{"id":223000,"date":"2021-06-10T06:15:57","date_gmt":"2021-06-09T22:15:57","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=223000"},"modified":"2021-06-09T22:19:28","modified_gmt":"2021-06-09T14:19:28","slug":"%e3%80%90%e5%9b%bd%e5%a4%96%e6%96%87%e7%8c%ae%e3%80%91nature%e8%af%84%e8%bf%b0%ef%bc%9a%e6%9e%84%e7%ad%91%e5%85%b7%e6%9c%89%e7%b1%bb%e9%92%99%e9%92%9b%e7%9f%bf%e7%bb%93%e6%9e%84%e8%b6%85%e8%8d%a7","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=223000","title":{"rendered":"Nature\u8bc4\u8ff0\uff1a\u6784\u7b51\u5177\u6709\u7c7b\u9499\u949b\u77ff\u7ed3\u6784\u8d85\u8367\u5149\u6676\u683c\u7684\u7eb3\u7c73\u6676"},"content":{"rendered":"<p><strong>\u3010\u7814\u7a76\u80cc\u666f\u3011<\/strong><\/p>\n<p>\u9499\u949b\u77ff\u6676\u4f53\u662f\u76ee\u524d\u5e7f\u53d7\u5173\u6ce8\uff0c\u5176\u81f3\u5c11\u7531\u4e09\u79cd\u4e0d\u540c\u7684\u79bb\u5b50\u7ec4\u6210\uff0c\u4ee5\u5353\u8d8a\u7684\u7535\u5b66\u548c\u5149\u5b66\u7279\u6027\u800c\u95fb\u540d\uff0c\u5728\u592a\u9633\u80fd\u7535\u6c60\u548c\u5149\u7535\u5668\u4ef6\u4e2d\u5177\u6709\u7a81\u51fa\u7684\u5e94\u7528\u6f5c\u529b\u3002\u6709\u7814\u7a76\u8868\u660e\uff0c\u5f53\u9499\u949b\u77ff\u7684\u7eb3\u7c73\u7acb\u65b9\u4f53\u4e0e\u5176\u4ed6\u6750\u6599\u7684\u7eb3\u7c73\u7403\u7ed3\u5408\u65f6\uff0c\u65e0\u8bba\u662f\u5426\u6709\u7b2c\u4e09\u7c7b\u7eb3\u7c73\u6676\u4f53\uff0c\u6240\u83b7\u5f97\u7684\u5404\u79cd\u7eb3\u7c73\u7ed3\u6784\u90fd\u53ef\u4ee5\u6392\u5217\u6210\u4e09\u7ef4\u201c\u8d85\u6676\u683c\u201d\uff0c\u5176\u6392\u5217\u65b9\u5f0f\u4e0e\u9499\u949b\u77ff\u4e2d\u7684\u79bb\u5b50\u6676\u683c\u76f8\u540c\u3002\u6b64\u5916\uff0c\u7eb3\u7c73\u7acb\u65b9\u4f53\u5728\u8d85\u6676\u683c\u4e2d\u7684\u9ad8\u5ea6\u6709\u5e8f\u53d6\u5411\u5bfc\u81f4\u4e86\u8d85\u8367\u5149\u73b0\u8c61\uff0c\u8fd9\u662f\u4e00\u79cd\u53ef\u80fd\u5177\u6709\u5b9e\u9645\u5e94\u7528\u7684\u5149\u5b50\u96c6\u4f53\u7206\u53d1\u3002\u81ea1993\u5e74\u9996\u6b21\u62a5\u9053\u4e86\u5236\u5907\u76f8\u540c\u5c3a\u5bf8\u548c\u5f62\u72b6\u7684\u7eb3\u7c73\u6676\u7684\u65b9\u6cd5\u540e\uff0c\u7814\u7a76\u4eba\u5458\u5f00\u59cb\u5236\u5907\u7531\u5355\u5206\u6563\u7eb3\u7c73\u6676\u6784\u6210\u7684\u8d85\u6676\u683c\u3002\u4ece\u6b64