{"id":225029,"date":"2021-07-25T06:30:29","date_gmt":"2021-07-24T22:30:29","guid":{"rendered":"http:\/\/www.cailiaoniu.com\/?p=225029"},"modified":"2021-07-24T21:44:43","modified_gmt":"2021-07-24T13:44:43","slug":"%e5%8d%97%e5%b7%a5%e5%a4%a7%e7%8e%8b%e7%90%b3%e6%95%99%e6%8e%88%e9%bb%84%e7%bb%b4%e9%99%a2%e5%a3%ab%e5%9b%a2%e9%98%9fnational-science-review%e7%bb%bc%e8%bf%b0%ef%bc%9a%e5%9f%ba%e4%ba%8e%e8%b6%85","status":"publish","type":"post","link":"http:\/\/www.cailiaoniu.com\/?p=225029","title":{"rendered":"\u5357\u5de5\u5927\u738b\u7433\u6559\u6388&#038;\u9ec4\u7ef4\u9662\u58eb\u56e2\u961fNational Science Review\u7efc\u8ff0\uff1a\u57fa\u4e8e\u8d85\u8584\u4e8c\u7ef4\u6742\u5316\u9499\u949b\u77ff\u7684\u67d4\u6027\u7535\u5b50\u548c\u5149\u7535\u5b50\u5e94\u7528&#8211;\u73b0\u72b6\u4e0e\u5c55\u671b"},"content":{"rendered":"<p><strong>\u5f15\u8a00\uff1a<\/strong><\/p>\n<p>\u65b0\u6750\u6599\u662f\u4eba\u7c7b\u8d56\u4ee5\u751f\u5b58\u7684\u7269\u8d28\u57fa\u7840\uff0c\u6bcf\u79cd\u65b0\u6750\u6599\u7684\u51fa\u73b0\u53ca\u5e94\u7528\u90fd\u5c06\u4f34\u968f\u7740\u73b0\u4ee3\u79d1\u5b66\u6280\u672f\u7684\u5de8\u5927\u98de\u8dc3\u3002\u65b0\u4e00\u4ee3\u67d4\u6027\u6750\u6599\u662f\u9769\u65b0\u73b0\u6709\u67d4\u6027\u7535\u5b50\u7684\u57fa\u7840\u3002\u65b0\u578b\u8d85\u8584\u4e8c\u7ef4\u6742\u5316\u9499\u949b\u77ff\u4e0d\u4f46\u5177\u6709\u4e8c\u7ef4\u6750\u6599\u7684\u7ed3\u6784\u7279\u5f81\uff0c\u800c\u4e14\u7ee7\u627f\u4e86\u6742\u5316\u9499\u949b\u77ff\u7684\u7269\u7406\u7279\u6027\uff0c\u4f8b\u5982\u5929\u7136\u7684\u67d4\u6027\u3001\u9ad8\u7684\u5438\u6536\/\u53d1\u5c04\u6548\u7387\u3001\u5927\u7684\u7f3a\u9677\u5bb9\u9650\u3001\u957f\u7684\u8ddd\u79bb\u8f7d\u6d41\u5b50\u6269\u6563\u7b49\uff0c\u975e\u5e38\u9002\u5408\u65b0\u578b\u67d4\u6027\u7535\u5b50\u548c\u5149\u7535\u5b50\u5668\u4ef6\u7684\u5f00\u53d1\u5e94\u7528\u3002<\/p>\n<p>\u8fd1\u5e74\u6765\uff0c\u8d85\u8584\u4e8c\u7ef4\u6742\u5316\u9499\u949b\u77ff\u56e0\u5176\u72ec\u7279\u7684\u4f18\u52bf\uff0c\u5305\u542b\u6709\u673a\u548c\u65e0\u673a\u4e24\u79cd\u6750\u6599\u7684\u7269\u7406\u7279\u5f81\uff0c\u5177\u6709\u79bb\u5b50\u8fc1\u79fb\u548c\u7535\u5b50\u4f20\u8f93\u7684\u53cc\u91cd\u8f93\u8fd0\u7279\u6027\uff0c\u4e0d\u4ec5\u9002\u7528\u4e8e\u65b0\u578b\u5149\u7535\u3001\u94c1\u7535\u3001\u78c1\u7535\u5668\u4ef6\u5f00\u53d1\uff0c\u800c\u4e14\u8fd8\u4fc3\u8fdb\u4e86\u4f4e\u529f\u8017\u3001\u591a\u529f\u80fd\u7684\u67d4\u6027\u7535\u5b50\u548c\u96c6\u6210\u7b49\u65b9\u9762\u7684\u53d1\u5c55\u3002<\/p>\n<p><strong>\u6210\u679