{"id":222056,"date":"2021-05-17T06:56:10","date_gmt":"2021-05-16T22:56:10","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=222056"},"modified":"2021-05-16T22:36:21","modified_gmt":"2021-05-16T14:36:21","slug":"adv-electron-mater-%e9%9d%a2%e5%90%91%e6%99%b6%e5%9c%86%e7%ba%a7%e7%9a%84%e4%ba%8c%e7%bb%b4%e8%bf%87%e6%b8%a1%e9%87%91%e5%b1%9e%e7%a1%ab%e6%97%8f%e5%8c%96%e5%90%88%e7%89%a9%e6%9d%90","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=222056","title":{"rendered":"Adv. Electron. Mater: \u9762\u5411\u6676\u5706\u7ea7\u7684\u4e8c\u7ef4\u8fc7\u6e21\u91d1\u5c5e\u786b\u65cf\u5316\u5408\u7269\u6750\u6599"},"content":{"rendered":"<p>\u534a\u5bfc\u4f53\u4ea7\u4e1a\u7684\u53d1\u5c55\u7531\u4e8e\u5c3a\u5bf8\u7f29\u5c0f\u9047\u5230\u7684\u91cf\u5b50\u6548\u5e94\u74f6\u9888\u800c\u6025\u5207\u5730\u547c\u5524\u4e0b\u4e00\u4ee3\u7684\u7535\u5b50\u6750\u6599\u3002\u4e8c\u7ef4\u6750\u6599\u7531\u4e8e\u539f\u5b50\u7ea7\u7684\u539a\u5ea6\u3001\u5728\u4f4e\u7ef4\u4e0b\u663e\u793a\u51fa\u4e0d\u540c\u4e8e\u4f53\u76f8\u6750\u6599\u7684\u5d2d\u65b0\u7684\u6027\u8d28\u3001\u4e0e\u73b0\u6709\u7684\u7535\u5b50\u5de5\u4e1a\u5de5\u827a\u80fd\u878d\u5408\u7684\u7279\u70b9\uff0c\u662f\u5f53\u4eca\u6750\u6599\u7814\u7a76\u7684\u70ed\u70b9\u3002\u800c\u8fc7\u6e21\u91d1\u5c5e\u786b\u65cf\u5316\u7269\uff08Transition Metal Chalcogenides\uff09\u62e5\u6709\u6781\u4f18\u5f02\u7684\u6027\u8d28\uff0c\u4f8b\u5982\u79cd\u7c7b\u548c\u6027\u8d28\u7684\u591a\u6837\u6027\uff0c\u80fd\u5e26\u7ed3\u6784\u4e2d\u5b58\u5728\u5e26\u9699\uff0c\u7535\u5b50\u7ed3\u6784\u7684\u5c42\u6570\u53ef\u8c03\u6027\uff0c\u80fd\u8c37\u6781\u5316\u5bfc\u81f4\u7684\u504f\u632f\u6001\u5dee\u522b\uff0c\u662f\u4e00\u79cd\u6781\u5177\u6f5c\u529b\u7684\u4e8c\u7ef4\u534a\u5bfc\u4f53\u7535\u5b50\u6750\u6599\uff0c\u6709\u671b\u6210\u4e3a\u65b0\u4e00\u4ee3\u5149\u7535\u5b50\u5668\u4ef6\u3001\u91cf\u5b50\u4fe1\u606f\u5668\u4ef6\u548c\u81ea\u65cb\u5668\u4ef6\u7684\u5173\u952e\u7ec4\u6210\u90e8\u5206\uff0c\u5f15\u8d77\u4e86\u4ea7\u5b66\u7814\u754c\u5e7f\u6cdb\u7684\u5174\u8da3\u3002\u800c\u5236\u5907\u6676\u5706\u7ea7\u7684\u4e8c\u7ef4\u8fc7\u6e21\u91d1\u5c5e\u786b\u65cf\u5316\u7269\u662f\u8fd9\u79cd\u6750\u6599\u8d70\u5411\u4ea7\u4e1a\u5e94\u7528\u7684\u5173\u952e\u548c\u5177\u6709\u6311\u6218\u6027\u7684\u4e00\u6b65\u3002<\/p>\n<p>\u8fd1\u65e5\u6d59\u6c5f\u5927\u5b66\u676d\u5dde\u56fd\u9645\u79d1\u521b\u4e2d\u5fc3\u5148\u8fdb\u534a\u5bfc\u4f53\u7814\u7a76\u9662<strong>\u738b\u4f69\u5251\u7814\u7a76\u5458<\/strong>\u5728\u7535\u5b50\u6750\u6599\u9886\u57df\u56fd\u9645\u77e5\u540d\u671f\u520a<em>Advanced Electronic Materials<\/em>\u53d1\u8868\u4e86\u9898\u4e3aTowards Wafer-Scale Production of Two-Dimensional Transition Metal