\u79d1\u5b66\u5bb6\u5c31\u80fd\u5b9a\u5236\u5404\u79cd\u5404\u6837\u7684\u7eb3\u7c73\u6676\u4f53\u5f62\u72b6\u548c\u5c3a\u5bf8\uff0c\u5e76\u63a7\u5236\u5b83\u4eec\u4e4b\u95f4\u7684\u76f8\u4e92\u4f5c\u7528\u548c\u73af\u5883\uff0c\u4ece\u800c\u5236\u9020\u51fa\u8303\u56f4\u5e7f\u6cdb\u7684\u7eb3\u7c73\u6676\u4f53\u8d85\u6676\u683c\u3002<\/p>\n<p><strong>\u3010\u6210\u679c\u7b80\u4ecb\u3011<\/strong><\/p>\n<p>\u8fd1\u65e5\uff0c<strong>\u5fb7\u56fd\u675c\u4f0a\u65af\u5821<\/strong><strong>&#8211;<\/strong><strong>\u57c3\u68ee\u5927\u5b66<\/strong><strong>Gerd Bacher<\/strong><strong>\u6559\u6388<\/strong>\u89e3\u8bfb\u4e86\u5177\u6709\u5b9a\u5236\u5f62\u72b6\u548c\u6210\u5206\u7684\u7eb3\u7c73\u6676\u4f53\u5df2\u88ab\u8bc1\u660e\u5f62\u6210\u7c7b\u4f3c\u4e8e\u9499\u949b\u77ff\u5316\u5408\u7269\u7684\u79bb\u5b50\u6676\u683c\u7684\u201c\u8d85\u6676\u683c\u201d\u9635\u5217\u7684\u8bba\u8457\uff0c\u540c\u65f6\u8868\u660e\u5176\u4e2d\u4e00\u79cd\u8d85\u6676\u683c\u8868\u73b0\u51fa\u4e00\u79cd\u53eb\u505a\u8d85\u8367\u5149\u7684\u73b0\u8c61\u3002\u8be5\u8bba\u6587\u4ee5\u9898\u4e3a\u201c<strong>Nanocrystals form a superfluorescent lattice mimicking the atomic structure of perovskite materials<\/strong>\u201d\u53d1\u8868\u5728\u77e5\u540d\u671f\u520a<strong>Nature<\/strong>\u4e0a\u3002<\/p>\n<p><strong>\u3010\u56fe\u6587\u5bfc\u8bfb\u3011<\/strong><\/p>\n<p>Cherniukh\u7b49\u4eba\u901a\u8fc7\u5b9e\u9a8c\u8bc1\u660e\uff0c\u7acb\u65b9\u548c\u7403\u5f62\u7a7a\u95f4\u7a33\u5b9a\u7eb3\u7c73\u6676\u4f53\u7684\u5171\u7ec4\u88c5\u5728\u5b9e\u9a8c\u4e0a\u662f\u53ef\u80fd\u7684\uff0c\u800c\u9499\u949b\u77ff\u7eb3\u7c73\u6676\u4f53\u7684\u7acb\u65b9\u5f62\u72b6\u5bfc\u81f4\u4e86\u4e0e\u5168\u7403\u5f62\u7cfb\u7edf\u76f8\u6bd4\u622a\u7136\u4e0d\u540c\u7684\u7ed3\u679c\u3002\u4f5c\u8005\u901a\u8fc7\u5c06\u9499\u949b\u77ffCsPbBr<sub>3<\/sub>\u7684\u7eb3\u7c73\u7acb\u65b9\u4f53\u4e0e\u94c1\u6c27\u5316\u7269\uff08Fe<sub>3<\/sub>O<sub>4<\/sub>\uff09\u6216NdGdF<sub>4<\/sub>\u7684\u7403\u5f62\u7eb3\u7c73\u6676\u4f53\u6df7\u5408\uff0c\u83b7\u5f97\u4e86\u4e8c\u5143\u8d85\u6676\u4f53\u3002\u800c\u901a\u8fc7\u5728\u6df7\u5408\u7269\u4e2d\u52a0\u5165\u622a\u65ad\u7acb\u65b9\u4f53\u786b\u5316\u94c5\u7eb3\u