c\u7b80\u4ecb\uff1a<\/strong><\/p>\n<p>\u8fd1\u671f\uff0c\u5357\u4eac\u5de5\u4e1a\u5927\u5b66\u738b\u7433\u6559\u6388\u548c\u9ec4\u7ef4\u9662\u58eb\uff08\u5171\u540c\u901a\u8baf\u4f5c\u8005\uff09\u7b49\u4eba\u57fa\u4e8e\u8d85\u8584\u4e8c\u7ef4\u6742\u5316\u9499\u949b\u77ff\u5149\u7535\u5b50\u5e94\u7528\u7684\u5feb\u901f\u53d1\u5c55\uff0c\u603b\u7ed3\u4e86\u8d85\u8584\u4e8c\u7ef4\u6742\u5316\u9499\u949b\u77ff\u7684\u5236\u5907\u65b9\u6cd5\u3001\u7269\u7406\u7279\u6027\u548c\u9002\u7528\u8303\u56f4\uff0c\u5e76\u5bf9\u5176\u6f5c\u5728\u7684\u67d4\u6027\u7535\u5b50\u548c\u5149\u7535\u5b50\u5e94\u7528\u7684\u53d1\u5c55\u673a\u9047\u548c\u53d1\u5c55\u524d\u666f\u8fdb\u884c\u4e86\u8ba8\u8bba\u3002\u9996\u5148\uff0c\u4f5c\u8005\u8be6\u7ec6\u603b\u7ed3\u4e86\u8d85\u8584\u4e8c\u7ef4\u9499\u949b\u77ff\u4e0e\u4f20\u7edf\u9499\u949b\u77ff\u5728\u751f\u957f\u65b9\u6cd5\u3001\u6676\u4f53\u7ed3\u6784\u548c\u7269\u7406\u6027\u8d28\u7684\u533a\u522b\u548c\u8054\u7cfb\u3002\u968f\u540e\uff0c\u603b\u7ed3\u4e86\u6742\u5316\u9499\u949b\u77ff\u5728\u5149\u7535\u9886\u57df\u7684\u5e94\u7528\uff0c\u5305\u62ecLED\uff0c\u6fc0\u5149\u5668\uff0c\u5149\u7535\u63a2\u6d4b\u5668\u4ee5\u53ca\u592a\u9633\u80fd\u7535\u6c60\u3002\u6700\u540e\uff0c\u6df1\u5165\u63a2\u8ba8\u4e86\u8d85\u8584\u4e8c\u7ef4\u6742\u5316\u9499\u949b\u77ff\u5728\u67d4\u6027\u5668\u4ef6\u5f00\u53d1\u548c\u5e94\u7528\u4e2d\u9047\u5230\u7684\u6311\u6218\uff0c\u5e76\u5bf9\u9499\u949b\u77ff\u5728\u672a\u6765\u67d4\u6027\u7535\u5b50\u3001\u5149\u7535\u5b50\u4e2d\u7684\u53d1\u5c55\u505a\u51fa\u4e86\u5c55\u671b\u3002\u8be5\u7efc\u8ff0\u4ee5\u9898\u4e3a\u201cUltrathin two-dimensional hybrid perovskites toward flexible electronics and optoelectronics \u201d\u53d1\u8868\u5728National Science Review\u4e0a\u3002<\/p>\n<p><strong>\u56fe\u6587\u5bfc\u8bfb\uff1a<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-225030 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/07\/1-6-e1627133857120.png\" alt=\"\" width=\"600\" height=\"446\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>1 <\/strong><strong>\u8d85\u8584\u4e8c\u7ef4\u6742\u5316\u9499\u949b\u77ff\u548c\u4f20\u7edf\u9499\u949b\u77ff\u5728\u6676\u4f53\u7ed3\u6784\u7ed3\u6784\u3001\u5236\u5907\u65b9\u6cd5\u548c\u7269\u7406\u7279\u6027\u4e0a\u7684\u533a\u522b\u548c\u5173\u8054\u3002<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"aligncenter wp-image-225031 size-full\" src=\"http:\/\/www.cailiaoniu.com\/wp-content\/uploads\/2021\/07\/2-5-e1627133868677.png\" alt=\"\" width=\"600\" height=\"448\" \/><\/p>\n<p><strong>\u56fe<\/strong><strong>2 <\/strong><strong>\uff08<\/strong><strong>a<\/strong><strong>\uff09\u5f53\u524d\u7684\u57fa\u4e8e\u6742\u5316\u9499\u949b\u77ff\u7684\u5149\u7535\u5668\u4ef6\u5e94\u7528\uff0c\u5305\u62ec<\/strong><strong>LED<\/strong><strong>\uff0c\u5149\u7535\u63a2\u6d4b\u5668\uff0c\u592a\u9633\u80fd\u7535\u6c60\u548c\u6fc0\u5149\u5668\u7b49\u3002\u8d85\u8584\u4e8c\u7ef4\u6742\u5316\u9499\u949b\u77ff\u5728\uff08<\/strong><strong>b<\/strong><strong>\uff09\u6750\u6599\u8bbe\u8ba1\u3001\uff08<\/strong><strong>c<\/strong><strong>\uff09\u6027\u80fd\u63a2\u7d22\u548c\uff08<\/strong><strong>c<\/strong><strong>\uff09\u5668\u4ef6\u96c6\u6210\u65b9\u9762\u7684\u5e94\u7528\u5c55\u671b\u3002<\/strong><\/p>\n<p>\u672c\u6587\u7531\u4f5c\u8005\u6295\u7a3f\u3002<\/p>\n","protected":false},"excerpt":{"rendered":"<p>\u5f15\u8a00\uff1a \u65b0\u6750\u6599\u662f\u4eba\u7c7b\u8d56\u4ee5\u751f\u5b58\u7684\u7269\u8d28\u57fa\u7840\uff0c\u6bcf\u79cd\u65b0\u6750\u6599\u7684\u51fa\u73b0\u53ca\u5e94\u7528\u90fd\u5c06\u4f34\u968f\u7740\u73b0\u4ee3\u79d1\u5b66\u6280\u672f\u7684\u5de8\u5927\u98de\u8dc3\u3002\u65b0\u4e00\u4ee3\u67d4\u6027\u6750\u6599\u662f\u9769\u65b0\u73b0\u6709\u67d4\u6027\u7535\u5b50\u7684\u57fa\u7840\u3002\u65b0\u578b\u8d85\u8584\u4e8c\u7ef4\u6742\u5316\u9499\u949b\u77ff\u4e0d&#8230;<\/p>\n","protected":false},"author":11454,"featured_media":0,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"footnotes":""},"categories":[215],"tags":[],"class_list":["post-225029","post","type-post","status-publish","format-standard","hentry","category-jiedu"],"_links":{"self":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/225029"}],"collection":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts"}],"about":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/users\/11454"}],"replies":[{"embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcomments&post=225029"}],"version-history":[{"count":1,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/225029\/revisions"}],"predecessor-version":[{"id":225032,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=\/wp\/v2\/posts\/225029\/revisions\/225032"}],"wp:attachment":[{"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fmedia&parent=225029"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Fcategories&post=225029"},{"taxonomy":"post_tag","embeddable":true,"href":"http:\/\/www.cailiaoniu.com\/index.php?rest_route=%2Fwp%2Fv2%2Ftags&post=225029"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}