \u57fa\u4e8e\u7535\u6781\/\u7535\u89e3\u8d28\u754c\u9762\u5904\u7684\u975e\u6cd5\u62c9\u7b2c\u79bb\u5b50\u5438\u9644\/\u89e3\u5438\uff0cEDLC\u7684\u5bff\u547d\u53ef\u957f\u8fbe\u767e\u4e07\u6b21\uff0c\u5145\u7535\/\u653e\u7535\u65f6\u95f4\u77ed\u81f3\u6570\u79d2\u3002\u4e3a\u4e86\u8fdb\u4e00\u6b65\u63d0\u5347EDLC\u7684\u80fd\u91cf\u5b58\u50a8\u6027\u80fd\uff0c\u53d1\u5c55\u65b0\u578b\u78b3\u6750\u6599\u5e76\u7406\u89e3\u5176\u7535\u8377\u5b58\u50a8\u673a\u5236\u5df2\u6210\u4e3a\u91cd\u8981\u7684\u7814\u7a76\u8bfe\u9898\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-217985 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/1-11.png\" alt=\"\" width=\"600\" height=\"470\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/1-11.png 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/02\/1-11-300x235.png 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p style=\"text-align: center;\">\u7535\u5316\u5b66\u77f3\u82f1\u5fae\u6676\u5929\u5e73\u793a\u610f\u56fe\uff08\u5de6\uff09\uff0c\u6eb6\u5242\u5316\u79bb\u5b50\u6db2\u4f53\u4e2d\u77f3\u58a8\u70ef\u8868\u9762\u79bb\u5b50\u54cd\u5e94\uff08\u53f3\uff09<\/p>\n<p>\u7ee7\u6b64\u524d\u5173\u4e8e\u77f3\u58a8\u70ef\u5728\u7eaf\u79bb\u5b50\u6db2\u4f53\u7535\u89e3\u6db2\u4e2d\u7684\u79bb\u5b50\u5b58\u50a8\u673a\u5236\u7814\u7a76<sup>1<\/sup>\uff0c\u4e2d\u56fd\u79d1\u5b66\u6280\u672f\u5927\u5b66\u6731\u5f66\u6b66\u7814\u7a76\u5c0f\u7ec4\u548c\u6cd5\u56fd\u8428\u5df4\u8482\u5c14\u5927\u5b66\u7684Patrice Simon\u7814\u7a76\u5c0f\u7ec4\u8fdb\u4e00\u6b65\u5408\u4f5c\u7814\u7a76\u4e86\u6eb6\u5242\u5316\u79bb\u5b50\u6db2\u4f53\u5728\u5355\u5c42\u77f3\u58a8\u70ef\uff08SLG\uff09\u8868\u9762\u7684\u7535\u5316\u5b66\u53cc\u7535\u5c42\u54cd\u5e94\u673a\u5236<sup>2<\/sup>\u3002 \u901a\u8fc7\u7535\u5316\u5b66\u963b\u6297\u8c31\u548c\u7535\u5316\u5b66\u77f3\u82f1\u6676\u4f53\u5fae\u5929\u5e73\uff08EQCM\uff09\u6d4b\u8bd5\uff0c\u7814\u7a76\u53d1\u73b0\uff1a\u52a0\u5165\u6eb6\u5242\u540e\uff0c\u5355\u5c42\u77f3\u58a8\u70ef\u548c\u79bb\u5b50\u6db2\u4f53\u7684\u754c\u9762\u8f7d\u6d41\u5b50\u5bc6\u5ea6\u660e\u663e\u589e\u52a0\uff0c\u5f62\u6210\u6eb6\u5242\u589e\u5f3a\u7684\u53cc\u7535\u5c42\u7535\u5bb9\u6548\u5e94\uff1b\u800c\u79bb\u5b50\u52a8\u529b\u5b66\u884c\u4e3a\u4e5f\u4e0e\u7eaf\u79bb\u5b50\u6db2\u4f53\u4e2d\u7684\u54cd\u5e94\u622a\u7136\u4e0d\u540c\u3002\u7814\u7a76\u8ba4\u4e3a\uff0c\u5728\u7eaf\u79bb\u5b50\u6db2\u4f53\u4e2d\uff0c\u9634\u9633\u79bb\u5b50\u4e4b\u95f4\u7684\u5f3a\u5e93\u4f26\u4f5c\u7528\u5360\u636e\u4e3b\u5bfc\uff1b\u6eb6\u5242\u5b58\u5728\u65f6\uff0c\u79bb\u5b50\u4e0e\u6eb6\u5242\u5206\u5b50\u95f4\u7684\u4f5c\u7528\u4f7f\u5f97\u9634\u9633\u79bb\u5b50\u95f4\u4e4b\u95f4\u7684\u4f5c\u7528\u529b\u51cf\u5f31\uff0c\u56e0\u6b64\u5728\u53cc\u7535\u5c42\u5145\u7535\u65f6\u4f1a\u89c2\u5bdf\u5230\u660e\u663e\u7684\u53cd\u79bb\u5b50\u5438\u9644\uff08counter-ion