7c73\u7c92\u5b50\uff0c\u4ed6\u4eec\u83b7\u5f97\u4e86\u4e09\u5143\u8d85\u6676\u683c\u3002\u8fc7\u6c27\u5316\u7269\u7684\u4e00\u822c\u516c\u5f0f\u662fABO<sub>3<\/sub>\uff0c\u5176\u4e2dA\u548cB\u4ee3\u8868\u5e26\u6b63\u7535\u7684\u79bb\u5b50\uff0c\u4e09\u4e2a\u6c27\u539f\u5b50\u662f\u5e26\u8d1f\u7535\u7684\u6c27\u5316\u7269\u79bb\u5b50\u3002\u5728\u4e09\u5143\u8d85\u6676\u683c\u4e2d\uff0c\u7eb3\u7c73\u7acb\u65b9\u4f53\u91c7\u7528\u7684\u6676\u683c\u4f4d\u7f6e\u76f8\u5f53\u4e8e\u6c27\u5316\u7269\u79bb\u5b50\u5728\u8fc7\u6c27\u5316\u7269\u6676\u683c\u4e2d\u7684\u4f4d\u7f6e\uff0c\u7403\u5f62\u7eb3\u7c73\u6676\u4f53\u5360\u636e\u4e86A\u4f4d\uff0c\u800cPbS\u7eb3\u7c73\u6676\u4f53\u5360\u636e\u4e86B\u4f4d\uff08\u56fea\uff09\u3002<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter size-full wp-image-223001\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/06\/1-1.jpg\" alt=\"\" width=\"600\" height=\"317\" srcset=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/06\/1-1.jpg 600w, http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/06\/1-1-300x159.jpg 300w\" sizes=\"(max-width: 600px) 100vw, 600px\" \/><\/p>\n<p><strong>\u7c7b\u9499\u949b\u77ff\u8d85\u6676\u683c\u7684\u7eb3\u7c73\u6676\u4f53\u3002<\/strong>\uff08a\uff09\u7403\u5f62\u3001\u7acb\u65b9\u4f53\u548c\u622a\u77ed\u7acb\u65b9\u4f53\u7eb3\u7c73\u6676\u4f53\u7684\u7ec4\u5408\u53ef\u4ee5\u5f62\u6210\u7c7b\u4f3c\u4e8e\u79bb\u5b50\u8fc7\u6c27\u5316\u7269\u6676\u683c\u7ed3\u6784\u7684\u6709\u5e8f\u6392\u5217\u3002\uff08b\uff09\u5728\u6ca1\u6709\u622a\u65ad\u7684\u7acb\u65b9\u4f53\u7eb3\u7c73\u6676\u4f53\u7684\u60c5\u51b5\u4e0b\u4e5f\u4f1a\u5f62\u6210\u8d85\u6676\u683c\u3002<\/p>\n<p>&nbsp;<\/p>\n<p>\u5728\u79bb\u5b50\u578b\u9499\u949b\u77ff\u6676\u4f53\u4e2d\uff0c\u81f3\u5c11\u9700\u8981\u4e09\u79cd\u4e0d\u540c\u534a\u5f84\u7684\u79bb\u5b50\u624d\u80fd\u5f62\u6210\u5177\u6709\u7279\u5f81\u7684\u9499\u949b\u77ff\u6676\u683c\u3002\u76f8\u6bd4\u4e4b\u4e0b\uff0cCherniukh\u7b49\u4eba\u89c2\u5bdf\u5230\uff0c\u7c7b\u9499\u949b\u77ff\u8d85\u6676\u683c\u53ef\u4ee5\u53ea\u4f7f\u7528\u4e24\u79cd\u7c7b\u578b\u7684\u7eb3\u7c73\u6676\u4f53\u3002\u8fd9\u662f\u56e0\u4e3a\u957f\u65b9\u4f53\u7eb3\u7c73\u6676\u4f53\u5177\u6709