Chalcogenides\u7684\u7efc\u8ff0\u6587\u7ae0\uff0c\u7cfb\u7edf\u5168\u9762\u5730\u603b\u7ed3\u4e86\u6676\u5706\u7ea7\u4e8c\u7ef4\u8fc7\u6e21\u91d1\u5c5e\u786b\u65cf\u5316\u7269\u6750\u6599\u7684\u6700\u65b0\u8fdb\u5c55\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-222073\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/000.jpg\" alt=\"\" width=\"1263\" height=\"695\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/000.jpg 1263w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/000-300x165.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/000-768x423.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/000-1024x563.jpg 1024w\" sizes=\"(max-width: 1263px) 100vw, 1263px\" \/><\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p>\u672c\u6587\u5f00\u7bc7\u603b\u7ed3\u4e86\u4e8c\u7ef4\u8fc7\u6e21\u91d1\u5c5e\u786b\u65cf\u5316\u7269\u7684\u4f18\u5f02\u7684\u6027\u8d28\u548c\u4ece\u5176\u4ed6\u4e8c\u7ef4\u6750\u6599\u4e2d\u8131\u9896\u800c\u51fa\u7684\u539f\u56e0\u3002\u968f\u540e\uff0c\u4f5c\u8005\u603b\u7ed3\u4e86\u5f53\u4eca\u751f\u957f\u6676\u5706\u7ea7\u4e8c\u7ef4\u8fc7\u6e21\u91d1\u5c5e\u786b\u65cf\u5316\u7269\u7684\u5404\u79cd\u65b9\u6cd5\u3001\u751f\u957f\u673a\u5236\u3001\u751f\u957f\u5c3a\u5bf8\u3001\u6676\u4f53\u8d28\u91cf\u3001\u5668\u4ef6\u6027\u8d28\uff0c\u5e76\u5206\u6790\u4e86\u4e0d\u540c\u65b9\u6cd5\u5404\u81ea\u7684\u4f18\u52bf\u548c\u52a3\u52bf\u3002\u968f\u5373\uff0c\u4f5c\u8005\u5206\u6790\u4e86\u6676\u5706\u7ea7\u751f\u957f\u7684\u5404\u79cd\u8c03\u63a7\u56e0\u7d20\uff0c\u4f8b\u5982\u6676\u7574\u5c3a\u5bf8\u3001\u8868\u9762\u5f62\u8c8c\u3001\u5c42\u6570\u3001\u76f8\u7ed3\u6784\u7b49\uff0c\u5e76\u5206\u522b\u5206\u6790\u548c\u63d0\u51fa\u4e86\u8c03\u63a7\u7684\u7b56\u7565\u3002\u7136\u540e\uff0c\u4f5c\u8005\u5c55\u73b0\u4e86\u73b0\u6709\u7684\u6676\u5706\u7ea7\u4e8c\u7ef4\u8fc7\u6e21\u91d1\u5c5e\u786b\u65cf\u5316\u7269\u7684\u5668\u4ef6\u5e94\u7528\u548c\u5173\u952e\u6307\u6807\uff0c\u4e3b\u8981\u662f\u7535\u5b50\u5b66\u5e94\u7528\u3001\u5149\u7535\u5b50\u5b66\u5e94\u7528\u548c\u5176\u4ed6\u7684\u4e00\u4e9b\u5e94\u7528\uff0c\u5e76\u63d0\u51fa\u4e86\u4e00\u4e9b\u4f18\u5316\u7684\u7b56\u7565\u3002\u6700\u540e\uff0c\u4f5c\u8005\u6307\u51fa\u4e86\u6676\u5706\u7ea7\u4e8c\u7ef4\u8fc7\u6e21\u91d1\u5c5e\u786b\u65cf\u5316\u7269\u9762\u4e34\u7684\u4e3b\u8981\u6311\u6218\uff08\u4f8b\u5982\u5355\u6676\u6027\u3001\u751f\u957f\u88c5\u7f6e\u548c\u6761\u4ef6\u7684\u521b\u65b0\u3001\u6750\u6599\u79cd\u7c7b\u548c\u5e94\u7528\u7684\u6269\u5145\u3001\u5f02\u8d28\u7ed3\u76f4\u63a5\u751f\u957f\u7b49\uff09\uff0c\u63d0\u51fa\u4e86\u672a\u6765\u6676\u5706\u7ea7\u6750\u6599\u7684\u4f18\u5316\u601d\u8def\u548c\u53d1\u5c55\u65b9\u5411\