adsorption\uff09\u6548\u5e94\u3002\u6b66\u6c49\u7406\u5de5\u5927\u5b66\u848b\u66f4\u5e73\u535a\u58eb\u534f\u52a9\u8fdb\u884c\u4e86\u5206\u5b50\u52a8\u529b\u5b66\u6a21\u62df\uff0c\u8fdb\u4e00\u6b65\u9a8c\u8bc1\u4e86\u4e0a\u8ff0\u7ed3\u679c\u3002<\/p>\n<p>\u8be5\u7814\u7a76\u4e5f\u8868\u660e\uff0c\u77f3\u58a8\u70ef\u754c\u9762\u7535\u5bb9\u5bf9\u78b3\u7ed3\u6784\u7279\u5f81-\u79bb\u5b50-\u6eb6\u5242\u5206\u5b50\u4e4b\u95f4\u7684\u590d\u6742\u76f8\u4e92\u4f5c\u7528\u9ad8\u5ea6\u654f\u611f\u3002\u5229\u7528\u5355\u5c42\u77f3\u58a8\u70ef\u4f5c\u4e3a\u7535\u6781\uff0c\u901a\u8fc7\u5fae\u6676\u5929\u5e73\u76f4\u63a5\u201c\u79f0\u91cd\u201d\u79bb\u5b50\uff0c\u5f00\u653e\u7535\u6781\u8868\u9762\u5df2\u7ecf\u5448\u73b0\u51fa\u4e0e\u591a\u5b54\u78b3\u7535\u6781\u4f8b\u5982\u6d3b\u6027\u70ad\u4e2d\u8fe5\u5f02\u7684\u7535\u8377\u5b58\u50a8\u673a\u7406\u3002\u7531\u4e8e\u77f3\u58a8\u70ef\u53ef\u4ee5\u88ab\u89c6\u4e3a\u6240\u6709\u5bfc\u7535\u78b3\u6750\u6599\u7684\u57fa\u672c\u7ed3\u6784\u5355\u5143\uff0c\u8be5\u7c7b\u5de5\u4f5c\u53ef\u671b\u4e3a\u78b3\u57fa\u8d85\u7ea7\u7535\u5bb9\u5668\u7684\u672a\u6765\u6539\u8fdb\u65b9\u6848\u63d0\u4f9b\u7406\u8bba\u57fa\u7840\u3002<\/p>\n<p>\u7814\u7a76\u6210\u679c\u4ee5\u201cElectrochemical characterization of single layer graphene \/ electrolyte interface: effect of solvent on the interfacial capacitance\u201d\u4e3a\u9898\u53d1\u8868\u5728\u6742\u5fd7\u300aAngew Chem Int Ed\u300b\u3002\u8be5\u7814\u7a76\u5de5\u4f5c\u5f97\u5230\u4e86\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u57fa\u91d1\u59d4\u3001the Agence Nationale de la Recherche\u3001\u56fd\u5bb6\u7559\u5b66\u57fa\u91d1\uff08CSC\uff09\u9879\u76ee\u7684\u652f\u6301\u3002<\/p>\n<p>1. Ye, J.; Wu, Y.-C.; Xu, K.; Ni, K.; Shu, N.; Taberna, P.-L.; Zhu, Y.; Simon, P., Charge Storage Mechanisms of Single-Layer Graphene in Ionic Liquid. Journal of the American Chemical Society 2019, 141 (42), 16559-16563.<\/p>\n<p>2. Wu, Y.; Ye, J.; Jiang, G.; Ni, K.; Shu, N.; Taberna, P.; Zhu, Y.; and Simon, P., Electrochemical characterization of single layer graphene \/ electrolyte interface: effect of solvent on the interfacial capacitance. Angew. Chem. Int. Ed., 2021, https:\/\/doi.org\/10.1002\/anie.202017057.<\/p>\n<p>\u672c\u6587\u7531\u4f5c\u8005\u6295\u7a3f\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u7535\u5316\u5b66\u53cc\u5c42\u7535\u5bb9\u5668\uff08EDLC\uff09\uff0c\u4e5f\u79f0\u4e3a\u8d85\u7ea7\u7535\u5bb9\u5668\uff0c\u662f\u9ad8\u529f\u7387\u80fd\u91cf\u5b58\u50a8\u7684\u6700\u4f73\u9009\u62e9\u4e4b\u4e00\u3002 \u57fa\u4e8e\u7535\u6781\/\u7535\u89e3\u8d28\u754c\u9762\u5904\u7684\u975e\u6cd5\u62c9\u7b2c\u79bb\u5b50\u5438\u9644\/\u89e3\u5438\uff0cEDLC\u7684\u5bff\u547d\u53ef\u957f\u8fbe\u767e\u4e07\u6b21\uff0c\u5145&#8230;<\/p>\n","protected":false},"author":11454,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-217984","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/217984"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/11454"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=217984"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/217984\/revisions"}],"predecessor-version":[{"id":217986,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/217984\/revisions\/217986"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=217984"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=217984"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=217984"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}