\u65cb\u8f6c\u81ea\u7531\u5ea6\u3002\u8fd9\u4e9b\u7eb3\u7c73\u6676\u4f53\u7684\u7acb\u65b9\u5f62\u72b6\u548c\u8868\u9762\u53ef\u53d8\u5f62\u6027\u4f7f\u5f97\u5b83\u4eec\u5728\u8d85\u6676\u683c\u4e2d\u88ab\u9501\u5b9a\u5728\u7279\u5b9a\u7684\u65b9\u5411\u4e0a\u3002<\/p>\n<p>\u6b64\u5916\uff0c\u4f5c\u8005\u8fd8\u53d1\u73b0\uff0c\u5bf9\u4e8e\u7531CsPbBr<sub>3<\/sub>\u7eb3\u7c73\u7acb\u65b9\u4f53\u548cFe<sub>3<\/sub>O<sub>4<\/sub>\u7eb3\u7c73\u7403\u7ec4\u6210\u7684\u4f53\u7cfb\uff0c\u4e24\u79cd\u7eb3\u7c73\u6676\u4f53\u7684\u76f8\u5bf9\u5c3a\u5bf8\u548c\u5206\u6570\u7684\u5fae\u5c0f\u53d8\u5316\u53ef\u4ee5\u5c06\u4ea7\u751f\u7684\u8d85\u6676\u683c\u4ece\u7acb\u65b9\u6392\u5217\u8f6c\u53d8\u4e3aABO<sub>3<\/sub>\u6392\u5217\uff08\u56feb\uff09\u3002\u5bf9\u8fd9\u4e9b\u4e8c\u5143\u8d85\u6676\u683c\u7684\u9ad8\u5206\u8fa8\u900f\u5c04\u7535\u5b50\u663e\u5fae\u955c\u548c\u7535\u5b50\u884d\u5c04\u7814\u7a76\u8868\u660e\uff0c\u7eb3\u7c73\u7acb\u65b9\u4f53\u7684\u53d6\u5411\u662f\u9ad8\u5ea6\u6709\u5e8f\u7684\u3002\u76f8\u6bd4\u4e4b\u4e0b\uff0c\u7403\u5f62\u7eb3\u7c73\u9897\u7c92\u4e2d\u6676\u683c\u7684\u8f74\u7ebf\u5177\u6709\u968f\u673a\u53d6\u5411\u3002<\/p>\n<p>\u5148\u524d\u5df2\u5728\u4ec5\u7531CsPbBr<sub>3<\/sub>\u7eb3\u7c73\u7acb\u65b9\u4f53\u5f62\u6210\u7684\u8d85\u6676\u683c\u4e2d\u89c2\u5bdf\u5230\u8d85\u8367\u5149\u3002\u7136\u800c\uff0cCherniukh\u53ca\u5176\u540c\u4e8b\u7684\u8d85\u6676\u683c\u4e2d\u9ad8\u8367\u5149CsPbBr<sub>3<\/sub>\u7eb3\u7c73\u7acb\u65b9\u4f53\u7684\u5468\u671f\u6027\u3001\u5806\u79ef\u5bc6\u5ea6\u548c\u53d6\u5411\u7684\u7075\u6d3b\u6027\u53ef\u4ee5\u5b9a\u5236\uff0c\u4e3a\u8fd9\u79cd\u73b0\u8c61\u7684\u7814\u7a76\u5f00\u8f9f\u4e86\u65b0\u7684\u9014\u5f84\u3002\u8d85\u8367\u5149\u8109\u51b2\u77ed\u81f322 ps\uff081 ps\u4e3a10<sup>-12<\/sup>\u79d2\uff09\uff0c\u8fd9\u4f7f\u5f97\u8fd9\u4e9b\u8d85\u6676\u683c\u6210\u4e3a\u5177\u6709\u5438\u5f15\u529b\u7684\u6f5c\u5728\u5019\u9009\u8005\uff0c\u53ef\u7528\u4f5c\u9ad8\u80fd\u6548\u3001\u8d85\u5feb\u7684\u5149\u53d1\u5c04\u5668\u3002<\/p>\n<p><strong>\u3010\u7ed3\u8bba\u5c55\u671b\u3011<\/strong><\/p>\n<p>\u662f\u4ec0\u4e48\uff1f\u4f3c\u4e4e\u53ef\u884c\u7684\u662f\uff0c\u8d85\u6676\u683c\u7684\u5bb6\u65cf\u