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-222074\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/002.jpg\" alt=\"\" width=\"270\" height=\"260\" \/><\/p>\n<p>\u8fd1\u5e74\u6765\u4e0d\u540c\u65b9\u6cd5\u751f\u957fTMC\u6700\u5927\u5c3a\u5bf8\u53d8\u5316\u6c14\u6ce1\u793a\u610f\u56fe\uff1a<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-222068\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/1-7.jpg\" alt=\"\" width=\"1320\" height=\"860\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/1-7.jpg 1320w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/1-7-300x195.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/1-7-768x500.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/1-7-1024x667.jpg 1024w\" sizes=\"(max-width: 1320px) 100vw, 1320px\" \/><\/p>\n<p>&nbsp;<\/p>\n<p>\u65b9\u6cd5\u793a\u4f8b\uff1aMOCVD<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-222069\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/2-6.jpg\" alt=\"\" width=\"1320\" height=\"831\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/2-6.jpg 1320w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/2-6-300x189.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/2-6-768x483.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/2-6-1024x645.jpg 1024w\" sizes=\"(max-width: 1320px) 100vw, 1320px\" \/><\/p>\n<p>\u5bf9\u4e8e\u6676\u7574\u5c3a\u5bf8\u5927\u5c0f\u7684\u63a7\u5236\uff1a<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-222070\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/3-6.jpg\" alt=\"\" width=\"1320\" height=\"1016\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/3-6.jpg 1320w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/3-6-300x231.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/3-6-768x591.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/3-6-1024x788.jpg 1024w\" sizes=\"(max-width: 1320px) 100vw, 1320px\" \/><\/p>\n<p>\u6676\u5706\u7ea7\u4e8c\u7ef4\u8fc7\u6e21\u91d1\u5c5e\u786b\u65cf\u5316\u7269\u7535\u5b50\u5b66\u5668\u4ef6\u5e94\u7528\uff1a<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-222071\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/4-7.jpg\" alt=\"\" width=\"1239\" height=\"882\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/4-7.jpg 1239w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/4-7-300x214.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/4-7-768x547.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/4-7-1024x729.jpg 1024w\" sizes=\"(max-width: 1239px) 100vw, 1239px\" \/><\/p>\n<p>\u6676\u5706\u7ea7\u4e8c\u7ef4\u8fc7\u6e21\u91d1\u5c5e\u786b\u65cf\u5316\u7269\u5149\u7535\u5b50\u5b66\u53ca\u5176\u4ed6\u5e94\u7528\uff1a<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-222072\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/5-5.jpg\" alt=\"\" width=\"1233\" height=\"894\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/5-5.jpg 1233w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/5-5-300x218.jpg 300w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/5-5-768x557.jpg 768w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/05\/5-5-1024x742.jpg 1024w\" sizes=\"(max-width: 1233px) 100vw, 1233px\" \/><\/p>\n<p>\u603b\u800c\u8a00\u4e4b\uff0c\u8be5\u7efc\u8ff0\u53ca\u65f6\u8be6\u7ec6\u603b\u7ed3\u4e86\u5f53\u4eca\u6676\u5706\u7ea7\u4e8c\u7ef4\u8fc7\u6e21\u91d1\u5c5e\u786b\u65cf\u5316\u7269\u7684\u751f\u957f\u548c\u5e94\u7528\uff0c\u5176\u4e2d\u4e00\u4e9b<strong>\u5bcc\u6709\u72ec\u521b\u6027\u7684\u89c6\u89d2\u548c\u8bc4\u8ff0<\/strong>\uff0c\u4e3a\u8be5\u9886\u57df\u7684\u53d1\u5c55\u63d0\u4f9b\u4e86\u89c1\u89e3\u3001\u6307\u660e\u4e86\u52a8\u5411\u3002<\/p>\n<p>\u6d59\u5927\u676d\u5dde\u79d1\u521b\u4e2d\u5fc3\u5148\u8fdb\u534a\u5bfc\u4f53\u7814\u7a76\u9662\u805a\u534a\u5bfc\u4f53\u9886\u57df\u7684\u56fd\u9645\u524d\u6cbf\u548c\u91cd\u5927\u79d1\u5b66\u95ee\u9898\uff0c\u7784\u51c6\u56fd\u5bb6\u5728\u4fe1\u606f\u3001\u80fd\u6e90\u7b49\u9886\u57df\u7684\u91cd\u5927\u6218\u7565\u9700\u6c42\uff0c\u4f9d\u6258\u957f\u4e09\u89d2\u533a\u57df\u9886\u5148\u7684\u4ea7\u4e1a\u4f18\u52bf\u3001\u6d59\u6c5f\u5927\u5b66\u96c4\u539a\u7684\u79d1\u7814\u5b9e\u529b\u548c\u676d\u5dde\u79d1\u521b\u4e2d\u5fc3\u521b\u65b0\u7684\u4f53\u5236\u673a\u5236\uff0c\u7740\u529b\u6253\u9020\u4e00\u4e2a\u56fd\u5185\u9886\u5148\u3001\u56fd\u9645\u5148\u8fdb\u7684\u524d\u6cbf\u6280\u672f\u521b\u65b0\u7814\u53d1\u5e73\u53f0\uff0c\u63a8\u52a8\u4ea7\u5b66\u7814\u6df1\u5ea6\u878d\u5408\u53d1\u5c55\u3002\u524d\u6cbf\u4ea4\u53c9\u7814\u7a76\u7ec4\u96b6\u5c5e\u4e8e\u5148\u8fdb\u534a\u5bfc\u4f53\u7814\u7a76\u9662\u534a\u5bfc\u4f53\u6750\u6599\u7814\u7a76\u5ba4\uff0c\u4e3b\u8981\u7814\u7a76\u65b9\u5411\u662f<strong>\u4e8c\u7ef4\u6750\u6599\u548c\u5bbd\u7981\u5e26\u534a\u5bfc\u4f53\u524d\u6cbf\u4ea4\u53c9\u65b9\u5411\u53ca\u4e24\u8005\u5f62\u6210\u5f02\u8d28\u7ed3\u5728\u7d2b\u5916\u5149\u7535\u63a2\u6d4b\u4e0a\u7684\u5e94\u7528<\/strong>\uff0c \u5e76\u4e14\u548c\u7814\u7a76\u5ba4\u5185\u5176\u4ed6\u65b9\u5411\u4e0a\u5c55\u5f00\u5408\u4f5c\u3002\u7814\u7a76\u7ec4\u4f9d\u6258\u79d1\u521b\u4e2d\u5fc3\u548c\u6d59\u6c5f\u5927\u5b66\u7845\u6750\u6599\u56fd\u5bb6\u91cd\u70b9\u5b9e\u9a8c\u5ba4\u4ee5\u53ca\u5fae\u7eb3\u52a0\u5de5\u5e73\u53f0\u7b49\u5f3a\u5927\u5e73\u53f0\uff0c\u62e5\u6709\u7b49\u79bb\u5b50\u589e\u5f3a\u5316\u5b66\u6c14\u76f8\u6c89\u79ef\uff0c\u8109\u51b2\u6fc0\u5149\u6c89\u79ef\u3001\u8584\u819c\u6c89\u79ef\u7cfb\u7edf\u7b49\u5148\u8fdb\u8bbe\u5907\u3002<\/p>\n<p>\u8bba\u6587\u94fe\u63a5\uff1ahttps:\/\/onlinelibrary.wiley.com\/doi\/10.1002\/aelm.202100278<\/p>\n<p><strong>\u3010\u4f5c\u8005\u4ecb\u7ecd\u3011<\/strong><\/p>\n<p>\u738b\u4f69\u5251\u7814\u7a76\u5458\u5728\u5317\u4eac\u5927\u5b66\u5143\u57f9\u5b66\u9662, \u7f8e\u56fdUniversity