7684\u8fdb\u4e00\u6b65\u6269\u5927\u662f\u8fd9\u4e2a\u7814\u7a76\u9886\u57df\u7684\u4e0b\u4e00\u6b65\u76ee\u6807\u3002Cherniukh\u7b49\u4eba\u7b80\u8981\u5730\u62a5\u544a\u5236\u4f5c\u7684\u5177\u6709\u67f1\u72b6\u7ed3\u6784\u7684\u4e8c\u5143\u8d85\u6676\u683c\uff0c\u4ee5\u53ca\u5177\u6709\u7c7b\u4f3c\u4e8e\u4e8c\u787c\u5316\u94dd\u6676\u4f53\u7ed3\u6784\u7684\u5176\u4ed6\u8d85\u6676\u683c\u3002<\/p>\n<p>\u8fd9\u4e00\u53d1\u73b0\u8fd8\u53ef\u80fd\u6709\u52a9\u4e8e\u5f00\u53d1\u8d85\u8367\u5149\u7684\u5e94\u7528\uff0c\u8d85\u8367\u5149\u5df2\u5728\u5404\u79cd\u539f\u5b50\u3001\u5206\u5b50\u548c\u7eb3\u7c73\u5c3a\u5ea6\u7cfb\u7edf\u4e2d\u88ab\u89c2\u5bdf\u5230\uff0c\u4f46\u5c1a\u672a\u5728\u8bbe\u5907\u4e2d\u5f97\u5230\u5e94\u7528\u3002\u5b9a\u5236\u8d85\u6676\u683c\u76843D\u7ed3\u6784\u7684\u80fd\u529b\u53ef\u80fd\u63d0\u4f9b\u4e00\u79cd\u968f\u610f\u5b9a\u5236\u8d85\u8367\u5149\u7684\u65b9\u6cd5\uff0c\u4ece\u800c\u4f7f\u5176\u80fd\u591f\u88ab\u7528\u4f5c\u4f8b\u5982\u91cf\u5b50\u5149\u6e90\u3002\u53cd\u8fc7\u6765\uff0c\u8fd9\u53ef\u80fd\u9700\u8981\u8fdb\u4e00\u6b65\u7684\u52aa\u529b\u6765\u6539\u5584\u8d85\u6676\u683c\u7684\u4e09\u7ef4\u6709\u5e8f\u6027\uff0c\u5e76\u589e\u52a0\u53ef\u5236\u5907\u7684\u6750\u6599\u7684\u5c3a\u5bf8\uff0c\u4ece\u800c\u4e25\u683c\u4fdd\u6301\u6709\u5e8f\u6027\u3002\u5f53\u8d85\u6676\u683c\u88ab\u6574\u5408\u5230\u4e00\u4e2a\u88c5\u7f6e\u4e2d\u65f6\uff0c\u53ef\u80fd\u8fd8\u9700\u8981\u7814\u7a76\u7a33\u5b9a\u6709\u5e8f\u7ed3\u6784\uff0c\u53ef\u80fd\u662f\u901a\u8fc7\u4f7f\u7528\u7eb3\u7c73\u6676\u4f53\u4e4b\u95f4\u7684\u8fde\u63a5\u5206\u5b50\u3002<\/p>\n<p>\u4e0e\u6b64\u540c\u65f6\uff0c\u65b0\u7684\u53d1\u73b0\u4e3a\u7814\u7a76\u4eba\u5458\u5c1d\u8bd5\u591a\u79cd\u7eb3\u7c73\u6676\u4f53\u7684\u7ec4\u5408\u5f00\u8f9f\u4e86\u9053\u8def\uff0c\u8fd9\u4e9b\u7eb3\u7c73\u6676\u4f53\u5177\u6709\u4e0d\u540c\u7684\u5c5e\u6027\u2014\u2014\u6bd4\u5982\u53d1\u5149\u3001\u78c1\u6027\u6216\u7edd\u7f18\u7279\u6027\u2014\u4f5c\u4e3a\u8d85\u6676\u683c\u7684\u6784\u5efa\u5757\u3002\u8fd9\u53ef\u80fd\u5bfc\u81f4\u6750\u6599\u5177\u6709\u591a\u79cd\u529f\u80fd\uff0c\u6240\u6709\u8fd9\u4e9b\u529f\u80fd\u90fd\u53ef\u4ee5\u901a\u8fc7\u7eb3\u7c73\u6676\u4f53\u4e4b\u95f4\u7684\u7a7a\u95f4\u6392\u5217\u548c\u8ddd\u79bb\u6765\u63a7\u5236\u3002<\/p>\n<p>\u6587\u732e\u94fe\u63a5\uff1a<a