of Pennsylvania, \u7f8e\u56fdUniversity of Massachusetts, Amherst\u5206\u522b\u83b7\u5f97\u7269\u7406\u5b66\u5b66\u58eb\u3001\u6750\u6599\u79d1\u5b66\u4e0e\u5de5\u7a0b\u7855\u58eb\u3001\u7269\u7406\u5b66\u535a\u58eb\u5b66\u4f4d\uff0c\u968f\u540e\u5728\u7f8e\u56fd\u7ebd\u7ea6\u5dde\u7acb\u5927\u5b66(Buffalo)\u7269\u7406\u7cfb\u505a\u535a\u58eb\u540e\u7814\u7a76\u30022021\u5e74\u52a0\u5165\u6d59\u6c5f\u5927\u5b66\u56fd\u9645\u79d1\u521b\u4e2d\u5fc3\u5148\u8fdb\u534a\u5bfc\u4f53\u7814\u7a76\u9662\u3002\u8fd1\u4e09\u5e74\u6765\u5728<em>ACS Nano, Nano Lett., Appl.Phys.Rev., Nat. Comm., Adv.Mater., Chem. Sci.<\/em>\u7b49\u56fd\u9645\u6743\u5a01\u671f\u520a\u53d1\u8868\u8bba\u658712\u7bc7(8\u7bc7\u4e2d\u79d1\u9662\u4e00\u533a)\uff0c\u5176\u4e2d\u7b2c\u4e00\u4f5c\u8005\/\u5171\u540c\u4e00\u4f5c7\u7bc7\uff0c\u7533\u8bf72\u9879\u4e13\u5229\u3002\u4e3b\u6301\u56fd\u5bb6\u81ea\u7136\u79d1\u5b66\u57fa\u91d1\u9752\u5e74\u57fa\u91d1\u4e00\u9879\uff08\u5728\u7814\uff09\u3002\u53d7\u9080\u4e3a<em>J. Magn. Magn. Mater.\u3001Nanoscale\u3001JPCC<\/em>\u7b49\u56fd\u9645\u520a\u7269\u5ba1\u7a3f\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u534a\u5bfc\u4f53\u4ea7\u4e1a\u7684\u53d1\u5c55\u7531\u4e8e\u5c3a\u5bf8\u7f29\u5c0f\u9047\u5230\u7684\u91cf\u5b50\u6548\u5e94\u74f6\u9888\u800c\u6025\u5207\u5730\u547c\u5524\u4e0b\u4e00\u4ee3\u7684\u7535\u5b50\u6750\u6599\u3002\u4e8c\u7ef4\u6750\u6599\u7531\u4e8e\u539f\u5b50\u7ea7\u7684\u539a\u5ea6\u3001\u5728\u4f4e\u7ef4\u4e0b\u663e\u793a\u51fa\u4e0d\u540c\u4e8e\u4f53\u76f8\u6750\u6599\u7684\u5d2d\u65b0\u7684\u6027\u8d28\u3001\u4e0e\u73b0\u6709\u7684\u7535\u5b50\u5de5\u4e1a&#8230;<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[2],"tags":[],"class_list":["post-222056","post","type-post","status-publish","format-standard","hentry","category-keji"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/222056"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=222056"}],"version-history":[{"count":3,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/222056\/revisions"}],"predecessor-version":[{"id":222077,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/222056\/revisions\/222077"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=222056"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=222056"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=222056"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}