href=\"https:\/\/www.nature.com\/articles\/d41586-021-01331-1\" target=\"_blank\" rel=\"noopener\">Nanocrystals form a superfluorescent lattice mimicking the atomic structure of perovskite materials<\/a> (<em>Nature <\/em><strong>2021<\/strong>, 593, 513-514)<\/p>\n<p>\u672c\u6587\u7531\u5927\u5175\u54e5\u4f9b\u7a3f\u3002<\/p>\n<p>\u6b22\u8fce\u5927\u5bb6\u5230\u6750\u6599\u4eba\u5ba3\u4f20\u79d1\u6280\u6210\u679c\u5e76\u5bf9\u6587\u732e\u8fdb\u884c\u6df1\u5165\u89e3\u8bfb\uff0c\u6295\u7a3f\u90ae\u7bb1\uff1a<a href=\"mailto:tougao@cailiaoren.com\">tougao@cailiaoren.com<\/a><\/p>\n<p>\u6295\u7a3f\u4ee5\u53ca\u5185\u5bb9\u5408\u4f5c\u53ef\u52a0\u7f16\u8f91\u5fae\u4fe1\uff1acailiaokefu<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u3010\u7814\u7a76\u80cc\u666f\u3011 \u9499\u949b\u77ff\u6676\u4f53\u662f\u76ee\u524d\u5e7f\u53d7\u5173\u6ce8\uff0c\u5176\u81f3\u5c11\u7531\u4e09\u79cd\u4e0d\u540c\u7684\u79bb\u5b50\u7ec4\u6210\uff0c\u4ee5\u5353\u8d8a\u7684\u7535\u5b66\u548c\u5149\u5b66\u7279\u6027\u800c\u95fb\u540d\uff0c\u5728\u592a\u9633\u80fd\u7535\u6c60\u548c\u5149\u7535\u5668\u4ef6\u4e2d\u5177\u6709\u7a81\u51fa\u7684\u5e94\u7528\u6f5c\u529b\u3002\u6709\u7814\u7a76\u8868\u660e\uff0c\u5f53\u9499\u949b&#8230;<\/p>\n","protected":false},"author":1004,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[234],"tags":[],"class_list":["post-223000","post","type-post","status-publish","format-standard","hentry","category-guandian"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/223000"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/1004"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=223000"}],"version-history":[{"count":4,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/223000\/revisions"}],"predecessor-version":[{"id":223091,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/223000\/revisions\/223091"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=223000"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=223000"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=223000"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}